An antistatic insole and its preparation method

By applying a two-component antistatic adhesive to the insole body and heating and pressurizing it to form an antistatic layer, the problems of complex preparation and high cost in the existing technology are solved, realizing simple and efficient production of antistatic insoles, meeting safety standards and improving comfort.

CN117397903BActive Publication Date: 2026-11-17JIHUA 3515 LEATHER & SHOES
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202311591295.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-27
Publication Date
2026-11-17
Estimated Expiration
2043-11-27

AI Technical Summary

Technical Problem

Existing antistatic shoe soles and insoles have complex manufacturing processes, high costs, and insufficient comfort.

Method used

A two-component antistatic adhesive is used, which is mixed evenly in a reaction vessel and then brushed onto the lower surface of the insole body. The permeation and cross-linking reaction is completed by heating and pressurizing the plate vulcanization to form an antistatic layer. Combined with the fiber fabric insole body, this ensures breathability and antistatic effect.

Benefits of technology

It simplifies the production process, reduces equipment energy consumption and costs, while meeting antistatic requirements, improving comfort, and ensuring that the resistance value meets safety standards.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117397903B_ABST
    Figure CN117397903B_ABST
Patent Text Reader

Abstract

This invention provides a method for preparing antistatic insoles. First, an antistatic adhesive is prepared: a two-component antistatic adhesive is designed, with each component stirred evenly in a reaction vessel and stored separately. When needed, the two-component antistatic adhesive is mixed evenly at a 1:1 mass ratio and uniformly applied to the lower surface of the insole body. The antistatic adhesive and the insole body undergo a cross-linking reaction through flat vulcanization under heat and pressure. The preparation method disclosed in this invention has a simple production process, reduces energy waste from large equipment, saves energy, and the method of mixing the adhesive as needed reduces production costs while ensuring quality. The antistatic insoles prepared by the method disclosed in this invention, after testing, meet the resistance value requirements of GB 21148-2020 for foot protection safety shoes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of shoemaking, specifically relating to an antistatic insole and its preparation method. Background Technology

[0002] As we all know, static electricity from the human body can cause countless problems in daily life. Furthermore, static electricity can pose serious hazards in industrial production, such as fires, especially in production workshops where smoking is strictly prohibited, such as chemical plants. Workers in these workshops need to wear appropriate conductive or anti-static shoes to prevent electrical sparks generated between static electricity from the feet and the insoles or soles of the shoes, which could lead to explosions or other disasters.

[0003] Antistatic insoles are generally achieved by embedding conductive metal wires or other structural elements into the fabric. While insoles with conductive metal wires meet the antistatic requirements, they are expensive. Insoles with structural antistatic elements do not provide the desired comfort level for customers.

[0004] Existing technologies also include shoe soles or insoles that achieve antistatic effects by adding conductive materials such as conductive carbon black and carbon nanotubes. For example, Chinese patents with application numbers 202310230846.3 and 202010012301.1 disclose a carbon nanotube antistatic shoe sole. Using carbon nanotubes as a conductive material can effectively improve the antistatic performance of the shoe sole material. However, in its preparation process, each raw material first needs to be mixed in an open mill, then mixed under pressure in a mixer, then mixed in an open mill again, and finally vulcanized in a vulcanizing machine to obtain the product. The preparation process is complex, requires a lot of equipment, and involves a large investment. Patent application number 202010012301.1 discloses an antistatic dual-density sole material, including a foamed midsole and a rubber outsole. The foamed midsole uses one or more of acetylene black, carbon fiber, and carbon nanotube antistatic agents, and the rubber outsole uses one or more of polyamide copolymer antistatic agents, ionic polymer antistatic agents, and polyoxyethylene ether antistatic agents. The preparation of the sole material also requires internal mixing and open mixing, which is a complex process. Summary of the Invention

[0005] To address the problem that existing antistatic shoe soles and insoles require complex manufacturing processes such as intensive mixing and open mixing, this invention provides an antistatic insole and its preparation method that meet antistatic requirements while having a simple, practical, and low-cost production process.

