Structural component and manufacturing method thereof, and electronic equipment

By processing the main body of the structure and the raised structure separately and assembling them into integral structural parts, the problems of low raw material utilization rate and large weight of the whole machine during CNC processing and forming are solved, and the cost reduction and lightweighting effects are achieved.

CN116727549BActive Publication Date: 2024-11-05HONOR DEVICE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211072285.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-09-02
Publication Date
2024-11-05
Estimated Expiration
2042-09-02

AI Technical Summary

Technical Problem

In the prior art, when the structural parts of consumer electronic products are processed and molded by CNC, the raw material utilization rate is low, resulting in high production costs, and the material density of the raised structure increases the weight of the whole machine, making it difficult to achieve lightness and thinness.

Method used

The first raw material is used to process the structural body and the second raw material is used to process the raised structure, and it is assembled into an integral structural part through the connection process, and the weight is reduced by using low-density materials to reduce production costs and mold design difficulties.

Benefits of technology

It improves the utilization rate of raw materials, reduces the production cost of structural parts, reduces the weight of the whole machine, realizes modular design and reuse of processing fixtures and molds, and meets the lightweight and thinning needs of electronic equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116727549B_ABST
    Figure CN116727549B_ABST
Patent Text Reader

Abstract

The present application provides a structural part and a manufacturing method thereof, and an electronic device. The manufacturing method of the structural part adopts a first raw material to process the structural body, adopts a second raw material to process the raised structure, and then connects the raised structure and the structural body that are processed separately through a connection process to form a whole structural part. In this way, the processing difficulty of the structural part can be reduced, excessive waste of raw materials can be avoided, the design difficulty and processing cost of the mold can be reduced, and the production cost of the structural part can be reduced; and the second raw material for making the raised structure can be a low-density material different from the first raw material for making the structural body, which can achieve weight reduction of the structural part, thereby reducing the weight of the whole electronic device. For the same series of products, it is conducive to realizing modular design and improving production efficiency, and it can also increase the reuse ratio of processing jigs and molds, and reduce the cost of jigs and molds.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of electronic equipment, and in particular to a structural component and a manufacturing method thereof, and electronic equipment. Background Art

[0002] Structural parts of consumer electronic products, such as the middle frame of mobile phones, the back cover of tablet computers, the bottom cover of laptop computers, etc., often need to design complex raised structures, such as screw bosses, battery compartment partitions, microphone support platforms, etc., in order to carry components such as main circuit boards, batteries, and display screens.

[0003] In the related art, the above-mentioned protruding structure is usually integrally formed on the structural part, that is, the protruding structure and the main structure of the structural part are integrally processed and formed, for example, the protruding structure and the main structure of the structural part are integrally processed and formed by CNC (Computerized Numerical Control). However, the utilization rate of raw materials is low in the structural parts integrally formed by CNC processing, and a large amount of raw materials are cut off and become waste during the CNC processing process, which causes the CNC processing machine to increase, resulting in high cost of the processed structural parts. Summary of the invention

[0004] The present application provides a structural component and a manufacturing method thereof, and an electronic device. The manufacturing method of the structural component can improve the utilization rate of raw materials, simplify mold design, and reduce the manufacturing cost of the structural component.

[0005] In a first aspect, the present application provides a method for manufacturing a structural member, which is used to form a structural member having a protruding structure, and the manufacturing method comprises:

[0006] Using a first raw material to process and form a structural body having a plate portion;

[0007] The second raw material is used to form a raised structure;

[0008] The protruding structure is connected to the plate surface of the plate portion to form a structural member.

[0009] The manufacturing method of the structural part provided in the present application is to use a first raw material to process the structural body, use a second raw material to process the raised structure, and then connect the raised structure and the structural body that are separately processed together through a connection process to form a whole structural part. In this way, the processing difficulty of the structural part can be reduced, excessive waste of raw materials can be avoided, the design difficulty and processing cost of the mold can be reduced, and the production cost of the structural part can be reduced; and the second raw material for making the raised structure can be a low-density material different from the first raw material for making the structural body, which can achieve weight reduction of the structural part, thereby reducing the weight of the entire electronic device. For the same series of products, it is conducive to realizing modular design and improving production efficiency, and it can also increase the reuse ratio of processing jigs and molds, and reduce the cost of jigs and molds.

[0010] In one possible implementation, the second raw material is different from the first raw material.

[0011] By using different materials to make the main structure and the raised structure respectively, the appropriate material can be selected to process the raised structure according to the force requirements, functional requirements and other conditions of the raised structure, thereby expanding the selection range of raw materials for making the raised structure and reducing the production cost of the structural parts.

[0012] In a possible implementation, the density of the second raw material is smaller than the density of the first raw material.

[0013] By selecting a material with a lower density to make the raised structure, the weight of the raised structure can be reduced, and the overall weight of the structural component can be reduced, thereby achieving the purpose of reducing the weight of the entire electronic device and meeting the demand for thinner and lighter electronic devices.

[0014] In a possible implementation, the second raw material is the same as the first raw material.

[0015] By using the same material to make the main structure and the protruding structure respectively, it is easy to prepare the ingredients, and only one material needs to be prepared to form the entire structure. In addition, since the second raw material is the same as the first raw material, there are fewer restrictions on the connection process between the protruding structure and the main structure, which can ensure that the protruding structure and the main structure are firmly connected.

[0016] In a possible implementation, the first raw material includes metal materials, inorganic non-metallic materials, organic polymer materials and modified materials and composite materials thereof.

[0017] In a possible implementation manner, processing to form a structural main body includes:

[0018] The structural body is formed by at least one molding process selected from CNC machining, die casting, stamping, 3D printing, hot bending, sintering, injection molding, compression molding, transfer molding, SMC, and hand lay-up molding.

[0019] In a possible implementation, the second raw material includes metal materials, inorganic non-metallic materials, organic polymer materials and modified materials thereof, composite materials, foamed materials, and aerogels.

[0020] In a possible implementation manner, forming the protruding structure by processing includes:

[0021] The structural body is formed by at least one molding process selected from the group consisting of CNC machining, die casting, stamping, 3D printing, hot bending, sintering, injection molding, compression molding, transfer molding, and SMC hand lay-up molding.

[0022] In a possible implementation, connecting the protruding structure to the board surface of the board portion includes:

[0023] The protruding structure is connected to the plate surface of the plate part by at least one connection process selected from welding, bonding, locking, riveting, hot-melt connection, mechanical clamping, and interference fit.

[0024] In a possible implementation, the protruding structure is connected to the board surface of the board portion by a bonding process, including:

[0025] The protruding structure is bonded to the board surface of the board part by at least one dispensing process selected from the group consisting of jet dispensing, contact dispensing and manual dispensing.

[0026] In a possible implementation, connecting the protruding structure to the board surface of the board portion includes:

[0027] The protruding structure is connected to the board surface of the board part by at least one of automated equipment assembly, fixture assembly, and manual assembly.

[0028] In a second aspect, the present application provides a structural component, which is manufactured by the manufacturing method described above.

