A mixed injection composition for carbon dioxide flooding and preparation method thereof
By using a mixed injection composition of sodium alginate, silicon-based cellulose and nanocomposites during the carbon dioxide flooding process, the problem of difficulty in controlling the fluidity of supercritical carbon dioxide in carbon dioxide flooding is solved, and the oil recovery rate and carbon dioxide sweep are improved. efficiency, enhancing the entry capability of the displacing fluid.
Patent Information
- Application Number
- CN202410977413.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2044-07-22
AI Technical Summary
In the process of carbon dioxide flooding, the low viscosity and fluidity of supercritical carbon dioxide make it difficult to control under complex formation conditions, leading to channeling phenomena and reducing oil recovery and carbon dioxide sweep efficiency.
A mixed injection composition is used, including sodium alginate, silicon-based cellulose and nanocomposites, and nanooxides are prepared through microwave, strong alkali etching and sol-gel methods to increase the specific surface area and active sites and reduce surface tension. Increase the viscosity and adsorption capacity, and improve the fluidity and wettability of the displacement fluid.
It improves the oil recovery rate and carbon dioxide sweep efficiency, reduces gas breakthrough and "fingering" phenomena, enhances the entry ability of the displacement fluid, and improves the sweep efficiency of the reservoir.
Smart Images

Figure CN118516099B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of carbon dioxide flooding, and in particular to a mixed injection composition for carbon dioxide flooding and a preparation method thereof. Background Art
[0002] As an important energy source, oil currently provides more than 40% of the total energy demand and more than 95% of vehicle fuel. However, the global total oil production is declining, but the energy demand is increasing year by year. In order to improve the oil and gas recovery rate and solve the increasingly serious contradiction between oil and gas supply and demand, the oil and gas production can be increased and unconventional oil and gas resources can be exploited by injecting high-pressure fluids. The most widely used are high-pressure water drive, steam drive and gas drive.
[0003] As a greenhouse gas, carbon dioxide is a non-polar molecule. Due to its low critical temperature and critical pressure, it has the characteristics of low viscosity, strong fluidity, and easy solubility in crude oil. It is easy to be miscible with crude oil. When injected into the formation, it can replenish the formation energy in time, play a role in reducing the viscosity of crude oil and improving the oil-water mobility ratio. Therefore, carbon dioxide flooding is widely used in the development of unconventional oil and gas resources such as coalbed methane reservoirs, shale gas reservoirs, heavy oil and super-heavy oil reservoirs, condensate gas reservoirs, low permeability reservoirs, carbonate reservoirs, complex fault block reservoirs, water-driven abandoned reservoirs and depleted gas reservoirs. It can not only improve the recovery rate, but also solve the problem of carbon dioxide storage, protect the atmospheric environment, and inhibit the greenhouse effect.
[0004] However, during the oil recovery process, supercritical carbon dioxide has a very low viscosity, close to that of gas, and flows well. It is difficult to control under complex formation conditions and is prone to crossflow, resulting in an unfavorable mobility ratio, reducing the carbon dioxide sweep efficiency and thus reducing the crude oil recovery rate.
[0005] In order to obtain a higher oil recovery rate, commonly used methods include increasing the viscosity of the displacement fluid, reducing the viscosity of the crude oil, reducing the interfacial tension between the displacement fluid and the crude oil, changing the wettability of the oil reservoir rock, etc. The patent application document with publication number CN103867169A discloses a method for controlling the mobility of carbon dioxide flooding using a gas-soluble surfactant, wherein the selected gas-soluble surfactant has a certain solubility in both water and supercritical carbon dioxide, and the carbon dioxide mobility is controlled by bubbling underground, thereby reducing the carbon dioxide mobility, increasing the carbon dioxide sweep efficiency, and improving the recovery rate. However, this method has high requirements for the surfactant used, and the solubility of supercritical carbon dioxide in the gas-soluble surfactant is limited, and the improvement of the carbon dioxide sweep efficiency is unclear. Summary of the invention
[0006] In order to solve the above-mentioned problems in carbon dioxide flooding and improve crude oil recovery, the present application provides a mixed injection composition for carbon dioxide flooding and a preparation method thereof.
[0007] A mixed injection composition for carbon dioxide flooding, comprising the following components in weight percentage: 0.3-0.5% sodium alginate, 1.2-1.5% silicon-based cellulose, 10-17% nanocomposite, and the balance water;
[0008] The method for preparing the nanocomposite comprises the following steps:
[0009] S1: Disperse polystyrene powder in methanol aqueous solution, heat to 50-60°C, add ammonia water, magnesium nitrate and aluminum nitrate, mix well and microwave for 2-3h, let the product stand and age for 18-24h, filter, wash, dry and calcine to obtain nanocomposite oxide;
[0010] S2: dispersing the above-mentioned nanocomposite oxide in a strong alkaline solution, stirring for 5-10 minutes, reacting at 90-105° C. for 6-24 hours, centrifuging, washing and drying the product to obtain a nano oxide;
[0011] S3: Disperse the above nano-oxide in an ethanol aqueous solution, add concentrated ammonia water and tetraethyl orthosilicate, stir and react for 8-15h, heat to 65-90°C, reflux for 2-6h, and dry to obtain.
