Tool for winding fiber fabric and related winding method
By adjusting the end area distance along the second axis on the fiber fabric winding tool and using different compaction equipment for compaction in different configurations, the problem of overlength and wrinkles caused by compaction during the winding process is solved and the fiber is achieved. Increased volume content and improved mechanical strength.
Patent Information
- Application Number
- CN202280066416.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-25
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-08-25
AI Technical Summary
During the winding process of fiber fabrics, excessive length caused by compaction leads to wrinkle defects, which reduces the mechanical strength of composite parts, and it is difficult to effectively reduce or eliminate such defects with existing technology.
A tool was designed to adjust the circumference of the rolled layers by gradually pulling or pulling the end region along a second axis on the support, and to change the shape of the support between retracted and extended configurations, using The first and second compaction devices perform compaction in the end area and center area respectively to reduce wrinkles.
It can effectively reduce or even eliminate wrinkle defects in fiber fabrics after compaction, ensure that the fiber volume content reaches the required value, and improve the mechanical strength and shape accuracy of composite parts.
Smart Images

Figure CN118043184B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a tool for winding fiber fabrics, in particular fiber fabrics produced by three-dimensional weaving, to obtain fiber preforms of composite material parts, and also to a related winding method. The present invention is suitable for manufacturing parts that can be used in different fields and different shapes, in particular for manufacturing aircraft parts, such as landing gear or gas turbine parts. Background Art
[0002] It is known to manufacture composite parts by winding a fiber fabric on a support and subsequently inserting a matrix material into the pores of the fabric. When leaving the weaving loom, the fiber fabric is "expanded", that is, it has a significant free volume of voids that are not occupied by fibers. Typically, the fiber volume content of the expanded fiber fabric is lower than the desired fiber volume content in the final part. Therefore, the wound fabric is compacted to reduce the thickness of each layer, thereby increasing the fiber volume content to the desired value. However, compaction can cause the fabric to be too long, which can cause wrinkles (also called local buckling defects) in the fabric when it is molded in the injection mold, which may reduce the mechanical strength of the component in operation. Figure 1 and Figure 2 A graphic representation of the excess length produced during compaction is given in FIG. Figure 1 The case of a wound fabric 1 having a partially circular geometry is shown. In this configuration, when compacting as indicated by the arrow C, the layers 3a-3n wound on the support F receive an overlength that increases the more the layers are placed towards the outside of the winding. This difference can be explained by the increase in the circumference of the layers as the winding progresses and as the winding is carried out. Therefore, the overlength Sn generated for the outermost layer 3n is the greatest. Figure 2 The generation of an overlength in a wound preform 1 having a partially rectilinear shape is shown. On this rectilinear portion, each wound layer 3a-3n receives the same overlength during compaction C, so that it changes from a length L1 to a length L2 greater than L1. Known documents CN 113 043 621 disclose a method for forming an annular reinforcement, and CN 113 021 939 discloses a method for forming a component based on continuous fibers and conventional fibers.
[0003] It is desirable to provide a tool for winding a fiber fabric and a related method which allow reducing or even eliminating wrinkle defects in the compacted fabric, the compacted fibers intended to form the fiber reinforcement of the part to be obtained. Summary of the invention
[0004] The invention relates to a tool for winding a fiber fabric, the tool comprising at least one support on which the fiber fabric is intended to be wound about a first winding axis, the support having at least two end regions which are spaced apart along a second axis transverse to the first axis,
[0005] It is characterized in that the tool includes a moving device, which is configured to change the shape of the support between a retracted structure and an extended structure by gradually pulling the end areas closer or farther along a second axis, and the tool includes a first compacting device and a second compacting device, the first compacting device being capable of performing compaction on the end areas at least in the retracted structure, and the second compacting device being different from the first compacting device and being capable of performing compaction on a central area located between the end areas in the extended structure.
