Anti-resonance hollow optical fiber preform and its preparation method

By using a central support tube and laser welding or absorption film to form a bond in anti-resonant hollow optical fiber, the problems of decreased mechanical strength and optical loss in existing processes are solved, and high-quality optical fiber manufacturing is achieved.

CN117836247BActive Publication Date: 2026-11-17CORNING INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202280055209.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-08-06
Filing Date
2022-07-27
Publication Date
2026-11-17
Estimated Expiration
2042-07-27

AI Technical Summary

Technical Problem

In existing anti-resonance hollow fiber manufacturing processes, there are problems such as adhesive compound detachment and suboptimal effects and decreased mechanical strength caused by laser welding.

Method used

A central support tube is used to fix the glass tube inside the hollow outer cladding. The joint is formed by laser welding or absorption film to avoid direct jointing to the outer cladding. The joint position is formed by using connecting components and heat source.

Benefits of technology

This improves the mechanical strength of anti-resonance optical fibers, reduces optical loss, and avoids the defects found in traditional processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117836247B_ABST
    Figure CN117836247B_ABST
Patent Text Reader

Abstract

An anti-resonance hollow optical fiber preform (100) includes an outer cladding (110), a plurality of structural tubes (120), and a central support tube (130). The outer cladding (110) has a length L, a central longitudinal axis, and a hollow interior. The plurality of structural tubes (120) are disposed within the hollow interior of the outer cladding (110), and the length of each of the plurality of structural tubes (120) extends along the length of the outer cladding (110). Furthermore, the central support tube (130) is disposed within the hollow interior of the outer cladding (110) such that the plurality of structural tubes (120) are disposed radially outside the central support tube (130), and the length of the central support tube (130) extends along the central longitudinal axis of the outer cladding (110). Additionally, the length of the central support tube (130) is less than the length L of the outer cladding (110). A method of manufacturing the preform (100) includes joining the central support tube (130) to the plurality of structural tubes (120).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application claims priority to U.S. Provisional Application No. 63 / 230,283, filed August 6, 2021, the contents of which are incorporated herein by reference in their entirety. Technical Field

[0002] This disclosure relates to an anti-resonance hollow optical fiber and a method for manufacturing the same. Background Technology

[0003] Anti-resonant hollow optical fiber traditionally comprises a hollow cladding containing multiple glass tubes. The diameter and thickness of each glass tube are smaller than the cladding. Each glass tube is bonded to the inner surface of the cladding, arranging them around the inner circumference of the cladding. Furthermore, each glass tube is parallel to the length of the cladding. The central portion of the cladding (around which the glass tubes are arranged) retains a void, forming an air-filled cavity. The resulting anti-resonant optical fiber guides light through the hollow portion of the core. This type of anti-resonant optical fiber reduces optical signal loss.

[0004] However, such anti-resonance optical fibers are extremely difficult to manufacture. Current manufacturing processes include using adhesive compounds or laser welding to bond the glass tube to the cladding. However, both processes result in suboptimal anti-resonance optical fibers. More specifically, even a small amount of the adhesive compound detaching and depositing on the glass tube will cause attenuation. Furthermore, laser welding can damage the cladding, leading to a decrease in the fiber's mechanical strength.

[0005] Therefore, it is necessary to produce an anti-resonant hollow optical fiber that will not produce such suboptimal results. Invention Overview

[0006] The independent claims describe exemplary methods for achieving this objective. The dependent claims define various implementations.

[0007] This disclosure relates to an anti-resonance hollow optical fiber and a method for manufacturing the same. The optical fiber is made from a preform including a central support tube for securing glass tubes within a hollow cladding. The length of each glass tube extends beyond the length of the cladding. However, the extension length of the central support tube is less than the length of the cladding. More specifically, the extension length of the central support tube is sufficient to secure the glass tubes around the inner circumference of the cladding. The glass tubes are disposed radially outside the central support tube, and the cladding is disposed radially outside the glass tubes. When manufacturing the anti-resonance hollow optical fiber using the preform, the portion of the preform including the central support tube is removed, resulting in a hollow optical fiber along its entire length.

[0008] According to a first aspect, an anti-resonance hollow optical fiber preform is disclosed, comprising an outer cladding, a plurality of structural tubes, and a central support tube. The outer cladding has a length, a central longitudinal axis, and a hollow interior. The plurality of structural tubes are disposed within the hollow interior of the outer cladding, and the length of each of the plurality of structural tubes extends the length of the outer cladding. Furthermore, the central support tube is disposed within the hollow interior of the outer cladding such that the plurality of structural tubes are located radially outside the central support tube, and the length of the central support tube extends along the central longitudinal axis of the outer cladding. Additionally, the length of the central support tube is less than the length of the outer cladding.

[0009] According to another aspect, a method for manufacturing an anti-resonance hollow optical fiber preform is disclosed. The method includes the steps of: joining a central support tube to a plurality of structural tubes such that the plurality of structural tubes are disposed radially outside the central support tube; and providing a hollow cladding surrounding the central support tube and the plurality of structural tubes. Each of the plurality of structural tubes extends the length of the cladding, and the length of the central support tube is less than the length of the cladding.

[0010] Although many different implementations are listed, these implementations may exist alone or in any possible combination. Exemplary implementations are shown and described below. Brief description of the attached figures

[0011] Figure 1 A perspective view of a preform for producing anti-resonant hollow optical fiber according to an embodiment of the present disclosure is shown.