[0012] In the above technical scheme, firstly, the aqueous solution of sodium alginate and silicon-based cellulose has a high viscosity, which can be used as a thickener for oil displacement fluid, reduce the flow velocity of the water phase in the reservoir, reduce the interference of the water phase on the flow of the oil phase, improve the fluidity of the oil phase, improve the permeability to the reservoir rock, change the surface wettability of the rock, reduce the interfacial tension between the oil displacement fluid and the crude oil, and thus improve the recovery rate of the crude oil; secondly, sodium alginate can react with metal ions in the formation, such as calcium ions, to form a gel, which is used to block the high permeability layer, and can also reduce gas breakthrough, thereby increasing the sweep efficiency of the oil reservoir and improving the recovery rate of crude oil; furthermore, silicon-based cellulose can adsorb and stabilize carbon dioxide molecules, so that the originally free carbon dioxide can participate more effectively in the oil displacement process, and at the same time can also reduce the mobility ratio of carbon dioxide to crude oil, reduce the "fingering" phenomenon of carbon dioxide, and improve the sweep efficiency of carbon dioxide, thereby improving the recovery rate of crude oil; in addition, silicon-based cellulose and sodium alginate have good biocompatibility and degradability, have little impact on the environment, and help to achieve green and sustainable oil field development.
[0013] During the preparation of the nanocomposite, a relatively stable nanocomposite oxide with a core-shell structure having polystyrene as a core and magnesium oxide and aluminum oxide as a shell is prepared by microwave action; the aluminum oxide in the polystyrene and shell is removed by high-temperature calcination and strong alkali corrosion to obtain a nano oxide with a large specific surface area, and the high content of magnesium oxide in the nano oxide can provide a large number of alkaline sites, which is conducive to the adsorption of carbon dioxide, greatly increasing the adsorption amount of carbon dioxide, thereby slowing down the phenomenon of carbon dioxide "fingering", improving the sweep efficiency of carbon dioxide, and further improving the recovery rate of crude oil; then, a silicon compound with low surface energy is loaded on the outside of the nano oxide by a sol-gel method, reducing the surface tension of the mixed injection composition used for carbon dioxide flooding, reducing the interfacial tension between the displacement fluid and the crude oil, making the displacement fluid easier to wet the rock surface and easier to enter the rock pores, thereby displacing the crude oil; moreover, the crude oil can also be emulsified and dispersed, reducing resistance, weakening the capillary end effect, enhancing the capillary self-imbibition phenomenon, and also facilitating the outflow of crude oil; in addition, after the nano oxide is loaded with silicon compounds, there are many surface active sites, which is more conducive to modification.
[0014] Preferably, in step S1, the mass ratio of the polystyrene powder, magnesium nitrate and aluminum nitrate is 1:(16-32):(5-12).
[0015] In the above technical solution, polystyrene is used as the core and magnesium oxide and aluminum oxide are used as the shell. In order to obtain a nano oxide with a stable structure and a large specific surface area, the amount of polystyrene powder, magnesium nitrate and aluminum nitrate added should be appropriate. If the amount of polystyrene powder added is too much and the amount of magnesium nitrate added is too little, after high-temperature calcination, polystyrene is removed, and the structure of the nano oxide may collapse, reducing the specific surface area; if the amount of polystyrene powder added is too little and the amount of magnesium nitrate added is too much, after high-temperature calcination, the specific surface area of the nano oxide will also decrease; if the amount of polystyrene powder and magnesium nitrate added is certain, when the amount of aluminum nitrate added is too much, after strong alkali corrosion, more and larger pores may be formed, which may easily cause the nano oxide structure to collapse and reduce the specific surface area; if the amount of aluminum nitrate added is too little, after strong alkali corrosion, the number of pores that may be formed is small, which will also reduce the specific surface area of the nano oxide.
[0016] Preferably, in step S3, the mass ratio of the nano-oxide to tetraethyl orthosilicate is 1:(10-25).
[0017] In the above technical solution, when the amount of nano-oxide added is certain, if the amount of tetraethyl orthosilicate added is too little, the surface tension of the obtained nano-composite is large, which is not conducive to rapid wetting of the rock, so the displacement fluid is not easy to quickly enter the rock pores to displace the crude oil. In addition, the number of active sites on the surface of the nano-oxide will also be reduced, which is not conducive to modification; if the amount of tetraethyl orthosilicate added is too much, it will not only increase the cost, but also may affect the adsorption performance of the nano-oxide for carbon dioxide, reduce the adsorption sites of the nano-oxide for carbon dioxide, which is not conducive to reducing the mobility of carbon dioxide, and will reduce the sweep efficiency of carbon dioxide, thereby reducing the recovery rate of crude oil.
