A SiC device with integrated SBD and preparation method thereof
By integrating a Schottky diode and a P-type floating island layer into SiC devices, the problem of excessive turn-on voltage of the SiC MOSFET body diode is solved, reverse freewheeling protection and switching losses are reduced, and the safety and stability of the device are improved.
Patent Information
- Application Number
- CN202311506113.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-13
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2043-11-13
AI Technical Summary
If the body diode of a SiC MOSFET has an excessively high turn-on voltage, it will be difficult to provide freewheeling protection under reverse bias, which will cause the SiC device to be easily damaged under reverse current.
Integrating a Schottky diode into a SiC device provides a reverse freewheeling path, protecting the SiC device from damage by excessive reverse current. It also protects the gate oxide layer and reduces switching losses through a P-type floating island layer.
It improves the safety and stability of SiC devices, enhances reverse freewheeling performance, and reduces switching losses.
Smart Images

Figure CN117238914B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a SiC device integrated with an SBD and a preparation method thereof. Background Art
[0002] The third generation semiconductor material silicon carbide has the characteristics of wide band gap, high breakdown field strength, high thermal conductivity, high saturated electron migration rate, stable physical and chemical properties, etc., and can be used in high temperature, high frequency, high power and extreme environment. Silicon carbide has a larger band gap and higher critical breakdown field strength. Compared with silicon power devices under the same conditions, the voltage resistance of silicon carbide devices is about 10 times that of silicon materials. In addition, silicon carbide devices have a high electron saturation rate, low forward on-resistance, and low power loss, which are suitable for high current and high power applications, reducing the requirements for heat dissipation equipment. SiC has unique physical, chemical and electrical properties and is a semiconductor material with great development potential in extreme application fields such as high temperature, high frequency, high power and radiation resistance. The insulation breakdown field strength of power devices made of silicon carbide is 10 times that of Si, the band gap is 3 times that of Si, and the impedance of the drift layer of SiC devices is lower than that of Si devices. High voltage resistance and low impedance can be achieved with MOSFET without conductivity modulation.
[0003] MOS field effect transistor power devices made of silicon carbide materials can withstand higher voltages and faster switching speeds than Si devices. For conventional Si MOS, its body diode turn-on voltage is only about 0.7V, so it is often used as a freewheeling channel under reverse bias of MOSFET. However, due to the wider bandgap of SiC material, the body diode turn-on voltage of SiC MOSFET is too high (2.7-3.0V), which makes it difficult to play the role of freewheeling protection MOSFET under reverse bias. Summary of the invention
[0004] The purpose of the present invention is to provide a SiC device with integrated SBD and a preparation method. The SiC device integrates a Schottky diode between the source and the drift layer. The turn-on voltage of the Schottky diode is much lower than that of the body diode. When the SiC device is in a reverse state, it can be turned on earlier than the body diode, providing a conduction path for reverse freewheeling, protecting the SiC device from being damaged by excessive reverse current, and adding a P-type floating island layer to protect the gate oxide layer and reduce switching losses, thereby significantly improving the electrical performance of the SiC device.
[0005] A SiC device with integrated SBD, comprising: an integrated SBD;
[0006] The integrated SBD is composed of a Schottky metal and a drift layer;
[0007] The Schottky metal is located between the source electrode and the drift layer and is adjacent to the source electrode and the drift layer;
[0008] The drift layer is located above and adjacent to the substrate.
[0009] Preferably, the drift layer comprises: a first drift layer and a second drift layer;
[0010] The first drift layer is located between and adjacent to the substrate and the second drift layer;
[0011] The second drift layer is located above the first drift layer.
[0012] Preferably, the doping concentration of the first drift layer is less than the doping concentration of the second drift layer.
[0013] Preferably, it also includes: a P-type floating island layer;
[0014] The P-type floating island layer is embedded in the drift layer;
[0015] The P-type floating island layers are stacked.
[0016] Preferably, the width of the P-type floating island layer located below is smaller than the width of the P-type floating island layer located above.
[0017] Preferably, the doping concentration of the first drift layer is 10 16 cm -3 .
[0018] Preferably, the doping concentration of the second drift layer is 10 17 cm -3 .
[0019] Preferably, the doping concentration of the P-type floating island layer is 10 18 cm -3 .
