A method for decoupling temperature and strain measurements using buried or distributed optical fibers
By using optical fibers with different temperature and strain sensitivity coefficients for decoupling measurement in an extremely large temperature-changing environment, the problem of cross-sensitivity of fiber sensor signals is solved, and accurate temperature and strain measurement of the matrix to be measured is achieved.
Patent Information
- Application Number
- CN202311746126.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-18
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2043-12-18
AI Technical Summary
In extremely large temperature-changing environments, the temperature and strain signals of optical fiber sensors are easily cross-sensitive. The existing compensation measurement methods are not suitable for the problem of all optical fibers being buried or distributed inside or on the measured structure, resulting in signal superposition.
The first and second optical fibers with different temperature and strain sensitivity coefficients are used to be buried or distributed inside the substrate to be measured, and the sensitivity coefficients are calibrated to perform decoupling measurement in an extremely large temperature-changing environment.
Accurate decoupling measurement of the temperature and strain at the same point of the matrix to be measured in an extremely large temperature-changing environment is achieved, avoiding signal superposition and improving the accuracy of measurement.
Smart Images

Figure CN118067185B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of decoupled measurement values of temperature and strain of an object to be measured using an optical fiber sensor, and in particular to a decoupled measurement method of temperature and strain in an extreme and greatly variable temperature environment using buried or distributed optical fibers. Background Art
[0002] Distributed fiber optic sensors, referred to as distributed optical fibers, have many advantages such as small size, light weight, high sensitivity, resistance to electromagnetic interference, and easy burial inside materials. They have been widely used in the health monitoring of large structures in civil engineering, bridges, aviation, and medical fields.
[0003] For materials and structures operating in extreme and large temperature change environments, temperature and stress always exist at the same time, and changes in temperature and stress (strain) can cause changes in optical fiber signals, resulting in the problem of cross-sensitivity of temperature and strain. At present, in order to solve the problem of cross-sensitivity of temperature and strain of optical fiber sensors in extreme and large temperature change environments, temperature or strain compensation measurement methods are proposed, that is, to eliminate the temperature or strain sensitivity of optical fiber sensors by some means. The above temperature and strain compensation measurement methods are not suitable for burying all optical fibers inside the measured structure or using adhesives to solidify and distribute them on the surface of the measured structure. The reason is that in extreme and large temperature change environments, the thermal expansion and contraction of the measured structure will bring thermal strain to the optical fiber; at the same time, changes in ambient temperature will also cause the optical fiber to produce thermo-optical effects, thereby causing the superposition of optical fiber signals. Summary of the invention
[0004] In order to solve the above problems, the present invention provides a method for decoupling temperature and strain measurement using buried or distributed optical fibers. The first optical fiber and the second optical fiber with different temperature and strain sensitivity coefficients are buried inside the substrate to be measured, or distributed on the surface of the substrate to be measured and after casting and curing, the temperature and strain at the same point of the substrate to be measured are decoupled and measured in an extremely large temperature change environment (400K-4.2K).
[0005] In order to achieve the above object, the present invention provides the following technical solutions:
[0006] A method for decoupling temperature and strain measurement using buried or distributed optical fiber, comprising the following steps:
[0007] S1. Selecting a first optical fiber and a second optical fiber having different temperature and strain sensitivity coefficients, and calibrating the temperature and strain sensitivity coefficients of the first optical fiber and the second optical fiber, respectively;
[0008] S2. The first optical fiber and the second optical fiber that have completed the calibration of the temperature and strain sensitivity coefficients are completely buried in the substrate to be measured, or are distributed on the surface of the substrate to be measured and after casting and curing, the decoupling of temperature and strain at the same point of the substrate to be measured is measured in an extremely large temperature change environment.
