Corrosion inhibitor feeding device and use method, application in needle coke production
By designing a corrosion inhibitor feeding device and using a combination of high-temperature vaporized corrosion inhibitors, arc-shaped spoilers, and spiral spoilers, the problems of high cost and poor anti-rust effect of liquid corrosion inhibitors were solved, and the mitigation effect was achieved. Uniform coating of corrosive agents and improved corrosion resistance of pipelines.
Patent Information
- Application Number
- CN202410659659.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-27
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-05-27
AI Technical Summary
In the production process of needle coke, liquid corrosion inhibitors are expensive and cannot enter the thermal equipment system in large quantities, resulting in a small effective amount of corrosion inhibitors during transportation, and the anti-rust effect of solid corrosion inhibitors in transportation pipelines is poor.
A corrosion inhibitor feeding device is designed, including a feeder, a preheater, a blower, a drying filter, a jet disk, a vortex heat pipe, a liquid feed pump, a feed pipe and an arc spoiler. The vaporized corrosion inhibitor vaporizes in the vortex heat-conducting tube and is introduced into the conveying pipeline through the material guide tube. The arc spoiler and spiral spoiler are used to achieve uniform coating and mixing.
The amount of corrosion inhibitor is reduced, the uniformity of the coating and the corrosion resistance of the transportation pipeline are improved, and the acidity of the light fraction is detected in real time to adjust the feeding strategy to ensure effective protection.
Smart Images

Figure CN118454426B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of needle coke production, and in particular to a corrosion inhibitor feeding device and a use method thereof, and application in needle coke production. Background Art
[0002] Needle coke is a high-quality variety of carbon material that has been vigorously developed. It has the appearance of a silver-grey, metallic-luster porous solid. Its structure has obvious flow texture, with large, few and slightly elliptical pores. The particles have a large aspect ratio, with a fibrous or needle-like texture and a lubricious feel. It is the raw material for producing high-end carbon products such as ultra-high power electrodes, special carbon materials, carbon fibers and their composite materials. Needle coke produced with petroleum residue as raw material is oil-based needle coke; needle coke produced with coal tar pitch and its fractions as raw material is coal-based needle coke. During the production of needle coke, the coking raw materials undergo thermal cracking and condensation reactions to form an intermediate phase liquid crystal. The generated oil and gas enter the distillation tower and are fractionated to obtain gas and light fractions. However, when the gas and light fractions are discharged, they are highly corrosive and will seriously damage the transmission pipeline. Therefore, it is necessary to introduce corrosion inhibitors into the gas transmission pipeline to enhance the corrosion resistance of the transmission pipeline.
[0003] The corrosion inhibitor tank in the corrosion inhibitor feeding device for needle coke production with application number CN202221546952.X can drive the corrosion inhibitor to be stably transported through the suction pipe, pneumatic diaphragm pump and conveying pipeline, and the liquid outlet and the conveying pipeline can be raised and lowered by the lifting rod and the lifting groove, and the liquid outlet and the conveying pipeline are clamped and fixed by the clamping block, so that it can be connected to the use equipment.
[0004] However, in actual use, corrosion inhibitors are divided into solid and liquid forms. The liquid corrosion inhibitors currently developed have a good anti-corrosion effect in the needle coke system pipeline. However, the cost of liquid corrosion inhibitors is relatively high, and liquid corrosion inhibitors cannot directly enter the thermal equipment system in large quantities with water vapor, resulting in a small amount of effective corrosion inhibitor in the transportation process, which will lead to excessive use of corrosion inhibitors. In addition, when the corrosion inhibitor is input into the transportation pipeline through the corrosion inhibitor tank, although a preheater can be used for preheating, the corrosion inhibitor is introduced in the form of steam.
[0005] In view of this, it is necessary for the present invention to provide a corrosion inhibitor feeding device and a method of use to solve the above problems. Summary of the invention
[0006] The object of the present invention is to provide a corrosion inhibitor feeding device and a method of use, and application in needle coke production, so as to solve the problems raised in the above background technology.
