A dual-gate control device and manufacturing method

By setting up N-type MOS and P-type MOS regions in the semiconductor power device and using PN junction isolation to achieve dual gate control, it solves the problem in the existing technology that high-voltage and high-current devices in the high-frequency field are difficult to achieve low loss, and achieves a better Fast turn-off and lower losses.

CN118507527BActive Publication Date: 2024-10-11SHANGHAI AIJI SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410961494.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-10-11
Estimated Expiration
2044-07-18

AI Technical Summary

Technical Problem

It is difficult for existing semiconductor power devices to achieve high voltage and large current while maintaining low loss in the high-frequency field. The on-state voltage drop of unipolar MOS devices is large, and the off-time of bipolar IGBT devices is long, which limits their operating frequency.

Method used

Design a dual-gate control device. By setting N-type MOS and P-type MOS regions on the substrate, and using the PN junction isolation between the first and second gates to achieve dual-gate control, in a single trench When the gate is working, a unipolar MOS is formed, and when two trench gates are used at the same time, a bipolar device is formed. The lateral PN junction is used to share the withstand voltage and prevent carrier interference, achieving faster turn-off.

Benefits of technology

It achieves flexible use of devices and low dynamic loss in the high-frequency field, is suitable for high-voltage and high-current applications, and reduces static loss and dynamic loss.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118507527B_ABST
    Figure CN118507527B_ABST
Patent Text Reader

Abstract

The present invention provides a dual-gate control device and a manufacturing method, the device comprising: a substrate, a front metal region is arranged on the front of the substrate, a back metal region is arranged on the back of the substrate, and the substrate comprises at least one N-type MOS region and at least one P-type MOS region located between the front metal region and the back metal region; a first gate is arranged on the front of the substrate, a second gate is arranged on the back of the substrate, a PN junction is arranged between the first gate and the second gate, the N-type MOS region and the P-type MOS region are separated by the PN junction, the first gate is used to control the conduction or shutoff of the N-type MOS region, and the second gate is used to control the conduction or shutoff of the P-type MOS region. This solution can realize that the semiconductor power device can form a unipolar P-type MOS or N-type MOS, and can also form a bipolar device; and the switching speed is fast, the loss is low, and it can be applied in the high-frequency field.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor power devices, and in particular to a dual-gate control device and a manufacturing method thereof. Background Art

[0002] MOS is the abbreviation of MOSFET (Metal-Oxide-Semiconductor Field-Effect Transistor). It is a unipolar device, generally divided into N-type MOS and P-type MOS according to the conductivity type, where N-type MOS conducts electricity through electrons and P-type MOS conducts electricity through holes. The advantage of MOS is fast switching speed and the operating frequency can reach 100MHZ. The disadvantage is that the on-state voltage drop is large (conduction loss is large), and it is difficult to make high-voltage and high-current devices.

[0003] IGBT (Insulate-Gate Bipolar Transistor) is an insulated gate bipolar transistor, which is a bipolar device. Electrons and holes participate in conduction at the same time, with a small on-state voltage drop (small conduction loss), and can be made into high-voltage and high-current devices. Generally, electrons are controlled by the front gate, and when the gate voltage is lower than the threshold voltage, the electron channel disappears immediately. However, holes are injected from the back collector, and the front gate cannot directly cut off the hole carrier current. It needs to be gradually reduced through carrier recombination until the hole current is cut off, resulting in a much longer turn-off time than unipolar MOS devices. Limited by dynamic losses, its operating frequency is up to tens of KHZ. Therefore, there is a need for a device that can be used in high-frequency fields (for example, switching frequencies above 100KHZ) and can achieve high voltage and high current. Summary of the invention

[0004] The purpose of the present invention is to provide a dual-gate control device and a manufacturing method, so that the semiconductor power device can form not only a unipolar P-type MOS or N-type MOS, but also a bipolar device; and the switching speed is fast, the loss is low, and it can be applied in the high-frequency field.

[0005] The technical solution provided by the present invention is as follows:

[0006] In a first aspect, the present application discloses a dual-gate control device, comprising:

[0007] A substrate, wherein a front metal region is disposed on the front side of the substrate, a back metal region is disposed on the back side of the substrate, and the substrate comprises at least one N-type MOS region and at least one P-type MOS region located between the front metal region and the back metal region;

[0008] A first gate is arranged on the front side of the substrate, and a second gate is arranged on the back side of the substrate. A PN junction is arranged between the first gate and the second gate, and the N-type MOS region and the P-type MOS region are separated by the PN junction. The first gate is used to control the conduction or shutoff of the N-type MOS region, and the second gate is used to control the conduction or shutoff of the P-type MOS region.