[0020] Preferably, the width of the P-type floating island layer is to .
[0021] A method for preparing a SiC device integrated with an SBD, comprising:
[0022] epitaxially growing a drift layer with a low doping concentration on the substrate;
[0023] Epitaxially growing a drift layer with a high doping concentration on the drift layer with a low doping concentration and ion implanting to form a P-type floating island layer, a P-body layer, a P+ region and an N+ region;
[0024] Etching the P+ region to form a groove;
[0025] Depositing a gate and etching the gate to form a trench;
[0026] The source and drain electrodes are deposited after the Schottky metal is deposited in the trench.
[0027] The present invention arranges a Schottky diode under the source for reverse freewheeling. When the SiC device works normally, the Schottky diode is in a high-resistance state and does not conduct. When the SiC device is connected to a reverse voltage, the Schottky diode turns on to provide a freewheeling channel, so that the current can flow from the source to the Schottky metal, then from the Schottky metal to the drift layer, from the drift layer to the substrate and finally to the drain. Due to the bandwidth gap of the silicon carbide material, the body diode turn-on voltage is very high, and it is difficult to protect the SiC device during reverse freewheeling. Therefore, the present invention adopts a Schottky diode to protect the SiC device. The turn-on voltage of the Schottky diode is much lower than that of the body diode, and a sufficient current path can be provided when the SiC device is reversed, thereby improving the safety and stability of the SiC device. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.
[0029] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0030] Figure 1 Schematic diagram of the structure of the SiC device of the present invention;
[0031] Figure 2 This is a schematic diagram of the SiC device preparation process of the present invention;
[0032] Figure 3 It is a schematic diagram of the structure of the SiC device preparation process of the present invention.
[0033] Description of reference numerals:
[0034] DETAILED DESCRIPTION
[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0036] It should be noted that all directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of the present invention are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0037] In addition, the descriptions of "first", "second", etc. in the present invention are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0038] MOS field effect transistor power devices made of silicon carbide materials can withstand higher voltages and faster switching speeds than Si devices. For conventional Si MOS, its body diode turn-on voltage is only about 0.7V, so it is often used as a freewheeling channel under reverse bias of MOSFET. However, due to the wider bandgap of SiC material, the body diode turn-on voltage of SiC MOSFET is too high (2.7-3.0V), which makes it difficult to play the role of freewheeling protection MOSFET under reverse bias.
[0039] The present invention arranges a Schottky diode under the source for reverse freewheeling. When the SiC device works normally, the Schottky diode is in a high-resistance state and does not conduct. When the SiC device is connected to a reverse voltage, the Schottky diode turns on to provide a freewheeling channel, so that the current can flow from the source to the Schottky metal, then from the Schottky metal to the drift layer, from the drift layer to the substrate and finally to the drain. Due to the bandwidth gap of the silicon carbide material, the body diode turn-on voltage is very high, and it is difficult to protect the SiC device during reverse freewheeling. Therefore, the present invention adopts a Schottky diode to protect the SiC device. The turn-on voltage of the Schottky diode is much lower than that of the body diode, and a sufficient current path can be provided when the SiC device is reversed, thereby improving the safety and stability of the SiC device.
[0040] Example 1
[0041] A SiC device with integrated SBD, reference Figure 1 , including: integrated SBD;
[0042] The integrated SBD consists of Schottky metal 4 and drift layer;
[0043] The contact surface between metal and semiconductor is divided into two types: Schottky contact and Ohm contact. Ohm contact is when the semiconductor doping concentration is very high, when the semiconductor with high doping concentration contacts with metal, a low barrier layer is formed, and electrons can pass through the barrier by tunneling effect, thus forming a low resistance Ohm contact. The characteristics of Ohm contact are that the current-voltage characteristic of the contact surface is linear, and the contact resistance is negligible relative to the bulk resistance of the semiconductor. When current passes through, the voltage drop generated is smaller than the voltage drop on the device. Schottky diode is a metal-semiconductor device made by using a noble metal (gold, silver, aluminum, platinum, etc.) as the positive electrode and an N-type semiconductor as the negative electrode, and utilizing the rectification characteristics of the barrier formed on the contact surface between the two. Because there are a large number of electrons in the N-type semiconductor and only a very small number of free electrons in the noble metal, the electrons diffuse from the semiconductor with high concentration to the metal with low concentration. Obviously, there are no holes in the metal, and there is no diffusion movement of holes from the metal to the semiconductor. By adjusting the structural parameters, a Schottky barrier is formed between the N-type substrate and the anode metal. When a forward bias is applied to both ends of the Schottky barrier (the anode metal is connected to the positive pole of the power supply, and the N-type substrate is connected to the negative pole of the power supply), the Schottky barrier layer becomes narrower and its internal resistance becomes smaller; conversely, if a reverse bias is applied to both ends of the Schottky barrier, the Schottky barrier layer becomes wider and its internal resistance becomes larger.
