Tulobuterol transdermal patch and preparation method thereof
By using a copolymer mixture of a pressure-sensitive adhesive layer and a polyester backing layer in tulobuterol transdermal patches, combined with stabilizers and penetration enhancers, the problems of poor compatibility and insufficient stability of the adhesive layer are solved. Achieved better drug release uniformity and stability in high temperature environments.
Patent Information
- Application Number
- CN202211590031.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-12
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2042-12-12
AI Technical Summary
Existing tulobuterol transdermal patches have problems such as poor compatibility in the adhesive layer, uneven drug release, and insufficient stability. In particular, drug sublimation in high-temperature environments leads to reduced content, affecting safety and durability.
The pressure-sensitive adhesive layer contains a mixture of copolymer A and copolymer B. The active ingredient is in the range of 1.5-5%. The ratio of copolymers A and B is 3:1-5:1. The backing layer is polyester and ethylene. - Vinyl acetate copolymer film, add anti-stick layer and stabilizer such as oleic acid or maleic acid, penetration enhancer azone, and the preparation method is to heat and coat evenly at 45-55°C to improve stability.
The transdermal absorption performance and stability of Tuloterol transdermal patch are improved, it is resistant to high temperature environment, the stabilizer is non-volatile, the dosage is accurate, it is convenient for production and storage, and it reduces the risk of uneven drug release and crystallization.
Smart Images

Figure CN118178357B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of medical technology, in particular to a novel tulobuterol transdermal patch and a preparation method thereof. Background Art
[0002] Asthma and chronic obstructive pulmonary disease (COPD) are common and frequently occurring diseases of the respiratory system. Asthma is a disease characterized by chronic airway inflammation and bronchial hyperresponsiveness. It is one of the common chronic diseases in children and young people; COPD is a chronic disease characterized by chronic bronchitis, airway remodeling and emphysema (alveolar destruction) leading to progressive and irreversible airflow obstruction. It is an inflammatory lung disease that often occurs in elderly patients.
[0003] Tulobutero l is chemically named (RS)-2-tert-butylamino-1-(2-chlorophenyl)ethanol and its molecular formula is C 12 H 18 C l NO, chemical structure is
[0004]
[0005] Tulobuterol is a selective β2 receptor agonist that has a strong and lasting dilating effect on bronchial smooth muscle. It is mainly used in the clinical treatment of bronchial asthma, chronic obstructive pulmonary disease, chronic bronchitis, etc.
[0006] The dosage forms of tulobuterol currently available in China include tablets, aerosols, ointments, syrups and emulsions, all of which have different defects in the treatment of asthma and COPD. Oral tablets are rapidly absorbed, and the effect can last for 4 to 6 hours, but the effective therapeutic concentration is maintained for a short time. In addition, oral administration can produce significant adverse reactions, such as tremors and palpitations. Aerosols take effect quickly but the duration of action is also short. In addition, due to the complex use procedures and the need for frequent use, patient compliance is poor and the treatment effect is also poor. Ointments and emulsions are also limited in clinical application because their application doses are difficult to accurately quantify.
[0007] Transdermal drug delivery system (TDDS), also known as transdermal patch, delivers drugs through the skin, allowing the drug to pass through the epidermis and be absorbed by the capillaries in the dermis into the blood circulation to achieve the purpose of treatment. This method of drug delivery has the advantages of long-term sustained release, maintaining stable blood drug concentration, reducing adverse drug reactions, avoiding first-pass liver effect and gastrointestinal inactivation effect, convenient administration, and patients can take the drug themselves. Tokyo Electric Power Company of Japan first developed the tulobuterol patch, which was launched in Japan in 1998 under the trade name Tape. In November 2006, the drug was granted an import drug registration certificate (trade name: Ami Aid). Preparation specifications are: 0.5mg (2.5cm 2 )、1.0mg(5cm 2 ) and 2.0mg(10cm 2 ). This product only needs to be applied once a day, which can reduce the peak and valley phenomenon of blood drug concentration, reduce adverse reactions, and is easy to use. It is especially suitable for patients who are relatively difficult to take oral preparations, such as the elderly or infants.