[0009] This solution sets at least one N-type MOS region and at least one P-type MOS region between the front metal region and the back metal region, and sets a first gate and a second gate, and isolates the N-type MOS region and the P-type MOS region through a PN junction between the first gate and the second gate, so that the device can achieve dual-gate control. When a single trench gate is working, a unipolar P-type MOS or N-type MOS can be formed. When two trench gates are used at the same time, a bipolar device can be formed, making the device more flexible to use and able to achieve faster shutdown, thereby obtaining lower dynamic losses and being suitable for high-frequency scenarios.

[0010] In some embodiments, it includes a P-type MOS region and two N-type MOS regions respectively located on both sides of the P-type MOS region;

[0011] The first gate and the second gate are each a group, and form two PN junctions to achieve isolation of one P-type MOS region and two N-type MOS regions;

[0012] The PN junction includes a P+ layer region close to the P-type MOS region and an N+ layer region close to the N-type MOS region.

[0013] This solution sets a P-type MOS region and two N-type MOS regions, and forms a P- / P+ / N+ / N- structure in the lateral direction. By utilizing the lateral PN junction depletion, on the one hand, the overall withstand voltage of the device can be shared, so that the device can be made thinner at the same withstand voltage, thereby reducing static loss; on the other hand, it can prevent a large number of hole carriers in the P-type MOS region from flowing to the N-type MOS region, and prevent a large number of electron carriers in the N-type MOS region from flowing to the P-type MOS region, thereby avoiding mutual interference between the two regions.

[0014] In some embodiments, the P-type MOS region includes:

[0015] A super junction P- region, located on the side of the P+ layer region;

[0016] A P-well region, disposed on the side of the first gate and between the super junction P-region and the front metal region;

[0017] An N-region, disposed on the side of the second gate and located between the super junction P-region and the back metal region;

[0018] A back deep N+ region located between the N- region and the back metal region;

[0019] The back shallow P+ region is located between the back deep N+ region and the second gate, and between the N- region and the back metal region.

[0020] In some embodiments, the N-type MOS region includes:

[0021] N- region, located on the side of the N+ layer region;

[0022] A back shallow N+ region, located on the side of the second gate and between the N- region and the back metal region;

[0023] A P-well region, in an L-shape, disposed on the side of the first gate and between the N-region and the front metal region;

[0024] A front shallow N+ region, disposed on the side of the first gate and between the N- region and the front metal region;

[0025] The front deep P+ region is located in the L-shaped opening of the P-well region and is isolated from the first gate by the front shallow N+ region and the P-well region. The front deep P+ region is also arranged between the P-well region and the front metal region.

[0026] In some embodiments, the first gate includes a front trench region, a front gate oxide layer located on an inner wall of the front trench region, and a front polysilicon gate located inside the front gate oxide layer;

[0027] The second gate includes a back trench region, a back gate oxide layer located on an inner wall of the back trench region, and a back polysilicon gate located inside the back gate oxide layer.

[0028] In some embodiments, the substrate is an N-type Si substrate or an N-type SiC substrate.

[0029] In a second aspect, the present application discloses a method for manufacturing a dual-gate control device, comprising the steps of:

[0030] Depositing an N+ type silicon thin layer and a P+ type silicon thin layer vertically on the substrate to form at least one PN junction;

[0031] A first gate and a second gate are formed at two ends of the PN junction, respectively, and are located on the front side and the back side of the substrate;

[0032] At least one N-type MOS region and at least one P-type MOS region are formed on both sides of the PN junction by ion implantation, the first gate is used to control the conduction or shutoff of the N-type MOS region, and the second gate is used to control the conduction or shutoff of the P-type MOS region;

[0033] A front metal region is formed on the front side of the substrate, and a back metal region is disposed on the back side of the substrate.

