A method for treating high-viscosity sludge

By combining microwave treatment, ultrasonic treatment and high-temperature anaerobic digestion, the problem of poor sludge dehydration is solved, efficient sludge treatment is achieved, sludge volume and heavy metal risks are reduced, and it is suitable for industrial large-scale production.

CN118545880BActive Publication Date: 2024-10-22LINYI ENVIRONMENTAL PROTECTION SCI RES INST CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411019310.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-10-22
Estimated Expiration
2044-07-29

AI Technical Summary

Technical Problem

Existing sludge treatment methods cannot effectively improve the dehydration of sludge, making it difficult for high-viscosity sludge to meet disposal standards, posing risks of environmental pollution and health threats.

Method used

After microwave treatment, polymer coagulant and magnetic nanoscale catalyst particles are added, followed by ultrasonic treatment and high-temperature anaerobic digestion, and finally a plate and frame filter press is used for deep dehydration.

Benefits of technology

It significantly reduces the organic content of sludge, eliminates pathogenic bacteria, solidifies heavy metals, improves dehydration performance, reduces the amount of sludge, increases the solid content of sludge, and achieves reduction, stabilization and resource treatment.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for treating high-viscosity sludge, wherein the method mainly adopts microwave treatment, adds a polymer coagulant; then performs ultrasonic treatment and adds magnetic nano-scale catalyst particles; performs high-temperature anaerobic digestion after heat treatment; and performs deep dehydration. The organic matter content of the sludge treated by the method of the invention is significantly reduced, pathogens are basically eliminated, heavy metals are solidified, and the dehydration performance is significantly improved, which can significantly reduce the COD value of the raw water and reduce the amount of sludge; while strengthening the efficiency of anaerobic digestion, it can reduce the operating cost; it realizes reduction, stabilization, harmlessness and resource utilization, which is beneficial to the subsequent sludge disposal, and the process operation is simple, safe and environmentally friendly, and suitable for large-scale industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for treating sludge, and more particularly to a method for treating high-viscosity sludge. Background Art

[0002] Sludge is an inevitable byproduct of wastewater resource utilization. Studies have shown that sludge is rich in elements such as nitrogen and phosphorus, making it a valuable resource. Especially in today's resource-constrained world, the scientific reuse of resources is extremely urgent. However, in addition to the aforementioned substances, sludge also contains many toxic and harmful substances, such as heavy metals and parasite eggs. Direct use of sludge without proper treatment can have significant impacts on the environment and humans.

[0003] The main hazards are as follows:

[0004] (1) Direct landfill treatment is currently the mainstream method of sludge treatment. Direct landfill will occupy land resources. At the same time, since the sludge contains many heavy metal elements, it may cause groundwater pollution.

[0005] (2) Parasite eggs and pathogenic microorganisms in sewage sludge can cause various diseases such as acute gastroenteritis, hepatitis, and sepsis in humans through direct or indirect contact with humans.

[0006] (3) Although sewage sludge is rich in nitrogen, phosphorus and other elements, if applied to fields in large quantities, it will destroy the soil structure and lose soil fertility. In addition, sewage sludge also contains heavy metals. Since heavy metals are very stable in nature, they can be enriched through the food chain and eventually enter the human body, posing a threat to human health and safety.

[0007] Currently, sludge is mainly classified according to the sewage treatment method, namely: primary sludge, excess sludge, concentrated sludge and digested sludge. Currently, most municipal sewage treatment plants use activated sludge and biofilm as the main treatment process. The main types and properties of sludge produced are as follows:

[0008] (1) Primary sludge refers to the sludge produced in the primary treatment process, namely the primary sedimentation tank. Primary sludge has a moisture content of up to 98% and contains a large amount of particulate matter, such as gravel, food residues, and textiles. It is usually a black-gray paste with an unpleasant odor.

[0009] (2) Excess sludge is the sludge produced by the biological water treatment process. Excess sludge is mainly composed of aerobic microorganisms and organic and inorganic substances attached to the microbial community. It does not contain large particles and is brown and flocculent. The moisture content of excess sludge is 95-99%. In addition, excess sludge also contains pathogens, heavy metals and other toxic and harmful substances. If not handled properly, harmful pollutants can enter the environment through migration and transformation, causing environmental pollution.