[0012] Figure 2 A preform along an embodiment of the present disclosure is shown. Figure 1 A cross-sectional view of the BB line;

[0013] Figures 3A-3E Cross-sectional views of various exemplary embodiments of the prefabricated component according to the present disclosure are shown;

[0014] Figure 4 An exemplary process for bonding glass materials to form a preform according to an embodiment of the present disclosure is shown;

[0015] Figure 5 Another exemplary process for bonding glass materials to form a preform according to an embodiment of the present disclosure is shown;

[0016] Figure 6A and 6B Cross-sectional views of various exemplary embodiments of prefabricated components according to other embodiments of this disclosure are shown; and

[0017] Figure 7 A schematic diagram of an exemplary drawing system is shown. Detailed Implementation

[0018] Other features and advantages of this disclosure are set forth in the following detailed description, which will be readily apparent to those skilled in the art from the description, or will be recognized by practicing the disclosure described herein, including the following detailed description, together with the claims and drawings.

[0019] The term “and / or” as used herein, when used to list two or more items, means that any one of the listed items may be used alone, or any combination of two or more of the listed items may be used. For example, if a composition is described as containing components A, B and / or C, then the composition may contain only A; only B; only C; a combination of A and B; a combination of A and C; a combination of B and C; or a combination of A, B and C.

[0020] In this document, relative terms, such as first and second, top and bottom, are used only to distinguish one entity or behavior from another, and are not required to require or imply any actual such relationship or order between these entities or behaviors.

[0021] Those skilled in the art will understand that the construction of the disclosure and other components is not limited to any particular material. Unless otherwise stated herein, other exemplary embodiments of this disclosure may be formed from a variety of materials.

[0022] It is equally important to note that the construction and arrangement of the elements in this disclosure, as shown in the exemplary embodiments, are illustrative only. Although only some embodiments are described in detail in this disclosure, those skilled in the art will readily understand that many modifications can be made (e.g., changes in the size, dimensions, structure, shape, and proportions of various elements; various parameters; mounting arrangements; the use of materials; orientations, etc.) without substantially departing from the novelty and non-obvious teachings and advantages of the subject matter. For example, an element shown as an integral form may be composed of multiple parts, or an element shown as multiple parts may be integrally formed; the operation of the interface may be reversed or otherwise altered; the structure of the system and / or the length or width of the elements, or connectors, or other elements may be changed; and the nature or number of adjustment positions between the elements may be changed. It should be noted that the elements and / or components of the system may be constructed from any of a variety of materials that provide sufficient strength or durability in any of a variety of colors, textures, and combinations. Therefore, all such modifications are included within the scope of this disclosure. Other substitutions, modifications, alterations, and omissions may be made to the design, operating conditions, and arrangements of desired and other exemplary embodiments without departing from the spirit of this disclosure.

[0023] Preferred embodiments of this disclosure will now be described in detail, examples of which are illustrated in the accompanying drawings. Where possible, the same reference numerals will be used in all the drawings to denote the same or similar parts.

[0024] Now for reference Figure 1 The illustration shows an exemplary anti-resonant hollow optical preform 100. The preform 100 has a length L, an outer diameter D, and a central longitudinal axis A. The preform 100 can be drawn to form an anti-resonant hollow optical fiber. As is known in the art, anti-resonant optical fiber is a type of hollow optical fiber. There are three types of hollow optical fibers. The first type is Bragg hollow fiber, where the cladding is a Bragg structure of a concentric periodic dielectric multilayer that confines light to a hollow (air) region. The second type is photonic bandgap hollow fiber, which uses a two-dimensional photonic crystal structure with periodically arranged air holes that confine light to the hollow region. The third type is anti-resonant hollow fiber, where the fiber includes one or more thin glass tubes to prevent light leakage from the air core. The wall thickness of the glass tube is chosen such that light at a specific wavelength does not resonate within the thin glass layers, resulting in zero transmittance through the glass tube wall. Figure 1 As shown, the prefabricated component 100 includes an outer cladding layer 110, a plurality of structural tubes 120, and one or more central support tubes 130. The structural tubes 120 are arranged radially around the central support tubes 130, and the outer cladding layer 110 is arranged radially around the structural tubes 120.

[0025] The outer cladding 110 is a hollow cylindrical member formed of glass. Therefore, the outer cladding 110 has a hollow interior, forming a ring-shaped donut in cross-section. In some embodiments, the outer cladding 110 is formed of doped or undoped silica glass. The length of the outer cladding 110 is equal to the length L of the preform 100. In some embodiments, the length of the outer cladding 110 (and therefore the length L of the preform 100) is about 10 cm to about 2 m, or about 25 cm to about 1.5 m, or about 50 cm to about 1 m.