[0034] In some embodiments, the method specifically comprises the steps of:

[0035] A deep groove is formed on the surface of the substrate, wherein the opening of the deep groove is located on the front side of the substrate;

[0036] Depositing the N+ type silicon thin layer and the P+ type silicon thin layer on the side walls of both sides of the deep trench to form two longitudinal PN junctions;

[0037] Filling P-type silicon in the deep trench to form a super junction P-region;

[0038] Ion implantation of trivalent elements on the front side of the substrate and thermal diffusion to form a P-well region;

[0039] The first gate and the second gate are respectively formed on the front side and the back side of the substrate and are located at two ends of the PN junction;

[0040] Ion implantation of pentavalent elements on the front and back sides of the substrate respectively and thermal diffusion to form a front shallow N+ region and a back shallow N+ region;

[0041] Ion implantation of a trivalent element on the back side of the substrate and thermal diffusion to form a shallow P+ region on the back side;

[0042] Ion implantation of a trivalent element into the front surface of the substrate and thermal diffusion to form a front deep P+ region;

[0043] Ion implantation of pentavalent elements on the back side of the substrate and thermal diffusion to form a back side deep N+ region;

[0044] Metal sputtering is performed on the front side and the back side of the substrate to form a front side metal region and a back side metal region respectively.

[0045] In some embodiments, the N+ type silicon thin layer and the P+ type silicon thin layer are deposited on the sidewalls of both sides of the deep trench to form two longitudinal PN junctions, specifically including:

[0046] The N+ type silicon thin layer is deposited in the area of ​​the deep groove; the N+ type silicon thin layer on the substrate surface and the bottom of the deep groove is etched away to form an N+ layer area located on the side wall of the deep groove; the P+ type silicon thin layer is deposited in the area of ​​the deep groove; the P+ type silicon thin layer on the substrate surface and the bottom of the deep groove is etched away to form a P+ layer area located on the side of the N+ layer area.

[0047] In some embodiments, the first gate and the second gate located at both ends of the PN junction are formed on the front side and the back side of the substrate, respectively, specifically including:

[0048] Grooves are etched on the front and back sides of the substrate to form a front groove region and a back groove region; a front gate oxide layer and a back gate oxide layer are thermally grown in the front groove region and the back groove region respectively; polysilicon is filled in the front gate oxide layer and the back gate oxide layer to form a front polysilicon gate and a back polysilicon gate.

[0049] A dual-gate control device and a manufacturing method provided by the present invention can realize dual-gate control. When a single trench gate is working, a unipolar P-type MOS or N-type MOS can be formed. When two trench gates are used at the same time, a bipolar device can be formed, making the device more flexible to use and able to achieve faster shutdown, thereby obtaining lower dynamic losses and being suitable for high-frequency scenarios. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] The preferred implementation scheme will be described below in a clear and understandable manner with reference to the accompanying drawings to further illustrate the above-mentioned characteristics, technical features, advantages and implementation methods of the present solution.

[0051] Figure 1 is a schematic diagram of the overall structure of an embodiment of the present invention;

[0052] Figure 2 It is a schematic diagram of the overall process of an embodiment of the present invention;

[0053] Figure 3 is a flow chart of an embodiment of the present invention;

[0054] Figure 4 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0055] Figure 5 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0056] Figure 6 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0057] Figure 7It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0058] Figure 8 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0059] Fig. 9 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0060] Fig.10 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0061] Fig.11 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0062] Fig.12 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0063] Fig.13 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0064] Fig.14 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0065] Fig.15 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0066] Fig.16 It is a schematic diagram of a manufacturing process of a method for manufacturing a dual-gate control device of the present invention;

[0067] Fig.17 It is a schematic diagram of a manufacturing process of the dual-gate control device manufacturing method of the present invention. DETAILED DESCRIPTION

[0068] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the specific implementation methods of the present invention will be described below with reference to the accompanying drawings. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings and other implementation methods can be obtained based on these drawings without creative work.

[0069] In order to simplify the drawings, only the parts related to the present invention are schematically shown in each figure, and they do not represent the actual structure of the product. In addition, in order to simplify the drawings and facilitate understanding, in some figures, only one of the parts with the same structure or function is schematically drawn or marked. In this article, "one" not only means "only one", but also means "more than one".

