A high heat dissipation fan-out packaging method and packaging structure
By using a combination technology of etched metal heat dissipation layer and high thermal conductivity film in fanout packages, the problems of complex process, high cost and poor heat dissipation of existing fanout packages are solved, and small-area packaging and high heat dissipation are achieved The effect meets the high reliability needs of high-power chips.
Patent Information
- Application Number
- CN202310652777.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-05
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2043-06-05
AI Technical Summary
The existing fan-out packaging methods have problems such as complex process, high cost, silicon-based fan-out packaging products that cannot be packaged with large thickness, plastic-sealed packaging, and large warping, which cannot meet the needs of small-area packaging and high heat dissipation.
The metal heat dissipation layer is made using ordinary silicon wafers, etching to form notches, sticking the chip and coating the film material, and re-wiring the signal to form a fan-out packaging structure with high heat conductivity, including the metal heat dissipation layer, chip, film material and wiring layer, achieving high heat dissipation and small area packaging.
It realizes small-area packaging, large-thickness chip packaging, good heat dissipation performance and high reliability, avoids metal oxidation corrosion and cutting collapse problems, shortens processing cycles and reduces costs.
Smart Images

Figure CN116581035B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of semiconductor technology, and in particular relates to a fan-out packaging method and packaging structure with high heat dissipation. Background Art
[0002] At present, fan-out packaging mainly includes two mainstream forms: silicon-based substrate fan-out and plastic-encapsulated substrate fan-out, but there are the following problems:
[0003] 1. The process is complex and the cost is high;
[0004] 2. The silicon-based fan-out substrate preparation process has limitations and cannot package products with thick chips. In addition, the silicon-based fan-out platform is large and cannot meet the packaging needs of small fan-out areas.
[0005] 3. The fan-out type package of the plastic encapsulated substrate has poor heat dissipation and large warpage, and requires the use of a temporary bonding process. Summary of the invention
[0006] In order to solve the technical problems existing in the prior art, an object of the present invention is to provide a fan-out packaging method and packaging structure with high heat dissipation.
[0007] In order to achieve the above purpose and the above technical effect, the technical solution adopted by the present invention is:
[0008] A high heat dissipation fan-out packaging method comprises the following steps:
[0009] 1) Prepare an ordinary silicon wafer, make a metal heat dissipation layer, then etch the metal heat dissipation layer, leaving only the metal heat dissipation layer at the bottom of the embedded chip, and form multiple gaps on the metal heat dissipation layer;
[0010] 2) Lay the chip with its functional surface facing upwards onto a silicon wafer with a metal heat dissipation layer in a certain arrangement;
[0011] 3) Cover the chip with film material around and on the surface to expose the chip pad metal layer;
[0012] 4) Lead the signal to the printed solder paste or solder ball by rewiring;
[0013] 5) Same as wafer-level packaging, separated into single chips.
[0014] Furthermore, in step 1), the metal heat dissipation layer is made by magnetron sputtering or evaporation, and the thickness of the metal heat dissipation layer is 5-20 μm.
[0015] Furthermore, in step 1), the gap is made by photolithography or wet etching of the metal heat dissipation layer, and the width of the gap is not less than 100 μm.
[0016] Furthermore, in step 2), the chip is bonded to the silicon wafer via a high thermal conductivity DAF film or conductive silver paste, and the thermal conductivity of the DAF film is 0.1-0.5 W / (m·K).
[0017] Furthermore, in step 4), the step of leading the signal to the printed solder paste or solder ball by rewiring includes:
[0018] A multi-layer wiring layer is formed by RDL rewiring, and then printed solder paste or solder balls are made on the wiring layer to realize the lead-out of chip signals;
[0019] If high reliability requirements are required, nickel-gold plating is performed on the surface of the wiring layer to prevent oxidation corrosion of the wiring layer, or a UBM pad layer is deposited under the tin solder ball.
[0020] Furthermore, the wiring layer is made of a metal material with good electrical conductivity, and the metal material includes Cu and Al.
[0021] The present invention also discloses a fan-out packaging structure with high heat dissipation, comprising:
[0022] Silicon wafer;
[0023] A metal heat dissipation layer is disposed on the silicon wafer, and has a plurality of notches;
[0024] The chip is arranged on the metal heat dissipation layer, avoiding the notch, with the functional surface of the chip facing upward;
[0025] The film material is wrapped around the chip and on the surface, exposing the chip pad metal layer;
[0026] Wiring layer;
[0027] Print solder paste or solder balls and place them on the wiring layer to lead out chip signals.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] 1) Compared with the existing silicon-based fan-out packaging method, the present invention can meet the packaging needs of small fan-out areas (single-side fan-out 20-30μm), and can also achieve packaging with thick embedded chips. It does not require silicon-based etching processes, and the yield and warping are more controllable. At the same time, it can meet the high heat dissipation requirements of high-power chips, and the heat dissipation metal layer around the separated chips is not exposed, which can avoid metal oxidation corrosion and the problem of chipping that affects cutting.
