Shale gas adsorption measurement method, device, system and readable storage medium

By using a dual-temperature zone environment in the shale gas adsorption experiment, recording the data of gas diffusion and adsorption from the low-temperature zone to the high-temperature zone, and combining pressure and temperature changes to calculate the amount of natural gas adsorbed by shale under high temperature, solving the problem of existing technology It solves the problem of upper limit of measurement temperature and improves measurement accuracy and equipment reusability.

CN118518533BActive Publication Date: 2024-10-18CHINA UNIV OF GEOSCIENCES (WUHAN)
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410826812.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-25
Publication Date
2024-10-18
Estimated Expiration
2044-06-25

AI Technical Summary

Technical Problem

In the existing technology, the maximum measurement temperature set in shale gas adsorption experiments cannot meet the deep high-temperature environment of underground reservoirs, resulting in the inability to clearly provide measurement result data suitable for the upper limit of temperature measurement.

Method used

A dual-temperature zone environment was used to conduct shale sample gas adsorption experiments. Through the diffusion of gas from the low-temperature zone to the high-temperature zone and adsorption on the rocks, combined with the pressure changes during the gas diffusion and adsorption process and the changes in the gas compression factor caused by the temperature difference in the dual-temperature zones, the calculation The amount of natural gas adsorbed by shale at high temperatures.

Benefits of technology

It improves the accuracy of adsorbed gas volume measurement results under deep high-temperature conditions, overcomes the shortcomings of traditional volumetric methods that cannot maintain high accuracy in high-temperature environments of 100°C and above, and protects high-precision instruments to ensure the reusability of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118518533B_ABST
    Figure CN118518533B_ABST
Patent Text Reader

Abstract

The present application discloses a shale gas adsorption measurement method, device, system and readable storage medium. The method of the present application controls the temperature in the first chamber according to a first preset temperature value, and controls the temperature in the second chamber according to a second preset temperature value; performs a preset number of adsorption control actions, obtains the amount of natural gas in the shale gas adsorption measurement system before the shale sample adsorbs natural gas corresponding to each adsorption control action, and the amount of natural gas in the shale gas adsorption measurement system after the shale sample adsorbs natural gas; according to the amount of natural gas before adsorption and the amount of natural gas after adsorption corresponding to each adsorption control action, determines the gas adsorption amount of the shale sample corresponding to each adsorption control action. It can restore the gas adsorption process of deep shale under long-term high temperature state, improve the accuracy of the adsorbed gas measurement results, and control the chamber where the high-precision instrument is located to maintain low temperature to protect the components.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of unconventional natural gas development, and in particular to a shale gas adsorption measurement method, device, system and readable storage medium. Background Art

[0002] Shale gas is a hot spot for unconventional natural gas development in my country. Shale gas adsorption experiments and the acquisition of adsorption characteristic parameters are important links and means for shale gas resource evaluation and production capacity prediction. In the prior art, the reference cylinder and the sample cylinder in the shale gas adsorption experiment are in the same temperature system. In order to avoid the pressure sensor that monitors the pressure of the reference cylinder or the sample cylinder from being exposed to high temperature for a long time, which may cause thermal aging of the internal structure of the pressure sensor, the maximum measurement temperature set in the experiment usually cannot meet the deep high temperature environment of the underground reservoir, and thus it is impossible to clearly give the measurement result data that can be used for the upper limit of temperature measurement. Summary of the invention

[0003] In view of this, the present application provides a shale gas adsorption measurement method, device, system and readable storage medium, the main purpose of which is to solve the technical problem that the highest measurement temperature of the experimental setting in the prior art is usually unable to meet the deep high temperature environment of the underground reservoir, and thus cannot clearly give measurement result data that can be used for the upper limit of temperature measurement.

[0004] According to the first aspect of the present application, a shale gas adsorption measurement method is provided, which is applicable to a shale gas adsorption measurement system. The shale gas adsorption measurement system includes a first chamber, a second chamber, a reference cylinder and a sample cylinder, wherein the reference cylinder is arranged in the first chamber, the sample cylinder is arranged in the second chamber, and a shale sample is placed in the sample cylinder. The method includes:

[0005] Controlling the temperature in the first chamber according to a first preset temperature value, and controlling the temperature in the second chamber according to a second preset temperature value, wherein the first preset temperature value is less than the second preset temperature value;

[0006] Execute a preset number of adsorption control actions to obtain a first mass and a second mass corresponding to each adsorption control action; the adsorption control action includes: introducing natural gas into a reference cylinder according to a preset pressure value, and controlling the natural gas in the reference cylinder to diffuse into the sample cylinder, so that the natural gas is adsorbed into the pore space of the shale sample; the first mass is the mass of the natural gas in the shale gas adsorption measurement system before the shale sample adsorbs the natural gas, and the second mass is the mass of the natural gas in the shale gas adsorption measurement system after the shale sample adsorbs the natural gas;

[0007] The gas adsorption amount of the shale sample corresponding to each adsorption control action is determined according to the first mass of substance and the second mass of substance corresponding to each adsorption control action.

[0008] According to the second aspect of the present application, a shale gas adsorption measurement device is provided, which is applicable to a shale gas adsorption measurement system. The shale gas adsorption measurement system includes a first chamber, a second chamber, a reference cylinder and a sample cylinder, wherein the reference cylinder is arranged in the first chamber, the sample cylinder is arranged in the second chamber, and a shale sample is placed in the sample cylinder. The device includes:

[0009] A control module, used to control the temperature in the first chamber according to a first preset temperature value, and to control the temperature in the second chamber according to a second preset temperature value, wherein the first preset temperature value is less than the second preset temperature value;

[0010] The acquisition module is used to execute a preset number of adsorption control actions to obtain a first mass amount and a second mass amount corresponding to each adsorption control action; the adsorption control action includes: introducing natural gas into a reference cylinder according to a preset pressure value, and controlling the natural gas in the reference cylinder to diffuse into the sample cylinder so that the natural gas is adsorbed into the pore space of the shale sample; the first mass amount is the amount of natural gas in the shale gas adsorption measurement system before the shale sample adsorbs natural gas, and the second mass amount is the amount of natural gas in the shale gas adsorption measurement system after the shale sample adsorbs natural gas; the determination module is used to determine the gas adsorption amount of the shale sample corresponding to each adsorption control action according to the first mass amount and the second mass amount corresponding to each adsorption control action.

[0011] According to the third aspect of the present application, a shale gas adsorption measurement system is provided, comprising: a first chamber; a second chamber; a reference cylinder, arranged in the first chamber, the reference cylinder comprising a first air inlet and an air outlet; a sample cylinder, arranged in the second chamber, the sample cylinder comprising a second air inlet, and the second air inlet is connected to the air outlet of the reference cylinder; a pressure sensor, arranged in the first chamber, the pressure sensor is used to detect the pressure value of the shale gas adsorption measurement system; a memory, the memory storing a program or instruction; a processor, connected to the memory, and the shale gas adsorption measurement method of the first aspect is implemented when the processor executes the program or instruction.

[0012] Optionally, the system also includes: a vacuum pumping component, which is used to vacuum the shale gas adsorption measurement system, and the vacuum pumping component includes a vacuum end, which is connected to the first air inlet of the reference cylinder; an inert gas source, which is used to introduce inert gas into the reference cylinder and the sample cylinder, and the inert gas source includes a first air outlet, which is connected to the first air inlet of the reference cylinder; a natural gas source, which is used to introduce natural gas into the reference cylinder and the sample cylinder, and the natural gas source includes a second air outlet, which is connected to the first air inlet of the reference cylinder; a first pipeline, one end of the first pipeline is connected to the air outlet of the reference cylinder, and the other end is connected to the second air inlet of the sample cylinder; a second pipeline, one end of the second pipeline is connected to the vacuum pumping component, the first air outlet of the inert gas source, and the second air outlet of the natural gas source, and the other end is connected to the first air inlet of the reference cylinder.

[0013] Optionally, the system also includes: a first temperature sensor, arranged in the first chamber, for detecting the temperature value of the first chamber; a second temperature sensor, arranged in the second chamber, for detecting the temperature value of the second chamber; a first valve, arranged in the first pipeline; and a second valve, arranged in the second pipeline.

[0014] According to a fourth aspect of the present application, a readable storage medium is provided, on which a program or instruction is stored. When the program or instruction is executed by a processor, the steps of the shale gas adsorption measurement method of the first aspect are implemented.

[0015] Through the above technical solution, the present application provides a shale gas adsorption measurement method, device, system and readable storage medium. By creating a dual-temperature zone environment to conduct shale sample gas adsorption experiments, the temperature data of the gas in the low-temperature zone diffusing to the high-temperature zone where the shale sample is located and adsorbed on the rock is recorded. The pressure change during gas diffusion and adsorption and the change in the gas compression factor caused by the temperature difference between the two temperature zones are combined to calculate the amount of natural gas adsorbed by shale rock under high-temperature conditions. It can truly restore the gas adsorption process of deep shale under long-term high-temperature conditions, improve the accuracy of the measurement results of adsorbed gas volume under deep high-temperature conditions, and overcome the defect that the traditional volumetric method for measuring gas adsorption volume cannot maintain high precision in a high-temperature environment of 100°C or above for a long time. At the same time, the chamber where the high-precision instrument is located is controlled to maintain a low temperature to protect the components and ensure the reusability of the equipment.