[0070] MOS tubes are unipolar devices, and are generally divided into N-type MOS and P-type MOS according to the conductivity type. N-type MOS conducts electricity through electrons, and P-type MOS conducts electricity through holes. The advantages of MOS are fast switching speed and the operating frequency can reach 100MHZ. The disadvantage is that the on-state voltage drop is large (conduction loss is large), and it is difficult to make high-voltage and high-current devices.

[0071] IGBT is a bipolar device. Electrons and holes participate in conduction at the same time. The on-state voltage drop is small (conduction loss is small), and it can be made into a high-voltage and high-current device. Generally, electrons are controlled by the front gate. When the gate voltage is lower than the threshold voltage, the electron channel disappears immediately. However, holes are injected from the back collector. The front gate cannot directly cut off the hole carrier current. It needs to be gradually reduced through carrier recombination until the hole current is cut off, resulting in a much longer turn-off time than the unipolar MOS device. Limited by dynamic losses, its operating frequency is up to tens of KHZ. This application combines the characteristics of MOS tubes and IGBTs to design a dual-gate control device. Combining the advantages of both, the device can achieve faster switching speed and low loss, and can be used in high-frequency fields. The following is a detailed description with reference to the accompanying drawings:

[0072] In one embodiment, Figure 1 As shown, the present application discloses a dual-gate control device, comprising: a substrate 1, a front metal region 13 is arranged on the front side of the substrate 1, a back metal region 14 is arranged on the back side of the substrate 1, and the substrate 1 comprises at least one N-type MOS region and at least one P-type MOS region located between the front metal region 13 and the back metal region 14; a first gate (gate G1) is arranged on the front side of the substrate 1, a second gate (gate G2) is arranged on the back side of the substrate 1, a PN junction is arranged between the first gate and the second gate, the N-type MOS region and the P-type MOS region are separated by the PN junction, the first gate is used to control the conduction or cut-off of the N-type MOS region, and the second gate is used to control the conduction or cut-off of the P-type MOS region.

[0073] like Figure 1 As shown, the front side of the substrate 1 of the present application refers to the upper side of the substrate 1 in the illustrated direction, and the back side of the substrate 1 refers to the lower side of the substrate 1 in the illustrated direction. In a specific implementation, the substrate is selected from an N-type Si substrate or an N-type SiC substrate. In other embodiments, adjustments can be made according to requirements, and the present application does not limit this.

[0074] The dual-gate control of the present application can trigger both gates at the same time, or trigger only one of the gates, which is more flexible. The device is composed of an N-type MOS region and a P-type MOS region, wherein the N-type MOS region is controlled by the front gate G1 to be turned on or off, and the P-type MOS region is controlled by the back gate G2 to be turned on or off. This solution is based on the original N-type trench gate MOS. By adding a trench gate P-type MOS area, N-type MOS relies on electrons for conduction, and P-type MOS relies on holes for conduction. The device structure is a dual-carrier (electron and hole) device. When the dual gates are triggered at the same time, the accumulation of dual carriers will make the static conduction loss of the device lower. In addition, in traditional IGBT devices, the hole carriers on the back are not controlled by the gate, and the hole carriers need to be gradually eliminated through recombination, resulting in a long turn-off time and high dynamic switching loss. It is not suitable for application in the high-frequency field (frequency above 100KHZ). This device controls hole injection by the back gate, and uses the back gate electrode G2 to achieve faster turn-off, thereby obtaining lower dynamic losses. It can be applied in the high-frequency field (frequency above 100KHZ) and is suitable for high-voltage and high-current devices.

[0075] The ratio of the N-type MOS region to the P-type MOS region can be designed according to actual application requirements, and this application does not impose any limitation thereto. A plurality of dual-gate control devices of the present invention are also connected in parallel to form a complete component.

[0076] This solution sets at least one N-type MOS region and at least one P-type MOS region between the front metal region 13 and the back metal region 14, and sets a first gate and a second gate, and isolates the N-type MOS region and the P-type MOS region through a PN junction between the first gate and the second gate, so that the device can achieve dual-gate control. When a single trench gate is working, a unipolar P-type MOS or N-type MOS can be formed. When two trench gates are used at the same time, a bipolar device can be formed, making the device more flexible to use and able to achieve faster shutdown, thereby obtaining lower dynamic losses and being suitable for high-frequency scenarios.

