Semi-solid forming device and method for composite metal materials

By using the inclined guide groove and extrusion block design in the composite metal material forming device, extrusion is achieved simultaneously on multiple bonding surfaces, solving the adhesion problem caused by uneven deformation of metal materials in the prior art, and improving the Formation quality.

CN118385520BActive Publication Date: 2024-11-15GUANGZHOU ZHONGSHAN FASTENER CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410628736.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-21
Publication Date
2024-11-15
Estimated Expiration
2044-05-21

AI Technical Summary

Technical Problem

When the existing composite metal molding molds apply extrusion pressure at the multi-layer joint surface, they cause uneven deformation of the surface of the metal material, affecting adhesion, and prone to voids and crack defects.

Method used

Design a semi-solid forming device for composite metal materials, adopting an inclined extension guide groove and an extrusion block. There are two intersecting extrusion surfaces on the extrusion block, which can extrude multiple joint surfaces simultaneously when closing the mold. Pressure, the two extrusion surfaces on the extrusion block are pushed through the lifting seat to move in the guide groove, ensuring that the metal material is squeezed in a vertical or approximately vertical direction, eliminating gaps and enhancing adhesion.

Benefits of technology

It effectively enhances the adhesion of composite metal materials, avoids the occurrence of voids and crack defects, and improves the molding yield rate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118385520B_ABST
    Figure CN118385520B_ABST
Patent Text Reader

Abstract

The present invention discloses a semi-solid forming device and method of composite metal materials, the forming device comprises a lower die, an upper die, and an extrusion mechanism; the upper die and the lower die form a cavity and a flow channel when the mold is closed, a first space and a second space are formed inside the cavity, and the first space and the second space have two intersecting bonding surfaces; the lower die is provided with an inclined extending guide groove, the top of the guide groove extends to the second space of the cavity to form an opening; the extrusion mechanism comprises a lifting seat, a driving unit, and an extrusion block, the lifting seat is provided with a push inclined surface, the extrusion block is movably connected in the guide groove, and a matching surface that abuts against the push inclined surface is provided at the bottom, and the top of the extrusion block forms two intersecting extrusion surfaces, and the two extrusion surfaces are used to simultaneously apply extrusion forces toward the two bonding surfaces to the metal material in the second space. The present invention can increase the adhesion of the two metal materials in the composite material and improve the yield rate of composite metal material forming.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of molds, and in particular to a semi-solid forming device and method for composite metal materials. Background Art

[0002] With the continuous development of metal material processing technology, multi-layer composite metal materials are gradually being used in the external frame of products. For example, in the 3C industry, in order to make the appearance of the product meet the requirements of lightweight, corrosion resistance and high strength, parts such as laptop computer frames and mobile phone frames are gradually using titanium-aluminum composite profiles. This composite metal material is usually processed and formed by an in-film inlay process, which is to first place a solid titanium alloy in the mold cavity, and then inject a fluid state (such as semi-solid) aluminum alloy material into the mold cavity. After the aluminum alloy material solidifies in the mold cavity, it is combined with the titanium alloy material. In order to make the two layers of metal materials have better adhesion after molding, it is usually necessary to set an extrusion mechanism inside the mold to apply extrusion force to the surfaces where the two layers of metal materials are combined with each other during the molding process. The bonding properties of the metal surface layer are increased by extrusion, so that the two layers of metal materials have better adhesion.

[0003] At present, the extrusion mechanisms set inside the forming molds used for composite metal materials all apply extrusion pressure to the workpiece to be formed inside the mold cavity in one direction. The extrusion pressure applied can only be applied well to one of the bonding surfaces of the two layers of metal materials. When the two layers of metal materials have more than two bonding surfaces, although the extrusion in a single direction can increase the adhesion of one of the bonding surfaces, the extrusion causes uneven deformation of the surface of the metal material, especially when extruded in a heated state. The uneven deformation of the surface of the metal material will seriously affect the adhesion of the two layers of metal materials at the other bonding surface, and it is very easy to produce defects such as gaps and cracks at the other bonding surface. Summary of the invention

[0004] The main purpose of the present invention is to provide a semi-solid forming device and method for composite metal materials, which can effectively increase the adhesion at the joint surface of two layers of metal materials in the composite metal and avoid the appearance of gaps and cracks at the joint.

[0005] To achieve the above object, the present invention adopts the following technical solution:

[0006] A semi-solid forming device for composite metal materials, comprising a lower die, an upper die located above the lower die, and an extrusion mechanism;

[0007] The upper mold and the lower mold form a mold cavity when the mold is closed, and a flow channel connected to the mold cavity for introducing semi-solid metal slurry into the mold cavity. The mold cavity forms a first space for accommodating solid metal material and a second space for accommodating semi-solid metal material. The first space and the second space have two intersecting joint surfaces.

[0008] The lower mold is provided with an inclined extending guide groove, the angle between the extending direction of the guide groove and the height direction is 45°, and the top of the guide groove extends to the second space of the cavity to form an opening;

[0009] The extrusion mechanism includes a lifting seat, a driving unit for driving the lifting seat to move up and down in the height direction relative to the lower mold, and an extrusion block. The lifting seat is provided with a push inclined surface. The extrusion block is movably connected to the guide groove, and a matching surface that abuts against the push inclined surface is provided at the bottom thereof. The matching surface cooperates with the push inclined surface to make the extrusion block move along the guide groove toward the direction close to the opening when the lifting seat moves upward. Two intersecting extrusion surfaces are formed on the top of the extrusion block. The two extrusion surfaces are used to simultaneously apply extrusion forces toward the two combining surfaces to the metal material in the second space when the extrusion block moves to the opening of the cavity.