[0029] The structural part provided by the present application includes a structural body and a protruding structure connected to the structural body. The structural body is processed by a first raw material, the protruding structure is processed by a second raw material, and the protruding structure and the structural body processed separately are connected together through a connection process to form a whole structural part. In this way, the processing difficulty of the structural part can be reduced, excessive waste of raw materials can be avoided, the design difficulty and processing cost of the mold can be reduced, and the production cost of the structural part can be reduced; and the second raw material for making the protruding structure can be a low-density material different from the first raw material for making the structural body, which can achieve weight reduction of the structural part, thereby reducing the weight of the whole electronic device. For the same series of products, it is conducive to realizing modular design and improving production efficiency, and it can also increase the reuse ratio of processing jigs and molds, and reduce the cost of jigs and molds.

[0030] In a third aspect, the present application provides an electronic device, comprising the structural component as described above.

[0031] The electronic device provided by the present application includes a structural part, and the structural part includes a structural body and a protruding structure connected to the structural body. The structural body is processed by using a first raw material, and the protruding structure is processed by using a second raw material, and then the protruding structure and the structural body processed separately are connected together through a connection process to form a structural part as a whole. In this way, the processing difficulty of the structural part can be reduced, excessive waste of raw materials can be avoided, the design difficulty and processing cost of the mold can be reduced, and the production cost of the structural part can be reduced; and the second raw material for making the protruding structure can be a low-density material different from the first raw material for making the structural body, which can achieve weight reduction of the structural part, thereby reducing the weight of the whole electronic device. For the same series of products, it is conducive to realizing modular design and improving production efficiency, and it can also increase the reuse ratio of processing jigs and molds, and reduce the cost of jigs and molds. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 A schematic diagram of the structure of an electronic device provided in an embodiment of the present application;

[0033] Figure 2 for Figure 1 Exploded diagram of

[0034] Figure 3 A front view of a battery, a main circuit board and a secondary circuit board provided in an embodiment of the present application assembled in a middle frame;

[0035] Figure 4 for Figure 3 Partial cross-sectional view at AA in the middle;

[0036] Figure 5a A schematic diagram of a structure in which a main circuit board provided in an embodiment of the present application is assembled in a middle frame;

[0037] Figure 5b Another structural schematic diagram of a main circuit board provided in an embodiment of the present application being assembled in a middle frame;

[0038] Figure 6 A schematic diagram of a structure in which a microphone installed on a main circuit board and a supporting platform thereof are assembled on a middle frame provided in an embodiment of the present application;

[0039] Figure 7 This is a schematic diagram of the partition strips formed integrally on the middle frame through CNC processing technology;

[0040] Figure 8 A schematic diagram of a partition bar formed integrally on a middle frame by a die-casting process;

[0041] Fig. 9A schematic diagram of a process for manufacturing a structural member provided in an embodiment of the present application;

[0042] Fig.10 A process flow chart of manufacturing a middle frame provided in an embodiment of the present application;

[0043] Fig.11 Another process flow chart of manufacturing the middle frame provided in the embodiment of the present application;

[0044] Fig.12 A third manufacturing process flow chart of the middle frame provided in an embodiment of the present application.

[0045] Description of reference numerals:

[0046] 1- Electronic equipment;

[0047] 10-Structural parts; 10a-Raw materials; 10b-Excess materials;

[0048] 11-structural body; 12-convex structure;

[0049] 121-partitioning strip; 122-mounting boss; 123-positioning column; 124-bearing platform;

[0050] 1211-connecting part; 1212-partitioning part; 1241-sound transmission channel;

[0051] 100-housing; 200-display screen; 300-battery; 400-main circuit board; 500-sub-circuit board; 600a-microphone; 600b-speaker;

[0052] 110-middle frame; 120-back cover;

[0053] 110a-middle frame body; 111-frame portion; 112-middle plate portion; 113-back glue; 114-screws;

[0054] 111a-sound inlet hole; 111b-sound outlet hole; 1121-positioning groove;

[0055] 2- Die casting mold;

[0056] 21-upper template; 22-lower template; 23-cavity;

[0057] 211-slot section;

[0058] a-first raw material; b-second raw material; c-bonding material. DETAILED DESCRIPTION

[0059] The terms used in the implementation section of this application are only used to explain the specific embodiments of this application and are not intended to limit this application.

[0060] The embodiment of the present application provides an electronic device, which can be a consumer electronic product. Exemplarily, the electronic device includes but is not limited to a mobile phone, a tablet computer (portable android device, PAD), a notebook computer (NoteBook Computer, referred to as: NoteBook), an ultra-mobile personal computer (ultra-mobile personal computer, UMPC), a walkie-talkie, a netbook, a POS (Point of sales) machine, a personal digital assistant (personal digital assistant, PDA), a wearable device, a virtual reality (virtual reality, VR) device, an augmented reality (augmented reality, AR) device, etc. The embodiment of the present application does not specifically limit the form of the terminal device.

[0061] In order to support components such as circuit boards, batteries, microphones, and camera modules, the structural parts of electronic products (such as the middle frame of a mobile phone, the back cover of a tablet computer, the bottom cover of a laptop computer, etc.) usually need to be designed with complex raised structures, such as mounting bosses for fixing circuit boards, positioning columns, battery compartment partition bars, microphone support platforms, etc.

[0062] Figure 1 This is a schematic diagram of the structure of an electronic device provided in an embodiment of the present application. Figure 1 As shown, taking the electronic device 1 as a mobile phone as an example, the electronic device 1 may include a housing 100 and a display screen 200. One side surface of the display screen 200 is used to display image information. This side surface of the display screen 200 is usually defined as its front side, and the other side surface opposite to its front side is its back side. The housing 100 is arranged around the side and back side of the display screen 200 to support and fix the display screen 200. The front side of the display screen 200 is exposed outside the housing 100 so that the user can view the display content of the display screen 200 or perform input operations on the electronic device 1. The display screen 200 and the housing 100 together enclose a storage space, and some devices of the electronic device 1 are arranged in the storage space. For example, the circuit board, battery 300, microphone 600a, camera module and other devices as mentioned above are arranged in the storage space.

[0063] Generally, the side surface where the display screen 200 is located is defined as the front surface of the electronic device 1, and the other side surface of the electronic device 1 opposite to the front surface is defined as the back surface thereof. When describing various components in the electronic device 1 below, corresponding to the front and back surfaces of the electronic device 1, the "front surface" of a component refers to the side surface of the component facing the front surface of the electronic device 1, and the "back surface" of a component refers to the side surface of the component facing the back surface of the electronic device 1.

[0064] Figure 2for Figure 1 Exploded view of . Figure 2 As shown, the housing 100 of the electronic device 1 may include a middle frame 110 and a back cover 120, the back cover 120 is located at the back of the electronic device 1, the middle frame 110 is connected between the display screen 200 and the back cover 120, the display screen 200 is supported on the front of the middle frame 110, and the back cover 120 is connected to the back of the middle frame 110. Among them, the middle frame 110 may include a frame portion 111 and a middle plate portion 112, the frame portion 111 is arranged around the display screen 200 and the back cover 120, the middle plate portion 112 is located in the area surrounded by the frame portion 111, and the edge of the middle plate portion 112 is connected to the inner side wall of the frame portion 111. Exemplarily, the middle plate portion 112 and the frame portion 111 may be an integrally formed structure.