[0077] In one embodiment, Figure 1 As shown, the dual-gate control device of the present application includes a P-type MOS region and two N-type MOS regions respectively located on both sides of the P-type MOS region; the first gate and the second gate are each a group, and two PN junctions are formed to achieve isolation of one P-type MOS region and two N-type MOS regions.

[0078] The PN junction includes a P+ layer region 3 close to the P-type MOS region and an N+ layer region 2 close to the N-type MOS region.

[0079] This solution sets a P-type MOS region and two N-type MOS regions, and forms a P- / P+ / N+ / N- structure in the lateral direction. By utilizing the lateral PN junction depletion, on the one hand, the overall withstand voltage of the device can be shared, so that the device can be made thinner at the same withstand voltage, thereby reducing static loss; on the other hand, it can prevent a large number of hole carriers in the P-type MOS region from flowing to the N-type MOS region, and prevent a large number of electron carriers in the N-type MOS region from flowing to the P-type MOS region, thereby avoiding mutual interference between the two regions.

[0080] In one embodiment, Figure 1 As shown, based on the aforementioned embodiment, the P-type MOS region includes: a super junction P-region 4, a P well region (Pwell region) 5, an N-region (i.e., the region of the substrate 1 itself), a back deep N+ region 12 and a back shallow P+ region 10.

[0081] The super junction P-region 4 is located on the side of the P+ layer region 3; the P well region 5 is arranged on the side of the first gate and is located between the super junction P-region 4 and the front metal region 13; the N-region is arranged on the side of the second gate and is located between the super junction P-region 4 and the back metal region 14; the back deep N+ region 12 is located between the N-region and the back metal region 14; the back shallow P+ region 10 is located between the back deep N+ region 12 and the second gate, and is located between the N-region and the back metal region 14.

[0082] Furthermore, the N-type MOS region includes: an N-region (ie, the region of the substrate 1 itself), a back shallow N+ region 9, a P well region (Pwell region) 5, a front shallow N+ region 8 and a front deep P+ region 11.

[0083] The N-region is located on the side of the N+ layer region 2; the back shallow N+ region 9 is located on the side of the second gate and between the N-region and the back metal region 14; the P-well region 5 is L-shaped, arranged on the side of the first gate and between the N-region and the front metal region 13; the front shallow N+ region 8 is arranged on the side of the first gate and between the N-region and the front metal region 13; the front deep P+ region 11 is located in the L-shaped opening of the P-well region 5, and is isolated from the first gate by the front shallow N+ region 8 and the P-well region 5, and the front deep P+ region 11 is also arranged between the P-well region 5 and the front metal region 13.

[0084] Furthermore, the first gate includes a front trench region 6.1, a front gate oxide layer 6.2 located on the inner wall of the front trench region 6.1, and a front polysilicon gate 6.3 located inside the front gate oxide layer 6.2.

[0085] The second gate includes a back trench region 7.1, a back gate oxide layer 7.2 located on the inner wall of the back trench region 7.1, and a back polysilicon gate 7.3 located inside the back gate oxide layer 7.2.

[0086] In this solution, the P-type MOS region is composed of a back metal region 14, a trench gate G2, a back shallow P+ region 10, a back deep N+ region 12, an N-region 1, a super junction P-region 4, a Pwell region 5, and a front metal region 13; the P-type MOS is turned on / off by the back trench gate G2, which is composed of a back trench region 7.1, a back gate oxide layer 7.2, and a back polysilicon gate 7.3. The N-type MOS region is composed of a back metal region 14, a trench gate G1, a back shallow N+ region 9, an N-region 1, a front deep P+ region 11, a front shallow N+ region 8, a Pwell region 5, and a front metal region 13; the N-type MOS is turned on / off by the front trench gate G1, which is composed of a front trench region 6.1, a front gate oxide layer 6.2, and a front polysilicon gate 6.3.

[0087] In one embodiment, Figure 2 As shown, the present application discloses a method for manufacturing a dual-gate control device, comprising the steps of:

[0088] S100, vertically depositing an N+ type silicon thin layer and a P+ type silicon thin layer on a substrate to form at least one PN junction;

[0089] S200, forming a first gate and a second gate located on the front side and the back side of the substrate at two ends of the PN junction respectively;

[0090] S300, forming at least one N-type MOS region and at least one P-type MOS region on both sides of the PN junction by ion implantation, wherein the first gate is used to control the conduction or shutoff of the N-type MOS region, and the second gate is used to control the conduction or shutoff of the P-type MOS region;

[0091] S400, forming a front metal region on the front side of the substrate, and providing a back metal region on the back side of the substrate.