[0030] 2) Compared with the original fan-out package of plastic encapsulated substrate, the present invention has controllable warping in the process, and no temporary bonding process, which shortens the processing cycle and reduces the cost. At the same time, the product structure of the present invention can meet the high heat dissipation requirements of high-power chips, and the heat dissipation metal layer around the separated chip is not exposed, which can avoid the problems of metal oxidation corrosion and cutting chipping, and the method of filling the glue layer to wrap the edge solves the problem of poor bonding between the heat dissipation metal layer and the upper and lower layers, meeting the performance requirements of high reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1-2 They are respectively structural schematic diagrams of step 1) of a high heat dissipation fan-out packaging method and packaging structure of the present invention;
[0032] Figure 3 It is a structural schematic diagram of step 2) of a high heat dissipation fan-out packaging method and packaging structure of the present invention;
[0033] Figure 4 It is a structural schematic diagram of step 3) of a high heat dissipation fan-out packaging method and packaging structure of the present invention;
[0034] Figure 5 It is a structural schematic diagram of step 4) of a high heat dissipation fan-out packaging method and packaging structure of the present invention;
[0035] Figure 6-7 They are respectively structural schematic diagrams of step 5) of a high heat dissipation fan-out packaging method and packaging structure of the present invention;. DETAILED DESCRIPTION
[0036] The present invention is described in detail below so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention.
[0037] A brief summary of one or more aspects is given below to provide a basic understanding of these aspects. This summary is not an exhaustive overview of all conceived aspects, and is neither intended to identify the key or critical elements of all aspects nor to define the scope of any or all aspects. Its only purpose is to give some concepts of one or more aspects in a simplified form as a prelude to a more detailed description that will be given later.
[0038] like Figure 1-7 As shown, a high heat dissipation fan-out packaging method includes the following steps:
[0039] 1) If Figure 1As shown, prepare an ordinary silicon wafer 1, and make a metal heat dissipation layer 3 according to the size of the chip 2 to be embedded. The thickness of the metal heat dissipation layer 3 is 5-20μm. The thicker the better the heat dissipation, but the cost will increase. The metal heat dissipation layer 3 can be made by magnetron sputtering or evaporation. Generally, the metal is Ni, Ti, Ag, Cu, and Al. The former adopts one-step sputtering, generally depositing Ti, Cu, and Al, and the latter adopts evaporation, generally depositing Ti, Ni, and Ag. The order of evaporation is titanium layer, nickel layer, and silver layer respectively. The metal heat dissipation layer 3 mainly plays the following roles: used for heat dissipation of the back of the chip 2. When the chip 2 is working, heat loss occurs and heat is generated. The heat can be released by heat conduction through the metal on the back of the chip 2, thereby playing a role in heat dissipation; for products where the chip 2 has a back gold that needs to be grounded, the metal heat dissipation layer 3 can be used for heat conduction release, and can also be used for grounding the back of the chip 2;
[0040] Considering the influence of the metal heat dissipation layer 3 on the bonding strength of the post-process and the chipping during cutting, photolithography or wet etching can be used to only retain the metal heat dissipation layer 3 at the bottom of the chip 2, such as Figure 2 As shown, at this time, because the chips 2 are placed at intervals, a gap 4 will be formed on the metal heat dissipation layer 3. The size of the gap 4 is determined according to the chip size. Through photoresist coating, exposure, development, and wet etching, a metal gap width of more than 100μm is formed. The contact area between the encapsulation material and the bottom silicon wafer 1 can be increased at the gap 4, and the bonding force between the encapsulation material and the silicon wafer 1 is improved. Similarly, after the metal heat dissipation layer 3 around the edge of the chip 2 forms a gap 4, the bonding force between the surrounding encapsulation material and the silicon wafer 1 can be improved, and at the same time, the chipping of the edge cutting after packaging can be improved, and the deformation and breakage of the cutting knife can be reduced during cutting.
[0041] 2) Then use a high thermal conductivity DAF film or a point conductive silver paste to attach the chip 2 to the silicon wafer 1 with the functional surface facing upward in a certain arrangement. The thermal conductivity of the DAF film is 0.1-0.5W / (m·K). Figure 3 If the chip 2 mounting accuracy is to be improved, a mark at a fixed position may be formed by photolithography and wet etching in the previous process.