[0016] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are listed below. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present application. Also, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:

[0018] Figure 1 A schematic diagram of a shale gas adsorption measurement method provided in an embodiment of the present application is shown;

[0019] Figure 2 A schematic diagram of temperature change in a shale gas adsorption measurement system provided in an embodiment of the present application is shown;

[0020] Figure 3A schematic structural diagram of a shale gas adsorption measurement device provided in an embodiment of the present application is shown;

[0021] Figure 4 A structural schematic diagram of a shale gas adsorption measurement system provided in an embodiment of the present application is shown.

[0022] in, Figure 4 The corresponding relationship between the reference numerals and the component names is as follows:

[0023] 300 shale gas adsorption measurement system, 301 first chamber, 302 second chamber, 303 reference cylinder, 304 sample cylinder, 305 pressure sensor, 306 vacuum assembly, 307 natural gas source, 308 inert gas source, 309 first pipeline, 310 second pipeline, 311 first temperature sensor, 312 second temperature sensor, 313 first valve, 314 second valve, 315 three-way connector, 316 heat insulation board. DETAILED DESCRIPTION

[0024] The exemplary embodiments of the present application will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present application and to fully convey the scope of the present application to those skilled in the art.

[0025] The present application embodiment provides a shale gas adsorption measurement method, such as Figure 1 As shown, the method includes:

[0026] S101 . Control the temperature in the first chamber according to a first preset temperature value, and control the temperature in the second chamber according to a second preset temperature value, wherein the first preset temperature value is smaller than the second preset temperature value.

[0027] In this step, the shale gas adsorption measurement method provided in the embodiment of the present application is executed by a shale gas adsorption measurement system. Specifically, the shale gas adsorption measurement system is provided with a first chamber and a second chamber, each of which is sealed. A reference cylinder is provided in the first chamber, and the reference cylinder is used to monitor gas changes or a baseline adsorption amount in the environment. The temperature of the reference cylinder changes with the temperature of the first chamber; a sample cylinder is provided in the second chamber, and the sample cylinder is used to add a shale sample to measure the adsorption amount of the gas. The temperature of the sample cylinder changes with the temperature of the second chamber.

[0028] Specifically, the temperature in the first chamber is set according to the first preset temperature value, and the temperature in the second chamber is set according to the second preset temperature value, wherein the second preset temperature value is a temperature higher than 100°C set according to the deep temperature stored in the actual formation, and the first temperature value is a low temperature lower than the second temperature value. By setting different temperature chamber temperatures, on the one hand, the temperature of the shale sample can meet the ultra-deep shale gas storage conditions, and on the other hand, the first chamber where the high-precision instrument (such as the pressure sensor) is located is kept at a low temperature to avoid the high-precision instrument being exposed to a high temperature environment for a long time to affect the measurement accuracy. Optionally, the first preset temperature value can be set to 40°C, and the second preset temperature value can be set to the ultra-deep shale formation temperature where the shale is located. Taking the southern part of the Sichuan Basin as an example, the burial depth of shale is mainly 3500m-4500m. Under the condition of a surface temperature of 15°C, the formation temperature of shale gas can reach 135°C. Therefore, when measuring the gas adsorption amount of the shale here, the second preset temperature value of the second chamber can be set to 135°C. By setting the temperatures of the first chamber and the second chamber respectively, a dual temperature zone setting of a low temperature zone (i.e., the first chamber) and a high temperature zone (i.e., the second chamber) is achieved, thereby avoiding direct contact between high temperature and high precision instruments, eliminating the influence of high temperature and high temperature changes on the performance and accuracy of high precision instruments, and protecting components to ensure the reusability of the equipment while ensuring that the experiment is suitable for deep shale gas adsorption environments, ensuring that the upper limit for high temperature measurements can ultimately be clearly given.

[0029] S102, execute the adsorption control action for a preset number of times, and obtain the first mass amount and the second mass amount corresponding to each adsorption control action; the adsorption control action includes: introducing natural gas into the reference cylinder according to the preset pressure value, and controlling the natural gas in the reference cylinder to diffuse into the sample cylinder, so that the natural gas is adsorbed into the pore space of the shale sample; the first mass amount is the amount of natural gas in the shale gas adsorption measurement system before the shale sample adsorbs natural gas, and the second mass amount is the amount of natural gas in the shale gas adsorption measurement system after the shale sample adsorbs natural gas. In this step, the gas storage capacity of the reservoir depends on the gas adsorption capacity of the shale rock. In order to better evaluate the gas storage potential of the reservoir, multiple rounds of adsorption control actions are set in the experiment to determine the adsorption behavior of natural gas in the pore space of the shale sample under different pressure conditions.

[0030] Specifically, in each round of adsorption control action, natural gas is first filled into the reference cylinder, and the gas pressure in the system before adsorption is recorded. Afterwards, the natural gas in the reference cylinder is diffused into the sample cylinder, so that the gas is adsorbed into the pore space of the shale sample, and the gas pressure in the system at the final state of adsorption equilibrium is recorded. By recording the temperature at which the gas in the low-temperature zone diffuses to the high-temperature zone where the shale sample is located and is adsorbed on the rock, combined with the pressure change during gas diffusion and adsorption and the change in the gas compression factor caused by the temperature difference between the two temperature zones, the amount of natural gas before the shale sample adsorbs natural gas under different pressure conditions and the amount of natural gas after the shale sample adsorbs natural gas are calculated.

[0031] S103, determining the gas adsorption amount of the shale sample corresponding to each adsorption control action according to the first mass of substance and the second mass of substance corresponding to each adsorption control action.

[0032] In this step, the adsorption increment of the shale sample in each adsorption control action is calculated by subtracting the amount of natural gas substance after the shale sample adsorbs natural gas from the amount of natural gas substance before the shale sample adsorbs natural gas in each adsorption control action.

[0033] The shale gas adsorption measurement method provided in the embodiment of the present application creates a dual-temperature zone environment to conduct a shale sample gas adsorption experiment, records the temperature data of the gas in the low-temperature zone diffusing to the high-temperature zone where the shale sample is located and adsorbed on the rock, and combines the pressure change during the gas diffusion and adsorption process and the change in the gas compression factor caused by the temperature difference between the dual-temperature zones to calculate the adsorption of natural gas by shale rock under high-temperature conditions. It can truly restore the gas adsorption process of deep shale under long-term high-temperature conditions, improve the accuracy of the measurement results of adsorbed gas volume under deep high-temperature conditions, overcome the defect that the traditional volumetric method for measuring gas adsorption volume cannot maintain high precision in a high-temperature environment of 100°C or above for a long time, and at the same time, control the chamber where the high-precision instrument is located to maintain a low temperature, protect the components, and ensure the reusability of the equipment.

[0034] Further, as a refinement and extension of the specific implementation of the above embodiment, in order to fully illustrate the specific implementation process of this embodiment, the embodiment of the present application provides another shale gas adsorption measurement method, which includes:

[0035] S201. Obtain the sample diameter, sample height, and sample mass of the shale sample.

[0036] In this step, a shale sample is drilled according to the sample diameter and sample height of the shale sample, the shale sample is placed in a drying box for drying, and then the rock quality of the shale sample is measured.

[0037] In practical applications, a shale columnar sample is drilled by a drilling machine, the diameter of the columnar sample can be 2.5 cm, and the height of the columnar sample does not exceed 10 cm. Afterwards, the shale sample is placed in a drying oven and dried to a constant weight, and the size of the shale sample, including dry weight, diameter D and length L, is measured using a vernier caliper and a balance. The measured dry weight is the sample mass M of the shale sample.

[0038] S202. Introduce inert gas into the reference cylinder and the sample cylinder to measure the skeleton volume, skeleton density and porosity of the shale sample.

[0039] In this step, in order to more comprehensively understand the physical properties and adsorption behavior of shale samples and provide valuable data and information for evaluating the potential of shale gas reservoirs, after sampling the shale samples, inert gas is introduced into the reference cylinder and the sample cylinder to measure the skeleton density (i.e., the fixed mass per unit volume of shale), skeleton volume (i.e., the solid mass of shale without pores or gas filling), and porosity (i.e., the ratio of the pore volume of shale to the total volume) of the shale samples.

[0040] In the embodiment of the present application, optionally, in step S202, inert gas is introduced into the reference cylinder and the sample cylinder to measure the skeleton volume, skeleton density and porosity of the shale sample, including the following steps:

[0041] S2021. Perform vacuum treatment on the reference cylinder, the sample cylinder and the first pipeline.

[0042] In this step, the shale sample is placed in the sample cylinder. At this time, there may be residual gas in the pore space of the shale. In order to ensure the accuracy of the experimental measurement, the vacuum component is started to vacuum the reference cylinder in the system, the residual gas of the shale sample in the sample cylinder, and the first pipeline to extract the residual gas in the pores of the shale sample.

[0043] S2022: Control the temperatures in the first chamber and the second chamber according to a first preset temperature value, and obtain a first temperature value of the first chamber and a second temperature value of the second chamber.

[0044] In this step, the first chamber and the second chamber are started, and the first chamber and the second chamber are set to the same first preset temperature value. At this time, the first temperature value of the first chamber is recorded, and the second temperature value is recorded. At this time, the first temperature value is equal to the second temperature value.