[0010] Preferably, an elastic element is provided between the extrusion block and the lower die, and the elastic element is used to always apply an elastic stress to the extrusion block so that the matching surface always abuts against the push inclined surface.

[0011] Preferably, a side surface of the lifting seat is provided with an inclined guide groove, the bottom surface of the guide groove forms a push inclined surface, and the bottom of the extrusion block is embedded in the guide groove and is confined between the two side walls of the guide groove.

[0012] Preferably, the lower mold includes a lower mold plate and a lower mold core embedded in the lower mold plate, the upper mold includes an upper mold plate and an upper mold core embedded in the upper mold plate, the upper surface of the lower mold core is provided with a downwardly recessed recess, the recess includes an outer wall, an inner wall and a bottom wall connected between the bottom of the outer wall and the bottom of the inner wall, and when the upper mold and the lower mold are closed, the bottom surface of the upper mold core and the outer wall, inner wall and bottom wall of the recess together form a molding cavity, a part of the opening is formed on the inner wall, and the other part is formed on the bottom wall, and the two extrusion surfaces on the extrusion block are flush with the inner wall and the bottom wall respectively when moving to the opening.

[0013] Preferably, the lower surface of the lower mold core is provided with an avoidance groove which is recessed upward for accommodating the lifting seat and enabling the lifting seat to move up and down therein, and the guide groove extends obliquely upward from the top surface of the avoidance groove to the position where the inner wall and the bottom wall of the recess are connected, and the thickness of the part of the extrusion block located outside the guide groove is greater than the thickness of the part of the extrusion block located inside the guide groove.

[0014] Preferably, one end of the recess is connected to and communicated with the flow channel, and an overflow groove extending from the other end of the recess toward the edge of the lower mold core is provided on the lower mold core, and the depth of the overflow groove gradually decreases from one end connected to the recess to the other end.

[0015] Preferably, the upper surface of the lower mold core protrudes from the upper surface of the lower mold plate so that the upper mold plate and the lower mold plate can be gap-matched when the upper mold and the lower mold are closed. The end of the overflow groove with a smaller depth extends to the edge of the lower mold core and is connected to the gap between the upper mold plate and the lower mold plate so that the overflow groove can discharge the air in the cavity to the outside of the upper and lower molds.

[0016] Preferably, the bottom surface of the overflow groove forms a plurality of guide surfaces arranged along the extension direction of the overflow groove, and the heights of the plurality of guide surfaces gradually increase from the end of the overflow groove connected with the recess toward the direction away from the recess, and two adjacent guide surfaces are connected together by a retaining wall extending along the height direction.

[0017] Preferably, the molding device also includes a feeding mechanism, which includes a lifting plate located below the lifting seat and fixed to the lifting seat, a push rod fixedly connected to the lifting plate and extending in the height direction, and a through hole extending downward from the guide surface with the lowest height on the overflow groove to the bottom surface of the lower mold core is provided on the lower mold core, and the push rod is connected to the through hole from bottom to top so as to move up and down with the lifting seat; the width of the guide surface with the lowest height in the overflow groove is greater than the width of other parts of the overflow groove so that the diameter of the through hole is greater than the width of the recessed position.

[0018] Preferably, the lower mold core includes a first mold core and a second mold core, the first mold core is provided with a through groove extending from its upper surface to its lower surface, the second mold core is embedded in the through groove and fixedly connected to the first mold core in a detachable manner, and the guide groove and the recess are surrounded by the side edge of the second mold core and the inner wall of the through groove.

[0019] Preferably, the lower mold is provided with a plurality of guide grooves arranged along the extension direction of the cavity, an extrusion block is embedded in each guide groove, the total opening length of the plurality of guide grooves is D, the length of the cavity is D2, and the ratio of D to D2 is greater than or equal to 68%.

[0020] Preferably, an inclined drainage surface is formed on the bottom surface where the flow channel is connected to the cavity, and the top of the drainage surface is connected to the bottom of the cavity so that the depth of the flow channel gradually increases from the inside to the outside. A push rod hole is provided on the lower mold, and the push rod hole extends upward from the bottom surface of the lower mold to the bottom of the drainage surface; the molding device also includes an ejection mechanism, which includes a top mold plate, a driving member for driving the top mold plate to move up and down, and a ejector rod fixed on the top mold plate and extending upward, the ejector rod is connected to the ejector rod hole from bottom to top and can extend into the flow channel as the top mold plate moves upward.

[0021] A semi-solid forming method for composite metal materials, using the above-mentioned forming device, placing a solid metal material in the first space of a mold cavity, injecting the semi-solid metal material into the second space of the mold cavity by injection, so that the semi-solid metal material and the solid metal material form a first bonding surface and a second bonding surface that intersect, and using two intersecting extrusion surfaces on an extrusion block to simultaneously apply an extrusion force to the semi-solid metal material. When the extrusion block extrude the semi-solid metal material, the two extrusion surfaces on the extrusion block face the first bonding surface and the second bonding surface respectively, and in the process of using the extrusion block to extrude the semi-solid metal, the upper mold and the lower mold are continuously heated.