[0018] Preferably, the nanocomposite is modified by a method comprising the following steps:
[0019] 1) Disperse the nanocomposite in water, add the diamine compound, stir and react for 8-16 hours, then add the dihalogenated hydrocarbon, heat to 80-95°C, react for 2-4 hours, and dry to obtain a quaternary ammonium salt mixture;
[0020] 2) Disperse the above quaternary ammonium salt mixture in water, add anionic surfactant, stir at 60-80°C for 12-24h, and dry the product.
[0021] In the above technical scheme, first, a diamine compound containing a tertiary amine group is grafted onto the nanocomposite, and the diamine compound reacts with a dihalogenated hydrocarbon to generate a quaternary ammonium salt with a positive charge, which not only plays the role of a surfactant, but the positive charge is also beneficial to the adsorption of carbon dioxide, increases the viscosity of carbon dioxide, reduces the "fingering" phenomenon, and increases the contact rate between carbon dioxide and crude oil, thereby improving the sweep efficiency of carbon dioxide and improving the recovery rate of crude oil; then, an anionic surfactant is added to the quaternary ammonium salt mixture, and the positively charged quaternary ammonium salt and the anionic surfactant interact with each other through strong cation-anion interactions, so that the nanocomposite has good fluidity, which is beneficial to synergize with carbon dioxide and improve the recovery rate of crude oil.
[0022] Preferably, in step 1), the mass ratio of the nanocomposite, the diamine compound and the dihalogenated hydrocarbon is 1:(0.2-0.6):(0.4-1).
[0023] In the above technical scheme, a diamine compound is first grafted on the surface of the nanocomposite. If the amount of the diamine compound added is too much, part of the diamine compound cannot be grafted to the surface of the nanocomposite. If the amount of the diamine compound added is too little, the grafting amount is correspondingly reduced, and the positive charge of the formed quaternary ammonium salt is reduced, and the adsorption effect on carbon dioxide is weakened; if the amount of the dihalogenated hydrocarbon added is too little, part of the grafted diamine compound cannot form a quaternary ammonium salt with a positive charge. If the amount of the dihalogenated hydrocarbon added is too much, part of the dihalogenated hydrocarbon cannot participate in the reaction to form a quaternary ammonium salt. Therefore, the mass ratio of the nanocomposite, the diamine compound and the dihalogenated hydrocarbon should be controlled within an appropriate range.
[0024] Preferably, in step 2), the anionic surfactant is one of sodium dodecyl sulfonate, sodium hexadecyl sulfonate and sodium octadecyl sulfonate.
[0025] By adopting the above technical scheme, firstly, the anionic surfactant can interact with the positively charged quaternary ammonium salt through cation-anion interaction, so that the nanocomposite has good fluidity, which is beneficial to cooperate with carbon dioxide and improve the recovery rate of crude oil; secondly, the introduction of sulfonate groups is beneficial to improve the acid resistance, salt resistance and temperature resistance of the mixed injection composition used for carbon dioxide flooding, making it easier to adapt to the formation environment; in addition, the fatty chain of the anionic surfactant is beneficial to displacing a wider range of crude oil, thereby improving the recovery rate of crude oil.
[0026] Preferably, in step 2), the mass ratio of the quaternary ammonium salt mixture to the anionic surfactant is 1:(2.3-4.2).
[0027] In the above technical solution, when the amount of the quaternary ammonium salt mixture added is certain, if the amount of the anionic surfactant added is too small, the interaction between the positive and negative charges will be weakened, which may affect the fluidity of the mixed injection composition used for carbon dioxide flooding, and further affect the displacement effect and crude oil recovery rate; if too much anionic surfactant is added, some of the anionic surfactant may be in a free state, which may also affect the oil displacement effect of the mixed injection composition used for carbon dioxide flooding.
[0028] A method for preparing a mixed injection composition for carbon dioxide flooding comprises the following steps:
[0029] Sodium alginate, silicon-based cellulose, nanocomposite and water are weighed according to the formula, and mixed evenly to obtain the product.
[0030] In the above technical scheme, after the mixed injection composition for carbon dioxide flooding and carbon dioxide act synergistically on the oil-bearing formation, the mixed injection composition for carbon dioxide flooding and carbon dioxide together form a displacement fluid to displace the crude oil in the formation. On the one hand, the mixed injection composition for carbon dioxide flooding has good fluidity and low surface energy, which can reduce the interfacial tension with crude oil, which is conducive to the mixed injection composition for carbon dioxide flooding and carbon dioxide entering the rock pores and squeezing out the crude oil; on the other hand, the mixed injection composition for carbon dioxide flooding has a large specific surface area and active sites that are conducive to the adsorption of carbon dioxide, which can adsorb a part of carbon dioxide, reduce the mobility of carbon dioxide, and improve the sweep efficiency of carbon dioxide, thereby improving the recovery rate of crude oil; on the third hand, the mixed injection composition for carbon dioxide flooding has a certain viscosity, which can reduce the mobility of the water phase in the oil reservoir, reduce the interference of the water phase on the oil phase, and improve the mobility of the oil phase, thereby improving the recovery rate of crude oil.