[0008] Tape is a single-layer crystalline patch. As the world's first transdermal patch for the treatment of asthma and COPD, its formulation process still has some defects. The tape adhesive layer uses a synthetic rubber polyisobutylene (PI B) matrix, and tulobuterol has limited solubility in PI B. The compatibility of tulobuterol, adhesives and additives in the adhesive layer of the Tape prescription is poor, and the drug has to be above the saturation concentration. In the supersaturated state, the release of tulobuterol from the adhesive layer is continuous, but this also leads to poor adhesion of the patch and initial drug release. In addition, if the storage environment changes, the drug precipitated to the surface of the adhesive layer will dissolve in the adhesive layer and then recrystallize again, causing changes in the size of the drug crystals, resulting in uneven percutaneous absorption and safety issues. Most importantly, because tulobuterol has certain sublimation characteristics, after experiencing a high-temperature storage environment, the drug in the patch sublimates, resulting in a significant reduction in the drug content in the patch. The security and stability of Tape need to be further improved.
[0009] Chinese patent application CN 115054590 A discloses a stable percutaneous absorption preparation containing tulobuterol, wherein the adhesive layer contains an acrylic pressure-sensitive adhesive and an amine compound, specifically, acrylic acid is polymerized from 2-ethylhexyl methacrylate, 2-ethylhexyl acrylate and dodecyl methacrylate, and the amine compound can be ammonia water, diethanolamine, ethylenediamine, ammonium acetate, ammonium chloride, etc. Among them, the amine compound plays the role of a stabilizer in the patch. Amine substances are liquid excipients, have a low boiling point, are highly volatile, and are easily volatilized during the preparation process, resulting in a decrease in the accuracy of the amount of excipient added. At the same time, due to its volatility, the production environment is polluted. Summary of the invention
[0010] Technical Problems to be Solved by the Invention
[0011] In view of the above technical problems, the object of the present invention is to provide a new tulobuterol transdermal patch with good transdermal absorption performance and better stability.
[0012] Technical solutions to technical issues
[0013] The invention provides a novel tulobuterol transdermal patch, which comprises a pressure-sensitive adhesive layer and a backing layer, wherein the pressure-sensitive adhesive layer contains a pressure-sensitive adhesive and an active ingredient, wherein the active ingredient is tulobuterol or a pharmaceutically acceptable salt thereof, and the pressure-sensitive adhesive is a mixture of a copolymer A and a copolymer B, wherein the copolymer A is a copolymer of vinyl acetate and isooctyl acrylate, and the copolymer B is a copolymer of 2-ethylhexyl acrylate, 2-hydroxyethyl acrylate and methyl acrylate, wherein the content of the active ingredient in the pressure-sensitive adhesive layer is in the range of 1.5% by weight to 5% by weight, and the balance is the pressure-sensitive adhesive.
[0014] In the tulobuterol transdermal patch of the present invention, the content of the active ingredient in the pressure-sensitive adhesive layer is preferably in the range of 2.5 wt% to 3.5 wt%, with the remainder being the pressure-sensitive adhesive. In the tulobuterol transdermal patch of the present invention, the weight ratio of the vinyl acetate content in the copolymer A to isooctyl acrylate is 1:2 to 2:1, preferably 1:1.5 to 1:1.
[0015] In the tulobuterol transdermal patch of the present invention, the content of 2-ethylhexyl acrylate in the copolymer B is 67-77% by weight, the content of 2-hydroxyethyl acrylate is 3-7% by weight, and the content of methyl acrylate is 20-26% by weight.
[0016] In the tulobuterol transdermal patch of the present invention, preferably, the content of 2-ethylhexyl acrylate in the copolymer B is 70-74% by weight, the content of 2-hydroxyethyl acrylate is 4-6% by weight, and the content of methyl acrylate is 22-24% by weight.
[0017] In the tulobuterol transdermal patch of the present invention, preferably, the content of 2-ethylhexyl acrylate in the copolymer B is 72% by weight, the content of 2-hydroxyethyl acrylate is 5% by weight, and the content of methyl acrylate is 23% by weight.
[0018] In the tulobuterol transdermal patch of the present invention, the weight ratio of the copolymer A to the copolymer B is 3:1 to 5:1, preferably 4:1.
[0019] In the tulobuterol transdermal patch of the present invention, the backing layer is preferably a polyester and ethylene-vinyl acetate copolymer film.