[0026] The outer diameter of the outer cladding 110 may be the outer diameter D of the preform 100. In some embodiments, the outer diameter of the outer cladding 110 (and therefore the outer diameter D of the preform 100) is about 10 mm or more, or about 20 mm or more, or about 40 mm or more, or about 60 mm or more, or about 80 mm or more, or about 100 mm or more, or about 120 mm or more. Alternatively or additionally, the outer diameter of the outer cladding 110 may be about 150 mm or less, or about 140 mm or less, or about 125 mm or less, or about 110 mm or less, or about 100 mm or less, or about 80 mm or less. In some embodiments, the outer diameter is about 10 mm to about 150 mm, or about 20 mm to about 125 mm, or about 10 mm to about 100 mm, or about 10 mm to about 50 mm. Furthermore, the inner diameter of the outer sheath 110 may be about 3 mm or greater, or about 5 mm or greater, or about 10 mm or greater, or about 20 mm or greater, or about 40 mm or greater, or about 60 mm or greater, or about 80 mm or greater, or about 100 mm or greater, or about 120 mm or greater. Alternatively or additionally, the inner diameter of the outer sheath 110 may be about 125 mm or less, or about 100 mm or less, about 80 mm or less, or about 60 mm or less, or about 40 mm or less, or about 20 mm or less, or about 10 mm or less. In some embodiments, the inner diameter is about 3 mm to about 125 mm, or about 10 mm to about 100 mm, or about 20 mm to about 60 mm. Therefore, the thickness of the outer sheath 110 is about 7 mm to about 25 mm, or about 8 mm to about 20 mm, or about 10 mm to about 18 mm, or about 12 mm to about 16 mm.

[0027] The structural tube 120 is a glass tube disposed within the hollow interior of the outer cladding 110. Similar to the outer cladding 110, the structural tube 120 is a hollow cylindrical member formed of glass. Therefore, each structural tube 120 forms a ring-shaped donut in cross-section. In some embodiments, the structural tube 120 is formed of doped or undoped silica glass. Figure 1 As shown, the length of each structural tube 120 extends the length of the outer sheath 110 (or substantially extends the length of the outer sheath 110). Therefore, the structural tube 120 and the outer sheath 110 can have the same length. However, each structural tube 120 has a smaller outer diameter than the outer diameter of the outer sheath 110. The outer diameter of the structural tube 120 can be about 10 mm or more, or about 15 mm or more, or about 20 mm or more, or about 25 mm or more. Alternatively or additionally, the outer diameter of the structural tube 120 is about 30 mm or less, or about 25 mm or less, or about 20 mm or less, or about 15 mm or less. In some embodiments, the diameter is about 10 mm to about 35 mm, or about 15 mm to about 30 mm.

[0028] The inner diameter of the structural tube 120 may be about 6 mm or greater, or about 8 mm or greater, or about 12 mm or greater, or about 16 mm or greater, or about 22 mm or greater, or about 24 mm or greater. Alternatively or additionally, the inner diameter of the structural tube 120 may be about 34 mm or less, or about 30 mm or less, or about 29 mm or less, or about 24 mm or less, or about 14 mm or less, or about 12 mm or less, or about 9 mm or less, or about 8 mm or less. In some embodiments, the inner diameter is about 6 mm to about 34 mm, or about 14 mm to about 29 mm. Therefore, the thickness of the structural tube 120 is about 0.5 mm to about 2 mm, or about 0.8 mm to about 1.8 mm, or about 1 mm to about 1.5 mm, or about 1.2 mm to about 1.4 mm. Thus, each structural tube 120 may have a thickness smaller than that of the outer cladding 110.

[0029] like Figure 1 As shown, structural tubes 120 are disposed radially inside the outer cladding 110 and spaced apart around the inner circumference 115 of the outer cladding 110, the inner circumference 115 forming the inner diameter of the outer cladding 110. In some embodiments, as described below, adjacent structural tubes 120 are spaced apart by gaps.

[0030] The outer diameter of each structural tube 120 is smaller than the inner diameter of the outer cladding 110. Therefore, the structural tube 120 does not occupy the entire hollow interior of the outer cladding 110. Instead, when the structural tubes 120 are spaced apart around the inner circumference 115 of the outer cladding 110, a hollow 140 is formed on the radially inner side of the structural tube 120. Figure 2 ).

[0031] As discussed further below, in some embodiments, compared to conventional anti-resonance hollow optical fibers, the structural tube 120 is not bonded to the inner surface of the cladding 110. Instead, the structural tube 120 is secured in place within the preform 100 by one or more central support tubes 130. Figure 1 As further shown, the central support tube 130 is disposed within the hollow interior of the outer cladding layer 110, such that the central support tube 130 is located radially inside both the outer cladding layer 110 and the structural tube 120. Therefore, the structural tube 120 is located radially outside the central support tube 130. Figure 1One embodiment is shown in which the preform 100 includes a first central support tube 132 at a first end 112 of the preform 100 and a second central support tube 134 at a second end 114 of the preform. However, it is also contemplated that the preform 100 may include only a single central support tube 130. For example, the preform 100 may include only the first central support tube 132 at the first end 112 of the preform. In some embodiments, it is also contemplated that one or more central support tubes 130 may be located between the first end 112 and the second end 114 of the preform 100, for example, at the central portion of the preform 100.

[0032] Similar to the cladding 110 and structural tube 120, the central support tube 130 is a hollow cylindrical member formed of glass. Therefore, each structural tube 120 forms an annular donut shape in cross-section. It should be noted that the central support tube 130 is hollow to allow gas to flow within the preform 100, thereby maintaining a predetermined pressure within the preform 100. In some embodiments, the central support tube 130 is formed of doped or undoped silica glass. As discussed further below, the portion of the preform 100 including the central support tube 130 may be discarded instead of being drawn into an optical fiber. Therefore, the central support tube 130 may be formed of a glass material of lower quality than that of the cladding 110 and / or structural tube 120. For example, the viscosity and / or purity of the material of the central support tube 130 may be lower than that of the materials of the cladding 110 and / or structural tube 120.

