A prediction method for electrochemical and mechanical properties of SOFC during hot and cold cycles

By analyzing the electrochemical impedance spectrum and mechanical properties of the SOFC stack, the electrochemical and mechanical property attenuation rules during the hot and cold cycle are revealed, a theoretical model is established, and the life is predicted, which solves the problem of unstable performance of the SOFC stack during hot and cold cycles. solve the problem and improve the stability and service life of the stack.

CN118483600BActive Publication Date: 2024-10-15CHINA UNIV OF PETROLEUM (EAST CHINA)
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202410933097.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-12
Publication Date
2024-10-15
Estimated Expiration
2044-07-12

AI Technical Summary

Technical Problem

The electrochemical and mechanical properties of solid oxide fuel cells (SOFC) are unstable during hot and cold cycles, leading to degradation of the stack and affecting its service life and power generation performance.

Method used

A method that includes preparing SOFC stacks, conducting hot and cold cycle tests, analyzing electrochemical impedance spectra, testing mechanical properties, revealing the attenuation coupling relationship between electrochemical and mechanical properties, and establishing a theoretical model is used to predict the attenuation rules of electrochemical and mechanical properties. and hot and cold cycle service life.

Benefits of technology

Effectively guide the operation and maintenance of SOFC stacks, reduce economic losses, promote the commercial application of SOFC, and improve the thermal cycle stability and thermal shock resistance of the stack.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118483600B_ABST
    Figure CN118483600B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for predicting electrochemical and mechanical properties in SOFC hot and cold cycles, and belongs to the technical field of solid oxide fuel cells. The present invention quantitatively analyzes the contribution of different electrode reaction processes to voltage decay by carrying out hot and cold cycle tests on SOFC stacks, measuring polarization curves and electrochemical impedance spectra using an electrochemical workstation, and testing the mechanical properties (bending strength, elastic modulus and hardness) after different hot and cold cycle services, and quantitatively correlating the electrochemical and mechanical properties of SOFC stacks using changes in Ni particles, revealing the coupling relationship between the attenuation of electrochemical and mechanical properties of SOFC stacks, and establishing a theoretical model for the attenuation of electrochemical and mechanical properties of SOFC stacks, which can accurately predict the changing laws of electrochemical and mechanical properties of SOFC stacks after different hot and cold cycle times, as well as the hot and cold cycle service life of SOFC stacks, which is of great significance to improving the thermal shock resistance of SOFC stacks in hot and cold cycles, and promoting the commercial application of SOFC.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of solid oxide fuel cells, and in particular relates to a method for predicting electrochemical and mechanical properties in a SOFC hot and cold cycle. Background Art

[0002] Solid Oxide Fuel Cell (SOFC) is an electrochemical device that can directly convert chemical energy in fuel into electrical energy under medium and high temperature conditions. Its advantages such as high efficiency, zero pollution and low noise make it have broad application prospects in fields such as distributed power generation and large-scale fixed power stations. In order to meet the long life requirements of commercial applications, SOFC needs to be able to operate continuously under harsh operating conditions and withstand temperature cycling changes during multiple start-stop processes. During the hot and cold cycle service of SOFC stacks, the electrode materials are subjected to harsh working conditions, resulting in the formation of temperature gradients inside the stack and uneven temperature distribution. Due to the mismatch of thermal expansion coefficients between the constituent materials of a single cell, excessive thermal stress will be generated inside the single cell. The high hardness and brittleness of ceramic materials and the various defects inside make the single cell prone to deformation, delamination and cracking in this environment, which significantly reduces the mechanical properties of SOFC components and affects the power generation performance and operating life of SOFC. In addition, during the hot and cold cycles, the nickel particles in the anode will undergo degradation phenomena such as coarsening, migration and depletion, which will not only reduce the conductivity and output voltage of the SOFC, but also cause micro cracks and defects inside the anode material, thereby reducing its bending strength and stability.

[0003] The mechanical strength and electrochemical stability of a single cell are crucial to ensure the high reliability of a SOFC stack. However, there is a lack of research on the correlation between the mechanical and electrochemical properties of a SOFC stack. This is because such research requires time and resources to conduct long-term performance investigations, and it is not easy to accurately distinguish the mechanisms that affect the degradation of a SOFC stack, because its performance degradation involves the weakening of the interaction between the components of the stack and the degradation of the components themselves. Therefore, in order to extend the service life of SOFC and expand its application areas, it is necessary to systematically study the degradation laws and coupling relationships between the electrochemical and mechanical properties of a SOFC stack during the hot and cold cycles, and reveal the potential degradation mechanisms. This is of great significance for improving the hot and cold cycle stability of SOFC. Summary of the invention

[0004] Solid oxide fuel cells (SOFCs) are highly efficient energy conversion devices that directly convert chemical energy in fuels into electrical energy. A key challenge to their commercialization is the thermal cycling instability of electrochemical and mechanical properties. Therefore, in order to extend the service life of SOFCs and expand their application areas, it is necessary to systematically study the attenuation laws of SOFC electrochemical and mechanical properties during thermal cycling and reveal the potential degradation mechanism, which is of great significance for improving the thermal cycling stability of SOFC stacks.

[0005] The purpose of the present invention is to overcome the above-mentioned deficiencies of the prior art and to provide a method for predicting the electrochemical and mechanical properties of SOFC in hot and cold cycles.