[0007] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a corrosion inhibitor feeding device, comprising a feeder, an air inlet pipe is fixedly installed at the bottom of the feeder, a preheater, a blower and a drying filter are sequentially installed on the air inlet pipe, an air jet disk connected to the air inlet pipe is fixed inside the feeder, a vortex heat conduction pipe is arranged above the air jet disk, a feed pipe connected to the vortex heat conduction pipe is fixedly installed on the outer wall of the feeder, a liquid feed pump is fixedly installed on the feed pipe, a discharge seat is fixed on the top of the feeder, a material guide pipe is connected and installed on the discharge seat, and the other end of the material guide pipe is fixedly installed with the feed seat;
[0008] An air guide channel is provided in the discharge seat, an annular heat preservation chamber is provided in the guide pipe, and an electric control valve is provided between the air guide channel and the heat preservation chamber, an exhaust pressure valve connected to the heat preservation chamber is fixed on the guide pipe, and a sampling valve is fixed on the guide pipe.
[0009] Preferably, the size of the vortex heat pipe matches that of the jet disk, and the surface of the vortex heat pipe is evenly provided with gasification holes opening upward, and the top of the jet disk is evenly provided with exhaust ports, and the exhaust ports face the vortex heat pipe.
[0010] Preferably, the inner cavity of the material guide tube is provided with a gasification channel along the axis, the inner part of the material discharge seat is provided with a material guide channel connected with the gasification channel, the heat preservation chamber is arranged outside the gasification channel, and the electric control valve controls the opening and closing state of the heat preservation chamber.
[0011] Preferably, the sampling valve is connected to a corrosion inhibitor concentration meter via a sampling tube, and the exhaust pressure valve and the electric control valve are both connected to a controller.
[0012] Preferably, the feeder is applied to a distillation tower in a process for preparing needle coke, and a mixing seat is fixed on the top of the distillation tower, the feed seat and the mixing seat are connected and assembled, the other end of the mixing seat is integrally formed and connected with a feed pipe in a 90-degree bent state, a pH meter is fixedly installed on the mixing seat, an arc-shaped spoiler plate accommodated inside the mixing seat is fixedly installed at the outlet of the feed seat, and a spiral spoiler plate arranged along the axial centerline direction is fixedly installed on the inner side wall of the feed pipe;
[0013] The lower end of the spiral spoiler is directly opposite to the arc spoiler, the tangent direction of the top end of the arc spoiler is directly corresponding to the inlet of the spiral spoiler, the pH meter is installed on the mixing seat at the corresponding position of the top end of the arc spoiler, and the pH meter and the top end of the arc spoiler are arranged on the same horizontal plane.
[0014] Preferably, the arc-shaped spoiler is a memory alloy sheet, the initial inclination angle of the top tangent direction of the arc-shaped spoiler is 60 degrees, and when the arc-shaped spoiler is bent to the final state under heat, the inclination angle of the top tangent direction of the arc-shaped spoiler is 30 degrees.
[0015] Preferably, a middle distillate oil discharge pipe is installed at the middle position of the side wall of the distillation tower, and a heavy distillate oil discharge pipe is installed at the bottom of the distillation tower.
[0016] The present invention also discloses a method for using the corrosion inhibitor feeding device, and the specific steps of the method for using the device are as follows:
[0017] S1: Start the blower. When the gas passes through the intake pipe, it will first be dried by the filter drier to obtain clean air. Then the preheater heats the clean air and then it is sprayed into the feeder through the jet disc, making the gas thermally conductive and completing the preheating of the feeder.
[0018] S2: Open the electric control valve, so that the hot air inside the feeder is directly introduced into the insulation chamber through the air guide channel. When the gas pressure value inside the insulation chamber reaches the threshold of the exhaust pressure valve, the gas is discharged through the exhaust pressure valve, so as to realize the discharge of the gas inside the feeder that has not been heated and dried, and ensure the dryness and consistency of the gas entering the feeder;
[0019] S3: As the preheater works, the temperature of the gas introduced into the feeder gradually increases. During this process, the high-temperature gas inside the feeder heats the vortex heat pipe, and the high-temperature gas introduced into the insulation chamber continues to preheat the feed pipe. When the temperature reaches the standard, the electric control valve is closed. At this time, high-temperature gas gathers in the insulation chamber, which has a heat preservation effect on the feed pipe.
