Pockmarked berry pattern glazed ceramics and preparation method thereof
By carving positioning pits and inlaying pitted particles on the ceramic glaze, combined with the specific components of the glaze and the glaze firing process, the problem of natural strawberry texture expression on the ceramic glaze is solved, and a unique and beautiful pitted strawberry pattern effect is achieved .
Patent Information
- Application Number
- CN202311164533.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-11
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2043-09-11
AI Technical Summary
The existing ceramic glaze is single in expression, the effect after firing is not natural enough, and it is difficult to achieve a natural strawberry texture effect.
The preparation method of pitted berry pattern glazed ceramics is adopted, by carving positioning pits and inlaying pitted particles on the body, applying the top glaze and then glaze firing in the kiln, using the annular pits and black pitted particles to form a unique Strawberry texture effect. The components of the top glaze include potash feldspar, calcite, quartz stone, dolomite, sodium silicate, bentonite, colorants and stabilizers. The pitted particles are composed of core materials and frit materials. Annular pits are formed during the glaze firing process. and black pitting, simulating the pits and seeds on a strawberry's surface.
The yellow-green effect of the glaze is achieved, showing the surface texture of unripe strawberries, which is uniquely beautiful. The combination of pit texture and black pitting forms a unique natural style.
Abstract
Description
Technical Field
[0001] The invention relates to the field of ceramics and preparation technology thereof, and in particular to pockmarked berry pattern glazed ceramics and a preparation method thereof. Background Art
[0002] Glaze is a colorless or colored glassy thin layer covering the surface of ceramic products. It is made of mineral raw materials (feldspar, quartz, talc, kaolin, etc.) and raw materials in a certain proportion (some raw materials can be made into frits first), ground into glaze slurry, applied to the surface of the body, and calcined at a certain temperature. It can increase the mechanical strength, thermal stability and dielectric strength of the product, and also beautify the objects, easy to wipe, and not corroded by dust and filth. Glaze can be divided into transparent glaze, opalescent glaze, matte glaze, glittering glaze, fluorescent glaze, monochrome glaze, color-changing glaze, textured glaze, etc. according to the appearance characteristics. Among them, the realization of textured glaze is mainly through painting or carving concave and convex textures on the body. The effect of fired glaze is not natural enough and the expression form is single. In view of this, this case is generated. Summary of the invention
[0003] An object of the present invention is to solve at least the above-mentioned problems through a pitted berry pattern glazed ceramic and a preparation method thereof.
[0004] In order to solve the above technical problems, the technical solution adopted by the present invention is as follows: a pitted berry-patterned glazed ceramic, comprising a body and a glaze, wherein the glaze is provided with pits of a color different from that of the glaze, and annular pits are distributed around the pits. The raw materials of the glaze include the following components by weight: 25-30 parts of potassium feldspar, 10-12 parts of calcite, 10-12 parts of quartz, 10-12 parts of dolomite, 5-8 parts of sodium silicate, 6-8 parts of bentonite, 5-6 parts of colorant, and 15-18 parts of stabilizer.
[0005] Preferably, the raw materials of the glaze include the following components by weight: 27 parts of potassium feldspar, 11 parts of calcite, 11 parts of quartz, 11 parts of dolomite, 6 parts of sodium silicate, 7 parts of bentonite, 5.5 parts of colorant, and 16 parts of stabilizer.
[0006] Preferably, the raw materials of the colorant include the following components by weight: 20-25 parts of tin dioxide, 25-30 parts of vanadium pentoxide, 10-15 parts of aluminum oxide, and 10-12 parts of quartz powder.
[0007] Preferably, the raw materials of the stabilizer include the following components by weight: 10-12 parts of spodumene, 8-10 parts of kaolin, 8-10 parts of alumina, 4-6 parts of sodium carboxymethyl cellulose and 4-6 parts of sodium alginate.
[0008] Preferably, the pitting and annular pits on the surface glaze are formed by glazing pitting particles, and the pitting particles include a core material and a frit material coated on an outer layer of the core material.
[0009] Preferably, the raw materials of the core material include the following components by weight: 10-12 parts of refractory clay, 15-18 parts of quartz stone, 5-8 parts of chromium trioxide, 5-8 parts of iron trioxide, 5-8 parts of manganese dioxide, and 5-8 parts of cobalt oxide.