[0042] 3) By pressing a thick film, the chip 2 is covered with a film material 5 around and on the surface. The film material 5 can be a photolithography film material or a non-photolithography film material. The film on the PAD on the surface of the chip 2 can be opened by exposure, development or laser drilling to expose the metal layer of the chip pad. Figure 4 If it is a photolithography film material, the photoresist on the chip pad surface is opened by coating, exposure and development, and the opening size is more than 20μm, and then the material is solidified; if it is a non-photolithography film material, it is first baked and solidified, and then laser drilling and cleaning are used to open the photoresist on the chip pad surface, and the opening size is also more than 20μm.
[0043] 4) A multi-layer wiring layer 6 is formed by RDL rewiring. The material of the wiring layer 6 can be a metal material with good conductivity such as Cu and Al. If high reliability is required, nickel-gold can be plated on the outermost metal layer to prevent oxidation and corrosion of the RDL layer, or a UBM pad layer can be deposited under the solder ball. The signal is led out by rewiring, that is, the signal on the pad is led out to the printed solder paste or the solder ball 7 formed by ball implantation. Figure 5 shown.
[0044] 5) Finally, the back of the silicon wafer 2 is thinned to the target thickness, the tracking code is printed, the signal is tested, and the packaged chip 2 is separated into individual chips. If the bonding strength of the heat dissipation metal and the filling glue around the edge of the chip 2, the exposed heat dissipation metal at the edge is prone to corrosion, and the influence of cutting and chipping are not considered, the final package structure is as follows Figure 6 If the bonding strength of the heat dissipation metal and the filling glue around the edge of the chip 2, the exposed heat dissipation metal at the edge is prone to corrosion, and the influence of cutting and chipping are considered, the final package structure is as follows Figure 7 As shown, high reliability performance requirements can be met.
[0045] A high heat dissipation fan-out packaging structure, comprising:
[0046] Silicon wafer 1;
[0047] A metal heat dissipation layer 3 is disposed on the silicon wafer 1, and has a plurality of notches 4;
[0048] The chip 2 is arranged on the metal heat dissipation layer 3, avoiding the notch 4, and the functional surface of the chip 1 faces upward;
[0049] The film material 5 is coated around and on the surface of the chip 2, exposing the chip pad metal layer;
[0050] Wiring layer 6;
[0051] Printed solder paste or solder balls 7 are arranged on the wiring layer 6 to realize the lead-out of the chip 1 signal.
[0052] Parts or structures not specifically described in the present invention may adopt existing technologies or existing products and will not be described in detail here.
[0053] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A high heat dissipation fan-out packaging method, characterized in that: The following steps are involved: 1) Prepare a common silicon wafer, make a metal heat dissipation layer, then etch the metal heat dissipation layer, leaving only the metal heat dissipation layer at the bottom of the embedded chip, and form multiple gaps on the metal heat dissipation layer; 2) Lay the chip with its functional surface facing upwards onto a silicon wafer with a metal heat dissipation layer in a certain arrangement; 3) Cover the chip with film material around and on the surface to expose the chip pad metal layer; 4) Lead the signal to the printed solder paste or solder ball by rewiring; 5) Separate into single chips with wafer-level packaging; In step 1), the metal heat dissipation layer is formed by magnetron sputtering or evaporation, and the thickness of the metal heat dissipation layer is 5-20 μm; In step 1), the gap is made by photolithography or wet etching of the metal heat dissipation layer, and the width of the gap is not less than 100 μm.
2. A high heat dissipation fan-out packaging method according to claim 1, characterized in that: In step 2), the chip is bonded to the silicon wafer via a high thermal conductivity DAF film or conductive silver paste, wherein the thermal conductivity of the DAF film is 0.1-0.5 W / (m·K).
3. A high heat dissipation fan-out packaging method according to claim 1, characterized in that: In step 4), the step of leading the signal to the printed solder paste or solder ball by rewiring includes: A multi-layer wiring layer is formed by RDL rewiring, and then printed solder paste or solder balls are made on the wiring layer to realize the lead-out of chip signals; If high reliability requirements are required, nickel-gold plating is performed on the surface of the wiring layer to prevent oxidation corrosion of the wiring layer, or a UBM pad layer is deposited under the tin solder ball.
4. A high heat dissipation fan-out packaging method according to claim 3, characterized in that: The wiring layer is made of a metal material with good electrical conductivity, and the metal material includes Cu and Al.
5. A fan-out packaging structure with high heat dissipation, characterized in that: The high heat dissipation fan-out packaging method according to any one of claims 1 to 4 is used to prepare the device, comprising: Silicon wafer; A metal heat dissipation layer is disposed on the silicon wafer, and has a plurality of notches; The chip is arranged on the metal heat dissipation layer, avoiding the notch, with the functional surface of the chip facing upward; The film material is wrapped around the chip and on the surface, exposing the chip pad metal layer; Wiring layer; Print solder paste or solder balls and place them on the wiring layer to lead out chip signals.