[0033] like Figure 1 As shown, the length of each central support tube 130 extends along the central longitudinal axis of the outer sheath 110. Therefore, the central support tube 130 is coaxial with the outer sheath 110 and parallel to the outer sheath 110 and the structural tube 120. However, the length of each central support tube 130 is less than the length of the outer sheath 110. Furthermore, the length of each central support tube 130 may be less than the length of the structural tube 120. In some embodiments, the length of each central support tube 130 is less than the length of at least one structural tube 120. In other embodiments, the length of each central support tube 130 is less than the length of each structural tube 120.

[0034] The length of each central support tube 130 is approximately half, one-third, one-quarter, one-fifth, one-sixth, one-tenth, one-fifteenth, one-twentieth, or one-thirtieth of the length of the outer sheath 110. For example, in some embodiments, the length of each central support tube 130 is approximately 20 cm or less, or approximately 15 cm or less, or approximately 10 cm or less, or approximately 7 cm or less, or approximately 5 cm or less, or approximately 3 cm or less, or approximately 2.5 cm or less, or approximately 2.25 cm or less, or approximately 2.0 cm or less, or approximately 1.75 cm or less, or approximately 1.5 cm or less, or approximately 1.25 cm or less, or approximately 1.0 cm or less, or approximately 0.5 cm or less. Alternatively or additionally, the length of each central support tube 130 is approximately 0.5 cm or greater, or approximately 1.0 cm or greater, or approximately 1.25 cm or greater, or approximately 1.5 cm or longer, or approximately 1.75 cm or greater, or approximately 2.0 cm or greater, or approximately 2.25 cm or greater, or approximately 2.5 cm or greater, or approximately 3 cm or greater, or approximately 5 cm or greater. In some embodiments, the length of each central support tube 130 is approximately 0.5 cm to approximately 10 cm, or approximately 1.0 cm to approximately 8 cm, or approximately 1.25 cm to approximately 5 cm. It is also conceivable that the first central support tube 132 may have a different length than the second central support tube 134.

[0035] The outer diameter of the central support tube 130 may be about 20 mm or greater, or about 25 mm or greater, or about 30 mm or greater, or about 35 mm or greater, or about 40 mm or greater, or about 45 mm or greater, or about 50 mm or greater. Alternatively or additionally, the outer diameter of the central support tube 130 may be about 70 mm or less, or about 65 mm or less, or about 60 mm or less, or about 55 mm or less, or about 50 mm or less, or about 45 mm or less, or about 40 mm or less. In some embodiments, the outer diameter is about 20 mm to about 70 mm, or about 25 mm to about 65 mm, or about 30 mm to about 60 mm. The inner diameter of the central support tube 130 can be about 10 mm or more, or about 12 mm or more, or about 18 mm or more, or about 20 mm or more, or about 24 mm or more, or about 26 mm or more, or about 30 mm or more, or about 34 mm or more. Alternatively or additionally, the inner diameter of the central support tube 130 can be about 60 mm or less, or about 54 mm or less, about 52 mm or less, or about 46 mm or less, or about 42 mm or less, or about 38 mm or less, or about 34 mm or less, or about 28 mm or less. The inner diameter can be from about 10 mm to about 60 mm, or from about 20 mm to about 40 mm. Therefore, the thickness of each central support tube 130 can be from about 5 mm to about 20 mm, or from about 10 mm to about 15 mm. Figure 1 As shown, the outer diameter of the central support tube 130 is larger than the outer diameter of each structural tube 120. However, as discussed further below, it is also conceivable that the outer diameter of the central support tube 130 is less than or equal to the outer diameter of one or more structural tubes 120. In some embodiments, the outer diameter of the central support tube 130 is smaller than the outer diameter of each structural tube 120. It is also conceivable that the first central support tube 132 may have a different outer diameter and / or inner diameter than the second central support tube 134.

[0036] Figure 2 Precast component 100 along Figure 1 Cross-sectional view of the middle BB line. (See diagram below.) Figure 2 As shown, the structural tubes 120 are arranged around the inner circumference 115 of the outer cladding 110, so that the hollow 140 is formed on the radial inner side of the structural tubes 120. Figure 2 This is a cross-sectional view of the central portion of precast component 100, therefore the central support tube 130 is not shown. Figure 1 and Figure 2 The embodiment shown is located at the end of the preform 100.

[0037] Figures 3A-3E Cross-sectional views of various exemplary embodiments of the central support tube 130 within the prefabricated component 100 are shown. More specifically, Figure 3A One embodiment is shown in which the structural tube 120 and the central support tube 130 both have the same outer diameter, inner diameter and thickness. Figure 3B One embodiment is shown in which the structural tube 120 and the central support tube 130 have the same outer diameter. However, in this embodiment, the central support tube 130 has a smaller inner diameter than the structural tube 120, and therefore a greater thickness. Figure 3C One embodiment is shown in which the central support tube 130 has a larger outer diameter and a larger inner diameter than the structural tube 120. Furthermore, in this embodiment, the central support tube 130 and the structural tube 120 have the same thickness, although it is also conceivable that they may include different thicknesses. Figure 3D One embodiment is shown in which the central support tube 130 has a smaller outer diameter and a smaller inner diameter than the structural tube 120. Furthermore, in this embodiment, the central support tube 130 has a smaller thickness than the structural tube 120.