[0009] In one preferred embodiment, in said S1, calibrating the temperature and strain sensitivity coefficients of the first optical fiber comprises the following steps:
[0010] S11. One end of the first optical fiber after the sensitization treatment is bonded to the surface of the calibration sample and set as the fixed end; the other end is freely placed on the surface of the calibration sample and set as the free end; a temperature sensor is installed at the connection position of the free end corresponding to the calibration sample; and the calibration sample is placed in the test system;
[0011] S12. Turn on the optical fiber modulator and record the initial optical fiber signals at the fixed end and the free end;
[0012] S13. Cool down the test system, turn on the fiber optic regulator and temperature collector, and record and store the fiber optic signal and temperature measurement data in real time;
[0013] S14. Using the free end optical fiber signal data and temperature data collected in S13, the temperature sensitivity coefficient of the first optical fiber is calibrated;
[0014] S15. Subtract the collected fixed-end optical fiber signal from the free-end optical fiber signal to obtain an optical fiber signal difference, where the optical fiber signal difference is the optical fiber signal caused by the thermal strain of the calibration sample; and calibrate the strain sensitivity coefficient of the first optical fiber using the theoretical thermal strain value of the calibration sample and the optical fiber signal difference.
[0015] In one of the preferred embodiments, in S11, the first optical fiber that has been subjected to the sensitization treatment is a distributed optical fiber that has been treated with different coating materials, and the coating material is a metal material or a non-metal material; the metal material is gold, copper or titanium; the non-metal material includes polyimide, epoxy resin, acrylate or polytetrafluoroethylene.
[0016] In one preferred embodiment, the first optical fiber is a distributed optical fiber having cores, claddings or central wavelengths of different diameters.
[0017] In one of the preferred embodiments, in S11, one end of the first optical fiber is bonded to the surface of the calibration sample block by a low-temperature adhesive and is set as a fixed end; after the fixed end is cured, the calibration sample block is placed in the test system.
[0018] In one preferred embodiment, in said S1, the following steps are also included:
[0019] S16. Calculate the theoretical thermal strain value of the calibration sample; use a polynomial to fit the thermal expansion coefficient of the calibration sample in a large temperature change environment of 400K-4.2K, and then calculate the theoretical thermal strain value in each temperature range:
[0020] α s (T) = a + bT + cT 2 +dT 3 +eT 4 +fT 5 ,
[0021]
[0022] Among them, αs(T) is the thermal expansion coefficient of the calibration sample in a large temperature change environment,
[0023] a, b, c, d, e and f are the fitting coefficients of thermal expansion coefficient,
[0024] Δε is the theoretical thermal strain value in the temperature range [T0, T].
[0025] In one preferred embodiment, the test system comprises an optical fiber demodulator, a temperature collector, a temperature sensor and a calibration sample block, and the calibration sample block is a thin and long calibration sample block.
[0026] In one preferred embodiment, in said S1, the temperature and strain sensitivity coefficients of the second optical fiber are calibrated by using a method for calibrating the temperature and strain sensitivity coefficients of the first optical fiber;
[0027] The second optical fiber is a distributed optical fiber treated with different coating materials, wherein the coating material is a metal material or a non-metal material; the metal material is gold, copper or titanium; the non-metal material includes polyimide, epoxy resin, acrylate or polytetrafluoroethylene;
[0028] The coating layer formed by the coating material of the second optical fiber is different from the coating layer formed by the coating material of the first optical fiber;
[0029] or the second optical fiber is a distributed optical fiber having a different diameter core, cladding or central wavelength;
[0030] The central wavelength, core and cladding of the second optical fiber are different from the central wavelength, core and cladding of the first optical fiber.
[0031] In one of the preferred embodiments, the temperature range of the extreme large temperature change environment is 400K-4.2K.
[0032] In one of the preferred embodiments, in S2, the first optical fiber and the second optical fiber that have completed the temperature and strain sensitivity coefficient calibration are placed on the surface of the substrate to be measured and cast and cured, and the first optical fiber and the second optical fiber that have completed the temperature and strain sensitivity coefficient calibration are cured on the surface of the substrate structure to be measured using an adhesive.
[0033] Based on the above technical solution, compared with the prior art:
[0034] The present invention provides a method for decoupling temperature and strain using embedded or distributed optical fibers. By using two optical fibers with different temperature and strain sensitivity coefficients, all of which are embedded in the interior of a substrate to be measured, or distributed on the surface of the substrate to be measured, after casting and curing, the decoupling of temperature and strain at the same point of the substrate to be measured can be accurately measured in an extremely large temperature change environment (400K-4.2K). BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 This is a flowchart of the method for realizing decoupled measurement of temperature and strain using buried or distributed optical fiber according to Example 1.