[0022] The present invention pushes the inclined extrusion block upward through the lifting seat, and the two intersecting extrusion surfaces on the extrusion block can simultaneously apply extrusion forces in two directions to the metal material in the cavity. The extrusion forces in the two directions are directly against the two intersecting bonding surfaces of the two metal materials, so that the metal material is extruded in a direction perpendicular or approximately perpendicular to the bonding surface to produce sufficient deformation, eliminating the gap between the two metal materials, preventing the appearance of gaps and cracks between the two, thereby increasing the adhesion of the two metal materials. Since the extrusion force applied by the extrusion block is directed toward the two bonding surfaces respectively, the extrusion force on the two metal materials is prevented from being parallel to the bonding surfaces of the two metal materials or the angle between the two metal materials and the bonding surfaces is too small, avoiding the situation where the two metal materials are peeled off during the extrusion process, and improving the yield rate of composite metal material molding. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0024] Figure 1 This is a schematic diagram of the structure of Embodiment 1 of the present invention;

[0025] Figure 2 for Figure 1 The enlarged view of the A in the figure illustrates a working state of the first embodiment;

[0026] Figure 3 This is another working state schematic diagram of the first embodiment of the present invention;

[0027] Figure 4 for Figure 1 Schematic diagram of the structure of the extrusion block;

[0028] Figure 5 for Figure 1 Schematic diagram of the assembly of the middle and lower mold cores and the lifting seat;

[0029] Figure 6 for Figure 1 Schematic diagram of the structure of the middle and lower mold core;

[0030] Figure 7 for Figure 6 B-direction view;

[0031] Figure 8 for Figure 6 Enlarged view at center C;

[0032] Fig. 9 It is a structural schematic diagram of the ejection mechanism in the first embodiment of the present invention;

[0033] Fig.10 This is a schematic diagram of the structure of Embodiment 2 of the present invention;

[0034] Fig.11 It is a schematic structural diagram of the lower mold core in the second embodiment of the present invention.

[0035] The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0036] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0037] It should be noted that all directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of the present invention are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0038] In addition, the descriptions of "first", "second", etc. in the present invention are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0039] See also Figure 1 , 2, 3, 4, 5, 6, 7, 8, and 9 show a semi-solid forming device for a composite metal material according to a first embodiment of the present invention, in particular, a device for forming a composite metal material composed of a titanium alloy and an aluminum alloy. The composite metal material can be used for the outer frames of laptop computers and mobile phones. During the forming process, the aluminum alloy layer of the composite metal material is injected into the mold cavity in a semi-solid manner.

[0040] The semi-solid forming device of the composite metal material specifically includes an upper mold 20, a lower mold 10, and an extrusion mechanism. The upper mold 20 and the lower mold 10 are arranged up and down. By moving the upper mold 20 downward, the upper mold 20 and the lower mold 10 can be molded together to form a cavity 40 at the parting surface of the two, and a flow channel 16 connected to the cavity 40. The semi-solid aluminum alloy slurry can be fed into the cavity 40 through the flow channel 16. The cavity 40 is consistent with the appearance of the composite metal material after molding, and its internal space forms a first space 41 for accommodating a solid titanium alloy material 51, and a second space 42 for accommodating a semi-solid aluminum alloy material 52. The first space 41 and the second space 42 have intersecting bonding surfaces 401 and 402, wherein the bonding surface 401 corresponds to one of the bonding surfaces 501 of the aluminum alloy material 52 and the titanium alloy material 51, and the bonding surface 402 corresponds to the other bonding surface 502 of the aluminum alloy material 52 and the titanium alloy material 51; see specifically Figure 2 , 3As shown, when the upper mold 20 and the lower mold 10 are in the open mold state, the titanium alloy material 51 is placed in the first space 41 of the cavity 40, and then the upper mold 20 and the lower mold 10 are closed, and the semi-solid aluminum alloy is injected from the runner 16 into the second space 42 of the cavity 40 by injection, so that the semi-solid aluminum alloy fills the second space 42. The lower die 10 is provided with an inclined guide groove 14, the inclination angle of the guide groove 14 is 45°, that is, the angle between the extension direction of the guide groove 14 and the height direction (Z direction in the figure) is 45°. The top of the guide groove 14 extends to the second space 42 of the cavity 40 and forms an opening 141; the extrusion mechanism includes a lifting seat 32, a cylinder 31, and an extrusion block 33. The cylinder 31 is located below the lower die 10. The telescopic rod of the cylinder 31 extends upward and is connected to a driving rod 34. The lifting seat 32 is fixedly connected to the top of the driving rod 34. Driven by the cylinder 31, the lifting seat 32 can move up and down in the height direction relative to the lower die 10. The lifting seat 32 is provided with a push inclined surface 321, and the push inclined surface 321 gradually tilts from bottom to top toward the middle of the lifting seat 32, so as to squeeze The pressing block 33 is movably connected in the guide groove 14, and a matching surface 333 that abuts against the pushing inclined surface 321 is provided at the bottom thereof. The matching surface 333 cooperates with the pushing inclined surface 321. When the lifting seat 32 moves upward, the matching surface 333 is pushed upward by the pushing inclined surface 321, so that the extrusion block 33 can move upward toward the opening 141 along the guide groove 14, and two intersecting extrusion surfaces 331 and 332 are formed on the top of the extrusion block 33. When the extrusion block 33 moves upward to the limit position in the guide groove 14, the extrusion surfaces 331 and 332 on the extrusion block 33 just move to the opening 141 of the guide groove 14. At the opening 141, the aluminum alloy material 52 in the second space 42 is pressurized by the extrusion surfaces 331 and 332 at the same time. Figure 3 As shown in the figure, the extrusion surface 331 faces the bonding surface 501, and the extrusion surface 332 faces the bonding surface 502. The forces applied by the intersecting extrusion surfaces 331 and 332 on the extrusion block 33 to the aluminum alloy material 52 are respectively directed to the bonding surface 501 and the bonding surface 502, that is, the extrusion block 33 is used to extrude the two intersecting bonding surfaces 501 and 502 of the titanium alloy material 51 and the aluminum alloy material 52 at the same time. In the process that the lifting seat 32 is continuously pushed upward by the oil cylinder 31, the extrusion block 33 maintains the tendency of moving upward along the guide groove 14, so that the pressure applied by the extrusion block 33 to the bonding surface 501 and the bonding surface 502 is maintained for a certain time. When the extrusion is completed, the oil cylinder 31 drives the lifting seat 32 to move downward, and the extrusion block 33 moves downward along the guide groove 14 under the action of its own gravity, so that the extrusion surfaces 331 and 332 are downwardly separated from the opening 141, releasing the extrusion of the aluminum alloy material 52, so as to facilitate the demolding of the formed composite material from the cavity 40.

