A melting welding device for solid laser slab and heat sink and its use method
Through the melt welding device connected by a symmetric welding unit and a heating pad, the complex temperature control and operation of the solid laser slat and heat sink welding process is solved, and the welding quality improvement and stress buffering capacity are enhanced. It is suitable for single-sided Or double-sided welding.
Patent Information
- Application Number
- CN202410462020.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-17
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-04-17
AI Technical Summary
The existing solid-state laser slat and heat sink welding methods have problems such as temperature control, pressure and solder surface quality requirements, complex operation, possible defects in welding surfaces, poor stress buffering capabilities, and inconvenient welding process.
Using a melt welding device including upper and lower symmetrical welding units, the welding unit is connected by heating pads, and precise welding is achieved using heating plates and positioning units. The solder casting and exhaust air outlet design ensure welding quality, and the segmentation of the welding zone constraint frame Structure and cast backflow nozzle improve operational ease.
It realizes the precision of solder shape after welding, improves stress buffering capacity, improves welding quality, bubble discharge, reduces solder surface quality requirements, is easy to operate and is suitable for single-sided or double-sided welding.
Smart Images

Figure CN118253840B_ABST
Abstract
Description
[0001] Technical field
[0002] The present invention specifically relates to a melting welding device for a solid laser slab and a heat sink and a use method thereof, belonging to the technical field of special welding. Background Art
[0003] A solid-state laser power amplifier module is a device module used to enhance laser power. It is usually composed of a solid gain medium, a pump source, a heat sink, optical components, and control electronic devices. Its working principle is to amplify the input laser signal by activating atoms or molecules in the solid gain medium to generate stimulated radiation.
[0004] Solid gain media are divided into different configurations. The configuration of the slab laser gain medium is slab-type, and a zigzag optical path is used to transmit the laser, which effectively eliminates the first-order thermal focusing and thermally induced birefringence effects, and can achieve better beam quality and higher output power.
[0005] A heat sink is a device used to dissipate heat. In solid-state lasers, it is mainly used to absorb and conduct the heat generated by the gain medium during operation, maintain the temperature of the slab within a safe range, and ensure its working stability. Heat sinks are usually made of materials with good thermal conductivity, such as aluminum alloy or copper, and are designed with a heat dissipation structure to increase the heat dissipation effect.
[0006] The slats and heat sinks in the solid-state laser power amplifier module need to be packaged to ensure the structural connection and sealing design between the slats and the heat sink, and low-melting-point solder is generally used for welding. Traditional welding processes can be divided into two types. One is the diffusion welding method, which uses welding wire or thin sheet solder and is installed in the order of heat sink-solder-slats. Under the action of temperature and pressure, they are bonded, and plastic deformation occurs locally. After a certain period of time, the atoms in the bonding layer diffuse with each other to form a whole. This method requires controlling the temperature below the melting point of the solder and maintaining the displacement and pressure for a certain period of time. The second is to use solder melting brazing method, place the solder on the welding surface of the heat sink, heat it until the solder melts, quickly stick the slats to be welded to the welding surface, fix the relative position, and wait for the solder to cool down to complete the welding.
[0007] The two existing welding methods have defects. Among them, the diffusion welding method has high requirements on the temperature control, pressure, solder surface quality and flatness of the welding equipment, and requires complex tooling. Because the welding pressurization process causes the solder layer to be thinned after welding, and the welding temperature is not below the melting point, there may be tiny defects on the welding surface after welding. During the repeated operation of the laser, the defects on the welding surface may cause the packaging of the heat sink and the strip to fail.
[0008] The solder melting brazing method has extremely high requirements on personnel operation during the welding process. During the welding process, the molten solder will flow out from between the slats and the heat sink irregularly. The shape of the solder after cooling is uncontrollable, which reduces the stress buffering capacity of the slats when the laser is running. In addition, the molten solder may enter the air when the slats are attached, and holes are easily formed after the solder cools, resulting in uneven heat dissipation of the slats. This welding method is more inconvenient for laser types that require welding heat sinks on both sides of the slats. Summary of the invention
[0009] In view of the deficiencies of the prior art, the present invention provides a melting welding device for a solid laser slab and a heat sink.
[0010] The present invention also provides a method for using the above-mentioned melting welding device for the solid laser slab and the heat sink.
