Cracked reinforced concrete bridge bearing capacity evaluation method

By using a tapping-scanning bridge inspection vehicle and short-time Fourier transform technology, the stiffness ratio and ultimate bending moment of reinforced concrete bridges are calculated, solving the problem of bridge load-bearing capacity assessment that relies on experience-based judgment in existing technologies, and achieving higher accuracy and lower cost assessment.

CN118194580BActive Publication Date: 2026-11-10CCCC INFRASTRUCTURE MAINTENANCE GRP CO LTD +2
View PDF 2 Cites -1 Cited by

Patent Information

Application Number
CN202410393731.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-02
Publication Date
2026-11-10
Estimated Expiration
2044-04-02

Smart Images

  • Figure CN118194580B_ABST
    Figure CN118194580B_ABST
Patent Text Reader

Abstract

The application discloses a bearing capacity evaluation method for a common reinforced concrete bridge with cracks, and when the acting bending moment is greater than the cracking bending moment, an expression of a strain unevenness coefficient is obtained, an expression of short-term stiffness of the concrete beam with cracks is obtained according to the expression of the strain unevenness coefficient, the sectional area of the steel bar is obtained according to the short-term stiffness, the ultimate bending moment is obtained according to the sectional area of the steel bar, and the residual bearing capacity of the concrete bridge is evaluated according to the ultimate bending moment. The parameters used in the application are obtained by field measurement, so that the influence of artificial experience on the bearing capacity evaluation of the concrete bridge is greatly reduced, the reliability is improved, the evaluation process is reduced, and the evaluation cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of bridge inspection technology, and in particular to a method for assessing the load-bearing capacity of ordinary reinforced concrete bridges with cracks. Background Technology

[0002] The main standards related to bridge assessment in my country are: (1) Highway Bridge and Culvert Maintenance Specifications (JTG)

[0003] 5120-2021 provides general provisions for bridge inspection, evaluation and maintenance. (2) The Technical Condition Evaluation Standard for Highway Bridges JTG / T H21-2011 incorporates the Highway Bridge and Culvert Maintenance Specifications JTG

[0004] Section 3.5 of "5120-2021" further refines the content of bridge assessment. (3) "Specifications for Testing and Evaluation of Bearing Capacity of Highway Bridges JTG / T J21-2011" specifies special inspection methods and references the bearing capacity calculation methods specified in the design specifications. The standards for urban bridges are similar.

[0005] Table 1 Existing Bridge Inspection Methods

[0006]

[0007] Referring to Table 1, in current routine bridge assessment work, the above three standards are often used in combination. For details on their relationships, please refer to [link / reference needed]. Figure 1 .

[0008] In summary, both the assessment of bridge technical condition and the calculation of load-bearing capacity rely heavily on experience-based scoring scales, which are highly subjective. While health monitoring systems can achieve real-time monitoring, their accuracy in detecting localized damage is low, and they cannot yet provide a reliable evaluation of bridge load-bearing capacity. Load testing is currently the only method that can accurately evaluate the actual load-bearing capacity of a bridge, but it requires traffic closure and is extremely expensive. Therefore, efforts have been made to develop other simple and reliable supplementary methods.

[0009] The Manual for Bridge Evaluation specifies the evaluation methods for old bridges in the United States. Although it is more detailed, its basic framework is similar to that of Chinese standards.

[0010] For ordinary reinforced concrete bridges with cracks, the actual load-bearing capacity often differs significantly from the design capacity due to construction errors, subsequent damage, and other factors. Statistical results from full-scale structural failure tests show that, because the design is conservative, the actual load-bearing capacity of the damaged structure is often greater than the design capacity. Since geometric dimensions, material parameters, and boundary conditions are difficult to accurately determine, obtaining the true load-bearing capacity through calculation and analysis (i.e., verification methods) is often extremely challenging. Summary of the Invention

[0011] To address the limitations and defects of existing technologies, this invention provides a method for assessing the load-bearing capacity of ordinary reinforced concrete bridges with cracks, comprising:

[0012] Obtain the acceleration of the tapping and scanning bridge inspection vehicle;

[0013] The weighted stiffness ratio θ is obtained based on the expression for acceleration and the short-time Fourier transform. W The expression;

[0014] According to the weighted stiffness ratio θ W The expression and the stiffness ratio θ are obtained by considering the adjacent moving windows containing damage. m ;

[0015] Estimate the short-term stiffness B of the complete beam based on design standards and drawings. s0 To obtain the short-term stiffness B of the damaged beam s =B s0 θ m ;

[0016] When the applied bending moment is greater than the cracking bending moment, the strain non-uniformity coefficient is obtained. The expression is as follows:

[0017]

[0018] Among them, f ct It is the axial tensile strength of concrete, M s1 A is the bending moment generated at this section by the permanent load. t η is the effective tensile concrete cross-sectional area, η is the equivalent internal force arm coefficient of the crack section, and h0 is the effective height.

[0019] The expression for obtaining the short-term stiffness of a cracked concrete beam is as follows:

[0020]

[0021] Among them, the structural verification coefficient ζ includes the equivalent internal force arm coefficient η of the crack section and the strain non-uniformity coefficient. The ratio of the tensile and compressive elastic moduli of concrete, the influence coefficient of the converted parameters of compressive concrete, γ' is the ratio of the area of ​​the compression flange to the effective area of ​​the web, E s and A s These are the elastic modulus and cross-sectional area of ​​ordinary steel bars in the tension zone, respectively. The reinforcement ratio ρ is equivalent to the cross-sectional area A of the prestressed steel bars. p ;

[0022] According to the short-term stiffness B s Obtain the cross-sectional area A of the prestressed steel bars p And the cross-sectional area A of ordinary steel bars s ;

[0023] When the height of the compression zone is not less than the distance from the resultant point of the compression zone reinforcement to the upper edge, the ultimate bending moment M u The expression is as follows:

[0024]

[0025] Where, x=(f s A s +f p A p -f s 'A s ′) / f c b f γ0 is the structural importance coefficient;

[0026] When the height of the compression zone is less than the distance from the resultant point of the compression zone reinforcement to the upper edge, the ultimate bending moment M u The expression is as follows:

[0027]

[0028] Wherein, γ0 is the structural importance coefficient;

[0029] According to the ultimate bending moment M u Assess the remaining load-bearing capacity of the concrete bridge.

[0030] Optionally, the step of obtaining the expression for the acceleration of the impact-scanning bridge inspection vehicle includes:

[0031] Obtain the acceleration of the tapping and scanning bridge inspection vehicle

[0032] Optionally, the weighted stiffness ratio θ is obtained based on the expression for the acceleration and the short-time Fourier transform. W The steps of the expression include:

[0033] The weighted stiffness ratio θ is obtained based on the expression for acceleration and the short-time Fourier transform. W The expression is as follows:

[0034]

[0035] Among them, the coefficients U, V, and W are related to the tapping frequency and the characteristics of the tapping scanning bridge inspection vehicle, and are obtained through a preset test.