[0006] The object of this invention is achieved in the following manner: A method for preparing an antistatic insole includes the following steps: a. Preparation of antistatic adhesive: Design a two-component antistatic adhesive, each component is stirred evenly in a reaction vessel and stored separately; b. Mix the two-component antistatic adhesive at a mass ratio of 1:1 evenly, and apply it evenly to the lower surface of the insole body. Complete the penetration and cross-linking reaction between the antistatic adhesive and the insole body through a plate vulcanization heating and pressurization method. The plate vulcanization temperature is 160±5℃, the time is 180±10s, and the pressure is 12±3 Mpa. The two-component antistatic adhesive comprises the following components by weight: 100 parts liquid nitrile rubber, 2.0-2.5 parts vulcanizing agent, 4.8-6.8 parts zinc oxide, 3.8-6.7 parts liquid tackifying resin, and a diluent to achieve a viscosity of 8±4 min / 100 ml at 25°C. The following components by weight fraction are: 100 parts liquid nitrile rubber, 0.68-0.89 parts first accelerator, 0.86-1.12 parts second accelerator, 0.41-0.52 parts third accelerator, 4.8-7.2 parts zinc oxide, 1.5-2.6 parts octadecanoic acid, 0.8-1.0 parts antioxidant 2-thiol-benzoimidazole, 20.4-28.6 parts acetylene black, and 10.6-15.7 parts carbon nanotube dispersion. Diluent is added to achieve a viscosity of 8±4 min / 100ml at 25℃.

[0007] The amount of antistatic adhesive applied to the lower surface of the insole body is 10g-15g.

[0008] The first accelerator is 2,2'-dithiodibenzothiazole, the second accelerator is N-cyclohexyl-2-benzothiazole sulfenamide, and the third accelerator is tetramethylthiuram disulfide.

[0009] An antistatic insole includes an insole body with uniformly distributed ventilation holes. The lower surface of the insole body is coated with the aforementioned antistatic adhesive to form a first antistatic layer. The antistatic adhesive overflows from the ventilation holes to the upper surface of the insole body, forming antistatic columns within the ventilation holes, and a second antistatic layer with dotted distribution is formed on the upper surface of the insole body.

[0010] The insole body is made of fiber fabric.

[0011] Compared to existing technologies, the preparation method disclosed in this invention has a simple production process, reduces energy waste from large-scale equipment, saves energy, and reduces production costs while ensuring quality by using the adhesive as needed. The antistatic insoles prepared by the method disclosed in this invention, after testing, meet the resistance value requirements of GB 21148-2020 for foot protection safety shoes. Attached Figure Description

[0012] Figure 1 This is a schematic diagram of the structure of the antistatic insole of the present invention.

[0013] Figure 2This is a cross-sectional view of the antistatic insole of the present invention. Detailed Implementation

[0014] A method for preparing an antistatic insole includes the following steps: a. Preparation of antistatic adhesive: Design a two-component antistatic adhesive, each component is stirred evenly in a reaction vessel and stored separately; b. Mix the two-component antistatic adhesive at a mass ratio of 1:1 evenly, apply it to the lower surface of the insole body, and complete the penetration and cross-linking reaction between the antistatic adhesive and the insole body through a plate vulcanization heating and pressurization method. The plate vulcanization temperature is 160±5℃, the time is 180±10s, and the pressure is 12±3 Mpa. The two-component antistatic adhesive includes component A: 100g liquid nitrile rubber, 2.0-2.5g vulcanizing agent, 4.8-6.8g zinc oxide, 3.8-6.7g liquid tackifying resin, and diluent added to achieve a viscosity of 8±4 min / 100ml at 25℃. Component B: Liquid nitrile rubber 100, first accelerator 0.68-0.89, second accelerator 0.86-1.12, third accelerator 0.41-0.52, zinc oxide 4.8-7.2, octadecanoic acid 1.5-2.6, antioxidant 2-thiol-benzoimidazole 0.8-1.0, acetylene black 20.4-28.6, carbon nanotube dispersion 10.6-15.7, with diluent added to achieve a viscosity of 8±4 min / 100ml at 25℃.