[0006] In order to achieve the above-mentioned purpose, the present invention adopts the following technical scheme: a method for predicting electrochemical and mechanical properties in SOFC hot and cold cycles, comprising the following steps: step S1: preparing the constituent materials of the SOFC stack, completing the assembly of the SOFC stack power generation and test system and the test preparation work, and determining the operating parameters of the SOFC stack hot and cold cycle test according to the actual service conditions; step S2: carrying out the hot and cold cycle test using the SOFC stack power generation and test system, and collecting the polarization curve and electrochemical impedance spectrum of the SOFC stack during each hot and cold cycle operation using an electronic load controller and an electrochemical workstation; step S3: analyzing and fitting the electrochemical impedance spectrum data of the SOFC stack using the relaxation time distribution method and the equivalent circuit model, and calculating Calculate the voltage loss caused by each electrode reaction process of SOFC during the hot and cold cycle and its contribution to the voltage attenuation; Step S4: Test the mechanical properties of the SOFC stack cells after different hot and cold cycle services; Step S5: Use a scanning electron microscope and an X-ray spectrometer to analyze the microstructural changes of the components of the SOFC stack before and after the hot and cold cycle test, and calculate the contents of various elements in the SOFC stack and the average diameter of the particles; Step S6: Reveal the coupling relationship between the electrochemical performance and mechanical performance attenuation of the SOFC stack, and establish a theoretical model for the electrochemical performance and mechanical performance attenuation of the SOFC stack; Step S7: Predict the electrochemical and mechanical properties of the SOFC stack after different hot and cold cycle times, as well as the hot and cold cycle service life of the SOFC stack.

[0007] Preferably, in step S1, the SOFC stack power generation and testing system includes a SOFC stack, an electronic load controller, an electrochemical workstation, a gas controller, a temperature controller and a data control terminal; a single cell in the SOFC stack includes a cathode, a barrier layer, an electrolyte, an anode functional layer and an anode support layer, which are assembled into a stack unit through a bipolar plate, a packaging material and a single cell; a plurality of stack units are assembled and combined and fastened together through sealing materials, a top plate, a base and bolts to form a high-power SOFC stack; the electronic load controller is used to adjust the load, change the current of the SOFC stack, and record the voltage response under different currents; the electrochemical workstation can generate the AC signal required for the electrochemical impedance spectroscopy test and measure the impedance change of the SOFC stack at different frequencies; the gas controller is used to control the fuel gas and The supply of oxidant maintains the gas flow and pressure required by the stack during the test; the temperature controller is used to heat or cool the SOFC stack and monitor the operating temperature of the SOFC stack; the electrodes of the SOFC stack are connected to the electronic load controller and the electrochemical workstation through cables, and the data interfaces of the electronic load controller and the electrochemical workstation are connected to the data control terminal through cables for data synchronization and remote control; when performing voltage testing, the electronic load controller will adjust the current, and the data control terminal will record the voltage response of the SOFC stack; when performing electrochemical impedance spectroscopy testing, the signal generator of the electrochemical workstation will apply a small-amplitude AC signal to the stack, and at the same time measure the impedance response signal of the SOFC stack, and then obtain the electrochemical impedance spectrum through the electrochemical analysis software in the data control terminal; The operating parameters of the SOFC stack hot and cold cycle test include temperature range, heating and cooling rates, gas type, gas flow rate, cycle frequency, number of cycles and current density; the operating temperature range is 650℃~800℃, and the reduction temperature range is 700℃~900℃; the heating rate is 0.5~2℃ / min, and the cooling rate is 0.5~1℃ / min; pure hydrogen and dry air are used as fuel and oxidant, respectively, and nitrogen is used as protective gas; during the heating process, dry nitrogen is supplied to the anode at a flow rate of 0.3~0.9 L / min, hydrogen is supplied to the anode at a flow rate of 0.3~0.9 L / min, and dry air is supplied to the cathode at a flow rate of 0.9~2.7 L / min.

[0008] Preferably, in step S2, the SOFC stack power generation and test system is used to set the temperature range of the hot and cold cycle and the heating and cooling rate of the SOFC stack, the gas supply program of the cathode and anode sides of the SOFC stack is set, and the SOFC stack is heated from room temperature to the reduction temperature for reduction. After the reduction is completed, the stack is cooled to the working temperature, and the SOFC stack is started to start the hot and cold cycle test; the polarization curve of the SOFC stack during each hot and cold cycle is collected by the electronic load controller, and the attenuation rate of the SOFC stack under the current density A1 is calculated, and the reference range of the current density A1 is 0 ~ 500 mA / cm 2 ; An electronic load controller and an electrochemical workstation are used to collect electrochemical impedance spectroscopy data under 3 to 5 DC biases during each hot and cold cycle of the SOFC stack; DC bias refers to the use of an electronic load controller to keep the SOFC stack at a constant DC current output, which is mainly used to simulate the load operation state of the SOFC in the actual power generation process.

[0009] Preferably, in step S3, the electrochemical impedance spectroscopy data in the cold and hot cycle process is processed using the relaxation time distribution method, the peaks on the relaxation time distribution diagram are distinguished according to the characteristics of different electrochemical reaction processes of the SOFC stack, and the change laws of different electrode reaction processes are qualitatively distinguished; the electrode reaction process is determined based on the distribution law obtained by the relaxation time distribution method, and a reasonable initial value is provided for the equivalent circuit model element; the ohmic impedance R is used to calculate the initial value of the equivalent circuit model element; ohm The equivalent circuit model composed of the inductor L and RQ units is used to fit the electrochemical impedance spectroscopy data, quantitatively determine the contribution of different electrode reaction processes to the voltage decay in the hot and cold cycles, and determine the contribution value of each electrode reaction process to the voltage decay and its ranking; in the relaxation time distribution method, the total impedance of the SOFC stack Expressed as ohmic impedance R ohm , polarization impedance R pol The sum of relaxation time Refers to the time required for an electrochemical process to reach equilibrium, where polarization impedance is expressed as relaxation time The integral from 0 to ∞ seconds is as follows: (1); where j and ω are imaginary units and angular frequencies, respectively; solve for different relaxation times Corresponding , that is, the relaxation time distribution diagram corresponding to the EIS data can be obtained, The expression is: γ ( τ ) = R 2 π ⋅ sin[( 1 − n ) π ] cosh[ n ln( τ / τ 0 )] − cos[( 1 − n ) π ] (2); R is the resistance, cosh is the hyperbolic cosine function, n is the number of electron transfers, Represents the relaxation time at the initial moment; the expression of the characteristic frequency f is: (3); In the equivalent circuit model, the equivalent circuit model consists of a series ohmic impedance R ohm , inductor L and RQ unit, the RQ unit is composed of a resistor R and a constant phase element CPE in parallel, and each RQ unit represents an electrode process on a specific time scale;

[0010] The calculation formula of the total impedance of the equivalent circuit model is: (4); where L self is the self-inductance of the equivalent circuit, L wire is the imaginary mutual inductance, L wire Used to reduce the interference of inductance and mutual inductance on the analysis results.

