Nanocolumn array substrate for Raman spectroscopy imaging, preparation method thereof, and detection chip

By forming isotropic etching treatment of mask patterns and functional layers on the wafer substrate, combined with shallow silicon etching technology, the accuracy and efficiency problems of micron column arrays in the prior art are solved, and high precision and high efficiency are achieved. Nanocolumn array substrate preparation, suitable for Raman spectral imaging detection of exosomes.

CN118458688BActive Publication Date: 2024-11-01PEKING UNIV
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202410910279.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-09
Publication Date
2024-11-01
Estimated Expiration
2044-07-09

AI Technical Summary

Technical Problem

The existing micro-column arrays prepared based on electron beam lithography technology have high accuracy requirements when detecting exosomes and are not suitable for large-scale production, with slow processing efficiency, making it difficult to achieve high-precision and high-efficiency mass production.

Method used

Using the preparation method of combining wafer substrate, original functional layer and mask pattern, nano-column array substrate is formed through isotropic etching treatment, which is used for exosome detection of Raman spectroscopy imaging, and is improved with shallow silicon etching technology. Accuracy and efficiency.

Benefits of technology

The preparation of high-precision nanocolumn array substrate is realized, the production efficiency and accuracy of the detection chip are improved, and it is suitable for efficient detection of exosomes in Raman spectral imaging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118458688B_ABST
    Figure CN118458688B_ABST
Patent Text Reader

Abstract

The present application provides a nanocolumn array substrate for Raman spectroscopy imaging, a preparation method thereof, and a detection chip, which relates to the technical field of detection chips, and provides a wafer substrate, on one side of which an original functional layer is formed; on the side of the original functional layer away from the wafer substrate, a plurality of first mask patterns arranged in an array along the row direction and the column direction are formed; the original functional layer is isotropically etched using the first mask pattern as a mask to form a plurality of original functional structures; the first mask pattern is removed, and the wafer substrate is subjected to shallow and deep silicon etching using the original functional structure as a mask to form a nanocolumn array substrate. This method combines isotropic etching to form a plurality of target functional structures arranged in an array on the wafer substrate, effectively improving the accuracy of the target functional structure formed by photolithography, and realizing the preparation of a high-precision nanocolumn array substrate through a low-precision photolithography technology that requires a mask, which is further applied to the detection of exosomes in Raman spectroscopy imaging.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of detection chips, and in particular to a nanorod array substrate for Raman spectroscopy imaging, a preparation method thereof, and a detection chip. Background Art

[0002] Exosomes are small extracellular vesicles with a lipid bilayer membrane structure and a diameter of about 30-180 nm. Recent studies have found that exosomes play an important role in physiological and pathological phenomena, such as antigen presentation in immunity, tumor growth and migration, and repair of tissue damage. Surface enhanced Raman scattering (SERS) technology is an emerging biomarker and is often used to detect exosomes.

[0003] The existing SERS-based exosome detection technology uses antibodies modified on micron column arrays and corresponding proteins on vesicles to specifically bind to achieve vesicle capture. It has high requirements on the precision of micron column arrays and is usually prepared by electron beam lithography. However, electron beam lithography is slow in processing efficiency and is not suitable for large-scale production of high-precision micron column arrays for detecting exosomes. Therefore, how to improve the preparation efficiency and mass production accuracy of high-precision micron column arrays has become a problem that needs to be solved in this field. Summary of the invention

[0004] The present application provides a nanocolumn array substrate for Raman spectroscopy imaging, a preparation method thereof, and a detection chip to solve the problem that the existing photolithography technology cannot mass-produce high-precision microcolumn arrays for detecting exosomes.

[0005] In a first aspect of an embodiment of the present application, a method for preparing a nanorod array substrate for Raman spectroscopy imaging is provided, the method comprising:

[0006] Providing a wafer substrate;

[0007] forming an original functional layer on one side of the wafer substrate, wherein the original functional layer is a single-atom film layer for binding target exosomes;

[0008] Forming a plurality of first mask patterns arranged in an array along row directions and column directions on a side of the original functional layer away from the wafer substrate;

[0009] Using the plurality of first mask patterns as masks, the original functional layer is isotropically etched to form a plurality of original functional structures, wherein the orthographic projections of the original functional structures on the wafer substrate are located inside the orthographic projections of the first mask patterns on the wafer substrate;

[0010] The multiple first mask patterns are removed, and the wafer substrate is subjected to shallow silicon etching using the multiple original functional structures as masks to form a nanocolumn array substrate, wherein the nanocolumn array substrate includes multiple target functional structures arranged in an array along the row direction and the column direction, and the nanocolumn array substrate is used for exosome detection based on Raman imaging.