[0045] Optionally, the shale gas adsorption measurement system further includes: a vacuum assembly, a first pipeline, a second pipeline, a pressure sensor, a first valve, and a second valve. The vacuum assembly is used to vacuum the reference cylinder and the first pipeline, and is also used to detect air tightness and vacuum the entire system after a complete adsorption process is completed. The vacuum assembly and the reference cylinder are connected through the second pipeline; the reference cylinder and the sample cylinder are connected through the first pipeline; the pressure sensor is arranged in the first chamber, and is used to simultaneously monitor the pressure values ​​of the reference cylinder and the sample cylinder during the experiment; the first valve is arranged on the first pipeline; and the second valve is arranged on the second pipeline. Before starting the first chamber and the second chamber, the first valve and the second valve are opened, and the vacuum assembly is started to vacuum the system. When the pressure reading in the system is close to 0 and remains stable, the first valve is closed and left to stand for 120 minutes. If the pressure sensor reading remains unchanged, it proves that the air tightness in the system is good, and subsequent experimental operations can be performed.

[0046] S2023. Fill the reference cylinder with inert gas and use a pressure sensor to obtain the pressure value before adsorption.

[0047] S2024. Control the inert gas in the reference cylinder to diffuse into the sample cylinder so that the inert gas is adsorbed into the pore space of the shale sample, and use a pressure sensor to obtain a pressure value after adsorption.

[0048] In steps S2022 to S2024, the shale gas adsorption measurement system further includes an inert gas source, which contains high-purity helium and is used to transport inert gas to the reference cylinder and the sample cylinder. The inert gas source is connected to the reference cylinder through a second pipeline. The first valve is closed, the second valve and the inert gas source are opened, and the inert gas is filled into the reference cylinder. When the reading of the pressure sensor is stable, the second valve is closed, and the pressure value of the pressure sensor at this time is recorded, which is the pressure value before the shale sample adsorbs the inert gas.

[0049] Further, the first valve is opened to allow the inert gas to diffuse into the sample cylinder and enter the pore space of the shale sample. After the reading of the pressure sensor becomes stable, the pressure value of the pressure sensor at this time is recorded, which is the pressure value of the shale sample after the inert gas is adsorbed.

[0050] In the prior art, when the volumetric method is used to measure shale gas adsorption in a deep high-temperature environment (such as a high temperature above 100°C), the reference cylinder and the sample cylinder are in an interconnected temperature environment. In order to meet the actual deep shale formation temperature, the temperature in the system is set to above 100°C. When the volumetric method is used to measure the isothermal adsorption of shale gas, an extremely high-precision (more than 0.05% of the full range) electronic pressure sensor is required. The pressure sensor is exposed to a high-temperature environment for a long time, causing the resistance value of the metal sensitive element in the electronic pressure sensor to change, thereby affecting the output signal of the pressure sensor, reducing the sensitivity of the sensor and the accuracy of the experimental results. In the related art, in order to avoid the pressure sensor being exposed to a high-temperature environment for a long time, the measurement temperature is usually reduced to 70°C-80°C, but the measurement temperature set in this way is not suitable for the deep shale gas adsorption environment, resulting in low accuracy of the experimental results. Based on the above technical problems, the present application proposes to set up dual temperature zones and set the pressure sensor in the low temperature zone, so as to overcome the defect that the traditional volumetric method for measuring gas adsorption cannot maintain high precision in a high temperature environment of 100°C or above for a long time. At the same time, the pressure sensor does not need to be in direct contact with the high temperature zone, thus protecting the components and ensuring the reusability of the equipment.

[0051] S2025. Determine, in the inert gas compression factor comparison table, a first compression factor corresponding to the first temperature value and the pressure value before adsorption, and a second compression factor corresponding to the second temperature value and the pressure value after adsorption.

[0052] In this step, the compression factor (i.e., correction factor) is a parameter that takes into account the degree of gas compression at different temperatures and pressures. Since the conditions (such as temperature and pressure) commonly used in the experimental process are different from the actual formation conditions, it is necessary to import the compression factor to convert the experimentally measured data into data under real formation conditions in order to more accurately evaluate the adsorption performance of shale gas.

[0053] Specifically, the inert gas compression factor comparison table is a table for reference of inert gas compression factors under different conditions, which lists the values ​​of inert gas compression factors under different temperatures and pressures. Through the comparison table, the first compression factor of the inert gas under the conditions of the first temperature value and the pressure value before adsorption, and the second compression factor under the conditions of the second temperature value and the pressure value after adsorption are obtained.

[0054] S2026. Acquire multiple volume parameters of the shale gas adsorption measurement system, wherein the multiple volume parameters include: a reference cylinder volume of a reference cylinder, a first portion of the pipeline volume of the first pipeline between the first chamber and the second chamber, a second portion of the pipeline volume of the first pipeline contained in the first chamber, and a third portion of the pipeline volume of the first pipeline contained in the second chamber.

[0055] In this step, the volumes of the reference cylinder, the sample cylinder, and the first pipeline in different temperature zones are obtained respectively, so as to facilitate the subsequent calculation of relevant information of gas behavior.

[0056] S2027, importing the pre-adsorption pressure value, the reference cylinder volume, the second part pipeline volume, the first compression factor and the first temperature value into the real gas state equation to generate a first equation;

[0057] The first equation is:

[0058] ;

[0059] Among them, the above P 0 is the pressure value before adsorption; the above V t is the sum of the reference cylinder volume and the first part of the pipeline volume; the above Z 0 For inert gas at temperature T 0 、Pressure P 0 The first compression factor under the condition; the above n 0 is the amount of inert gas; R is the thermodynamic constant, R = 8.315 J / mol·K; T 0 is the first temperature value.

[0060] In this step, before the shale sample adsorbs the inert gas, the first valve is in a closed state and the inert gas is stored in the first chamber. At this time, the total volume of the first chamber is obtained by adding the reference cylinder volume to the second part of the pipeline volume, and the pre-adsorption pressure value, the first temperature value, the total volume of the first chamber and the first compression factor before the shale sample adsorbs the inert gas are introduced into the real gas state equation to describe the relationship between the state of the gas before adsorption and the pressure, temperature and volume.

[0061] In practical applications, the first valve arranged on the first pipeline in the shale gas adsorption measurement system can be arranged near the first chamber and close to the boundary of the first chamber on the side close to the temperature rising zone. In this way, the volume in the first chamber can be regarded as the sum of the reference cylinder volume and the volume of the second part of the pipeline, and the partial pipeline volume from the first valve in the first pipeline to the boundary of the first chamber can be ignored due to its small value.

[0062] S2028, importing the post-adsorption pressure value, multiple volume parameters, the second compression factor and the second temperature value into the real gas state equation to generate a second equation;

[0063] The second equation is:

[0064] ;

[0065] Among them, the above is the pressure value after adsorption; the above V lis the volume of the second part of the pipeline; the above V f is the free space volume in the second chamber excluding the skeleton volume of the shale sample; For inert gas at temperature ,pressure The second compression factor under the conditions; is the second temperature value, and the first temperature value is equal to the second temperature value.

[0066] In this step, the first valve is opened to allow the inert gas to be adsorbed into the pore space of the shale sample. At this time, the remaining gas is distributed in the first chamber, the first part of the pipeline, and the free space of the second chamber, wherein the free space of the second chamber refers to the space in the second chamber except the shale sample, which can be obtained by adding the volume of the sample cylinder to the sum of the volume of the third part of the pipeline, minus the skeleton volume of the shale sample. At this time, the post-adsorption pressure value, the second temperature value, the total volume of the second chamber (i.e., the sum of the volume of the sample cylinder plus the volume of the third part of the pipeline) and the second compression factor after the shale sample adsorbs the inert gas are introduced into the real gas state equation to describe the relationship between the state of the gas after adsorption and the pressure, temperature and volume.

[0067] S2029. Use the first equation and the second equation to calculate the skeleton volume, skeleton density and porosity of the shale sample.

[0068] In this step, the gas state before adsorption and the gas state after adsorption are combined to calculate the skeleton volume, skeleton density and porosity of the shale sample.

[0069] Through the above method, in the experimental process of studying the adsorption behavior of shale to natural gas, the rock skeleton density, skeleton volume and porosity of the shale sample are jointly measured, which helps to more comprehensively understand the physical properties and characteristics of the rock, and provide more comprehensive and reliable data for the study of shale rock. At the same time, there is no need to conduct separate experiments to determine the physical characteristics of shale samples, which effectively improves the efficiency of shale rock research.

[0070] In the embodiment of the present application, optionally, in step S2029, the skeleton volume, skeleton density and porosity of the shale sample are calculated using the first equation and the second equation, specifically including:

[0071] Combining the first equation and the second equation, constructing a third equation corresponding to the free space volume of the second chamber;

[0072] The third equation is:

[0073] .

[0074] Constructing a first mapping relationship between the free space volume of the second chamber and the volume of the sample cylinder, the skeleton volume, and the volume of the third portion of the pipeline;

[0075] The first mapping relationship is:

[0076] ;

[0077] Wherein, the above Va is the sum of the volume of the sample cylinder and the volume of the third part of the pipeline; and the above Vs is the skeleton volume.

[0078] It can be understood that the free space of the second chamber is the space in the second chamber except the shale sample. Therefore, the free space volume of the second chamber is the sum of the sample cylinder volume and the third part pipeline volume, minus the skeleton volume of the shale sample.

[0079] According to the above formula, the skeleton volume of the shale sample is calculated as:

[0080] .