[0011] Preferably, in step S4, after the hot and cold cycles, the SOFC stack is dismantled to analyze the mechanical properties of each component of the single cell; the mechanical properties of the single cell include bending strength, elastic modulus and hardness, the bending strength is tested using a small punch testing machine, and the elastic modulus and hardness are tested using a high-precision nanoindentation instrument; before the small punch test, the single cell is processed into a disc-shaped specimen with a diameter of 10 mm by laser cutting, and each type of single cell specimen completes more than 20 small punch tests, and the Weibull statistical method is used to analyze the dispersion of the bending strength of the single cell; before the nanoindentation test, the cross section of the single cell is polished to obtain a flat surface.

[0012] Preferably, in step S5, a scanning electron microscope (SEM) and an X-ray energy dispersive spectrometer (EDS) are used to study the microstructure and element distribution of each component of the single battery after different hot and cold cycles, and the size of the element particles in each electrode is calculated from the SEM and EDS images using the image processing software ImageJ; the average equivalent circular diameter φ of the Ni element particles in the single battery sample before and after the hot and cold cycles is calculated using the area weighted algorithm. ECD .

[0013] Preferably, in step S6, according to the output voltage of SOFC, the bending strength of the single cell, and the average equivalent circular diameter φ of the Ni element particles ECD , elastic modulus and hardness with the number of hot and cold cycles, and establish a theoretical model for the coupling of electrochemical and mechanical performance attenuation of SOFC stacks: (5); where y is the output voltage of SOFC, the bending strength of the single cell, and the average equivalent circular diameter of Ni element particles φ ECD , elastic modulus and hardness; x is the number of hot and cold cycles, x ≥ 1 and is a positive integer; C is the SOFC output voltage corresponding to y, the bending strength of the single cell, and the average equivalent circular diameter φ of the Ni element particles ECD, the initial value of any one of the properties including elastic modulus and hardness, and the specific value of C is obtained by testing after the first hot and cold cycle; n is the attenuation coefficient.

[0014] Preferably, in step S7, the failure thresholds of the electrochemical and mechanical properties of the SOFC stack are defined as 20% to 80%, and the hot and cold cycle service life of the SOFC stack is predicted based on the theoretical model in step S6.

[0015] Beneficial technical effects brought by the present invention: The present invention provides a method for predicting the electrochemical and mechanical properties of SOFC in hot and cold cycles, which can effectively guide the operation and maintenance of SOFC stacks in hot and cold cycle service, reduce economic losses, accelerate the research and development cycle, and develop low-cost and highly resistant to hot and cold cycle service SOFC stacks, and promote the commercial application of SOFC. The main advantages of the present invention are: 1. The degradation of the electrochemical performance of the SOFC stack under hot and cold cycle service conditions is due to the decline in the interaction between the components of the stack and the degradation of the components of the stack itself. It is not easy to distinguish the accurate electrochemical performance degradation mechanism that affects the SOFC stack. Based on the measurement and analysis of polarization curves and electrochemical impedance spectra, the present invention uses the relaxation time distribution method and the equivalent circuit model to quantitatively analyze the contribution of different electrode reaction processes to voltage attenuation during the hot and cold cycle service of the SOFC stack.

[0016] 2. The key challenge facing the commercialization of SOFC is the instability of electrochemical and mechanical properties during hot and cold cycles. The present invention quantitatively correlates the electrochemical and mechanical properties (bending strength, elastic modulus and hardness) of the SOFC stack using the changes in Ni particles during hot and cold cycles, reveals the coupling relationship between the attenuation of electrochemical and mechanical properties of the SOFC stack, and establishes a theoretical model of the attenuation of SOFC output voltage and mechanical properties during hot and cold cycle service, which is of great significance for improving the thermal shock resistance of SOFC stacks during hot and cold cycles. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 is a flow chart of the method of the present invention; Figure 2 This is a schematic diagram of the components and connection methods of the SOFC stack power generation and testing system; Figure 3 It is a schematic diagram of the structure of the SOFC stack; Figure 4 It is a schematic diagram of the structure of a single cell cross section in a SOFC stack; Figure 5 Schematic diagram of the IVP curve during the SOFC stack hot and cold cycle test; Figure 6 It is the Nyquist diagram of the SOFC stack under 0A DC bias during the hot and cold cycle; Figure 7 This is the DRT distribution diagram under 0A DC bias during the hot and cold cycle of the SOFC stack; Figure 8Schematic diagram of the ECM fitting results of ohmic impedance in the 1st to 10th hot and cold cycles; Fig. 9 Schematic diagram of the percentage contribution of each electrode reaction process to voltage decay in the 1st to 10th hot and cold cycles; Fig.10 Schematic diagram of the elastic modulus of each component of a single cell after different number of cycles; Fig.11 Schematic diagram of the hardness of each component of a single battery after different cycles; ① is the cathode; ② is the barrier layer; ③ is the electrolyte layer; ④ is the anode functional layer; ⑤ is the anode support layer; Fig.12 Schematic diagram of the change curves of SOFC voltage, flexural strength and the proportion of SPSPs in Ni particles with thermal cycles; Fig.13 Schematic diagram of the change curve of SOFC elastic modulus with hot and cold cycles; Fig.14 Schematic diagram of the change curve of SOFC hardness with hot and cold cycles; Fig.15 It is a schematic diagram for comparing the experimental value and the model value of the output voltage; Fig.16 Schematic diagram for comparison between experimental and model values ​​of flexural strength. DETAILED DESCRIPTION

[0018] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments: Solid oxide fuel cells (SOFCs) are a highly efficient energy conversion device that directly converts chemical energy in fuel into electrical energy. A key challenge faced in achieving commercialization is the instability of electrochemical and mechanical properties in thermal cycles. Therefore, in order to extend the service life of SOFCs and expand the application areas of SOFCs, it is necessary to systematically study the attenuation law of SOFC electrochemical and mechanical properties during thermal cycles and reveal the potential degradation mechanism, which is of great significance to improving the thermal cycle stability of SOFC stacks.