[0010] Preferably, the raw materials of the frit material include the following components by weight: 12-15 parts of spodumene, 5-8 parts of sodium oxide, 10-12 parts of nepheline orthoclase, 8-10 parts of quartz, 14-15 parts of calcium carbonate, and 4-6 parts of CMC glue.
[0011] The method for preparing the above-mentioned pockmarked berry-patterned glazed ceramics comprises the following steps:
[0012] Step a, preparing a green body and drying it;
[0013] Step b, carving a positioning pit on the blank;
[0014] Step c, embedding pit particles in the positioning pits of the blank;
[0015] Step d, applying glaze on the surface of the body;
[0016] Step e, putting the glaze into the kiln for firing. After firing, annular pits are formed around the pitting particles, and the pitting particles protrude from the annular pits.
[0017] Preferably, in step c, the pitted particles are adhered to the pits of the blank by quick-drying glue.
[0018] Preferably, in step e, during the glaze firing process, the temperature is raised to 1150 degrees Celsius, kept warm for 1-2 hours, then dropped to 1050 degrees Celsius within 20-30 minutes, kept warm for 3-4 hours, then cooled to 500-600 degrees Celsius within 3-4 hours, and then cooled naturally.
[0019] From the above description, it can be seen that the pockmarked berry-patterned glazed ceramics and the preparation method thereof provided by the present invention have the following beneficial effects: the melting point of the core of the pockmarked particles is higher than that of the surface material, and the temperature is rapidly raised to 1150 degrees Celsius during the glaze firing process, and then dropped to 1050 degrees Celsius, so that the low-melting-point material on the surface of the pockmarked particles can be further fully melted, and the melting point of the low-melting-point material on the surface of the pockmarked particles is lower than that of the surface glaze, and annular pits are formed around the core of the pockmarked particles after glaze firing; the surface of the surface glaze has a pit texture distributed in a dotted manner, with black pockmarks inlaid in between, and the surface glaze is yellow-green, and its overall glaze effect resembles the surface texture of an unripe strawberry, which is unique in beauty. DETAILED DESCRIPTION
[0020] The present invention is further described below through specific implementation modes.
[0021] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.
[0022] The present invention discloses a glazed ceramic with pitted berry pattern, comprising a body and a glaze, wherein the glaze is provided with pitted berries of different colors from the glaze, and annular pits are provided around the pits, and the raw materials of the glaze include the following components by weight: 25-30 parts of potassium feldspar, 10-12 parts of calcite, 10-12 parts of quartz, 10-12 parts of dolomite, 5-8 parts of sodium silicate, 6-8 parts of bentonite, 5-6 parts of colorant, and 15-18 parts of stabilizer. The surface of the glaze has a pit texture distributed in a dotted manner, inlaid with black pits, and the glaze presents a yellow-green color. The overall glaze effect is similar to the surface texture of an unripe strawberry, and has a unique aesthetic feeling. The pit texture is similar to the pits on the surface of the strawberry, and the black pits are similar to the seeds on the surface of the strawberry.
[0023] The raw materials of the glaze include the following components by weight: 27 parts of potassium feldspar, 11 parts of calcite, 11 parts of quartz, 11 parts of dolomite, 6 parts of sodium silicate, 7 parts of bentonite, 5.5 parts of colorant, and 16 parts of stabilizer.
[0024] The raw materials of the pigment include the following components by weight: 20-25 parts of tin dioxide, 25-30 parts of vanadium pentoxide, 10-15 parts of aluminum oxide, and 10-12 parts of quartz powder. The components of the pigment are calcined at 1300 degrees Celsius, cooled and crushed to obtain yellow-green pigment powder.
[0025] The raw materials of the stabilizer include the following components by weight: 10-12 parts of spodumene, 8-10 parts of kaolin, 8-10 parts of alumina, 4-6 parts of sodium carboxymethyl cellulose and 4-6 parts of sodium alginate. Kaolin and alumina as stabilizers can significantly improve the bonding of body and glaze, and the compounding of sodium carboxymethyl cellulose and sodium alginate can improve the stability of glaze, making it difficult for glaze to precipitate. By changing the electromagnetic field charge of glaze, the elements resist each other, thereby maintaining a uniform suspension state, thereby improving the stability and strength of glaze.