[0006] The invention proposes a tool to allow the end zones to be pulled towards each other as the winding progresses, i.e., at each turn of the fiber fabric or at a portion of a turn of the fiber fabric, in order to adjust the circumference of each wound layer to a predetermined value, thereby allowing to offset the differences in excess lengths of the different layers during compaction by the first compaction device. Thus, at each additional turn or at a portion of a turn, the fabric is wound by reducing the distance between the end zones to take into account the increase in excess lengths caused by compaction, and this reduction continues until the layer becomes the outermost layer of the winding (see Figure 1 ), until the last turn, when a minimum distance corresponding to the so-called "retracted" configuration of the support is reached. After compaction by a first compacting device in the retracted configuration, the distance between the end regions increases until entering the so-called "extended" configuration, in which the wound layer is tightened to remove wrinkles, optionally in the local compacted areas, the distance between the end regions substantially corresponding to the final dimensions of the component to be obtained. Compacting is then continued in the central area with a second compacting device to form a fabric in this area. Thus, after compaction, a component preform is obtained having the desired fiber volume capacity and in which the wrinkle defects of the fabric are greatly reduced or even completely eliminated. The invention is suitable for the manufacture of fiber reinforcements that define an internal volume and form a closed contour, advantageously made of a fiber fabric obtained by three-dimensional weaving. As described below, the invention concerns different geometries of the component, such as components alternating between elongated areas extending essentially in a straight line and curved or fully circular areas, or components having a circular or elliptical geometry.
[0007] In one example of an embodiment, each end region includes a distal end and two side portions located on each side of the distal end and on one side of the central region, and wherein the first compaction device includes a first compaction element and a second compaction element, the first compaction element being capable of performing compaction on the distal end of each end region, and the second compaction element being capable of performing compaction on the side portion of each end region, with a compaction component toward the central region.
[0008] Application of a compaction component toward the central region advantageously repels excess elongation created during compaction of the end regions toward the central region, thereby further neutralizing wrinkles when transitioning to an extended configuration.
[0009] In particular, the second compacting element may have at least one lateral surface which forms a non-zero angle with a normal of the support at this surface.
[0010] Said properties advantageously assist in repelling excess length created upon compaction of the end regions toward the central region, thereby further neutralizing wrinkles upon transition to the expanded configuration.
[0011] The first compacting device may be configured to perform compaction by the second compacting element after performing compaction by the first compacting element.
[0012] Compaction is performed on the end regions in a sequential manner, first on the distal end and then on the sides, to further promote rejection of excess length towards the central region.
[0013] In one example of embodiment, the end region defines a circular winding surface.
[0014] The present invention also relates to a method for manufacturing a fiber preform using the above tool, comprising at least:
[0015] - winding the fiber fabric around the first winding axis on the support by gradually reducing the distance between the end regions along the second axis to a predetermined value during winding until the support is transferred into the retracted configuration;
[0016] - a first compaction of the winding at the end region by means of a first compaction device with the support in the retracted configuration;
[0017] - after said first compaction, tightening the windings in the central zone by increasing the distance between the end zones along the second axis so as to transform the support from the retracted configuration to the extended configuration; and
[0018] - With the support in the extended configuration, a second compaction of the winding takes place in the central region by means of a second compacting device.
[0019] In one example of embodiment, the first compaction comprises compaction performed by a first compaction element on a distal end of the winding, followed by compaction performed by a second compaction element on a side of the end region, with a compaction component directed towards the central region.
[0020] In one embodiment, the fiber fabric is obtained by three-dimensional weaving.
[0021] In one embodiment, the fiber fabric has a region of decreasing thickness near each end thereof.
[0022] Said characteristics advantageously prevent sudden local variations in the fiber volume content at the start and end winding points.
[0023] The present invention also relates to a method for manufacturing a composite material component, comprising at least:
[0024] - manufacturing a fiber preform by implementing the above method; and
[0025] - Formation of a matrix in the pores of the fiber preform just produced in order to obtain a composite component.
[0026] The matrix can generally be formed by introducing a matrix material into the pores of the fiber preform and then curing the matrix material. A resin can be injected into the pores of the fiber preform and the resin can be crosslinked to obtain the matrix. The component formed can be a composite material with an organic matrix or, as a variant, a composite material with a ceramic matrix. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] [ Figure 1 ] Figure 1 The excess length that occurs when compacting a winding of a fiber fabric layer having a partially circular shape is schematically shown.
[0028] [ Figure 2 ] Figure 2 The excess length that occurs when compacting a winding of a fiber fabric layer having a partially rectilinear shape is schematically shown.
[0029] [ Figure 3 ] Figure 3 The first winding turn of a fiber fabric in one example of the present invention is schematically shown.