[0019] The present invention establishes a prediction method for electrochemical and mechanical properties in SOFC hot and cold cycles, and uses polarization curves, electrochemical impedance spectroscopy (EIS) and distribution of relaxation time (DRT) technology to analyze the electrochemical attenuation mechanism of SOFC stacks. The small punch test (SPT) and nanoindentation test are used to analyze the change law of the mechanical properties (bending strength, elastic modulus and hardness) of the single cell with hot and cold cycles. In the hot and cold cycles, the anode Ni particles undergo substantial degradation phenomena such as coarsening, migration and depletion, which not only reduce the conductivity and output voltage of SOFC, but also cause micro cracks and defects in the anode material, reducing the bending strength and stability of the anode. Therefore, the present invention quantitatively correlates the electrochemical and mechanical properties of the SOFC stack using the change of Ni particles.

[0020] A method for predicting electrochemical and mechanical properties of SOFC during hot and cold cycles, the process is as follows: Figure 1As shown, the following steps are included: S1: preparing the constituent materials of the SOFC stack, completing the assembly of the SOFC stack power generation and test system and the test preparation work, and determining the operating parameters of the SOFC stack hot and cold cycle test according to the actual service conditions.

[0021] like Figure 2 As shown, the SOFC stack power generation and test system consists of a SOFC stack, an electronic load controller, an electrochemical workstation, a gas controller, a temperature controller and a data control terminal. The single cell in the SOFC stack consists of a cathode, a barrier layer, an electrolyte, an anode functional layer and an anode support layer, and is assembled into a stack unit through bipolar plates, packaging materials and single cells; then multiple stack units are combined and fastened through sealing materials, top plates, bases and bolts to form a high-power SOFC stack. The electronic load controller is used to adjust the load, change the current of the SOFC stack, and record the voltage response under different currents. The electrochemical workstation contains a signal generator for generating the required alternating current (AC) signal for EIS testing to measure the impedance changes of the stack at different frequencies. The gas controller is used to control the supply of fuel gas and oxidant to maintain the gas flow and pressure required by the stack during the test. The temperature controller is used to heat or cool the SOFC stack and monitor the operating temperature of the SOFC stack. The electrodes of the SOFC stack are connected to the electronic load controller and the electrochemical workstation via cables. The data interfaces of the electronic load controller and the electrochemical workstation are connected to the data control terminal via cables for data synchronization and remote control. When performing voltage tests, the electronic load controller adjusts the current, and the data control terminal records the voltage response of the SOFC stack. When performing electrochemical impedance spectroscopy tests, the signal generator of the electrochemical workstation applies a small-amplitude AC signal to the stack, while measuring the impedance response signal of the SOFC stack, and then obtains the electrochemical impedance spectrum through the electrochemical analysis software in the data control terminal.

[0022] In the present invention, a 120×120 mm 2 The effective active reaction area of ​​a single SOFC stack composed of cells is 100×100 mm 2 The structure of the SOFC stack is shown in the figure below: Figure 3 As shown, the structure of a single cell cross section in a SOFC stack is as follows Figure 4As shown. The materials of the anode support layer (ASL) and the anode functional layer (AFL) are both Ni-YSZ, with thicknesses of 400~500 μm and 8~10 μm, respectively. The material of the electrolyte is YSZ, with a thickness of 8~10 μm. The material of the barrier layer is GDC, with a thickness of 5~10 μm. The material of the cathode is LSC, with a thickness of 20~30 μm. Among them, Crofer 22 APU stainless steel is used in the manufacture of metal bipolar plates. The silver mesh is placed between the cathode and the bipolar plate as a cathode gas distributor and current collector. Glass ceramic sealing materials are used in SOFC stacks to maintain the airtightness between the battery and the bipolar plate.

[0023] Before the hot and cold cycle test, the SOFC stack was installed in an electric heating furnace and gradually heated to the reduction temperature and the operating temperature, and then the power generation performance of the SOFC stack was evaluated. A heating rate of 1°C / min and a cooling rate of 0.5°C / min were used for the hot and cold cycle process of the SOFC stack, and the cycle temperature varied between room temperature and 750°C. Pure hydrogen and dry air were used as fuel and oxidant, respectively, and nitrogen was used as a protective gas. During the heating process, dry nitrogen was supplied to the anode at a flow rate of 0.5 L / min. After the temperature reached 750°C, 0.5 L / min of hydrogen was supplied to the anode, and dry air was supplied to the cathode at a flow rate of 1.5 L / min. After the test was completed, it was cooled to room temperature at a rate of 0.5°C / min to complete a cycle. In this embodiment, the SOFC stack was subjected to a total of 10 hot and cold cycle tests.

[0024] Step S2: Use the SOFC stack power generation and test system to carry out hot and cold cycle tests, and use the electronic load controller and electrochemical workstation to collect the polarization curve and electrochemical impedance spectrum of the SOFC stack during each hot and cold cycle operation.