[0031] The above technical solution of the present application includes at least the following beneficial effects:
[0032] 1. The carrier of the nanocomposite in the present application is a nanomaterial with a small particle size and a large specific surface area, which is easier to enter the ultra-low permeability matrix and has many alkaline sites, which is conducive to the adsorption of carbon dioxide; in addition, the silicon compound with low surface energy in the nanocomposite can reduce the surface tension of the mixed injection composition used for carbon dioxide flooding; and the hydrophilic groups on the surface make it easier to wet the rock, enter the rock pores, and displace the crude oil;
[0033] 2. In the present application, the nanocomposite is modified by grafting a quaternary ammonium salt with a positive charge on the surface of the nanocomposite. The positive charge is conducive to the adsorption of carbon dioxide, increasing the viscosity of carbon dioxide, and increasing the sweep efficiency of carbon dioxide, thereby improving the oil recovery rate; and, through the interaction of positive and negative charges, anionic surfactants are adsorbed on the surface of the nanocomposite to improve the fluidity of the nanocomposite, thereby enhancing the synergistic effect with carbon dioxide and improving the oil recovery rate;
[0034] 3. In the present application, sodium alginate and silicon-based cellulose can increase the viscosity of the mixed injection composition used for carbon dioxide flooding, reduce the mobility of the water phase in the oil reservoir, reduce the interference of the water phase with the oil phase, and improve the fluidity of the oil phase. It can also improve the adsorption of carbon dioxide, improve the mobility ratio of the displacement fluid to crude oil, and increase the sweep efficiency of carbon dioxide, thereby increasing the recovery rate of crude oil; in addition, it can also play a plugging role in the high permeability layer section in the oil reservoir, reduce gas breakthrough and "fingering" phenomenon, and improve the recovery rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 It is a graph showing the changing trend of the interfacial tension between the displacement fluid and crude oil.
[0036] Figure 2 It is a changing trend chart of crude oil recovery rate. DETAILED DESCRIPTION
[0037] The present application is further described in detail below with reference to the embodiments.
[0038] Unless otherwise specified, the raw materials used in the examples and comparative examples of the present application are all commercially available.
[0039] Example
[0040] Example 1
[0041] The mixed injection composition for carbon dioxide flooding in this embodiment comprises the following components in weight percentage: 0.3% sodium alginate, 1.2% silicon-based cellulose, 10% nanocomposite, and the balance is water;
[0042] The method for preparing the nanocomposite in this embodiment comprises the following steps:
[0043] S1: Weigh 1 g of polystyrene powder, 100 mL of methanol and 50 mL of deionized water, place in a flask, ultrasonically disperse for 0.5 h, heat to 50 ° C, add 80 mL of 30% ammonia water, 16 g of magnesium nitrate and 5 g of aluminum nitrate, mix and stir evenly, and microwave for 3 h. Let the product stand and age for 24 h, filter, wash and dry, and then calcine in a muffle furnace at 550 ° C for 3 h to obtain a nanocomposite oxide;
[0044] S2: Disperse the above nanocomposite oxide in a sodium hydroxide solution with a concentration of 3 mol / L, stir for 5 min, transfer to a reactor, react at 90°C for 24 h, and after the reaction, centrifuge the product, wash it with distilled water and anhydrous ethanol alternately for several times until it is neutral, and dry it at 80°C for 2 h to obtain nano oxide;
[0045] S3: Weigh 2 g of the above nano oxide, 50 mL of ethanol, 50 mL of deionized water and 5 mL of concentrated ammonia water, place in a three-necked flask, ultrasonically disperse for 2 h, add 20 g of tetraethyl orthosilicate, continue stirring and reacting for 8 h, heat to 65 ° C, reflux for 6 h, and dry to obtain;
[0046] The method for preparing the mixed injection composition for carbon dioxide flooding in this embodiment comprises the following steps:
[0047] According to the formula, 0.3 g of sodium alginate, 1.2 g of silicon-based cellulose, 10 g of nanocomposite and 88.5 g of deionized water were weighed, and mixed and stirred evenly to obtain the product.