[0044] The present invention uses Schottky metal 4 and N-type SiC epitaxial layer to form a heterojunction, which is turned on when the SiC device is in a reverse state and is in a high resistance state when the SiC device is working normally. When the SiC device is reversely conducted, the current flows from the source 10 to the Schottky metal 4, then from the Schottky metal 4 to the drift layer, from the drift layer to the substrate 12, and finally from the substrate 12 to the drain 11. The turn-on voltage of the Schottky diode is much lower than the turn-on voltage of the SiC device body diode, which can effectively improve the reverse performance of the SiC device.
[0045] The Schottky metal 4 is located between the source 10 and the drift layer and is adjacent to the source 10 and the drift layer;
[0046] The Schottky diode composed of the Schottky metal 4 and the N-type SiC epitaxial layer is used to provide a reverse freewheeling channel. As a preferred embodiment, the Schottky metal 4 of the present invention is arranged between the source 10 and the drift layer and is adjacent to the source 10 and the drift layer. When the source 10 is connected to a high potential (positive electricity) and the drain 11 is connected to a low potential (negative electricity), the current can flow from the source 10 through the Schottky diode and then flow to the drain 11.
[0047] The drift layer is located above and adjacent to the substrate 12 .
[0048] The electric field distribution of the drift layer plays a key role in the conduction characteristics and current control of the MOSFET. When the gate voltage is applied to the MOSFET, the electric field distribution in the drift region is modulated by the gate voltage, thereby controlling the current flow between the source 10 and the drain 11. When the MOSFET is working, the current between the source 10 and the drain 11 is mainly transmitted through the drift layer. The doping type and concentration of the drift layer determine the conduction type (N-type or P-type) and size of the current. The structure and characteristics of the drift layer directly affect the current control capability of the MOS tube. By adjusting the shape, size and doping concentration of the drift layer, precise control of the current can be achieved to meet the requirements of different applications.
[0049] Preferably, the drift layer comprises: a first drift layer 1 and a second drift layer 3;
[0050] The first drift layer 1 is located between the substrate 12 and the second drift layer 3 and is adjacent to the substrate 12 and the second drift layer 3;
[0051] The second drift layer 3 is located above the first drift layer 1 .
[0052] Preferably, the doping concentration of the first drift layer 1 is lower than the doping concentration of the second drift layer 3 .
[0053] The present invention provides two drift layers with different doping concentrations, the lower layer is the first drift layer 1, and the upper layer is the second drift layer 3. In order to allow current to flow normally through the SiC device, the doping concentration of the first drift layer 1 is set to be lower than the doping concentration of the second drift layer 3. When the SiC device works normally, the current flows from the drain 11 to the first drift layer 1, then from the first drift layer 1 to the second drift layer 3 and finally to the source 10. If the doping concentration of the first drift layer 1 is greater than the doping concentration of the second drift layer 3, it will be difficult for the current to flow from the first drift layer 1 to the second drift layer 3, resulting in a decrease in the electrical performance of the SiC device and affecting the normal operation of the SiC device.
[0054] Compared with the conventional drift layer with uniform doping concentration, the present invention increases the doping concentration of the second drift layer 3 in order to reduce the on-resistance and increase the current path. In the present invention, the area ratio of the first drift layer 1 to the second drift layer 3 is 1:1 to 1.5:1. If the area ratio of the first drift layer 1 to the second drift layer 3 is too different, the forward voltage withstand capability of the SiC device will be insufficient. If the proportion of the second drift layer 3 is small, the improvement effect on the on-resistance will be weakened. As a preferred embodiment, the present invention sets the area ratio of the first drift layer 1 to the second drift layer 3 to 1:1, which significantly improves the forward performance of the SiC device.