[0020] In the tulobuterol transdermal patch of the present invention, the patch preferably further comprises an anti-adhesive layer, wherein the anti-adhesive layer is a polyethylene terephthalate film containing a fluoride coating, and the anti-adhesive layer serves as a release film to protect the pressure-sensitive adhesive layer and is discarded when used.
[0021] In the tulobuterol transdermal patch of the present invention, the pressure-sensitive adhesive layer of the patch preferably further contains azone, a penetration enhancer, and the content of azone is not less than 4% by weight, more preferably 4% to 8% by weight, based on the weight of the pressure-sensitive adhesive layer of the patch.
[0022] In the tulobuterol transdermal patch of the present invention, the pressure-sensitive adhesive layer of the patch preferably further contains a stabilizer, and the stabilizer is preferably selected from one or more of oleic acid, maleic acid or stearic acid. The content of the stabilizer is 0.3 to 0.6 weight % based on the weight of the pressure-sensitive adhesive layer in the patch.
[0023] The thickness of the pressure-sensitive adhesive layer of the tulobuterol transdermal patch of the present invention is preferably 65 to 70 μm.
[0024] The present invention also provides a method for preparing a tulobuterol transdermal patch, comprising preparing a tulobuterol bulk drug or a pharmaceutically acceptable salt thereof into a solution, uniformly mixing the solution with a pressure-sensitive adhesive, coating the solution on an anti-adhesive layer, heating the solution at 45-55° C. to volatilize the solvent (ethyl acetate and ethanol), adding a backing layer, and uniformly applying pressure to obtain a transdermal patch.
[0025] In the preparation method of the tulobuterol transdermal patch of the present invention, the solvent is a volatile solvent, preferably an alcohol solvent, more preferably ethanol.
[0026] Beneficial technical effects
[0027] The present invention and the original transdermal patch Compared with the conventional tape, the transdermal absorption performance is good, the stability of the preparation is better, the tolerance to high temperature environment is good, and the content of the patch is stable during the storage period. In addition, the stabilizer in the present invention is an acid, which is a solid auxiliary material, has physical stability under the production and storage conditions of the preparation, is non-volatile, and the addition amount is accurate, which is convenient for production and storage. DETAILED DESCRIPTION
[0028] Material:
[0029] 87-4098, 87-2677, 87-2852, Du ro-
[0030] 87-2510: purchased from Henkel, Germany;
[0031] Cotran TM 9733、Cotran TM 9701、Cotran TM 9720: purchased from 3M China Co., Ltd.
[0032] Scotchpak TM 9744: Purchased from 3M China Ltd.
[0033] Experimental Animals:
[0034] Japanese large-eared white rabbits, male, 1.5-2.0 kg, were purchased from the Experimental Animal Center of Shenyang Pharmaceutical University;
[0035] Male rats were purchased from the Experimental Animal Center of Shenyang Pharmaceutical University.
[0036] Preparation of transdermal patches
[0037] Take the tulobuterol raw material and solvent, stir until the drug is completely dissolved, add the pressure-sensitive adhesive, continue stirring until the solution is uniform, let it stand, and apply it on the anti-adhesive layer with a thickness of about 350 μm. Let it stand for a while, heat it at about 45-55° C. for 10 minutes to remove the organic solvent in the adhesive layer, take it out, cover it with a backing layer, and evenly apply pressure to obtain a transdermal patch.
[0038] The solvent is not particularly limited, as long as it has good solubility for tulobuterol or a pharmaceutically acceptable salt thereof. Volatile solvents such as alcohols and ethyl acetate are preferred. Considering accessibility and environmental friendliness, alcohol solvents are preferred, and ethanol is particularly preferred.