[0011] In an optional embodiment of the present application, the forming of a plurality of first mask patterns arranged in an array along row directions and column directions on a side of the original functional layer away from the wafer substrate comprises:

[0012] forming a first mask layer on a side of the original functional layer facing away from the wafer substrate;

[0013] The first mask layer is exposed and developed based on a first mask plate to form the plurality of first mask patterns arranged in an array along the row direction and the column direction.

[0014] In an optional embodiment of the present application, the isotropic etching process is performed on the original functional layer using the multiple first mask patterns as masks to form multiple original functional structures, including:

[0015] Determining a preset etching time based on an etching rate corresponding to the material of the original functional layer;

[0016] Using the plurality of first mask patterns as masks, immersing the wafer substrate in an etching solution for etching;

[0017] After the isotropic etching process is performed for the preset etching time, a plurality of the original functional structures are formed.

[0018] In an optional embodiment of the present application, the original functional layer includes a first original functional sublayer and a second original functional sublayer, the second original functional sublayer is arranged on a side of the wafer substrate away from the first original functional sublayer, and the original functional layer is isotropically etched using the multiple first mask patterns as masks to form multiple original functional structures, including:

[0019] Using the plurality of first mask patterns as masks, the second original functional sublayer is isotropically etched to form a plurality of second original functional substructures, wherein the orthographic projections of the second original functional substructures on the wafer substrate are located inside the orthographic projections of the first mask patterns on the wafer substrate;

[0020] The multiple first mask patterns are removed, and the first original functional sublayer is anisotropically etched using the multiple second original functional substructures as masks to obtain the multiple original functional structures, wherein the orthographic projection of the second original functional substructure on the wafer substrate coincides with the orthographic projection of the original functional structure on the wafer substrate.

[0021] In an optional embodiment of the present application, the width of the original functional structure along the row direction and / or along the column direction is less than or equal to 1 micron.

[0022] In an optional embodiment of the present application, the material of the original functional layer includes at least one of the following: titanium oxide or chromium-gold alloy.

[0023] In an optional embodiment of the present application, the target functional structure includes nanocolumns and the original functional structure, and the height of the nanocolumns along a first direction is greater than or equal to 1 micron and less than or equal to 2 microns, and the first direction is the direction from the wafer substrate to the original functional layer.

[0024] In a second aspect of an embodiment of the present application, a nanorod array substrate for Raman spectroscopy imaging is provided, wherein the nanorod array substrate is prepared by using any method for preparing a nanorod array substrate for Raman spectroscopy imaging described in the first aspect.

[0025] In a third aspect of an embodiment of the present application, a detection chip is provided, wherein the detection chip comprises a nanocolumn array substrate for Raman spectroscopy imaging as described in the second aspect above.

[0026] The present application includes the following advantages: the present application provides a nanocolumn array substrate for Raman spectroscopy imaging, a preparation method thereof, and a detection chip, by providing a wafer substrate; forming an original functional layer on one side of the wafer substrate, wherein the original functional layer is a single atomic film layer for binding target exosomes; forming a plurality of first mask patterns arranged in an array along row directions and column directions on a side of the original functional layer away from the wafer substrate; isotropically etching the original functional layer using the plurality of first mask patterns as masks to form a plurality of original functional structures, wherein the orthographic projection of the original functional structure on the wafer substrate is located inside the orthographic projection of the first mask pattern on the wafer substrate; removing the plurality of first mask patterns, and performing shallow silicon etching on the wafer substrate using the plurality of original functional structures as masks to form a nanocolumn array substrate, wherein the nanocolumn array substrate includes a plurality of target functional structures arranged in an array along the row directions and the column directions, and the nanocolumn array substrate is used for exosome detection based on Raman imaging. The preparation method of the present application is combined with isotropic etching to form multiple target functional structures arranged in an array on a wafer substrate, which can effectively improve the accuracy of the target functional structures formed by lithography, thereby enabling the preparation of high-precision nanorod array substrates through low-precision lithography technology that requires a mask, effectively improving the preparation efficiency and accuracy of the nanorod array substrate, and further applying it to the detection of exosomes in Raman spectroscopy imaging. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the description of the embodiments of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0028] Figure 1 It is a schematic flow chart of a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0029] Figure 2 It is a top view of a wafer substrate in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0030] Figure 3 It is a schematic cross-sectional view taken along line A-A' of forming an original functional layer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0031] Figure 4 This is one of the AA' cross-sectional schematic diagrams of forming a first mask layer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0032] Figure 5 is a schematic diagram of a first mask proposed in an embodiment of the present application;