[0055] Preferably, it also includes: a P-type floating island layer 2;
[0056] The P-type floating island layer 2 is embedded in the drift layer;
[0057] A floating island device (floating junction device) refers to a special power device that is embedded in the drift layer, not directly connected to the electrode, and is a region with an opposite doping type to the drift layer. In a floating island device with an N-type drift layer doping type, the floating island structure is composed of a P-type doped semiconductor. SiC devices use a new withstand voltage structure - a floating island structure, in order to improve the restrictive relationship between breakdown voltage and specific on-resistance and overcome the disadvantage of high difficulty in superjunction manufacturing process. By introducing multiple floating island structures of opposite doping types in the silicon-based drift layer, the power device can increase resistivity and reduce power loss without changing the breakdown voltage. The fundamental reason is that the floating island introduces a new electric field peak in the drift layer, which reduces the maximum electric field peak in the drift layer. Therefore, under the same breakdown voltage, the specific on-resistance of the device can also be reduced by increasing the doping concentration of the drift layer. And the breakdown voltage of power SiC devices with floating island structures will increase with the increase of the number of floating islands.
[0058] The P-type floating island layer is stacked in 2 layers.
[0059] The present invention increases the withstand voltage performance and gate oxide reliability of SiC devices and reduces gate-drain capacitance by setting at least one P-type floating island. As a preferred embodiment, the present invention sets four P-type floating islands, which are embedded on both sides of the drift layer, with two P-type floating islands on the left and two P-type floating islands on the right. Multiple P-type layers are stacked on one side, and the interval between the P-type floating islands is determined by the number and thickness of the P-type floating islands. The preparation method of the P-type floating island is as follows: when the drift layer is epitaxially grown to a certain thickness, ion implantation is performed on the upper layer of the drift layer to prepare two A P-type floating island is formed, and then a thin drift layer is grown epitaxially. Then, ion implantation is performed again in the epitaxial drift layer to form a second P-type floating island layer 2. Then, epitaxy is performed again on top of the P-type floating island layer 2 to complete the formation of the drift layer. The higher the doping concentration of the P-type floating island layer 2 and the larger the width, the stronger the protection of the gate oxide layer 8 and the ability to improve the withstand voltage performance. However, when making the P-type floating island layer 2, care must be taken to leave enough current path. Therefore, the doping concentration and width of the P-type floating island layer 2 should be set with an upper limit based on the performance of the SiC device.
[0060] The present invention introduces a plurality of P-type floating island layers 2 with a doping type opposite to that of the drift layer (N-drift layer) into the device drift layer, thereby improving the voltage resistance performance of the SiC device without affecting the current path of the SiC device itself, effectively improving the restrictive relationship between the breakdown voltage and the specific on-resistance of the traditional SiC device, and the P-type floating island layer 2 can also protect the gate oxide layer 8 of the JFET region to prevent the gate oxide layer 8 from breaking down prematurely, and the P-type floating island can reduce the overlapping area of the gate 7 and the drain 11, reduce the gate-drain capacitance, reduce the switching loss, and improve the electrical performance of the SiC device.
[0061] Preferably, the width of the P-type floating island layer 2 located below is smaller than the width of the P-type floating island layer 2 located above.
[0062] The width of the P-type floating island layer 2 is set according to the electric field strength distribution of the SiC device. As a preferred embodiment, the present invention sets the width of the P-type floating island layer 2 located below to be smaller than the width of the P-type floating island layer 2 located above. This can better smooth the electric field lines, reduce the electric field strength in the JFET region, and protect the gate oxide layer 8 from being broken down prematurely.
[0063] Preferably, the doping concentration of the first drift layer 1 is 10 16 cm -3 .
[0064] Preferably, the doping concentration of the second drift layer 3 is 10 17 cm -3 .
[0065] In SiC devices, appropriately increasing the doping concentration of the drift layer can reduce the on-resistance. In order to reduce the on-resistance and enable the SiC device to work normally, the present invention appropriately increases the doping concentration of the second drift layer 3, so that the on-resistance of the SiC device is significantly reduced. As a preferred embodiment, the present invention sets the doping concentration of the first drift layer 1 to 10 16 cm -3 , the doping concentration of the second drift layer 3 is set to 10 17 cm -3 .