[0081] Further, constructing a second mapping relationship between porosity and skeleton volume and sample data of the shale sample;

[0082] The second mapping relationship is:

[0083] ;

[0084] Among them, the above is the porosity; is the diameter of the shale sample; and the above L is the height of the shale sample.

[0085] Further, the porosity is calculated using the second mapping relationship and the skeleton volume;

[0086] The porosity is:

[0087] .

[0088] Further, constructing a third mapping relationship between the skeleton density, the sample mass of the shale sample, and the skeleton volume;

[0089] The third mapping relationship is:

[0090] ;

[0091] Wherein, the above M is the sample mass of the shale sample.

[0092] Further, using the third mapping relationship and the skeleton volume, the skeleton density is calculated;

[0093] The skeleton density is:

[0094] .

[0095] S2030, exhausting the inert gas in the reference cylinder, the sample cylinder and the first pipeline.

[0096] In this step, after measuring various data of the shale sample, the second valve and the vacuum assembly are opened to perform vacuum processing to exhaust the inert gas in the system, and then the first valve and the second valve are closed.

[0097] S203 , controlling the temperature in the first chamber according to a first preset temperature value, and controlling the temperature in the second chamber according to a second preset temperature value, wherein the first preset temperature value is smaller than the second preset temperature value.

[0098] In this step, shale is usually in an ultra-deep formation environment with high temperature and pressure. In order to better simulate the actual geological conditions of shale gas reservoirs and more accurately evaluate the adsorption performance of shale gas, the temperature of the second chamber where the sample cylinder containing the shale sample is located is adjusted to above 100°C to match the formation temperature. Since the pressure sensor is installed in the first chamber, the pressure sensor cannot maintain the instrument sensitivity and stable measurement accuracy for a long time in a high temperature environment above 100°C. Therefore, the temperature of the first chamber is kept unchanged so that the first chamber is maintained at the first preset temperature value.

[0099] S204: Set the number of adsorption control actions to i.

[0100] S205 . According to the preset pressure value corresponding to the i-th adsorption control action, natural gas is introduced into the reference cylinder, and the pressure value before adsorption is obtained by using a pressure sensor.

[0101] In steps S204 and S205, the shale gas adsorption measurement system also includes a natural gas source, and the outlet of the natural gas source is connected to the inlet of the reference cylinder through a second pipeline. In order to measure the adsorption amount of the shale sample under different pressure conditions, it is necessary to perform multiple adsorption control actions according to the change of the preset pressure value. For each adsorption control action i, the second valve and the natural gas source outlet valve are opened, and the first valve is kept in a closed state, so that the natural gas diffuses into the reference cylinder. When the reading of the pressure sensor reaches the preset pressure value corresponding to the i-th adsorption control action and remains stable, the gas supply is stopped, and the second valve and the natural gas source outlet valve are closed. At this time, the reading of the pressure sensor is recorded, which is the pre-adsorption pressure value before the shale sample adsorbs natural gas.

[0102] S206: Obtain a third temperature value of the first chamber.

[0103] The temperature in the first chamber remains constant, that is, the third temperature value is the same as the first temperature value and the second temperature value.

[0104] S207. Determine, in the comparison table of natural gas compression factors, a third compression factor corresponding to the third temperature value and the pre-adsorption pressure value.

[0105] S208, importing the pre-adsorption pressure value, the third temperature value, the third compression factor, the reference cylinder volume and the second part of the pipeline volume into the real gas state equation to calculate the amount of natural gas in the first chamber before the shale sample adsorbs natural gas.

[0106] In steps S206 to S208, the natural gas is obtained at P i and T 0 The third compression factor under the conditions. The pressure value before adsorption, the third temperature value, the third compression factor, the reference cylinder volume, and the second part of the pipeline volume are introduced into the real gas state equation to obtain:

[0107] ;

[0108] Wherein, the above i is the number of adsorption control actions, i is a positive integer greater than 0; is the pressure value before adsorption in the i-th adsorption control action; is the third temperature value in the first chamber during the i-th adsorption control action; For natural gas in P i and T 0 The third compression factor under conditions.

[0109] The above formula is converted to calculate the amount of natural gas in the first chamber before adsorption in the i-th adsorption control action:

[0110] .

[0111] S209, obtaining the amount of natural gas in the free space of the second chamber after the shale sample absorbs natural gas in the (i-1)th adsorption control action, and the amount of natural gas in the first part of the pipeline after the shale sample absorbs natural gas.

[0112] S210. Calculate the first mass amount corresponding to the i-th adsorption control action based on the amount of natural gas in the first chamber before the shale sample absorbs natural gas in the i-th adsorption control action, the amount of natural gas in the free space of the second chamber after the shale sample absorbs natural gas in the i-1-th adsorption control action, and the amount of natural gas in the first part of the pipeline after the shale sample absorbs natural gas in the i-1-th adsorption control action.

[0113] In steps S209 and S210, for the first adsorption control action, after natural gas is introduced into the reference cylinder, the second chamber and the first part of the pipeline are in a vacuum state, and the amount of natural gas in the first chamber is the amount of natural gas before adsorption in the system.

[0114] After the first adsorption control action is completed, the reference cylinder and the second part of the pipeline need to be evacuated to measure the next pressure point. In order to save gas consumption and experimental time, the first valve is closed during vacuuming so that the natural gas in the sample cylinder and the first part of the pipeline will not be extracted. In the subsequent adsorption control action, after calculating the amount of new natural gas in the first chamber, add the amount of free natural gas in the free space of the high temperature zone of the previous round of experiments and the amount of free natural gas in the temperature rise zone of the previous round of experiments, which is the second amount of substance before adsorption in the system:

[0115] ;

[0116] in Above is the amount of natural gas in the free space of the second chamber after the shale sample adsorbs natural gas in the i-1th adsorption control action; It is the amount of the first part of the natural gas in the pipeline after the shale sample adsorbs the natural gas in the i-1th adsorption control action.

[0117] In practical applications, for the first adsorption control action during the experiment, and are all 0, so we only need to calculate n 1 The amount of gas before adsorption can be obtained. For any subsequent adsorption control action, such as the second adsorption control action, after natural gas is filled into the reference cylinder, the amount of gas before adsorption in the low temperature zone is calculated. , and then retrieve the first adsorption control action in the experimental data and , adding the three together can get the amount of the substance in the gas before adsorption in the second round of adsorption control action.

[0118] S211. For the i-th adsorption control action, control the natural gas in the reference cylinder to diffuse to the sample cylinder through the first pipeline, so that the natural gas is adsorbed into the pore space of the shale sample, and use the pressure sensor to obtain the pressure value after adsorption.

[0119] In this step, for the i-th adsorption control action, after recording the pre-adsorption pressure value before adsorption, the first valve is opened to allow the natural gas in the reference cylinder to diffuse into the sample cylinder through the first pipeline and adsorb into the pore space of the shale sample. After the reading of the pressure sensor stabilizes, the post-adsorption pressure value is recorded.

[0120] S212: Obtain a fourth temperature value of the second chamber.

[0121] In this step, in the adsorption control action, the temperature of the second chamber is set to the ultra-deep shale formation temperature (above 100°C) to study the adsorption of natural gas by shale under real ultra-deep shale gas reservoir conditions. This has important practical significance for optimizing gas exploration and development under complex geological conditions.

[0122] S213. Determine, in the natural gas compression factor comparison table, a fourth compression factor corresponding to the third temperature value and the pressure value after adsorption, and a fifth compression factor corresponding to the fourth temperature value and the pressure value after adsorption.

[0123] In this step, after the pressure after adsorption in the system is stabilized, the fourth compression factor of natural gas under the conditions of the third temperature value and the pressure value before adsorption, and the fifth compression factor under the conditions of the fourth temperature value and the pressure value after adsorption are found in the natural gas compression factor comparison table.

[0124] S214, introducing the pressure value after adsorption, the reference cylinder volume, the second part pipeline volume, the third temperature value and the fourth compression factor into the real gas state equation to calculate the amount of natural gas in the first chamber after the shale sample adsorbs natural gas.

[0125] In this step, after the shale sample adsorbs natural gas, the post-adsorption pressure value of the first chamber, the volume of the first chamber (the sum of the reference cylinder volume and the second part of the pipeline volume), the third temperature value and the fourth compression factor are introduced into the real gas state equation to obtain:

[0126] ;

[0127] Among them, the above is the pressure value after adsorption in the i-th adsorption control action; For natural gas and The fourth compression factor under conditions.

[0128] Then, the above formula is converted to calculate the amount of gas in the low temperature zone after adsorption:

[0129] .

[0130] S215, importing the post-adsorption pressure value, the third part pipeline volume, the sample cylinder volume, the skeleton volume, the fifth compression factor and the fourth temperature value into the real gas state equation to calculate the amount of natural gas in the free space of the second chamber after the shale sample adsorbs natural gas.

[0131] In this step, the post-adsorption pressure value, the free space volume of the second chamber (the sum of the sample cylinder volume plus the third part of the pipeline volume, minus the skeleton volume of the shale sample), the fifth compression factor and the fourth temperature value are introduced into the real gas state equation to obtain:

[0132] ;

[0133] Among them, the above For natural gas and The fifth compression factor under the conditions; is a fourth temperature value of the second chamber.

[0134] Then, the above formula is transformed to calculate the amount of gas in the free space in the high temperature zone after adsorption, excluding the skeleton volume of the shale sample:

[0135] .

[0136] S216. Construct a temperature variation function in the first part of the pipeline.

