A tocopherol block polyether and its preparation method and application
By using tocopherol block polyether as surfactant for aqueous organic pigments, the problems of environmental toxicity and poor pigment dispersion of traditional surfactants are solved, and higher pigment dispersion, coloring power and stability are achieved, replacing the traditional alkylphenol polyoxyethylene ether agent.
Patent Information
- Application Number
- CN202410315972.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-20
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-03-20
AI Technical Summary
Existing aqueous organic pigment surfactants such as alkylphenol polyoxyethylene ether are bioaccumulative, carcinogenic and acute toxic in the environment, resulting in their ban or restriction, resulting in poor dispersion and stability of pigments in aqueous inks. Good question.
Tocopherol block polyether is used as a substitute and its structure is prepared through a specific preparation method, which is used for surface modification of pigments and improves the dispersion and stability of pigments in aqueous systems.
Tocopherol block polyether is non-toxic and non-irritating. It can significantly improve the dispersion, coloring and brightness of pigments at an addition amount of 2~5%, while reducing the viscosity of water-based ink and improving storage stability, replacing traditional Surfactants have better environmental protection performance.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of organic pigment additives and fine chemical industry, in particular to a tocopherol block polyether and a preparation method and application thereof. Background Art
[0002] Water-based ink is an important environmentally friendly product in the printing industry. It is of great significance to promote the sustained and stable development of the field of water-based ink. Organic pigments play an important role in the development of water-based ink, but organic pigments have problems such as poor water dispersion. For example, when ordinary azo pigments are used in water-based systems, they have high viscosity and poor storage stability, resulting in unstable quality of printed products. Azo pigments can be surface treated to transform the hydrophobic surface of the pigment into a hydrophilic surface to improve dispersibility in the water-based medium system.
[0003] In addition, alkylphenol polyoxyethylene ether (APEO) surfactants can be added during the synthesis and post-treatment of pigments for surface modification. APEO surfactants have excellent emulsification, wetting and dispersing effects and can improve the application performance of pigments in water-based systems. However, APEO contains alkyl chains and ethoxylated repeating unit chains bonded to phenyl rings, which degrade into alkylphenols (AP) in the environment and ultimately introduce higher toxicity. Therefore, APEO and its metabolite AP are widely considered to be an environmental hormone with certain bioaccumulation, carcinogenicity, acute toxicity, aquatic toxicity, etc., and have gradually been banned or restricted around the world.
[0004] Therefore, the development of environmentally friendly water-based organic pigment surface-modified dispersants is of great significance to improving the application performance of organic pigments in water-based systems. Summary of the invention
[0005] In order to solve the problem of poor environmental performance of dispersants for surface modification of water-based organic pigments, the present invention aims to provide a tocopherol block polyether and a preparation method and application thereof, which can replace alkylphenol polyoxyethylene ether surfactants.
[0006] In order to achieve the above object, the present invention is implemented through the following technical solutions:
[0007] A tocopherol block polyether, the structural formula of which is shown in Formula I:
[0008]
[0009] The present invention also includes a method for preparing the tocopherol block polyether, comprising the following steps:
[0010] Add tocopherol and the first catalyst to a reactor, heat to 80-85°C, dehydrate under negative pressure and heat to 100-105°C, replace with nitrogen three times, start adding propylene oxide, control the temperature at 130-145°C, and the pressure does not exceed 0.3MPa. After the propylene oxide feeding is completed, continue to react for 50-70 minutes; cool to 100-110°C, vacuum dehydrate for 30-40 minutes, cool to 80°C, add the second catalyst, heat to 110-115°C, dehydrate under negative pressure for 30-40 minutes, replace with nitrogen three times, start adding ethylene oxide, control the temperature at 110-125°C, continue to react for 30-40 minutes after the ethylene oxide feeding is completed, cool to 90-100°C, vacuum treat for 30-40 minutes, and then cool to below 80°C, add glacial acetic acid to adjust the pH to 6-8, stir for half an hour, and cool to 20-30°C to obtain a tocopherol block polyether;
[0011] The first catalyst and the second catalyst are inorganic strong bases;
[0012] The mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:1.5-3:260-410:1.5-3:610-820.