[0065] Exemplarily, the display screen 200 is supported as a whole on the middle plate portion 112 of the middle frame 110, and the edge of the display screen 200 overlaps the front end surface of the frame portion 111 of the middle frame 110 (the end surface of the frame portion 111 facing the front of the electronic device 1), and the display screen 200 can be connected and fixed to the middle frame 110 by means of a frame glue. The edge of the back cover 120 overlaps the rear end surface of the frame portion 111 of the middle frame 110 (the end surface of the frame portion 111 facing the back of the electronic device 1), and can be connected and fixed to the frame portion 111 by means of a frame glue. There is a gap between the middle plate portion 112 of the middle frame 110 and the back cover 120, and the gap forms a receiving space as described above, so that a device can be set in the receiving space between the middle plate portion 112 of the middle frame 110 and the back cover 120. As mentioned above, as a structural member 10 for supporting and fixing the screen and the back cover 120 , a complex protruding structure 12 is usually provided on the middle frame 110 , and these components are supported, fixed or positioned by the protruding structure 12 .

[0066] The following uses the middle frame 110 as the structural member 10 to exemplarily illustrate the protruding structure 12 on the structural member 10 .

[0067] Figure 3 A front view of a battery, a main circuit board and a secondary circuit board provided in an embodiment of the present application assembled in a middle frame; Figure 4 for Figure 3 Partial cross-sectional view at AA. Figure 3 As shown in the figure, the raised structure 12 provided on the middle frame 110 is taken as a partition bar 121 as an example. Figure 3 and Figure 4 As shown, the partition strip 121 is, for example, a strip-shaped structure raised on the surface (e.g., the back side) of the middle plate portion 112 of the middle frame 110. The partition strip 121 can, for example, extend along the width direction (X direction) of the middle frame 110. The function of the partition strip 121 is to separate a battery compartment (not shown in the figure) on the back side of the middle frame 110. The battery compartment is the area where the battery 300 is arranged.

[0068] Figure 3 It is shown that two raised partition bars 121 are provided at intervals on the back of the middle frame 110. After the middle frame 110 and the back cover 120 are assembled, there may be a gap between the partition bar 121 and the back cover 120, or the partition bar 121 may abut against the back cover 120 or be connected to the back cover 120 by bonding or the like. The area between the two partition bars 121 in the space between the middle frame 110 and the back cover 120 forms a battery compartment, and the battery 300 may be installed in this area. The areas on both sides of the two partition bars 121 may be used to install other devices. For example, the side area of ​​one partition bar 121 is used to set the main circuit board 400, which is the core circuit board for controlling the electronic device 1, and the side area of ​​the other partition bar 121 is used to set the auxiliary circuit board 500, which is mainly used to control a single component or several components. For example, the auxiliary circuit board 500 is used to control the display screen 200, and the auxiliary circuit board 500 may be electrically connected to the main circuit board 400. Refer to Figure 4 As shown, the battery 300 can be bonded to the middle frame 110 by, for example, adhesive 113 , and the main circuit board 400 can be fixed to the middle frame 110 by, for example, screws 114 .

[0069] It should be understood that Figure 3 This is an example of a method of setting the partition bar 121 on the middle frame 110. In actual applications, there may be one or more than three partition bars 121 set on the middle frame 110. The partition bar 121 may also extend along the length direction (Y direction) of the middle frame 110, or the partition bar 121 may also extend obliquely (the extension direction is a direction between the X direction and the Y direction). This embodiment does not limit this.

[0070] Figure 5a A schematic diagram of a structure in which the main circuit board provided in the embodiment of the present application is assembled in the middle frame. Figure 5a As shown, for the method of locking the main circuit board 400 on the middle frame 110, the protruding structure 12 provided on the middle frame 110 generally further includes a mounting boss 122, the mounting boss 122 protrudes on the surface (e.g., the back surface) of the middle plate portion 112 of the middle frame 110, and a screw hole (not shown in the figure) is provided on the mounting boss 122, and the main circuit board 400 is locked on the middle frame 110 by means of screws 114 screwed into the screw holes. For example, as shown in FIG. Figure 5a As shown in , the main circuit board 400 is provided with an avoidance groove. When the main circuit board 400 is installed, the avoidance groove on the main circuit board 400 corresponds to the mounting boss 122 on the middle frame 110. The avoidance groove is used to accommodate the mounting boss 122. On the one hand, the main circuit board 400 can be roughly positioned, and on the other hand, the space occupied by the main circuit board 400 is reduced.

[0071] Figure 5bAnother structural schematic diagram of the main circuit board provided in the embodiment of the present application being assembled in the middle frame. Figure 5b As shown, in order to accurately position the main circuit board 400, in some embodiments, the protruding structure 12 provided on the middle frame 110 may further include a positioning column 123. The positioning column 123 may, for example, extend out from the surface (e.g., the back side) of the middle plate portion 112 of the middle frame 110. Accordingly, a positioning hole (not shown in the figure) may be provided on the main circuit board 400. When assembling the main circuit board 400, align the positioning hole of the main circuit board 400 with the positioning column 123 on the middle frame 110 so that the positioning column 123 passes through the positioning hole of the main circuit board 400 to position the main circuit board 400.

[0072] Figure 6 This is a schematic diagram of a structure in which a microphone installed on a main circuit board and a supporting platform thereof are assembled on a middle frame according to an embodiment of the present application. Figure 6 As shown, in order to support the microphone 600a, the protruding structure 12 provided on the middle frame 110 may further include a bearing platform 124. The bearing platform 124 may, for example, be protruded on the surface (e.g., the back surface) of the middle plate portion 112 of the middle frame 110. The microphone 600a may, for example, be mounted on the surface of the main circuit board 400 facing the middle frame 110. The microphone 600a is arranged opposite to the bearing platform 124. When the main circuit board 400 is assembled, the microphone 600a is supported on the bearing platform 124. A sound transmission channel 1241 is provided in the bearing platform 124. One end of the sound transmission channel 1241 is connected to the outside world. The other end of the sound transmission channel 1241 extends to the surface of the bearing platform 124 supporting the microphone 600a. The sound transmission channel 1241 serves as a sound receiving channel. The sound signal from the outside world is transmitted to the microphone 600a through the sound receiving channel.

[0073] Exemplarily, the carrier 124 can be arranged near the edge of the middle frame 110, for example, the carrier 124 can be fitted with the frame portion 111 of the middle frame 110, so that the sound receiving channel on the carrier 124 is connected to the sound inlet 111a provided on the frame portion 111, and accordingly, the microphone 600a can also be arranged near the frame portion 111, and the microphone 600a can be mounted on the edge area of ​​the circuit board near the frame portion 111, for example. External sound signals enter the electronic device 1 through the air inlet and are transmitted to the microphone 600a through the sound receiving channel.