[0025] The SOFC stack was measured from 0 mA / cm using the IT8511 programmable DC electronic load controller. 2 Up to 500 mA / cm 2 The polarization curve under current density of 0A to 50A is as follows: Figure 5 As shown in Figure 2, when the SOFC stack is in service from the first to the tenth cold and hot cycle, the voltage at 500 mA / cm 2The output voltage attenuation rate under current density reached 12.36%. The electrochemical impedance spectroscopy data of the SOFC stack under five DC biases of 0A, 10A, 20A, 30A, and 40A were collected using the IT8511 programmable DC electronic load controller of ITECH and the Gamry Reference 3000AE electrochemical workstation during the hot and cold cycle. DC bias refers to the use of an electronic load controller to keep the SOFC stack at a constant DC current output, which is mainly used to simulate the load operation state of SOFC during the actual power generation process. Among them, the Nyquist data under 0A DC bias are as follows: Figure 6 As shown. From this, we can clearly distinguish the ohmic resistance R caused by pure charge transfer ohm (Right now Figure 6 The left intercept on the horizontal axis Zre) and the polarization impedance R caused by diffusion, electrochemical reaction, etc. pol (Right now Figure 6 The difference between the right intercept and the left intercept on the horizontal axis Zre). ohm The growth rate after 10 hot and cold cycles reached 33.65%, R pol The smallest growth rate was only 10.16%.

[0026] S3: The electrochemical impedance spectroscopy (EIS) data of the SOFC stack are analyzed and fitted using the distribution relaxation time (DRT) method and equivalent circuit model (ECM) to calculate the voltage loss caused by each electrode reaction process of the SOFC during the hot and cold cycles and its contribution to the voltage decay.

[0027] The distribution relaxation time (DRT) method is an advanced method for analyzing electrochemical impedance spectroscopy (EIS) data. This method is particularly suitable for processing impedance data of complex electrochemical systems, especially when the electrode processes of the system include processes on multiple time scales. In the relaxation time distribution method, the total impedance of the SOFC stack is Expressed as ohmic impedance R ohm , polarization impedance R pol The sum of relaxation time Refers to the time required for an electrochemical process to reach equilibrium, where polarization impedance is expressed as relaxation time The integral from 0 to ∞ seconds is as follows: (1); where j and ω are imaginary units and angular frequencies, respectively; solve for different relaxation times Corresponding , that is, the relaxation time distribution diagram corresponding to the EIS data can be obtained. The expression is: γ ( τ ) = R 2 π ⋅ sin[( 1 − n ) π ] cosh[ n ln( τ / τ 0 )] − cos[( 1 − n ) π ] (2); R is the resistance, cosh is the hyperbolic cosine function, n is the number of electron transfers, Represents the relaxation time at the initial moment; the expression of the characteristic frequency f is: (3) The DRT method was used to process the EIS data under five DC biases of 0A, 10A, 20A, 30A, and 40A during the hot and cold cycle. The open source software EISART compiled by Tsinghua University was used to perform DRT calculations on the EIS data. The peaks on the DRT graph were distinguished according to the different characteristics of the electrochemical reaction process of the SOFC stack. The DRT evolution results under 0A DC bias are shown in Figure 2. Figure 7 As shown. For the SOFC structure used in this study, four characteristic peaks can be distinguished in a single DRT graph. Among them, the characteristic peak P A1 (100 ~ 1000Hz) corresponds to the charge transfer reaction and ion transport near the three-phase boundary (TPB) at the anode. C1 (10 ~ 100 Hz) corresponds to the cathode side O2 surface exchange kinetics and O 2− Diffusion. Characteristic peak P A2 (1 ~ 10Hz) corresponds to the anode gas phase diffusion and conversion. Characteristic peak P C2 (0.1 ~1Hz) corresponds to cathode gas phase diffusion and conversion. Under 0A DC bias, the peak value P A1 After 10 cycles of hot and cold, the 2 Increased to 1.308 Ω·cm 2 , the growth rate reached 58.42%. At the same time, the peak value P corresponding to the oxygen reduction reaction kinetics on the cathode side C1 It also increased by 57.77% after 10 hot and cold cycles. DRT was used to distinguish the changing rules of different electrode reaction processes and provide reasonable initial values ​​for ECM fitting.

[0028] In the equivalent circuit model, the equivalent circuit model consists of a series ohmic impedance R ohm , inductor L and RQ unit, the RQ unit is composed of resistor R and constant phase element CPE in parallel, each RQ unit represents an electrode process on a specific time scale; the calculation formula of the total impedance of the equivalent circuit model is: (4); where L self is the self-inductance of the equivalent circuit, L wire is the imaginary mutual inductance, L wire Used to reduce the interference of inductance and mutual inductance on the analysis results.

[0029] Based on the distribution law of the above DRT curve, four electrode reaction processes are determined. In this embodiment, the ohmic impedance (R ohm ), inductance (L) and four RQ units to fit the EIS data. Ohmic impedance ( ) The ECM fitting results are as follows Figure 8 The shaded area in the figure represents the overpotential growth caused by ohmic impedance from the 1st to the 10th hot-cold cycle, that is, the voltage loss caused by ohmic impedance during the 10 hot-cold cycles.

[0030] The ECM fitting results are used to determine the contribution of different electrode reaction processes to voltage decay during the hot and cold cycles, such as Fig. 9 shown. The degradation of (ohmic impedance) dominates the overall performance degradation, with a contribution rate of 57.13%. The second largest contribution comes from R A1 (TPB charge transfer reaction and ion transport on the anode side), the contribution rate is 37.38%. C1 (O2 surface exchange kinetics and O 2- The contribution rate of diffusion is 6.99%. C2 The contribution of (cathode gas phase diffusion and conversion) is 6.58%. A2 The contribution of (anode gas phase diffusion and conversion) is negative (-8.08%). The order of contribution of each electrode reaction process to voltage decay is R S > R A1 > R C1 > R C2 > R A2 .

[0031] S4: Test the mechanical properties of SOFC stack cells after different hot and cold cycles.

[0032] The mechanical properties of a single cell include bending strength, elastic modulus and hardness. The bending strength is tested by a small punch test (SPT) using a small punch testing machine, while the elastic modulus and hardness are tested using a high-precision nanoindentation instrument.