[0013] The reaction equation is as follows:
[0014]
[0015] Where m=20~30, n=60~80.
[0016] Preferably, the first catalyst and the second catalyst are sodium hydroxide or potassium hydroxide.
[0017] Preferably, the mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:2-2.5:300-350:2-3:650-700.
[0018] Preferably, the reaction temperature after adding propylene oxide is 135-140°C.
[0019] Preferably, the reaction temperature after adding ethylene oxide is 115-120°C.
[0020] The present invention also includes the use of tocopherol block polyether in surface modification during the synthesis of organic pigments.
[0021] Preferably, the amount added to the organic pigment is 2-5% of the pigment mass.
[0022] Compared with the prior art, the present invention has the following advantages:
[0023] The tocopherol block polyether structure of the present invention contains propoxy and ethoxy structures. During the preparation process, the molar ratio of propylene oxide to ethylene oxide is controlled to be about 20-30:60-80 to obtain the tocopherol block polyether. The tocopherol block polyether of this structure has a strong adsorption effect on the surface of the pigment, so that the pigment has good dispersibility in the aqueous system.
[0024] The tocopherol block polyether of the present invention can completely replace alkylphenol polyoxyethylene ether and is non-toxic, non-irritating and safe. The addition amount of the tocopherol block polyether in the pigment is only 2-5%, which can improve the pigment dispersibility and the coloring power and brightness of the pigment. DETAILED DESCRIPTION
[0025] The purpose of the present invention is to provide a tocopherol block polyether and a preparation method and application thereof. The present invention is further described below in conjunction with specific embodiments.
[0026] Example 1 A method for preparing a tocopherol block polyether comprises the following steps:
[0027] 1 kg of tocopherol and 15 g of sodium hydroxide were added to a reactor, the temperature was raised to 80° C., the temperature was raised to 100° C. by negative pressure dehydration, and after nitrogen replacement for three times, 2.6 kg of propylene oxide was added, the temperature was controlled at 130° C., the pressure did not exceed 0.3 MPa, and the reaction was continued for 70 minutes after the propylene oxide feeding was completed; the temperature was lowered to 100° C., vacuum dehydration was performed for 30 minutes, the temperature was lowered to 80° C., 15 g of sodium hydroxide was added, the temperature was raised to 110° C., the temperature was raised to negative pressure dehydration for 40 minutes, nitrogen replacement was performed for three times, 6.1 kg of ethylene oxide was added, the temperature was controlled at 110° C., the reaction was continued for 40 minutes after the ethylene oxide feeding was completed, the temperature was lowered to 90° C., the temperature was lowered to below 80° C. after vacuum treatment for 30 minutes, glacial acetic acid was added to adjust the pH to 6, stirred for half an hour, and the temperature was lowered to 20° C. to obtain a tocopherol block polyether;
[0028] The mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:1.5:260:1.5:610.
[0029] Example 2 A method for preparing a tocopherol block polyether comprises the following steps:
[0030] 1 kg of tocopherol and 30 g of potassium hydroxide were added to a reactor, the temperature was raised to 85°C, the temperature was raised to 105°C by negative pressure dehydration, and after nitrogen replacement for three times, 4.1 kg of propylene oxide was added, the temperature was controlled at 145°C, the pressure did not exceed 0.3 MPa, and the reaction was continued for 50 minutes after the propylene oxide feeding was completed; the temperature was lowered to 110°C, vacuum dehydration was performed for 40 minutes, the temperature was lowered to 80°C, 30 g of potassium hydroxide was added, the temperature was raised to 115°C, negative pressure dehydration was performed for 40 minutes, nitrogen replacement was performed for three times, 8.2 kg of ethylene oxide was added, the temperature was controlled at 125°C, the reaction was continued for 30 minutes after the ethylene oxide feeding was completed, the temperature was lowered to 100°C, the temperature was lowered to below 80°C after vacuum treatment for 40 minutes, glacial acetic acid was added to adjust the pH to 8, the mixture was stirred for half an hour, and the temperature was lowered to 20-30°C to obtain a tocopherol block polyether;
[0031] The mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:3:410:3:820.