[0026] The pitting and annular pits on the surface glaze are formed by glazing the pitting particles. The pitting particles include a core material and a frit material coated on the outer layer of the core material. The pitting particles can be prepared by the following method: first, the core material is fired, and the particle size is 1.5-2mm. The components of the frit material are configured in proportion and fully mixed. After clamping the core material with tweezers, it is immersed in a ceramic binder, so that the binder adheres to the surface of the core material, and then immersed in the raw material of the frit material. The raw material powder of the frit material is adsorbed on the binder. After the frit material is quickly dried by hot air, it is gently tapped to separate the pitting particles from the tweezers, and then the pitting particles are re-clamped by changing the angle of the tweezers. The above steps are repeated until the frit material reaches the specified thickness. The thickness of the frit material is about 0.5-1.5mm.
[0027] The raw materials of the core material include the following components by weight: 10-12 parts of refractory clay, 15-18 parts of quartz, 5-8 parts of chromium trioxide, 5-8 parts of ferric oxide, 5-8 parts of manganese dioxide, and 5-8 parts of cobalt oxide. Refractory clay has good refractory properties and can significantly increase the melting point of the core material. In addition to the relatively high content of quartz and coloring oxides, the melting point of the core material is relatively high, and the overall shape and color stability can be maintained during the low-temperature glaze firing process. After the components of the core material are ball-milled and mixed, they are calcined at a high temperature of 1300 degrees Celsius, and then broken into black particles of the required particle size after cooling. Particles with appropriate particle sizes are selected for use; during the glaze firing process, the frit material on the surface of the core material melts first due to its good fluidity, and at the same time drives the surface glaze to melt. In addition, the core material has a larger particle diameter, so the core material protrudes from the surface glaze after firing.
[0028] The raw materials of the frit material include the following components by weight: 12-15 parts of spodumene, 5-8 parts of sodium oxide, 10-12 parts of nepheline orthoclase, 8-10 parts of quartz, 14-15 parts of calcium carbonate, and 4-6 parts of CMC glue. The proportion of alkaline oxides in the fluxes such as spodumene, sodium oxide, nepheline orthoclase in the frit material is relatively high, so that the melting point of the frit material is lower than that of the core material and the glaze, so it has stronger fluidity during the glaze firing process. In addition, in the process of preparing the pitted particles, a ceramic organic binder is added to the surface layer, and the ceramic organic binder is decomposed and carbonized during the glaze firing process, thereby forming annular pits around the core material during the glaze firing process.
[0029] The preparation method of the pockmarked berry pattern glazed ceramic comprises the following steps:
[0030] Step a, preparing a green body and drying it;
[0031] Step b, carving a positioning pit on the blank;
[0032] Step c, embedding pit particles in the positioning pits of the blank;
[0033] Step d, applying glaze on the surface of the body;
[0034] Step e, glaze firing in a kiln. After glaze firing, annular pits are formed around the pitting particles, and the pitting particles protrude from the annular pits. In step d, the thickness of the top glaze is lower than the pitting particles. In addition, during the glaze firing process, the top glaze has good fluidity, so that the top glaze covering the surface of the pitting particles spreads outward during glazing, and most of the pitting particles protrude from the top glaze and are not covered by the top glaze.
[0035] In step c, the pitted particles are glued to the pits of the blank by quick-drying glue. The pits carved on the blank are circular or nearly circular, and the pitted particles are adapted to the pit shapes of the blank. During operation, quick-drying glue is first applied to the pits, and then the pitted particles are clamped and fixed in the pits by tweezers; the quick-drying glue has other functions: the quick-drying glue is a polymer substance, and the gas generated by decomposition during glaze firing overflows from around the pitted particles, accelerating the formation of the annular pit area; because the quick-drying glue is located between the blank and the pitted particles, and when the pitted particles are prepared, the outer layer also includes a ceramic binder, and some undecomposed organic carbon is deposited, resulting in black halos around the pitted particles.
[0036] In step e, during the glaze firing process, the temperature is raised to 1150 degrees Celsius, kept warm for 1-2 hours, then dropped to 1050 degrees Celsius within 20-30 minutes, kept warm for 3-4 hours, then cooled to 500-600 degrees Celsius within 3-4 hours, and then cooled naturally. The melting point of the core of the pitting particles is higher than that of the surface material. During the glaze firing process, the temperature is quickly raised to 1150 degrees Celsius, and kept warm for a short time to make the pitting particles slightly melted, eliminating the edges and corners of the core material and making it smoother; then dropped to 1050 degrees Celsius, so that the low-melting-point material on the surface of the pitting particles is further fully melted. The melting point of the low-melting-point material on the surface of the pitting particles is lower than that of the glaze, so its flow rate is faster than that of the glaze. In addition, stabilizers are added to the glaze, and the low-melting-point material on the surface of the pitting particles flows out. After the glaze is fired, an annular pit is formed around the core of the pitting particles, and it is quickly cooled to 500-600 degrees Celsius to shape the annular pit.