[0033] Figure 6 AA' is a schematic cross-sectional view of forming a first mask pattern in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0034] Figure 7 It is a schematic cross-sectional view taken along line A-A' of etching the original functional layer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0035] Figure 8 It is a schematic cross-sectional view taken along line A-A' of forming an original functional structure in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application;

[0036] Fig. 9 It is a schematic cross-sectional view taken along line A-A' of forming a nanocolumn array in a method for preparing a nanocolumn array substrate for Raman spectroscopy imaging provided in an embodiment of the present application;

[0037] Fig.10 It is a schematic cross-sectional view taken along line AA' of forming a first original functional sublayer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application;

[0038] Fig.11 It is a schematic cross-sectional view taken along line AA' of forming a second original functional sublayer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application;

[0039] Fig.12 This is the second AA' cross-sectional schematic diagram of forming a first mask layer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0040] Fig.13 AA' is a schematic cross-sectional view of forming a first mask pattern in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application;

[0041] Fig.14 It is a schematic cross-sectional view taken along line AA' of etching the second original functional sublayer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application;

[0042] Fig.15 It is a schematic cross-sectional view taken along line A-A' of forming a plurality of second original functional substructures in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application;

[0043] Fig.16 It is a schematic cross-sectional view taken along line A-A' of forming an original functional structure in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application;

[0044] Fig.17 AA' cross-sectional schematic diagram of a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application.

[0045] Explanation of the reference numerals: 101: wafer substrate; 201: original functional layer; 202: first original functional sublayer; 203: second original functional sublayer; 205: second original functional substructure; 301: first mask layer; 302: first mask pattern; 402: original functional structure; 501: target functional structure; 503: nanopillar. DETAILED DESCRIPTION

[0046] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0047] Exosomes are small extracellular vesicles with a lipid bilayer membrane structure and a diameter of about 30-180nm. Recent studies have found that exosomes play an important role in physiological and pathological phenomena, such as antigen presentation in immunity, tumor growth and migration, and repair of tissue damage. Surface enhanced Raman scattering (SERS) technology is an emerging biomarker and is often used to detect exosomes.

[0048] Existing SERS-based exosome detection technology uses antibodies modified on micro-pillar arrays to specifically bind to corresponding proteins on vesicles to capture vesicles. It has high requirements on the precision of micro-pillar arrays and is usually prepared by electron beam lithography. However, electron beam lithography is not suitable for large-scale production of micro-pillar arrays for detecting exosomes due to its slow processing efficiency and high processing cost.

[0049] Based on this, the present application embodiment provides a method for preparing a nanorod array substrate for Raman spectroscopy imaging in the first aspect, referring to Figure 1 , Figure 1 1 is a schematic flow chart of a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application, wherein the preparation method comprises the following steps:

[0050] Step 101: providing a wafer substrate;

[0051] Step 102: forming an original functional layer on one side of the wafer substrate, wherein the original functional layer is a single atomic film layer for binding target exosomes;

[0052] Step 103: forming a plurality of first mask patterns arranged in an array along row directions and column directions on a side of the original functional layer away from the wafer substrate;

[0053] Step 104: performing isotropic etching on the original functional layer using the plurality of first mask patterns as masks to form a plurality of original functional structures, wherein the orthographic projections of the original functional structures on the wafer substrate are located inside the orthographic projections of the first mask patterns on the wafer substrate;

[0054] Step 105: remove the multiple first mask patterns, and perform shallow silicon etching on the wafer substrate using the multiple original functional structures as masks to form a nanorod array substrate, wherein the nanorod array substrate includes multiple target functional structures arranged in an array along the row direction and the column direction, and the nanorod array substrate is used for exosome detection based on Raman imaging.

[0055] When implementing step 101, refer to Figure 2 , Figure 2 It is a top view of a wafer substrate in a method for preparing a nanocolumn array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application. The present application adopts a silicon wafer as the substrate material of the nanocolumn array substrate, wherein the thickness of the wafer substrate 101 is greater than the thickness of other hierarchical materials in the preparation process of the nanocolumn array substrate. It should be noted that in the method for preparing a nanocolumn array substrate provided in an embodiment of the present application, the "thickness" of each partial structure involved refers to the dimension of each partial structure in a direction perpendicular to the upper and lower flat surfaces of the wafer substrate 101, that is, the dimension of the wafer substrate 101 in a direction pointing to other hierarchical structures (such as the original functional layer 201, etc.) in the preparation process of the nanocolumn array substrate.