[0038] It should also be noted that, Figures 3A-3D In each embodiment, the structural tube 120 has uniform dimensions. Therefore, for example, Figure 3AAll structural tubes 120 in the present invention have the same dimensions, including the same outer diameter, inner diameter, and thickness. However, in the embodiments disclosed herein, it is also conceivable that one or more structural tubes 120 may have dimensions different from those of one or more other structural tubes 120. For example, referring again... Figure 3A In one embodiment, one or more structural tubes 120 may be thicker than one or more other structural tubes 120.

[0039] exist Figure 3A , 3B In the exemplary 3D implementation, each structural tube 120 is in direct contact with its adjacent structural tube 120. Therefore, structural tube 120 forms a contact point 150 with its adjacent structural tube 120. However, in Figure 3C In this embodiment, adjacent structural tubes 120 do not directly contact each other. Therefore, in this embodiment, the prefabricated component 100 does not include the contact point 150 between adjacent structural tubes 120. Instead, in Figure 3C In this embodiment, adjacent structural tubes 120 are separated by a gap G. Figure 3E It shows Figure 3C A magnified view of a portion is provided to better illustrate the gap G. As disclosed herein, the gap G is the minimum distance between adjacent structural tubes 120 that are not in direct contact with each other. The length of the gap G may be consistent among the structural tubes 120 in the same preform 100, such that all structural tubes 120 are uniformly spaced around the inner circumference 115. However, it is also conceivable that the structural tubes 120 are not all uniformly spaced around the circumference 115, such that, for example, the length of the first gap G between the first and second structural tubes 120 is at least different from the length of the second gap G between the third and fourth structural tubes 120.

[0040] The length of the gap G can be approximately 1 mm or greater, or approximately 1.2 mm or greater, or approximately 1.4 mm or greater, or approximately 1.6 mm or greater, or approximately 1.8 mm or greater, or approximately 2 mm or greater, or approximately 2.2 mm or greater, or approximately 2.4 mm or greater, or approximately 2.6 mm or greater, or approximately 2.8 mm or greater, or approximately 3 mm or greater, or approximately 3.2 mm or greater, or approximately 3.4 mm or greater, or approximately 3.6 mm or greater, or approximately 3.8 mm or greater, or approximately 4 mm or greater. Alternatively or additionally, the length of the gap G may be about 5 mm or less, or about 4.8 mm or less, or about 4.6 mm or less, or about 4.4 mm or less, or about 4.4 mm or less, or about 4.2 mm or less, or about 4 mm or less, or about 3.8 mm or less, or about 3.6 mm or less, or about 3.4 mm or less, or about 3.2 mm or less, or about 3 mm or less. In some embodiments, the length is about 1 mm to about 5 mm, or about 2.5 mm to about 4.5 mm, or about 3 mm to about 4 mm.

[0041] Although this article references Figure 3C and 3E While the gap G is disclosed, it is also conceivable that one or more other embodiments may include the gap G between the structural tubes 120. For example, an embodiment in which the central support tube 130 has a greater thickness than the structural tubes 120, for example... Figure 3B The illustrated embodiment may include a gap G between adjacent structural tubes 120.

[0042] It should also be noted that Figure 3A , 3B The embodiments shown in section 3C illustrate an exemplary embodiment in which the prefabricated component 100 includes six structural tubes 120. However, Figure 3D An exemplary embodiment includes five structural tubes 120. It is further envisioned that the prefabricated component 100 of the embodiments disclosed herein may include more or fewer structural tubes 120. For example, the prefabricated component 100 may include one or more, or two or more, or three or more, or four or more, or five or more, or six or more, or seven or more, or eight or more, or nine or more, or ten or more, or eleven or more, or twelve or more structural tubes 120. Additionally or alternatively, the prefabricated component 100 may include 20 or fewer, or 19 or fewer, or 18 or fewer, or 17 or fewer, or 16 or fewer, or 15 or fewer, or 14 or fewer, or 13 or fewer, or 12 or fewer, or 11 or fewer, or 10 or fewer, or nine or fewer, or eight or fewer structural tubes 120. In some embodiments, the preform 100 includes 4 to 10 structural tubes 120, or 5 to 8 structural tubes 120.

[0043] As described above, structural tube 120 can form contact point 150 with adjacent structural tubes 120. Furthermore, as... Figures 3A-3EAs shown, the structural tube 120 may form a contact point 160 with the outer cladding 110 and a contact point 170 with the central support tube 130. Contact points 150, 160, and 170 may each be a distinct direct contact point between different glass components or between portions of different glass components that are in direct contact with each other. Although the structural tube 120 contacts the outer cladding 110 at contact point 160, in some embodiments, the structural tube 120 is not engaged with the outer cladding 110. By not engaging the structural tube 120 with the outer cladding 110, it helps to avoid damage to the outer cladding 110. For example, laser welding the structural tube 120 to the outer cladding 110 may cause partial breakage of the outer cladding 110, potentially damaging it. Any damage to the outer cladding 100 may result in a decrease in the mechanical strength of the fibers. Therefore, embodiments of this disclosure include situations where the structural tube 120 is not engaged with the outer cladding 110, even though the components are still in direct contact with each other at contact point 160.

[0044] However, in other embodiments, it is also conceivable that the structural tube 120 is joined to the outer cladding 110 at contact point 160. Furthermore, the structural tube 120 may be joined to the central support tube 130 at contact point 170. Additionally or alternatively, the structural tube 120 may be joined to an adjacent structural tube 120 at contact point 150. Thus, contact points 160, 150, and / or 170 can form engagement locations.