[0037] The above are only some specific implementation methods of the present invention, but the design concept of the present invention is not limited thereto. Any non-substantial changes to the present invention using this concept shall be deemed as an infringement of the protection scope of the present invention.
Claims
1. Pockmarked berry pattern glazed ceramics, characterized by: The invention comprises a body and a glaze, wherein the glaze is provided with pits of different colors from the glaze, and annular pits are provided around the pits, and the raw materials of the glaze include the following components by weight: 25-30 parts of potassium feldspar, 10-12 parts of calcite, 10-12 parts of quartz, 10-12 parts of dolomite, 5-8 parts of sodium silicate, 6-8 parts of bentonite, 5-6 parts of colorant, and 15-18 parts of stabilizer; the pits and annular pits on the glaze are formed by glazing the pitted particles, and the pitted particles include a core The raw materials of the core material include the following components by weight: 10-12 parts of refractory clay, 15-18 parts of quartz, 5-8 parts of chromium trioxide, 5-8 parts of iron trioxide, 5-8 parts of manganese dioxide, and 5-8 parts of cobalt oxide; the raw materials of the frit material include the following components by weight: 12-15 parts of spodumene, 5-8 parts of sodium oxide, 10-12 parts of nepheline orthoclase, 8-10 parts of quartz, 14-15 parts of calcium carbonate, and 4-6 parts of CMC glue; The method for preparing the pockmarked berry pattern glazed ceramic comprises the following steps: Step a, preparing a green body and drying it; Step b, carving a positioning pit on the blank; Step c, embedding pit particles in the positioning pits of the blank; Step d, applying glaze on the surface of the body; Step e, putting the mixture into a kiln for glaze firing, after which an annular pit is formed around the pitted particles, and the pitted particles protrude from the annular pit; In the step e, during the glaze firing process, the temperature is raised to 1150 degrees Celsius, kept at this temperature for 1-2 hours, then lowered to 1050 degrees Celsius within 20-30 minutes, kept at this temperature for 3-4 hours, then cooled to 500-600 degrees Celsius within 3-4 hours, and then cooled naturally; The pitted particles are prepared by the following method: first, the core material is fired to a particle size of 1.5-2 mm, the components of the frit are configured in proportion and fully mixed, the core material is clamped by tweezers and immersed in a ceramic binder, the binder is adhered to the surface of the core material, and then immersed in the raw material of the frit material, the raw material powder of the frit material is adsorbed on the binder, the frit material is quickly dried by hot air, and then gently tapped to separate the pitted particles from the tweezers, and then the tweezers are changed The angle of the pitted particles is re-clamped, and the above steps are repeated until the frit material reaches a specified thickness. The thickness of the frit material is 0.5-1.5 mm.
2. The pockmarked berry pattern glazed ceramic according to claim 1, characterized in that: The raw materials of the glaze include the following components by weight: 27 parts of potassium feldspar, 11 parts of calcite, 11 parts of quartz, 11 parts of dolomite, 6 parts of sodium silicate, 7 parts of bentonite, 5.5 parts of colorant, and 16 parts of stabilizer.
3. The pockmarked berry pattern glazed ceramic according to claim 1, characterized in that: The raw materials of the colorant include the following components by weight: 20-25 parts of tin dioxide, 25-30 parts of vanadium pentoxide, 10-15 parts of aluminum oxide, and 10-12 parts of quartz powder.
4. The pockmarked berry pattern glazed ceramic according to claim 1, characterized in that: The raw materials of the stabilizer include the following components by weight: 10-12 parts of spodumene, 8-10 parts of kaolin, 8-10 parts of alumina, 4-6 parts of sodium carboxymethyl cellulose and 4-6 parts of sodium alginate.
5. The pockmarked berry pattern glazed ceramic according to claim 1, characterized in that: In the step c, the pitted particles are adhered to the pits of the blank by using quick-drying glue.