[0137] S217, integrating the temperature change function, and calculating the fitting temperature in the first portion of the pipeline according to the integrated temperature change function and the length value of the first portion of the pipeline.

[0138] S218. Determine the sixth compression factor corresponding to the fitting temperature and the pressure value after adsorption in the natural gas compression factor comparison table.

[0139] In steps S216 to S218, if Figure 2 As shown, it is a schematic diagram of temperature changes in different areas of the shale gas adsorption measurement system. Figure 2 The horizontal axis is the pipeline length of the pipeline in different areas, and the vertical axis is the temperature corresponding to different pipeline positions in different areas. Among them, the temperature in the heating zone (i.e., in the first part of the pipeline) increases linearly as it approaches the high temperature zone from the low temperature zone along the length of the pipeline. Obviously, the temperature in the heating zone is not a constant. The temperature at different pipes in the heating zone is different, and the temperature field is linearly distributed in one-dimensional unidirectional direction. Therefore, the temperature change function in the heating zone is constructed:

[0140] ;

[0141] Among them, any pipeline position within the first part of the pipeline mentioned above; is the temperature value at l; the above L l is the length of the first section of the pipeline.

[0142] After that, the temperature change function is integrated and divided by the length of the pipeline in the heating zone to obtain the fitting temperature in the heating zone:

[0143] .

[0144] Furthermore, based on the natural gas compression factor comparison table, the sixth compression factor of natural gas under the conditions of fitting temperature and post-adsorption pressure value is determined.

[0145] S219, importing the post-adsorption pressure value, the first part of the pipeline volume, the fourth compression factor and the fitting temperature into the real gas state equation to construct the fourth equation.

[0146] S220, using the fitting temperature in the first pipeline and the fourth equation, calculate the amount of natural gas in the first pipeline after the shale sample adsorbs the natural gas.

[0147] In steps S219 and S220, the pressure value after adsorption, the first part of the pipeline volume, the fourth compression factor and the fitting temperature are introduced into the real gas state equation to construct the fourth equation:

[0148] ;

[0149] Among them, the above It is the amount of the natural gas in the first part of the pipeline after the shale sample adsorbs the natural gas in the i-th adsorption control action.

[0150] Furthermore, the amount of natural gas in the first part of the pipeline after the shale sample adsorbs natural gas is calculated using the fitting temperature in the first part of the pipeline and the fourth equation:

[0151] ;

[0152] Among them, the above For natural gas , The sixth compression factor under conditions.

[0153] S221. Calculate the second mass of the natural gas corresponding to the i-th adsorption control action according to the mass of the natural gas in the first chamber, the mass of the natural gas in the free space of the second chamber, and the mass of the natural gas in the first part of the pipeline after the shale sample adsorbs the natural gas.

[0154] In this step, the above steps are used to calculate the amount of gas substance after adsorption in the low temperature zone, high temperature zone and temperature rise zone in the i-th adsorption control action. Finally, the amount of gas substance after adsorption in the low temperature zone, high temperature zone and temperature rise zone is added together to obtain the amount of gas substance after the i-th adsorption control action is completed:

[0155] .

[0156] S222. Determine the gas adsorption amount of the shale sample corresponding to each adsorption control action according to the first mass of substance and the second mass of substance corresponding to each adsorption control action.

[0157] In this step, the first substance mass n before adsorption of the i-th round of adsorption control action is calculated. i , and the amount of the second substance after adsorption N i After that, calculate the pressure ,temperature Shale adsorption increment under conditions Among them, for the first adsorption control action, after the vacuum pumping phase at the beginning of the experiment, the gas adsorption amount of the shale sample is 0. Therefore, the shale adsorption increment calculated by the first adsorption control action is: .

[0158] Optionally, the calculated shale adsorption increment is also equivalent to the total shale adsorption amount in this adsorption control action, and then the shale adsorption amount per unit mass can be calculated based on the shale mass and the total shale adsorption amount:

[0159] .

[0160] Optionally, after all adsorption control actions are completed, the shale adsorption increments of each round are added together to calculate the total shale adsorption amount of the entire experiment.

[0161] In practical applications, after the adsorption amount of shale rock under different pressures is obtained from the experiment, an isotherm curve can be drawn based on the shale adsorption amount and multiple preset pressure values ​​of multiple rounds of adsorption control actions, where the horizontal axis is the preset pressure value of each round of adsorption control action, and the vertical axis is the shale adsorption amount of each round of adsorption control action. Furthermore, the Langmuir volume and Langmuir pressure can be obtained by calculation based on the Langmuir (adsorption isotherm) equation.

[0162] In the above method, a dual temperature zone is set in the system, and the pressure and temperature data of the gas in the low temperature zone diffusing to the high temperature zone where the shale sample is located and adsorbed on the shale are recorded. Based on the law of conservation of matter and the actual gas state equation, and considering the pressure change during gas diffusion and adsorption and the change in the gas compression factor caused by the temperature difference between the two temperature zones, the gas adsorption calculation formula of the two temperature zones is combined to calculate the adsorption amount of natural gas by shale under high temperature conditions. The defect that the experimental pressure sensor for measuring gas adsorption by volumetric method in related technologies cannot maintain the instrument sensitivity and temperature measurement accuracy for a long time at high temperatures above 100°C is solved. In addition, the skeleton density, skeleton volume and porosity of shale are jointly determined through the experimental process of determining the free volume of the sample cylinder with inert gas, which truly realizes the adsorption process of deep shale on gas under long-term high temperature conditions, and effectively improves the accuracy of the evaluation results of shale porosity and adsorbed gas under deep high temperature conditions.

[0163] Further, as Figure 1 The specific implementation of the method, the embodiment of the present application provides a shale gas adsorption measurement device 200, which is applicable to a shale gas adsorption measurement system, the shale gas adsorption measurement system includes a first chamber, a second chamber, a reference cylinder and a sample cylinder, wherein the reference cylinder is arranged in the first chamber, the sample cylinder is arranged in the second chamber, and a shale sample is placed in the sample cylinder, such as Figure 3 As shown, the device includes: a control module 201, an acquisition module 202 and a determination module 203.

[0164] A control module 201, configured to control the temperature in the first chamber according to a first preset temperature value, and control the temperature in the second chamber according to a second preset temperature value, wherein the first preset temperature value is less than the second preset temperature value;

[0165] The acquisition module 202 is used to perform a preset number of adsorption control actions and acquire a first mass and a second mass corresponding to each adsorption control action; the adsorption control action includes: introducing natural gas into the reference cylinder according to a preset pressure value, and controlling the natural gas in the reference cylinder to diffuse into the sample cylinder so that the natural gas is adsorbed into the pore space of the shale sample; the first mass is the mass of the natural gas in the shale gas adsorption measurement system before the shale sample adsorbs the natural gas, and the second mass is the mass of the natural gas in the shale gas adsorption measurement system after the shale sample adsorbs the natural gas;

[0166] The determination module 203 is used to determine the gas adsorption amount of the shale sample corresponding to each adsorption control action according to the first mass of substance and the second mass of substance corresponding to each adsorption control action.

[0167] In a specific application scenario, optionally, the shale gas adsorption measurement system further includes: a first pipeline and a pressure sensor, the first pipeline is used to connect the reference cylinder and the sample cylinder, and the device further includes: a generation module 204 and a calculation module 205.

[0168] The acquisition module 202 is also used to obtain the sample diameter, sample height and sample mass of the shale sample;

[0169] The control module 201 is further used to control the temperature in the first chamber and the second chamber according to the first preset temperature value; the acquisition module 202 is further used to acquire the first temperature value of the first chamber and the second temperature value of the second chamber;

[0170] The control module 201 is also used to perform vacuum processing on the shale gas adsorption measurement system;

[0171] The control module 201 is also used to control the inert gas in the reference cylinder to diffuse into the sample cylinder so that the inert gas is adsorbed into the pore space of the shale sample; the acquisition module 202 is also used to obtain the pressure value after adsorption using the pressure sensor;

[0172] The determination module 203 is further used to determine, in the inert gas compressibility factor comparison table, a first compressibility factor corresponding to the first temperature value and the pressure value before adsorption, and a second compressibility factor corresponding to the second temperature value and the pressure value after adsorption;

[0173] The acquisition module 202 is further used to acquire a plurality of volume parameters of the shale gas adsorption measurement system, wherein the plurality of volume parameters include: a reference cylinder volume of the reference cylinder, a first portion of the pipeline volume of the first pipeline located between the first chamber and the second chamber, a second portion of the pipeline volume of the first pipeline contained in the first chamber, and a third portion of the pipeline volume of the first pipeline contained in the second chamber;

[0174] A generating module 204 is used to introduce the pre-adsorption pressure value, the reference cylinder volume, the second part pipeline volume, the first compressibility factor and the first temperature value into the real gas state equation to generate a first equation;

[0175] The first equation is:

[0176] ;

[0177] Among them, the above P 0 is the pressure value before adsorption; the above V t is the sum of the reference cylinder volume and the second part of the pipeline volume; the above Z 0 For inert gas at T 0 , P 0 The first compression factor under the condition; the above n 0 is the amount of inert gas; R is a thermodynamic constant; T0 is the first temperature value;

[0178] The generation module 204 is also used to import the post-adsorption pressure value, multiple volume parameters, the second compression factor and the second temperature value into the real gas state equation to generate a second equation;

[0179] The second equation is:

[0180] ;

[0181] Among them, the above is the pressure value after adsorption; the above V l is the volume of the first part of the pipeline; the above V f is the free space volume in the second chamber excluding the skeleton volume of the shale sample; For inert gas , The second compression factor under the conditions; is the second temperature value;

[0182] A calculation module 205, for calculating the skeleton volume, skeleton density and porosity of the shale sample using the first equation and the second equation;

[0183] The control module 201 is also used to exhaust the inert gas in the shale gas adsorption measurement system.