[0066] Preferably, the doping concentration of the P-type floating island layer 2 is 10 18 cm -3 .
[0067] Because the P-type floating island needs to balance the charge with the drift layer, the doping concentration of the P-type floating island layer 2 is affected by the doping concentration of the drift layer. When the SiC device is in the reverse state, the P-type floating island layer 2 and the drift layer deplete each other. If the doping concentration of the drift layer is high, the doping concentration of the P-type floating island layer 2 will also increase accordingly. If the concentration of the drift layer is too low, it will not be able to reduce the on-resistance of the SiC device. In addition, the doping concentration of the P-type floating island layer 2 is also affected by the thickness of the gate oxide layer 8. If the gate oxide layer 8 is thin and has a weak withstand voltage, the doping concentration of the P-type floating island layer 2 must be increased. The higher the doping concentration of the P-type floating island layer 2, the stronger the ability to improve the distribution of the electric field lines and the better the protection of the gate oxide layer 8. However, when the doping concentration of the P-type floating island layer 2 is increased, sufficient current paths must be left. Therefore, as a preferred embodiment, the present invention sets the doping concentration of the P-type floating island layer 2 to 10 18 cm -3, which can not only better protect the gate oxide layer 8, but also reduce switching losses, greatly improving the electrical performance of SiC devices.
[0068] Preferably, the width of the P-type floating island layer 2 is 1 / 4 of the width of the SiC device. to .
[0069] The width of the P-type floating island layer 2 will also affect the protection capability of the gate oxide layer 8 and the impact on the current path. The wider the width of the P-type floating island layer 2, the stronger the protection capability of the gate oxide layer 8 becomes, while the current path becomes smaller. If the width of the P-type floating island layer 2 is too narrow, the protection capability of the gate oxide layer 8 is insufficient. Therefore, the present invention sets the minimum width of the P-type floating island layer 2 to be 1 / 4 of the width of the SiC device. If the width of the P-type floating island layer 2 is too wide, the current path of the SiC device will be narrowed. Therefore, the present invention sets the maximum width of the P-type floating island layer 2 to be 1 / 4 of the width of the SiC device. In this range, the P-type floating island layer 2 can better protect the gate oxide layer 8 while leaving enough current path.
[0070] Example 2
[0071] A method for preparing a SiC device with integrated SBD, referring to Figure 2 , 3, including:
[0072] S100, epitaxially growing a drift layer (first drift layer 1) with a low doping concentration on the substrate 12;
[0073] The epitaxial process refers to the process of growing a completely ordered single crystal layer on the substrate 12. Generally speaking, the epitaxial process is to grow a crystal layer with the same lattice orientation as the original substrate on a single crystal substrate. The epitaxial process is widely used in semiconductor manufacturing, such as epitaxial silicon wafers in the integrated circuit industry. Embedded source and drain epitaxial growth of MOS transistors, epitaxial growth on LED substrates, etc. Depending on the phase state of the growth source, the epitaxial growth method is divided into solid phase epitaxy, liquid phase epitaxy, and vapor phase epitaxy. In integrated circuit manufacturing, the commonly used epitaxial methods are solid phase epitaxy and vapor phase epitaxy.
[0074] Solid phase epitaxy refers to the growth of a single crystal layer on a substrate using a solid source. For example, thermal annealing after ion implantation is actually a solid phase epitaxy process. During ion implantation, the silicon atoms of the silicon wafer are bombarded by high-energy implanted ions, leaving their original lattice positions and becoming amorphous, forming a surface amorphous silicon layer. After high-temperature thermal annealing, the amorphous atoms return to their lattice positions and remain consistent with the atomic crystal orientation inside the substrate.