[0036] Optionally, the step of adjusting the weighted stiffness ratio θ W The expression and the stiffness ratio θ are obtained by considering the adjacent moving windows containing damage. m The steps include:

[0037] The stiffness at non-abrupt locations is the baseline value (EI) 0 and is uniformly distributed, while the stiffness at abrupt changes is (EI). d Eight window units constitute a time period. When the overlap rate of adjacent moving windows in the short-time Fourier transform is (1-1 / 8), abrupt stiffness is set to occupy one unit, and the stiffness of the remaining seven units is the reference value (EI)0. The weighted stiffness ratio θ is then used to determine the optimal stiffness. W The expression and adjacent moving windows containing damage are used to obtain the stiffness ratio θ. m The expression is as follows:

[0038]

[0039] Where, N s Let s represent the actual position of the abrupt stiffness within the moving window, where s is the sequence number of the moving window, and the window function is the same as that used in the short-time Fourier transform. For Haiming Window.

[0040] Optionally, the lateral load distribution coefficient of the multi-section T-beam containing diaphragms is calculated using the hinged plate method. The loading mode of the T-beam results in the following distribution of deflection and internal force along the length x direction:

[0041]

[0042] Among them, w i For deflection, M i For bending moment, Q i For shear force, p i For the equivalent lateral load, C is a constant, and the magnitude distribution of p is the lateral load distribution between the beams;

[0043] The corresponding expression obtained based on the deformation compatibility conditions is as follows:

[0044]

[0045] in, It is the vertical deflection of the main beam under unit load. It is the vertical deflection caused by the unit shear force. It is the vertical deflection of the flange under unit shear force, vertical deflection. Vertical deflection and vertical deflection The expression is as follows:

[0046]

[0047] Where L is the beam length, EI is the bending stiffness, GJ is the torsional stiffness, and b1 is the beam width. For functions related to the load form and boundary conditions, I1 is the longitudinal bending moment of inertia per unit plate width with the longitudinal direction of the beam as the principal axis, and d1 is the cross-sectional geometric parameter;

[0048] The expression for the lateral load distribution of the T-beam is as follows:

[0049]

[0050] Set the deflection w downwards as positive, and the rotation angle... Counterclockwise is positive, g i (x) represents the distributed hinge force;

[0051] When the distributed load p(x) acts on i p When the center of beam is 0 < x < a, a + b < x < l, the expression is as follows:

[0052] For beam number one: For i (i = 2, 3, ..., n) T Beam No. -1:

[0053] For i p Beam number:

[0054] For n T Beam number:

[0055] When the deflection on both sides of the hinge is the same, the expression is as follows:

[0056]

[0057] When the distributed load p(x) acts on i p At the center of beam , when a≤x≤a+b, the hinge joint does not transmit shear force, and the displacements on both sides of the connection point are different, yielding the following expression:

[0058] For i p -1 Beam:

[0059] For i p Beam number:

[0060] For i p Beam No. 1:

[0061] Wherein, δ is used to determine whether it is a unilateral injury or a bilateral injury. If it is a unilateral injury, δ = 1; if it is a bilateral injury, δ = 0.

[0062] When the distributed load p(x) acts on i p When the center of beam X is x = 0 and x = l, the expression for the boundary conditions is as follows:

[0063]

[0064] The deflection and rotation angle of the T-beam are expanded into a series, substituted into the above expression, and the coefficients in the series expansion are solved using the method of undetermined coefficients. The above expression is used to describe the deformation law of the multi-piece T-beam model.

[0065] Optional, also includes:

[0066] Select the location of the cross-section, calculate the deflection of the intermediate beam of the cross-section, compare the deflection of the intermediate beam of the cross-section with the deflection of the intermediate beam without considering damage, and evaluate the deflection change of the cross-section caused by transverse connection damage. According to the transverse distribution theory, the ratio of deflections is the ratio of actual load, as expressed below:

[0067]

[0068] Among them, w c For the deflection of a specific section of the intermediate beam without lateral connection damage, w d p is the deflection of a specific section of the damaged intermediate beam. c p represents the equivalent load without lateral connection damage. d Indicates the equivalent load that causes damage;

[0069] The relative change of the equivalent load is obtained from expression (24).

[0070] Based on the relationship between stiffness and bearing capacity, the stiffness loss of the equivalent load is calculated, and it is determined that the increase in the load factor leads to a decrease in the equivalent bearing capacity. The expression is as follows:

[0071]

[0072] in, and These represent the load-bearing capacity with and without damage, respectively, utilizing the relative changes in load-bearing capacity. Inverse calculation of the relative change in stiffness caused by transverse connection damage

[0073] Optional, also includes:

[0074] Let the lateral load factor be g0, and the corresponding lateral factor of the equivalent single beam model be g. td According to expression (35), the relative change value of the equivalent ultimate bending moment is 1-g. td / g0, the corresponding relative change in stiffness is obtained through the reverse process. Obtain the stiffness (EI) of the intact beam with good transverse connections. t0 Stiffness (EI) of a single, undamaged beam b0 The relationship expression is as follows:

[0075]

[0076] When the lateral connections are undamaged but the main beam is damaged, the stiffness of the damaged main beam in the equivalent single-beam model is (EI). d The stiffness (EI) of a single, undamaged beam is obtained. b0 stiffness ratio as a reference The stiffness (EI) of the overall model where the lateral connections are undamaged but the main beam is damaged. td The stiffness (EI) of the corresponding equivalent single beam model. d The relationship is in For relative changes in stiffness, according to and The expression obtained is as follows:

[0077]

[0078] When the transverse connection is damaged but the main beam is undamaged, the measured θ m Characterized as transverse connectivity damage θ mt ;

[0079] When there is localized damage to the transverse connection and localized damage to the main beam, the stiffness is set to (EI). td The relative change in stiffness is The expression obtained is as follows:

[0080]

[0081]

[0082] When the transverse connection has overall damage and the main beam has overall damage, according to (EI) t0 Solve for the equivalent stiffness (EI) of the transversely connected damaged joint. t1 The relative change in stiffness is obtained as follows In expression (37) Replace with Perform the calculation.

[0083] The present invention has the following beneficial effects:

[0084] This invention provides a method for assessing the load-bearing capacity of ordinary reinforced concrete bridges with cracks. When the applied bending moment exceeds the cracking bending moment, an expression for the strain non-uniformity coefficient is obtained. Based on the expression for the strain non-uniformity coefficient, an expression for the short-term stiffness of the cracked concrete beam is derived. The cross-sectional area of ​​the reinforcing steel is obtained from the short-term stiffness, and the ultimate bending moment is obtained from the cross-sectional area of ​​the reinforcing steel. The remaining load-bearing capacity of the concrete bridge is then assessed based on the ultimate bending moment. The parameters used in this invention are obtained from on-site measurements, significantly reducing the influence of human experience on the assessment of the load-bearing capacity of concrete bridges, improving reliability, reducing the assessment process, and lowering assessment costs. Attached Figure Description

[0085] Figure 1 This is a schematic diagram of the existing highway bridge evaluation standard system.

[0086] Figure 2 This is a schematic diagram of the load-deflection curve of a flexural concrete beam provided in Embodiment 1 of the present invention.

[0087] Figure 3 This is a normalized Hamming window schematic diagram provided in Embodiment 1 of the present invention.

[0088] Figure 4a This is a schematic diagram of variable calculation provided in Embodiment 1 of the present invention.

[0089] Figure 4b This is another schematic diagram of variable calculation provided in Embodiment 1 of the present invention.

[0090] Figure 5 This is a schematic diagram of the load-bearing capacity assessment process provided in Embodiment 1 of the present invention.

[0091] Figure 6 This is a schematic diagram of the internal forces and deformations of a T-beam provided in Embodiment 1 of the present invention.