[0010] (3) The mixed sludge composed of the unreturned excess sludge and the primary sedimentation tank sludge enters the thickening tank to produce concentrated sludge. The sludge is thickened mainly by reducing the sludge moisture content and reducing the sludge volume, so that the sludge moisture content reaches 80-85%. Therefore, concentrated sludge has the characteristics of high sludge concentration and low moisture content.

[0011] (4) The sludge produced after the residual sludge is digested (aerobic or anaerobic digestion) is digested sludge. The sludge after aerobic digestion is brown to dark brown flocs with a water content of about 96-98%. At the same time, the sludge after aerobic digestion is easier to dehydrate. The sludge after anaerobic digestion is dark brown or black viscous liquid with a foul odor and a water content of about 90-97%. After anaerobic digestion, the morphological characteristics and chemical composition of the sludge flocs have changed to a certain extent. The proteins and polysaccharides in the hydrolyzed EPS (Extracellular Polymeric Substances) will be released into the sludge and converted into methane, carbon dioxide, humic acid, etc. The degradation of EPS will also reduce the sludge particle size. It is reported that the increase in the concentration of organic matter (protein, polysaccharides, etc.) in the sludge EPS may lead to poor sludge dewatering. Therefore, anaerobic digestion causes the release of organic matter, which deteriorates the dewatering and filterability of the sludge.

[0012] Currently, there are three main sludge treatment and disposal technologies: sanitary landfill, sludge incineration, and agricultural utilization.

[0013] (1) Sanitary landfill: Sanitary landfill technology for sewage sludge was the most commonly used sludge disposal method in the early days. This technology mainly involves dehydrating the sludge and then transporting it directly to a landfill for disposal. It is divided into separate landfill and mixed landfill. Mixed landfill is to mix domestic waste with sludge and then landfill it for disposal. Due to land resource limitations and the potential pollution of leachate to soil and groundwater, this technology has been restricted and its share in sludge treatment and disposal technologies has been decreasing recently.

[0014] (2) Incineration: Sludge incineration technology refers to the technology of high-temperature heat treatment of sludge under oxygen supply conditions. It is usually used to dispose of toxic and hazardous residual sludge. The sludge produced by urban sewage usually contains a large amount of organic matter and cellulose. Direct incineration of sludge after dehydration can effectively carbonize organic matter, kill pathogens and parasite eggs, and reduce sludge volume. It has gradually become the mainstream sludge treatment and disposal technology.

[0015] (3) Agricultural utilization: Agricultural utilization is also called land utilization. Land utilization of sewage sludge refers to the application of sewage sludge to farmland, orchards, vegetable plots, woodlands, municipal greening, etc. Sludge is rich in beneficial components such as organic matter, nitrogen, phosphorus, and potassium. It is also water-absorbent and sticky, which can improve the physical and chemical properties of the soil, promote soil agglomeration, increase the water retention capacity of aggregates, and reduce soil erosion.

[0016] In summary, my country currently produces a large amount of sludge. Reducing sludge production is crucial. Therefore, there is an urgent need to improve sludge dewaterability and thereby fundamentally reduce sludge production. Sludge treatment primarily involves sludge conditioning, concentration, and dewatering. After concentration, the sludge moisture content remains above 90%, while after dewatering, the moisture content remains around 80%, resulting in high-viscosity sludge that does not meet the standards for subsequent sludge disposal. Therefore, sludge conditioning is necessary before dewatering to improve its dewaterability. Summary of the Invention

[0017] The following is a summary of some aspects of the present invention and is not intended to limit the present invention. In the event of a discrepancy between the disclosure of this specification and a reference, the disclosure of this specification shall prevail.

[0018] The purpose of the present invention is to overcome the disadvantages of the existing sludge treatment methods that the treatment effect is not ideal and to provide a method for treating high-viscosity sludge.

[0019] A method for treating high-viscosity sludge comprises the following steps:

[0020] Step 1: microwave the sludge, then add a polymer coagulant, stir and let it stand;

[0021] Step 2, subjecting the sludge treated in step 1 to ultrasonic treatment, and then adding magnetic nano-scale catalyst particles;

[0022] Step 3, heat-treating the sludge treated in step 2, followed by high-temperature anaerobic digestion;

[0023] Step 4: Deeply dehydrate the sludge treated in step 3 using a plate and frame filter press.

[0024] Furthermore, in the microwave treatment in step 1, the microwave power is 300-600 W and the microwave time is 20-50 s.