[0045] In some embodiments, these joints are formed by laser welding, for example using a carbon monoxide (CO) laser, a carbon dioxide (CO2) laser, or a yttrium-doped laser, such as a yttrium aluminum garnet (YAG) laser. In some embodiments, the laser is a yttrium-doped laser with a wavelength of 1.06 micrometers, or an ND:YAG laser with a wavelength of 0.06 micrometers, delivering a laser beam with pulses having a pulse power of 0.1-2.0 kW. In other embodiments, the laser is an Er:YAG laser with a wavelength of 1.5 to 1.8 micrometers. In other embodiments, the laser is a carbon monoxide laser with a wavelength of 10 micrometers or less, or 8 micrometers or less, or 5 micrometers or less, or 4 micrometers or less, or 2 micrometers or less. Carbon monoxide lasers may be preferred over carbon dioxide lasers because they penetrate deeper into the silica glass, resulting in less surface damage and higher weld strength between different glass components.

[0046] The laser can modify the glass material to the required depth. In some embodiments, the depth is about 0.1 micrometers to about 5 mm, or about 10 micrometers to about 4 mm, or about 50 micrometers to about 3 mm, or about 100 micrometers to about 2 mm, or about 200 micrometers to about 1 mm, or about 200 micrometers to about 800 micrometers.

[0047] The laser can be a pulsed laser, which generates a single laser pulse or a group of pulses of a pulse-line focused laser beam to interact with the glass material. The laser beam is characterized by the creation of a focal line of induced absorption within the glass material, thereby causing material modification within the material. The pulse duration of the laser can be selected such that significant heat transfer (thermal diffusion) does not occur within the material. In some embodiments, the pulse duration is from about 0.1 ps to 100 ps, ​​and preferably less than 15 ps.

[0048] The average diameter δ (spot diameter) of the laser beam focal line is between approximately 0.3 μm and approximately 5.0 μm, or between approximately 1.0 μm and approximately 3.0 μm, or between approximately 0.4 μm and approximately 4.0 μm. The pulse repetition frequency of the laser is between approximately 10 kHz and approximately 1000 kHz (e.g., approximately 100 kHz), and / or because the laser operates as a single-pulse laser or as a group-pulse laser, the energy of each group pulse is between 40 μJ and 1000 μJ, and / or the average laser power measured at the laser beam output side is between approximately 10 watts and approximately 100 watts (e.g., between approximately 30 watts and approximately 50 watts).

[0049] For a more detailed explanation of the laser and the imaging system used to generate such a laser, please refer to U.S. Patent Publication No. US20140199519, the entire contents of which are incorporated herein by reference.

[0050] By using the laser welding process described above to join contact points 150, 160, and / or 170, it is possible, for example, to weld structural tube 120 to central support tube 130. Furthermore, this allows one or more structural tubes 120 to be joined to adjacent structural tubes 120.

[0051] In some embodiments, the formation of the mating sites (formed at contact points 160, 150, and / or 170) can be achieved not only using the laser as described above, but also using an absorption film. For example... Figure 4 As shown, an absorbent membrane 220 is used to bond a first glass material 200 to a second glass material 210. As described above, each of the first glass material 200 and the second glass material 210 can be an outer cladding layer 110, a structural tube 120, and a central support tube 130 to form contact points 150, 160, and 170. In the first example, the first glass material 200 is a structural tube 120, and the second glass material 210 is a central support tube 130. In the second example, the first glass material 200 is a first structural tube 120, and the second glass material 210 is a second structural tube 120. The absorbent membrane 220 is disposed at least at the contact point between the first glass material 200 and the second glass material 210. Figure 4Step A). ​​The laser beam of the laser can have a sufficient wavelength to penetrate the materials of the first glass material 200 and the second glass material 210. However, the laser beam cannot penetrate the material of the absorption film 220; instead, the absorption film 220 absorbs the laser beam at this wavelength. Therefore, the laser beam at this wavelength induces absorption in the absorption film 220. The absorption film 220 is heated by the laser beam to form a bond 225 between the first and second glass materials 200, 210, which are unaffected by the laser beam. Figure 4 Step B). In some embodiments, the wavelength of the laser beam is 1060 nm. Next, the remaining portion of the absorption film 220 is removed, for example by chemical treatment ( Figure 4 Step C). In some embodiments, the absorbent film 220 is removed by a chemical etching step.

[0052] In some embodiments, the absorption film 220 is a metallic material, such as stainless steel, aluminum, copper, titanium, chromium, or other thin metal films, with a melting temperature between about 600°C and about 1300°C, and an absorptivity greater than about 30% at a specified laser wavelength. The thickness of the absorption film 220 may be about 20 nm or greater, or about 40 nm or greater, or about 60 nm or greater, or about 80 nm or greater, or about 100 nm or greater. Alternatively or additionally, the thickness of the absorption film 220 may be about 200 nm or less, or about 180 nm or less, or about 160 nm or less, or about 140 nm or less, or about 120 nm or less, or about 100 nm or less, or about 80 nm or less. In some embodiments, the thickness is about 60 nm to about 120 nm, or about 80 nm to about 100 nm.