[0020] S4: After closing the solenoid valve, the liquid feed pump starts working (in this way, when the corrosion inhibitor flows through the material guide pipe, it is still within the time period of heat preservation in the material guide pipe, which can avoid continuous heat dissipation and cooling during the long production process, and the insulation effect decreases and disappears over time), and the liquid corrosion inhibitor is injected into the vortex heat conduction pipe through the feed pipe. The liquid corrosion inhibitor is quickly vaporized inside the vortex heat conduction pipe under high temperature and sprayed out from the vaporization hole. In this way, the liquid corrosion inhibitor introduced into the vortex heat conduction pipe is continuously vaporized. The effective components of the vaporized corrosion inhibitor are introduced into the mixing seat through the high-temperature clean air through the discharge seat, the material guide pipe, and the feed seat. The vaporized corrosion inhibitor and the light fraction discharged from the distillation tower are mixed and enter the spiral spoiler under the turbulence of the arc spoiler, and then enter the feed pipe after being turbulent by the spiral spoiler. In this way, the corrosion inhibitor components act on the inner wall of the feed pipe in a spiral feeding manner to complete the anti-corrosion effect.
[0021] The invention also discloses the application of a corrosion inhibitor feeding device in the production of needle coke.
[0022] Technical effects and advantages of the present invention:
[0023] 1. In the present invention, the gasified corrosion inhibitor discharged from the guide pipe is introduced into the mixing seat through the feed seat. Under the turbulent effect of the arc spoiler, the gasified corrosion inhibitor airflow can be directly guided to the spiral spoiler to avoid the airflow directly blowing to the inner wall of the mixing seat and generating turbulence, resulting in uneven coating of the corrosion inhibitor. The gasified corrosion inhibitor entering the spiral spoiler can flow along the spiral spoiler and form a swirling corrosion inhibitor airflow in the feed pipe, which is convenient for the gasified corrosion inhibitor to be evenly coated on the inner wall of the feed pipe. This can reduce the amount of corrosion inhibitor used and improve the uniformity of the corrosion inhibitor coating, thereby improving the corrosion resistance of the feed pipe.
[0024] 2. The arc-shaped spoiler of the present invention can block the light fraction, so that the light fraction airflow can only flow between the arc-shaped spoiler and the inner wall of the mixing seat, which has a gathering and guiding effect on the light fraction. At this time, the pH meter can accurately detect the pH of the light fraction in real time to prevent the light fraction from being too dispersed and affecting the pH detection. The flow of the gas corrosion inhibitor airflow can be used to accelerate the flow of the light fraction and increase the discharge speed of the light fraction, so that the gasification corrosion inhibitor airflow and the light fraction airflow are gathered at the spiral spoiler and synchronously transported along the spiral spoiler. In this way, the gasification corrosion inhibitor airflow can be fully mixed with the light fraction. At the same time, as the mixed gas flows, the gasification corrosion inhibitor is evenly coated on the inner wall of the feed pipe to complete the corrosion protection of the feed pipe.
[0025] 3. The pH meter of the present invention can detect the acidity of the light fraction in real time, so that the feeding strategy of the feeder can be adjusted in real time according to the acidity of the light fraction, so that the feed pipe can be better protected when the acidity of the light fraction changes. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a schematic diagram of the overall structure of the present invention;
[0027] Figure 2 It is a schematic diagram of the overall structure of the feeder of the present invention;
[0028] Figure 3 This is a schematic diagram of the cross-sectional structure of the feeder of the present invention;
[0029] Figure 4 This is a schematic diagram of the cross-sectional structure of the assembly of the material discharging seat and the material guiding pipe of the present invention;
[0030] Figure 5 It is a schematic diagram of the structure of the vortex heat conducting pipe of the present invention;
[0031] Figure 6 This is a schematic diagram of the cross-sectional structure of the distillation tower assembly of the present invention;
[0032] Figure 7 It is a schematic diagram of the assembly structure of the present invention.