[0032] Example 3 A method for preparing a tocopherol block polyether comprises the following steps:
[0033] 1 kg of tocopherol and 20 g of sodium hydroxide were added to a reactor, the temperature was raised to 82 ° C, the temperature was raised to 102 ° C under negative pressure dehydration, and after nitrogen replacement three times, 3 kg of propylene oxide was added, the temperature was controlled at 135 ° C, the pressure did not exceed 0.3 MPa, and the reaction was continued for 55 minutes after the propylene oxide was added; the temperature was lowered to 105 ° C, vacuum dehydration was performed for 32 minutes, the temperature was lowered to 80 ° C, 20 g of potassium hydroxide was added, the temperature was raised to 112 ° C, the temperature was raised to 32 minutes under negative pressure dehydration, and after nitrogen replacement three times, 6.5 kg of ethylene oxide was added, the temperature was controlled at 115 ° C, the reaction was continued for 32 minutes after the ethylene oxide was added, the temperature was lowered to 95 ° C, the temperature was lowered to below 80 ° C after vacuum treatment for 32 minutes, glacial acetic acid was added to adjust the pH to 6.5, stirred for half an hour, and cooled to 22 ° C to obtain a tocopherol block polyether;
[0034] The mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:2:300:2:650.
[0035] Example 4 A method for preparing a tocopherol block polyether comprises the following steps:
[0036] 1 kg of tocopherol and 25 g of potassium hydroxide were added to a reactor, the temperature was raised to 84 ° C, the temperature was raised to 102 ° C under negative pressure dehydration, and after nitrogen replacement three times, 3.5 kg of propylene oxide was added, the temperature was controlled at 140 ° C, the pressure did not exceed 0.3 MPa, and the reaction was continued for 60 minutes after the propylene oxide feeding was completed; the temperature was lowered to 102 ° C, vacuum dehydration was performed for 32 minutes, the temperature was lowered to 80 ° C, 30 g of sodium hydroxide was added, the temperature was raised to 112 ° C, the temperature was lowered to 32 minutes under negative pressure, and after nitrogen replacement three times, 7 kg of ethylene oxide was added, the temperature was controlled at 120 ° C, and the reaction was continued for 35 minutes after the ethylene oxide feeding was completed, the temperature was lowered to 98 ° C, and the temperature was lowered to below 80 ° C after vacuum treatment for 38 minutes, glacial acetic acid was added to adjust the pH to 7.5, stirred for half an hour, and cooled to 25 ° C to obtain a tocopherol block polyether;
[0037] The mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:2.5:350:3:700.
[0038] Example 5 A method for preparing a tocopherol block polyether comprises the following steps:
[0039] 1 kg of tocopherol and 22 g of potassium hydroxide were added to a reactor, the temperature was raised to 82 ° C, the temperature was raised to 104 ° C under negative pressure dehydration, and after nitrogen replacement three times, 3.2 kg of propylene oxide was added, the temperature was controlled at 138 ° C, the pressure did not exceed 0.3 MPa, and the reaction was continued for 65 minutes after the propylene oxide feeding was completed; the temperature was lowered to 105 ° C, vacuum dehydration was performed for 35 minutes, the temperature was lowered to 80 ° C, 25 g of potassium hydroxide was added, the temperature was raised to 114 ° C, the temperature was raised to 35 minutes under negative pressure dehydration, and after nitrogen replacement three times, 6.8 kg of ethylene oxide was added, the temperature was controlled at 118 ° C, and the reaction was continued for 38 minutes after the ethylene oxide feeding was completed, the temperature was lowered to 95 ° C, and the temperature was lowered to below 80 ° C after vacuum treatment for 35 minutes, glacial acetic acid was added to adjust the pH to 7.0, stirred for half an hour, and cooled to 28 ° C to obtain a tocopherol block polyether;
[0040] The mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:2.2:320:2.5:680.