[0053] In some other embodiments, a connecting member and a heat source are used to form a mating location (formed at contact points 150, 160, and / or 170). For example... Figure 5 As shown, the connecting member 230 can be disposed on at least one of the first and second glass materials 200 and 210. Figure 5 Step A). ​​Then, a heat source can locally heat the connecting member 230 to form a joint 235 between the first glass material 200 and the second glass material 210. Figure 5(Step B) In some embodiments, the connecting member 230 is one or more layers of silica soot, such as pure silica soot, so heating the connecting member 230 causes the silica soot to sinter and solidify. Therefore, no additional step is needed to remove excess material from the connecting member 230. Instead, the solidified silica soot becomes part of the preform 100. The connecting member 230 may include the same material as the structural tube 120 and / or the cladding 110. In embodiments where the connecting member 230 is solidified in a solidification furnace, the connecting member 230 may be doped with a dopant, such as fluorine (F) or chlorine (Cl), which advantageously reduces the contact angle between the first and second glass materials 200, 210. Reducing the contact angle between the glass materials allows for a smaller connection point between the glass materials, thereby reducing light loss within the drawn optical fiber. Dopants (such as F or Cl) affect the wettability of the glass materials, thereby reducing the contact angle between the glass materials. The heat source can be a laser, a flame, or other heat source known in the art as described above.

[0054] Figure 6A and 6B Other exemplary embodiments of the prefabricated component 100 are shown. For example... Figure 6A As shown, the prefabricated component 100 may include two types of rings for the structured tube 120, such as an outer ring 122 and an inner ring 124. In Figure 6A In this embodiment, the inner diameter and outer diameter of the structural tube 120 with inner ring 124 are larger than those of the structural tube 120 with outer ring 122. Furthermore, in... Figure 6B In some embodiments, the structural tube 120 includes nested tubes. More specifically, the structural tube 120 includes an inner tube 126 (second structural tube) nested within an outer tube 128 (first structural tube). However, this disclosure is not limited to the exemplary arrangement disclosed herein. Other embodiments of the prefabricated component 100 may also be considered.

[0055] Embodiments of this disclosure also include a method of manufacturing the preform 100. Such a method includes joining a central support tube 130 to a plurality of structural tubes 120 such that the plurality of structural tubes 120 are disposed radially outside the central support tube 120. In some embodiments, the joining step includes joining a first central support tube 132 and a second central support tube 134 to the structural tubes 120. As described above, joining can be performed at contact point 170. Furthermore, the plurality of structural tubes 120 can be joined to each other at contact point 150. In some embodiments, the plurality of structural tubes 120 are also joined to an outer cladding 110 at contact point 160. In other embodiments, the plurality of structural tubes 120 are not joined to the outer cladding 110. As described above, the joining at contact points 150, 160, and / or 170 can be provided by welding, such as laser welding, an absorption membrane 220, or a connecting member 230 (e.g., silica soot). The method of manufacturing the preform 100 also includes providing an outer cladding 110 surrounding the central support tube 130 and the structural tubes 120. This step is performed before or after the aforementioned joining step. In some embodiments, the structural tube 120 is first joined to the central support tube 130 before being placed within the outer sheath 110.

[0056] Embodiments of this disclosure also include drawing optical fibers from preform 100. Figure 7 A drawing system 700 for drawing optical fibers according to an embodiment disclosed herein is shown. The exemplary drawing system 700 includes a furnace 705 for heating a preform 100 to its glass melt temperature. The furnace 705 may be disposed in a drawing tower. In some embodiments, the furnace 705 includes a heater such that the preform 100 is consumed and drawn into an optical fiber 720 as it descends toward the heater. Portions of the preform 100 including the central support tube 130 may be removed and discarded so that they are not drawn into the final optical fiber 720. For example, the portion of the preform 100 including the central support tube 130 may be heated to a temperature sufficient to transform these portions of the preform, causing a glass gob to melt and fall from the preform 100 under the influence of gravity. The gob corresponds to the portion of the preform 100 including the central support tube 130. An operator may further peel and remove additional glass from the preform 100 until the portion of the preform 100 including the central support tube 130 is completely removed. In one example, a first end (e.g., first end 112) of the preform 100 includes a central support tube 130, and this first end is heated into a droplet and removed from the preform 100. After the desired portion is removed from the preform 100, the preform 100 can continue to be heated by the furnace 705 and drawn into an optical fiber 720. Therefore, embodiments of this disclosure include removing the central support tube 130 from the preform 100 before drawing the preform 100 into an optical fiber 720.

[0057] In addition, such as Figure 7 As shown, the drawing system 700 includes non-contact measurement sensors 710, 715 for measuring the dimensions (e.g., diameter control) of the drawn (bare) optical fiber 720 exiting the furnace 705. A cooling zone 730 is located downstream of the measurement sensors 710, 715 and is configured to cool the bare optical fiber 720. A coating zone 740 is located downstream of the cooling zone 730 and is configured to deposit a protective coating material 745 onto the bare optical fiber 720 to form a coated optical fiber 725. A tensioning wheel 750 is located downstream of the coating zone 740. The tensioning wheel 750 has a surface 755 that pulls (draws) the coated optical fiber 725. A set of guide wheels 760, each having a corresponding surface 765, is located downstream of the tensioning wheel 750. The guide wheels 760 are used to guide the coated fiber 725 to an optical fiber take-up spool (“spool”) 770 to store the coated optical fiber 725. Embodiments of this disclosure can be used to form anti-resonant hollow optical fibers.