[0025] Furthermore, in the microwave treatment in step 1, the microwave power is 500 W and the microwave time is 30 s.

[0026] Furthermore, the polymer coagulant in step 1 is a copolymer of polyferric chloride and polyacrylamide.

[0027] Preferably, the amount of the high molecular weight coagulant copolymer is 0.5-2% of the weight of the sludge.

[0028] More preferably, the amount of the high molecular weight coagulant copolymer is 0.7% of the weight of the sludge.

[0029] Furthermore, the polymer coagulant in step 1 is a copolymer of polyferric chloride and polyacrylamide.

[0030] Preferably, the mass ratio of polyferric chloride to polyacrylamide in the polymer coagulant copolymer is 5:(2-5).

[0031] More preferably, the mass ratio of polyferric chloride to polyacrylamide in the polymer coagulant copolymer is 5:2.

[0032] Furthermore, in the ultrasonic treatment in step 2, the frequency of the ultrasonic treatment is 20-40 kHz, and the ultrasonic treatment time is 5-10 min.

[0033] Furthermore, in the ultrasonic treatment in step 2, the frequency of the ultrasonic treatment is 30 kHz and the ultrasonic treatment time is 5 min.

[0034] Furthermore, the amount of the magnetic nano-scale catalyst particles in step 2 is 0.5-3% of the weight of the sludge.

[0035] Preferably, the amount of the magnetic nano-scale catalyst particles is 2% of the weight of the sludge.

[0036] Furthermore, the magnetic nano-scale catalyst particles in step 2 contain, in terms of metal elements, 80-90 wt % of a metallic iron component and 5-20 wt % of a metallic aluminum component.

[0037] Preferably, the magnetic nano-scale catalyst particles in step 2 contain 85% by weight of metallic iron components and 15% by weight of metallic aluminum components, calculated as metal elements.

[0038] Furthermore, the preparation method of the above-mentioned magnetic nano-scale catalyst particles is:

[0039] Ferric nitrate and aluminum nitrate were dissolved in distilled water, and the resulting solution was placed in a 30°C water bath and stirred at 350 rpm. A 30% by weight sodium hydroxide solution was then slowly added dropwise to adjust the pH to between 7 and 8, and the mixture was allowed to age for 5 hours. The resulting reaction product was then filtered, and the filter cake was washed twice with distilled water, and the filtration was repeated. The washed filter cake was dried in a 110°C oven for 10 hours, ground, and then calcined in a 550°C muffle furnace for 5 hours. Finally, it was washed with water to obtain amorphous ultrafine particles. The catalyst particles contained 85% by weight of iron and 15% by weight of aluminum, calculated as metal elements.

[0040] Furthermore, in step 3, the heat treatment temperature is 45-50°C, and the heat treatment time is 0.5-1h; in step 3, the high-temperature anaerobic digestion is carried out, the digestion temperature is controlled at 50-55°C, the pH is controlled at 6.5-7, and the digestion time is 8-24h.

[0041] Preferably, the heat treatment temperature in step 3 is 47° C., and the heat treatment time is 0.5 h. In step 3, the high-temperature anaerobic digestion is carried out, the digestion temperature is controlled at 52° C., the pH is controlled at 6.7, and the digestion time is 10 h.

[0042] Furthermore, in step 4, a plate and frame filter press is used for deep dehydration, wherein the mud inlet pressure is 0.1-0.3 MPa, the plate and frame pressure is controlled to be 1.0-1.5 MPa and the pressure is maintained for 15-20 minutes.

[0043] Preferably, in step 4, a plate and frame filter press is used for deep dehydration, wherein the mud inlet pressure is 0.2 MPa, the plate and frame pressure is controlled to be 1.2 MPa and the pressure is maintained for 15 minutes.

[0044] Beneficial technical effects of the present invention

[0045] Compared with the prior art, the technical solution of the present invention has the following advantages:

[0046] 1. The present invention pre-treats the sludge with microwaves and then adds a polymer coagulant, wherein the polymer coagulant is a copolymer.

[0047] By modifying the polymer coagulant, the netting effect on particles in the water is improved. After ultrasonic treatment, magnetic nano-scale catalyst particles are added. The nano-scale structural modification of the catalyst particles increases the adsorption force while also increasing the surface contact area, making the catalytic effect significant. Through the above sludge treatment steps, especially the treatment of high-viscosity sludge, the synergistic effect between the steps makes the organic matter content of the treated sludge significantly reduced, the sludge has a disinfection effect, pathogens are basically eliminated, heavy metals are solidified, the dehydration performance is significantly improved, the COD value of the raw water is reduced, the sludge volume is reduced, and the sludge solid content is increased.