[0033] In the figure: 1. feeder; 2. air inlet pipe; 3. preheater; 4. blower; 5. filter drier; 6. feed pipe; 7. liquid feed pump; 8. discharge seat; 9. guide pipe; 10. air guide channel; 11. insulation chamber; 12. electric control valve; 13. exhaust pressure valve; 14. sampling valve; 15. jet disc; 16. vortex heat conduction pipe; 161. gasification hole; 17. feed seat; 18. distillation tower; 19. mixing seat; 20. feed pipe; 21. pH meter; 22. middle distillate oil discharge pipe; 23. heavy distillate oil discharge pipe; 24. arc spoiler; 25. spiral spoiler. DETAILED DESCRIPTION
[0034] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. Example 1
[0035] like Figures 1 to 7 As shown, this embodiment provides a corrosion inhibitor feeding device, including a feeder 1, an air intake pipe 2 is fixedly mounted at the bottom of the feeder 1, and a preheater 3, a blower 4 and a drying filter 5 are sequentially installed on the air intake pipe 2. When the blower 4 is started, the gas will first be dried by the drying filter 5 to obtain clean air when passing through the air intake pipe 2. A jet disk 15 connected to the air intake pipe 2 is fixed inside the feeder 1. The preheater 3 heats the clean air and then sprays it into the feeder 1 through the jet disk 15, so that the gas is dried and heated, thereby completing the preheating effect on the feeder 1.
[0036] See also Figure 3 A vortex heat conducting pipe 16 is arranged above the jet disc 15, a feed pipe 6 connected to the vortex heat conducting pipe 16 is fixed to the outer wall of the feeder 1, a liquid feed pump 7 is fixedly mounted on the feed pipe 6, a discharge seat 8 is fixed on the top of the feeder 1, a material guide pipe 9 is connected to the discharge seat 8, a feed seat 17 is fixedly mounted on the other end of the material guide pipe 9, an air guide channel 10 is opened in the discharge seat 8, an annular heat preservation chamber 11 is arranged in the material guide pipe 9, and the air guide channel 10 An electric control valve 12 is provided in communication with the insulation chamber 11, an exhaust pressure valve 13 in communication with the insulation chamber 11 is fixed on the material guide pipe 9, a sampling valve 14 is fixed on the material guide pipe 9 between the discharge seat 8 and the exhaust pressure valve 13, the size of the vortex heat conducting pipe 16 matches the size of the jet disk 15, and the surface of the vortex heat conducting pipe 16 is evenly provided with gasification holes 161 with openings facing upward, and the top of the jet disk 15 is evenly provided with exhaust ports, and the exhaust ports are directly opposite to the vortex heat conducting pipe 16.
[0037] The sampling valve 14 is connected to a corrosion inhibitor concentration meter (the prior art commonly used in the needle coke production process, which will not be described in detail here) through a sampling tube. The concentration of the gasified corrosion inhibitor derived from the guide pipe 9 can be directly measured through the corrosion inhibitor concentration meter. The exhaust pressure valve 13 and the electric control valve 12 are both connected to the controller. In actual use, after the electric control valve 12 is opened by the controller, the hot air inside the feeder 1 is directly introduced into the insulation chamber 11 through the air guide channel 10. When the gas pressure value inside the insulation chamber 11 reaches the threshold value of the exhaust pressure valve 13, the gas passes through the exhaust pressure valve 13. Valve 13 discharges, realizing the discharge of the unheated and undried gas inside the feeder 1, ensuring the dryness and consistency of the gas entering the feeder 1. As the preheater 3 works, the temperature of the gas introduced into the feeder 1 gradually increases. In this process, the high-temperature gas inside the feeder 1 heats the vortex heat pipe 16, and the high-temperature gas introduced into the insulation chamber 11 continues to preheat the guide pipe 9. When the temperature standard is reached, the electric control valve 12 is closed. At this time, high-temperature gas gathers in the insulation chamber 11, which has an insulation effect on the guide pipe 9.
[0038] Among them, the inner cavity of the material guide pipe 9 is provided with a gasification channel along the axial line, the inner part of the material discharge seat 8 is provided with a material guide channel connected with the gasification channel, the insulation chamber 11 is arranged on the outside of the gasification channel, and the electric control valve 12 controls the opening and closing state of the insulation chamber 11 to ensure the preheating and heat preservation effect of the insulation chamber 11 on the gasification channel, thereby preventing the gasified corrosion inhibitor from being condensed into liquid when it encounters cold during transportation.