[0092] This solution sets at least one N-type MOS region and at least one P-type MOS region between the front metal region and the back metal region, and sets a first gate and a second gate, and isolates the N-type MOS region and the P-type MOS region through a PN junction between the first gate and the second gate, so that the device can achieve dual-gate control. When a single trench gate is working, a unipolar P-type MOS or N-type MOS can be formed. When two trench gates are used at the same time, a bipolar device can be formed, making the device more flexible to use and able to achieve faster shutdown, thereby obtaining lower dynamic losses and being suitable for high-frequency scenarios.

[0093] In one embodiment, Figure 3 As shown, based on the above-mentioned embodiments, the manufacturing method of the dual-gate control device disclosed in the present application specifically includes the steps of:

[0094] S10, opening a deep groove on the surface of the substrate, wherein the opening of the deep groove is located on the front side of the substrate;

[0095] S20, depositing an N+ type silicon thin layer and a P+ type silicon thin layer on the side walls of both sides of the deep trench to form two longitudinal PN junctions;

[0096] S30, filling the deep trench with P-type silicon to form a super junction P-region;

[0097] S40, ion implanting a trivalent element into the front side of the substrate and thermally diffusing the implant to form a P-well region;

[0098] S50, forming a first gate and a second gate located at two ends of the PN junction on the front side and the back side of the substrate respectively;

[0099] S60, ion implanting pentavalent elements into the front and back sides of the substrate respectively and thermally diffusing them to form a front shallow N+ region and a back shallow N+ region;

[0100] S70, ion implanting a trivalent element on the back side of the substrate and thermally diffusing it to form a shallow P+ region on the back side; ion implanting a trivalent element on the front side of the substrate and thermally diffusing it to form a deep P+ region on the front side;

[0101] S80, ion implanting pentavalent elements on the back side of the substrate and thermally diffusing the elements to form a deep N+ region on the back side;

[0102] S90, performing metal sputtering on the front side and the back side of the substrate to form a front side metal region and a back side metal region respectively.

[0103] In one embodiment, based on the above-mentioned embodiment, an N+ type silicon thin layer and a P+ type silicon thin layer are deposited on the sidewalls of both sides of the deep trench to form two longitudinal PN junctions, specifically including:

[0104] S21, depositing an N+ type silicon thin layer in the deep groove area;

[0105] S22, etching away the N+ type silicon thin layer on the substrate surface and the bottom of the deep trench to form an N+ layer region located on the sidewall of the deep trench;

[0106] S23, depositing a P+ type silicon thin layer in the deep groove area;

[0107] S24, etching away the P+ type silicon thin layer on the substrate surface and the bottom of the deep trench to form a P+ layer region located on the side of the N+ layer region.

[0108] Furthermore, a first gate and a second gate located at both ends of the PN junction are formed on the front side and the back side of the substrate respectively, specifically comprising:

[0109] S51, etching grooves on the front side and the back side of the substrate to form a front side groove region and a back side groove region respectively;

[0110] S52, thermally growing a front gate oxide layer and a back gate oxide layer in the front trench region and the back trench region respectively;

[0111] S53, filling polysilicon in the front gate oxide layer and the back gate oxide layer respectively to form a front polysilicon gate and a back polysilicon gate.

[0112] In one embodiment, based on the above-mentioned embodiment, the manufacturing method of the dual-gate control device disclosed in the present application has the following specific manufacturing steps:

[0113] S1, such as Figure 4 As shown, a substrate 1 required for manufacturing a device is selected, and the substrate 1 is selected as an N-type Si substrate or an N-type SiC substrate;

[0114] S2, such as Figure 5 As shown, a deep groove is opened on an N-type silicon substrate 1, and the opening of the deep groove is located on the front side of the substrate 1;

[0115] S3, such as Figure 6 As shown, a thin N+ type silicon layer is deposited near the deep trench (on the front side of the substrate 1);

[0116] S4, such as Figure 7 As shown, the N+ type silicon thin layer on the surface of the substrate 1 and the bottom of the deep groove is etched away to form a vertical N+ layer region 2;