[0036] Figure 2 This is a flowchart of calibrating the temperature and strain sensitivity coefficients of the first optical fiber in Example 1.
[0037] Figure 3 This is a structural block diagram of the test system of Example 1.
[0038] Figure 4 This is a schematic diagram of the structure for calibrating the temperature and strain sensitivity coefficients of the first optical fiber in Example 2.
[0039] Figure 5 This is a schematic diagram of the structure of Example 3 in which two optical frequency domain reflectometers (OFDR) are completely buried inside epoxy resin to achieve temperature and strain decoupling measurement.
[0040] Figure 6 This is a schematic diagram of the structure of Example 4 in which two optical frequency domain reflectometers (OFDR) are completely solidified on the surface of oxygen-free copper to achieve temperature and strain decoupling measurement. DETAILED DESCRIPTION
[0041] In order to facilitate the understanding of the present invention, the present invention will be described more comprehensively in conjunction with the accompanying drawings and specific embodiments. The preferred embodiments of the present invention are provided in the accompanying drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thoroughly understood.
[0042] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be an intermediate element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time.
[0043] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, or the positions or positional relationships in which the product of the invention is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.
[0044] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used in the specification of the present invention herein are only for the purpose of describing specific embodiments and are not intended to limit the present invention.
[0045] Example 1
[0046] refer to Figure 1 This embodiment provides a method for decoupling temperature and strain using buried or distributed optical fibers, which specifically includes the following steps:
[0047] S1. Selecting a first optical fiber and a second optical fiber having different temperature and strain sensitivity coefficients, and calibrating the temperature and strain sensitivity coefficients of the first optical fiber and the second optical fiber, respectively;
[0048] S2. The first optical fiber and the second optical fiber that have completed the calibration of the temperature and strain sensitivity coefficients are completely buried in the substrate to be measured, or are distributed on the surface of the substrate to be measured and after casting and curing, the temperature and strain decoupling of the substrate to be measured is measured in an extremely large temperature change environment.
[0049] Among them, the temperature range of the extreme large temperature change environment is 400K-4.2K;
[0050] In S2, the first optical fiber and the second optical fiber that have completed the temperature and strain sensitivity coefficient calibration are placed on the surface of the substrate to be measured and cast and cured. Specifically, the first optical fiber and the second optical fiber that have completed the temperature and strain sensitivity coefficient calibration are cured on the surface of the substrate structure to be measured using an adhesive, such as a low-temperature adhesive.
[0051] refer to Figure 2In S1, the temperature and strain sensitivity coefficients of the first optical fiber are calibrated, which specifically includes the following steps:
[0052] S11. One end of the first optical fiber after the sensitization treatment is bonded to the surface of the calibration sample and set as the fixed end; the other end is freely placed on the surface of the calibration sample and set as the free end; a temperature sensor is installed at the connection position of the free end corresponding to the calibration sample; and the calibration sample is placed in the test system;
[0053] S12. Turn on the optical fiber modulator and record the initial optical fiber signals at the fixed end and the free end;
[0054] S13. Cool down the test system, turn on the fiber optic regulator and temperature collector, and record and store the fiber optic signal and temperature measurement data in real time;
[0055] S14. Using the free end optical fiber signal data and temperature data collected in S13, the temperature sensitivity coefficient of the first optical fiber is calibrated;
[0056] S15. Subtract the collected fixed-end optical fiber signal from the free-end optical fiber signal to obtain an optical fiber signal difference, where the optical fiber signal difference is the optical fiber signal caused by the thermal strain of the calibration sample; and calibrate the strain sensitivity coefficient of the first optical fiber using the theoretical thermal strain value of the calibration sample and the optical fiber signal difference.
[0057] It should be noted that in S11, the first optical fiber that has been subjected to the sensitization treatment is a distributed optical fiber that has been treated with different coating materials, and the coating material is a metal material or a non-metal material; the metal material or the non-metal material is coated on the surface of the first optical fiber to form a coating layer, thereby sensitizing the first optical fiber.
[0058] In some embodiments, the metal material is gold, copper or titanium; in some embodiments, the non-metal material includes polyimide, epoxy resin, acrylate or polytetrafluoroethylene, and the non-metal material can also be a polymer material that can sensitize the first optical fiber.