[0033] 1) Test of the bending strength of a single cell: Before the SPT experiment, the single cell was processed into a disc-shaped specimen with a diameter of 10 mm by laser cutting, and then polished. In order to improve the reliability of the bending strength test results, more than 20 SPT tests were conducted on each type of single cell specimen, and the dispersion of its bending strength was analyzed using the Weibull statistical method. The thickness of the anode support layer and the functional layer accounts for more than 95% of the total thickness of the single cell. The cathode, barrier layer and electrolyte have very limited effects on the bending strength of the battery. Therefore, the anode is used as the main basis for the analysis of the bending strength of the single cell. The average bending strength of the single cell after different numbers of hot and cold cycles is shown in Table 1. The initial bending strength of the single cell reached 306.54 MPa, which gradually decreased with the progress of the hot and cold cycles. After 10 hot and cold cycles, the bending strength attenuation rate reached 54.14%.

[0034] Table 1 Average bending strength of single cells after different hot and cold cycles

[0035]

[0036] 2) Testing of elastic modulus and hardness of each component of a single cell: Before the nanoindentation test, the cross section of the single cell consisting of cathode / barrier electrolyte / AFL / ASL was polished with a 0.5μm diamond suspension to obtain a flat surface. During the nanoindentation test, the peak load was 20mN, the loading time was 20 seconds, and then unloaded within 20 seconds. The elastic modulus and hardness of each component of the single cell after different number of cycles are shown in Figure 2. Fig.10 , Fig.11 As shown. The elastic modulus and hardness of the single cell in various states show a distribution pattern of first increasing and then decreasing along the test path. The maximum elastic modulus and hardness of the unserviced sample both appear at the electrolyte position, with average values ​​reaching 219.08 GPa and 18.41 GPa, respectively. The minimum values ​​are 40.57 GPa and 2.62 GPa, respectively, located at the cathode of the single cell. In terms of elastic modulus, after 10 hot and cold cycles, the attenuation rates of the anode support layer and the barrier layer reached 73.38% and 72.60%, respectively; the cathode also reached more than 66.57%, and the electrolyte had the lowest attenuation rate, only 25.56%. In terms of hardness, after 10 hot and cold cycles, the attenuation rates of the anode support layer and the barrier layer reached 87.83% and 94.35%, respectively, and the cathode also reached more than 78.44%. The attenuation rate of the electrolyte also reached 40.51%.

[0037] S5: Scanning electron microscope and X-ray spectrometer are used to analyze the microstructural changes of the SOFC stack components before and after the hot and cold cycle test, and the content of various elements in the SOFC stack and the average diameter of the particles are calculated.

[0038] After the SOFC stack was subjected to hot and cold cycling, it was dismantled and the single cell was evaluated for morphology. Scanning electron microscopy and X-ray energy dispersive spectrometer (EDS) were used to study the changes in the microstructure and element distribution in different regions of the SOFC single cell. The size of the element particles in each electrode before and after the hot and cold cycling was calculated from the SEM and EDS images obtained from S5 using the image processing software ImageJ. The proportion of each type of Ni particle in the SOFC anode after different number of cycles is shown in Table 2. The Ni particle size of the anode before and after the hot and cold cycling was calculated from the EDS image using ImageJ software. The average equivalent circular diameter (φ) of the Ni particles of the unserviced sample was calculated using the area-weighted algorithm. ECD ) is 1.257 μm, and the diameter increases to 1.739 μm after 10 hot and cold cycles. According to the equivalent circle diameter of nickel particles, large particle size particles (LPSPs, 3<φ ECD <10 μm), medium-sized particles (MPSPs, 1<φ ECD<3μm) and small particle size particles (SPSPs, 0<φ ECD <1 μm) were clearly identified. In the unserviced samples, the proportion of SPSPs reached 66.67% at the highest, LPSPs was 1.88% at the lowest, and MPSPs reached 30.05%. The proportion of SPSPs gradually decreased with the progress of the hot and cold cycles, and decreased to 40.72% at the 10th hot and cold cycle. The change pattern of MPSPs was completely opposite, increasing from 30.05% to 48.50% after ten hot and cold cycles.

[0039] Table 2 Proportion of various types of Ni particles in SOFC anode after different cycles

[0040]

[0041] S6: Reveal the coupling relationship between the electrochemical performance and mechanical performance attenuation of SOFC stack, and establish a theoretical model for the electrochemical performance and mechanical performance attenuation of SOFC stack.

[0042] During the hot and cold cycle, the anode Ni particles undergo substantial degradation phenomena such as coarsening, migration and depletion. This not only affects the conductivity and chemical stability of the SOFC anode side, but also makes it more likely to cause structural problems during service. The curves of SOFC output voltage, single cell bending strength, elastic modulus and hardness changing with hot and cold cycles are shown in Figure 2. Fig.12 , Fig.13 , Fig.14 As shown in the figure, it can be found that the output voltage of SOFC, the bending strength of the single cell, and the average equivalent circular diameter of Ni element particles φ ECD The changes of elastic modulus and hardness with the number of hot and cold cycles are all in logarithmic form. Therefore, the logarithmic formula can be used to establish a theoretical model for the changes of SOFC electrochemical, mechanical properties and microstructure under hot and cold cycles. The theoretical model formula is as follows: (5); where y is the output voltage of SOFC, the bending strength of the single cell, and the average equivalent circular diameter of Ni element particles φ ECD , elastic modulus and hardness; x is the number of hot and cold cycles, x ≥ 1 and is a positive integer; C is the SOFC output voltage corresponding to parameter y, the bending strength of the single cell, and the average equivalent circular diameter φ of the Ni element particles ECD The initial value of any one of the properties of the single cell elastic modulus and hardness is obtained by testing after the first hot and cold cycle. n is the attenuation coefficient.