[0011] The technical solution of the present invention is:
[0012] A melting welding device for a solid laser slab and a heat sink comprises two symmetrically arranged upper and lower welding units, the two welding units being connected via heating pads on both sides;
[0013] The welding unit comprises a heating plate and a positioning unit arranged on the inner side of the heating plate; the positioning unit comprises a sleeved welding zone constraint inner frame and a welding zone constraint outer frame, an inner positioning block is embedded in the welding zone constraint inner frame, and the thickness of the welding zone constraint inner frame and the welding zone constraint outer frame are corresponding; the outer edge of the welding zone constraint inner frame and the inner edge of the welding zone constraint outer frame form a welding area; the welding zone constraint outer frame is provided with a pouring port and an exhaust riser;
[0014] The inner positioning blocks of the two welding units are respectively embedded in the two heat sinks to be welded; the plate strips to be welded are clamped between the positioning units of the two welding units.
[0015] Preferably, the heating plate includes a positioning pin hole, an integral fixing screw hole, an inner positioning block fixing hole and a heating rod.
[0016] Preferably, the inner positioning block comprises an inner frame quick-release hole positioning groove and an inner positioning block fixing screw hole; the welding area constraining inner frame is provided with an inner frame quick-release hole matching with the inner frame quick-release hole positioning groove.
[0017] Preferably, a heating rod is embedded in the heating pad block; the heating pad block is also provided with an integral fixing screw hole, a positioning pin hole, and a pouring port heating surface.
[0018] Preferably, the welding area constraint outer frame is a segmented structure; each segment of the welding area constraint outer frame is connected through a stepped joint and a fixing hole.
[0019] A method for using the above-mentioned melting welding device for solid-state laser slab and heat sink comprises the following steps:
[0020] 1) The segments of the welding area constraint frame are spliced together through the stepped splicing interface and fixed together through the fixing holes;
[0021] 2) Install the slats, welding zone constraint inner frame, welding zone constraint outer frame, and heat sink in sequence; embed the inner positioning block into the welding zone constraint inner frame, install the heating plate and heating pad and fix them; set temperature sensors at the slats and heat sink;
[0022] 3) Heat the heat sink and the slats through the heating plate. When the heat sink and the slats reach 180°C, reduce the heating power and enter the insulation stage; pour the molten solder through the pouring port, and observe the exhaust riser at the same time. When the exhaust riser is filled with molten solder, stop the pouring process;
[0023] 4) After pouring is completed, enter the cooling stage. When the temperature of the heat sink and the slats drops to 150°C, slow down the cooling speed and control the time to drop to 135°C to more than 40 minutes; after the solder solidifies, cool it to room temperature; remove the overall fixing bolts, take out the heating plate, heating pad, and inner positioning block; remove the welding area constraint inner frame, remove the split welding area constraint outer frame, remove the residual solder, and complete the welding process.
[0024] Preferably, the specific method for fixing in step 2) is: match the positioning groove of the inner frame quick-release hole with the inner frame quick-release hole, and connect the heating plate with the inner positioning block by matching the inner positioning block fixing hole with the inner positioning block fixing screw hole; install the positioning pin at the positioning pin hole of the heating plate, and the positioning pin positions the left and right heating pads through the positioning pin hole of the heating pad; and fix the whole by passing the bolts through the fixing screw holes of the heating plate and the heating pad.
[0025] Preferably, the pouring of the molten solder in step 3) is achieved by a solder pouring device; the solder pouring device includes a pouring backflow nozzle and a molten pool, and a heating rod and a temperature sensor are arranged in the molten pool; the backflow nozzle is made of copper; the initial section of molten solder is poured out and discarded through the pouring backflow nozzle, and the remaining solder is discarded after the pouring is completed.
[0026] Further preferably, the solder melting pouring device is installed in a nitrogen glove box; the water and oxygen content in the nitrogen glove box is less than 50 ppm.
[0027] Preferably, the heat sink and the strips are plated.
[0028] The beneficial effects of the present invention are:
[0029] 1) It can ensure that the solder after welding can achieve the precise shape and thickness of the laser structure design. The residual stress of the solder itself after welding is small, which has a better stress buffering effect on the operation of the strip.
[0030] 2) The solder temperature is above the melting point. Compared with diffusion soldering, the higher the temperature, the better the effect of the mutual diffusion reaction between the solder and the base material can be ensured.
[0031] 3) Bubbles can be discharged during the welding process to ensure welding quality.
[0032] 4) Low requirements on solder surface quality.