[0039] It is worth noting that the present invention also discloses an application of the corrosion inhibitor feeding device as described above in the production of needle coke. The feeder 1 provided by the present invention is applied to a distillation tower 18 in the process of preparing needle coke. An intermediate distillate oil discharge pipe 22 is installed at the middle position of the side wall of the distillation tower 18, and a heavy distillate oil discharge pipe 23 is installed at the bottom of the distillation tower 18. During the distillation process of the distillation tower 18, the supply of the gasification corrosion inhibitor is realized through the cooperation of the feeder 1, and the light distillate conveying pipeline is protected from corrosion in real time to improve the corrosion resistance. Specifically:
[0040] See also Figure 1 , Figure 6 and Figure 7 A mixing seat 19 is fixed on the top of the distillation tower 18, the feed seat 17 and the mixing seat 19 are connected and assembled, the other end of the mixing seat 19 is integrally formed and connected with a feed pipe 20 which is bent at 90 degrees, a pH meter 21 is fixedly assembled on the mixing seat 19, an arc-shaped spoiler 24 housed inside the mixing seat 19 is fixedly arranged at the outlet of the feed seat 17, and a spiral spoiler 25 arranged along the axial direction is fixedly arranged on the inner wall of the feed pipe 20.
[0041] The vaporized corrosion inhibitor discharged from the guide pipe 9 is introduced into the mixing seat 19 through the feed seat 17. Under the turbulent effect of the arc-shaped spoiler 24, the vaporized corrosion inhibitor airflow can be directly guided to the spiral spoiler 25, so as to avoid the airflow directly blowing to the inner wall of the mixing seat 19 and generating turbulence, resulting in uneven coating of the corrosion inhibitor. The vaporized corrosion inhibitor entering the spiral spoiler 25 can flow along the spiral spoiler 25, and can form a swirling corrosion inhibitor airflow in the feed pipe 20, so that the vaporized corrosion inhibitor is evenly coated on the inner wall of the feed pipe 20. This can reduce the amount of corrosion inhibitor used while improving the uniformity of the corrosion inhibitor coating and the corrosion resistance of the feed pipe 20.
[0042] It is worth noting that see 6 and Figure 7 The lower end of the spiral spoiler 25 is directly opposite to the arc spoiler 24, and the tangential direction of the top of the arc spoiler 24 corresponds to the entrance of the spiral spoiler 25. The pH meter 21 is installed on the mixing seat 19 and at the corresponding position of the top of the arc spoiler 24. The pH meter 21 and the top of the arc spoiler 24 are arranged on the same horizontal plane. When the gasification corrosion inhibitor is introduced from the feed seat 17 into the mixing seat 19, the arc spoiler 24 can change the direction of the airflow, so that the airflow flows directly into the spiral spoiler 25, ensuring the consistency of the airflow, and improving the efficiency of the gasification corrosion inhibitor coating on the feed pipe 20. In this way, while achieving airflow guidance, it can prevent the gasification corrosion inhibitor airflow from generating resistance to the light fraction discharged from the distillation tower 18, and when the light fraction in the distillation tower 18 is transported through the mixing seat 19, the arc spoiler 24 can block the light fraction, so that the light fraction airflow only It can flow between the arc-shaped spoiler 24 and the inner wall of the mixing seat 19, and has a gathering and guiding effect on the light fraction. At this time, the pH meter can accurately detect the pH of the light fraction in real time to prevent the light fraction from being too dispersed and affecting the pH detection. In addition, the gasification corrosion inhibitor airflow and the light fraction airflow are introduced into the conveying pipe 20 together, and the flow rate of the gasification corrosion inhibitor airflow is greater than the flow rate of the light fraction airflow. In this way, the flow of the gas corrosion inhibitor airflow can be used to accelerate the flow of the light fraction and increase the discharge speed of the light fraction, so that the gasification corrosion inhibitor airflow and the light fraction airflow are gathered at the spiral spoiler 25 and synchronously transported along the spiral spoiler 25. In this way, the gasification corrosion inhibitor airflow can be fully mixed with the light fraction. At the same time, as the mixed gas flows, the gasification corrosion inhibitor is evenly coated on the inner wall of the conveying pipe 20 to complete the corrosion protection of the conveying pipe 20.
[0043] It is worth noting that the arc-shaped spoiler 24 is a memory alloy sheet, and the initial inclination angle of the top tangent direction of the arc-shaped spoiler 24 is 60 degrees. The arc-shaped spoiler 24 will gradually bend when heated under heating conditions, that is, the arc-shaped spoiler 24 will gradually move closer to the horizontal direction, so that the angle between the top of the arc-shaped spoiler 24 and the horizontal direction will become smaller and smaller, and the inclination angle of the top tangent direction in the final state after heating is 30 degrees.