[0015] The first accelerator is 2,2'-dithiodibenzothiazole, the second accelerator is N-cyclohexyl-2-benzothiazole sulfenamide, and the third accelerator is tetramethylthiuram disulfide.

[0016] like Figure 1 , Figure 2 As shown, an antistatic insole includes an insole body 1 with uniformly distributed ventilation holes 2. The lower surface of the insole body 1 is coated with the aforementioned antistatic adhesive to form a first antistatic layer 3. The antistatic adhesive overflows from the ventilation holes 2 onto the upper surface of the insole body 1, forming antistatic columns 5 within the ventilation holes. A second antistatic layer 4 is formed on the upper surface of the insole body in a dotted pattern. The second antistatic layer 4 radiates from the ventilation holes to the surrounding area, i.e., it is discontinuous on the upper surface of the insole body.

[0017] The material of the insole body 1 is preferably fiber fabric.

[0018] Example 1 a. Prepare a two-component antistatic adhesive according to the following weight fractions, and stir the raw materials of components A and B separately in a reaction vessel until homogeneous, and store them separately; Component A includes: 100 kg of liquid nitrile rubber, 2.1 kg of vulcanizing agent, 5.1 kg of zinc oxide, 4.2 kg of liquid tackifying resin coumarone, and diluents ethyl acetate and xylene to achieve a viscosity of 8 ± 4 min / 100 ml at 25 °C. Component B: 100 kg of liquid nitrile rubber, 0.69 kg of first accelerator 2,2'-dithiodibenzothiazole, 0.89 kg of second accelerator N-cyclohexyl-2-benzothiazole sulfenamide, 0.43 kg of third accelerator tetramethylthiuram disulfide, 5.1 kg of zinc oxide, 1.6 kg of octadecanoic acid, 0.8 kg of antioxidant 2-thiol-benzoimidazole, 21 kg of acetylene black, 11 kg of carbon nanotube dispersion, and diluent added to achieve a viscosity of 8±4 min / 100 ml at 25℃; b. Mix the prepared two-component antistatic adhesive at a mass ratio of 1:1 and apply it evenly to the lower surface of the insole body. The amount of adhesive applied is 10g-15g per insole. The antistatic adhesive and the insole body are penetrated and cross-linked by a plate vulcanization heating and pressurization method. The plate vulcanization temperature is 160±5℃, the time is 180±10s, and the pressure is 12±3 MPa to obtain the finished antistatic insole.

[0019] Because the insole body has evenly distributed ventilation holes 2, when the antistatic liquid or antistatic adhesive penetrates into the upper surface of the insole body through the ventilation holes 2, it fills the ventilation holes, forming antistatic columns 5. The antistatic liquid or antistatic adhesive continues to spread on the upper surface of the insole body, forming a second antistatic layer 4 distributed in a dotted pattern. The second antistatic layer 4 radiates outward from the ventilation holes 2, meaning that the second antistatic layer 4 is discontinuous on the upper surface of the insole body. The second antistatic layer 4 and the antistatic adhesive columns in the ventilation holes ensure a permanent antistatic effect.

[0020] A further preferred embodiment involves using a fiber fabric for the insole body. The fiber fabric provides excellent breathability, allowing the antistatic adhesive or liquid to penetrate the upper surface of the insole body through the gaps in the fibers, thus ensuring a strong bond between the antistatic adhesive or liquid and the insole body. The antistatic pillar 5 is surrounded by fiber fabric, guaranteeing the insole's breathability and improving wearing comfort while maintaining antistatic effectiveness.

[0021] Antistatic performance test of antistatic insoles: The test method follows the national standard GB / T 20991-2007, Test Method for Personal Protective Equipment Footwear. It should be noted that, since this test method is for finished footwear testing, the 4 kg, 5 mm diameter stainless steel beads are replaced with 4 kg stainless steel weights, as stainless steel beads cannot be used for testing on insoles. The test standard follows GB 21148-2020, Requirements for Foot Protection Safety Footwear, with a resistance value greater than 100 kΩ and less than or equal to 1000 MΩ.

