A method for preparing a shielded gate power device and a shielded gate power device

By setting grooves on the shielded gate structure, the relative area between the gate and the shielded gate is reduced, and the problem of excessive gate source parasitic capacitance in the prior art is solved, the switching speed of the device is improved and the loss is reduced .

CN116864383BActive Publication Date: 2024-11-22SHANGHAI GONGCHENG SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310877606.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-07-17
Publication Date
2024-11-22
Estimated Expiration
2043-07-17

AI Technical Summary

Technical Problem

In the existing shielded gate trench MOSFET devices, the gate source parasitic capacitance Cgs due to the excessive large amount of the gate source parasitic capacitance Cgs caused by the provision of the isolation dielectric layer between the gate and the shielded gate, which affects the switching performance of the device.

Method used

At least one groove is provided on the shielded gate structure to reduce the relative area between the gate and the shielded gate, thereby reducing the inter-plate capacitance Cgs, increasing the switching speed and reducing losses.

Benefits of technology

By reducing the capacitance between the plates, the switching speed of the device is increased and the loss is reduced, and the problem of excessive gate-source parasitic capacitance is solved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116864383B_ABST
    Figure CN116864383B_ABST
Patent Text Reader

Abstract

The present invention provides a shielded gate power device and a preparation method thereof, the preparation method of the shielded gate power device comprising: providing a semiconductor layer; forming a groove in the semiconductor layer; forming a shielded gate in the groove, wherein the upper surface of the shielded gate is lower than the top surface of the groove, and part of the material of the shielded gate close to the gate side is removed to form at least one groove; forming a gate in the groove, the gate being located above the shielded gate. The preparation method of the shielded gate power device of the present invention reduces the relative area between the gate and the shielded gate by providing at least one groove on the shielded gate structure, thereby reducing the inter-plate capacitance Cgs, reducing the input capacitance, accelerating the switching speed, and reducing the loss.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of semiconductor integrated circuit manufacturing, and relates to a method for preparing a shielded gate trench power device and a shielded gate power device. Background Art

[0002] Among power MOSFET devices, shielded gate trench MOSFET has attracted more and more attention due to its advantages such as lower on-resistance and faster switching speed than traditional trench MOSFET. In order to improve the voltage resistance of the device and reduce the internal resistance of the device, shielded gate trench MOSFET with various structures has appeared one after another, such as Figure 1 , which is a schematic cross-sectional structure diagram of a trench structure of a shielded gate trench MOSFET with a top-bottom structure, includes a semiconductor layer 01 , a trench 011 , a field oxide layer 012 , a shielded gate 013 , a gate 014 , and a gate oxide layer 015 .

[0003] In the patent with publication number CN115799307A, the researchers proposed that an air cavity can be prepared between the gate conductive layer and the shielding gate layer as an isolation layer. Since air has a good isolation and withstand voltage effect and a very low dielectric constant, on the basis of ensuring the source-drain withstand voltage of the device, the gate-source withstand voltage of the device can be significantly improved, and the gate-source parasitic capacitance Cgs can be greatly reduced, thereby increasing the switching speed of the device and reducing switching losses.

[0004] However, in some special application scenarios or for cost reduction considerations, this problem cannot be solved by setting an air cavity in the shielded gate trench MOSFET structure. Instead, the entire dielectric layer surrounds the gate shielding layer as a whole, forcing R&D personnel to consider reducing the gate-source parasitic capacitance Cgs from other angles. Summary of the invention

[0005] In view of the above-mentioned deficiencies in the prior art, an object of the present invention is to provide a shielded gate power device and a method for preparing the same, aiming to solve the problem in the prior art that a parasitic capacitance Cgs is generated between the gate and the shielding gate due to the isolation of an isolation dielectric layer between the gate and the shielding gate, thereby greatly affecting the switching performance of the device.

[0006] In a first aspect, the present invention provides a method for preparing a shielded gate power device, comprising:

[0007] providing a semiconductor layer;

[0008] forming a trench in the semiconductor layer;

[0009] forming a shielding gate in the trench, wherein the upper surface of the shielding gate is lower than the top surface of the trench, and a portion of the material of the shielding gate close to one side of the gate is removed to form at least one groove;

[0010] A gate is formed in the trench, and the gate is located above the shielding gate.