[0056] Specifically, when the nanorod array substrate is used to capture target exosomes, the original functional layer formed on one side of the wafer substrate is used to bind the single atomic film layer of the target exosomes. Figure 3 , Figure 3This is a schematic cross-sectional view of A-A' of forming an original functional layer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application. An original functional layer 201 is formed on one side of the wafer substrate 101. The original functional layer 201 is a single atomic membrane layer, including a target capture material for capturing target exosomes. The nanorod array substrate prepared by the preparation method proposed in the present application can be directly combined with exosomes having a phospholipid bilayer to achieve the capture of target proteins on the exosomes. The target proteins free in the serum can avoid binding to the target capture material because they do not have the phospholipid bilayer structure of the exosome vesicles, effectively improving the effect of exosome detection, and can be used for detecting exosomes in Raman spectroscopy imaging.

[0057] In some optional embodiments, the material of the original functional layer 201 may be an oxidized metal material or an alloy material. Optionally, the material of the original functional layer 201 includes at least one of the following: titanium oxide (TiO2) or chromium-gold alloy (Cr / Au). When the original functional layer is a single atomic film layer that binds to the target exosomes, the substance that can capture the exosomes can indirectly capture the exosomes.

[0058] In some optional embodiments, in order to improve the binding effect of the material of the original functional layer 201 on the target exosomes, the original functional layer 201 is a single atomic film layer. In the embodiment of the present application, the method of forming the original functional layer 201 on one side of the wafer substrate 101 includes but is not limited to an electron beam evaporation process and an atomic layer deposition (ALD) process, etc. Exemplarily, when the material of the original functional layer 201 is a chromium-gold alloy (Cr / Au), an electron beam evaporation process is used to evaporate the target functional materials (Au and Cr) into a gaseous state, and then the gaseous target functional materials are deposited on one side of the wafer substrate 101 in a high vacuum chamber to form a single-atom original functional layer 201; when the material of the original functional layer 201 is titanium oxide (TiO2), an atomic layer deposition (ALD) process is used to uniformly deposit the target functional material on one side of the wafer substrate 101 to form a single-atom original functional layer 201.

[0059] In some optional embodiments, in order to ensure that the original functional layer 201 can be effectively formed on one side of the wafer substrate 101, before depositing the original functional layer 201, one side of the wafer substrate 101 is polished, and then the original functional layer 201 is formed on the side of the polished wafer substrate 101.

[0060] When step 103 is specifically implemented, in order to improve the efficiency of the process flow of preparing the nanorod array substrate for Raman spectroscopy imaging and reduce the preparation cost, UV photolithography is used to form a first mask pattern using photoresist as the first mask. Figure 4 , Figure 4 The A-A' cross-sectional schematic diagram of forming the first mask layer in the preparation method of a nanorod array substrate for Raman spectroscopy imaging proposed in the embodiment of the present application, the first mask layer 301 is formed on the side of the original functional layer 201 away from the wafer substrate 101, and the first mask layer 301 covers the original functional layer 201 on the entire surface. Specifically, the wafer substrate 101 with the original functional layer 201 is placed on the wafer tray of the glue machine, and after vacuum adsorption, photoresist is evenly dripped to cover about three-quarters of the wafer area, and the glue machine is started after the speed is set. For example, the first step speed of the glue machine can be set to 1500 rpm, the acceleration is 500 rpm / s, and the time lasts for 10 s; the second step speed of the glue machine is 4000 rpm, the acceleration is 1500 rpm / s, and the time lasts for 30 s). After the glue program is set to end, it is pre-baked in a drying machine at 97°C for 2 minutes to obtain the first mask layer 301. Optionally, the thickness of the first mask layer 301 is 1.5 microns.

[0061] After forming the first mask layer 301, the first mask layer 301 is patterned based on the first mask plate to form a first mask pattern. Figure 5 , Figure 5 This is a schematic diagram of a first mask plate proposed in an embodiment of the present application. The first mask plate includes a mask pattern of a square array with a size of 2 µm. Based on the first mask plate, the first mask layer 301 is exposed and developed to form a first mask pattern 302 arranged in an array along the row direction and the column direction. Figure 6 , Figure 6The A-A' cross-sectional diagram of forming a first mask pattern in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application is as follows: a wafer substrate 101 formed with a first mask layer 301 is placed on a wafer tray of a photolithography machine and vacuumed; at the same time, the first mask is placed on a mask chuck, and ultraviolet exposure is performed after setting photolithography parameters. For example, the photolithography parameters may be: hard contact, exposure parameter 18.58 mJ / cm 2 , exposure time 5.4 s; then prepare a developer, immerse the wafer substrate after exposure treatment in 100 ml of the developer and shake it evenly for 30 s of development treatment, then immediately rinse the residual developer with deionized water, and blow dry with a nitrogen gun to obtain the first mask pattern 302. Optionally, the ratio of the developer is: the ratio of developer AZ400K to deionized water is 1:4.