[0074] It should be stated that Figure 6Taking the microphone 600a that converts sound signals into electrical signals as an example, the support method of the microphone 600a on the middle frame 110 and the channel for collecting sound signals are explained. In addition to the microphone 600a, the transducer set in the electronic device 1 usually also includes a speaker 600b. Contrary to the signal conversion method of the microphone 600a, the speaker 600b converts the electrical signal into a sound signal and outputs it to the outside. Similar to the microphone 600a, the speaker 600b can also adopt the following method: Figure 6 The support platform 124 shown is supported on the middle frame 110. At this time, the sound transmission channel 1241 set in the support platform 124 can be used as a sound output channel, and the sound output channel can be connected to the sound output hole 111b set on the frame portion 111. The sound signal emitted by the speaker 600b is transmitted to the outside world through the sound output channel and the sound output hole 111b in turn.

[0075] The above lists that the raised structure 12 set on the middle frame 110 may include a partition bar 121 for separating the battery compartment, a mounting boss 122 for installing screws 114 to lock the main circuit board 400, a positioning column 123 for positioning the main circuit board 400, and a supporting platform 124 for supporting the microphone 600a / speaker 600b. It can be understood that in actual applications, the middle frame 110 may also have other raised structures 12 for fixing or limiting other devices. The embodiments of the present application do not limit the number, shape, position, function, etc. of the raised structures 12 on the middle frame 110.

[0076] In the related art, the above-mentioned protruding structure 12, such as the partition bar 121, the mounting boss 122, the positioning column 123 and the bearing platform 124, is usually integrally formed on the middle frame 110, for example, the protruding structure 12 is integrally formed on the surface of the middle plate portion 112 of the middle frame 110. The following are some examples of the manner in which the protruding structure 12 is integrally formed on the middle frame 110.

[0077] In some embodiments, a CNC (Computerized Numerical Control) processing technique may be used to integrally form the middle frame 110 and the protruding structure 12 protruding from the middle frame 110 . Figure 7 This is a schematic diagram of the partition strips integrated into the middle frame through CNC processing technology. Figure 7 As shown, taking the raised structure 12 on the middle frame 110 as the partition bar 121 as an example, for details, refer to Figure 7 As shown, a raw material 10a is provided first, and the raw material 10a is, for example, a metal material. Figure 7 As shown, the raw material 10 a is then cut to remove excess material 10 b , thereby forming the middle frame 110 and the partition strips 121 protruding from the middle frame 110 .

[0078] It can be understood that, in addition to the partition strip 121, other raised structures 12 on the middle frame 110 can also be integrally formed on the middle frame 110 through CNC processing technology. For example, the above-mentioned mounting boss 122, positioning column 123 and supporting platform 124 can all be integrally formed on the middle frame 110 through CNC processing technology. Here, only the partition strip 121 is used as an example for explanation.

[0079] In other embodiments, a die-casting process may be used to integrally form the middle frame 110 and the protruding structure 12 protruding from the middle frame 110 . Figure 8 This is a schematic diagram of the partition strips formed integrally on the middle frame through the die-casting process. Figure 8 As shown in the figure, a cross-sectional view of a partial structure of the die-casting mold 2 is shown. Since a raised partition bar 121 needs to be formed on the middle frame 110, the cavity 23 of the die-casting mold 2 needs to be designed with a fine structure corresponding to the partition bar 121, that is, a fine groove section 211 needs to be processed on the upper mold plate 21 or the lower mold plate 22 (the upper mold plate 21 is taken as an example in the figure) of the die-casting mold 2. Figure 8 As shown, liquid raw materials (such as molten metal) are injected into the die-casting mold 2, and after the raw materials are cooled, the middle frame 110 with the partition bars 121 can be formed.

[0080] Similarly, in addition to the partition strip 121, other protruding structures 12 on the middle frame 110, such as the above-mentioned mounting boss 122, positioning column 123 or supporting platform 124, can also be integrally formed on the middle frame 110 through a die-casting process. Here, only the partition strip 121 is used as an example for explanation.

[0081] In addition, the middle frame 110 and the protruding structure 12 protruding from the middle frame 110 can also be integrally formed by an injection molding process. For example, for the support platform 124 supporting the microphone 600a / speaker 600b, the support platform 124 has a sound transmission channel 1241, and in order to ensure the effect of the microphone 600a / speaker 600b, it is required that the support platform 124 and the microphone 600a / speaker 600b have good sealing. The support platform 124 can be made of a material different from that of the middle frame 110. In this case, the middle frame 110 and the support platform 124 can be integrally formed by an injection molding process. On the one hand, it is convenient to form the support platform 124 with a complex structure, and on the other hand, it can also meet the different material requirements of the support platform 124 and the middle frame 110.

[0082] However, for the integrated molding of the middle frame 110 and the raised structure 12 on the middle frame 110 by CNC machining, it is necessary to provide a raw material 10a with a relatively large thickness, and then, the thickness of the middle frame 110 is retained, and all parts other than the raised structure 12 are cut off, so a large amount of raw material 10a is cut and becomes waste, and the utilization rate of the raw material 10a is low, resulting in a high production cost of the middle frame 110. In addition, in order to ensure the strength of the middle frame 110 and the appearance of the electronic device 1, the middle frame 110 is usually made of metal material. In this way, when the raised structure 12 on the middle frame 110 is integrated by CNC machining, the raised structure 12 must also be made of the same metal material as the middle frame 110, and the density of the raised structure 12 is high, which increases the weight of the whole device.

[0083] For the integrally formed middle frame 110 and the protruding structure 12 on the middle frame 110 by the die-casting process or the injection molding process, the corresponding fine structures need to be processed at the positions corresponding to the protruding structure 12 on the die-casting mold 2 or the injection mold, which increases the design difficulty and processing cost of the mold. The mold (especially the die-casting mold 2) places high requirements on the fluidity of the liquid raw materials, which limits the selection range of the raw materials.

[0084] It should be noted that the above only takes the middle frame 110 as an example to illustrate the raised structure 12 on the middle frame 110 and the method of integrally forming the raised structure 12 on the middle frame 110 in the related technology. In actual applications, almost all structural parts 10 for supporting and fixing related devices of consumer electronic products are provided with similar raised structures 12. For example, the structural parts 10 of electronic devices such as the back shell of the tablet computer, the bottom shell of the laptop computer, the bottom shell of the netbook, the shell of the wearable device, etc. mentioned above are all provided with raised structures 12, which will not be repeated here.

[0085] In view of this, the embodiment of the present application improves the manufacturing method of the structural part in the electronic device, forms the structural body and the protruding structure of the structural part by separate processing, and then connects the protruding structure to the structural body to assemble the structural part. The processing difficulty of the structural part is reduced, the waste of raw materials is avoided, and the protruding structure can be processed by matching and selecting appropriate materials, which can reduce the overall weight of the structural part; for the structural body and / or protruding structure of the structural part formed by the die-casting molding process or the injection molding process, the design difficulty and processing cost of the mold can be reduced, and the requirements for the fluidity of the liquid raw materials are also reduced.

[0086] The following is a detailed description of the method for manufacturing the structural member of the embodiment of the present application.

[0087] It should be understood that for different types of electronic devices, the structural member 10 used to support, fix and limit the corresponding devices is different. Exemplarily, the structural member 10 can be the aforementioned middle frame of the mobile phone, the back shell of the tablet computer, the bottom shell of the notebook computer, the bottom shell of the netbook, the housing of the wearable device and other components. This embodiment does not specifically limit the shape, size and position of the structural member 10 in the electronic device.