[0030] [ Figure 4 ] Figure 4 The fiber fabric is schematically shown at the completion of winding in an example of the present invention, wherein the center distance of the tool is in a retracted configuration.
[0031] [ Figure 5 ] Figure 5 The compaction of a wound fiber fabric on the end region of a support by a first compacting device in an example of the invention is schematically shown, wherein the center distance of the tools is in a retracted configuration.
[0032] [ Figure 6 ] Figure 6 In an example of the invention, the transition to the extended configuration and the compaction in this configuration by the second compacting device are shown.
[0033] [ Figure 7 ] Figure 7 Details of variants of fiber fabrics that can be used for the invention are schematically shown.
[0034] [ Figure 8 ] Figure 8 The transition to the retracted configuration according to a variant of the invention is schematically shown.
[0035] [ Fig. 9 ] Fig. 9 A variant of a tool according to the invention is schematically shown, which is suitable for producing a casing for a gas turbine engine. DETAILED DESCRIPTION
[0036] Figures 3 to 6 An example of the invention is shown which is intended to produce a component with an elongated geometry, such as a landing gear strut or a brake rod. Fig. 9 As mentioned above, the present invention is still applicable to other types of components.
[0037] The following paragraphs explain in detail the determination of the length of fabric to be wound per turn or part of a turn, depending on the component under consideration.
[0038] Initially, the dimensions of the component to be obtained are known (after compaction), ie in particular its length and thickness, and also the desired fiber volume content.
[0039] The initial thickness of the fabric is also known (before compaction), i.e., "expanded" as described above, with the fiber volume content typically being less than that required for the part. Taking into account the expansion of the fabric, the number of fabric winding turns to be performed corresponds to the number of turns required to obtain the desired thickness and fiber volume content in the final part.
[0040] A geometric calculation of each layer of the winding shows the excess length in the central region produced when the end regions are compacted. Figure 1 As shown, these excesses vary with the position of the wound layer within the total thickness. From this, the length to be chosen for the winding of each layer of fabric is then deduced, and the distance separating the end zones is chosen for each turn or part of a turn, so as to obtain the desired length of the final part after the excesses are created when the end zones are compacted, without causing any wrinkles in the fabric.
[0041] In a preliminary step of winding, a fiber fabric 12 is first obtained by a technique known per se. The fiber fabric 12 may be formed by three-dimensional weaving which obtains the properties of the fabric remaining constant over the entire dimensions of the fabric 12 or which causes a change in at least one of the weaving, the warp / weft ratio or the material used for the woven yarns, depending on the envisaged application.
[0042] use Figure 3The tool 10 in the illustrated configuration begins to wind the fabric 12. The tool 10 generally comprises a support 14 around which the fabric 12 is intended to be wound. The winding is performed around a first winding axis X1 perpendicular to the plane of the drawing. The support 14 defines end regions 16 and 18, which are here two and spaced apart along a second axis X2 transverse to (e.g., perpendicular to) the first axis X1. The end regions 16, 18 each comprise a distal end 16a, 18a and a side portion 16b, 18b located on the side of the central region 17, where the distal ends 16a, 18a form the "nose" of these regions 16, 18, the distal ends 16a, 18a being contained between the two side portions 16b, 18b. The end regions 16, 18 define loops or corners around which the orientation of the fabric 12 changes, and in the illustrated example, the fabric makes a U-turn around each end region 16, 18 during winding. The end regions 16, 18 may be of convex shape as shown. In the example shown, the cross-sections of the end regions 16, 18 relative to the first axis X1 form a circular shape, for example substantially circular, and have different sizes. An example of a support having two end regions 16, 18 is shown, but it is within the scope of the invention if the support has more than two end regions defining the corners around which the fabric is to be wound. In the example shown, when the fabric 12 is wound, the central region 17 does not have any part of the wound fabric supported thereon, but if this is the case as described below, it will be within the scope of the invention.