[0048] Example 2
[0049] The mixed injection composition for carbon dioxide flooding in this embodiment comprises the following components in weight percentage: 0.5% sodium alginate, 1.5% silicon-based cellulose, 17% nanocomposite, and the balance is water;
[0050] The method for preparing the nanocomposite in this embodiment comprises the following steps:
[0051] S1: Weigh 1 g of polystyrene powder, 100 mL of methanol and 50 mL of deionized water, place in a flask, ultrasonically disperse for 0.5 h, heat to 60 ° C, add 80 mL of 30% ammonia water, 16 g of magnesium nitrate and 5 g of aluminum nitrate, mix and stir evenly, and microwave for 2 h. Let the product stand and age for 24 h, filter, wash and dry, and then calcine in a muffle furnace at 550 ° C for 3 h to obtain a nanocomposite oxide;
[0052] S2: Disperse the above nanocomposite oxide in a potassium hydroxide solution with a concentration of 3 mol / L, stir for 10 min, transfer to a reactor, react at 105°C for 6 h, and after the reaction, centrifuge the product, wash it with distilled water and anhydrous ethanol alternately for several times until it is neutral, and dry it at 80°C for 2 h to obtain nano oxide;
[0053] S3: Weigh 2 g of the above nano oxide, 50 mL of ethanol, 50 mL of deionized water and 5 mL of concentrated ammonia water, place in a three-necked flask, ultrasonically disperse for 2 h, add 20 g of tetraethyl orthosilicate, continue stirring and reacting for 15 h, heat to 90 ° C, reflux for 2 h, and dry to obtain;
[0054] The method for preparing the mixed injection composition for carbon dioxide flooding in this embodiment comprises the following steps:
[0055] According to the formula, 0.5 g of sodium alginate, 1.5 g of silicon-based cellulose, 17 g of nanocomposite and 81 g of deionized water were weighed, and mixed and stirred evenly to obtain the product.
[0056] Example 3
[0057] The mixed injection composition for carbon dioxide flooding in this embodiment comprises the following components in weight percentage: 0.5% sodium alginate, 1.5% silicon-based cellulose, 15% nanocomposite, and the balance is water;
[0058] The method for preparing the nanocomposite in this embodiment comprises the following steps:
[0059] S1: Weigh 1 g of polystyrene powder, 100 mL of methanol and 50 mL of deionized water, place in a flask, ultrasonically disperse for 0.5 h, heat to 60 ° C, add 80 mL of 30% ammonia water, 16 g of magnesium nitrate and 5 g of aluminum nitrate, mix and stir evenly, and microwave for 3 h. Let the product stand and age for 18 h, filter, wash and dry, and then calcine in a muffle furnace at 550 ° C for 3 h to obtain a nanocomposite oxide;
[0060] S2: Disperse the above nanocomposite oxide in a potassium hydroxide solution with a concentration of 3 mol / L, transfer to a reactor after stirring for 10 min, react at 95°C for 12 h, and after the reaction, centrifuge the product, wash it with distilled water and anhydrous ethanol alternately for several times until it is neutral, and dry it at 80°C for 2 h to obtain nano oxide;
[0061] S3: Weigh 2 g of the above nano oxide, 50 mL of ethanol, 50 mL of deionized water and 5 mL of concentrated ammonia water, place in a three-necked flask, ultrasonically disperse for 2 h, add 20 g of tetraethyl orthosilicate, continue stirring and reacting for 12 h, heat to 80 ° C, reflux for 4 h, and dry to obtain;
[0062] The method for preparing the mixed injection composition for carbon dioxide flooding in this embodiment comprises the following steps:
[0063] According to the formula, 0.5 g of sodium alginate, 1.5 g of silicon-based cellulose, 15 g of nanocomposite and 83 g of deionized water were weighed, and mixed and stirred evenly to obtain the product.
[0064] Example 4
[0065] The weight percentage components of the mixed injection composition used for carbon dioxide flooding in this embodiment are the same as those in Example 3;
[0066] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 3 in that:
[0067] S1: Weigh 1 g of polystyrene powder, 100 mL of methanol and 50 mL of deionized water, place in a flask, ultrasonically disperse for 0.5 h, heat to 60 ° C, add 80 mL of 30% ammonia water, 32 g of magnesium nitrate and 12 g of aluminum nitrate, mix and stir evenly, and microwave for 3 h. Let the product stand and age for 18 h. After filtration, washing and drying, place in a muffle furnace at 550 ° C and calcine for 3 h to obtain a nanocomposite oxide;
[0068] The remaining steps are the same as those in Example 3;
[0069] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 3.
[0070] Example 5
[0071] The weight percentage components of the mixed injection composition used for carbon dioxide flooding in this embodiment are the same as those in Example 3;
[0072] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 3 in that:
[0073] S1: Weigh 1 g of polystyrene powder, 100 mL of methanol and 50 mL of deionized water, place in a flask, ultrasonically disperse for 0.5 h, heat to 60 ° C, add 80 mL of 30% ammonia water, 25 g of magnesium nitrate and 8 g of aluminum nitrate, mix and stir evenly, and microwave for 3 h. Let the product stand and age for 18 h. After filtration, washing and drying, place in a muffle furnace at 550 ° C and calcine for 3 h to obtain a nanocomposite oxide;
[0074] The remaining steps are the same as those in Example 3;
[0075] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 3.
[0076] Example 6
[0077] The weight percentage components of the mixed injection composition used for carbon dioxide flooding in this embodiment are the same as those in Example 5;
[0078] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 5 in that:
[0079] S3: Weigh 2 g of the above nano oxide, 50 mL of ethanol, 50 mL of deionized water and 5 mL of concentrated ammonia water, place in a three-necked flask, ultrasonically disperse for 2 h, add 50 g of tetraethyl orthosilicate, continue stirring and reacting for 12 h, heat to 80 ° C, reflux for 4 h, and dry to obtain;
[0080] The remaining steps are the same as those in Example 5;
[0081] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 5.