[0044] In actual use, the first round of gasification corrosion inhibitor coating operation is completed in advance through the feeder 1, and then the light fraction discharged from the distillation tower 18 during operation is introduced into the feed pipe 20 through the mixing seat 19, and then discharged for collection, so as to facilitate unified processing in the next step. In the process of light fraction discharge, the pH meter 21 can detect the acidity of the light fraction in real time, so that the feeding strategy of the feeder 1 can be adjusted in real time according to the acidity of the light fraction, so that the feed pipe 20 can be better protected when the acidity of the light fraction changes. The specific process is as follows:
[0045] When the pH meter 21 detects that the acidity of the light fraction has decreased from the standard value and is not less than the first threshold value, it indicates that the acidity of the light fraction has increased, but the corrosiveness is still not great. Therefore, in order to reduce the contact time between the light fraction and the inner wall of the feed pipe 20, the controller controls the blower 4 to increase its power, thereby increasing the feed rate of the gasified corrosion inhibitor discharged from the feed guide pipe 9. The gasified corrosion inhibitor airflow with increased speed will intensify the flow rate of the light fraction in the mixing seat 19, thereby increasing the flow rate of the light fraction in the feed pipe 20. This will greatly reduce the contact time between the light fraction and the inner wall of the feed pipe 20, thereby improving the corrosion protection of the feed pipe 20.
[0046] When the pH meter 21 detects that the acidity of the light fraction has dropped from the standard value to no more than the first threshold value, it indicates that the acidity of the light fraction has increased significantly and is in a strong acid state. At this time, the corrosiveness of the light fraction to the feed pipe 20 increases. At this time, the controller controls the preheater 3 to increase the power, so that the heat supply increases. When the vortex heat pipe 16 is heated, the amount of corrosion inhibitor vaporized per unit time can be increased. At the same time, the controller controls the liquid feed pump 7 to increase the liquid supply, so that the concentration of the gas corrosion inhibitor discharged from the feed pipe 9 increases. In this way, when the gasified corrosion inhibitor is led out from the feed seat 17, not only the concentration increases but also the temperature increases. Such a temperature increase can cause the arc spoiler 24 to be heated, and then the curvature begins to decrease, that is, the top of the arc spoiler 24 and the inner wall of the mixing seat 19 The smaller the air flow channel between them, the reduced air flow channel can be used to increase the flow velocity of the light fraction, and the flow velocity of the gasification corrosion inhibitor flowing from the arc spoiler 24 will be reduced. In this way, the accelerated light fraction speed is used to drive the gasification corrosion inhibitor with a reduced speed to flow. Since the flow velocity of the gasification corrosion inhibitor is reduced, and the concentration of the gasification corrosion inhibitor is increased, the amount of gasification corrosion inhibitor mixed in the amount of light fraction flowing per unit time will increase significantly. In this way, the amount of corrosion inhibitor in the light fraction can be increased to block its corrosive effect on the feed pipe 20. At the same time, the effective ingredients of the gasification corrosion inhibitor will adhere to the inner wall of the feed pipe 20 as the light fraction airflow flows, which can further achieve the barrier of the light fraction and complete the corrosion protection of the inner wall of the feed pipe 20.
[0047] When the pH meter 21 detects that the acidity of the light fraction has dropped from the standard value to the second threshold value, it indicates that the acidity of the light fraction discharged from the distillation tower 18 is too high, which is an over-standard production. At this time, the distillation tower 18 should be shut down to check the setting parameters to ensure that the acidity of the discharged light fraction is within the acceptable range. Example 2
[0048] This embodiment also discloses a method for using the corrosion inhibitor feeding device as described above, and the specific steps of the method for using the device are as follows:
[0049] S1: Start the blower 4. When the gas passes through the air inlet pipe 2, it will first be dried by the drying filter 5 to obtain clean air. Then, the preheater 3 heats the clean air. Then, the preheater 3 injects the clean air into the feeder 1 through the jet disc 15, so that the gas has thermal conductivity and completes the preheating of the feeder 1.