[0092] Figure 7 This is a schematic diagram of transverse connection damage provided in Embodiment 1 of the present invention.

[0093] Figure 8 This is a schematic diagram of the load-bearing capacity assessment process considering lateral connections provided in Embodiment 1 of the present invention. Detailed Implementation

[0094] To enable those skilled in the art to better understand the technical solution of the present invention, the method for evaluating the load-bearing capacity of ordinary reinforced concrete bridges with cracks provided by the present invention will be described in detail below with reference to the accompanying drawings.

[0095] Example 1

[0096] 1.1 Bridge Evaluation Standards

[0097] Assessing the actual load-bearing capacity of a bridge is essentially an inverse problem. The key to solving this inverse problem is using the correct model and reliably measuring the parameters within that model. The following will explain how the tapping scan method can detect the rate of change of the bending stiffness of a bridge section, from which the equivalent reinforcement ratio can be derived. This allows for the development of appropriate and reasonable load-bearing capacity assessment methods for small- to medium-span concrete bridges, in conjunction with current standards.

[0098] The design specifications for assessing the load-bearing capacity of bridges under long-term conditions (service phase) include two aspects:

[0099] (1) Ultimate limit state of bearing capacity: mainly examines strength and stability;

[0100] (2) Normal service limit state: mainly examines stiffness and crack resistance.

[0101] After obtaining the bridge's technical, material, and frequency conditions, the load-bearing capacity assessment scale is calculated using the following formula:

[0102]

[0103] Among them: the assessment scale D1 for the defect status is the technical condition level of the bridge, with a weight α1 = 0.4; the assessment scale D2 for the material strength is determined based on the measured value of the concrete strength and Table 5.3.5 of the specification, with a weight α1 = 0.3; the assessment scale D3 for the natural frequency is determined based on the ratio of the measured value (through dynamic load test) and the calculated value of the bridge's natural frequency, referring to Table 5.9.2 of the specification, with a weight α1 = 0.3.

[0104] After obtaining the verification and evaluation scale, the ultimate bearing capacity of reinforced concrete bridges is evaluated using the following formula:

[0105] γ0S≤R(f d ,ξ c α dc ,ξ s α ds )Z1(1-ξ e (2)

[0106] Wherein, γ0 is the structural importance coefficient, as specified in Section 4.1.5 of the standard;

[0107] S is the load effect function, specified in Section 4.1.5 of the code, and can be adjusted according to actual conditions using the live load correction factor ξ specified in Section 7.7.7 of the code. q Make corrections;

[0108] R is the resistance effect function, as specified in Chapter 5 of the standard;

[0109] f d It is the design value of material strength;

[0110] α dc These are the geometric parameters of concrete;

[0111] α ds These are the geometric parameters of the reinforcing bars;

[0112] Z1 is the bearing capacity verification coefficient, which can be found in Table 7.7.1-2 of the code based on the D value;

[0113] ξ e It is the load-bearing capacity deterioration coefficient, which can be found in section 7.7.4 of the specification based on the material testing results;

[0114] ξ c It is the reduction factor for concrete section, which can be found in section 7.7.5 of the specification based on the results of visual inspection;

[0115] ξ s It is the reduction factor for the steel reinforcement section, which can be found in section 7.7.6 of the specification based on the visual inspection results.

[0116] In formula (2), the verification coefficient Z1 and the reduction coefficient in the resistance effect function R contain empirical data from manual scoring. They need to be judged and estimated by experts based on the actual situation of the bridge, and may differ from the actual situation. When the bridge's load-bearing capacity cannot be determined by formula (2), it needs to be evaluated through static load tests.

[0117] In static load tests, the efficiency calculated according to the following formula should be between 0.95 and 1.05:

[0118]

[0119] Among them, S s S' is the maximum calculated value of internal force, stress, or deformation of the control section corresponding to a certain loading test item (see Table 8.1.3 in the specification); S' is the most unfavorable calculated value of internal force, stress, or deformation of the control section caused by the check load; μ is the impact coefficient, as specified in Section 4.3.2 of the specification.

[0120] In static load tests, a bridge's load-bearing capacity is deemed insufficient if any of the following conditions are met:

[0121] (1) The structural verification coefficient ζ of the main measuring points is greater than 1.

[0122]

[0123] Among them, S eS represents the measured value of displacement or strain. s These are the calculated values ​​for displacement or strain.

[0124] (2) The equivalent residual displacement or strain at the main measuring points exceeds 20%.

[0125]

[0126] Among them, S P S represents the measured value of residual displacement or residual strain. t This refers to the measured total displacement or total strain under the test load.

[0127] (3) The crack width exceeds the specification in Table 7.3.4, and the crack closure width after unloading is less than 2 / 3 of the width of the crack.

[0128] (4) The bridge foundation experienced unstable settlement and deformation.

[0129] When the bearing capacity of a bridge is determined to be insufficient according to the above-mentioned regulations, the check coefficient Z2 can be determined according to the maximum value of the displacement check coefficient and the strain check coefficient, as specified in Table 8.3.2 of the regulations, to replace Z1 in formula (2) for recalculation. If the ratio of the action effect to the resistance effect is less than 1.05, the bearing capacity of the bridge meets the requirements; otherwise, it can be determined that the bearing capacity of the bridge is insufficient.

[0130] 1.2 Bearing capacity assessment based on cross-sectional stiffness

[0131] This embodiment assesses the change in the load-bearing capacity of a concrete beam by measuring the change in its ultimate bending moment. The ultimate bending moment depends on the beam's cross-sectional geometry, material parameters, and the equivalent cross-sectional area of ​​the reinforcing steel. The equivalent cross-sectional area of ​​the reinforcing steel reflects its stress state and significantly affects the beam's load-bearing capacity. Based on the relationship between short-term bending stiffness and the equivalent cross-sectional area of ​​the reinforcing steel in the design code, changes in the short-term bending stiffness of the cross-section can be converted into changes in the equivalent cross-sectional area of ​​the reinforcing steel. Therefore, the change in the beam's ultimate bending moment can be inverted using the beam cross-sectional bending stiffness ratio detected by the tapping scan method. Compared to the existing load-bearing capacity calculation methods in the code described in Section 1.1, this method uses parameters obtained from field measurements, thus greatly reducing the influence of human experience on load-bearing capacity assessment and theoretically should be more reliable.

[0132] The impact of damage on beam section stiffness is obvious. Ren Baoshuang et al. introduced the bond coefficient of steel reinforcement to correct the strain non-uniformity coefficient of tensile reinforcement, thereby estimating the impact of damage on short-term stiffness. He Shuanhai et al. developed a series of methods to estimate the nominal reinforcement ratio of actual RC bridges and further evaluate the bridge's load-bearing capacity. The basic idea is to obtain the flexural stiffness of the section through crack statistical characteristics, static tests, or dynamic tests, thereby inverting the nominal reinforcement ratio. Gu Xianglin et al. also derived an estimation formula for the flexural stiffness of the RC beam section from cracking to longitudinal steel yielding, finding that stiffness is related to the concrete strength grade and reinforcement ratio. This makes it possible to find the relationship between section stiffness and ultimate bearing capacity.