[0033] 5) It can be used for welding the single side of the slat to the heat sink, and it can also be used for welding the double sides of the slat to the heat sink. It is easy to install and disassemble, the tooling can be reused, it is easy to use, and has low requirements for personnel operation. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 It is a schematic diagram of the overall structure of the melting welding device of the solid laser slab and the heat sink of the present invention;
[0035] Figure 2 It is a structural exploded diagram of the melting welding device of the solid laser slab and the heat sink of the present invention;
[0036] Figure 3 It is a structural schematic diagram of the heating plate of the present invention;
[0037] Figure 4 This is a schematic diagram of the structure of the inner positioning block of the present invention;
[0038] Figure 5 It is a structural schematic diagram of the inner frame quick-release hole positioning groove of the present invention;
[0039] Figure 6 This is a schematic diagram of the structure of the fixing screw hole of the inner positioning block of the present invention;
[0040] Figure 7 It is a schematic diagram of the structure of the slats of the present invention;
[0041] Figure 8 This is a schematic diagram of the structure of the inner frame quick-release hole of the present invention;
[0042] Fig. 9 It is a structural schematic diagram of the welding area constraint outer frame of the present invention;
[0043] Fig.10 It is a structural schematic diagram of the welding area constraint outer frame and the welding area constraint inner frame being cooperatively connected according to the present invention;
[0044] Fig.11 It is a structural schematic diagram of the heating pad block of the present invention;
[0045] Among them, 1. heating plate, 1-1. positioning pin hole, 1-2. integral fixing screw hole, 1-3. inner positioning block fixing hole, 1-4. heating rod, 2. inner positioning block, 2-1. inner frame quick release hole positioning groove, 2-2. inner positioning block fixing screw hole, 3. heat sink, 4. welding area constrained outer frame, 4-1. exhaust riser, 4-2. stepped joint, 4-3. pouring gate, 4-4. fixing hole, 5. welding area constrained inner frame, 5-1. inner frame quick release hole, 6. heating pad, 6-1. pouring gate heating surface, 7. slats. DETAILED DESCRIPTION
[0046] Some embodiments of the present invention are described in detail below in conjunction with the accompanying drawings.
[0047] Example 1
[0048] A melting welding device for a solid laser slab and a heat sink, comprising two symmetrically arranged upper and lower welding units, the two welding units being connected via heating pads 6 on both sides;
[0049] The welding unit includes a heating plate 1 and a positioning unit arranged on the inner side of the heating plate 1; the positioning unit includes a sleeved welding zone constraint inner frame 5 and a welding zone constraint outer frame 4, an inner positioning block 2 is embedded in the welding zone constraint inner frame 5, and the thickness of the welding zone constraint inner frame 5 and the welding zone constraint outer frame 4 are corresponding; the outer edge of the welding zone constraint inner frame 5 and the inner edge of the welding zone constraint outer frame 4 form a welding area; the welding zone constraint outer frame 4 is provided with a pouring port 4-3 and an exhaust riser 4-1;
[0050] The inner positioning blocks 2 of the two welding units are respectively embedded in the two heat sinks 3 to be welded; the plate strip 7 to be welded is clamped between the positioning units of the two welding units.
[0051] The thickness of the welding area constraint inner frame 5 and the welding area constraint outer frame 4 is the welding thickness; after the welding area is filled with pouring, the excess solder and gas are discharged through the exhaust riser 4-1. After welding is completed, the welding area constraint inner frame 5 is taken out through the inner frame quick release hole 5-1. The pouring port 4-3 and the exhaust riser 4-1 provide pouring and exhaust for the molten solder respectively.
[0052] The welding area restraining inner frame 5 and the welding area restraining outer frame 4 are made of heat-resistant engineering plastics, or even aluminum; this embodiment uses polytetrafluoroethylene, which is heat-resistant and has a low friction coefficient and is easy to disassemble.
[0053] Example 2
[0054] As described in the fusion welding device of the solid laser slab and the heat sink in Example 1, further, the heating plate 1 includes a positioning pin hole 1-1, an integral fixing screw hole 1-2, an inner positioning block fixing hole 1-3 and a heating rod 1-4. The heating plate 1 is responsible for heating and clamping and positioning various parts of the fusion welding device.
[0055] The inner positioning block 2 includes an inner frame quick release hole positioning groove 2-1 and an inner positioning block fixing screw hole 2-2; the welding area constraining inner frame is provided with an inner frame quick release hole 5-1 that matches the inner frame quick release hole positioning groove 2-1. The inner positioning block 2 is responsible for positioning the welding area constraining the inner frame and conducting the heat of the heating plate to the slats.