[0117] S5, such as Figure 8 As shown, a P+ type silicon thin layer is deposited near the deep trench (on the front side of the substrate 1);

[0118] S6, such as Fig. 9 As shown, the P+ silicon thin layer on the surface of the substrate 1 and the bottom of the deep groove is etched away to form a longitudinal P+ layer region 3; so that a P- / P+ / N+ / N- structure is formed in the lateral direction of the substrate 1. By utilizing the lateral PN junction depletion, on the one hand, the overall withstand voltage of the device can be shared, so that the device can be made thinner under the same withstand voltage, thereby reducing static loss; at the same time, it can prevent a large number of hole carriers in the P-type MOS region from flowing to the N-type MOS region, and prevent a large number of electron carriers in the N-type MOS region from flowing to the P-type MOS region, thereby avoiding mutual interference between the two regions;

[0119] S7, such as Fig.10 As shown, P-type silicon is filled in the deep trench to form a super junction P- region 4, and the super junction P- region 4 is located on the side of the P+ layer region 3;

[0120] S8, such as Fig.11 As shown, a trivalent element is ion-implanted on the front side of the substrate 1 and thermally diffused to form a P-hydrazine region 5, and the P-well region 5 is arranged on the side of the first gate and between the super junction P-region 4 and the front metal region 13;

[0121] S9, such as Fig.12 As shown, trenches are etched on the front and back sides of the substrate 1 to form a front trench region 6.1 and a back trench region 7.1;

[0122] S10, such as Fig.13 As shown, a front gate oxide layer 6.2 and a back gate oxide layer 7.2 are formed by thermal growth in the front trench region 6.1 and the back trench region 7.1, and polysilicon is filled in the front gate oxide layer 6.2 and the back gate oxide layer 7.2 to form a front polysilicon gate 6.3 and a back polysilicon gate 7.3;

[0123] S11, such as Fig.14 As shown, 5-valent elements are ion-implanted into the front and back sides of the substrate 1 and thermally diffused to form a front shallow N+ region 8 and a back shallow N+ region 9. The front shallow N+ region 8 is arranged on the side of the first gate and is located between the N- region and the front metal region 13. The back shallow N+ region 9 is located on the side of the second gate and is located between the N- region and the back metal region 14.

[0124] S12, such as Fig.15 As shown, a trivalent element is ion-implanted on the back side of the substrate 1 and thermally diffused to form a back shallow P+ region 10, the shallow P+ region 10 is located between the back deep N+ region 12 and the second gate, and between the N- region and the back metal region 14;

[0125] S13, such as Fig.16 As shown, a trivalent element is ion-implanted and thermally diffused on the front side of the substrate 1 to form a front deep P+ region 11, the front deep P+ region 11 is located in the L-shaped opening of the P-well region 5, and is isolated from the first gate by the front shallow N+ region 8 and the P-well region 5, and the front deep P+ region 11 is also arranged between the P-well region 5 and the front metal region 13;

[0126] S14, such as Fig.17 As shown, a 5-valent element is ion-implanted and thermally diffused on the back side of the substrate 1 to form a back side deep N+ region 12, and the back side deep N+ region 12 is located between the N- region and the back side metal region 14;

[0127] S15, sputtering metal on the front side of the substrate 1 to form a front metal region 13 and a back metal region 14 to form a final product, such as Figure 1 shown.

[0128] It should be noted that the above embodiments can be freely combined as needed. The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered as the protection scope of the present invention.

Claims

1. A dual-gate control device, characterized in that: include: A substrate, wherein a front metal region is disposed on the front side of the substrate, a back metal region is disposed on the back side of the substrate, and the substrate comprises a P-type MOS region located between the front metal region and the back metal region and two N-type MOS regions respectively located on both sides of the P-type MOS region; A group of first gates are arranged on the front side of the substrate, and a group of second gates are arranged on the back side of the substrate. A PN junction is arranged between the first gates and the corresponding second gates to form two PN junctions to achieve isolation of one P-type MOS region and two N-type MOS regions. The PN junction includes a P+ layer region close to the P-type MOS region and an N+ layer region close to the N-type MOS region. The first gate is used to control the conduction or disconnection of the N-type MOS region, and the second gate is used to control the conduction or disconnection of the P-type MOS region.