[0039] Skin penetration test
[0040] The skin permeability of the abdominal skin of white rabbits was measured using an in vitro diffusion cell. That is, the skin of white rabbits was placed in an in vitro diffusion cell having a permeation area of 1.13 square centimeters, and 0.75 ml of a 2:1 mixture of polyethylene glycol 200 (macrogol 200) and phosphate buffer was used as a receiver fluid, and each preparation was adhered to the skin on the donor side (n=4). The receiver liquid was stirred for 24 hours while being maintained at 37°C, and the concentration of the compound tulobuterol or its salt in the receiver liquid was measured by high performance liquid chromatography (chromatographic column: YMC AM312 ODS 5 μm (6 mmφ×150 mm; YMC), mobile phase: 0.01 mol / L aqueous solution containing sodium dodecyl sulfate (pH adjusted to 2.4 with phosphoric acid): acetonitrile: methanol (2:5:3), column temperature: 40°C, flow rate: 1.0 ml / min), and the permeation amount (cumulative permeation amount) of the compound in each formulation was determined.
[0041] Example
[0042] The present invention is described in detail below with reference to the examples. The examples illustrate detailed implementation methods and processes to fully disclose and demonstrate that the invention can be implemented. The examples do not represent limitations on the invention, and the protection scope of the present invention is not limited to the following examples. Based on the specific examples in the present invention, all other embodiments obtained by ordinary technicians in the field without creative work belong to the protection scope of the present invention.
[0043] In the examples of the present invention, unless otherwise specified, all raw material components are commercially available products well known to those skilled in the art; in the examples of the present invention, unless otherwise specified, the technical means used are conventional means well known to those skilled in the art. The progress of the reaction of the present invention can be monitored by conventional monitoring methods in the art (such as TLC, LCMS or NMR), and the reaction endpoint is generally taken as the disappearance of the reaction substrate.
[0044] The experimental methods in the embodiments of the specification without specifying specific conditions are usually carried out according to the conventional conditions in the art or the conditions recommended by the manufacturer. In the present invention, unless otherwise specified, "parts" means parts by weight, and "%" means percentage by weight. In the present invention, unless otherwise specified, "above", "below", "within" means including the number itself.
[0045] 1. Screening of pressure-sensitive adhesive matrix
[0046] Pressure-sensitive adhesive (hereinafter sometimes referred to as PSA) refers to an adhesive that is sensitive to pressure and can be firmly bonded to an adherend by simply applying pressure. As the matrix of a pressure-sensitive adhesive dispersion patch, it not only serves as a carrier of the drug, but also can regulate the release of the drug. Pressure-sensitive adhesives have a great influence on the permeation behavior of drugs, so the inventors first screened pressure-sensitive adhesives.
[0047] 87-4098: Polyacrylate pressure-sensitive adhesive without polar groups, copolymer of 40 wt% to 50 wt% vinyl acetate and 50 wt% to 60 wt% isooctyl acrylate, solid content of 38.5 wt%, solvent is ethyl acetate;
[0048] 87-2677: Polyacrylate pressure-sensitive adhesive containing carboxyl groups;
[0049] 87-2852: Polyacrylate pressure-sensitive adhesive containing carboxyl groups 87-2510: Polyacrylate pressure-sensitive adhesive containing hydroxyl groups;
[0050] DURO 87-2510: Polyacrylate pressure-sensitive adhesive containing hydroxyl functional groups, a copolymer of 2-ethylhexyl acrylate (72 weight %), 2-hydroxyethyl acrylate (5 weight %) and methyl acrylate (23 weight %), with a solid content of 40.5 weight %, and the solvent is ethyl acetate.
[0051] Take about 50 mg of tulobuterol API and about 0.45 mL of ethanol, place them in a 10 mL beaker, add a magnetic rotor to stir until the drug is completely dissolved in ethanol, add about 4.5 g of pressure-sensitive adhesive, continue stirring for at least 2 h, stop stirring and let stand for 30 min, and apply it on the anti-adhesive layer (Scotchpak TM 9744), let it stand at room temperature for 10 min, put it in a 50°C oven for 10 min, take it out and cover it with a backing layer (Cotran TM 9733), and after applying pressure evenly, remove the entire patch and place it at room temperature for later use. The patch part with a pressure-sensitive adhesive layer thickness of about 80 μm was selected for transdermal testing to calculate the cumulative permeation amount (ug / cm 2 ) is used as an indicator to screen pressure-sensitive adhesives.
[0052] The experimental results are shown in Table 1.
[0053] Table 1 Screening of pressure sensitive adhesive
[0054]
[0055] As shown in Table 1, Model 87-4098 and The patch prepared with 87-2510 pressure-sensitive adhesive can obtain a much higher 87-2677 and The cumulative transmittance of 87-2852 is ten to one hundred times that of 2677 and 2852.