[0043] The first turn is wound, resulting in the first layer C1 of the fiber fabric 12 being wound around the support 14, setting the distance between the end regions 16, 18 to an initial value D1 ( Figure 3 ). The distance between the end regions 16, 18 may correspond to the distance between the distal ends 16a and 18a measured along the second axis X2 as shown. Initially, one end of the fabric is attached to the support 14, for example at a point in the central region 17, by means of an attachment device (not shown) of the preform, such as a clamping device. This attachment can be obtained by various methods, for example using an adhesive tape or by clamping. Position indicators may also be provided for the support and the fabric, for example by providing the fabric with an identification element intended to be placed above a predetermined position on the support 14 to confirm that the winding of the fabric 12 has been correctly carried out. As a variant or combination, the fabric 12 may be provided with a mechanical element intended to cooperate with a mechanical element provided on the support 14 to confirm the proper positioning of the fabric 12, such as a system of hooks and loops. The first turn of the first layer C1 of the winding is performed by tensioning the fabric 12 to prevent wrinkles, such as Figure 3Once the first turn is completed, the first layer C1 can be temporarily held in place, for example, at the end regions 16, 18, or even at the distal ends 16a, 18a. This temporary holding in place can be done using any suitable device, for example by clamping, optionally with the aid of a compacting element 22 (in combination with the following Figure 5 Description) obtained.
[0044] The tool 10 comprises a movement device (not shown) capable of changing the shape of the support during winding. Once the first winding turn is completed, the movement device pulls the end zones towards each other along the second axis X2 and sets the distance between these zones 16, 18 to a predetermined value resulting from the above-mentioned geometric model, so that the winding of the second layer of fabric 12 can be carried out in a similar manner to the winding of the first layer C1, and thereafter, at each winding turn, the zones 16, 18 are brought closer together until reaching a distance of 1.50° after the last layer Cn of fabric 12 is wound. Figure 4 The configuration shown ends. This configuration corresponds to a retracted configuration of the support in which the distance between the end regions 16, 18 is a minimum of the value D2. In the example considered, the bringing together of the regions 16, 18 is performed at each turn, but it remains within the scope of the invention if such a bringing together is performed at each part of a turn, for example at each U-turn. The movement device is configured to allow an incremental reduction of the distance between the end regions 16, 18 and includes a position locking mechanism that allows the desired distance between the end regions 16, 18 to be set for the turn considered. A person skilled in the art will be able to determine that various movement systems are suitable, using movement systems such as screws or jacks. Figure 4 It can be noted that before compaction, the last layer Cn of the winding may not show any significant wrinkling, however, due to the gradual reduction in the distance between the end regions 16, 18 as and when the winding progresses, once the winding is completed, the lower layers do show wrinkling (see wrinkle P1 of layer C1 and wrinkle Pn-1 of the penultimate layer Cn-1). This wrinkling becomes more pronounced the closer the layers in the winding are to the innermost layers.
[0045] Once the winding is completed, the support is in Figure 4 in the retracted configuration and begins to compact the fabric wound in several layers C1-Cn.
[0046] The compaction is carried out in several steps and begins by first compacting the windings C1-Cn at the end regions 16, 18. Figure 5This compaction uses a first compacting device 20 which, in the example shown, comprises several compacting elements 22, 24 which may be of a shape varying according to the desired shape of the winding to be compressed and which are, for example, in the form of blocks or plates. The first compacting device 20 compacts the windings C1-Cn while the support is arranged in a retracted configuration, such as Figure 5 As shown. In the example shown, the windings C1-Cn are first compacted at the distal ends 16a, 18a by means of a first compacting element 22 (applying a compacting pressure in the direction of the arrow PC1), and subsequently the side portions 16b, 18b are compacted by means of a second compacting element 24 different from the first compacting element 22 (applying a compacting pressure in the direction of the arrow PC2, one component of which is directed toward the central area). The second compacting element 24 has at least one lateral surface 24a which forms a non-zero angle α with the normal N of the windings C1-Cn at this surface 24a. The compaction on the end regions 16, 18 can be performed symmetrically with respect to the second axis X2. Even if the compaction at the distal ends 16a, 18a and the side portions 16b, 18b is performed simultaneously on each end region 16, 18 by the same compacting element, rather than with several different elements 22, 24 as shown in the figure, this will still be within the scope of the invention. In general, it will be noted that the compaction can be performed by applying a predefined compacting pressure or by applying a predefined movement.
[0047] Figure 5 It shows the resulting over-length of the different winding layers C1-Cn after compaction of the end regions 16, 18. As mentioned before, an over-length of the last layer Cn compared to the first layer C1 is observed.