[0041] Example-6 Application of the obtained tocopherol block polyether
[0042] The tocopherol block polyether or OP-10 obtained in Example 1 was used in the preparation of Pigment Yellow 83 to modify Pigment Yellow 83 as follows:
[0043] Preparation of Pigment Yellow 83
[0044] ① Preparation of diazo solution: add 100ml of water, 16g of hydrochloric acid and 10g of DCB to a 500ml beaker, beat for 30 minutes, add ice to cool to 0-3℃; quickly add 5.8g of sodium nitrite solution, stir for 60 minutes, add aminosulfonic acid to remove excess sodium nitrite, adjust KI test paper to slightly blue, adjust V=300ml, T=0℃ for coupling;
[0045] ② Preparation of coupling solution: Add 200ml of water, 3.75g of sodium hydroxide, and 22.5g of AS-IRG to a 500ml beaker, stir to dissolve and clarify, adjust the temperature to T=15℃, V=320ml, and wait for acid precipitation;
[0046] ③ Preparation of acid precipitation solution: Add 200ml water, 6.5g glacial acetic acid and 7.1g anhydrous sodium acetate into a 3000ml beaker, stir and dissolve, adjust T=18℃, V=300ml;
[0047] ④ Acid precipitation: Add the coupling liquid to the acid precipitation liquid within 30-40 minutes, the end point T = within 20 ° C, pH = 5.6-6.0, stir for 15 minutes, add 1.6g of dispersant A aqueous solution, stir for 15 minutes, and set aside;
[0048] ⑤ Coupling and post-treatment: add the diazo solution dropwise into the coupling component, temperature T = 16-20 ° C time t = 140-150 minutes, use NaOH solution to control pH = 4.5-5.0 during the coupling process, after 100 minutes of coupling, heat to 35 ° C, slow down the coupling speed, measure the excess of diazonium salt several times to ensure that it is not excessive, after the coupling is completed, T = 35-40 ° C, pH = 4.3-4.5, diazonium salt is not excessive, stir for 30 minutes; heat to above T = 95 ° C, complete the color change, keep warm for 30 minutes, cool to below 65 ° C, filter and rinse until the conductivity is within 100, and dry at 90 ° C.
[0049] When the dispersant A is the tocopherol block polyether prepared in Example 1, it is Example 6, and when the dispersant A is OP-10, it is Comparative Example 1.
[0050] Example 7 Application of the Tocopherol Block Polyether Obtained
[0051] The tocopherol block polyether obtained in Example 2 or Peregal OS-15 was used in the preparation process of Pigment Yellow 14 to modify Pigment Yellow 14 as follows:
[0052] Preparation of Pigment Yellow 14
[0053] ① Preparation of diazo solution: add 150ml water, 16.6g hydrochloric acid and 10g DCB to a 500ml beaker, beat for 30 minutes, add ice to cool to 0℃, add 5.8g sodium nitrite solution, stir for 60 minutes; add aminosulfonic acid to remove excess sodium nitrite, adjust KI test paper to slightly blue, adjust V=350ml, T=0℃ for coupling;
[0054] ② Preparation of coupling liquid: Add 200ml of water to a 2L beaker, add 13.4g of 30% liquid caustic soda and 15.6g of o-methylbis(ethyl)acetate, stir to dissolve, add 8.0g of acetic acid for acid precipitation, and the acid precipitation is completed in 15 minutes, pH = 5.6-6.0, temperature 15℃, add 0.52g of dispersant B in water solution and stir for 15 minutes;
[0055] ③ Coupling and post-treatment: add diazo solution to the coupling solution within 80-90 minutes, during which the pH is controlled at 4.5-5.0 with alkaline solution to prevent excessive diazo component; after coupling, stir for 30 minutes, heat to 80°C, add 0.3g aluminum sulfate solution, pH = 5.0, continue to heat to 90°C and keep warm for 30 minutes, cool to below 65°C, filter, and dry at 80°C.
[0056] When the dispersant B is the tocopherol block polyether prepared in Example 1, it is Example 7, and when the dispersant B is Peregal OS-15, it is Comparative Example 2.