[0056] 2. Screening of backing layer
[0057] The backing layer is one of the important components of the drug pressure-sensitive adhesive dispersion patch. The backing layer can affect the release of the drug from the patch and the hydration state of the skin. The inventors chose 3M's Cotran TM 9733、Cotran TM 9701、Cotran TM 9720These three different types were investigated as backing layers.
[0058] Cotran TM 9733 is a polyester and ethylene-vinyl acetate copolymer film with a thickness of 48 μm;
[0059] Cotran TM 9720 is a translucent low-density polyethylene (PE) film with a thickness of 76 μm;
[0060] Cotran TM 9701 is a translucent low-density polyurethane (PU) film with a thickness of 50 μm;
[0061] Take about 150 mg of tulobuterol API and about 1.35 mL of ethanol, place them in a 25 mL beaker, add a magnetic rotor to stir until the drug is completely dissolved in ethanol, and add the pressure-sensitive adhesive. 87-4098 is 10.8g, Duro- 87-2510 is 2.7g. Continue stirring for at least 2 hours. After stopping stirring, let it stand for 30 minutes. Divide it into 3 parts and apply them on the anti-sticking layer Scotchpak at a thickness of 350μm. TM 9744, let it stand at room temperature for 10 min, put it in a 45-55℃ oven for 10 min, take it out and cover it with the above three backing layers respectively, apply pressure evenly, remove the whole patch, and let it stand at room temperature for use, select the patch part with a thickness of about 80μm for transdermal test, and select the backing layer based on the cumulative penetration amount.
[0062] Results show: Cotran TM The cumulative permeation is the largest when 9733 is used as the backing layer. The experimental results are shown in Table 2.
[0063] Table 2 Screening of backing layer screening
[0064] prescription Backing layer <![CDATA[Cumulative permeation amount (μg / cm 2 )(mean ± SD)]]> B1 <![CDATA[Cotran TM 9733]]> 239.9±9.2 B2 <![CDATA[Cotran TM 9701]]> 100.8±39.6 B3 <![CDATA[Cotran TM 9720]]> 207.4±25.4
[0065] 3. Screening of the thickness of the pressure-sensitive adhesive layer of the patch
[0066] The prescribed amount of tulobuterol API and ethanol were placed in a 10 mL beaker and stirred with a magnetic rotor until the drug was completely dissolved in the ethanol. The prescribed amount of pressure-sensitive adhesive was added. 87-4098 and 87-2510, continue stirring for at least 1 hour, stop stirring and let stand for 30 minutes, and apply it on the anti-sticking layer Scotchpak at the prescribed coating thickness. TM 9744, let stand at room temperature for 10 min, put in a 45-55℃ oven for 10 min, take out and cover with backing layer Cotran TM 9733, after applying pressure evenly, remove the entire patch and place it at room temperature for later use, and select the thickness of the pressure-sensitive adhesive layer in the prescription design for transdermal drug delivery test.
[0067] The results show that the thickness of the pressure-sensitive adhesive layer is selected to be 65-70 μm. The experimental results are shown in Table 3.
[0068] Table 3 Screening of the thickness of the pressure-sensitive adhesive layer in the patch
[0069]
[0070]
[0071] 4. Screening of patch stabilizers
[0072] 4.1 Impact on release
[0073] The prescribed amount of tulobuterol API, stabilizer (molar ratio with drug 1:1) stearic acid SA, oleic acid OA, maleic acid MA, tartaric acid TA, fumaric acid FA, citric acid CA and ethanol were placed in a 10 mL beaker, and a magnetic rotor was added to stir until the drug and stabilizer were completely dissolved in ethanol, and the prescribed amount of pressure-sensitive adhesive was added. 87-4098 and 87-2510, continue stirring for at least 1 hour, stop stirring and let stand for 30 minutes, and apply on the anti-sticking layer Scotchpak at a coating thickness of 0.35 mm. TM 9744, let stand at room temperature for 10 min, put in a 45-55℃ oven for 10 min, take out and cover with backing layer Cotran TM 9733, after applying pressure evenly, remove the entire patch and place it at room temperature for later use.