[0022] The resistance of the prepared antistatic insole was measured to be 37 MΩ, which meets the requirements of GB 21148-2020 for foot protection safety shoes, which stipulates that the resistance should be greater than 100kΩ and less than or equal to 1000 MΩ.

[0023] Example 2 Component A of the antistatic adhesive: 100 kg of liquid nitrile rubber, 2.3 kg of vulcanizing agent, 5.5 kg of zinc oxide, 4.5 kg of liquid tackifying resin, add diluent, stir and dilute in a reaction vessel to reach a viscosity of 8±4 min / 100ml (25℃). Component B: 100 kg of liquid nitrile rubber, 0.71 kg of first accelerator 2,2'-dithiodibenzothiazole, 0.92 kg of second accelerator N-cyclohexyl-2-benzothiazole sulfenamide, 0.49 kg of third accelerator tetramethylthiuram disulfide, 5.5 kg of zinc oxide, 1.8 kg of octadecanoic acid, 0.9 kg of antioxidant 2-thiol-benzoimidazole, 25 kg of acetylene black, 12 kg of carbon nanotube dispersion, add diluent, stir and dilute in the reactor to reach a viscosity of 8±4 min / 100ml (25℃).

[0024] The resistance of the prepared antistatic insole was measured to be 36 MΩ.

[0025] Example 3 Component A of the antistatic adhesive: 100 kg of liquid nitrile rubber, 2.5 kg of vulcanizing agent, 6.1 kg of zinc oxide, and 4.8 kg of liquid tackifying resin; Component B: 100 kg liquid nitrile rubber, 0.81 kg of first accelerator 2,2'-dithiodibenzothiazole, 1.0 kg of second accelerator N-cyclohexyl-2-benzothiazole sulfenamide, 0.50 kg of third accelerator tetramethylthiuram disulfide, 5.8 kg zinc oxide, 2.0 kg octadecanoic acid, 1.0 kg of antioxidant 2-thiol-benzoimidazole, 28 kg acetylene black, and 15 kg carbon nanotube dispersion. Other process conditions are the same as in Example 1.

[0026] The resistance of the prepared antistatic insole was measured to be 32 MΩ.

[0027] Example 4 Component A of the antistatic adhesive: 100 kg of liquid nitrile rubber, 2.5 kg of vulcanizing agent, 6.8 kg of zinc oxide, and 6.7 kg of liquid tackifying resin; Component B: 100 kg of liquid nitrile rubber, 0.89 kg of first accelerator 2,2'-dithiodibenzothiazole, 1.12 kg of second accelerator N-cyclohexyl-2-benzothiazole sulfenamide, 0.52 kg of third accelerator tetramethylthiuram disulfide, 7.2 kg of zinc oxide, 2.6 kg of octadecanoic acid, 1.0 kg of antioxidant 2-thiol-benzoimidazole, 28.6 kg of acetylene black, and 15.7 kg of carbon nanotube dispersion. Other process conditions are the same as in Example 1.

[0028] The resistance of the prepared antistatic insole was measured to be 31 MΩ.

[0029] Example 5 Component A of the antistatic adhesive: 100 kg of liquid nitrile rubber, 2.0 kg of vulcanizing agent, 4.8 kg of zinc oxide, and 3.8 kg of liquid tackifying resin; Component B: 100 kg of liquid nitrile rubber, 0.68 kg of first accelerator 2,2'-dithiodibenzothiazole, 0.86 kg of second accelerator N-cyclohexyl-2-benzothiazole sulfenamide, 0.41 kg of third accelerator tetramethylthiuram disulfide, 4.8 kg of zinc oxide, 1.5 kg of octadecanoic acid, 0.8 kg of antioxidant 2-thiol-benzoimidazole, 20.4 kg of acetylene black, and 10.6 kg of carbon nanotube dispersion. Other process conditions are the same as in Example 1.

[0030] The resistance of the prepared antistatic insole was measured to be 38 MΩ.