[0011] The method for preparing a shielded gate power device of the present invention reduces the relative area between the gate and the shielding gate by setting at least one groove on the shielding gate structure, thereby reducing the inter-plate capacitance Cgs, reducing the input capacitance, increasing the switching speed, and reducing the loss.

[0012] In one embodiment, before forming the shielding gate in the trench, the method further includes:

[0013] Forming a field oxide material layer on the sidewalls and bottom of the trench on the upper surface of the semiconductor layer;

[0014] The shielding gate is formed on a surface of the field oxide material layer away from the semiconductor layer.

[0015] In one embodiment, forming a shielding gate in the trench includes:

[0016] Filling a shielding gate material on the field oxide material layer to form a shielding gate material layer;

[0017] Depositing silicon nitride material on the shielding gate material layer and etching back to form silicon nitride sidewalls;

[0018] The shielding gate material layer is etched, and the area not covered and protected by the silicon nitride sidewalls is removed to form a groove, and the shielding gate material layer is etched into a shielding gate with a groove.

[0019] In one embodiment, after forming the shielding gate in the trench, the method further includes:

[0020] Removing silicon nitride sidewalls;

[0021] Removing a portion of the field oxide material layer away from the bottom of the trench so that the height of the field oxide material layer is lower than the upper surface of the shielding gate;

[0022] A material is deposited on the field oxide material layer and the shielding gate and then etched back to form an inter-gate oxide layer.

[0023] In one embodiment, the inter-gate oxide layer and the field oxide material layer cover the shielding gate.

[0024] In one embodiment, forming a gate in the trench specifically includes:

[0025] Growing a gate oxide layer on an upper sidewall of the trench away from the inter-gate oxide layer and on an upper surface of the semiconductor layer;

[0026] A material is deposited on the inter-gate oxide layer and etched back to form a gate.

[0027] On the other hand, the present invention also provides a shielded gate power device, comprising:

[0028] Semiconductor layer;

[0029] A trench is located in the semiconductor layer;

[0030] A shielding gate is located in the trench, and an upper surface of the shielding gate is lower than a top surface of the trench;

[0031] A gate, located in the trench and above the shielding gate, with a spacing from the shielding gate;

[0032] Wherein, at least one groove is provided on a side of the shielding grid close to the grid.

[0033] The shielded gate power device of the present invention reduces the relative area between the gate and the shielding gate by providing at least one groove on the shielding gate structure, thereby reducing the inter-plate capacitance Cgs, reducing the input capacitance, increasing the switching speed and reducing the loss.

[0034] In one of the embodiments, a groove is provided on one side of the shielding gate close to the gate, and the depth of the groove is 2000 angstroms.

[0035] In one of the embodiments, the groove opening width is greater than 1000 angstroms, and the top single side of the shielding gate is greater than 500 angstroms. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the following is a brief introduction to the drawings required for use in the embodiments or the prior art descriptions. Obviously, the drawings described below are some embodiments of the present invention, not all embodiments. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative labor.

[0037] Figure 1 A schematic diagram of the cross-sectional structure of an existing shielded gate trench MOSFET;

[0038] Figure 2 A flowchart of a method for preparing a shielded gate power device provided in one embodiment of the present invention;

[0039] Figure 3-Figure 9A schematic structural diagram of an intermediate state of a shielded gate power device in a method for preparing a shielded gate power device provided in an embodiment of the present invention;

[0040] Fig.10 A schematic structural diagram of a shielded gate power device provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0041] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present invention are shown in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.

[0042] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used in the specification of the present invention herein are only for the purpose of describing specific embodiments and are not intended to limit the present invention.