[0048] Once the end regions 16, 18 have been compacted, these regions 16 and 18 are again pulled apart by the movement system until they are separated by a third distance D3 ( D2 ) greater than the second distance D2. Figure 6 ) until. In this case, the support is transformed into an extended configuration. The third distance D3 may correspond to the desired dimensions of the component to be obtained, for example to its desired length. It should be noted that the third distance D3 may be greater than the initial distance D1 to take into account the overlength produced at the first layer C1 during compaction by the first compacting device. In the extended configuration, the layers C1-Cn are tightened again on the central area 17 to eliminate the wrinkles that occurred previously. The compaction is then performed with the second compacting device 32. In the example shown, a base 30 is inserted before this compaction, the base 30 being intended to support the windings C1-Cn while they are compacted by the second compacting device 32. Compaction is then applied in the direction of the arrow PC3 to make the windings C1-Cn consistent on the central area 17. It should be noted that during this construction, the compaction can be maintained by the first compacting device 20, as Figure 6 as shown, or as a variation of releasing this compaction.
[0049] The tool 10 comprises a control unit (not shown) capable of controlling the movement device and the compaction device 20 , 32 .
[0050] A description of an example of forming a fiber reinforcement of a composite component having a desired size and a desired fiber volume content has just been given. Figure 7 and Figure 8 The description is intended to describe a variant of the invention for producing components which also have an elongated geometry.
[0051] exist Figure 7 In a variant of the invention, the thickness of the fabric 120 wound on the support 140 is not constant. The fabric is initially attached to the support at the first longitudinal end 120a for winding. The thickness of the fabric increases starting from the first end 120a and then decreases in the direction of the second longitudinal end 120b. The fabric has regions 122a and 122b of decreasing thickness adjacent to the ends 120a and 120b, and its thickness decreases as the fabric approaches these ends 120a and 120b. The region 122b is advantageously superimposed on the region 122a so that once the winding is completed, the region 122b has the same number of fibers in the entire weave around the component. Figure 7 Also shown is the support 140 at the beginning of the winding operation, extending over a central zone 170 between the end zones 160, 180. In this figure, the support 140 is shown with a substantially rectilinear shape in the central zone 170, but if this is not the case, it will remain within the scope of the invention, as a variant the support could have a concave shape in this zone, for example a diabolo shape seen in cross section relative to the winding axis X1.
[0052] Figure 8 The relative movement of the end regions 160, 180 in an alternative is shown. The support 140 may comprise two parts 162 and 182, each of which comprises one of the end regions 160 or 180 and extends above the central region 170, and an adjustment device consisting of two elements 171 movable along the winding axis X1 to give the adjustment device a width that varies along this axis. By pulling apart the elements 171 along the winding axis X1, the parts 162 and 182 can be pulled towards each other and therefore also towards the end regions, thereby transitioning to the retracted configuration. The transition to the extended configuration can be made by a reverse movement.
[0053] A matrix is then formed in the pores of the fiber reinforcement using techniques known per se, for example via injection of a resin followed by cross-linking of the resin. If necessary, it should be noted that additional fiber reinforcements may be added to the wound fiber reinforcement formed by the technique of the invention, for example in the inner space defined by the wound fiber reinforcement, and then the two fiber reinforcements are densified jointly to obtain a composite component. As a variant, these fiber reinforcements may be densified separately and then combined to form the component.
[0054] Just combined Figures 3 to 8 The manufacture of components having elongated geometries has been described. Fig. 9 This is the case with components having a substantially circular geometry, here a casing for a gas turbine.
[0055] exist Fig. 9 In the example of , a support 240 is used, which includes two truncated cone rollers, each of which defines end regions 260 and 280. The winding of the fabric 220 begins with the end regions 260 and 280 spaced apart by a first distance D1. The end regions 260 and 280 gradually approach each other as the winding proceeds in a manner similar to the description given above. Once in the retracted configuration (the distance between the end regions 260, 280 is equal to D2), compactions PC1, PC2 are performed on the end regions 260, 280 as described above. Then, the support is converted into an extended configuration (the distance D3 separating the end regions 260, 280 is greater than D2), and compaction PC3 is performed on the central region after adding the support 230 to support the winding.