[0048] 2. The present invention can greatly shorten the anaerobic digestion reaction time of sludge through early pretreatment, increase the biogas production during the anaerobic digestion process, enhance the anaerobic digestion efficiency, and the biogas generated by high-temperature anaerobic digestion of sludge can be used as energy for heat treatment, which can reduce operating costs and save energy and reduce consumption.

[0049] 3. The solid content of the treated sludge is greatly improved, and the reduction effect is obvious, achieving reduction, stabilization, harmlessness and resource utilization, which is beneficial to the subsequent sludge disposal. The process operation is simple, safe and environmentally friendly, and suitable for large-scale industrial production. DETAILED DESCRIPTION

[0050] Unless otherwise indicated or there is an obvious conflict in the context, all technical and scientific terms used herein have the same meaning as commonly understood by those of ordinary skill in the art to which the invention belongs. In the event of a conflict, the definitions provided herein shall prevail. When a trade name appears in this article, it is intended to refer to the corresponding commercial product or its active ingredient. All patents, published patent applications and publications cited herein are incorporated herein by reference.

[0051] 1. In the following examples, the COD removal rate of sludge was calculated according to the following formula:

[0052] COD removal rate = (COD of untreated sludge - COD of treated sludge) / COD of untreated sludge multiplied by 100%;

[0053] Among them, the COD of untreated sludge and the COD of treated sludge were both measured according to the potassium dichromate titration method.

[0054] 2. In the following examples, the solid content of the sludge was calculated according to the following formula:

[0055] Sludge solid content = dry matter weight divided by the initial sludge sample weight, multiplied by 100%;

[0056] 3. Preparation of nano-scale catalyst particles:

[0057] Ferric nitrate and aluminum nitrate were dissolved in distilled water, and the resulting solution was placed in a 30°C water bath and stirred at 350 rpm. A 30% by weight sodium hydroxide solution was then slowly added dropwise to adjust the pH to between 7 and 8, and the mixture was allowed to age for 5 hours. The resulting reaction product was then filtered, and the filter cake was washed twice with distilled water, and the filtration was repeated. The washed filter cake was dried in a 110°C oven for 10 hours, ground, and then calcined in a 550°C muffle furnace for 5 hours. Finally, it was washed with water to obtain amorphous ultrafine particles. The catalyst particles contained 85% by weight of iron and 15% by weight of aluminum, calculated as metal elements.

[0058] Example 1:

[0059] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0060] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0061] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0062] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.67%, and the solid content of the sludge after dehydration is 78%.

[0063] Example 2:

[0064] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 300W and a microwave time of 20s. For every 100 parts by weight of the sludge, add 0.5 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0065] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0066] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0067] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.52%, and the solid content of the sludge after dehydration is 71%.

[0068] Example 3:

[0069] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0070] 2. The sludge from step 1 was ultrasonically treated at a frequency of 20 kHz for 5 minutes. 0.5 parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0071] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0072] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.55%, and the solid content of the sludge after dehydration is 70%.

[0073] Example 4:

[0074] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0075] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0076] 3. Then it enters the heat treatment device, the heat treatment temperature is 45℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 50℃, the pH is controlled at 6.5, and the digestion time is 8h;

[0077] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.59%, and the solid content of the sludge after dehydration is 73%.

[0078] Example 5:

[0079] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0080] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0081] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0082] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.1 MPa, the plate and frame pressure is controlled to 1.0 MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.60%, and the solid content of the sludge after dehydration is 71%.

[0083] Example 6:

[0084] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 600W and a microwave time of 50s. For every 100 parts by weight of the sludge, add 2 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2). Stir for 5 minutes and then let it stand.

[0085] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0086] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0087] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.56%, and the solid content of the sludge after dehydration is 74%.

[0088] Example 7:

[0089] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0090] 2. The sludge from step 1 was ultrasonically treated at a frequency of 40 kHz for 10 minutes. Three parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0091] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0092] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.58%, and the solid content of the sludge after dehydration is 72%.