[0082] Example 7
[0083] The weight percentage components of the mixed injection composition used for carbon dioxide flooding in this embodiment are the same as those in Example 5;
[0084] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 5 in that:
[0085] S3: Weigh 2 g of the above nano oxide, 50 mL of ethanol, 50 mL of deionized water and 5 mL of concentrated ammonia water, place in a three-necked flask, ultrasonically disperse for 2 h, add 38 g of tetraethyl orthosilicate, continue stirring and reacting for 12 h, heat to 80 ° C, reflux for 4 h, and dry to obtain;
[0086] The remaining steps are the same as those in Example 5;
[0087] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 5.
[0088] Example 8
[0089] The weight percentage components of the mixed injection composition used for carbon dioxide flooding in this embodiment are the same as those in Example 7;
[0090] The method for preparing the nanocomposite in this embodiment comprises the following steps:
[0091] S1: Weigh 1 g of polystyrene powder, 100 mL of methanol and 50 mL of deionized water, place in a flask, ultrasonically disperse for 0.5 h, heat to 60 ° C, add 80 mL of 30% ammonia water, 25 g of magnesium nitrate and 8 g of aluminum nitrate, mix and stir evenly, and microwave for 3 h. Let the product stand and age for 18 h. After filtration, washing and drying, place in a muffle furnace at 550 ° C and calcine for 3 h to obtain a nanocomposite oxide;
[0092] S2: Disperse the above nanocomposite oxide in a potassium hydroxide solution with a concentration of 3 mol / L, transfer to a reactor after stirring for 10 min, react at 95°C for 12 h, and after the reaction, centrifuge the product, wash it with distilled water and anhydrous ethanol alternately for several times until it is neutral, and dry it at 80°C for 2 h to obtain nano oxide;
[0093] S3: Weigh 2 g of the above nano oxide, 50 mL of ethanol, 50 mL of deionized water and 5 mL of concentrated ammonia water, place in a three-necked flask, ultrasonically disperse for 2 h, add 38 g of tetraethyl orthosilicate, continue stirring and reacting for 12 h, heat to 80 ° C, reflux for 4 h, and dry to obtain modified nano oxide;
[0094] S4: Weigh 5 g of the modified nano-oxide and 200 mL of deionized water, place in a three-necked flask, ultrasonically disperse for 2 h, add 1 g of N,N-dimethyl-1,4-butanediamine, stir and react for 8 h, then add 2 g of 1,4-dibromobutane, heat to 80°C, react for 4 h, and dry to obtain a quaternary ammonium salt mixture;
[0095] S5: Weigh 10 g of the above quaternary ammonium salt mixture and 300 mL of deionized water, put them in a flask, mix them evenly, add 23 g of sodium octadecyl sulfonate, stir at 60° C. for 24 h, and dry the product to obtain;
[0096] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 7.
[0097] Example 9
[0098] The weight percentage components of the mixed injection composition used for carbon dioxide flooding in this embodiment are the same as those in Example 8;
[0099] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 8 in that:
[0100] S4: Weigh 5 g of the modified nano-oxide and 200 mL of deionized water, place in a three-necked flask, ultrasonically disperse for 2 h, add 3 g of N,N-dimethylethylenediamine, stir and react for 16 h, then add 5 g of 1,3-dichloropropane, heat to 95°C, react for 2 h, and dry to obtain a quaternary ammonium salt mixture;
[0101] S5: Weigh 10 g of the above quaternary ammonium salt mixture and 300 mL of deionized water, put them in a flask, mix them evenly, add 23 g of sodium octadecyl sulfonate, stir at 80° C. for 12 h, and dry the product to obtain;
[0102] The remaining steps are the same as those in Example 8;
[0103] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 8.
[0104] Example 10
[0105] The weight percentage components of the mixed injection composition used for carbon dioxide flooding in this embodiment are the same as those in Example 8;
[0106] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 8 in that:
[0107] S4: Weigh 5 g of the modified nano-oxide and 200 mL of deionized water, place in a three-necked flask, ultrasonically disperse for 2 h, add 2 g of N,N-dimethyl-1,3-propylenediamine, stir and react for 16 h, then add 3 g of 1,3-dibromopropane, heat to 90°C, react for 3 h, and dry to obtain a quaternary ammonium salt mixture;
[0108] S5: Weigh 10 g of the above quaternary ammonium salt mixture and 300 mL of deionized water, put them in a flask, mix them evenly, add 23 g of sodium octadecyl sulfonate, stir at 70° C. for 15 h, and dry the product to obtain;
[0109] The remaining steps are the same as those in Example 8;
[0110] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 8.
[0111] Embodiment 11
[0112] The weight percentage components of the mixed injection composition for carbon dioxide flooding in this embodiment are the same as those in Example 10;
[0113] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 10 in that:
[0114] S5: Weigh 10 g of the above quaternary ammonium salt mixture and 300 mL of deionized water, put them in a flask, mix them evenly, add 42 g of sodium dodecyl sulfate, stir at 70° C. for 15 h, and dry the product to obtain;
[0115] The remaining steps are the same as those in Example 10;
[0116] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 10.