[0057] Application of the Tocopherol Block Polyether Obtained in Examples 8 to 10
[0058] The tocopherol block polyether or OP-7 obtained in Examples 3 to 5 was used in the preparation process of Pigment Red 57:1 to modify Pigment Red 57:1 as follows:
[0059] Preparation of Pigment Red 57:1
[0060] ① Preparation of diazo solution: add 150ml water, 2.4g sodium hydroxide, 11.22g 4B acid into a 500ml beaker, dissolve clearly at room temperature, add 4.4g sodium nitrite to make a solution, add ice to cool to 0-3℃, quickly add 19.4g hydrochloric acid, T=2℃, V=400ml, stir for 30min, and set aside;
[0061] ② Preparation of coupling liquid: Add 150ml of water, 6.0g of sodium hydroxide, and 15.6g of 2,3-acid to a 2000ml beaker, dissolve clearly, add the clear rosin solution (obtained by heating and dissolving 1.0g of rosin, 0.3g of sodium hydroxide and water), adjust T=11℃, V=400ml;
[0062] ③ Coupling: Add the diazo solution to the coupling solution within 15 minutes, the reaction temperature is 11-14°C, the end point temperature is 13-14°C, and the end point pH is 6.5-7.0;
[0063] ④ Post-treatment: adjust the pH to 12 with 20% sodium hydroxide solution, T=14℃; stir for 15min, add 0.8g dispersant C, pH=11.8, T=18℃; after 30min, add 23g calcium chloride solution, test pH=10.2, adjust pH=11.8 with 20% sodium hydroxide solution, T=19℃; after 15min, heat to 75℃, add 10g strontium chloride and 2.3g magnesium chloride, continue to heat to 95℃, keep warm for half an hour; cool to 75℃, adjust pH=6.0-6.5 with aluminum sulfate solution, stir for 15min; wash with water, filter; dry at 85℃.
[0064] When the dispersant C is the tocopherol block polyether prepared in Examples 3 to 5, they are Examples 8 to 10 respectively, and when the dispersant C is OP-7, it is Comparative Example 3.
[0065] The pigments prepared in Examples 6 to 10 and the pigments prepared in Comparative Examples 1 to 3 were prepared into water-based inks for testing. The composition of the water-based ink is as follows: by weight, 15 parts of pigment, 8.3 parts of acrylic resin, 1.2 parts of isopropyl alcohol, 13.5 parts of water, and 60 parts of 2-3 mm glass beads. During the preparation, the above mixture was dispersed for 60 minutes using an oscillator to obtain a water-based ink, and then the water-based ink: white Nippon paint was blended at a ratio of 1:19 to obtain a diluted color, and the tinting strength of the diluted color was tested.
[0066] The water-based ink was scraped on the coated paper with a No. 6 wire rod, and the diluted color was scraped on the coated paper with a No. 10 wire rod. After the ink layer was dried, the color and tinting strength were tested with an X-Rite colorimeter, and the glossiness was tested with a JFL-BZ60° gloss meter. The water-based ink prepared with the pigment of Example 6 was used as the standard, the water-based ink prepared with the pigment of Example 7 was used as the standard, and the water-based ink prepared with the pigment of Example 2 was used as the standard. The water-based ink prepared with the pigment of Examples 8 to 10 was used as the standard for the water-based ink prepared with the pigment of Comparative Example 3. The color measurement data of the water-based ink are shown in Table 1.
[0067] Table 1 Color shade, tinting strength and glossiness of water-based printing inks prepared with pigments
[0068]
[0069] It can be seen from the results in Table 1 that Example 6 is slightly darker in color (ΔL<0), the red light is slightly stronger (Δh<0), the vividness is improved (ΔC>0), and the color strength is improved by 5.7% compared with Comparative Example 1; Example 7 is slightly darker in color (ΔL<0), the red light is slightly stronger (Δh<0), the vividness is significantly improved (ΔC>0), and the color strength is improved by 10.7% compared with Comparative Example 2; Examples 8 to 10 are slightly darker in color (ΔL<0), the blue light is slightly stronger (Δh<0), the vividness is improved (ΔC>0), and the color strength is improved by 6.0%, 7.2% and 7.8%, respectively, compared with Comparative Example 3; the aqueous ink prepared by using the tocopherol block polyether of the present invention as a dispersant has higher gloss than the existing dispersant.
[0070] The viscosity of the water-based ink was tested with a Brookfield DV-III viscometer (25°C), then sealed, placed in a 55°C oven for 7 days, taken out, cooled to 25°C, and then tested with a Brookfield DV-II viscometer. The test results are shown in Table 2.