[0062] When the step 104 is specifically implemented, in order to obtain a plurality of original functional structures that are aligned and uniform in size after one etching, the original functional layer 201 is isotropically etched using a plurality of the first mask patterns 302 as masks to form a plurality of original functional structures 402, so that the orthographic projection of the original functional structure 402 on the wafer substrate 101 is located inside the orthographic projection of the first mask pattern 302 on the wafer substrate 101. Among them, isotropic etching refers to etching that is equal in all directions, which means that the direction of the substrate does not affect the way the etchant removes the material. When an etchant (a corrosive chemical) is applied to a masked wafer, etching occurs at the same rate in areas not covered by the mask in all directions, thereby producing rounded edges. In the present application, the method of isotropic etching can be wet etching or other equivalent methods that achieve an isotropic etching effect.

[0063] Specifically, see Figure 7 , Figure 7It is a schematic cross-sectional view of etching the original functional layer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application. After forming a plurality of first mask patterns 302, a preset etching time is determined based on the etching rate corresponding to the material of the original functional layer 201, and the wafer substrate 101 on which the plurality of first mask patterns 302 are formed is placed in an etching solution using the plurality of first mask patterns 302 as a mask, and then the original functional layer 201 is corroded based on the preset etching time to form a plurality of original functional structures 402, and the size of each original functional structure 402 is smaller than the size of each corresponding first mask pattern 302. Exemplarily, the etching solution is an iodine potassium iodide etching solution, wherein the iodine potassium iodide etching solution is a mixed solution of iodine, potassium iodide and water, and the mixing ratio of the etching solution used in the present application is iodine: potassium iodide: water = 1:4:20. After the etching is completed, rinse with deionized water and blow dry the surface with nitrogen.

[0064] In an optional embodiment of the present application, the etching time is selected so that the original functional layer 201 can be etched into a pattern with a width less than or equal to 1 micron along the row direction and / or along the column direction after the etching time.

[0065] When implementing step 105, refer to Figure 8 , Figure 8 This is a schematic diagram of the A-A' cross section of the original functional structure formed in the method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application. After obtaining a plurality of original functional structures 402, the plurality of first mask patterns 302 are removed to obtain a plurality of original functional structures 402 arranged in an array along the row direction and the column direction. Optionally, the first mask pattern 302 can be removed by etching. Since the isotropic etching process can make the size of the original functional structure smaller, the wafer substrate can be etched using the original functional structure as a mask to obtain a nanorod array with higher precision. Specifically, refer to Fig. 9 , Fig. 9 A schematic diagram of the A-A' cross-section of a nanocolumn array formed in a method for preparing a nanocolumn array substrate for Raman spectroscopy imaging provided in an embodiment of the present application, wherein the wafer substrate 101 is subjected to shallow silicon etching using a plurality of the original functional structures 402 as a mask to form a nanocolumn array substrate, wherein the nanocolumn array substrate includes a plurality of target functional structures 501 arranged in an array along the row direction and the column direction. The target functional structure 501 includes a nanocolumn and the original functional structure, wherein the height of the nanocolumn along a first direction is greater than or equal to 1 micron and less than or equal to 2 microns, and the first direction is the direction from the wafer substrate 101 to the original functional layer 201.

[0066] Exemplarily, the method for removing the multiple first mask patterns is as follows: placing the wafer substrate with multiple original functional structures in an acetone solution, ultrasonically cleaning for 5 minutes, cleaning the silicon wafer with ethanol and deionized water in turn, then drying with nitrogen, and placing the wafer substrate in a plasma stripper for 5 minutes to remove the first mask pattern. The method for shallow silicon etching is as follows: placing the wafer substrate with the first mask pattern removed in a transfer chamber of a silicon etching (ICP-Si) instrument, evacuating and selecting a silicon etching program, selecting an etching time according to the etching rate of the wafer substrate, and running the program to obtain a nanopillar array composed of a target functional structure with a height of about 1 µm.

[0067] In some optional implementations, the orthographic projection shape of the target functional structure 501 on the wafer substrate 101 may be a circle, a regular polygon or other irregular shapes. Preferably, the orthographic projection shape of the target functional structure 501 on the wafer substrate 101 is a square.