[0041] The above-mentioned oil cylinder 31 serves as a driving unit, which is used to drive the lifting seat 32 to move up and down. At the same time, when the extrusion block 33 applies pressure to the workpiece, it can apply a relatively large upward thrust to the lifting seat 32, thereby ensuring that the extrusion block 33 applies sufficient extrusion force to the workpiece to meet the bonding requirements of the aluminum alloy material 52 and the titanium alloy material 51. Based on this, the oil cylinder 31 is used as the preferred driving unit. In fact, as long as the above requirements can be met, in other embodiments, other hydraulic cylinders, air cylinders, etc. can be used as driving units instead of the oil cylinder 31.

[0042] Combination Figure 4 , 5 As shown, an inclined guide groove 322 is provided on the side of the lifting seat 32, and the bottom surface of the guide groove 322 forms a push inclined surface 321. The bottom of the extrusion block 33 is embedded in the guide groove 322, and the bottom of the extrusion block 33 is limited between the walls on both sides of the guide groove 322; the bottom of the extrusion block 33 is guided by the guide groove 322, and when the lifting seat 32 pushes the extrusion block 33 to move upward, the extrusion block 33 can be prevented from swinging in the direction perpendicular to the plane formed by the movement direction of the lifting seat 32 and the extension direction of the guide groove 14 (i.e., the X direction in the figure), so that the extrusion surface 331 and the extrusion surface 332 on the extrusion block 33 are respectively opposite to the bonding surface 501 and the bonding surface 502 to extrude the aluminum alloy material 52, ensuring that the surface of the workpiece after forming is flat, without more post-processing processes. The push inclined surface 321 of the lifting seat 32 and the inner wall of the guide groove 322 can be subjected to corresponding surface treatment to make them have better wear resistance. Similarly, the matching surface 333 of the extrusion block 33 and other parts in contact with the lifting seat 32 are also subjected to corresponding surface treatment to increase the wear resistance of the extrusion block 33 and prevent the extrusion block 33 and the lifting seat 32 from causing significant wear after a long period of relative movement. By increasing the wear resistance of the contact part between the extrusion block 33 and the lifting seat 32, the forming accuracy of the workpiece can be ensured.

[0043] See also Figure 1As shown, in the molding device of the present invention, the lower mold 10 includes a lower mold plate 11 and a lower mold core embedded in the lower mold plate 11. In a preferred embodiment, the lower mold core is a combined structure, which specifically includes a first mold core 12 and a second mold core 13; the upper mold 20 includes an upper mold plate 21 and an upper mold core 22 embedded in the upper mold plate 21; the upper surface of the lower mold core is provided with a downwardly recessed recess 15, the recess 15 includes an outer side wall 152, an inner side wall 151 and a bottom wall 153, the bottom wall 153 is connected between the outer side wall 152 and the bottom of the inner side wall 151, and the mold cavity 40 is entirely composed of the internal space of the recess 15, that is, after the upper mold 20 and the lower mold 10 are molded together, the bottom surface of the upper mold core 22 and the outer side wall 152, the inner side wall 151 and the bottom wall 153 of the recess 15 are surrounded by the mold cavity 40. The molding cavity 40, in a specific embodiment of the present invention, is formed by the bottom surface of the upper mold core 22 and the outer wall 152, the inner wall 151 and the bottom wall 153 of the recess 15 to form a long strip-shaped molding cavity 40 that matches the shape of the workpiece to be molded. The opening 141 of the guide groove 14 is located at the position where the inner wall 151 and the bottom wall 153 are connected, that is, a part of the opening 141 is formed on the inner wall 151, and the other part is formed on the bottom wall 153. When the extrusion block 33 is pushed upward to the limit position by the lifting seat 32, the extrusion surface 331 of the extrusion block 33 is flush with the bottom wall 153, and the extrusion surface 332 of the extrusion block 33 is flush with the inner wall 151. In this way, the extrusion surfaces 331 and 332 of the extrusion block 33 are kept consistent with the inner wall surface of the molding cavity 40, ensuring that the shape of the workpiece meets the requirements after extrusion.