[0056] Those skilled in the art will appreciate that the present invention may be applied to other types of components, such as other gas turbine components, particularly outlet guide vanes.
Claims
1. A tool (10) for winding a fiber fabric (12; 120; 220), comprising at least one support (14; 140; 240) on which the fiber fabric is intended to be wound around a first winding axis (X1), the support having at least two end regions (16; 160; 260; 18; 180; 280) spaced apart along a second axis (X2) transverse to the first winding axis, It is characterized in that The tool comprises a movement device configured to change the shape of the support between a retracted structure and an extended structure by gradually bringing the end regions closer or farther apart along the second axis, and the tool comprises a first compacting device (20) and a second compacting device (32), the first compacting device being capable of performing compaction (PC1; PC2) on the end regions at least in the retracted structure, the second compacting device being different from the first compacting device and being capable of performing compaction (PC3) on a central region (17) located between the end regions in the extended structure, and wherein each end region comprises a distal end (16a; 18a) and two side portions (16b; 18b), the side portions being located on each side of the distal end and on one side of the central region, and wherein the first compacting device comprises a first compacting element (22) and a second compacting element (24), the first compacting element being capable of performing compaction (PC1) on the distal end of each end region, the second compacting element being capable of performing compaction on the side portion of each end region, wherein there is a compaction component toward the central region.
2. The tool according to claim 1, It is characterized in that The second compacting element (24) has at least one lateral surface (24a) forming a non-zero angle (α) with a normal (N) of the support (14; 140; 240) at said surface.
3. The tool (10) according to claim 1 or 2, It is characterized in that The first compacting device (20) is configured to perform compaction (PC2) by the second compacting element (24) after performing compaction (PC1) by the first compacting element (22).
4. The tool (10) according to claim 1, It is characterized in that The end region (16; 160; 260; 18; 180; 280) defines a winding surface having a circular shape.
5. A method for manufacturing a fiber preform using a tool (10) for winding a fiber fabric (12; 120; 220), the tool comprising at least one support (14; 140; 240) on which the fiber fabric is intended to be wound around a first winding axis (X1), the support having at least two end regions (16; 160; 260; 18; 180; 280) spaced apart along a second axis (X2) transverse to the first winding axis, the tool comprising a movement device, the movement The device is configured to change the shape of the support between a retracted configuration and an extended configuration by gradually bringing the end regions closer together or apart along the second axis, and the tool comprises a first compacting device (20) and a second compacting device (32), the first compacting device being capable of performing compaction (PC1; PC2) on the end regions at least in the retracted configuration, and the second compacting device, unlike the first compacting device, being capable of performing compaction (PC3) on a central region (17) located between the end regions in the extended configuration, The method at least include: - winding the fiber fabric around the first winding axis on the support by gradually reducing the distance between the end areas along the second axis to a predetermined value during winding until the support is transferred into a retracted configuration; - a first compaction of the winding at the end region by means of the first compacting device, with the support in the retracted configuration; - after said first compaction, tightening said windings in said central zone by increasing the distance between said end zones along said second axis so as to transform said support from said retracted configuration into said extended configuration; as well as - With the support in the extended configuration, a second compaction of the winding in the central region is carried out by means of the second compacting device.
6. The method according to claim 5, It is characterized in that The first compaction comprises compaction (PC1) performed by the first compaction element (22) on the distal end (16a; 18a) of the end region, followed by compaction (PC2) performed by the second compaction element (24) on the side (16b; 18b) of the end region, wherein a compaction component is directed toward the central region (17).
7. The method according to any one of claims 5 and 6, It is characterized in that The fiber fabric (12; 120; 220) is obtained by three-dimensional weaving.
8. The method according to claim 5, It is characterized in that The fiber fabric (12; 120; 220) has a region (122a; 122b) of gradually decreasing thickness near each end (120a; 120b) thereof.
9. A method for manufacturing a composite material component, comprising at least include: - Manufacturing a fiber preform by implementing the method according to claim 7 or 8; as well as - Formation of a matrix in the pores of the fiber preform just produced in order to obtain a composite component.
Citation Information
Patent Citations
Method for compacting a preform and associated compacting device (membrane)
CA3070779A1
Continuous debulking systems
CN101209591A