[0068] In an optional embodiment of the present application, when the original functional layer 201 includes a first original functional sublayer 202 and a second original functional sublayer 203, the second original functional sublayer 203 is disposed on a side of the wafer substrate 101 away from the first original functional sublayer 202. Fig.10 , Fig.10 1 is a schematic cross-sectional view of forming a first original functional sublayer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application, wherein a first original functional sublayer 202 is formed on one side of the wafer substrate 101, and the first original functional sublayer 202 is a single atomic film layer, including a target capture material for capturing target exosomes; and then referring to Fig.11 , Fig.11 It is a schematic diagram of the A-A' cross section of forming a second original functional sublayer in a method for preparing a nanorod array substrate for Raman spectroscopy imaging provided in an embodiment of the present application, wherein the second original functional sublayer 203 is formed on the side of the first original functional sublayer 202 away from the wafer substrate 101.

[0069] After forming the first original functional sublayer, refer to Fig.12 , Fig.12This is the second A-A' cross-sectional schematic diagram of forming the first mask layer in the method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application, wherein the first mask layer 301 is formed on the side of the second original functional sublayer 203 away from the wafer substrate 101, and the first mask layer 301 covers the entire surface of the second original functional sublayer 203. Specifically, the wafer substrate 101 formed with the second original functional sublayer 203 is placed on the wafer tray of the coating machine, and after vacuum adsorption is firm, photoresist is evenly dripped to cover approximately three-quarters of the wafer area, and the coating machine is started after the speed is set.

[0070] After forming the first mask layer 301, the first mask layer 301 is patterned based on the first mask plate to form a first mask pattern. Figure 5 , Figure 5 This is a schematic diagram of a first mask provided in an embodiment of the present application, wherein the first mask includes a mask pattern of a square array with a size of 2 µm. Fig.13 , Fig.13 It is a schematic diagram of the A-A' cross-section of forming a first mask pattern in a method for preparing a nanorod array substrate for Raman spectroscopy imaging proposed in an embodiment of the present application. Based on the first mask plate, the first mask layer 301 is exposed and developed to form a first mask pattern 302 arranged in an array along the row and column directions.

[0071] In an optional embodiment of the present application, the method of performing isotropic etching on the original functional layer 201 using the plurality of first mask patterns 302 as masks to form a plurality of original functional structures is specifically as follows: Fig.14 , Fig.14 The A-A' cross-sectional schematic diagram of etching the second original functional sublayer in a method for preparing a nanorod array substrate provided in an embodiment of the present application, wherein the second original functional sublayer 203 is isotropically etched using the first mask pattern 302 as a mask to form a plurality of second original functional substructures 205, wherein the orthographic projection of the second original functional substructure 205 on the wafer substrate 101 is located inside the orthographic projection of the first mask pattern 302 on the wafer substrate 101, that is, after the isotropic etching treatment, the size of each second original functional substructure obtained is smaller than the size of the first mask pattern.

[0072] See also Fig.15 , Fig.15This is a schematic cross-sectional view of A-A' of forming a plurality of second original functional substructures in a method for preparing a nanopillar array substrate for Raman spectroscopy imaging provided in an embodiment of the present application. After the second original functional sublayer is isotropically etched to obtain a plurality of second original functional substructures 205, the plurality of first mask patterns 302 are removed to obtain a plurality of second original functional substructures 205 arrayed along the row direction and the column direction. Optionally, the first mask pattern 302 can be removed by etching. Since the isotropic etching process can make the size of the original functional structure smaller, etching the wafer substrate using the original functional structure as a mask can obtain a nanopillar array with higher precision.

[0073] See also Fig.16 , Fig.16 A schematic diagram of the A-A' cross section of the original functional structure formed in the method for preparing a nanocolumn array substrate for Raman spectroscopy imaging provided in an embodiment of the present application, wherein the first original functional sublayer 202 is anisotropically etched using the multiple second original functional substructures 205 as a mask to form multiple original functional structures 402, and the orthographic projections of the multiple second original functional substructures 205 on the wafer substrate 101 coincide with the orthographic projections of the original functional structures 402 on the wafer substrate 101. Exemplarily, the wafer substrate formed with the second original functional substructure is placed in the transfer chamber of a III-V etcher, the anisotropic etching procedure for the first original functional sublayer is selected, and the first original functional sublayer exposed under the second original functional substructure is etched away using the second original functional substructure as a mask.

[0074] The above-mentioned isotropic etching process is the same as the operation in the specific implementation step 104. The above-mentioned anisotropic etching refers to etching that occurs at different rates in different directions, depending on the orientation of the substrate crystal plane. Due to the single crystal structure of silicon, certain etchants can selectively etch silicon along certain planes or angles depending on the orientation of the silicon. By changing the time, etching chemicals and the orientation of the silicon crystal, many different shapes and channels can be etched in the silicon wafer.