[0043] It should be understood that when an element or layer is referred to as being "on, " "adjacent to, " "connected to, " or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. On the contrary, when an element is referred to as being "directly on, " "directly adjacent to, " "directly connected to, " or "directly coupled to" other elements or layers, there may be no intervening elements or layers. It should be understood that, although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, doping types, and / or parts, these elements, components, regions, layers, doping types, and / or parts should not be limited by these terms. These terms are merely used to distinguish one element, component, region, layer, doping type, or part from another element, component, region, layer, doping type, or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer, doping type or portion discussed below may be represented as a second element, component, region, layer or portion; for example, the first doping type may be referred to as the second doping type, and similarly, the second doping type may be referred to as the first doping type; the first doping type and the second doping type are different doping types, for example, the first doping type may be P-type and the second doping type may be N-type, or the first doping type may be N-type and the second doping type may be P-type.

[0044] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," etc., may be used herein to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that, in addition to the orientations shown in the figures, spatially relative terms also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is turned over, the element or feature described as "under other elements" or "under it" or "under it" will be oriented as "on" the other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.

[0045] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that when the terms "consisting of" and / or "comprising" are used in this specification, the presence of the features, integers, steps, operations, elements and / or components may be determined, but the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups is not excluded. At the same time, when used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0046] The technical solution of the present invention is described in detail with specific embodiments below. The following specific embodiments can be combined with each other, and the same or similar concepts or processes may not be described in detail in some embodiments.

[0047] Among power MOSFET devices, shielded gate trench MOSFET has attracted more and more attention due to its advantages such as lower on-resistance and faster switching speed than traditional trench MOSFET. In order to improve the voltage resistance of the device and reduce the internal resistance of the device, shielded gate trench MOSFET with various structures has appeared one after another, such as Figure 1 , which is a schematic cross-sectional structure diagram of a trench structure of a shielded gate trench MOSFET with a top-bottom structure, includes a semiconductor layer 01 , a trench 011 , a field oxide layer 012 , a shielded gate 013 , a gate 014 , and a gate oxide layer 015 .

[0048] In the patent with publication number CN115799307A, the researchers proposed that an air cavity can be prepared between the gate conductive layer and the shielding gate layer as an isolation layer. Since air has a good isolation and withstand voltage effect and a very low dielectric constant, on the basis of ensuring the source-drain withstand voltage of the device, the gate-source withstand voltage of the device can be significantly improved, and the gate-source parasitic capacitance Cgs can be greatly reduced, thereby increasing the switching speed of the device and reducing switching losses.

[0049] However, in some special application scenarios or for cost reduction considerations, an isolation layer is not provided in the shielded gate trench MOSFET structure, but the entire dielectric layer surrounds the gate shielding layer as a whole, thus forcing R&D personnel to consider reducing the gate-source parasitic capacitance Cgs from other angles.

[0050] Based on the problems existing in the prior art, an embodiment of the present invention provides a method for preparing a shielded gate trench power device and a shielded gate trench power device.

[0051] In one embodiment, see Figure 2 The present invention provides a method for preparing a shielded gate power device, comprising:

[0052] S10: providing a semiconductor layer;

[0053] S20: forming a groove in the semiconductor layer;

[0054] S30: forming a shielding gate in the trench, wherein a portion of the material of the shielding gate close to one side of the gate is removed to form at least one groove, wherein the upper surface of the shielding gate is lower than the top surface of the trench;

[0055] S40: forming a gate in the trench, wherein the gate is located above the shielding gate

[0056] The method for preparing a shielded gate power device of the present invention reduces the relative area between the gate and the shielding gate by setting at least one groove on the shielding gate structure, thereby reducing the inter-plate capacitance Cgs, reducing the input capacitance, increasing the switching speed, and reducing the loss.

[0057] See also Figure 3 In one of the optional embodiments, S10 specifically includes:

[0058] S101: providing a semiconductor layer 20;

[0059] S102: depositing oxide on the semiconductor layer 20 as a mask layer 30 to prepare for the next step of forming trenches.

[0060] See also Figure 4In one of the optional embodiments, S20 specifically includes performing photolithography and etching operations on the semiconductor layer 20 covered by the mask layer 30 to form the groove 21.