[0184] In a specific application scenario, optionally, the first measurement module 202 is specifically used to:

[0185] Combining the first equation and the second equation, constructing a third equation corresponding to the free space volume of the second chamber;

[0186] The third equation is:

[0187] ;

[0188] Constructing a first mapping relationship between the free space volume of the second chamber and the volume of the sample cylinder, the skeleton volume, and the volume of the third portion of the pipeline;

[0189] The first mapping relationship is:

[0190] ;

[0191] Among them, the above V a is the sum of the volume of the sample cylinder and the volume of the third part of the pipeline; the above V s is the skeleton volume;

[0192] Calculate the skeleton volume using the third equation and the first mapping relationship;

[0193] The volume of the skeleton is:

[0194] ;

[0195] constructing a second mapping relationship between porosity and skeleton volume and sample data of the shale sample;

[0196] The second mapping relationship is:

[0197] ;

[0198] Among them, the above is the porosity; is the diameter of the shale sample; the above L is the height of the shale sample;

[0199] Calculate the porosity using the second mapping relationship and the skeleton volume;

[0200] The porosity is:

[0201] ;

[0202] constructing a third mapping relationship between skeleton density, sample mass of the shale sample and skeleton volume;

[0203] The third mapping relationship is:

[0204] ;

[0205] Wherein, the above M is the sample mass of the shale sample;

[0206] Calculate the skeleton density using the third mapping relationship and the skeleton volume;

[0207] The skeleton density is:

[0208] .

[0209] In a specific application scenario, optionally, the acquisition module 202 is used to:

[0210] Set the number of adsorption control actions to i;

[0211] According to the preset pressure value corresponding to the i-th adsorption control action, natural gas is introduced into the reference cylinder, and the pressure value before adsorption is obtained by using the pressure sensor;

[0212] obtaining a third temperature value of the first chamber;

[0213] In the comparison table of natural gas compression factors, determine the third compression factor corresponding to the third temperature value and the pre-adsorption pressure value;

[0214] The pressure value before adsorption, the third temperature value, the third compression factor, the reference cylinder volume and the second part pipeline volume are introduced into the real gas state equation to calculate the amount of natural gas in the first chamber before the shale sample adsorbs natural gas;

[0215] Before the shale sample adsorbs natural gas, the amount of natural gas in the first chamber is:

[0216] ;

[0217] Wherein, the above i is the number of adsorption control actions, i is a positive integer greater than 0; is the pre-adsorption pressure value of the shale sample before the adsorption of natural gas in the i-th adsorption control action; is the third temperature value in the first chamber; For natural gas in P i and T 0 The third compression factor under the conditions;

[0218] Obtaining the amount of natural gas in the free space of the second chamber after the shale sample absorbs the natural gas in the i-1th adsorption control action, and the amount of natural gas in the first part of the pipeline after the shale sample absorbs the natural gas;

[0219] Calculate the first mass of the substance corresponding to the i-th adsorption control action according to the amount of the substance of the natural gas in the first chamber before the shale sample adsorbs the natural gas in the i-th adsorption control action, the amount of the substance of the natural gas in the free space of the second chamber after the shale sample adsorbs the natural gas in the i-1-th adsorption control action, and the amount of the substance of the natural gas in the first part of the pipeline after the shale sample adsorbs the natural gas in the i-1-th adsorption control action;

[0220] The first mass of substance corresponding to the i-th adsorption control action is:

[0221] ;

[0222] in Above is the amount of natural gas in the free space of the second chamber after the shale sample adsorbs natural gas in the i-1th adsorption control action; It is the amount of natural gas in the first part of the pipeline after the shale sample adsorbs natural gas in the i-1th adsorption control action.

[0223] In a specific application scenario, optionally, the acquisition module 202 is further used to:

[0224] For the i-th adsorption control action, the natural gas in the reference cylinder is controlled to diffuse to the sample cylinder through the first pipeline, so that the natural gas is adsorbed into the pore space of the shale sample, and the pressure value after adsorption is obtained by using the pressure sensor;

[0225] acquiring a fourth temperature value of the second chamber;

[0226] In the natural gas compression factor comparison table, determine the fourth compression factor corresponding to the third temperature value and the pressure value after adsorption, and the fifth compression factor corresponding to the fourth temperature value and the pressure value after adsorption;

[0227] The pressure value after adsorption, the volume of the reference cylinder, the volume of the second part of the pipeline, the third temperature value and the fourth compression factor are introduced into the real gas state equation to calculate the amount of natural gas in the first chamber after the shale sample adsorbs natural gas;

[0228] After the shale sample adsorbs natural gas, the amount of natural gas in the first chamber is:

[0229] ;

[0230] Among them, the above is the pressure value after adsorption in the i-th adsorption control action; For natural gas and The fourth compression factor under the conditions;

[0231] The pressure value after adsorption, the volume of the third part pipeline, the volume of the sample cylinder, the volume of the skeleton, the fifth compression factor and the fourth temperature value are introduced into the real gas state equation to calculate the amount of natural gas in the free space of the second chamber after the shale sample adsorbs natural gas;

[0232] After the shale sample adsorbs natural gas, the amount of natural gas in the free space of the second chamber is:

[0233] ;

[0234] Among them, the above For natural gas and The fifth compression factor under the conditions; is a fourth temperature value of the second chamber;

[0235] Constructing a temperature variation function in the first part of the pipeline;

[0236] The temperature change function is:

[0237] ;

[0238] Among them, any pipeline position within the first part of the pipeline mentioned above; is the temperature value at l; the above L l is the length of the first part of the pipeline;

[0239] Integrating the temperature variation function, and calculating the fitting temperature in the first portion of the pipeline according to the integrated temperature variation function and the length value of the first portion of the pipeline;

[0240] The fitted temperature in the first part of the pipeline is:

[0241] ;

[0242] In the natural gas compression factor comparison table, determine the sixth compression factor corresponding to the fitting temperature and the pressure value after adsorption;

[0243] The pressure value after adsorption, the volume of the first part of the pipeline, the sixth compressibility factor and the fitting temperature are introduced into the real gas state equation to construct the fourth equation;

[0244] The fourth equation is:

[0245] ;

[0246] Among them, the above is the amount of natural gas in the first part of the pipeline after the shale sample adsorbs natural gas in the i-th adsorption control action;

[0247] Calculating the amount of natural gas in the first part of the pipeline after the shale sample adsorbs the natural gas using the fitted temperature in the first part of the pipeline and the fourth equation;

[0248] After the shale sample adsorbs natural gas, the amount of natural gas in the first part of the pipeline is:

[0249] ;

[0250] Among them, the above For natural gas , The sixth compression factor under the conditions;

[0251] Calculate the second mass of the substance corresponding to the i-th adsorption control action according to the mass of the natural gas in the first chamber, the mass of the natural gas in the free space of the second chamber, and the mass of the natural gas in the first part of the pipeline after the shale sample adsorbs the natural gas in the i-th adsorption control action;

[0252] The second mass of substance corresponding to the i-th adsorption control action is:

[0253] .

[0254] The shale gas adsorption measurement device 200 provided in the present application sets up a dual temperature zone in the system, and records the pressure and temperature data of the gas in the low temperature zone diffusing to the high temperature zone where the shale sample is located and adsorbed on the shale. Based on the law of conservation of matter and the actual gas state equation, and considering the pressure change during the gas diffusion and adsorption process and the change in the gas compression factor caused by the temperature difference between the two temperature zones, combined with the dual temperature zone gas adsorption calculation formula, the adsorption amount of natural gas by shale under high temperature conditions is calculated. The defect that the experimental pressure sensor for measuring gas adsorption by volumetric method in the related technology cannot maintain the instrument sensitivity and temperature measurement accuracy for a long time at a high temperature above 100°C is solved. In addition, the skeleton density, skeleton volume and porosity of shale are jointly determined through the experimental process of determining the free volume of the sample cylinder with inert gas, and the adsorption process of gas by deep shale under long-term high temperature conditions is truly realized, effectively improving the accuracy of the evaluation results of shale porosity and adsorbed gas under deep high temperature conditions.

[0255] In an exemplary embodiment, the present application also provides a shale gas adsorption measurement system 300, including: a first chamber 301; a second chamber 302; a reference cylinder 303, arranged in the first chamber 301, the reference cylinder 303 includes a first air inlet and an air outlet; a sample cylinder 304, arranged in the second chamber 302, the sample cylinder 304 includes a second air inlet, and the second air inlet is connected to the air outlet of the reference cylinder 303; a pressure sensor 305, arranged in the first chamber 301, the pressure sensor 305 is used to detect the pressure value of the shale gas adsorption measurement system 300; a memory, the memory stores a program or instruction; a processor, connected to the memory, and the shale gas adsorption measurement method in the above embodiment is implemented when the processor executes the program or instruction.