[0133] The above analysis mainly focuses on RC bridges (ordinary reinforced concrete bridges). For PC bridges (prestressed concrete bridges), He Shuanhai et al. also developed a method for estimating section stiffness based on statistical characteristics of cracks, combined with the finite element method to calculate bearing capacity. In fact, compared to RC beams, prestressing only increases the cracking moment (i.e., adds a stress-relieving moment), ensuring the beam does not crack during normal service (full prestressing and partial prestressing of type A) or has very small cracks (partial prestressing of type B), thus fully utilizing the performance of concrete and high-strength steel, saving materials, and reducing self-weight. However, the stress state of PC beams at failure is similar to that of RC beams, and the calculation methods are basically the same, so their ultimate bearing capacity does not change. That is, prestressing "cannot create miracles beyond the inherent strength of the material itself." This actually follows the basic mechanical principle: ultimate bearing capacity is related to the equilibrium state of the structure under load, and prestressing is self-equilibrium, so it does not affect the ultimate bearing capacity of the structure. Furthermore, the pretension in prestressed steel cables is usually less than 10... 7 The prestress generated in the concrete, N, is still a small amount compared to the elastic modulus of the concrete, so the stress stiffening / softening effect caused by prestress can be ignored. Therefore, the stiffness of the PC beam under undamaged conditions is basically the stiffness of the concrete section (due to the very low reinforcement ratio, the contribution of the steel bars to the stiffness is very small). If the section stiffness of the PC beam changes, it indicates that significant damage has occurred. In this case, the ultimate bearing capacity can still be assessed by inverting the equivalent cross-sectional area (or reinforcement ratio) of the steel bars.

[0134] like Figure 2As shown, the stiffness of the reinforced concrete beam is divided into three stages. Before cracking (Stage I), the stiffness is at its maximum and remains constant. After cracking (Stage II), the tensile concrete gradually loses its load-bearing capacity, leading to a continuous decrease in stiffness. When the tensile reinforcement yields (Stage III), the stiffness continues to decrease and quickly reaches the ultimate limit state. The damage in Stage I is very minor and can be ignored. Stage III is very close to the ultimate bearing state, which is unacceptable in practice. Therefore, damage assessment only focuses on Stage II.

[0135] In static load tests, the bearing capacity is judged based on the ratio between the measured and design values ​​of the displacement or strain of the main control section (see formula (4)). Displacement reflects the overall structural characteristics of the bridge, while strain reflects the stiffness level of the section. Since the load test adopts a step-by-step loading mode, the structural performance can be reflected by the varying trends of the measured and design values ​​of the displacement or strain of the main control section with different loads. This embodiment mainly analyzes the influence of section bending stiffness on the load-strain curve. Compared to an undamaged section, a damaged section has lower stiffness; therefore, when the load applied in the load test is... Figure 2 In Stage I, the load-strain curve of the damaged section has a smaller slope. The decrease in the beam's load-bearing capacity means that the beam can enter Stage II under lower loads. Therefore, as the load in the load test increases stepwise, compared to the undamaged section, the intersection of Stage I and Stage II in the load-strain curve of the damaged section will appear at lower loads, making the nonlinear characteristics of the curve easier to observe in actual measurements. When the load in the load test continues to increase to Stage III, the high stress distribution of the concrete leads to its plastic behavior at lower loads, and the nonlinear characteristics of the curve become more pronounced.

[0136] Therefore, by analyzing the strain variation trend of the main control sections in the load test with the load, the bearing capacity assessment method of this embodiment can be compared with the data from the load test. Compared with the undamaged beam, the nonlinear characteristics in the load-strain curve of the damaged beam, which has a weaker bearing capacity, begin to appear at lower loads.

[0137] 2.1 Relationship between ultimate bending moment and cross-sectional area of ​​reinforcing steel

[0138] Considering a prestressed concrete T-beam with longitudinal internal reinforcement in both the compression and tension zones, according to the provisions of clauses 5.2.2 to 5.2.4 in the code, its ultimate bending moment M u The calculation method depends on the height of the compression zone. The stress mode of the reinforcing bars depends on their position in the equivalent section.

[0139] When the sum of the bearing capacity of the concrete in the flange zone and the reinforcement in the compression zone of a T-section is not less than the bearing capacity of the reinforcement in the tension zone, the height of the compression zone is calculated as a rectangular section. When the height of the compression zone is not less than the distance from the resultant point of the compression reinforcement to the upper edge, the ultimate bending moment is calculated according to 5.2.2-1; otherwise, it should be calculated according to 5.2.4-1 or 5.2.4-2. When only ordinary reinforcement is used in the compression zone, the calculation formula according to 5.2.2-1 is as follows:

[0140]

[0141] Where, x=(f s A s +f p A p -f s 'A s ′) / f c b f The definition of the correlation coefficient can be found in the specification.

[0142] The calculation formula according to 5.2.4-2 is as follows:

[0143]

[0144] As can be seen, the above formulas all explicitly include the cross-sectional area of ​​the reinforcing bars.

[0145] When the sum of the bearing capacity of the concrete in the flange zone and the reinforcement in the compression zone of a T-section is less than the bearing capacity of the reinforcement in the tension zone, the height of the compression zone is calculated according to the T-section. In this case, the geometric parameters of the web need to be considered. The positional relationship between the height of the compression zone and the resultant force point of the reinforcement in the compression zone also needs to be considered. The calculation method for the ultimate bending moment is similar to that for a rectangular section.

[0146] With fixed geometric parameters of the concrete section, M u The strength of the concrete and reinforcing steel, as well as the cross-sectional area of ​​the steel reinforcement, are determined. When cracks, voids, or other damage occur in the substructure of a bridge, if the condition of the reinforcing steel remains unchanged, then M... u The condition itself remains unchanged. However, this damage can potentially cause corrosion of the reinforcing steel or reduce the bond strength between the steel and concrete, thereby reducing M. u Since the strength parameters typically change little, the damage can be equated to a change in the cross-sectional area of ​​the reinforcing steel.

[0147] In fact, the ultimate bearing capacity formulas in the specifications are all derived based on the plane section assumption. This assumption holds true when the reinforcing steel and concrete in the non-cracked section are tightly bonded together, thus providing a constraint that makes the cracked section approximately a plane after deformation under load. If corrosion, longitudinal cracking, or other reasons reduce the bond strength between the reinforcing steel and concrete, then the plane section assumption cannot be guaranteed. In this case, the plane section assumption is still used, but the effect of this damage is converted into a change in the cross-sectional area of ​​the reinforcing steel, which is a simple (compared to analysis using a complex finite element model) equivalent treatment method. Furthermore, in actual analysis, it is generally assumed that the geometry of the beam does not change, so the cross-sectional area of ​​the reinforcing steel can also be expressed using the reinforcement ratio ρ.

[0148] It is evident that, based on the appropriate relationship between the bending stiffness of the cross-section and the cross-sectional area of ​​the reinforcing bar, the cross-sectional area of ​​the reinforcing bar can be derived, and the measured value can be used to determine this value. c The ultimate bearing capacity can be estimated using the corresponding formulas in the specifications. However, existing methods for obtaining the flexural stiffness of a bridge section either rely on empirical estimation, static or dynamic tests, or even finite element models. The advantage of the impact-scan method is that it can directly obtain the change in the flexural stiffness of the bridge section.

[0149] Based on the above analysis, a new rapid bridge load-bearing capacity assessment method can indeed be developed based on the impact scanning damage detection method, minimizing reliance on empirical parameters and avoiding expensive load tests and cumbersome finite element calculations. Compared with the verification method in the code, this new method is equivalent to directly determining the concrete section reduction factor ξ in formula (2). c Reduction factor for steel reinforcement section ξ s And the bearing capacity verification coefficient Z1. The bearing capacity deterioration coefficient ξ in formula (2) e It is a prediction of the bridge's quality deterioration within the time remaining until the next inspection, which can still be determined according to Section 7.7.4 of the regulations, or by extrapolating from historical inspection data.