[0061] See also Figure 5 In one embodiment, before forming the shielding gate in the trench, S30 further includes:

[0062] A field oxide material layer 40 is formed on the sidewalls and the bottom of the trench 21 on the upper surface of the semiconductor layer 20 ; before this, the mask layer 30 originally formed for forming the trench 21 needs to be removed.

[0063] The shielding gate is formed on a surface of the field oxide material layer 40 away from the semiconductor layer 20 .

[0064] See also Figure 6 In one of the optional embodiments, step S30 specifically includes:

[0065] S301: filling the field oxide material layer 40 with a shielding gate material to form a shielding gate material layer 23;

[0066] S302: See Figure 7 , silicon nitride material is deposited on the shielding gate material 23 and etched back to form silicon nitride sidewalls 24. It should be noted that the sidewalls 24 here can also be made of other nitride materials, silicon nitride is just one of them, and is not a limitation.

[0067] S303: Continue reading Figure 7 , the shielding gate material layer 23 is etched, and the area not covered and protected by the silicon nitride sidewall 24 is removed to form a groove 25 , and the shielding gate material layer 23 is etched into a shielding gate with a groove 25 .

[0068] As an example, the number of the grooves 25 may be one, two or other numbers. When a plurality of grooves 25 are provided, the grooves 25 may be arranged evenly or unevenly as required.

[0069] As an example, the semiconductor layer 20 may be at least one doped layer, for example, at least one epitaxial doped layer; in this case, the semiconductor layer 20 may be formed on a substrate (not shown). Of course, in other examples, the semiconductor layer 20 may also be a doped substrate. It should be noted that the doping concentration range in the semiconductor layer 20 may be set according to actual conditions and is not limited here.

[0070] As an example, the material of the semiconductor layer 20 may include but is not limited to silicon, silicon germanium, silicon carbide, gallium nitride or other suitable semiconductor materials.

[0071] Reference Figure 8 In one of the optional embodiments, after forming the shielding gate in the trench, step 30 further includes:

[0072] S31: removing the silicon nitride sidewall 24;

[0073] S32: removing a portion of the field oxide material layer 40 away from the bottom of the trench 21 so that the height of the field oxide material layer 40 is lower than the upper surface of the shielding gate. Optionally, the process of removing the field oxide layer may be a wet etching process.

[0074] S33: Reference Fig. 9 , depositing material on the field oxide material layer 40 and the shielding gate and etching back to form an inter-gate oxide layer 26 .

[0075] Continue reading Fig. 9 In one embodiment, the inter-gate oxide layer 26 and the field oxide material layer 40 cover the shielding gate.

[0076] Reference Fig.10 In one of the optional embodiments, step 40 of forming a gate in the trench specifically includes:

[0077] S401: growing a gate oxide layer 27 on the upper sidewall of the trench 21 away from the inter-gate oxide layer 26 and on the surface of the semiconductor layer 20;

[0078] S402 : depositing materials on the inter-gate oxide layer 26 and etching back to form a gate 28 .

[0079] Subsequent processes also include P body implant, N plus implant, ILD deposition, CT lithography, aluminum layer deposition, aluminum layer lithography, passivation layer deposition, and passivation layer lithography, which are similar to conventional processes and will not be elaborated on.

[0080] In another embodiment, please refer to Fig.10 The present invention provides a shielded gate power device, which includes: a semiconductor layer 20; a groove 21, located in the semiconductor layer 20; a shielding gate (not marked in the figure, equivalent to the groove 25 of the shielding gate material layer), located in the groove 21, and the upper surface of the shielding gate 23 is lower than the top surface of the groove 21; a gate 28, located in the groove 21 and above the shielding gate, and having a spacing from the shielding gate 23; at least one groove 25 is provided on the shielding gate close to the gate side.

[0081] The shielded gate power device of the present invention reduces the relative area between the gate and the shielding gate by providing at least one groove on the shielding gate structure, thereby reducing the inter-plate capacitance Cgs, reducing the input capacitance, increasing the switching speed and reducing the loss.