[0043] The fitting values ​​of the attenuation coefficient n of the electrochemical and mechanical performance curves of SOFC during the hot and cold cycle service obtained by experimental test fitting are shown in Table 3. It can be concluded that the attenuation coefficient n corresponding to the bending strength of the single cell is the smallest, only 0.414, which means that the attenuation phenomenon is most serious in the early stage of the hot and cold cycle and gradually slows down in the later stage. Secondly, the attenuation coefficient n corresponding to the elastic modulus of each component of the single cell is between 0.500 and 0.709. Current density 300 mA / cm 2 That is, the attenuation coefficient n corresponding to the output voltage at 30A is the largest, reaching 8.018, and its attenuation curve decreases most slowly.

[0044] Table 3 Fitting values ​​of attenuation coefficient n of electrochemical and mechanical properties curves

[0045]

[0046] Comparison of the test and model values ​​of output voltage and single cell bending strength Fig.15 , Fig.16 Taking the output voltage at 30A and the bending strength of a single cell as an example, it can be found that the experimental values ​​are in good agreement with the model calculation values ​​obtained by formula (4).

[0047] Step S7: predicting the electrochemical and mechanical properties of the SOFC stack after different numbers of hot and cold cycles, as well as the hot and cold cycle service life of the SOFC stack.

[0048] Due to the difference between the electrochemical and mechanical properties of SOFC, when the electrochemical performance of SOFC drops to 50% of the initial performance, the low power generation efficiency will reduce the economic benefits of SOFC equipment. In addition, when the failure of SOFC mechanical performance reaches 50%, it indicates that serious mechanical damage has occurred inside SOFC, which will further affect the electrochemical performance of SOFC stack. Therefore, the failure threshold of electrochemical and mechanical properties of SOFC stack is defined as 50%. At 300 mA / cm 2 For example, when the SOFC stack is at 300 mA / cm 2 When the output voltage decays to 50% of the output voltage of the first hot and cold cycle, its electrochemical performance life is considered to have ended. Taking the bending strength of a single cell as an example, when the bending strength of a single cell in a SOFC stack decays to 50% of the bending strength of the first hot and cold cycle, its electrochemical performance life is considered to have ended.

[0049] According to the theoretical model and failure threshold in S6, the electrochemical and mechanical properties of SOFC stack are predicted, and it can be obtained that SOFC stack at 300 mA / cm 2The hot and cold cycle life of the output voltage is 42 times, and the hot and cold cycle life of the bending strength of a single cell in the SOFC stack is 22 times. Comprehensive analysis shows that the hot and cold cycle life of the SOFC stack is 22 times.

[0050] Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by technicians in this technical field within the essential scope of the present invention should also fall within the protection scope of the present invention.

Claims

1. A method for predicting electrochemical and mechanical properties of a SOFC stack during hot and cold cycles, characterized in that: The steps include: Step S1: preparing the constituent materials of the SOFC stack, completing the assembly of the SOFC stack power generation and test system and the test preparation work, and determining the operating parameters of the SOFC stack cold and hot cycle test according to the actual service conditions; Step S2: using the SOFC stack power generation and test system to carry out a hot and cold cycle test, and using an electronic load controller and an electrochemical workstation to collect polarization curves and electrochemical impedance spectra of the SOFC stack during each hot and cold cycle operation; Step S3: Analyze and fit the electrochemical impedance spectrum data of the SOFC stack using the relaxation time distribution method and the equivalent circuit model, and calculate the voltage loss caused by each electrode reaction process of the SOFC in the hot and cold cycle and the contribution value to the voltage decay; Step S4: testing the mechanical properties of the SOFC stack cells after different hot and cold cycle services; Step S5: using a scanning electron microscope and an X-ray spectrometer to analyze the microstructure change rules of each component of the SOFC stack before and after the hot and cold cycle test, and calculating the content of various elements in the SOFC stack and the average diameter of the particles; Step S6: revealing the coupling relationship between the electrochemical performance and mechanical performance attenuation of the SOFC stack, and establishing a theoretical model for the electrochemical performance and mechanical performance attenuation of the SOFC stack; According to the output voltage of SOFC, the bending strength of single cell, and the average equivalent circular diameter of Ni element particles The change law of elastic modulus and hardness with the number of hot and cold cycles is used to establish a theoretical model for the coupling of electrochemical performance and mechanical performance attenuation of SOFC stack: Where y is the output voltage of SOFC, the bending strength of the single cell, and the average equivalent circular diameter of Ni element particles. The parameter value of any one of the properties of elastic modulus and hardness; x is the number of hot and cold cycles, x≥1 and is a positive integer; C is the SOFC output voltage corresponding to y, the bending strength of the single cell, and the average equivalent circular diameter of the Ni element particles The initial value of any property of elastic modulus and hardness, the specific value of C is obtained by testing after the first hot and cold cycle; n is the attenuation coefficient; Step S7: predicting the electrochemical and mechanical properties of the SOFC stack after different hot and cold cycle times, as well as the hot and cold cycle service life of the SOFC stack; In step S3, the electrochemical impedance spectroscopy data in the cold and hot cycle process is processed using the relaxation time distribution method, and the peaks on the relaxation time distribution diagram are distinguished according to the characteristics of different electrochemical reaction processes of the SOFC stack, and the change laws of different electrode reaction processes are qualitatively distinguished; the electrode reaction process is determined based on the distribution law obtained by the relaxation time distribution method, and a reasonable initial value is provided for the equivalent circuit model element; the ohmic impedance R is used to calculate the initial value of .... ohm An equivalent circuit model consisting of , inductor L and RQ units is used to fit the electrochemical impedance spectroscopy data, quantitatively determine the contribution of different electrode reaction processes to voltage decay in the hot and cold cycles, and determine the contribution value of each electrode reaction process to voltage decay and its ranking; In the relaxation time distribution method, the total impedance Z(ω) of the SOFC stack is expressed as the ohmic impedance R ohm , polarization impedance R pol The relaxation time τ refers to the time required for the electrochemical process to reach equilibrium, where the polarization impedance is expressed as the integral of the relaxation time τ from 0 to ∞ seconds, as shown in the following formula: Where j and ω are imaginary units and angular frequencies, respectively. Solving for γ(τ) corresponding to different relaxation times τ, we can obtain the relaxation time distribution diagram corresponding to the electrochemical impedance spectroscopy data, and the expression of γ(τ) is: Where R is the resistance, cosh is the hyperbolic cosine function, n is the number of electron transfers, and τ0 represents the relaxation time at the initial moment; The expression of characteristic frequency f is: In the equivalent circuit model, the equivalent circuit model consists of a series ohmic impedance R ohm , inductor L and RQ unit, the RQ unit is composed of a resistor R and a constant phase element CPE in parallel, and each RQ unit represents an electrode process on a specific time scale; The calculation formula of the total impedance of the equivalent circuit model is: Among them, L self is the self-inductance of the equivalent circuit, L wire is the imaginary mutual inductance, L wire Used to reduce the interference of inductance and mutual inductance on the analysis results.