[0117] Example 12
[0118] The weight percentage components of the mixed injection composition for carbon dioxide flooding in this embodiment are the same as those in Example 10;
[0119] The preparation method of the nanocomposite in this embodiment is different from that in Embodiment 10 in that:
[0120] S5: Weigh 10 g of the above quaternary ammonium salt mixture and 300 mL of deionized water, put them in a flask, mix them evenly, add 34 g of sodium hexadecyl sulfonate, stir at 70° C. for 15 h, and dry the product to obtain;
[0121] The remaining steps are the same as those in Example 10;
[0122] The preparation method of the mixed injection composition for carbon dioxide flooding in this example is the same as that in Example 10.
[0123] Comparative Example
[0124] Comparative Example 1
[0125] The mixed injection composition for carbon dioxide flooding in this comparative example comprises the following components in weight percentage: 0.3% sodium alginate, 1.2% silicon-based cellulose, and the balance water;
[0126] The preparation method of the mixed injection composition for carbon dioxide flooding in this comparative example comprises the following steps:
[0127] According to the formula, weigh 0.3 g of sodium alginate, 1.2 g of silicon-based cellulose and 98.5 g of deionized water, mix and stir evenly to obtain the product.
[0128] Comparative Example 2
[0129] The mixed injection composition for carbon dioxide flooding in this comparative example comprises the following components in weight percentage: 0.3% sodium alginate, 1.2% silicon-based cellulose, 10% sodium hexadecyl sulfate, and the balance is water;
[0130] A method for preparing a mixed injection composition for carbon dioxide flooding comprises the following steps:
[0131] According to the formula, 0.3 g of sodium alginate, 1.2 g of silicon-based cellulose, 10 g of sodium hexadecyl sulfate and 88.5 g of deionized water were weighed, and mixed and stirred evenly to obtain the product.
[0132] Performance testing
[0133] Detection method:
[0134] 1. Interfacial tension test with crude oil
[0135] The interfacial tension between the displacement fluid and crude oil in a block of Daqing Oilfield at 25 MPa was measured using a supercritical carbon dioxide interfacial tension meter when pure carbon dioxide was used as the displacement fluid and the mixed injection composition for carbon dioxide flooding of Examples 1-12 and Comparative Examples 1-2 was used in conjunction with carbon dioxide as the displacement fluid. The measurement results are shown in the attached Figure 1 The properties of crude oil in a block of Daqing Oilfield are shown in Table 1 below:
[0136] Table 1 Crude oil properties in a block of Daqing Oilfield
[0137]
[0138] 2. Crude oil recovery rate test
[0139] The capillary displacement experiment supporting device was used to measure the crude oil recovery factor at 76°C and 25MPa. The specific test method is as follows:
[0140] ① Take crude oil samples from a block in Daqing Oilfield, prepare formation oil according to the high-pressure physical property parameters of formation oil, and measure its high-pressure physical property parameters;
[0141] ② Heat the capillary tube to a constant temperature and then evacuate it. Use a constant pressure pump to press the crude oil sample into the capillary tube model. Stop the pump when the pump reaches 2PV and record the volume of crude oil injected into the coil.
[0142] ③ Raise the pressure to above the saturation pressure, and displace at a constant speed of 0.45mL / min. When the oil and gas section appears at the outlet, start testing the oil-gas ratio. When the calculated oil-gas ratio is 38.1m³ / t, the saturated live oil is completed, and the outlet of the live oil kettle is closed;
[0143] ④ Inject the mixed injection composition for carbon dioxide flooding of Example 1-12 and Comparative Example 1-2 with a crude oil mass fraction of 1% in the form of a slug. After the injection is completed, carbon dioxide is used to displace at a constant rate of 0.25 mL / min. The oil production, gas production, etc. are recorded every 0.1 PV. When the displacement reaches 1.2 PV, the experiment is stopped;
[0144] ⑤ A control group was set up, that is, only carbon dioxide was used for displacement at a constant rate of 0.25 mL / min, and the oil production, gas production, etc. were recorded every 0.1 PV. When the displacement reached 1.2 PV, the experiment was stopped, and the mixed injection composition for carbon dioxide flooding of Example 1-12 and Comparative Example 1-2 with a crude oil mass fraction of 1% was not injected in the form of a slug;
[0145] The test results of crude oil recovery are attached. Figure 2 .
[0146] Results Analysis
[0147] By comparison Figure 1 and Figure 2 It can be seen from the data of Comparative Examples 1-2 and Examples 1-3 and the observed experimental phenomena that the mixed injection composition for carbon dioxide flooding and carbon dioxide synergistically flooding oil can greatly improve the crude oil recovery rate, and can effectively improve the "fingering" phenomenon of carbon dioxide during displacement, improve the sweep efficiency, and thus improve the crude oil recovery rate; moreover, the mixed injection composition for carbon dioxide flooding can reduce the interfacial tension between the displacement fluid and the crude oil to a certain extent, improve the wetting effect, and improve the crude oil recovery rate.