[0044] In a preferred embodiment in which the lower mold core is set as a combined structure, a through groove 120 is provided on the first mold core 12, which runs through its upper surface to its lower surface. The second mold core 13 is embedded in the through groove 120, and the second mold core 13 is detachably fixed to the first mold core 12 by bolts or other connection methods. The above-mentioned recess 15 is surrounded by the side edge of the second mold core 13 and the inner wall of the through groove 120 on the first mold core 12. Similarly, the guide groove 14 is surrounded by the side edge of the second mold core 13 and the inner wall of the through groove 120 on the first mold core 12. For example, a groove-shaped structure can be machined on the inner wall of the through groove 120. When the second mold core 13 is embedded in the through groove 120, Finally, the side edge of the second mold core 13 is made to cover the notch of the groove-shaped structure. In this way, by setting the lower mold core as the above-mentioned split combined structure, the recess 15 and the guide groove 14 can be processed by machining, thereby improving the accuracy of the recess 15 and the guide groove 14. Especially when the accuracy of the guide groove 14 is improved, the guide groove 14 can better guide the extrusion block 33, and there is a relatively small fitting gap between the extrusion block 33 and the inner wall surface of the guide groove 14. The relatively small fitting gap can discharge a small part of the gas inside the cavity 40 downward from the guide groove 14, and at the same time can prevent the semi-solid aluminum alloy material from flowing out along the guide groove 14 after being injected into the cavity 40. After the second mold core 13 is embedded in the through groove 120 of the first mold core 12, the lower half of the through groove 120 is not filled by the second mold core 13, thereby forming an avoidance groove formed by the lower surface of the first mold core 12 being recessed upward on the lower mold core, and the lifting seat 32 is placed in the avoidance groove, which has enough space to avoid the up and down movement of the lifting seat 32, so that the lifting seat 32 can move up and down in the avoidance groove, and the guide groove 14 extends upward from the top surface of the avoidance groove to the position where the inner side wall 151 and the bottom wall 153 of the above-mentioned recess 15 are connected. By setting the avoidance groove and embedding the lifting seat 32 in the avoidance groove, the height of the entire device will be reduced, which is conducive to fully utilizing the space of the lower mold 20, and the guide groove 14 extends upward from the top surface of the avoidance groove. On the premise of satisfying the guiding role of the extrusion block 33, the guide groove 14 has a relatively small extension size, so that the extrusion block 33 can be set as follows Figure 4 The structure shown, that is, the portion of the extrusion block 33 that passes through the guide groove 14 can match the size of the cavity 40 and has a relatively small thickness, and the portion of the extrusion block 33 located outside the guide groove 14 has a relatively large thickness, ensuring that the extrusion block 33 has better strength, avoiding deformation of the extrusion block 33 when pushed by the lifting seat 32, so that the extrusion block 33 can extrude the aluminum alloy material 52 according to the designed angle, thereby improving the extrusion accuracy of the extrusion block 33 on the workpiece.

[0045] See also Figure 5 , 67. A plurality of guide grooves 14 are arranged along the extension direction of the cavity 40 on the lower die 10. An extrusion block 33 is embedded in each guide groove 14. The length of the opening 141 of each guide groove 14 is D1. The length of the cavity 40 is D2 (i.e., the length of the above-mentioned recess 15 is D2). The total length of the plurality of openings 141 is D, wherein the ratio of D to D2 is greater than or equal to 68%. That is, the size of the portion of the workpiece located inside the cavity 40 that is extruded by the extrusion block 33 is 68% of the total length of the workpiece. Therefore, by providing a plurality of extrusion blocks 33, extrusion can be performed at different positions of the workpiece, and the positions where the workpiece is extruded are relatively more, so that the aluminum alloy material 52 can be fully combined with the titanium alloy material 51. By setting the lower die core as the above-mentioned combined structure, it is convenient to process a plurality of guide grooves 14 on the lower die core, so that the guide grooves can be densely distributed on the lower die core in a relatively small spacing manner, which is conducive to increasing the proportion of the extruded portion of the workpiece, and further conducive to the combination of the aluminum alloy material 52 and the titanium alloy material 51. It should be noted that, when multiple extrusion blocks 33 are provided, the length dimension of the extrusion surface on each extrusion block 33 may be different. For example, the length of the opening 141 located in the middle of the cavity 40 may be set to be relatively large, and the length of the openings 141 at both ends of the cavity 40 may be set to be relatively small, so that the force area when the aluminum alloy material 52 and the titanium alloy material 51 are extruded at the middle of the cavity 40 is relatively large, which facilitates the elimination of the gap between the aluminum alloy material 52 and the titanium alloy material 51. In short, the ratio of the sum of the lengths of all the openings 141 to the total length of the cavity 40 is maintained at more than 68%, which is a preferred embodiment.

[0046] See also Figure 6 , 7One end of the recess 15 is connected and conducted with the flow channel 16, and the semi-solid aluminum alloy material can be injected into the cavity 40 formed by the recess 15 through the flow channel 16. The lower mold core is also provided with an overflow groove 17 extending from the other end of the recess 15 toward the edge of the lower mold core. The depth of the overflow groove 17 gradually decreases from one end connected to the recess 15 toward the other end. The air inside the cavity 40 can be discharged to the outside through the overflow groove 17. At the same time, the depth of the overflow groove 17 gradually changes to form a variable diameter structure inside the overflow groove 17. The overflow groove 17 with a variable diameter structure can slow down the flow of the semi-solid aluminum alloy material inside it, and has a slow flow effect on the semi-solid aluminum alloy material. While slowing down the flow of the semi-solid aluminum alloy material in the overflow groove 17, the space inside the cavity 40 can be discharged through the overflow groove 17 as much as possible. The upper surface of the lower mold core protrudes from the upper surface of the lower mold core 11. When the lower mold 10 and the upper mold 20 are closed, the upper surface of the lower mold core contacts the lower surface of the upper mold core 22, so that a smaller gap is formed between the lower template 11 and the upper template 21. The end of the overflow groove 16 with a relatively small depth extends to the edge of the upper surface of the lower mold core, so that the edge of the overflow groove 16 is connected to the gap between the upper template 21 and the lower template 11. The space inside the cavity 40 can be discharged to the external environment through the overflow groove 16 and the gap between the upper template 21 and the lower template 11. In this way, the exhaust function can be achieved only by protruding the lower mold core from the upper surface of the lower template 11. There is no need to set complex exhaust channels on the upper mold 20 and the lower mold 10, which simplifies the structure of the molding device.