2. The dual-gate control device according to claim 1, characterized in that: The P-type MOS region includes: A super junction P- region, located on the side of the P+ layer region; A P-well region, disposed on the side of the first gate and between the super junction P-region and the front metal region; An N-region, disposed on the side of the second gate and located between the super junction P-region and the back metal region; A back deep N+ region located between the N- region and the back metal region; The back shallow P+ region is located between the back deep N+ region and the second gate, and between the N- region and the back metal region.

3. The dual-gate control device according to claim 1, characterized in that: The N-type MOS region includes: N- region, located on the side of the N+ layer region; A back shallow N+ region, located on the side of the second gate and between the N- region and the back metal region; A P-well region, in an L-shape, disposed on the side of the first gate and between the N-region and the front metal region; A front shallow N+ region, disposed on the side of the first gate and between the N- region and the front metal region; The front deep P+ region is located in the L-shaped opening of the P-well region and is isolated from the first gate by the front shallow N+ region and the P-well region. The front deep P+ region is also arranged between the P-well region and the front metal region.

4. The dual-gate control device according to claim 1, characterized in that: The first gate includes a front trench region, a front gate oxide layer located on the inner wall of the front trench region, and a front polysilicon gate located inside the front gate oxide layer; The second gate includes a back trench region, a back gate oxide layer located on an inner wall of the back trench region, and a back polysilicon gate located inside the back gate oxide layer.

5. The dual-gate control device according to claim 1, characterized in that: The substrate is an N-type Si substrate or an N-type SiC substrate.

6. A method for manufacturing a dual-gate control device, characterized in that: Includes steps: A deep groove is formed on the surface of the substrate, wherein the opening of the deep groove is located on the front side of the substrate; Depositing an N+ type silicon thin layer and a P+ type silicon thin layer on the side walls of both sides of the deep trench to form two longitudinal PN junctions; specifically comprising: depositing the N+ type silicon thin layer in the area of ​​the deep trench; etching away the N+ type silicon thin layer on the surface of the substrate and the bottom of the deep trench to form an N+ layer area located on the side wall of the deep trench; depositing the P+ type silicon thin layer in the area of ​​the deep trench; etching away the P+ type silicon thin layer on the surface of the substrate and the bottom of the deep trench to form a P+ layer area located on the side of the N+ layer area; A first gate and a second gate are formed at two ends of the PN junction, respectively, and are located on the front side and the back side of the substrate; A P-type MOS region and two N-type MOS regions respectively located on both sides of the P-type MOS region are formed by ion implantation, and the two PN junctions are used to separate the P-type MOS region from the two N-type MOS regions, wherein the first gate is used to control the on or off of the N-type MOS region, and the second gate is used to control the on or off of the P-type MOS region; A front metal region is formed on the front side of the substrate, and a back metal region is disposed on the back side of the substrate.

7. The manufacturing method according to claim 6, characterized in that: After depositing an N+ type silicon thin layer and a P+ type silicon thin layer on the side walls of the deep trench to form two longitudinal PN junctions, the method specifically includes the following steps: Filling P-type silicon in the deep trench to form a super junction P-region; Ion implantation of trivalent elements on the front side of the substrate and thermal diffusion to form a P-well region; The first gate and the second gate are respectively formed on the front side and the back side of the substrate and are located at two ends of the PN junction; Ion implantation of pentavalent elements on the front and back sides of the substrate respectively and thermal diffusion to form a front shallow N+ region and a back shallow N+ region; Ion implantation of a trivalent element on the back side of the substrate and thermal diffusion to form a shallow P+ region on the back side; Ion implantation of a trivalent element into the front surface of the substrate and thermal diffusion to form a front deep P+ region; Ion implantation of pentavalent elements on the back side of the substrate and thermal diffusion to form a back side deep N+ region; Metal sputtering is performed on the front side and the back side of the substrate to form a front side metal region and a back side metal region respectively.

8. The manufacturing method according to claim 6, characterized in that: The first gate and the second gate located at both ends of the PN junction are formed on the front and back sides of the substrate respectively, specifically comprising: Etching grooves on the front side and the back side of the substrate to form a front side groove region and a back side groove region respectively; Thermally grow a front gate oxide layer and a back gate oxide layer in the front trench region and the back trench region, respectively; The front gate oxide layer and the back gate oxide layer are respectively filled with polysilicon to form a front polysilicon gate and a back polysilicon gate.