[0056] A heating rod 1-4 is embedded in the heating pad 6; the heating pad 6 is also provided with an integral fixing screw hole 1-2, a positioning pin hole 1-1, and a pouring port heating surface 6-1.
[0057] Example 3
[0058] As described in the fusion welding device of the solid laser slat and the heat sink in the first embodiment, further, the welding area constraint outer frame 4 is a segmented structure (the welding area constraint outer frame 4 in this embodiment is a four-segment structure); each segment of the welding area constraint outer frame 4 is connected by a stepped joint 4-2 and a fixing hole 4-4. During welding, the inner edge constrains and seals the molten solder. After welding is completed, due to the solidification of the solder, the welding area constraint combined outer frame 4 is sandwiched between the heat sink 3 and the slat 7, and is easy to remove by disassembling the segmented structure.
[0059] Example 4
[0060] A method for using the melting welding device for a solid laser slab and a heat sink as described in Examples 1-3 comprises the following steps:
[0061] 1) The four segments of the welding area constraint frame are spliced together through the stepped splicing interface 4-2 and fixed together through the fixing holes 4-4;
[0062] 2) Install the slats 7, the welding zone constraint inner frame 5, the welding zone constraint outer frame 4, and the heat sink 3 in sequence; embed the inner positioning block 2 into the welding zone constraint inner frame 5, install the heating plate 1 and the heating pad 6 and fix them; set temperature sensors at the slats 7 and the heat sink 3;
[0063] The specific method of fixing in step 2) is: match the inner frame quick-release hole positioning groove 2-1 with the inner frame quick-release hole 5-1, and connect the heating plate 1 with the inner positioning block 2 by matching the inner positioning block fixing hole 1-3 with the inner positioning block fixing screw hole 2-2; install the positioning pin at the positioning pin hole 1-1 of the heating plate 1, and the positioning pin positions the left and right heating pads 6 through the positioning pin hole 1-1 of the heating pad 6; pass the bolts through the fixing screw holes 1-2 of the heating plate 1 and the heating pad 6 to fix the whole.
[0064] 3) Heat the heat sink 3 and the slat 7 through the heating plate 1. When the heat sink and the slat reach 180°C, reduce the heating power and enter the insulation stage; pour molten solder through the pouring port 4-3, and observe the exhaust riser 4-1 at the same time. When the exhaust riser 4-1 is filled with molten solder, stop the pouring process; the solder uses a low melting point alloy, not limited to tin-bismuth alloy, including other low melting point and softer alloys formed by indium, tin, bismuth, silver, etc. In this embodiment, tin-bismuth alloy is used as solder.
[0065] 4) After pouring, enter the cooling stage. When the temperature of the heat sink 3 and the strip 7 drops to 150°C, slow down the cooling speed and control the time to drop to 135°C to more than 40 minutes. After the solder solidifies, cool it to room temperature. Remove the overall fixing bolts, take out the heating plate 1, heating pad 6, and inner positioning block 2. Remove the welding zone constraint inner frame 5, remove the welding zone constraint outer frame 4, remove the residual solder, and complete the welding process. By controlling the cooling, the residual stress and shrinkage and loosening phenomenon of the solder solidification process can be reduced.
[0066] Example 5
[0067] A method for using a melting welding device for a solid laser slab and a heat sink as described in Example 4, wherein further, the pouring of the molten solder in step 3) is achieved by a solder pouring device; the solder pouring device comprises a pouring backflow nozzle and a molten pool, a heating rod and a temperature sensor are provided in the molten pool; the backflow nozzle is made of copper; the initial section of molten solder is poured out and discarded through the pouring backflow nozzle, and the remaining solder is discarded after the pouring is completed. The backflow nozzle is made of copper material with good thermal conductivity and wettability, and the molten solder pouring process is smoother. To ensure the quality of the solder, only the middle part of the molten solder is used.
[0068] The heating plate and the molten pool can be made of heat-conducting metals such as copper or aluminum.
[0069] Example 6
[0070] A method for using the melting welding device for a solid laser slab and a heat sink as described in Example 5, further comprising installing a solder melting pouring device in a nitrogen glove box; the water and oxygen content in the nitrogen glove box is less than 50 ppm. The glove box is suitable for modules with high welding quality requirements, providing a nitrogen operating environment to prevent oxidation of the molten solder.
[0071] Example 7
[0072] A method for using the fusion welding device of the solid laser slab and the heat sink as described in Example 4, further, the heat sink 3 and the slab 7 are subjected to coating treatment, such as tin, bismuth, silver, gold, etc. The coating treatment can improve the welding quality.