[0047] In order to form the above-mentioned variable diameter structure of the overflow groove 17, the bottom surface of the overflow groove 17 can be set as an inclined surface. Of course, in a preferred embodiment, the overflow groove 17 can also be set as follows: Figure 8The stepped structure shown in the figure is that a plurality of guide surfaces 171 are formed on the bottom surface of the overflow groove 17 and are arranged in the extending direction of the overflow groove 17. At the end of the overflow groove 17 connected with the concave position 15, the heights of the plurality of guide surfaces 171 gradually increase in the direction away from the concave position 15. In other words, the overflow groove 17 is divided into a plurality of continuous sections with gradually changing depths. Two adjacent guide surfaces 171 are connected together by a retaining wall 172 extending in the height direction. When the semi-solid aluminum alloy material overflows from the mold cavity 40, the liquid level of the semi-solid aluminum alloy material in the section where the overflow groove 17 communicates with the mold cavity 40 gradually increases, and the air is discharged through the overflow groove 17. The flow groove 17 is squeezed outward, and when the critical surface between the air inside the overflow groove 17 and the aluminum alloy material reaches the top height of the first baffle wall 172, the aluminum alloy material overflows to the second guide surface 171 through the first baffle wall 172. In this way, by setting the overflow groove 17 as a stepped structure, the slow flow of the aluminum alloy material inside the overflow groove is achieved, and the semi-solid aluminum alloy material entering the overflow groove 17 squeezes the air inside the cavity 40 and the overflow groove 17 outward in a layered manner, so that the air inside the cavity 40 and the overflow groove 17 can be exhausted, thereby avoiding the formation of an empty bag inside the cavity 40, and then avoiding defects in the formed workpiece.

[0048] See also Figure 5As shown, the molding device of the present invention also includes a feeding mechanism, which includes a lifting plate 35 and a push rod 36 located below the lifting seat 32. The lifting plate 35 is fixedly connected to the lifting seat 32, and the push rod 36 is fixedly connected to the lifting plate 35 and extends in the height direction. The lower mold core is provided with a through hole 173 extending downward from the guide surface 171 with the lowest height of the overflow groove to the bottom surface of the lower mold core. The push rod is connected in the through hole 173 from bottom to top and can move up and down with the lifting seat 32. The width of the guide surface 171 with the highest height in the overflow groove 17 is large. The width of other parts of the overflow groove 171 makes the diameter of the through hole 173 larger than the width of the recess 15. When the extrusion block 33 moves upward with the lifting seat 32 to extrude the workpiece, the push rod 36 moves upward with the lifting seat 32, which can apply an upward extrusion force to the aluminum alloy material in the deepest part of the overflow groove 171, so that the aluminum alloy material in the overflow groove 171 is extruded and deformed. In the process of the aluminum alloy material being extruded, it can be deformed toward the inside of the cavity 40 to supplement the aluminum alloy material inside the cavity. Since the through hole 173 is set at the position where the overflow groove 171 has the greatest depth, the aluminum alloy material can be deformed relatively greatly when the push rod 36 extrude the aluminum alloy material, thereby achieving the purpose of replenishing the aluminum alloy material into the cavity. In addition, since the width of the overflow groove 171 where the through hole 173 is set is increased, the through hole 173 has a diameter greater than the width of the recess 15, the top surface area of ​​the push rod 36 is relatively large, and the area of ​​the aluminum alloy material located inside the overflow groove 171 and squeezed by the push rod 36 is larger, thereby further causing the aluminum alloy material located inside the overflow groove 171 to produce a larger deformation when being squeezed by the push rod 36.

[0049] like Figure 6 , 7 , 9, and combined Figure 1As shown in the figure, the bottom surface of the position where the flow channel 16 is connected to the mold cavity 40 forms an inclined drainage surface 161, and the top of the drainage surface 161 is connected to the bottom of the mold cavity 40, so that the depth of the flow channel 16 gradually increases from the inside to the outside (that is, the depth gradually increases from one end connected to the mold cavity 40 to the other end); the drainage surface 161 is used to guide the semi-solid aluminum alloy material entering the mold cavity, and by setting the inclined drainage surface 161, the part where the flow channel 16 is connected to the mold cavity 40 forms a necking structure, so as to increase the flow velocity of the semi-solid aluminum alloy material when entering the mold cavity 40, so as to facilitate the semi-solid aluminum alloy material to enter the mold cavity. The second space 42 of 40 is filled with aluminum alloy material, and a push rod hole 162 is set on the lower mold 10. Specifically, the push rod hole 162 is set on the lower mold core, and extends upward from the bottom surface of the lower mold core to the bottom of the guide surface 161; the molding device of the present invention also includes an ejection mechanism, the ejection mechanism includes a top mold plate 61, a hydraulic cylinder 62 for driving the top mold plate 61 to move up and down, and a push rod 63 fixed on the top mold plate 61 and extending upward, the push rod 63 is connected to the push rod hole 162 from bottom to top, and can extend into the flow channel 16 as the top mold plate 61 moves upward. After the workpiece is formed, the upper mold 20 is moved to separate the upper mold 20 from the lower mold 10, and the hydraulic cylinder 62 is started to drive the top mold plate 61 to move upward, and then the ejector rod 63 is pushed upward. The ejector rod 63 passes through the top of the ejector rod hole 162 upward, and lifts the workpiece scraps located in the flow channel 16, so that the formed workpiece is separated from the cavity 40. Since the workpiece scraps located in the flow channel 16 are lifted by the ejector rod 63 to realize the demolding of the workpiece, the surface of the workpiece will not be damaged during the demolding process, especially when the ejector rod 63 directly lifts the workpiece upward, the bonding surface 51 and the bonding surface 52 in the workpiece are subjected to a large impact and cracked. The ejector rod hole 162 for the ejector rod 63 to pass through is set at the bottom of the drainage surface 161, ensuring that the drainage surface 161 is a relatively complete surface, and then preventing the gap between the ejector rod 63 and the ejector rod hole 162 from affecting the flow of the semi-solid aluminum alloy material. It should be noted that the hydraulic cylinder 62 mentioned above can also be replaced by other driving components, as long as it can drive the top template 61 to move up and down.