[0150] 2.2 Relationship between equivalent cross-sectional area and stiffness of reinforcing bars

[0151] Since the cracking of prestressed concrete beams affects the variation of their short-term stiffness, it is necessary to first calculate the cracking moment. According to the code, the expression for the cracking moment is:

[0152] M cr =(σ pc +γf tk )W0 (8)

[0153] Where, σ pc It is the prestressing stress in the concrete generated at the edge by the prestressing force, γ is the plastic influence coefficient of the section modulus of the concrete, and ftk It is the standard value of the axial tensile strength of concrete. I0 is the elastic modulus of the tension edge of the equivalent section, I0 is the equivalent moment of inertia of the section (calculated for the entire section), x0 is the height of the compression zone, and h is the section height.

[0154] σ in formula (8) pc This significantly affects the magnitude of the cracking moment. According to the code, the calculation method for short-term stiffness differs when the relationship between the cracking moment and the applied moment is different.

[0155] (1) σ in the cracking bending moment pc Dominant, the applied bending moment is less than the cracking bending moment.

[0156] According to Clause 7.2.3 of the standard, the short-term stiffness B s The calculation formula is:

[0157] B s =0.95E c I0 (9)

[0158] Among them, E c I0 is the elastic modulus of concrete. The formula for calculating I0 is:

[0159]

[0160] in, b, h, b f h f All are cross-sectional geometric parameters. A pi h pi Let A be the area and height of the prestressed steel reinforcement at the i-th cross-section. si h si Let α be the area and height of the ordinary reinforcing steel at the i-th cross-section. p and α s These are the ratios of the elastic modulus of prestressed steel bars and ordinary steel bars to concrete, respectively. For the sum of the cross-sectional areas of the prestressed steel bars, It is the sum of the cross-sectional areas of ordinary steel bars.

[0161] Since the cross-sectional area of ​​the steel reinforcement differs from that of the concrete by at least two orders of magnitude, and the ratio of the elastic modulus of the steel reinforcement to that of the concrete is usually less than 10, it can be seen from formula (10) that the cross-sectional area of ​​the steel reinforcement accounts for a very small proportion of I0. With other parameters remaining constant, a small change in I0 will result in a large change in the cross-sectional area of ​​the steel reinforcement. Therefore, the short-term stiffness in formula (9) is less sensitive to changes in the equivalent cross-sectional area of ​​the steel reinforcement; thus, a small change in stiffness will lead to a large change in the reinforcement ratio, thereby causing a significant change in the bearing capacity.

[0162] (2)σ pc The bending moment is smaller than the cracking bending moment.

[0163] At this stage, the concrete beam still approximately satisfies the plane section assumption. However, the strain of both the tensile reinforcement and the compressive concrete in the cracked concrete beam is non-uniform; therefore, strain non-uniformity coefficients are introduced separately. and This is used to characterize the ratio of the average strain of the entire beam to the strain at the crack section under quasi-permanent load. Based on experimental data, we can obtain... Empirical formula:

[0164]

[0165] Among them, f ct It is the axial tensile strength of concrete; M s1 It is the bending moment generated at this section by the permanent load; A t η is the effective tensile concrete cross-sectional area; η is the equivalent internal force arm coefficient of the crack section; h0 is the effective height.

[0166] Based on the plane section assumption and empirical formulas based on experimental data, the formula for calculating the short-term stiffness of cracked concrete beams can be obtained:

[0167]

[0168] Among them, ζ includes η, The influence of the ratio of tensile to compressive elastic modulus of concrete and the equivalent parameters of compressive concrete; while γ' is the ratio of the area of ​​the compression flange to the effective area of ​​the web; E s and A s These are the elastic modulus and cross-sectional area of ​​ordinary steel reinforcement in the tension zone, respectively. From formula (12), it can be seen that B... s It incorporates the effects of geometry, tensile reinforcement, concrete material properties, and reinforcement ratio ρ, and decreases with increasing load. Because it uses many empirical formulas based on measured data, it generally agrees well with actual measurements.

[0169] Another approach to calculating short-term stiffness under cracking conditions is to decompose the cracked zone of length l into an overall cross-sectional segment of length α1l and a cracked cross-sectional segment of length α2l, where the coefficients are determined based on experimental data.

[0170] The standard uses formula (12) to calculate the short-term stiffness of RC beams; for PC beams, it still uses... Figure 2 Based on the bilinear assumption and experimental data, the following calculation method is given:

[0171]

[0172] Among them, M sThe bending moment under combined action, A p and A s γ represents the cross-sectional area of ​​prestressed steel bars and ordinary steel bars in the tension zone, respectively. f is the ratio of the cross-sectional area of ​​the tension flange to the effective area of ​​the web, b is the width of the web, and h0 is the effective height of the cross-section.

[0173] Compared to the case without cracking, the stiffness becomes more sensitive to changes in the area of ​​the reinforcing bars. Substituting the expression for the cracking moment into formula (13), we get:

[0174]

[0175] Since x0 and I0 are less affected by the reinforcement ratio, B s Mainly composed of A explicitly included in the above formula p and A s The terms and σ pc Dominant. Based on calculation and analysis, and Since they are of the same order of magnitude, the terms in the denominator of the above equation can be combined, and because... Much greater than 1, therefore approximately satisfying B s ∝(A p +A s ).

[0176] 2.3 Inversion of True Stiffness Ratio

[0177] Based on our derivation of the sensitivity of the impact-scanning damage method for damaged bridges, the acceleration of the impact-scanning bridge inspection vehicle is:

[0178]

[0179] Where, θ W It is the rate of change of the beam's bending stiffness; the coefficients U, V, and W are related to the impact frequency and the characteristics of the testing vehicle, and can be calibrated through experiments. When the impact frequency and the testing vehicle frequency are close, the acceleration signal is most sensitive to damage.

[0180] The stiffness change rate obtained by the above method uses weighted stiffness, which needs to be converted into actual stiffness before load-bearing capacity assessment. The calculation method for weighted stiffness based on Short-Time Fourier Transform (STFT) is as follows:

[0181]

[0182]

[0183] Among them, (EI) i The bending stiffness in each window unit This is typically taken as a Hamming window. θW This is the weighted stiffness ratio. When using the stiffness ratio to inversely deduce the actual stiffness EI, the following assumptions can be introduced:

[0184] Assumption 1: The stiffness at non-abrupt points is uniformly distributed, with a baseline value (EI) of 0; the stiffness at abrupt changes is (EI). d ;

[0185] Assumption 2: Eight elements constitute a time period. When the overlap rate of adjacent moving windows in the STFT is (1-1 / 8), let the abrupt stiffness occupy one element (the width of the damage), and the remaining seven elements be the reference stiffness value. Then, based on formula (17) and the adjacent moving windows containing the damage, the stiffness ratio can be obtained as:

[0186]

[0187] Where, N s The actual position of the abrupt stiffness within the sliding window is represented by 's', where 's' denotes the window number. The window function is consistent with that used in STFT.