[0075] The growth methods of vapor phase epitaxy include chemical vapor epitaxy (CVE), molecular beam epitaxy (MBD), atomic layer epitaxy (ALE), etc. In the embodiment of the present invention, chemical vapor epitaxy (CVE) is used to form the N-drift layer. The principles of chemical vapor epitaxy and chemical vapor deposition (CVD) are basically the same. Both are processes for depositing thin films by chemically reacting on the surface of the wafer after gas mixing; the difference is that because chemical vapor epitaxy grows a single crystal layer, the requirements for the impurity content in the equipment and the cleanliness of the silicon wafer surface are higher. In integrated circuit manufacturing, CVE can also be used for epitaxial silicon wafer process and MOS transistor embedded source and drain epitaxial process. The epitaxial silicon wafer process is to epitaxially grow a layer of single crystal silicon on the surface of the silicon wafer. Compared with the original silicon substrate, the epitaxial silicon layer has higher purity and fewer lattice defects, thereby improving the yield of semiconductor manufacturing. In addition, the growth thickness and doping concentration of the epitaxial silicon layer grown on the silicon wafer can be flexibly designed, which brings flexibility to the design of the device, such as reducing substrate resistance and enhancing substrate isolation. The embedded source-drain epitaxy process refers to the process of epitaxially growing doped germanium silicon or silicon in the source-drain region of the transistor. The main advantages of introducing the embedded source-drain epitaxy process include: growing a pseudocrystalline layer containing stress due to lattice adaptation, improving channel carrier mobility; in-situ doping of the source and drain can reduce the parasitic resistance of the source-drain junction and reduce the defects of high-energy ion implantation.
[0076] S200, epitaxially growing a drift layer with a high doping concentration on the drift layer with a low doping concentration and ion implanting to form a P-type floating island layer 2, a P-body layer 9, a P+ region 5 and an N+ region 6;
[0077] The present invention forms a P-type floating island layer 2, a P+ region 5 and an N+ region 6 by ion implantation. Ion implantation is to launch an ion beam in a vacuum toward a solid material. After the ion beam hits the solid material, it is resisted by the solid material and its speed is slowly reduced, and finally stays in the solid material. The ions of an element are accelerated into a solid target, thereby changing the physical, chemical or electrical properties of the target. Ion implantation is often used in the manufacture of semiconductor devices, metal surface treatment and materials science research. If the ions stop and remain in the target, the ions will change the elemental composition of the target (if the ions are different from the composition of the target). Ion implantation beamline designs all contain a common set of functional components. The main part of the ion beamline includes a device called an ion source for generating ion species. The source is tightly coupled to a bias electrode to extract ions into the beamline, and most commonly is coupled to a certain way of selecting specific ion species for transmission into the main accelerator part. "Mass" selection accompanies the extracted ion beam passing through a magnetic field region, with its exit path restricted by blocking holes or "slits" that allow only ions with the mass and velocity / charge to continue along the beam line. If the target surface is larger than the ion beam diameter, and the implant dose is evenly distributed over the target surface, some combination of beam scanning and wafer motion can be used. Finally, the surface to be implanted is combined with some method for collecting the accumulated charge of the implanted ions so that the delivered dose can be measured in a continuous manner, and the implant process stopped at the desired dose level.
[0078] Doping semiconductors with boron, phosphorus or arsenic is a common application of ion implantation. When implanted into a semiconductor, each dopant atom can create a charge carrier in the semiconductor after annealing. It can create a hole for a P-type dopant and an electron for an N-type dopant. This changes the conductivity of the semiconductor near the doped area.
[0079] S300, etching the P+ region 5 to form a groove;
[0080] The present invention etches both sides of the P+ region 5 to form polysilicon grooves. Etching is a process of selectively removing unwanted materials from the surface of a silicon wafer by chemical or physical methods. It is a general term for stripping and removing materials by solution, reactive ions or other mechanical methods. Etching technology is mainly divided into dry etching and wet etching. Dry etching mainly uses reactive gases and plasma for etching; wet etching mainly uses chemical reagents to react with the etched material for etching.
[0081] Ion beam etching is a physical dry etching process. Hereby, argon ions are irradiated onto the surface in an ion beam of about 1 to 3 keV. Due to the energy of the ions, they impact the material on the surface. The wafer is fed vertically or tilted into the ion beam and the etching process is absolutely anisotropic. The selectivity is low, since there is no differentiation of the individual layers. The gases and the abraded material are evacuated by the vacuum pump, however, since the reaction products are not gaseous, particles can be deposited on the wafer or on the chamber walls. All materials can be etched with this method and due to the vertical irradiation, the wear on the vertical walls is low.