[0075] For example, the material of the first original functional sublayer 202 may be titanium oxide, and the material of the second original functional sublayer 203 may be chromium-gold alloy. When the first original functional sublayer is used as a single atomic membrane layer for binding target exosomes, the exosomes can be directly captured. In this case, the second original functional sublayer only serves as a mask layer and does not have the function of binding target exosomes.

[0076] In the method of preparing a nanocolumn array substrate, two anisotropic etching processes are often used for processing, but this method will cause deviations in the shape and size of the target functional structure finally formed, resulting in low precision of small-size images produced in batches. In the present application, by combining isotropic etching and anisotropic etching, the original functional layer is firstly subjected to isotropic etching. Since the isotropic etching process can achieve equal etching in all directions of the original functional layer, the original functional substructure obtained is small in size and high in precision. Then, the wafer substrate is subjected to shallow silicon etching based on the original functional substructure as a mask to form a nanocolumn array substrate. Since the size of the original functional substructure after isotropic etching is uniform and equal, on this basis, the nanocolumn array substrate prepared with the original functional substructure as a mask ensures the precision of the original functional substructure while effectively improving the preparation efficiency of the nanocolumn array substrate and reducing the preparation cost.

[0077] An embodiment of the present application provides a method for preparing a nanocolumn array substrate for Raman spectroscopy imaging, comprising providing a wafer substrate; forming an original functional layer on one side of the wafer substrate, wherein the original functional layer is a single atomic film layer for binding target exosomes; forming a plurality of first mask patterns arranged in an array along row directions and column directions on a side of the original functional layer away from the wafer substrate; isotropically etching the original functional layer using the plurality of first mask patterns as masks to form a plurality of original functional structures, wherein the orthographic projections of the original functional structures on the wafer substrate are located inside the orthographic projections of the first mask patterns on the wafer substrate; removing the plurality of first mask patterns, and performing shallow silicon etching on the wafer substrate using the plurality of original functional structures as masks to form a nanocolumn array substrate, wherein the nanocolumn array substrate includes a plurality of target functional structures arranged in an array along the row directions and the column directions, and the nanocolumn array substrate is used for exosome detection based on Raman imaging. The preparation method of the present application is combined with isotropic etching to form multiple target functional structures arranged in an array on a wafer substrate, which can effectively improve the accuracy of the target functional structures formed by lithography, thereby enabling the preparation of high-precision nanorod array substrates through low-precision lithography technology that requires a mask, effectively improving the preparation efficiency and accuracy of the nanorod array substrate, and further applying it to the detection of exosomes in Raman spectroscopy imaging.

[0078] Based on the same application concept, an embodiment of the present application discloses a nanorod array substrate for Raman spectroscopy imaging, wherein the nanorod array substrate is prepared by using the preparation method of the nanorod array substrate described in the embodiment of the present application.

[0079] In some optional embodiments, see Fig.17 , Fig.171 is a schematic cross-sectional view taken along the line A-A' of a nanocolumn array substrate for Raman spectroscopy imaging provided in an embodiment of the present application, wherein the nanocolumn array substrate comprises: a wafer substrate 101, a plurality of nanocolumns 503 arranged in an array along the row direction and the column direction are convexly provided on one side of the wafer substrate 101, an original functional structure 402 is provided on the top surface of the nanocolumns 503, the original functional structure 402 comprises a single atomic film layer for binding target exosomes, the original functional structure 402 and the nanocolumns 503 constitute the target functional structure 501, and the material of the original functional structure is titanium oxide.

[0080] Based on the same application concept, an embodiment of the present application discloses a detection chip, which includes the nanorod array substrate for Raman spectroscopy imaging described in the embodiment of the present application, and the detection chip is used to detect whether target exosomes exist in the substance to be tested, and the number of target exosomes in the substance to be tested.

[0081] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0082] In the description of this specification, it should be understood that the terms "center", "thickness", "up", "down", "front", "back", "horizontal", "top", "bottom", "inside", "outside", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0083] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0084] In the present application, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0085] The above application provides many different embodiments or examples to realize the different structures of the present application. In order to simplify the present application, the parts and settings of specific examples are described above. Of course, they are only examples, and the purpose is not to limit the present application. In addition, the present application can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplification and clarity, which itself does not indicate the relationship between the various embodiments and / or settings discussed.

[0086] The term "one embodiment", "embodiment" or "one or more embodiments" herein means that a particular feature, structure or characteristic described in conjunction with the embodiment is included in at least one embodiment of the present application. In addition, please note that the examples of the term "in one embodiment" here do not necessarily all refer to the same embodiment.