2. The method for predicting electrochemical and mechanical properties of a SOFC stack during a cold and hot cycle according to claim 1, characterized in that: In step S1, the SOFC stack power generation and test system includes a SOFC stack, an electronic load controller, an electrochemical workstation, a gas controller, a temperature controller and a data control terminal; a single cell in the SOFC stack includes a cathode, a barrier layer, an electrolyte, an anode functional layer and an anode support layer, and is assembled into a stack unit through a bipolar plate, a packaging material and a single cell; a plurality of stack units are assembled and combined and fastened together through sealing materials, a top plate, a base and bolts to form a high-power SOFC stack; the electronic load controller is used to adjust the load, change the current of the SOFC stack, and record the current under different currents. pressure response; the electrochemical workstation can generate the AC signal required for electrochemical impedance spectroscopy testing and measure the impedance changes of the SOFC stack at different frequencies; the gas controller is used to control the supply of fuel gas and oxidant to maintain the gas flow and pressure required by the stack during the test; the temperature controller is used to heat or cool the SOFC stack and monitor the operating temperature of the SOFC stack; the electrodes of the SOFC stack are connected to the electronic load controller and the electrochemical workstation through cables, and the data interfaces of the electronic load controller and the electrochemical workstation are connected to the data control terminal through cables for data synchronization and remote control; The operating parameters of the SOFC stack thermal cycle test include temperature range, heating and cooling rate, gas type, gas flow rate, cycle frequency, number of cycles and current density; the operating temperature range is 650℃~800℃, and the reduction temperature range is 700℃~900℃; the heating rate is 0.5~2℃ / min, and the cooling rate is 0.5~1℃ / min; pure hydrogen and dry air are used as fuel and oxidant respectively, and nitrogen is used as protective gas; During the heating process, dry nitrogen is supplied to the anode at a flow rate of 0.3 to 0.9 L / min, hydrogen is supplied to the anode at a flow rate of 0.3 to 0.9 L / min, and dry air is supplied to the cathode at a flow rate of 0.9 to 2.7 L / min.

3. The method for predicting electrochemical and mechanical properties of a SOFC stack during a cold and hot cycle according to claim 1, characterized in that: In step S2, the SOFC stack power generation and test system is used to set the hot and cold cycle temperature range and the heating and cooling rate of the SOFC stack, set the gas supply program on the cathode and anode sides of the SOFC stack, and heat the SOFC stack from room temperature to the reduction temperature for reduction. After the reduction is completed, the stack is cooled to the operating temperature, and the SOFC stack is started to start the hot and cold cycle test; The polarization curve of the SOFC stack during each hot and cold cycle is collected by an electronic load controller, and the attenuation rate of the SOFC stack at current density A1 is calculated. The reference range of current density A1 is 0-500 mA / cm 2 ; Use an electronic load controller and an electrochemical workstation to collect electrochemical impedance spectroscopy data under 3 to 5 DC biases during each hot and cold cycle of the SOFC stack.

4. The method for predicting electrochemical and mechanical properties of a SOFC stack during a cold and hot cycle according to claim 1, characterized in that: In step S4, the SOFC stack is dismantled after the hot and cold cycles to analyze the mechanical properties of each component of the single cell; the mechanical properties of the single cell include bending strength, elastic modulus and hardness. The bending strength is tested using a small punch testing machine, and the Weibull statistical method is used to analyze the dispersion of the bending strength of the single cell; the elastic modulus and hardness are tested using a high-precision nanoindentation instrument.

5. The method for predicting electrochemical and mechanical properties of a SOFC stack during a cold and hot cycle according to claim 1, characterized in that: In step S5, a scanning electron microscope and an X-ray spectrometer are used to study the microstructure and element distribution of each component of the single battery after different cold and hot cycles. The image processing software ImageJ is used to calculate the size of the element particles in each electrode from the images of the scanning electron microscope and the X-ray spectrometer; the average equivalent circle diameter of the Ni element particles in the single battery sample before and after the cold and hot cycles is calculated using an area weighted algorithm.

6. The method for predicting electrochemical and mechanical properties of a SOFC stack during a cold and hot cycle according to claim 1, characterized in that: In step S7, the failure thresholds of the electrochemical and mechanical properties of the SOFC stack are defined as 20% to 80%, and the hot and cold cycle service life of the SOFC stack is predicted based on the theoretical model in step S6.

Citation Information

Patent Citations

  • Method for testing mechanical properties of anode-electrolyte-cathode component of SOFC (solid oxide fuel cell)

    CN116296903A

  • Fuel cell life prediction method based on impedance spectrum relaxation time distribution

    CN116699434A

  • Solid oxide fuel cell stack electrochemical performance life prediction method

    CN116879781A

  • Service life prediction method for structural damage and electrochemical performance attenuation of SOFC (Solid Oxide Fuel Cell) electric pile

    CN116959634A

  • Decoupling analysis method of lithium deposition kinetics based on relaxation time distribution

    CN117630667A