Claims
1. A melting welding device for a solid laser slab and a heat sink, characterized in that: It includes two symmetrically arranged upper and lower welding units, and the two welding units are connected by heating pads on both sides; The welding unit comprises a heating plate and a positioning unit arranged on the inner side of the heating plate; the positioning unit comprises a sleeved welding zone constraint inner frame and a welding zone constraint outer frame, an inner positioning block is embedded in the welding zone constraint inner frame, and the thickness of the welding zone constraint inner frame and the welding zone constraint outer frame are corresponding; the outer edge of the welding zone constraint inner frame and the inner edge of the welding zone constraint outer frame form a welding area; the welding zone constraint outer frame is provided with a pouring port and an exhaust riser; The inner positioning blocks of the two welding units are respectively embedded in the two heat sinks to be welded; the plate strips to be welded are clamped between the positioning units of the two welding units.
2. The melting welding device for solid-state laser slab and heat sink according to claim 1, characterized in that: The heating plate comprises a positioning pin hole, an integral fixing screw hole, an inner positioning block fixing hole and a heating rod.
3. The melting welding device for solid-state laser slab and heat sink according to claim 1, characterized in that: The inner positioning block comprises an inner frame quick-release hole positioning groove and an inner positioning block fixing screw hole; the welding area constraining inner frame is provided with an inner frame quick-release hole matching with the inner frame quick-release hole positioning groove.
4. The melting welding device for solid-state laser slab and heat sink according to claim 1, characterized in that: A heating rod is embedded in the heating pad block; the heating pad block is also provided with an integral fixing screw hole, a positioning pin hole, and a pouring port heating surface.
5. The melting welding device for solid-state laser slab and heat sink according to claim 1, characterized in that: The welding area constraint outer frame is a segmented structure; each segment of the welding area constraint outer frame is connected through a stepped joint and a fixing hole.
6. A method for using the melting welding device for a solid-state laser slab and a heat sink as claimed in any one of claims 1 to 5, characterized in that: The steps include: 1) The segments of the welding area constraint frame are spliced together through the stepped splicing interface and fixed together through the fixing holes; 2) Install the slats, welding zone constraint inner frame, welding zone constraint outer frame, and heat sink in sequence; embed the inner positioning block into the welding zone constraint inner frame, install the heating plate and heating pad and fix them; set temperature sensors at the slats and heat sink; 3) Heat the heat sink and the slats through the heating plate. When the heat sink and the slats reach 180°C, reduce the heating power and enter the insulation stage; pour the molten solder through the pouring port, and observe the exhaust riser at the same time. When the exhaust riser is filled with molten solder, stop the pouring process; 4) After pouring is completed, enter the cooling stage. When the temperature of the heat sink and the slats drops to 150°C, slow down the cooling speed and control the time to drop to 135°C to more than 40 minutes; after the solder solidifies, cool it to room temperature; remove the overall fixing bolts, take out the heating plate, heating pad, and inner positioning block; remove the welding area constraint inner frame, remove the split welding area constraint outer frame, remove the residual solder, and complete the welding process.
7. The method for using the fusion welding device for solid-state laser slab and heat sink according to claim 6, characterized in that: The specific method of fixing in step 2) is: match the positioning groove of the inner frame quick-release hole with the inner frame quick-release hole, and connect the heating plate with the inner positioning block by matching the inner positioning block fixing hole with the inner positioning block fixing screw hole; install the positioning pin at the positioning pin hole of the heating plate, and the positioning pin positions the left and right heating pads through the positioning pin hole of the heating pad; fix the whole by passing the bolt through the fixing screw holes of the heating plate and the heating pad.
8. The method for using the fusion welding device for solid-state laser slab and heat sink according to claim 6, characterized in that: The pouring of the molten solder in step 3) is achieved by a solder pouring device; the solder pouring device includes a pouring backflow nozzle and a molten pool, in which a heating rod and a temperature sensor are arranged; the backflow nozzle is made of copper; the initial section of molten solder is poured out and discarded through the pouring backflow nozzle, and the remaining solder is discarded after the pouring is completed.
9. The method for using the fusion welding device for solid-state laser slab and heat sink according to claim 8, characterized in that: The solder melting pouring device is installed in a nitrogen glove box; the water and oxygen content in the nitrogen glove box is less than 50ppm.
10. The method for using the fusion welding device for solid-state laser slab and heat sink according to claim 6, characterized in that: Heat sinks and slats are plated.