[0059] In other embodiments, the first optical fiber is a distributed optical fiber having cores, claddings, or central wavelengths of different diameters.
[0060] It should also be noted that in S11, one end of the first optical fiber is bonded to the surface of the calibration sample block by a low-temperature adhesive and is set as a fixed end; after the fixed end is cured, the calibration sample block is placed in the test system.
[0061] refer to Figure 3 In the decoupling measurement method of this embodiment, the test system 100 used includes an optical fiber demodulator 1, a temperature collector 2, a temperature sensor 3 and a calibration sample 4. The calibration sample is a thin and long calibration sample, such as a thin and long oxygen-free copper.
[0062] Since the temperature and strain sensitivity coefficients of the two optical fibers used in this embodiment are different from each other, it is also necessary to calibrate the temperature and strain sensitivity coefficients of the second optical fiber. Specifically, the temperature and strain sensitivity coefficients of the second optical fiber are calibrated by using the method for calibrating the temperature and strain sensitivity coefficients of the first optical fiber.
[0063] Specifically, the second optical fiber is also subjected to a sensitization treatment, and is a distributed optical fiber treated with different coating materials, and the coating material is a metal material or a non-metal material; in some embodiments, the metal material is gold, copper or titanium; in some embodiments, the non-metal material includes polyimide, epoxy resin, acrylate or polytetrafluoroethylene. It should be noted that the coating layer formed by the coating material of the second optical fiber is different from the coating layer formed by the coating material of the first optical fiber.
[0064] In other embodiments, the second optical fiber is a distributed optical fiber having a core, cladding or central wavelength of different diameters; it should be noted that the central wavelength, core and cladding of the second optical fiber are different from the central wavelength, core and cladding of the first optical fiber.
[0065] Further references Figure 2 , in S1, the following steps are also included:
[0066] S16. Calculate the theoretical thermal strain value of the calibration sample; use a polynomial to fit the thermal expansion coefficient of the calibration sample in a large temperature change environment of 400K-4.2K, and then calculate the theoretical thermal strain value in each temperature range:
[0067] α s (T) = a + bT + cT 2 +dT 3 +eT 4 +fT 5 ,
[0068]
[0069] Among them, αs(T) is the thermal expansion coefficient of the calibration sample in a large temperature change environment,
[0070] a, b, c, d, e and f are the fitting coefficients of thermal expansion coefficient,
[0071] Δε is the theoretical thermal strain value in the temperature range [T0, T].
[0072] The present embodiment provides a method for decoupling temperature and strain by using embedded or distributed optical fibers. By using two optical fibers with different temperature and strain sensitivity coefficients, all of which are embedded in the interior of the substrate to be measured, or distributed on the surface of the substrate to be measured, after casting and curing, the decoupling of temperature and strain at the same point of the substrate to be measured can be accurately measured in an extremely large temperature change environment (400K-4.2K).
[0073] Example 2
[0074] This embodiment provides a method for calibrating the temperature and strain sensitivity coefficients of an optical fiber, wherein the optical fiber is a single optical frequency domain reflectometer (OFDR), which can be a first optical fiber or a second optical fiber. For example, after the strain and temperature sensitivity coefficients of the first optical fiber in an extreme large temperature change environment are calibrated, the same method is used to calibrate the strain and temperature sensitivity coefficients of the first optical fiber in an extreme large temperature change environment.
[0075] In this embodiment, the first optical fiber is described as a frequency domain reflectometer (OFDR1).
[0076] like Figure 4 As shown, first, one end of the OFDR treated with different coating materials is bonded to the surface of the calibration block using a low-temperature adhesive 5 to form a first area L1; the other end is freely placed on the surface of the calibration block to form a second area L2, and a temperature sensor 3 is installed at the same position. After the OFDR1 is cured, the calibration block 4 is freely placed in the test system. Among them, the low-temperature adhesive 5 is a thermally conductive potting glue, and its model can be Stycast 2850ft; the calibration block 4 is a thin and long oxygen-free copper. The first area L1 is used to measure temperature and strain; the second area L2 is used to measure temperature.