[0188] Based on the above assumptions, it can be deduced that when the moving window gradually slides in units of one cell, the weighted stiffness ratio reaches its maximum value when the damaged cell is located at the position of the 6th cell in a time interval. The proof is as follows:

[0189] Based on hypothesis 2, the window function can be divided into 8 equal units. The weights within each unit are summed to obtain a new weight vector, which is then normalized to obtain [z1 z2...z8]. T Without loss of generality, assume the stiffness distribution is [1 1 1 1 1 1 1 1 1 1θ1 11 1 1 1 1 1]. Calculation yields (EI). W It is [1 11+z8(θ-1)1+z7(θ-1)…1+z1(θ-1)1]. Therefore θ W The distribution is

[0190] When θ > 1, θ W The maximum value in satisfies Right now

[0191]

[0192] Right now

[0193]

[0194] make x2=z j+1 +z j-1 -2z jThe following figure shows the sample point distribution of the Hamming window. It can be seen that when j = 6, x1 < 0 and x2 < 0; when j = 7, x1 << x2 and x2 > 0. Therefore, when i = 6, formula (20) is satisfied, θ W Take the maximum value.

[0195] When θ < 1, θ W The positional pattern of the minimum value is consistent with that described above.

[0196] After calculating the stiffness change using the above method, the equivalent cross-sectional area of ​​the reinforcing steel can be obtained in the next section.

[0197] 2.4 Evaluation Methods

[0198] Based on the relationships between Sections 2.1 and 2.3, this section presents a load-bearing capacity assessment algorithm based on stiffness ratio. In Section 2.3, a complete beam is used as the benchmark, and the stiffness ratio θ... m This reflects the relative change in the bending stiffness of the cross section. Let the short-term stiffness of the complete beam be B. s0 This can be estimated based on design requirements and drawings. Therefore, the short-term stiffness of the damaged beam is B. s =B s0 θ m Through section B in section 2.2 s By understanding the relationship between the cross-sectional area of ​​the reinforcing bars and ... ultimate bending moment (as described in Section 2.1), the remaining load-bearing capacity of the beam can be assessed. The calculation process is as follows: Figure 5 As shown.

[0199] Furthermore, the above solution process is reversible, and the degree of stiffness change of the section can be inverted based on the relative change of the ultimate bending moment. This inverse process is used later in the text to solve for the equivalent stiffness change corresponding to the change in the equivalent ultimate bending moment.

[0200] The method in Section 2 only considers the load-bearing capacity assessment of a single beam. However, actual beams are connected to adjacent beams, so the contribution of the transverse connections between beams to the flexural stiffness of the main beam section needs to be considered. Based on the calculation method of the lateral load distribution coefficient, the lateral load distribution is calculated separately when the main beam section has no stiffness loss but the transverse connections are damaged, and when the main beam section has no flexural stiffness loss and the transverse connections are intact. By comparing the load distributions of these two types of damage, the damage in the transverse connections is equivalent to the loss of flexural stiffness of the main beam section.

[0201] 3.1 Load lateral distribution coefficient

[0202] The calculation object is a T-section beam containing a small number of diaphragms, and the lateral load distribution coefficient can be calculated using the hinged plate method. This method assumes that adjacent main beams are rigidly connected, and the joints can transfer shear force. The diaphragms are treated by averaging their lateral bending stiffness along the longitudinal direction (length direction) of the beam. The basic principles of this method are as follows:

[0203] To facilitate the analysis and understanding of the impact of transverse connection damage on the transverse load distribution factor, consider Figure 6 The n shown T The adjacent T-shaped cross-section beams (the left-side edge beam is defined as beam number one, and the rest are arranged in ascending order), with a focus on i. p Damage to the transverse connections on both sides of the beam affects i p The influence of the lateral load distribution coefficient on beam number 1.

[0204] For two adjacent beams, the theory of lateral load distribution indicates that there exists a special loading mode that causes the distribution of deflection and internal force along the length x-direction to satisfy the following:

[0205]

[0206] Among them, w i For deflection, M i For bending moment, Q i For shear force, p i For the equivalent lateral load, C is a constant. The amplitude distribution of p in this case is the lateral load distribution between the beams.

[0207] For T-beams, the primary consideration is a hinged connection. By cutting the joint, a distributed hinged force g can be defined. i (x). Then, based on the deformation compatibility conditions, we can obtain... Figure 6 The model corresponds to the following relationship:

[0208]

[0209] in It is the vertical deflection of the main beam under unit load. It is the vertical deflection caused by the unit shear force. It is the vertical deflection of the lower flange under unit shear force:

[0210]

[0211] Where L is the beam length, EI is the bending stiffness, GJ is the torsional stiffness, and b1 is the beam width. Related to the load form and boundary conditions, I1 is the longitudinal bending moment of inertia per unit plate width (including the contribution of the diaphragms) with the longitudinal direction of the beam as the principal axis, h is the flange thickness, and the meaning of d1 can be found in [the table below]. Figure 6 .

[0212] At this time, the lateral load distribution is as follows:

[0213]

[0214] 3.2 Equivalent stiffness of transverse connection damage

[0215] The basic method of this embodiment is as follows: taking the case where the main beam is undamaged and the transverse connections are intact as a benchmark, the transverse load distribution coefficient of each beam is obtained; then the transverse load distribution of the main beam is calculated when the transverse connections are damaged but the transverse beams are intact; and the equivalent stiffness loss is obtained based on the load variation level. For example... Figure 7 As shown, the blue area indicates the location of lateral connection damage, with the downward deflection w defined as positive and the angle... Counterclockwise is positive. Ignoring local flange deflection caused by shear force, when the distributed load p(x) acts on i... p When the center of beam is reached, the following equation can be established: (a) When 0 < x < a, a + b < x < l:

[0216] Beam No. 1:

[0217] i(i=2,3,…,n T Beam No. -1:

[0218] i p Beam number:

[0219] n T Beam number:

[0220] The deflection on both sides of the hinge should be the same, therefore the following must also be satisfied:

[0221]

[0222] (b) When a≤x≤a+b, the hinge joint does not transmit shear force; the displacements on the left and right sides of the connection point can be different:

[0223] i p -1 Beam:

[0224] i p Beam number: i p Beam No. 1:

[0225] δ is used to determine whether the injury is unilateral (left side in this example) or bilateral. If it is unilateral, δ = 1; if it is bilateral, δ = 0. When it is a unilateral transverse connection injury, the undamaged side should also satisfy equation (29).

[0226] (c) When x = 0 and x = 1, the boundary conditions are:

[0227]

[0228] In the above equation, according to the classical lateral distribution theory, the rotation angles at the supports are assumed to be zero. Since the T-beam has low restraint torsional stiffness, the damage occurs far from the supports, and the influence of the restraint moment is temporarily ignored. Expanding the beam's deflection and rotation angles into a series and substituting them into the above equation, the coefficients in the series expansion can be solved using the method of undetermined coefficients. Then, selecting the location of the section of interest, the deflection of the intermediate beam is calculated, and compared with the deflection of the intermediate beam without considering damage. This allows for an assessment of the deflection change at that section due to lateral connection damage. According to the lateral distribution theory, the ratio of deflections is approximately considered to be the ratio of actual loads, i.e.

[0229]

[0230] Where w c w d p represents the deflection at specific cross-sections of the intermediate beam, with and without transverse connection damage, respectively. c p d These represent the equivalent loads in the two cases, respectively.