[0050] Fig.10 FIG. 2 shows a schematic diagram of the structure of the second embodiment of the present invention. Unlike the first embodiment in which the extrusion block is reset by its own gravity, the second embodiment applies reverse pressure to the extrusion block by a spring to reset the extrusion block. Fig.10In the illustrated embodiment 2, the components that realize the same function are marked with the same reference numerals; a spring 37 is arranged between the extrusion block 33 and the lower die, and the spring 37 always applies an elastic stress to the extrusion block 33, so that the bottom of the extrusion block 33 always abuts against the push inclined surface 321 of the lifting seat 32, and when the lifting seat 32 moves upward, the extrusion block 33 is pushed upward, so that the extrusion block 33 moves upward along the guide groove 14, and at the same time, the extrusion block 33 squeezes the spring 37 to shrink the spring 37, and when the lifting seat 32 moves downward, the extrusion block 33 is pushed downward by the elastic stress of the spring 37, so that the extrusion block 33 is reset. The spring 37 can be replaced by other elastic elements, such as elastic rubber blocks.

[0051] Fig.11 The lower mold core 18 of the second embodiment of the present invention is shown. Different from the split structure of the lower mold core in the first embodiment, the lower mold core 18 in the second embodiment adopts an integrated structure. The integrated lower mold core 18 is also applicable to the first embodiment.

[0052] The semi-solid forming method of the composite metal material of the present invention adopts the above-mentioned forming device, which comprises the following steps:

[0053] S1, when the upper mold and the lower mold are in the mold opening state, the solid titanium alloy material 51 is placed in the mold cavity 40, the titanium alloy material 51 fills the first space 41 of the mold cavity 40, the upper mold and the lower mold are closed and locked by a clamping mechanism;

[0054] S2, injecting a semi-solid aluminum alloy material 52 into the mold cavity 40 by injection, so that the semi-solid aluminum alloy material 52 fills the second space 42 of the mold cavity 40, and after the aluminum alloy material 52 fills the second space 42, the aluminum alloy material 52 and the titanium alloy material 51 form a first bonding surface 501 and a second bonding surface 502 intersecting each other;

[0055] S3, start the oil cylinder 31, drive the lifting seat 32 to move upward, and push the inclined surface 321 of the lifting seat 32 to push the inclined extrusion block 33 upward to the opening 141 of the guide groove 14, and use the two intersecting extrusion surfaces 331 and 332 on the extrusion block 33 to extrude the semi-solid aluminum alloy material 52 at the same time, and the extrusion forces applied by the extrusion surfaces 331 and 332 to the semi-solid aluminum alloy material 52 are respectively directed toward the first bonding surface 501 and the second bonding surface 502, that is, at the first bonding surface The aluminum alloy material 52 is extruded in the normal direction of the first bonding surface 502 and the second bonding surface 502, so that the oil cylinder 31 maintains an upward thrust on the lifting seat 32, and the extrusion block 33 applies a certain extrusion force to the aluminum alloy material 52 and maintains it for a certain time. The two metals penetrate each other after a certain deformation at the first bonding surface 502 and the second bonding surface 502, so as to increase the adhesion between the two metals. During the extrusion process, the upper mold and the lower mold are continuously heated to keep the internal temperature of the cavity 40 between 350°C and 420°C.

[0056] In the present invention, the inclined extrusion block is pushed upward by the lifting seat, and the two intersecting extrusion surfaces on the extrusion block can simultaneously apply extrusion forces in two directions to the metal material in the cavity. The extrusion forces in the two directions are directly against the two intersecting bonding surfaces of the two metal materials, so that the metal material is extruded in a direction perpendicular or approximately perpendicular to the bonding surface to produce sufficient deformation, eliminating the gap between the two metal materials, preventing the appearance of gaps and cracks between the two, thereby increasing the adhesion of the two metal materials. Since the extrusion force applied by the extrusion block is directed toward the two bonding surfaces respectively, the extrusion force on the two metal materials is prevented from being parallel to the bonding surfaces of the two metal materials or the angle between the two metal materials and the bonding surfaces is too small, and the two metal materials are prevented from being peeled off during the extrusion process, thereby improving the yield rate of composite metal material molding.

[0057] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the inventive concept of the present invention, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present invention.

Claims

1. A semi-solid forming device for composite metal materials, characterized in that: It includes a lower die, an upper die located above the lower die, and an extrusion mechanism; The upper mold and the lower mold form a mold cavity when the mold is closed, and a flow channel connected to the mold cavity for introducing semi-solid metal slurry into the mold cavity. The mold cavity forms a first space for accommodating solid metal material and a second space for accommodating semi-solid metal material. The first space and the second space have two intersecting joint surfaces. The lower mold is provided with an inclined extending guide groove, the angle between the extending direction of the guide groove and the height direction is 45°, and the top of the guide groove extends to the second space of the cavity to form an opening; The extrusion mechanism includes a lifting seat, a driving unit for driving the lifting seat to move up and down in the height direction relative to the lower mold, and an extrusion block. The lifting seat is provided with a push inclined surface. The extrusion block is movably connected to the guide groove, and a matching surface that abuts against the push inclined surface is provided at the bottom thereof. The matching surface cooperates with the push inclined surface to make the extrusion block move along the guide groove toward the direction close to the opening when the lifting seat moves upward. Two intersecting extrusion surfaces are formed on the top of the extrusion block. The two extrusion surfaces are used to simultaneously apply extrusion forces toward the two combining surfaces to the metal material in the second space when the extrusion block moves to the opening of the cavity.