[0050] S2: Open the electric control valve 12, so that the hot air inside the feeder 1 is directly introduced into the heat preservation chamber 11 through the air guide channel 10. When the gas pressure value inside the heat preservation chamber 11 reaches the threshold value of the exhaust pressure valve 13, the gas is discharged through the exhaust pressure valve 13, so as to realize the discharge of the unheated dry gas inside the feeder 1, and ensure the dryness and consistency of the gas entering the feeder 1;
[0051] S3: As the preheater 3 works, the temperature of the gas introduced into the feeder 1 gradually increases. During this process, the high-temperature gas inside the feeder 1 heats the vortex heat-conducting pipe 16, and the high-temperature gas introduced into the heat-insulating chamber 11 continues to preheat the material guide pipe 9. When the temperature reaches the standard, the electric control valve 12 is closed. At this time, the high-temperature gas is accumulated in the heat-insulating chamber 11, which has a heat-insulating effect on the material guide pipe 9.
[0052] S4: After closing the solenoid valve 12, the liquid feeding pump 7 starts to work (so that when the corrosion inhibitor flows through the material guide pipe 9, it is still within the time period of the material guide pipe 9 for insulation, which can avoid continuous heat dissipation and cooling during the long production process, and the insulation effect is reduced to disappear over time), and the liquid corrosion inhibitor is injected into the vortex heat conducting pipe 16 through the feed pipe 6. The liquid corrosion inhibitor is quickly vaporized inside the vortex heat conducting pipe 16 under the high temperature state, and is ejected from the vaporization hole 161. The effective components of the vaporized corrosion inhibitor are introduced into the mixing seat 19 through the high-temperature clean air through the discharge seat 8, the material guide pipe 9, and the feed seat 17. The vaporized corrosion inhibitor and the light fraction discharged from the distillation tower 18 are mixed and enter the spiral spoiler 25 under the turbulence of the arc spoiler 24, and then enter the feed pipe 20 after being turbulent by the spiral spoiler 25. In this way, the corrosion inhibitor components act on the inner wall of the feed pipe 20 in a spiral feeding manner to complete the anti-corrosion effect.
[0053] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A corrosion inhibitor feeding device, comprising a feeder (1), wherein an air inlet pipe (2) is fixedly mounted at the bottom of the feeder (1), and a preheater (3), a blower (4) and a drying filter (5) are sequentially mounted on the air inlet pipe (2), characterized in that: The feeder (1) is internally fixed with an air jet disc (15) connected to the air inlet pipe (2), a vortex heat conduction pipe (16) is arranged above the air jet disc (15), a feed pipe (6) connected to the vortex heat conduction pipe (16) is fixed to the outer wall of the feeder (1), a liquid feed pump (7) is fixedly mounted on the feed pipe (6), a discharge seat (8) is fixed on the top of the feeder (1), a material guide pipe (9) is connected to the discharge seat (8), and a feed seat (17) is fixedly mounted on the other end of the material guide pipe (9); An air guide channel (10) is provided in the material discharging seat (8), an annular heat preservation chamber (11) is provided in the material guiding pipe (9), an electric control valve (12) is provided in communication between the air guide channel (10) and the heat preservation chamber (11), an exhaust pressure valve (13) in communication with the heat preservation chamber (11) is fixed on the material guiding pipe (9), and a sampling valve (14) is fixed on the material guiding pipe (9); The feeder (1) is applied to a distillation tower (18) in a process for preparing needle coke, and a mixing seat (19) is fixed on the top of the distillation tower (18), the feed seat (17) and the mixing seat (19) are connected and assembled, the other end of the mixing seat (19) is integrally formed and connected with a feed pipe (20) in a 90-degree bent state, a pH meter (21) is fixedly assembled on the mixing seat (19), an arc-shaped spoiler (24) stored in the mixing seat (19) is fixedly arranged at the outlet of the feed seat (17), and a spiral spoiler (25) arranged along the axial direction is fixedly arranged on the inner wall of the feed pipe (20); The lower end of the spiral spoiler (25) is directly opposite to the arc spoiler (24), the tangent direction of the top end of the arc spoiler (24) is directly corresponding to the inlet of the spiral spoiler (25), the pH meter (21) is installed on the mixing seat (19) at a position corresponding to the top end of the arc spoiler (24), and the pH meter (21) and the top end of the arc spoiler (24) are arranged on the same horizontal plane; The arc-shaped spoiler (24) is a memory alloy sheet, the initial inclination angle of the top tangent direction of the arc-shaped spoiler (24) is 60 degrees, and when the arc-shaped spoiler (24) is bent to a final state under heat, the inclination angle of the top tangent direction of the arc-shaped spoiler (24) is 30 degrees; A middle distillate oil discharge pipe (22) is installed at the middle position of the side wall of the distillation tower (18), and a heavy distillate oil discharge pipe (23) is installed at the bottom of the distillation tower (18).