[0087] In the description provided herein, a large number of specific details are described. However, it is understood that the embodiments of the present application can be practiced without these specific details. In some instances, well-known methods, structures and techniques are not shown in detail so as not to obscure the understanding of this description.

[0088] Finally, it should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or terminal device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or terminal device. In the absence of further restrictions, the elements defined by the sentence "including one..." do not exclude the existence of other identical elements in the process, method, article or terminal device including the elements.

[0089] The above is a detailed introduction to a nanorod array substrate for Raman spectroscopy imaging, a preparation method thereof, and a detection chip provided by the present application. Specific examples are used in this article to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea. At the same time, for a person skilled in the art, according to the idea of ​​the present application, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A method for preparing a nanorod array substrate for Raman spectroscopy imaging, characterized in that: The method comprises: Providing a wafer substrate; Forming an original functional layer on one side of the wafer substrate, the original functional layer comprising a first original functional sublayer and a second original functional sublayer, the second original functional sublayer being arranged on a side of the wafer substrate away from the first original functional sublayer, the first original functional sublayer being a single atomic film layer for directly binding to target exosomes, the material of the first original functional sublayer being titanium oxide, and the material of the second original functional sublayer being a chromium-gold alloy; Forming a plurality of first mask patterns arranged in an array along row directions and column directions on a side of the original functional layer away from the wafer substrate; Using the plurality of first mask patterns as masks, the second original functional sublayer is isotropically etched to form a plurality of second original functional substructures, wherein the orthographic projections of the second original functional substructures on the wafer substrate are located inside the orthographic projections of the first mask patterns on the wafer substrate; Removing the plurality of first mask patterns, and performing anisotropic etching on the first original functional sublayer using the plurality of second original functional substructures as masks to obtain a plurality of original functional structures, wherein the orthographic projection of the second original functional substructure on the wafer substrate coincides with the orthographic projection of the original functional structure on the wafer substrate; The multiple second original functional substructures are removed, and the wafer substrate is subjected to shallow silicon etching using the multiple original functional structures as masks to form a nanocolumn array substrate, wherein the nanocolumn array substrate includes multiple target functional structures arranged in an array along the row direction and the column direction, and the nanocolumn array substrate is used for exosome detection based on Raman imaging.

2. The method for preparing a nanorod array substrate for Raman spectroscopy imaging according to claim 1, characterized in that: The method of forming a plurality of first mask patterns arranged in an array along row directions and column directions on a side of the original functional layer away from the wafer substrate comprises: forming a first mask layer on a side of the original functional layer facing away from the wafer substrate; The first mask layer is exposed and developed based on a first mask plate to form the plurality of first mask patterns arranged in an array along the row direction and the column direction.

3. The method for preparing a nanorod array substrate for Raman spectroscopy imaging according to claim 1, characterized in that: The isotropically etching the second original functional sublayer using the plurality of first mask patterns as masks comprises: Determining a preset etching time based on an etching rate corresponding to the material of the original functional layer; Using the plurality of first mask patterns as masks, immersing the wafer substrate in an etching solution for etching; The second original functional sublayer is subjected to the isotropic etching process for the preset etching time.

4. The method for preparing a nanorod array substrate for Raman spectroscopy imaging according to any one of claims 1 to 3, characterized in that: The width of the original functional structure along the row direction and / or along the column direction is less than or equal to 1 micrometer.

5. The method for preparing a nanorod array substrate for Raman spectroscopy imaging according to claim 1, characterized in that: The target functional structure includes a nanocolumn and the original functional structure. The height of the nanocolumn along a first direction is greater than or equal to 1 micron and less than or equal to 2 microns. The first direction is the direction from the wafer substrate to the original functional layer.

6. A nanorod array substrate for Raman spectroscopy imaging, characterized in that: The nanocolumn array substrate is prepared by using the method for preparing a nanocolumn array substrate for Raman spectroscopy imaging according to any one of claims 1 to 5.

7. A detection chip, characterized in that: The detection chip comprises the nanorod array substrate for Raman spectroscopy imaging as claimed in claim 6.

Citation Information

Patent Citations

  • Preparation method of large-area sequential controllable surface-enhanced Raman active substrate

    CN102621128A

  • Enhanced Raman spectroscopy test piece device and test piece manufacturing method

    CN102954956A

  • Large-area uniform three-dimensional composite nanometer structure and preparation method thereof

    CN108622848A

  • LSPR reflective biosensor chip and preparation method, recycling method and application thereof

    CN111829990A

  • Composite surface-enhanced Raman substrate and preparation method thereof

    CN117949430A