[0082] Plasma etching is an absolutely chemical etching process with the advantage that the wafer surface is not damaged by accelerated ions. Due to the movable particles of the etching gas, the etching profile is isotropic, so this method is used to remove entire film layers (such as backside cleaning after thermal oxidation). One type of reactor used for plasma etching is a downstream reactor. The plasma is thus ignited at a high frequency of 2.45 GHz by impact ionization, the location of which is separated from the wafer.
[0083] The etching rate depends on the pressure, the power of the HF generator, the process gas, the actual gas flow rate and the wafer temperature. Anisotropy increases with increasing HF power, decreasing pressure and decreasing temperature. The uniformity of the etching process depends on the gas, the distance between the two electrodes and the material of the electrodes. If the distance is too small, the plasma cannot be dispersed inhomogeneously, which leads to inhomogeneities. If the distance of the electrodes is increased, the etching rate decreases because the plasma is distributed in an enlarged volume. For the electrodes, carbon has proven to be the material of choice. Since fluorine and chlorine also attack carbon, the electrodes produce a uniform strained plasma, so the wafer edge is affected in the same way as the wafer center. Selectivity and etching rate depend largely on the process gas. For silicon and silicon compounds, fluorine and chlorine are mainly used.
[0084] S400, depositing a gate 7 and etching the gate 7 to form a groove;
[0085] The steps of depositing the gate 7 are: formation of the gate oxide layer 8 and deposition of polysilicon. The present invention uses wet oxidation or dry oxidation to deposit the oxide layer. According to the different oxidants in the oxidation reaction, the thermal oxidation process can be divided into dry oxidation and wet oxidation. The former uses pure oxygen to produce a silicon dioxide layer, which is slow but the oxide layer is thin and dense. The latter requires the use of oxygen and highly soluble water vapor at the same time. Its characteristics are fast growth rate but relatively thick protective layer and low density. Wet oxidation has two main steps: the mass transfer process of oxygen in the air from the gas phase to the liquid phase; the chemical reaction between dissolved oxygen and the matrix. If the mass transfer process affects the overall reaction rate, it can be eliminated by strengthening the stirring. In an embodiment of the present invention, the rate of forming the source 10 oxide layer by wet oxygen oxidation can be controlled by controlling the temperature, pressure, and concentration of the reaction gas during wet oxygen oxidation, thereby achieving the purpose of controlling the thickness of the source 10 oxide layer.
[0086] Dry oxidation uses high-temperature pure oxygen to react directly with the wafer. Dry oxidation uses only pure oxygen (O2), so the growth rate of the oxide film is slow. It is mainly used to form thin films and can form oxides with good conductivity. The advantage of dry oxidation is that it does not produce by-products (H2) and the uniformity and density of the oxide film are high.
[0087] Polysilicon deposition is to form gate electrodes and local connections on the first layer of polysilicon (Poly1) stacked with silicide, and the second layer of polysilicon (Poly2) forms the contact plug between the source 10 / drain 11 and the unit connection. The silicide is stacked on the third layer of polysilicon (Poly3) to form the unit connection, and the fourth layer of polysilicon (Poly4) and the fifth layer of polysilicon (Poly5) form the two electrodes of the storage capacitor, sandwiched between which is a high-dielectric dielectric. In order to maintain the required capacitance value, the size of the capacitor can be reduced by using a high-dielectric dielectric. Polysilicon deposition is a low-pressure chemical vapor deposition (LPCVD). By directly inputting the doping gas of trihydride arsenic (AH3), trihydride phosphine (PH3) or diborane (B2H6) into the silicon material gas of silane or DCS in the reaction chamber (i.e., the furnace tube), the polysilicon doping process of on-site low-pressure chemical vapor deposition can be carried out. Polysilicon deposition is carried out at a low pressure of 0.2-1.0 Torr and a deposition temperature between 600 and 650°C, using pure silane or silane diluted with nitrogen to a purity of 20% to 30%. The deposition rate of both deposition processes is between 100-200Å / min, which is mainly determined by the temperature during deposition.
[0088] S500 , depositing the Schottky metal 4 in the trench and then depositing the source 10 and the drain 11 .