2. The corrosion inhibitor feeding device according to claim 1, characterized in that: The size of the vortex heat conducting pipe (16) matches that of the jet disk (15), and the surface of the vortex heat conducting pipe (16) is evenly provided with gasification holes (161) opening upward, and the top of the jet disk (15) is evenly provided with exhaust ports, which are directly opposite to the vortex heat conducting pipe (16).
3. The corrosion inhibitor feeding device according to claim 2, characterized in that: The inner cavity of the material guide pipe (9) is provided with a gasification channel along the axis, the inner cavity of the material discharge seat (8) is provided with a material guide channel connected to the gasification channel, the heat preservation chamber (11) is arranged outside the gasification channel, and the electric control valve (12) controls the opening and closing state of the heat preservation chamber (11).
4. The corrosion inhibitor feeding device according to claim 3, characterized in that: The sampling valve (14) is connected to a corrosion inhibitor concentration meter via a sampling tube, and the exhaust pressure valve (13) and the electric control valve (12) are both connected to a controller.
5. A method for using the corrosion inhibitor feeding device according to claim 4, characterized in that: The specific steps of use are: S1: Start the blower (4). When the gas passes through the air inlet pipe (2), it is first dried by the drying filter (5) to obtain clean air. Then, the preheater (3) heats the clean air. The clean air is then injected into the feeder (1) through the jet disc (15), so that the gas has thermal conductivity, thereby completing the preheating of the feeder (1); S2: Open the electric control valve (12), so that the hot air inside the feeder (1) is directly introduced into the heat preservation chamber (11) through the air guide channel (10), and when the gas pressure value inside the heat preservation chamber (11) reaches the threshold value of the exhaust pressure valve (13), the gas is discharged through the exhaust pressure valve (13), so that the unheated dry gas inside the feeder (1) is discharged to the outside, thereby ensuring the dryness and consistency of the gas entering the feeder (1); S3: As the preheater (3) works, the temperature of the gas introduced into the feeder (1) gradually increases. During this process, the high-temperature gas inside the feeder (1) heats the vortex heat conducting pipe (16), while the high-temperature gas introduced into the heat preservation chamber (11) continues to preheat the material guide pipe (9). When the temperature reaches the standard, the electric control valve (12) is closed. At this time, the high-temperature gas is accumulated in the heat preservation chamber (11), which has a heat preservation effect on the material guide pipe (9); S4: After closing the electric control valve (12), the liquid feed pump (7) starts to work. In this way, when the corrosion inhibitor flows through the material guide pipe (9), it is still within the time period of heat preservation in the material guide pipe (9), which can avoid continuous heat dissipation and cooling during the long production process. The heat preservation effect decreases and disappears over time. The liquid corrosion inhibitor is injected into the vortex heat conduction pipe (16) through the feed pipe (6). The liquid corrosion inhibitor is quickly vaporized inside the vortex heat conduction pipe (16) in a high temperature state and is ejected from the vaporization hole (161). In this way, it is continuously vaporized and introduced into the vortex heat conduction pipe ( The liquid corrosion inhibitor in 16) is vaporized, and the effective components of the corrosion inhibitor are introduced into the mixing seat (19) along with the high-temperature clean air through the discharge seat (8), the guide pipe (9), and the feed seat (17). The vaporized corrosion inhibitor and the light fraction discharged from the distillation tower (18) are mixed and enter the spiral spoiler (25) under the turbulence of the arc spoiler (24), and then enter the feed pipe (20) after being turbulent by the spiral spoiler (25). In this way, the corrosion inhibitor components act on the inner wall of the feed pipe (20) in a spiral feeding manner to complete the anti-corrosion effect.
6. Use of the corrosion inhibitor feeding device according to any one of claims 1 to 4 in needle coke production.
Citation Information
Patent Citations
Corrosion inhibitor feeding device for needle coke production
CN217627610U
Gas supply equipment and bactericide supply method
CN117224723A
Liquid corrosion inhibitor gasification device
CN216813788U