[0256] In a specific application scenario, the system may further include: a vacuum pumping component 306 for vacuuming the shale gas adsorption measurement system 300, the vacuum pumping component 306 including a vacuum pumping end connected to the first air inlet of the reference cylinder 303; an inert gas source 308 for introducing inert gas into the reference cylinder 303 and the sample cylinder 304, the inert gas source 308 including a first air outlet end connected to the air inlet of the reference cylinder 303; a natural gas source 307 for introducing natural gas into the reference cylinder 303 and the sample cylinder 304. 04 introduces natural gas, the natural gas source 307 includes a second gas outlet end, and the second gas outlet end is connected to the first gas inlet of the reference cylinder 303; a first pipeline 309, one end of the first pipeline 309 is connected to the gas outlet of the reference cylinder 303, and the other end is connected to the second gas inlet of the sample cylinder 304; a second pipeline 310, one end of the second pipeline 310 is connected to the gas extraction end of the vacuum pumping component 306, the first gas outlet end of the inert gas source 308 and the second gas outlet end of the natural gas source 307, and the other end is connected to the first gas inlet of the reference cylinder 303.

[0257] In a specific application scenario, optionally, the system also includes: a first temperature sensor 311, arranged in the first chamber 301, for detecting the temperature value of the first chamber 301; a second temperature sensor 312, arranged in the second chamber 302, for detecting the temperature value of the second chamber 302; a first valve 313, arranged in the first pipeline 309; and a second valve 314, arranged in the second pipeline 310.

[0258] The shale gas adsorption measurement system 300 provided in the present application includes a first chamber 301 and a second chamber 302, and the reference cylinder 303 and the sample cylinder are respectively set in different temperature environments and connected through a first pipeline 309. Further, the system also includes a pressure sensor 305, a first temperature sensor 311 and a second temperature sensor 312, wherein the pressure sensor 305 and the first temperature sensor 311 are set in the first chamber 301, and the second temperature sensor 312 is set in the second chamber 302. The temperature of the low temperature zone and the high temperature zone is detected by the first temperature sensor 311 and the second temperature sensor 312 to ensure that the gas compression factor is accurate. The system also includes a vacuum assembly 306, an inert gas source 308, a natural gas source 307, a three-way joint 315 and a second pipeline 310. Specifically, the vacuum assembly 306, the inert gas source 308, the three-way joint 315 and the natural gas source 307 are connected to the reference cylinder 303 through the second pipeline 310. Furthermore, the system further includes a first valve 313 and a second valve 314 . The first valve 313 is disposed on the first pipeline 309 , and the second valve 314 is disposed on the second pipeline 310 .

[0259] Optionally, a heat insulation plate 316 is provided on the wall of the second chamber 302 close to the first pipeline 309 to ensure that the temperature of the first pipeline 309 between the dual temperature zones increases linearly from low temperature to high temperature.

[0260] In an exemplary embodiment, the present application also provides a readable storage medium having a computer program stored thereon, and when the computer program is executed by a processor, the steps of the shale gas adsorption measurement method are implemented.

[0261] Through the description of the above implementation methods, those skilled in the art can clearly understand that the present application can be implemented by hardware, or by means of software plus a necessary general hardware platform. Based on such an understanding, the technical solution of the present application can be embodied in the form of a software product, which can be stored in a non-volatile readable storage medium (which can be a CD-ROM, a USB flash drive, a mobile hard disk, etc.), including a number of instructions for enabling an electronic device (which can be a personal computer, a server, or a network device, etc.) to execute the methods described in each implementation scenario of the present application.

[0262] Those skilled in the art will appreciate that the accompanying drawings are merely schematic diagrams of a preferred implementation scenario, and the modules or processes in the accompanying drawings are not necessarily required for implementing the present application.

[0263] Those skilled in the art will appreciate that the modules in the devices in the implementation scenario can be distributed in the devices in the implementation scenario according to the implementation scenario description, or can be changed accordingly and located in one or more devices different from the implementation scenario. The modules in the above implementation scenario can be combined into one module, or can be further split into multiple units.

[0264] The above application serial numbers are for description only and do not represent the advantages or disadvantages of the implementation scenarios.

[0265] The above disclosure only discloses several specific implementation scenarios of the present application. However, the present application is not limited thereto, and any changes that can be conceived by technicians in this field should fall within the scope of protection of the present application.

Claims

1. A shale gas adsorption measurement method, characterized in that: Applicable to a shale gas adsorption measurement system, the shale gas adsorption measurement system comprises a first chamber, a second chamber, a reference cylinder and a sample cylinder, wherein the reference cylinder is arranged in the first chamber, the sample cylinder is arranged in the second chamber, and a shale sample is placed in the sample cylinder, the method comprises: Controlling the temperature in the first chamber according to a first preset temperature value, and controlling the temperature in the second chamber according to a second preset temperature value, wherein the first preset temperature value is less than the second preset temperature value; Execute a preset number of adsorption control actions to obtain a first mass amount and a second mass amount corresponding to each adsorption control action; the adsorption control action includes: introducing natural gas into the reference cylinder according to a preset pressure value, and controlling the natural gas in the reference cylinder to diffuse into the sample cylinder, so that the natural gas is adsorbed into the pore space of the shale sample; the first mass amount is the amount of the natural gas in the shale gas adsorption measurement system before the shale sample adsorbs the natural gas, and the second mass amount is the amount of the natural gas in the shale gas adsorption measurement system after the shale sample adsorbs the natural gas; determining the gas adsorption amount of the shale sample corresponding to each adsorption control action according to the first substance amount and the second substance amount corresponding to each adsorption control action; The step of obtaining the first substance amount corresponding to each adsorption control action specifically includes: Set the number of adsorption control actions to i; According to the preset pressure value corresponding to the i-th adsorption control action, the natural gas is introduced into the reference cylinder, and the pressure value before adsorption is obtained by using a pressure sensor; Acquiring a third temperature value of the first chamber; Determine, in a comparison table of natural gas compression factors, a third compression factor corresponding to the third temperature value and the pre-adsorption pressure value; The pressure value before adsorption, the third temperature value, the third compression factor, the reference cylinder volume and the second part of the pipeline volume are introduced into the real gas state equation to calculate the amount of natural gas in the first chamber before the shale sample adsorbs natural gas; Before the shale sample adsorbs natural gas, the amount of natural gas in the first chamber is: ; Wherein, the above i is the number of adsorption control actions, i is a positive integer greater than 0; is the pre-adsorption pressure value of the shale sample before the adsorption of natural gas in the i-th adsorption control action; the above V t is the sum of the reference cylinder volume and the second part pipeline volume; is the third temperature value in the first chamber; For natural gas in P i and the third compression factor under T0 conditions; the above R is a thermodynamic constant; Obtaining the amount of natural gas in the free space of the second chamber after the shale sample absorbs the natural gas in the i-1th adsorption control action, and the amount of natural gas in the first part of the pipeline after the shale sample absorbs the natural gas; Calculate the first substance amount corresponding to the i-th adsorption control action according to the amount of the natural gas substance in the first chamber before the shale sample adsorbs the natural gas in the i-th adsorption control action, the amount of the natural gas substance in the free space of the second chamber after the shale sample adsorbs the natural gas in the i-1-th adsorption control action, and the amount of the natural gas substance in the first part of the pipeline after the shale sample adsorbs the natural gas in the i-1-th adsorption control action; The amount of the substance in the natural gas corresponding to the i-th adsorption control action, the first amount of substance, is: ; in Above is the pre-adsorption pressure value of the shale sample before the adsorption of natural gas in the i-th adsorption control action; the above V t is the sum of the reference cylinder volume and the second part pipeline volume; is the third temperature value in the first chamber; For natural gas in P i and the third compression factor under T0 conditions; the above is the amount of natural gas in the free space of the second chamber after the shale sample adsorbs natural gas in the i-1th adsorption control action; is the amount of natural gas in the first part of the pipeline after the shale sample adsorbs natural gas in the i-1th adsorption control action; The step of obtaining the amount of the second substance corresponding to each adsorption control action specifically includes: For the i-th adsorption control action, the natural gas in the reference cylinder is controlled to diffuse to the sample cylinder through the first pipeline, so that the natural gas is adsorbed into the pore space of the shale sample, and the pressure value after adsorption is obtained by using the pressure sensor; acquiring a fourth temperature value of the second chamber; In the natural gas compression factor comparison table, determining a fourth compression factor corresponding to the third temperature value and the post-adsorption pressure value, and a fifth compression factor corresponding to the fourth temperature value and the post-adsorption pressure value; The post-adsorption pressure value, the reference cylinder volume, the second part pipeline volume, the third temperature value and the fourth compression factor are introduced into the real gas state equation to calculate the amount of the natural gas in the first chamber after the shale sample adsorbs the natural gas; After the shale sample adsorbs the natural gas, the amount of the natural gas in the first chamber is: ; Among them, the above is the post-adsorption pressure value of the shale sample after natural gas adsorption in the i-th adsorption control action; the above V t is the sum of the reference cylinder volume and the second part pipeline volume; For natural gas and The fourth compression factor under the conditions; the above R is a thermodynamic constant; the above is a third temperature value in the first chamber; Importing the post-adsorption pressure value, the third part pipeline volume, the sample cylinder volume, the skeleton volume, the fifth compression factor and the fourth temperature value into the real gas state equation to calculate the amount of natural gas in the free space of the second chamber after the shale sample adsorbs the natural gas; After the shale sample adsorbs the natural gas, the amount of the natural gas in the free space of the second chamber is: ; Among them, the above is the post-adsorption pressure value of the shale sample after natural gas adsorption in the i-th adsorption control action; the above V f is the free space volume in the second chamber excluding the skeleton volume of the shale sample; For natural gas and The fifth compression factor under the conditions; is a fourth temperature value of the second chamber; Constructing a temperature variation function within the first portion of the pipeline; The temperature change function is: ; Wherein, the above l is the length from the left end point in the first part of the pipeline to any pipeline position; is the temperature value at l; the above L l is the length of the first part of the pipeline; is the fourth temperature value of the second chamber; is a third temperature value in the first chamber; Integrating the temperature change function, and calculating a fitting temperature in the first portion of the pipeline according to the integrated temperature change function and the length of the first portion of the pipeline; The fitted temperature in the first portion of the pipeline is: ; In the natural gas compression factor comparison table, determining the sixth compression factor corresponding to the fitting temperature and the post-adsorption pressure value; Importing the post-adsorption pressure value, the first portion of the pipeline volume, the sixth compressibility factor and the fitting temperature into a real gas state equation to construct a fourth equation; The fourth equation is: ; Among them, the above is the post-adsorption pressure value of the shale sample after natural gas adsorption in the i-th adsorption control action; the above V l is the volume of the first part of the pipeline; For natural gas and The fourth compression factor under the conditions; is the amount of natural gas in the first part of the pipeline after the shale sample adsorbs natural gas in the i-th adsorption control action; is the fitting temperature in the first part of the pipeline; Calculating the amount of the natural gas in the first portion of the pipeline after the shale sample adsorbs the natural gas using the fitted temperature in the first portion of the pipeline and the fourth equation; After the shale sample absorbs the natural gas, the amount of the natural gas in the first part of the pipeline is: ; Among them, the above For natural gas , The sixth compression factor under the conditions; Calculating the second substance amount corresponding to the i-th adsorption control action according to the amount of the natural gas substance in the first chamber, the amount of the natural gas substance in the free space of the second chamber, and the amount of the natural gas substance in the first portion of the pipeline after the shale sample adsorbs the natural gas; The amount of the second substance corresponding to the i-th adsorption control action is: 。 2. The method according to claim 1, characterized in that The shale gas adsorption measurement system further includes: a first pipeline and a pressure sensor, the first pipeline is used to connect the reference cylinder and the sample cylinder, the pressure sensor is arranged in the first chamber, and before performing the preset number of adsorption control actions, the method further includes: Obtaining a sample diameter, a sample height, and a sample mass of the shale sample; Performing a vacuum process on the reference cylinder, the sample cylinder and the first pipeline; Controlling the temperatures in the first chamber and the second chamber according to the first preset temperature value, and acquiring a first temperature value of the first chamber and a second temperature value of the second chamber; Filling the reference cylinder with inert gas, and obtaining the pressure value before adsorption using the pressure sensor; Controlling the inert gas in the reference cylinder to diffuse into the sample cylinder so that the inert gas is adsorbed into the pore space of the shale sample, and using the pressure sensor to obtain a pressure value after adsorption; In the inert gas compressibility factor comparison table, determine the first compressibility factor corresponding to the first temperature value and the pressure value before adsorption, and the second compressibility factor corresponding to the second temperature value and the pressure value after adsorption; Acquire a plurality of volume parameters of the shale gas adsorption measurement system, wherein the plurality of volume parameters include: a reference cylinder volume of the reference cylinder, a first portion of the pipeline volume of the first pipeline between the first chamber and the second chamber, a second portion of the pipeline volume of the first pipeline contained in the first chamber, and a third portion of the pipeline volume of the first pipeline contained in the second chamber; Importing the pre-adsorption pressure value, the reference cylinder volume, the second portion of the pipeline volume, the first compressibility factor and the first temperature value into a real gas state equation to generate a first equation; The first equation is: ; Wherein, the above P0 is the pressure value before adsorption; the above V t is the sum of the reference cylinder volume and the second part pipeline volume; the above Z0 is the first compression factor of the inert gas under T0 and P0 conditions; the above n0 is the amount of the inert gas; the above R is a thermodynamic constant; the above T0 is the first temperature value; Importing the post-adsorption pressure value, the plurality of volume parameters, the second compressibility factor and the second temperature value into a real gas state equation to generate a second equation; The second equation is: ; Among them, the above is the pressure value after adsorption; the above V l is the volume of the first part of the pipeline; the above V f is the free space volume in the second chamber excluding the skeleton volume of the shale sample; For inert gas , The second compression factor under the conditions; is the second temperature value; Calculating the skeleton volume, skeleton density and porosity of the shale sample using the first equation and the second equation; The inert gas in the reference cylinder, the sample cylinder and the first pipeline is evacuated.