[0089] Metal electrode deposition processes are divided into chemical vapor deposition (CVD) and physical vapor deposition (PVD). CVD refers to a method of depositing a coating on a wafer surface by chemical means, generally by applying energy to a mixed gas. Assuming that a substance (A) is deposited on the surface of a wafer, two gases (B and C) that can generate substance (A) are first input into the deposition equipment, and then energy is applied to the gases to cause a chemical reaction between gases B and C.
[0090] PVD (physical vapor deposition) coating technology is mainly divided into three categories: vacuum evaporation coating, vacuum sputtering coating and vacuum ion coating. The main methods of physical vapor deposition are: vacuum evaporation, sputtering, arc plasma coating, ion coating and molecular beam epitaxy. The corresponding vacuum coating equipment includes vacuum evaporation coating machine, vacuum sputtering coating machine and vacuum ion coating machine.
[0091] Both chemical vapor deposition (CVD) and physical vapor deposition (PVD) can be used as technical means for depositing metal electrodes. In an embodiment of the present invention, a chemical vapor deposition method is used to deposit metal electrodes. The chemical vapor deposition process is divided into three stages: diffusion of the reaction gas to the substrate surface, adsorption of the reaction gas on the substrate surface, chemical reaction on the substrate surface to form a solid deposit, and separation of the generated gas phase byproducts from the substrate surface. The most common chemical vapor deposition reactions are: thermal decomposition reaction, chemical synthesis reaction, and chemical transport reaction. Usually, TiC or TiN is deposited by introducing TiCl4, H2, CH4 and other gases into a reaction chamber at 850~1100°C, and a coating is formed on the substrate surface through chemical reaction.
[0092] The present invention sets a Schottky diode under the source 10 for reverse freewheeling. When the SiC device works normally, the Schottky diode is in a high-resistance state and does not conduct. When the SiC device is connected to a reverse voltage, the Schottky diode turns on to provide a freewheeling channel, so that the current can flow from the source 10 to the Schottky metal 4, then from the Schottky metal 4 to the drift layer, from the drift layer to the substrate 12, and finally to the drain 11. Due to the bandwidth gap of the silicon carbide material, the body diode turn-on voltage is very high, and it is difficult to protect the SiC device during reverse freewheeling. Therefore, the present invention adopts a Schottky diode to protect the SiC device. The turn-on voltage of the Schottky diode is much lower than that of the body diode, and a sufficient current path can be provided when the SiC device is reversed, thereby improving the safety and stability of the SiC device.
[0093] The foregoing is merely a specific embodiment of the present invention, which enables those skilled in the art to understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features claimed herein.
Claims
1. A SiC device with integrated SBD, characterized in that: include: Integrated SBD; The integrated SBD comprises a Schottky metal, a P-type floating island layer and a drift layer; The drift layer consists of a first drift layer and a second drift layer; The Schottky metal is located between the source electrode and the second drift layer and is adjacent to the source electrode and the second drift layer; The first drift layer is located between and adjacent to the substrate and the second drift layer; The second drift layer is located above the first drift layer; The doping concentration of the first drift layer is less than the doping concentration of the second drift layer; The P-type floating island layer is embedded in the first drift layer and the second drift layer; The P-type floating island layer is embedded in the drift layer; The P-type floating islands are arranged in layers; The width of the P-type floating island layer located below is smaller than the width of the P-type floating island layer located above.
2. A SiC device with integrated SBD according to claim 1, characterized in that: The doping concentration of the first drift layer is 10 16 cm -3 ; The doping concentration of the second drift layer is 10 17 cm -3 ; The doping concentration of the P-type floating island layer is 10 18 cm -3 ; The width of the P-type floating island layer is 1 / 4 of the width of the SiC device. to .
3. A method for preparing a SiC device with integrated SBD, using the SiC device with integrated SBD as claimed in claim 1, characterized in that: include: epitaxially growing a drift layer with a low doping concentration on the substrate; Epitaxially growing a drift layer with a high doping concentration on the drift layer with a low doping concentration and ion implanting to form a P-type floating island layer, a P-body layer, a P+ region and an N+ region; Etching the P+ region to form a groove; Depositing a gate and etching the gate to form a trench; The source and drain electrodes are deposited after the Schottky metal is deposited in the trench.