[0088] Fig. 9 This is a schematic diagram of the process of manufacturing a structural member provided in an embodiment of the present application. Fig. 9 As shown, when processing and manufacturing a structural part with a protruding structure, a first raw material can be used to process and form a structural main body, and the structural main body has a plate portion. At the same time, a second raw material can be used to process and form a protruding structure. Thereafter, the protruding structure is connected to the plate surface of the plate portion of the structural main body through a connection process to assemble to form a structural part.

[0089] According to the position and function of the structural part in the electronic device, the plate portion of the structural body may include a flat plate portion, that is, the plate surface of at least part of the plate portion is a plane, or the plate portion of the structural body as a whole has a certain curvature, the plate surface of the plate portion is a curved surface with a certain curvature, or the plate portion may also be in other shapes. In addition, for the raised structure connected to the plate surface of the plate portion of the structural body, according to the function of the raised structure, the raised structure may be located at different positions on the plate portion, and the raised structure may also have different shapes, which is not limited in this embodiment.

[0090] Continuing to take the middle frame of the mobile phone as an example, refer to Figure 2 As shown, the structural body 11 of the structural member 10 may include a frame portion 111 of the middle frame 110 and a middle plate portion 112 connected to the inner side of the frame portion 111. The plate portion of the structural body 11 is the middle plate portion 112 of the middle frame 110. The protruding structure 12 is connected to the middle plate portion 112 of the middle frame 110. Figures 3 to 6 As shown, the raised structure 12 may, for example, include a partition bar 121 as described above for separating the battery compartment, a mounting boss 122 for installing screws 114 to lock the main circuit board 400, a positioning column 123 for positioning the main circuit board 400, and a supporting platform 124 for supporting the microphone 600a / speaker 600b.

[0091] Specifically, Figures 3 to 6 Taking the middle frame 110 shown in the figure as the structural member 10 as an example, the manufacturing method of the structural member 10 includes the following steps:

[0092] S100, using a first raw material to process and form a structural body having a plate portion.

[0093] Among them, the first raw material processed to form the structural body 11 can be a metal material, for example, the first raw material can be stainless steel, aluminum alloy, magnesium alloy, titanium alloy, etc.; or, the first raw material can also be an inorganic non-metallic material, for example, the first raw material can be ceramic, glass, nano-ceramics, microcrystalline glass, etc.; or, the first raw material can be an organic polymer and its modified material, for example, the first raw material is polycarbonate (Polycarbonate, PC), polybutylene terephthalate (polybutylene terephthalate, PBT), polyamide (Polyamide, PA), polyether ether ketone (Peekmaterials, PEEK), etc., and their blends, polymer alloys, modified materials after adding inorganic fillers (such as glass fibers, nano whiskers, carbon nanotubes, montmorillonite, talc, etc.) and other modified components (including but not limited to antioxidants, antibacterial agents, impact modifiers, etc.); or, the first raw material can be a composite material, for example, the first raw material can be a carbon fiber composite material, a glass fiber composite material, an aramid fiber composite material or a composite material mixed with multiple fiber materials.

[0094] Furthermore, the first raw material may be processed into the structural body 11 by using one molding process or a combination of multiple molding processes. Exemplarily, the molding process for forming the structural body 11 may include at least one of CNC machining, die casting, stamping, 3D printing, hot bending, sintering, injection molding, compression molding, transfer molding, SMC (Sheet Molding Compound), and hand lay-up molding.

[0095] S200, using the second raw material to form a raised structure.

[0096] The second raw material processed to form the protruding structure 12 may be a metal material, for example, the second raw material may be stainless steel, aluminum alloy, magnesium alloy, titanium alloy, etc.; or, the second raw material may be an inorganic non-metallic material, for example, the second raw material may be ceramic, glass, nano-ceramics, microcrystalline glass, etc.; or, the second raw material may be an organic polymer and its modified material, for example, the second raw material is PC, PBT, PA, PEEK, etc., and its blends, polymer alloys, modified materials after adding inorganic fillers (such as glass fibers, nano whiskers, carbon nanotubes, montmorillonite, talc, etc.) and other modified components (including but not limited to antioxidants, antibacterial agents, impact modifiers, etc.); or, the second raw material may be a composite material, for example, the first raw material may be a carbon fiber composite material, a glass fiber composite material, an aramid fiber composite material or a composite material mixed with multiple fiber materials; the second raw material may also be a foaming material and aerogel, etc.

[0097] Similarly, the second raw material may be processed into the protruding structure 12 by a molding process or a combination of multiple molding processes. Exemplarily, the molding process for forming the protruding structure 12 may include at least one of CNC machining, die casting, stamping, 3D printing, hot bending, sintering, injection molding, compression molding, transfer molding, SMC, and hand lay-up molding.

[0098] Among them, for the first raw material constituting the structural body 11 and the second raw material constituting the protruding structure 12, the second raw material can be the same as or different from the first raw material according to the shape and size of the protruding structure 12, the force requirements, the connection method with the structural body 11 and other conditions.

[0099] In some embodiments, the same material can be used to form the structural body 11 and the protruding structure 12, that is, the second raw material and the first raw material are the same material, for example, the first raw material constituting the structural body 11 and the second raw material constituting the protruding structure 12 are both metal materials. In this way, it is convenient to prepare the ingredients, and only one material needs to be prepared to form the entire structure 10. In addition, since the second raw material is the same as the first raw material, there are fewer restrictions on the connection process between the protruding structure 12 and the structural body 11, which can ensure that the protruding structure 12 is firmly connected to the structural body 11.

[0100] In other embodiments, different materials may be used to form the structural body 11 and the protruding structure 12, that is, the second raw material and the first raw material are different materials. For example, the first raw material constituting the structural body 11 may be a metal material, and the second raw material constituting the protruding structure 12 may be a composite material. In this way, the protruding structure 12 may be processed with a suitable material according to the force requirements, functional requirements and other conditions of the protruding structure 12, thereby expanding the selection range of raw materials for making the protruding structure 12 and reducing the production cost of the structural member 10.

[0101] For example, a material with a lower density can be selected to make the protruding structure 12, that is, the density of the second raw material can be lower than that of the first raw material. For example, the first raw material constituting the structural body 11 can be a metal material, and the second raw material constituting the protruding structure 12 can be a carbon fiber composite material or foam material, aerogel, etc. with a lower density. In this way, the weight of the protruding structure 12 can be reduced, and the overall weight of the structural member 10 can be reduced, so as to achieve the purpose of reducing the weight of the entire electronic device and meet the requirements of thinness and lightness of the electronic device.

[0102] S300, connecting the protruding structure to the plate surface of the plate portion to form a structural member.

[0103] For the separately processed protruding structure 12 and the separately processed structural body 11, according to the material, shape, size and functional requirements of the protruding structure 12, a suitable connection process can be selected to connect the protruding structure 12 to the plate surface of the plate portion of the structural body 11. Exemplarily, the connection process for connecting the protruding structure 12 to the plate surface of the plate portion of the structural body 11 includes but is not limited to at least one of welding, bonding, locking, riveting, hot melt connection, mechanical clamping and the like, which can be a single connection process or a combination of two or more connection processes. Among them, for a single protruding structure 12, one process can be used to connect it to the plate portion of the structural body 11; for a plurality of different protruding structures 12, different protruding structures 12 can be connected to the plate surface of the plate portion of the structural body 11 using the same process or different processes.