[0077] Then, turn on the fiber demodulator and temperature collector, cool down the test system, and record the OFDR optical frequency signal and temperature data in real time.
[0078] Finally, the temperature sensitivity coefficient of OFDR is calibrated using the recorded temperature and free-end fiber signal, and the recorded fixed-end fiber signal is subtracted from the free-end fiber signal. The strain sensitivity coefficient of the optical fiber is calibrated using the theoretical thermal strain of the calibration sample and the fiber signal.
[0079] Considering that the thermal expansion coefficient of the calibration sample has a strong temperature dependence in an extreme temperature change environment (400K-4.2K), it is necessary to use a polynomial to fit the thermal expansion coefficient of the calibration sample in a temperature change environment of 400K-4.2K, and then calculate the theoretical thermal strain in each temperature range. The calculation method is as follows:
[0080] α s (T) = a + bT + cT 2+dT 3 +eT 4 +fT 5
[0081]
[0082] Among them, αs(T) is the thermal expansion coefficient of the calibration sample in a large temperature change environment,
[0083] a, b, c, d, e and f are the fitting coefficients of thermal expansion coefficient,
[0084] Δε is the theoretical thermal strain value in the temperature range [T0, T].
[0085] The same method is used to calibrate the strain and temperature sensitivity coefficients of the second optical fiber, which is also a frequency domain reflectometer (OFDR), in an extreme temperature change environment. It should be noted that the temperature and strain sensitivity coefficients of the second optical fiber are different from those of the first optical fiber.
[0086] Example 3
[0087] like Figure 5 As shown, in this embodiment, two optical frequency domain reflectometers (OFDR) are completely buried inside the epoxy resin to achieve temperature and strain decoupling measurement.
[0088] Firstly, two OFDRs with different temperature and strain sensitivity coefficients, namely, the first optical fiber OFDR1 and the second optical fiber OFDR2, are selected and placed in an epoxy resin 6 curing mold, and the epoxy resin 6 is poured and cured in a vacuum environment.
[0089] The samples are then placed in a test system that can provide an extremely wide temperature change environment for a temperature drop test.
[0090] Finally, the decoupled measurement of the temperature and strain inside the epoxy resin 6 is realized by using the first optical fiber OFDR1 and the second optical fiber OFDR2, two optical frequency domain reflectometers with different temperature and strain sensitivity coefficients. The calculation formula is:
[0091]
[0092] in,
[0093] Kε1 is the strain sensitivity coefficient of the first optical fiber;
[0094] Kε2 is the strain sensitivity coefficient of the second optical fiber;
[0095] K T1 is the temperature sensitivity coefficient of the first optical fiber;
[0096] K T2 is the temperature sensitivity coefficient of the second optical fiber.
[0097] The above parameters are different from each other. The above calculation formula can be used to calculate the temperature and strain of the substrate to be measured by the optical fiber.
[0098] Example 4
[0099] like Figure 6 As shown, in this embodiment, two optical frequency domain reflectometers (OFDR) are all solidified on the surface of oxygen-free copper to achieve temperature and strain decoupling measurement.
[0100] First, the oxygen-free copper 41 is placed in the adhesive 51 curing mold, two OFDRs with different temperature and strain sensitivity coefficients are selected, namely the first optical fiber OFDR1 and the second optical fiber OFDR2 are placed on the surface of the oxygen-free copper, and the pouring and curing of the adhesive 51 are completed.
[0101] The samples are then placed in a test system that can provide an extremely wide temperature change environment for a temperature drop test.
[0102] Finally, the decoupled measurement of the internal temperature and strain of the oxygen-free copper 41 is achieved by using the first optical fiber OFDR1 and the second optical fiber OFDR2, two optical frequency domain reflectometers with different temperature and strain sensitivity coefficients.
[0103] The above contents are merely examples and illustrations of the structure of the present invention, and the description is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, and these obvious replacement forms all belong to the protection scope of the present invention.