3. The method according to claim 2, characterized in that The step of calculating the skeleton volume, the skeleton density and the porosity of the shale sample by using the first equation and the second equation specifically includes: Combining the first equation and the second equation to construct a third equation corresponding to the free space volume of the second chamber; The third-party programs are: ; Constructing a first mapping relationship between the free space volume of the second chamber and the volume of the sample cylinder, the skeleton volume, and the volume of the third portion of the pipeline; The first mapping relationship is: ; Among them, the above V a is the sum of the volume of the sample cylinder and the volume of the third part of the pipeline; the above V s is the skeleton volume; Calculating the skeleton volume using the third equation and the first mapping relationship; The skeleton volume is: ; constructing a second mapping relationship between the porosity and the skeleton volume and sample data of the shale sample; The second mapping relationship is: ; Among them, the above is the porosity; is the sample diameter of the shale sample; the above L is the sample height of the shale sample; Calculating the porosity using the second mapping relationship and the skeleton volume; The porosity is: ; constructing a third mapping relationship between the skeleton density, the sample mass of the shale sample and the skeleton volume; The third mapping relationship is: ; Wherein, the above M is the sample mass of the shale sample; Calculating the skeleton density by using the third mapping relationship and the skeleton volume; The skeleton density is: 。 4. A device for implementing the shale gas adsorption measurement method of claim 1, characterized in that: Applicable to a shale gas adsorption measurement system, the shale gas adsorption measurement system comprises a first chamber, a second chamber, a reference cylinder and a sample cylinder, wherein the reference cylinder is arranged in the first chamber, the sample cylinder is arranged in the second chamber, a shale sample is placed in the sample cylinder, and the device comprises: a control module, configured to control the temperature in the first chamber according to a first preset temperature value, and control the temperature in the second chamber according to a second preset temperature value, wherein the first preset temperature value is less than the second preset temperature value; An execution module is used to execute a preset number of adsorption control actions; an acquisition module is used to acquire a first mass of substance and a second mass of substance corresponding to each adsorption control action; the adsorption control action includes: introducing natural gas into the reference cylinder according to a preset pressure value, and controlling the natural gas in the reference cylinder to diffuse into the sample cylinder so that the natural gas is adsorbed into the pore space of the shale sample; the first mass of substance is the amount of natural gas in the shale gas adsorption measurement system before the shale sample adsorbs natural gas, and the second mass of substance is the amount of natural gas in the shale gas adsorption measurement system after the shale sample adsorbs natural gas; The determination module is used to determine the gas adsorption amount of the shale sample corresponding to each adsorption control action according to the first substance amount and the second substance amount corresponding to each adsorption control action.

5. A shale gas adsorption measurement system, characterized in that: include: First chamber; Second chamber; A reference cylinder is disposed in the first chamber, and the reference cylinder includes a first air inlet and an air outlet; A sample cylinder, disposed in the second chamber, the sample cylinder comprising a second air inlet, the second air inlet being communicated with the air outlet of the reference cylinder; A pressure sensor is disposed in the first chamber, and is used to detect a pressure value of the shale gas adsorption measurement system; A memory storing programs or instructions; A processor is connected to the memory, and when the processor executes the program or instruction, the shale gas adsorption measurement method according to any one of claims 1 to 3 is implemented.

6. The shale gas adsorption measurement system according to claim 5, characterized in that: Also includes: A vacuum pumping component, used for vacuuming the shale gas adsorption measurement system, wherein the vacuum pumping component comprises a vacuuming end, and the vacuuming end is connected to the first air inlet of the reference cylinder; An inert gas source, used to introduce inert gas into the reference cylinder and the sample cylinder, the inert gas source comprising a first gas outlet end, the first gas outlet end being connected to the gas inlet of the reference cylinder; A natural gas source, used to introduce natural gas into the reference cylinder and the sample cylinder, the natural gas source comprising a second gas outlet, the second gas outlet being connected to the first gas inlet of the reference cylinder; a first pipeline, one end of which is connected to the gas outlet of the reference cylinder, and the other end of which is connected to the second gas inlet of the sample cylinder; A second pipeline, one end of which is connected to the vacuum end of the vacuum pumping assembly, the first gas outlet end of the inert gas source and the second gas outlet end of the natural gas source, and the other end is connected to the first gas inlet of the reference cylinder.

7. The shale gas adsorption measurement system according to claim 6, characterized in that: Also includes: A first temperature sensor, disposed in the first chamber, for detecting a temperature value of the first chamber; A second temperature sensor, disposed in the second chamber, for detecting a temperature value of the second chamber; a first valve, disposed on the first pipeline; The second valve is arranged on the second pipeline.

8. A readable storage medium, characterized in that: The readable storage medium stores a program or instruction, and when the program or instruction is executed by a processor, the steps of the shale gas adsorption measurement method according to any one of claims 1 to 3 are implemented.