[0231] By comparing with formula (24), the relative change of load can be obtained. Damage to the transverse connections increased the stress on the intermediate beam, therefore Compared to a complete beam, damage to the transverse connections increases the beam's load factor, meaning the beam will reach its ultimate strength earlier as the load gradually increases. Converting this load change to short-term stiffness, the damage to the transverse connections can be considered a loss of short-term stiffness in the beam. Section 2.4 presents the relationship between stiffness and bearing capacity; therefore, when calculating this equivalent stiffness loss, the increase in the load factor can be approximated as a decrease in the equivalent bearing capacity, i.e.:

[0232]

[0233] in, and These represent the load-bearing capacity with and without damage, respectively, in conjunction with Section 2.4. Figure 5 The calculation process utilizes the relative change in bearing capacity. The relative change in stiffness caused by damage to the transverse connection can be solved in reverse.

[0234] 3.3 Considering the corrected stiffness ratio for lateral connections

[0235] exist Figure 5 In the evaluation method, the stiffness ratio obtained using formula (18) is the stiffness (EI) of an intact beam with good transverse connection.t0 As a reference (i.e., θ) m (The denominator in the definition). However, when inverting the cross-sectional area of ​​the reinforcing bars, a single beam model is used, requiring the stiffness (EI) of a single, lossless beam to be employed. b0 stiffness ratio θ as the reference r To perform the calculation, θ needs to be... m Convert to θ r .

[0236] When the transverse connections are intact and the main beam (intermediate beam) is undamaged, let Figure 6 The lateral load factor is g0. In the corresponding equivalent single beam model, both lateral connections are damaged, while the main beam remains undamaged, and the lateral load factor is g. td Therefore, according to formula (35), the relative change value of the equivalent ultimate bending moment is 1-g. td / g0, the corresponding relative change in stiffness can be obtained by reversing the process in Section 2.4. Therefore, (EI) is obtained. t0 and (EI) b0 The relationship between them:

[0237]

[0238] Because (EI) t0 >(EI) b0 ,so

[0239] Since the stiffness ratio is defined differently under different damage conditions, θ needs to be discussed separately for each case. r and θ m Relationship:

[0240] (1) The transverse connection is intact, but the main beam is damaged.

[0241] Let the stiffness of the damaged main beam in the single-beam model be (EI). d ,but Similar to the undamaged case, the stiffness (EI) of the overall model with intact lateral connections but damaged main beams is calculated. td Stiffness (EI) of a single-beam model d The relationship can be represented as in This represents a relative change in stiffness. Therefore, we can conclude that:

[0242]

[0243] The above formula uses Because the effect of local damage to the beam on w is negligible.

[0244] (2) The transverse connection is damaged, but the main beam is undamaged. Measured θm This characterizes lateral connectivity damage and can be denoted as θ. mt .

[0245] (3) Both the transverse connection and the main beam have local damage. The benchmark is the stiffness of the undamaged beam with intact transverse connection.

[0246] Let the stiffness be (EI) when both the transverse connection and the main beam are damaged. td The relative change in stiffness is Based on the same reasoning, we can conclude that:

[0247]

[0248] Therefore:

[0249]

[0250] (4) The transverse connection has a wide range of damage, and the main beam is damaged in this area. Therefore, the benchmark is the stiffness of the undamaged beam with the transverse connection damaged.

[0251] At this point, first press Solve (EI). t0 The method used was to solve for the equivalent stiffness (EI) when the transverse connection is damaged. t1 The relative change in stiffness is obtained as follows Then, in case (1) Replace with Perform the calculation.

[0252] Other situations can be handled in a similar manner.

[0253] Therefore, the process for assessing the load-bearing capacity of lateral connections is as follows: Figure 8 As shown.

[0254] Taking a certain span of a bridge as an example, the second beam of this span (see...) was examined using the tapping and scanning method. Figure 6 (Definition) The test was conducted, and the stiffness ratio θ can be calculated based on the obtained acceleration of the test vehicle. m The value is 0.9219. Based on the lateral load distribution coefficient for the undamaged condition in Section 3.1, and combined with the calculation method for beam deflection with lateral connection damage in Section 3.3, when considering a lateral connection damage width of 1m, compared to an intact beam, unilateral lateral connection damage leads to a deflection change of approximately 3.00%; lateral connection damage on both sides leads to a deflection change of approximately 4.42%. When the lateral connection damage width is 0.5m, compared to an intact beam, unilateral lateral connection damage leads to a deflection change of approximately 1.66%; lateral connection damage on both sides leads to a deflection change of approximately 2.39%.

[0255] Based on the above results, the relative change in stiffness corresponding to the change in deflection can be calculated using equation (35). For example, for a transverse connection with a damage width of 1m, the stiffness ratio corresponding to a single-sided damage is approximately 0.98, and the stiffness ratio corresponding to a double-sided damage is approximately 0.97. When there is a single-sided local damage in the transverse connection at this location, Then, the corrected stiffness ratio θ is calculated according to the algorithm shown in Section 3.3. r =0.9219×0.98 / 0.97≈0.93, and based on this, the bearing capacity loss of this section can be calculated as 9.97% using the algorithm in Section 2.4.

[0256] On-site inspection revealed repairs on both sides of the transverse connections of beam No. 2. This condition falls between unilateral and bilateral localized damage, with damage widths ranging from approximately 0.5m to 1m. Based on this information and the aforementioned calculation method, the predicted load-bearing capacity loss for this span of the bridge may be between 7.2% and 10.7%.

[0257] This embodiment provides a method for assessing the load-bearing capacity of a conventional reinforced concrete bridge with cracks. When the applied bending moment exceeds the cracking moment, an expression for the strain non-uniformity coefficient is obtained. Based on this expression, the short-term stiffness of the cracked concrete beam is derived. The cross-sectional area of ​​the reinforcing steel is then obtained from the short-term stiffness, and the ultimate bending moment is calculated from the cross-sectional area. Finally, the remaining load-bearing capacity of the concrete bridge is assessed based on the ultimate bending moment. The parameters used in this embodiment are obtained through on-site measurements, significantly reducing the influence of human experience on the assessment of the load-bearing capacity of concrete bridges, improving reliability, simplifying the assessment process, and lowering assessment costs.

[0258] It is understood that the above embodiments are merely exemplary implementations used to illustrate the principles of the present invention, and the present invention is not limited thereto. For those skilled in the art, various modifications and improvements can be made without departing from the spirit and essence of the present invention, and these modifications and improvements are also considered to be within the scope of protection of the present invention.