[0104] When the protruding structure 12 is connected to the structural body 11 by bonding, the protruding structure 12 and the structural body 11 can be bonded together by using a dispensing process such as jet dispensing, contact dispensing, and manual dispensing. Similarly, for a single protruding structure 12, a dispensing process can be used to connect it to the plate portion of the structural body 11; for a plurality of different protruding structures 12, different protruding structures 12 can be connected to the plate portion of the structural body 11 by using the same process or different processes. Exemplarily, when the protruding structure 12 is connected to the structural body 11 by using a jet dispensing process, the glue can be sprayed out at a very fast speed through a nozzle arranged above on the side surface where the protruding structure 12 is connected to the structural body 11 or on the surface area of ​​the structural body 11 corresponding to the protruding structure 12. For example, the nozzle can spray more than 200 precisely measured glue dots per second. As the nozzle moves, the glue dots can form various required line types (such as solid lines, dotted lines, etc.), and the spraying range can be precisely controlled.

[0105] The contact dispensing process is used to connect the protruding structure 12 to the structural body 11. Different from the non-contact dispensing process (jet dispensing process), the contact dispensing process relies on the dispensing needle to contact the surface to be dispensed (for example, the side surface where the protruding structure is connected to the structural body or the surface area of ​​the structural body corresponding to the protruding structure). After a period of time, the glue liquid infiltrates the surface, and then the dispensing needle moves upward. The glue liquid is separated from the dispensing needle by the viscous force between the dispensing needle and the surface, thereby forming a glue spot on the surface.

[0106] For connecting the raised structure 12 to the structural body 11 by manual glue dispensing, glue can be dispensed manually using a manual glue dispensing machine or a manual glue gun on the surface to be glued (for example, the surface on one side where the raised structure is connected to the structural body or the surface area on the structural body corresponding to the raised structure). This process is simple and low-cost.

[0107] When assembling the protruding structure 12 and the structural body 11, according to the size of the structural body 11 and the protruding structure 12, the assembly accuracy requirements, the connection process selection and other conditions, the assembly methods such as automated equipment assembly, fixture assembly, and manual assembly can be selected to connect the protruding structure 12 to the structural body 11. Among them, the automated equipment assembly can determine the relative positions of the structural body 11 and the protruding structure 12 through visual inspection technology, and complete the self-alignment and automatic assembly of the protruding structure 12 and the structural body 11 through the equipment; the fixture assembly can be to clamp and fix the structural body 11 on the fixture, align the protruding structure 12 with the corresponding part of the structural body 11 through mechanical movement or manual methods, and then complete the connection between the protruding structure 12 and the structural body 11; the manual assembly can be to completely manually position and align the protruding structure 12 and the structural body 11, and then connect the protruding structure 12 to the structural body 11.

[0108] Taking the example of connecting the protruding structure 12 to the structural main body 11 through the bonding process, after aligning the protruding structure 12 on the structural main body 11, the glue curing process used can be selected according to the bonding material, and the specific process parameters are subject to the requirements of bonding reliability and product reliability, including but not limited to thermal curing, moisture curing, light curing, two-component mixed curing, solvent volatilization curing, hot melt cooling and other curing methods. Among them, for a single protruding structure 12, a curing process can be used to achieve a fixed connection between the protruding structure 12 and the structural main body 11; for a plurality of different protruding structures 12, according to the selection of the bonding material, different protruding structures 12 can use the same curing process or different curing processes to achieve a fixed connection with the structural main body 11.

[0109] This embodiment reduces the processing difficulty of the structural part 10 by separately processing the structural body 11 and the protruding structure 12 of the structural part 10, and then connecting the protruding structure 12 to the plate surface of the plate portion of the structural body 11 through a connection process. For the method of using CNC processing technology to make the structural body 11 and / or the protruding structure 12, since the shapes of the separate structural body 11 and the separate protruding structure 12 are relatively regular, excessive waste of raw materials is avoided, and the production cost of the structural part 10 is reduced. For the method of using die-casting molding or injection molding technology to make the structural body 11 and / or the protruding structure 12, the design difficulty and processing cost of the mold are reduced. In addition, the protruding structure 12 can be made of a low-density material different from the structural body 11, which can achieve weight reduction of the structural part 10, and then reduce the weight of the entire electronic device 1.

[0110] In addition, for the structural parts 10 of the same series of products, it is conducive to realizing modular design, improving the production efficiency of the electronic device 1, and reducing the production cost of the electronic device 1. For example, for mobile phones of different models in the same series, the structural parts 10 (middle frame 110) of the mobile phone can use the structural body 11 of the same shape and size, and can use the same raw materials and the same molding method to make the structural body 11, which enhances the versatility of the structural body 11 and improves the production efficiency of the structural body 11. As for the raised structure 12 on the structural part 10, it is only necessary to add the corresponding raised structure 12 according to different product designs, and the same raised structure 12 (such as the same partition bar 121) can also be applied to mobile phones of different series and different models.

[0111] Similarly, for products of the same series but different models, if the shape and size of the main body 11 of the structural part 10 are exactly the same, when the main body 11 of the structural part 10 is made by CNC processing technology, the reuse ratio of CNC jigs can be increased. Similarly, when the main body 11 of the structural part 10 is made by die-casting or injection molding technology, the reuse ratio of molds can also be increased, which can reduce the cost of jigs and molds. When the protruding structure 12 and the main body 11 are assembled by fixture assembly, the reuse ratio of the assembly jig of the structural part 10 can also be increased, the degree of freedom of the assembly production line can be increased, and the assembly cost can be reduced.

[0112] The following takes the structural member 10 as the middle frame 110 of the mobile phone as an example to exemplify the manufacturing process of the structural member 10 of this embodiment. The middle frame 110 is defined as including a middle frame body 110a and a protruding structure 12. The middle frame body 110a may include, for example, a frame portion 111 and a main structure of a middle plate portion 112 connected to the inner side of the frame portion 111. The protruding structure 12 may, for example, be connected to the plate surface of the middle plate portion 112.

[0113] Example 1

[0114] Fig.10 A manufacturing process flow chart of the middle frame provided in the embodiment of the present application. Fig.10 As shown, as an example, taking the raised structure 12 on the middle frame body 110a as a partition strip 121, an aluminum alloy profile can be used as the first raw material a to be processed into the middle frame body 110a, and a carbon fiber composite material (plate) can be used as the second raw material b to be processed into the partition strip 121, and then the partition strip 121 is connected to the middle frame body 110a through a bonding process.