[0058] While various embodiments have been described herein, these embodiments are shown as examples only and not as limitations. It is obvious that, based on the teachings and guidance set forth herein, some modifications and improvements are intended to fall within the meaning and scope of equivalents of the disclosed embodiments. Therefore, it will be apparent to those skilled in the art that various changes in form and detail can be made to the embodiments disclosed herein without departing from the spirit and scope of this disclosure. It should be understood by those skilled in the art that the elements in the embodiments given herein are not necessarily mutually exclusive, but can be interchanged to meet various needs.

[0059] It should be understood that the phrases or terms used herein are for descriptive purposes and not for limitation. The breadth and scope of this disclosure should not be limited to any of the exemplary embodiments described above, but should be defined solely by the appended claims and their equivalents.

Claims

1. An anti-resonance hollow optical fiber preform, comprising: The outer cladding layer has a length, a central longitudinal axis, and a hollow interior; Multiple structural tubes are disposed inside the hollow interior of the outer cladding layer, and the length of each of the multiple structural tubes extends the length of the outer cladding layer; and A central support tube is disposed within the hollow interior of the outer cladding layer, such that the plurality of structural tubes are positioned radially outward from the central support tube. The length of the central support tube extends along the central longitudinal axis of the outer cladding layer, and the length of the central support tube is less than the length of the outer cladding layer. Each of the plurality of structural tubes is connected to the central support tube. The plurality of structural tubes are not joined to the outer cladding.

2. The anti-resonant hollow optical fiber preform of claim 1, wherein, The length of the central support tube is 3 cm or less.

3. The anti-resonant hollow optical fiber preform of claim 2, wherein, The length of the central support tube is 2 cm or less.

4. The anti-resonance hollow optical fiber preform as described in claim 1, wherein, Each of the plurality of structural tubes is welded to the central support tube.

5. The anti-resonance hollow optical fiber preform as described in claim 1, wherein, The plurality of structural tubes are joined to the central support tube by a silica soot layer.

6. The anti-resonance hollow optical fiber preform as described in claim 1, wherein, The central support tube is disposed at the first end of the outer sheath, and the outer sheath also includes a second central support tube disposed at the second end of the outer sheath. The plurality of structural tubes are disposed radially outside the second central support tube, and the length of the second central support tube is less than the length of the outer sheath.

7. The anti-resonance hollow optical fiber preform as described in claim 6, wherein the central support tube does not contact the second central support tube.

8. The anti-resonance hollow optical fiber preform of claim 1, wherein each of the plurality of structural tubes comprises silica glass.

9. The anti-resonance hollow optical fiber preform according to any one of claims 1-8, wherein each of the plurality of structural tubes is a hollow tube.

10. The anti-resonance hollow optical fiber preform as described in claim 9, further comprising a second structural tube disposed within each of the plurality of structural tubes.

11. The anti-resonance hollow optical fiber preform according to any one of claims 1-8, wherein the central support tube is a hollow tube.

12. The anti-resonance hollow optical fiber preform according to any one of claims 1-8, wherein, The outer diameter of the central support tube is larger than the outer diameter of each of the plurality of structural tubes.

13. The anti-resonance hollow optical fiber preform according to any one of claims 1-8, wherein, The outer diameter of the central support tube is smaller than the outer diameter of each of the plurality of structural tubes.

14. The anti-resonance hollow optical fiber preform according to any one of claims 1-8, wherein each structural tube in the structural tube is in contact with the adjacent structural tube.

15. The anti-resonance hollow optical fiber preform according to any one of claims 1-8, wherein the structural tube does not contact adjacent structural tubes.

16. A method for manufacturing an anti-resonance hollow optical fiber preform, the method comprising: The central support tube is joined to multiple structural tubes such that the multiple structural tubes are arranged radially outside the central support tube; and A hollow outer cladding layer is provided around the central support tube and the plurality of structural tubes. In this configuration, each of the plurality of structural tubes extends beyond the length of the outer cladding layer, and the length of the central support tube is less than the length of the outer cladding layer. The plurality of structural tubes are not joined to the outer cladding.

17. The method of claim 16, further comprising using a CO laser to join the central support tube to the plurality of structural tubes.

18. The method of claim 17, wherein the CO laser has a wavelength of 8 micrometers or less.

19. The method of claim 18, wherein the CO laser has a wavelength of 5 micrometers or less.

20. The method of claim 16, further comprising joining the central support tube to the plurality of structural tubes by heating a membrane on the central support tube.

21. The method of claim 16, further comprising bonding the central support tube to the plurality of structural tubes by sintering silica glass frit on the central support tube.

22. The method of any one of claims 16-21, further comprising: At the first end of the structural tube, the central support tube is joined to the plurality of structural tubes; At the second end of the structural tube, a second central support tube is joined to the plurality of structural tubes, such that the structural tube is located radially outside the second central support tube; A hollow outer cladding layer is provided around the second central support tube and the plurality of structural tubes. The length of the second central support tube is less than the length of the outer sheath.

23. The method according to any one of claims 16-21, wherein the central support tube, the plurality of structural tubes, and the outer cladding constitute a prefabricated component. The method further includes removing the central support tube before drawing the preform into an optical fiber.

24. The method of claim 23, wherein, Removing the central support tube includes heating the first end of the preform, the central support tube being disposed at the first end of the preform.

Citation Information

Patent Citations

  • Method and device for the laser-based machining of sheet-like substrates