[0074] Patches with a pressure-sensitive adhesive layer thickness of 65 to 70 μm in the prescription design were selected for transdermal drug delivery test. The diameter of the patch was 1 cm 2 . Place the cellophane membrane on a horizontal diffusion cell, apply the patch on the cellophane membrane, fix it toward the receiving cell, add 4.0 mL of phosphate buffer solution (PBS, pH 7.4) to the diffusion cell, and add a stirrer to the diffusion cell. Under continuous stirring, take samples from the diffusion cell at 0.5, 1, 2, 3, 4, 6, 8, 10, and 12 h, with a sampling volume of 2 mL, and immediately add new PBS. After the sample was centrifuged at 16000 rpm and -5°C for 7 min, the release amount per unit area (ug / cm 2 ).
[0075] The results show that the release rates of the patches containing maleic acid (MA), tartaric acid (TA), fumaric acid (FA) and citric acid (CA) are all low, and the inhibitory effect on the drug is good. The release rate (%) is the release amount per unit area / drug content per unit area. The experimental results are shown in Table 4.
[0076] Table 4 Screening of patch stabilizers
[0077]
[0078]
[0079] 4.2 Whether there is crystal precipitation
[0080] The prescribed amount of tulobuterol API was mixed with the prescribed amount of maleic acid (MA), tartaric acid (TA), fumaric acid (FA), citric acid (CA) and ethanol, and after all of them were dissolved, the prescribed amount of pressure-sensitive adhesive was added. 87-4098 and 87-2510 (4:1) mixture was stirred for 1 hour, allowed to stand for 0.5 hour to remove air bubbles, and then coated with Scotchpak TM 9744 was coated with 0.35 mm, left at room temperature for 10 min, and then dried in an oven at 50°C for 5 min. Cotran backing layer was used to cover the backing layer. TM 9733.
[0081] Investigation method: Store in a constant temperature and humidity chamber away from light, and investigate at 40℃ for 1.5 months and 60℃ for 10 days. Determine the content of tulobuterol in the patch at 0 days, 10 days and 1.5 months, and compare the sample content at the two test temperatures with that at 0 day to obtain the percentage decrease of the sample and the reference preparation.
[0082] The results show that the four prescriptions can achieve a reduction in the content determination of the stability study that is basically consistent with the commercially available amount. The addition amount of maleic acid MA is between 0.3% and 0.4% by weight of the pressure-sensitive adhesive layer, the addition amount of fumaric acid FA is 0.35% to 0.4% by weight of the pressure-sensitive adhesive layer, the addition amount of tartaric acid TA is 0.4% to 0.5% by weight of the pressure-sensitive adhesive layer, and the addition amount of citric acid CA is 0.5% to 0.6% by weight of the pressure-sensitive adhesive layer, which can achieve the effect of stabilizing tulobuterol without crystallization. The experimental results are shown in Table 5.
[0083] Table 5 Screening of stabilizers
[0084]
[0085]
[0086] 5. Screening of penetration enhancers
[0087] 3 wt% of tulobuterol API, stabilizer such as maleic acid (0.35 wt%), penetration enhancer (azone, isopropyl palmitate, isopropyl myristate, 3 wt%) and ethanol were mixed, and after all dissolved, the remaining amount of pressure-sensitive adhesive was added. 87-4098 and 87-2510 (4:1) mixture was stirred for 1 hour, allowed to stand for 0.5 hour to remove air bubbles, and then coated with Scotchpak TM 9744 was coated with 0.35 mm, placed at room temperature for 10 min, and then dried in an oven at 50°C for 5 min. Cotran backing layer was used to cover the TM 9733, 65-70 μm patches were selected for transdermal administration test.
[0088] The results showed that Azone had the strongest effect on drug penetration, with a percutaneous penetration of 220.3±11.5μg / cm 2 about.
[0089] 6. Screening of the amount of Azone added
[0090] Mix 3 wt% of tulobuterol API, stabilizer maleic acid (0.35 wt%), ethanol and permeation enhancer azone, and add the remaining pressure-sensitive adhesive after all are dissolved. 87-4098 and 87-2510 (4:1) mixture was stirred for 1 hour, allowed to stand for 0.5 hour to remove air bubbles, and coated on the anti-sticking layer Scotchpak with a thickness of 0.35 mm. TM 9744, placed at room temperature for 10 minutes, and then dried in an oven at 50°C for 5 minutes. Cover with backing layer CotranTM 9733. Patches of 65 to 70 μm were prepared and tested for transdermal administration on isolated rat skin.