[0115] Specifically, first, the middle frame body 110a is processed using aluminum alloy profiles, for example Fig.10As shown in , the aluminum alloy profile can be processed into the middle frame body 110a by CNC processing technology. After the aluminum alloy profile is processed by CNC, the basic structure of the middle frame body 110a is formed. After that, it is processed by nano injection molding, anodizing and other processes to form the middle frame body 110a that meets the requirements. Exemplarily, the purpose of nano injection molding can be to form a specific plastic structure on the middle frame body 110a to meet the signal radiation requirements of the mobile phone antenna; anodizing can be to process the surface of the middle frame body 110a (such as the outer wall surface of the frame part 111) to meet the appearance requirements of the mobile phone.

[0116] Among them, the model of aluminum alloy is based on meeting the requirements of product design and reliability, and the specific process parameters of CNC processing, nano injection molding and anodizing are based on meeting the requirements of product design and appearance. This example does not make specific restrictions.

[0117] The partition strip 121 is processed using carbon fiber composite materials, for example Fig.10 As shown in , a carbon fiber composite material (plate) of a specific thickness is processed by CNC processing technology to form a partition bar 121 of a specific size. Among them, the thickness, performance, carbon fiber grade and other parameters of the carbon fiber composite material (plate), the size of the partition bar 121 finally formed, etc., are based on meeting the product design requirements and reliability, and this example does not make specific restrictions. Exemplarily, the size of the partition bar 121 can be: 65mm long, 3mm high, and 0.6mm thick (wide).

[0118] After the middle frame body 110a and the partition strip 121 are manufactured respectively, the partition strip 121 is bonded to the middle frame body 110a through a bonding process. After the glue between the partition strip 121 and the middle frame body 110a is completely cured, the partition strip 121 made of carbon fiber composite material and the middle frame body 110a made of aluminum alloy profile are connected as a whole to form a complete middle frame 110.

[0119] Among them, the adhesive material c used to connect the partition strip 121 and the middle frame body 110a is based on meeting the requirements of bonding reliability and product reliability. The main resin of the glue includes but is not limited to polyurethane, acrylate, modified acrylic acid, silicone, modified silane, epoxy resin, modified epoxy resin, polyimide, phenolic resin, etc., and this embodiment does not make specific restrictions on this. Exemplarily, according to factors such as the cost, curing conditions, process difficulty and curing speed of the adhesive material c, a two-component acrylic structural adhesive can be selected as the adhesive material c, and the mixing ratio can be, for example, 10:1.

[0120] When the partition bar 121 is bonded to the middle frame body 110a by the bonding material c, the above-mentioned dispensing process such as jet dispensing, contact dispensing or manual dispensing can be used to connect the partition bar 121 and the middle frame body 110a. For example, according to factors such as dispensing accuracy and process control, a contact dispensing process can be selected, and a dispensing valve for contact dispensing can be a screw valve, for example; or, other dispensing processes such as jet dispensing or manual dispensing can also be selected, and this example does not make specific restrictions.

[0121] As for the assembly method between the partition bar 121 and the middle frame body 110a, the above-mentioned automated equipment assembly, fixture assembly, manual assembly and other assembly methods can be adopted. For example, according to factors such as assembly accuracy, assembly efficiency and assembly cost, the fixture assembly method can be selected. Alternatively, other assembly methods such as automated equipment assembly and manual assembly can also be selected, and this example does not make specific restrictions.

[0122] After the partition strip 121 is aligned on the middle frame body 110a, the glue curing process is selected according to the adhesive material c, and the above-mentioned curing methods such as heat curing, moisture curing, light curing, two-component mixed curing, solvent volatilization curing, hot melt cooling, etc. can be used. Exemplarily, for the method of selecting a two-component acrylic structural adhesive as the adhesive material c, no special curing conditions are required between the partition strip 121 and the middle frame body 110a, the ambient temperature can be controlled at 25±2°C, the ambient humidity can be controlled at 50±10%RH (Relative Humidity), and the pressure holding and standing time after dispensing can be, for example, 15 minutes.

[0123] Example 2

[0124] Fig.11 Another process flow chart of manufacturing the middle frame provided in the embodiment of the present application. Fig.11 As shown, as an example, continuing to take the raised structure 12 on the middle frame body 110a as the partition strip 121, an aluminum alloy profile can be used as the first raw material a, processed into the middle frame body 110a, and a carbon fiber reinforced PEEK material can be used as the second raw material b, processed into the partition strip 121, and then the partition strip 121 is connected to the middle frame body 110a by a locking method.

[0125] Different from Example 1, in this example, a positioning groove 1121 is provided on the middle plate portion 112 of the middle frame body 110a, and the partition bar 121 is installed in the positioning groove 1121, and the partition bar 121 is positioned by the positioning groove 1121. The partition bar 121 may include a connecting portion 1211 and a partition portion 1212, the connecting portion 1211 is embedded in the positioning groove 1121, the partition portion 1212 is located on the side surface of the connecting portion 1211 away from the bottom of the positioning groove 1121, the partition portion 1212 may, for example, extend vertically from the connecting portion 1211, the thickness of the connecting portion 1211 may match the depth of the positioning groove 1121, the surface of the connecting portion 1211 is flush with the board surface of the middle plate portion 112, the partition portion 1212 extends on the board surface of the middle plate portion 112, and the battery compartment is separated by the partition portion 1212. Among them, the partition bar 121 can, for example, be a "T"-shaped structure, and the partition portion 1212 can be located in the middle part of the connecting portion 1211. In this way, it is convenient to set screw holes in the areas of the connecting portion 1211 exposed on both sides of the partition portion 1212, so that the partition bar 121 can be locked on the middle frame body 110a by screwing the screws 114 into the screw holes.

[0126] Similar to Example 1, the aluminum alloy profile can be processed into the middle frame body 110a by CNC processing technology, or the aluminum alloy profile can be processed into the middle frame body 110a by die casting technology, and the positioning groove 1121 is processed at a specific position of the middle frame body 110a to facilitate the subsequent positioning and assembly of the partition strip 121. The aluminum alloy profile is processed by CNC processing technology or die casting technology to form the basic structure of the middle frame body 110a, and then it is processed by nano injection molding, surface spraying and other processes to form a middle frame body 110a that meets the requirements. Among them, similar to the purpose of anodizing described in Example 1, the main purpose of surface spraying of the middle frame body 110a is to meet the appearance requirements of the mobile phone.

[0127] Among them, the model of aluminum alloy is based on meeting the requirements of product design and reliability, the specific process parameters of CNC processing or die-casting, nano injection molding and surface spraying, the position, size, processing accuracy and other parameters of the positioning groove 1121 reserved on the middle frame body 110a are based on meeting the requirements of product design and appearance, and this example does not make specific restrictions.

[0128] Reference Fig.11As shown, the particles of carbon fiber reinforced PEEK material are formed into the above-mentioned "T"-shaped partition strip 121 after injection molding or CNC processing, so as to facilitate assembly with the positioning groove 1121 reserved on the middle frame body 110a. Among them, the brand of PEEK raw material, the brand of carbon fiber, the carbon fiber content, other auxiliary ingredients, etc. in the carbon fiber reinforced PEEK material, the specific process parameters of injection molding and CNC processing, and the size of the final partition strip 121 are based on meeting the product design and reliability requirements, and this example does not make specific restrictions. For example, PEEK+30% carbon fiber can be selected as the second raw material b for making the partition strip 121.