[0031] It should be noted that: raw materials not specified in detail are all commonly used raw materials in existing technologies. For example, coumarone is used as the liquid thickening resin, and ethyl acetate and xylene are used as diluents. Ethyl acetate is mainly used to reduce the viscosity of the liquid. Its dosage can be adjusted reasonably according to factors such as liquid viscosity and temperature. It has little impact on antistatic performance. Xylene is used to make the adhesive applied to the insole body cure as soon as possible without affecting the antistatic performance, so it is not described in detail.

[0032] The raw material dosage in the above embodiments is in kg, which is only for the convenience of description. The dosage of raw materials can be adjusted proportionally according to the production capacity and the capacity of instruments and equipment such as reaction vessels to meet the production conditions without affecting its antistatic ability.

[0033] The antistatic insole preparation method disclosed in this invention has a simple production process, reduces energy waste from large equipment, saves energy, and reduces production costs while ensuring quality by mixing the adhesive as needed.

[0034] The antistatic insole prepared by the method disclosed in this invention has a resistance value greater than 32MΩ, which meets the resistance value requirements of GB21148-2020 for foot protection safety shoes.

[0035] The above description is only a preferred embodiment of the present invention. It should be noted that those skilled in the art can make several changes and improvements without departing from the overall concept of the present invention, and these should also be considered within the scope of protection of the present invention.

Claims

1. A method for preparing an antistatic insole, characterized in that: Includes the following steps, a. Preparation of antistatic adhesive: Design a two-component antistatic adhesive, each component is stirred evenly in a reaction vessel and stored separately; b. Mix the two-component antistatic adhesive at a mass ratio of 1:1 evenly, and apply it evenly to the lower surface of the insole body. Complete the penetration and cross-linking reaction between the antistatic adhesive and the insole body through a plate vulcanization heating and pressurization method. The plate vulcanization temperature is 160±5℃, the time is 180±10s, and the pressure is 12±3 Mpa. The two-component antistatic adhesive comprises the following components by weight: 100 parts liquid nitrile rubber, 2.0-2.5 parts vulcanizing agent, 4.8-6.8 parts zinc oxide, 3.8-6.7 parts liquid tackifying resin, and a diluent to achieve a viscosity of 8±4 min / 100ml at 25℃. The following components by weight fraction are: 100 parts liquid nitrile rubber, 0.68-0.89 parts first accelerator, 0.86-1.12 parts second accelerator, 0.41-0.52 parts third accelerator, 4.8-7.2 parts zinc oxide, 1.5-2.6 parts octadecanoic acid, 0.8-1.0 parts antioxidant 2-thiol-benzoimidazole, 20.4-28.6 parts acetylene black, and 10.6-15.7 parts carbon nanotube dispersion. Diluent is added to achieve a viscosity of 8±4 min / 100ml at 25℃.

2. The method for preparing an antistatic insole according to claim 1, characterized in that: The amount of antistatic adhesive applied to the lower surface of the insole body is 10g-15g.

3. The method for preparing an antistatic insole according to claim 1, characterized in that: The first accelerator is 2,2'-dithiodibenzothiazole, the second accelerator is N-cyclohexyl-2-benzothiazole sulfenamide, and the third accelerator is tetramethylthiuram disulfide.

4. An antistatic insole, comprising an insole body (1), characterized in that: The insole body (1) has evenly distributed ventilation holes (2), and the lower surface of the insole body is coated with any of the antistatic adhesives described in claims 1-3 to form a first antistatic layer (3). The antistatic adhesive overflows from the ventilation holes (2) to the upper surface of the insole body, forming antistatic columns (5) in the ventilation holes, and forming a second antistatic layer (4) with dotted distribution on the upper surface of the insole body.

5. The antistatic insole according to claim 4, characterized in that: The insole body is made of fiber fabric.

Citation Information

Patent Citations

  • Antistatic dual-density rubber primer and preparation method thereof

    CN111138735A

  • Carbon nanotube antistatic sole and preparation method thereof

    CN116253937A

  • Antistatic insole

    CN221469193U