[0091] The experimental results are shown in Table 6. The results show that azone has a good penetration-promoting effect on tulobuterol, and azone, which accounts for about 5% by weight of the pressure-sensitive adhesive layer, can achieve the same penetration amount as the commercially available product. Therefore, in the patch of the present invention, the content range of the penetration enhancer is not less than 5% by weight, preferably not less than 4% by weight.
[0092] Table 6 Screening of Azone Addition Amount
[0093]
[0094]
[0095] 7. Investigation of adhesive enhancers for patches
[0096] According to the prescription in Table 6, pressure-sensitive adhesives containing different proportions were prepared. 87-4098 and A transdermal patch of a mixture of 87-2510.
[0097] According to the adhesion test method of General Chapter 0952 of the 2020 edition of the Chinese Pharmacopoeia, the initial adhesion, sustained adhesion and peel strength of the above three patches were measured, and the results are shown in Table 7. The results show that: 87-4098 and The patch with the mixture of 87-2510 (4:1) had better adhesion.
[0098] Table 6:
[0099]
[0100] Table 7:
[0101] Initial adhesion (ball number) Holding force (h) Peel strength (kN / m) Patch 1 7 3.45 0.35 Patch 2 6 7.32 0.46 Patch 3 5 10.95 0.68
[0102] Based on the above adhesion test data, the prescription with a mixing ratio of 4098:2510 of pressure-sensitive adhesive of 4:1 was selected as the most preferred mixing ratio.
[0103] The protection content of the present invention is not limited to the above embodiments. Without departing from the spirit and scope of the inventive concept, changes and substitutions that can be thought of by those skilled in the art are included in the present invention, and the protection scope is defined by the attached claims.
Claims
1. A tulobuterol transdermal patch comprising a pressure-sensitive adhesive layer and a backing layer, characterized in that: The pressure-sensitive adhesive layer comprises a pressure-sensitive adhesive and an active ingredient, wherein the active ingredient is tulobuterol or a pharmaceutically acceptable salt thereof, and the pressure-sensitive adhesive comprises a mixture of copolymer A and copolymer B, wherein copolymer A is a copolymer of vinyl acetate and isooctyl acrylate, and copolymer B is a copolymer of 2-ethylhexyl acrylate, 2-hydroxyethyl acrylate and methyl acrylate, wherein the content of the active ingredient in the pressure-sensitive adhesive layer is 1.5 wt % to 5 wt %; The pressure-sensitive adhesive is a mixture of copolymer A and copolymer B in a weight ratio of 4:1; The patch also contains azone, a penetration enhancer, the content of which accounts for 4% to 8% by weight of the pressure-sensitive adhesive layer; The patch also contains maleic acid as a stabilizer, and the content of the stabilizer in the pressure-sensitive adhesive layer is 0.3 wt % to 0.6 wt %; In the copolymer A, the weight ratio of vinyl acetate to isooctyl acrylate is 1:2 to 2:1; In the copolymer B, the content of 2-ethylhexyl acrylate is 67-77% by weight, the content of 2-hydroxyethyl acrylate is 3-7% by weight, and the content of methyl acrylate is 20-26% by weight; The backing layer is a polyester and ethylene-vinyl acetate copolymer film.
2. The tulobuterol transdermal patch according to claim 1, further comprising an anti-adhesive layer, wherein the anti-adhesive layer is a polyethylene terephthalate film containing a fluoride coating.
3. The tulobuterol transdermal patch according to claim 1, wherein the thickness of the pressure-sensitive adhesive layer is 65 to 70 μm.
4. The method for preparing a tulobuterol transdermal patch according to any one of claims 1 to 3, comprising preparing a solution of tulobuterol bulk drug or a pharmaceutically acceptable salt thereof, maleic acid and azone, uniformly mixing the solution with a pressure-sensitive adhesive, coating the solution on a release layer, heating and drying the solution, adding a backing layer, and uniformly applying pressure to obtain a transdermal patch.