[0148] By comparison Figure 1 and Figure 2 It can be seen from the data of Examples 3-5 that when the magnesium oxide content in the nanocomposite is increased, it is beneficial to improve the oil recovery rate. This may be because magnesium oxide can provide more alkaline sites, which is beneficial to the adsorption of carbon dioxide and improves the sweep efficiency of the displacement fluid, thereby improving the oil recovery rate.
[0149] By comparison Figure 1 and Figure 2 It can be seen from the data of Examples 5-7 that the low surface energy substances in the nanocomposite and the hydrophilic groups on the surface are beneficial to improving the oil recovery rate. This may be because the reduced surface tension of the nanocomposite and the hydrophilic groups are beneficial to driving fluid into the core pores and displacing the crude oil.
[0150] By comparison Figure 1 and Figure 2 It can be seen from the data of Examples 7-12 that the interaction between the positive charges and the negative charges in the nanocomposite is beneficial to reducing the interfacial tension between the displacement fluid and the crude oil and improving the crude oil recovery rate.
[0151] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.
Claims
1. A mixed injection composition for carbon dioxide flooding, characterized in that: The composition comprises the following components in weight percentage: 0.3-0.5% sodium alginate, 1.2-1.5% silicon-based cellulose, 10-17% nanocomposite, and the balance is water; The method for preparing the nanocomposite comprises the following steps: S1: Disperse polystyrene powder in methanol aqueous solution, heat to 50-60°C, add ammonia water, magnesium nitrate and aluminum nitrate, mix well and microwave for 2-3h, let the product stand and age for 18-24h, filter, wash, dry and calcine to obtain nanocomposite oxide; S2: dispersing the above-mentioned nanocomposite oxide in a strong alkaline solution, stirring for 5-10 minutes, reacting at 90-105° C. for 6-24 hours, centrifuging, washing and drying the product to obtain a nano oxide; S3: Disperse the above nano-oxide in an ethanol aqueous solution, add concentrated ammonia water and tetraethyl orthosilicate, stir and react for 8-15h, heat to 65-90°C, reflux for 2-6h, and dry to obtain.
2. The mixed injection composition for carbon dioxide flooding according to claim 1, characterized in that: In step S1, the mass ratio of the polystyrene powder, magnesium nitrate and aluminum nitrate is 1:(16-32):(5-12).
3. The mixed injection composition for carbon dioxide flooding according to claim 1, characterized in that: In step S2, the strong alkaline solution is a 3 mol / L sodium hydroxide solution or a 3 mol / L potassium hydroxide solution.
4. The mixed injection composition for carbon dioxide flooding according to claim 1, characterized in that: In step S3, the mass ratio of the nano-oxide to tetraethyl orthosilicate is 1:(10-25).
5. The mixed injection composition for carbon dioxide flooding according to claim 1, characterized in that: The nanocomposite is modified by a method comprising the following steps: 1) Disperse the nanocomposite in water, add the diamine compound, stir and react for 8-16 hours, then add the dihalogenated hydrocarbon, heat to 80-95°C, react for 2-4 hours, and dry to obtain a quaternary ammonium salt mixture; 2) Disperse the above quaternary ammonium salt mixture in water, add anionic surfactant, stir at 60-80°C for 12-24h, and dry the product.
6. The mixed injection composition for carbon dioxide flooding according to claim 5, characterized in that: In step 1), the diamine compound is one of N,N-dimethylethylenediamine, N,N-dimethyl-1,3-propylenediamine and N,N-dimethyl-1,4-butanediamine; the dihalogenated hydrocarbon is one of 1,3-dibromopropane, 1,3-dichloropropane and 1,4-dibromobutane.
7. The mixed injection composition for carbon dioxide flooding according to claim 5, characterized in that: In step 1), the mass ratio of the nanocomposite, the diamine compound and the dihalogenated hydrocarbon is 1:(0.2-0.6):(0.4-1).
8. The mixed injection composition for carbon dioxide flooding according to claim 5, characterized in that: In step 2), the anionic surfactant is one of sodium dodecyl sulfonate, sodium hexadecyl sulfonate and sodium octadecyl sulfonate.
9. The mixed injection composition for carbon dioxide flooding according to claim 5, characterized in that: In step 2), the mass ratio of the quaternary ammonium salt mixture to the anionic surfactant is 1:(2.3-4.2).
10. A method for preparing a mixed injection composition for carbon dioxide flooding according to any one of claims 1 to 9, characterized in that: The steps include: Sodium alginate, silicon-based cellulose, nanocomposite and water are weighed according to the formula, and mixed evenly to obtain the product.
Citation Information
Patent Citations
Method for applying gas-soluble surfactant to fluidity control of carbon dioxide oil displacement
CN103867169A
Nano-composite capable of preventing CO2 channeling for tight reservoir and preparation method of nano-composite
CN107353886A
Thixotropic reinforced foam system and preparation method thereof
CN114381253A