[0129] After the middle frame body 110a and the partition bar 121 are respectively manufactured, the partition bar 121 is connected to the middle frame body 110a by screws 114 by locking, so as to form a complete middle frame 110. As for the assembly method between the partition bar 121 and the middle frame body 110a, the above-mentioned automated equipment assembly, fixture assembly, manual assembly and other assembly methods can be adopted. For example, according to factors such as assembly method, assembly accuracy, assembly efficiency and assembly cost, a manual assembly method can be selected. Alternatively, other assembly methods such as automatic equipment assembly and fixture assembly can also be selected, and this example does not make specific restrictions.

[0130] Among them, the specific process parameters for locking the screw 114 and the size, type, thread shape, torque, whether there is a fastener and other parameters of the screw 114 are based on meeting the product design, assembly accuracy and reliability requirements, and this example does not make specific restrictions.

[0131] Example 3

[0132] Fig.12 This is a flowchart of the third manufacturing process of the middle frame provided in the embodiment of the present application. Fig.12 As shown, as an example, taking the raised structure 12 on the middle frame body 110a as a supporting platform 124 for supporting and fixing the microphone 600a or the speaker 600b, an aluminum alloy profile can be used as the first raw material a to be processed into the middle frame body 110a, and graphene aerogel can be used as the second raw material b to be processed into the supporting platform 124, and then the supporting platform 124 is connected to the middle frame body 110a through a bonding process.

[0133] Similar to Example 1, the aluminum alloy profile can be processed into the middle frame body 110a by CNC processing technology, and the aluminum alloy profile is processed by CNC processing, nano injection molding, anodizing and other processes to form a middle frame body 110a that meets the requirements. Among them, the model of the aluminum alloy is based on meeting the product design and reliability requirements, and the specific process parameters of CNC processing, nano injection molding and anodizing are based on meeting the product design and appearance requirements, and this example does not make specific restrictions.

[0134] The graphene aerogel of a specific size is subjected to die cutting, mechanical processing and other processes to form a specifically designed carrier 124. Among them, the performance, density, internal graphene size, etc. of the graphene aerogel, the specific process parameters of die cutting and mechanical processing, the design and size of the carrier 124 finally formed, etc., are based on meeting the product design requirements and reliability, and this example does not make specific restrictions. Exemplarily, the size of the carrier 124 can be: 4mm long, 3mm wide, and 1.6mm high.

[0135] In addition, in addition to graphene aerogel, other aerogels and foaming materials, such as polyurethane foaming materials, silicon aerogel, etc., can also be used to make the supporting platform 124, and this example does not make specific limitations.

[0136] After the middle frame body 110a and the supporting platform 124 are respectively manufactured, the supporting platform 124 is bonded to the middle frame body 110a through a bonding process. After the glue between the supporting platform 124 and the middle frame body 110a is completely cured, the supporting platform 124 made of graphene aerogel and the middle frame body 110a made of aluminum alloy profile are connected as a whole to form a complete middle frame 110.

[0137] The adhesive material c used to connect the carrier 124 and the middle frame body 110a is based on the requirements of bonding reliability and product reliability. The main resin of the glue can be the materials listed in Example 1, which will not be repeated here. For example, according to factors such as the cost, reliability and dispensing process of the adhesive material c, a single-component epoxy thermosetting adhesive can be selected as the adhesive material c.

[0138] The above-mentioned dispensing process such as jet dispensing, contact dispensing or manual dispensing can be used to connect the carrier 124 and the middle frame body 110a. For example, considering the factors of accurately controlling the amount of glue and avoiding the impact of overflow on assembly, the jet dispensing process can be selected, or other dispensing processes such as contact dispensing or manual dispensing can be selected, and this example does not make specific restrictions.

[0139] As for the assembly method between the carrier 124 and the middle frame body 110a, the above-mentioned automated equipment assembly, fixture assembly, manual assembly, etc. can be adopted to meet the product assembly accuracy and reliability requirements. For example, considering that the sound transmission channel 1241 of the carrier 124 needs to accurately correspond to the sound inlet hole 111a / sound outlet hole 111b on the middle frame body 110a, the automated equipment assembly method can be selected.

[0140] After the carrier 124 is aligned on the middle frame body 110a, a glue curing process is selected according to the adhesive material c, and the curing process listed in Example 1 can be used for glue curing, which will not be repeated here. For example, since this example selects a single-component epoxy thermosetting adhesive as the adhesive material c, the curing process can be selected as thermal curing, and the curing equipment can be selected as a vertical curing furnace, the curing temperature is, for example, 80°C, and the curing time is, for example, 60 minutes.

[0141] In the description of the embodiments of the present application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, or it can be an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the embodiments of the present application can be understood according to specific circumstances.

[0142] The terms "first", "second", "third", "fourth", etc. (if any) in the description and claims of the embodiments of the present application and the above-mentioned drawings are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence.

Claims

1. A method for manufacturing a structural member, used to form a structural member with a protruding structure, characterized in that: include: The first raw material is used to process and form a frame portion of the middle frame and a middle plate portion connected to the inner side of the frame portion; Processing a positioning groove on the middle plate portion; The second raw material is used to form a T-shaped partition bar, wherein the partition bar comprises a connecting portion and a partition portion, wherein the partition portion is located on a side surface of the connecting portion away from the bottom of the positioning groove, and the partition portion is located in the middle of the connecting portion; Processing screw holes in the areas of the connecting portion exposed on both sides of the partition portion; The connecting portion is embedded into the positioning groove, and then the partition bar is locked on the middle plate portion by screwing a screw into the screw hole to form a structural member; Wherein, the density of the second raw material is smaller than the density of the first raw material.

2. The method according to claim 1, characterized in that: The second raw material is different from the first raw material.

3. The production method according to any one of claims 1 to 2, characterized in that: The first raw material includes metal materials, inorganic non-metallic materials, organic polymer materials and modified materials and composite materials thereof.

4. The production method according to any one of claims 1 to 2, characterized in that: Processing and forming the frame portion and the middle plate portion includes: The frame portion and the middle plate portion are formed by at least one molding process selected from the group consisting of CNC machining, die casting, stamping, 3D printing, hot bending, sintering, injection molding, compression molding, transfer molding, SMC, and hand lay-up molding.

5. The production method according to any one of claims 1 to 2, characterized in that: The second raw material includes metal materials, inorganic non-metal materials, organic polymer materials and modified materials thereof, composite materials, foaming materials, and aerogels.

6. The method according to any one of claims 1 to 2, characterized in that: Processing to form the partition strip includes: The partition strip is formed by at least one molding process selected from the group consisting of CNC machining, die casting, stamping, 3D printing, hot bending, sintering, injection molding, compression molding, transfer molding, SMC, and hand lay-up molding.

7. The production method according to any one of claims 1 to 2, characterized in that: Connecting the partition strip to the plate surface of the middle plate portion includes: The partition strip is connected to the board surface of the middle board portion by at least one of automated equipment assembly, fixture assembly, and manual assembly.

8. A structural member, characterized in that: The structural member is manufactured by the manufacturing method described in any one of claims 1 to 7.

9. An electronic device, characterized in that: Comprising the structural member described in claim 8.