2. The semi-solid forming device of the composite metal material according to claim 1, characterized in that: An elastic element is arranged between the extrusion block and the lower die, and the elastic element is used to always apply an elastic stress to the extrusion block so that the matching surface always abuts against the push inclined surface.

3. The semi-solid forming device of composite metal material according to claim 1, characterized in that: The side of the lifting seat is provided with an inclined guide groove, the bottom surface of the guide groove forms a push inclined surface, and the bottom of the extrusion block is embedded in the guide groove and is limited between the two side walls of the guide groove.

4. The semi-solid forming device of the composite metal material according to any one of claims 1 to 3, characterized in that: The lower mold includes a lower mold plate and a lower mold core embedded in the lower mold plate, the upper mold includes an upper mold plate and an upper mold core embedded in the upper mold plate, the upper surface of the lower mold core is provided with a downwardly recessed recess, the recess includes an outer wall, an inner wall and a bottom wall connected between the bottom of the outer wall and the bottom of the inner wall, when the upper mold and the lower mold are closed, the bottom surface of the upper mold core and the outer wall, inner wall and bottom wall of the recess jointly enclose a forming cavity, a part of the opening is formed on the inner wall, and the other part is formed on the bottom wall, and the two extrusion surfaces on the extrusion block are flush with the inner wall and the bottom wall respectively when moving to the opening.

5. The semi-solid forming device of composite metal material according to claim 4, characterized in that: The lower surface of the lower mold core is provided with an avoidance groove which is recessed upward for accommodating the lifting seat and enabling the lifting seat to move up and down therein. The guide groove extends obliquely upward from the top surface of the avoidance groove to the position where the inner side wall and the bottom wall of the recess are connected. The thickness of the part of the extrusion block located outside the guide groove is greater than the thickness of the part of the extrusion block located inside the guide groove.

6. The semi-solid forming device of composite metal material according to claim 4, characterized in that: One end of the concave is connected to and communicated with the flow channel, and an overflow groove extending from the other end of the concave to the edge of the lower mold core is provided on the lower mold core, and the depth of the overflow groove gradually decreases from one end connected with the concave to the other end.

7. The semi-solid forming device of composite metal material according to claim 6, characterized in that: The upper surface of the lower mold core protrudes from the upper surface of the lower mold plate so that the upper mold plate and the lower mold plate can be gap-matched when the upper mold and the lower mold are closed. The end of the overflow groove with a smaller depth extends to the edge of the lower mold core and is connected to the gap between the upper mold plate and the lower mold plate so that the overflow groove can discharge the air in the cavity to the outside of the upper mold and the lower mold.

8. The semi-solid forming device of composite metal material according to claim 6, characterized in that: The bottom surface of the overflow groove forms multiple guide surfaces arranged along the extension direction of the overflow groove. The heights of the multiple guide surfaces gradually increase from the end of the overflow groove connected to the recess toward the direction away from the recess. Two adjacent guide surfaces are connected together by a retaining wall extending along the height direction.

9. The semi-solid forming device of composite metal material according to claim 8, characterized in that: The molding device also includes a feeding mechanism, which includes a lifting plate located below the lifting seat and fixed to the lifting seat, a push rod fixedly connected to the lifting plate and extending in the height direction, a through hole extending downward from the lowest guide surface on the overflow groove to the bottom surface of the lower mold core is provided on the lower mold core, and the push rod is connected to the through hole from bottom to top to move up and down with the lifting seat; the width of the guide surface at the lowest height in the overflow groove is greater than the width of other parts of the overflow groove so that the diameter of the through hole is greater than the width of the recessed position.

10. The semi-solid forming device of composite metal material according to claim 4, characterized in that: The lower mold core includes a first mold core and a second mold core. The first mold core is provided with a through groove extending from its upper surface to its lower surface. The second mold core is embedded in the through groove and fixedly connected to the first mold core in a detachable manner. The guide groove and the recess are surrounded by the side edge of the second mold core and the inner wall of the through groove.

11. The semi-solid forming device of composite metal material according to claim 1, characterized in that: The lower mold is provided with multiple guide grooves arranged along the extension direction of the cavity, and an extrusion block is embedded in each guide groove. The total opening length of the multiple guide grooves is D, and the length of the cavity is D2, wherein the ratio of D to D2 is greater than or equal to 68%.

12. The semi-solid forming device of composite metal material according to claim 1, characterized in that: An inclined drainage surface is formed on the bottom surface where the flow channel is connected to the cavity, and the top of the drainage surface is connected to the bottom of the cavity so that the depth of the flow channel gradually increases from the inside to the outside. A push rod hole is provided on the lower mold, and the push rod hole extends upward from the bottom surface of the lower mold to the bottom of the drainage surface; the molding device also includes an ejection mechanism, which includes a top mold plate, a driving member for driving the top mold plate to move up and down, and a ejector rod fixed on the top mold plate and extending upward, the ejector rod is connected to the ejector rod hole from bottom to top and can extend into the flow channel as the top mold plate moves upward.

13. A semi-solid forming method of a composite metal material, characterized in that: A semi-solid forming device for composite metal materials according to any one of claims 1 to 12 is used to place a solid metal material in the first space of a mold cavity, and the semi-solid metal material is injected into the second space of the mold cavity so that the semi-solid metal material and the solid metal material form a first bonding surface and a second bonding surface that intersect, and two intersecting extrusion surfaces on an extrusion block are used to simultaneously apply an extrusion force to the semi-solid metal material. When the extrusion block extrude the semi-solid metal material, the two extrusion surfaces on the extrusion block face the first bonding surface and the second bonding surface, respectively, and in the process of extruding the semi-solid metal by the extrusion block, the upper mold and the lower mold are continuously heated.