[0071] Table 2 Initial viscosity of water-based ink and viscosity after standing
[0072]
[0073] It can be seen from the results in Table 2 that the aqueous ink prepared by using the tocopherol block polyether of the present invention as a dispersant to modify the pigment can significantly reduce the viscosity of the aqueous ink compared with the existing dispersant, and the viscosity is even lower after being placed. The aqueous ink has a lower viscosity and better storage stability.
[0074] The particle size and wetting angle of the pigment powder obtained in Examples 6 to 10 were tested, wherein the detection process of the pigment powder particle size was as follows: 0.1 g of the obtained pigment was fully wetted with 1 ml of surfactant AEO-6 solution (concentration 30%), and then water was added to 25-30 ml for ultrasonic dispersion for 5 min, and then 800 ml of water was added for ultrasonic dispersion for 2 min, and the particle size distribution curve was obtained by analysis and detection by Malvern laser particle size analyzer. The wetting angle detection process of the pigment powder was as follows: 0.5 g of powdered pigment was first weighed, and it was placed in a tableting mold and tableted for 30 seconds, and then placed in an EasyDrop contact angle measuring instrument manufactured by KRUSS, Germany, for measurement. The contact angle of the sample was tested at room temperature with water as the medium. The test results are shown in Table 3.
[0075] Table 3 Contact angle and particle size of pigments
[0076]
[0077] It can be seen from the results in Table 3 that the modified pigment prepared by using the tocopherol block polyether of the present invention as a dispersant has a significantly smaller particle size than the pigment prepared by the existing dispersant, the particle size distribution is more concentrated, and the pigment contact angle is reduced, indicating that the hydrophilicity of the pigment is improved and the dispersion performance of the pigment in the aqueous medium is better.
Claims
1. An application of tocopherol block polyether for surface modification in the synthesis process of organic pigments, characterized in that: The structural formula of tocopherol block polyether is shown in Formula I: Formula I; In formula (I), m=20-30, n=60-80; The raw materials for preparing the tocopherol block polyether include tocopherol, propylene oxide and ethylene oxide, wherein the mass ratio of tocopherol:propylene oxide:ethylene oxide is 100:300-350:650-700.
2. The application of the tocopherol block polyether according to claim 1 for surface modification in the synthesis process of organic pigments, characterized in that: The amount added to organic pigments is 2~5% of the pigment mass.
3. The application of the tocopherol block polyether according to claim 1 for surface modification in the synthesis process of organic pigments, characterized in that: The preparation method of the tocopherol block polyether comprises the following steps: Add tocopherol and the first catalyst into the reactor, raise the temperature to 80-85°C, dehydrate under negative pressure and raise the temperature to 100-105°C, replace with nitrogen three times, start adding propylene oxide, control the temperature at 130-145°C, and keep the pressure below 0.3MPa. After the addition of propylene oxide, continue the reaction for 50-70 minutes; Cooling to 100-110°C, vacuum dehydration for 30-40 minutes, cooling to 80°C, adding the second catalyst, heating to 110-115°C, vacuum dehydration for 30-40 minutes, nitrogen replacement three times, starting to add ethylene oxide, controlling the temperature at 110-125°C, continuing the reaction for 30-40 minutes after the ethylene oxide feeding is completed, cooling to 90-100°C, vacuum treatment for 30-40 minutes, cooling to below 80°C, adding glacial acetic acid to adjust the pH to 6-8, stirring for half an hour, cooling to 20-30°C, and obtaining a tocopherol block polyether; The first catalyst and the second catalyst are inorganic strong bases; The mass ratio of the tocopherol, the first catalyst, propylene oxide, the second catalyst and ethylene oxide is 100:2-2.5:300-350:2-3:650-700.
4. The use of the tocopherol block polyether according to claim 3 for surface modification in the synthesis process of organic pigments, characterized in that: The first catalyst and the second catalyst are sodium hydroxide or potassium hydroxide.
5. The use of the tocopherol block polyether according to claim 3 for surface modification in the synthesis process of organic pigments, characterized in that: The reaction temperature after adding propylene oxide is 135~140℃.