Claims

1. A method for assessing the load-bearing capacity of a conventional reinforced concrete bridge with cracks, characterized in that, include: Obtain the acceleration of the tapping and scanning bridge inspection vehicle; The weighted stiffness ratio is obtained based on the expression for acceleration and the short-time Fourier transform. The expression; According to the weighted stiffness ratio The expression and the stiffness ratio obtained from adjacent moving windows containing damage ; Estimate the short-term stiffness of the complete beam based on design standards and drawings. To obtain the short-term stiffness of the damaged beam ; When the applied bending moment is greater than the cracking bending moment, the strain non-uniformity coefficient of the tensile reinforcement is obtained. The expression is as follows: (11) in, It is the axial tensile strength of concrete. M s1 It is the bending moment generated by the permanent load at this section. A t It is the effective tensile cross-sectional area of ​​concrete. η It is the equivalent internal force arm coefficient of the crack section. h 0 is the effective height; The expression for obtaining the short-term stiffness of a cracked concrete beam is as follows: (12) Among them, structural verification coefficient ζ Includes the equivalent internal force arm coefficient of the crack section. η Coefficient of non-uniformity of compressive concrete strain The influence of the ratio of tensile to compressive elastic modulus of concrete and the conversion parameters of compressive concrete. γ' It is the ratio of the area of ​​the compression flange to the effective area of ​​the web. and These are the elastic modulus and cross-sectional area of ​​ordinary steel bars in the tension zone, and the reinforcement ratio. ρ Equivalent to the cross-sectional area of ​​prestressed steel bars ; Based on the short-term stiffness Obtain the cross-sectional area of ​​prestressed steel bars and the cross-sectional area of ​​ordinary steel bars ; When the height of the compression zone is not less than the distance from the resultant point of the compression zone reinforcement to the upper edge, the ultimate bending moment is... M u The expression is as follows: (6) in, , γ 0 represents the structural importance coefficient; When the height of the compression zone is less than the distance from the resultant point of the compression zone reinforcement to the upper edge, the ultimate bending moment... M u The expression is as follows: (7) in, γ 0 represents the structural importance coefficient; According to the ultimate bending moment M u Assess the remaining load-bearing capacity of the concrete bridge; The weighted stiffness ratio is obtained based on the expression for the acceleration and the short-time Fourier transform. The steps of the expression include: The weighted stiffness ratio is obtained based on the expression for acceleration and the short-time Fourier transform. The expression is as follows: (15) The acceleration of the tapping and scanning bridge inspection vehicle; Among them, coefficient U, V, W The results are related to the tapping frequency and the characteristics of the tapping-scanning bridge inspection vehicle, and are obtained through a pre-set test. The weighted stiffness ratio The expression and the stiffness ratio obtained from adjacent moving windows containing damage The steps include: The stiffness at the non-abrupt point is the reference value. Moreover, it is uniformly distributed, and the stiffness at the abrupt change is... Eight window units constitute a time period. When the overlap rate of adjacent moving windows in the short-time Fourier transform is (1-1 / 8), abrupt stiffness is set to occupy one unit, and the stiffness of the remaining seven units is the reference value. According to the weighted stiffness ratio The expression and adjacent moving windows containing damage are used to obtain the stiffness ratio. The expression is as follows: (18) in, The actual position of the abrupt stiffness within the moving window. This indicates the sequence number of the moving window, and the window function is the same as the window function used in the short-time Fourier transform. For Haiming Window.

2. The method for assessing the load-bearing capacity of ordinary reinforced concrete bridges with cracks according to claim 1, characterized in that, The lateral load distribution coefficient of a multi-section T-beam containing diaphragms is calculated using the hinged plate method. The loading mode of the T-beams results in the following distribution of deflection and internal forces along the length x direction: (21) in, For deflection, For bending moment, For shear force, For the equivalent lateral load, It is a constant. The amplitude distribution is the lateral distribution of the load between the beams; The corresponding expression obtained based on the deformation compatibility conditions is as follows: (22) in, It is the vertical deflection of the main beam under unit load. It is the vertical deflection caused by the unit shear force. It is the vertical deflection of the flange under unit shear force, vertical deflection. Vertical deflection and vertical deflection The expression is as follows: , , (23) in, L Let be the length of the beam. EI For bending stiffness, GJ To increase torsional stiffness, b 1 represents the width of the beam. For functions related to the load form and boundary conditions, Let be the longitudinal moment of inertia per unit width of the plate, with the longitudinal direction of the beam as the principal axis. d 1 represents the cross-sectional geometric parameters; The expression for the lateral load distribution of the T-beam is as follows: (24) Set deflection w Downward is positive, corner φ Counterclockwise is positive. g i ( x ) represents the distributed hinge force; When distributed load p ( x ) function in The center of the beam, At that time, the expression obtained is as follows: For beam number one: (25) for i ( i= 2,3, … , - Beam No. 1: , (26) for Beam number: , (27) for Beam number: , (28) When the deflection on both sides of the hinge is the same, the expression is as follows: (29) When distributed load p ( x ) function in The center of the beam, When the hinge joint does not transmit shear force, the displacements on both sides of the connection point are different, resulting in the following expression: for Beam number: , (30) for Beam number: , (31) for Beam number: , (32) in, This is used to determine whether the injury is unilateral or bilateral. If it is unilateral... If it is a bilateral injury, ; When distributed load p ( x ) function in The center of the beam, The expression for obtaining the boundary conditions is as follows: (33) The deflection and rotation angle of the T-beam are expanded into a series, substituted into the above expression, and the coefficients in the series expansion are solved using the method of undetermined coefficients. The above expression is used to describe the deformation law of the multi-piece T-beam model.

3. The method for assessing the load-bearing capacity of ordinary reinforced concrete bridges with cracks according to claim 2, characterized in that, Also includes: Select the location of the cross-section, calculate the deflection of the intermediate beam of the cross-section, compare the deflection of the intermediate beam of the cross-section with the deflection of the intermediate beam without considering damage, and evaluate the deflection change of the cross-section caused by transverse connection damage. According to the transverse distribution theory, the ratio of deflections is the ratio of actual load, as expressed below: (34) in, w c For the deflection of a specific section of the intermediate beam without lateral connection damage, w d For the deflection of a specific section of the damaged intermediate beam, p c This represents the equivalent load without lateral connection damage. p d Indicates the equivalent load that causes damage; The relative change of the equivalent load is obtained from expression (24). ; Based on the relationship between stiffness and bearing capacity, the stiffness loss of the equivalent load is calculated, and it is determined that the increase in the load factor leads to a decrease in the equivalent bearing capacity. The expression is as follows: (35) in, and These represent the load-bearing capacity with and without damage, respectively, utilizing the relative changes in load-bearing capacity. Inverse calculation of the relative change in stiffness caused by transverse connection damage .

4. The method for assessing the load-bearing capacity of ordinary reinforced concrete bridges with cracks according to claim 3, characterized in that, Also includes: Set the lateral load factor as g 0, the corresponding lateral coefficient of the equivalent single beam model is g td According to expression (35), the relative change value of the equivalent ultimate bending moment is obtained. The corresponding relative change in stiffness is obtained by reversing the process. The stiffness of a perfectly horizontally connected, undamaged beam is obtained. EI ) t0 Stiffness of a single, undamaged beam ( EI ) b0 The relationship expression is as follows: (36) When the lateral connections are undamaged but the main beam is damaged, the stiffness of the damaged main beam in the corresponding equivalent single-beam model is: The stiffness of a single, undamaged beam is obtained. EI ) b0 stiffness ratio as a reference The stiffness of the overall model where the lateral connections are undamaged while the main beam is damaged. Stiffness of the corresponding equivalent single beam model The relationship is ,in For relative changes in stiffness, according to and The expression obtained is as follows: (37) When the transverse connection is damaged but the main beam is undamaged, the actual measurement... Characterized as transverse connectivity damage ; When there is localized damage to the transverse connection and localized damage to the main beam, the stiffness is set to... The relative change in stiffness is The resulting expression is as follows: (38) (39) When the transverse connection has overall damage and the main beam has overall damage, according to Solve for the equivalent stiffness of the transverse connection with damage. The relative change in stiffness is obtained as follows , in expression (37) Replace with Perform the calculation.

Citation Information

Patent Citations

  • Knocking scan type bridge damage detecting system

    CN103076393A

  • Passive excitation type bridge flaw detection device

    CN114674919A