Claims
1. A method for decoupling temperature and strain measurement using buried or distributed optical fiber, characterized in that: The following steps are involved: S1. Selecting a first optical fiber and a second optical fiber having different temperature and strain sensitivity coefficients, and calibrating the temperature and strain sensitivity coefficients of the first optical fiber and the second optical fiber, respectively; S2. The first optical fiber and the second optical fiber, which have completed the calibration of the temperature and strain sensitivity coefficients, are completely buried in the substrate to be measured, or distributed on the surface of the substrate to be measured and poured and cured, and the temperature and strain decoupling of the same point of the substrate to be measured are measured in an extremely large temperature change environment; The central wavelength, core and cladding of the second optical fiber are different from the central wavelength, core and cladding of the first optical fiber; The temperature range of the extreme large temperature change environment is 400K-4.2K; In S1, the temperature and strain sensitivity coefficients of the first optical fiber are calibrated, including the following steps: S11. One end of the first optical fiber after the sensitization treatment is bonded to the surface of the calibration sample and set as the fixed end; the other end is freely placed on the surface of the calibration sample and set as the free end; a temperature sensor is installed at the connection position of the free end corresponding to the calibration sample; and the calibration sample is placed in the test system; S12. Turn on the optical fiber modulator and record the initial optical fiber signals at the fixed end and the free end; S13. Cool down the test system, turn on the fiber optic regulator and temperature collector, and record and store the fiber optic signal and temperature measurement data in real time; S14. Using the free end optical fiber signal data and temperature data collected in S13, the temperature sensitivity coefficient of the first optical fiber is calibrated; S15. The collected fixed-end optical fiber signal is subtracted from the free-end optical fiber signal to obtain an optical fiber signal difference, wherein the optical fiber signal difference is an optical fiber signal caused by thermal strain of the calibration sample; the strain sensitivity coefficient of the first optical fiber is calibrated using the theoretical thermal strain value of the calibration sample and the optical fiber signal difference; S16. Calculate the theoretical thermal strain value of the calibration sample; use a polynomial to fit the thermal expansion coefficient of the calibration sample in a large temperature change environment of 400K-4.2K, and then calculate the theoretical thermal strain value in each temperature range: α s (T)=a+bT+cT 2 +dT 3 +eT 4 +fT 5 , Among them, αs(T) is the thermal expansion coefficient of the calibration sample in a large temperature change environment, a, b, c, d, e and f are the fitting coefficients of thermal expansion coefficient, Δε is the theoretical thermal strain value in the temperature range [T0, T].
2. The method for decoupling temperature and strain using buried or distributed optical fiber according to claim 1, characterized in that: In S11, the first optical fiber that has undergone sensitization treatment is a distributed optical fiber that has been treated with different coating materials, and the coating material is a metal material or a non-metal material; the metal material is gold, copper or titanium; the non-metal material includes polyimide, epoxy resin, acrylate or polytetrafluoroethylene.
3. The method for decoupling temperature and strain using buried or distributed optical fiber according to claim 1, characterized in that: In S11, one end of the first optical fiber is bonded to the surface of the calibration sample block by a low-temperature adhesive and is set as a fixed end; after the fixed end is cured, the calibration sample block is placed in a test system.
4. The method for decoupling temperature and strain using buried or distributed optical fiber according to claim 1, characterized in that: The test system comprises an optical fiber demodulator, a temperature collector, a temperature sensor and a calibration sample block, wherein the calibration sample block is a thin and long calibration sample block.
5. The method for decoupling temperature and strain using buried or distributed optical fiber according to claim 1, characterized in that: In S1, the temperature and strain sensitivity coefficients of the second optical fiber are calibrated by using the method for calibrating the temperature and strain sensitivity coefficients of the first optical fiber; The second optical fiber is a distributed optical fiber treated with different coating materials, wherein the coating material is a metal material or a non-metal material; the metal material is gold, copper or titanium; the non-metal material includes polyimide, epoxy resin, acrylate or polytetrafluoroethylene; The coating layer formed by the coating material of the second optical fiber is different from the coating layer formed by the coating material of the first optical fiber.
6. The method for decoupling temperature and strain using buried or distributed optical fiber according to claim 1, characterized in that: In S2, the first optical fiber and the second optical fiber that have completed the temperature and strain sensitivity coefficient calibration are placed on the surface of the substrate to be measured and cast and cured, and the first optical fiber and the second optical fiber that have completed the temperature and strain sensitivity coefficient calibration are cured on the surface of the substrate structure to be measured using an adhesive.