[0082] As an example, the semiconductor layer 20 may be at least one doped layer, for example, at least one epitaxial doped layer; in this case, the semiconductor layer 20 may be formed on a substrate (not shown). Of course, in other examples, the semiconductor layer 20 may also be a doped substrate. It should be noted that the doping concentration range in the semiconductor layer 20 may be set according to actual conditions and is not limited here.

[0083] As an example, the material of the semiconductor layer 20 may include but is not limited to silicon, silicon germanium, silicon carbide, gallium nitride or other suitable semiconductor materials.

[0084] As an example, the depth of the trench 21 is smaller than the thickness of the semiconductor layer 20 .

[0085] In an optional embodiment, a groove 25 is provided on one side of the shielding gate close to the gate, and the shielding gate loses part of its area after the groove is formed on the side close to the gate;

[0086] In one of the optional embodiments, a groove 25 is provided on one side of the shielding gate 23 close to the gate 28 , and the depth of the groove 25 is 2000 angstroms.

[0087] In one of the optional embodiments, the opening width of the groove 25 is greater than 1000 angstroms, and the top single side of the shielding gate 23 is greater than 500 angstroms.

[0088] From the capacitance formula between the two plates, C=εrS / 4πkd, it can be seen that the capacitance between the plates is proportional to the relative area between the two plates and inversely proportional to the distance between the two plates. Setting a shielded gate with a groove can be regarded as reducing the relative area between the two plates, thereby reducing the capacitance between the plates. The device input capacitance includes Cgs and Cgd. The size of the input capacitance affects the charging and discharging time of the gate capacitance, that is, it affects the gate switching speed. The smaller Cgs is, the smaller the input capacitance is, the faster the switching speed is, and the loss is reduced.

[0089] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for preparing a shielded gate power device, characterized in that: include: providing a semiconductor layer; forming a trench in the semiconductor layer; Forming a field oxide material layer on the sidewalls and bottom of the trench on the upper surface of the semiconductor layer; A shielding gate is formed on a surface of the field oxide material layer away from the semiconductor layer; Filling a shielding gate material on the field oxide material layer to form a shielding gate material layer; Depositing silicon nitride material on the shielding gate material layer and etching back to form silicon nitride sidewalls; The shielding gate material layer is etched, and the area not covered and protected by the silicon nitride sidewall is removed to form a groove, and the shielding gate material layer is etched into a shielding gate with a groove; wherein the upper surface of the shielding gate is lower than the top surface of the trench, and a portion of the material of the shielding gate close to one side of the gate is removed to form at least one groove; A gate is formed in the trench, and the gate is located above the shielding gate.

2. The method for preparing a shielded gate power device according to claim 1, characterized in that: After forming the shielding gate in the trench, the method further includes: Removing silicon nitride sidewalls; Removing a portion of the field oxide material layer away from the bottom of the trench so that the height of the field oxide material layer is lower than the upper surface of the shielding gate; A material is deposited on the field oxide material layer and the shielding gate and then etched back to form an inter-gate oxide layer.

3. The method for preparing a shielded gate power device according to claim 2, characterized in that: The inter-gate oxide layer and the field oxide material layer cover the shielding gate.

4. The method for preparing a shielded gate power device according to claim 3, characterized in that: Forming a gate in the trench specifically includes: Growing a gate oxide layer on an upper sidewall of the trench away from the inter-gate oxide layer and an upper surface of the semiconductor layer; A material is deposited on the inter-gate oxide layer and etched back to form a gate.

5. A shielded gate power device, which is prepared by the method for preparing a shielded gate power device according to any one of claims 1 to 4, characterized in that: include: Semiconductor layer; A trench is located in the semiconductor layer; A shielding gate is located in the trench, and an upper surface of the shielding gate is lower than a top surface of the trench; A gate, located in the trench and above the shielding gate, with a spacing from the shielding gate; Wherein, at least one groove is provided on one side of the shielding grid close to the grid; The top of the shielding gate has a single side greater than 500 angstroms.

6. The shielded gate power device according to claim 5, characterized in that: At least one groove is provided on the shielding gate near one side of the gate, and the depth of the groove is 2000 angstroms.