[0093] Example 8:

[0094] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0095] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0096] 3. Then it enters the heat treatment device, the heat treatment temperature is 50℃, the heat treatment time is 1h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 55℃, the pH is controlled at 7, and the digestion time is 24h;

[0097] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.51%, and the solid content of the sludge after dehydration is 71%.

[0098] Example 9:

[0099] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0100] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0101] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0102] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.3MPa, the plate and frame pressure is controlled to 1.5MPa and the pressure is maintained for 20 minutes. The COD removal rate of the sludge is 99.55%, and the solid content of the sludge after dehydration is 73%.

[0103] Example 10:

[0104] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 200W and a microwave time of 15s. For every 100 parts by weight of the sludge, add 0.3 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:1), stir for 5 minutes, and then let it stand.

[0105] 2. The sludge from step 1 was ultrasonically treated at a frequency of 15 kHz for 2 minutes. 0.3 parts by weight of magnetic nano-scale catalyst particles (containing 70% by weight of metallic iron and 30% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0106] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0107] 4. A high-pressure diaphragm filter press was used to deeply dehydrate the digested sludge. The sludge inlet pressure was 0.2 MPa, the plate and frame pressure was controlled to 1.2 MPa and the pressure was maintained for 15 minutes. The COD removal rate of the sludge was 93.67%, and the solid content of the sludge after dehydration was 48%.

[0108] Example 11:

[0109] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0110] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0111] 3. Then it enters the heat treatment device, the heat treatment temperature is 40℃, the heat treatment time is 0.2h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 45℃, the pH is controlled at 6.0, and the digestion time is 6h;

[0112] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.05MPa, the plate and frame pressure is controlled to 0.8MPa and the pressure is maintained for 10 minutes. The COD removal rate of the sludge is 95.37%, and the solid content of the sludge after dehydration is 45%.

[0113] Example 12:

[0114] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 700W and a microwave time of 60s. For every 100 parts by weight of the sludge, add 3 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:7), stir for 5 minutes, and then let it stand.

[0115] 2. The sludge from step 1 was ultrasonically treated at a frequency of 50 kHz for 15 minutes. Four parts by weight of magnetic nano-scale catalyst particles (containing 96% by weight of metallic iron and 4% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0116] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0117] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 95.62%, and the solid content of the sludge after dehydration is 43%.

[0118] Example 13:

[0119] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0120] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0121] 3. Then it enters the heat treatment device, the heat treatment temperature is 55℃, the heat treatment time is 2h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 60℃, the pH is controlled at 7.5, and the digestion time is 26h;

[0122] 4. A high-pressure diaphragm filter press was used to deeply dehydrate the digested sludge. The sludge inlet pressure was 0.5 MPa, the plate and frame pressure was controlled to 2.0 MPa and the pressure was maintained for 30 minutes. The COD removal rate of the sludge was 94.71%, and the solid content of the sludge after dehydration was 46%.

[0123] Example 14:

[0124] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 400W and a microwave time of 40s. For every 100 parts by weight of the sludge, add 1.0 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:3), stir for 5 minutes, and then let it stand.

[0125] 2. The sludge from step 1 was ultrasonically treated at a frequency of 25 kHz for 7 minutes. 2.5 parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0126] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0127] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.2MPa and the pressure is maintained for 15 minutes. The COD removal rate of the sludge is 99.54%, and the solid content of the sludge after dehydration is 74%.

[0128] Example 15:

[0129] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0130] 2. The sludge from step 1 was ultrasonically treated at a frequency of 30 kHz for 5 minutes. Two parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0131] 3. Then it enters the heat treatment device, the heat treatment temperature is 46℃, the heat treatment time is 0.7h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 54℃, the pH is controlled at 6.8, and the digestion time is 12h;

[0132] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.4MPa and the pressure is maintained for 18 minutes. The COD removal rate of the sludge is 99.57%, and the solid content of the sludge after dehydration is 75%.

[0133] Example 16:

[0134] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 400W and a microwave time of 40s. Add 1.0 part by weight of a polymer coagulant polyacrylamide to 100 parts by weight of the sludge, stir for 5 minutes and then let it stand;

[0135] 2. The sludge from step 1 was ultrasonically treated at a frequency of 25 kHz for 7 minutes. 2.5 parts by weight of magnetic nano-scale catalyst particles (containing 85% by weight of metallic iron and 15% by weight of metallic aluminum) were added to 100 parts by weight of the sludge.

[0136] 3. Then it enters the heat treatment device, the heat treatment temperature is 47℃, the heat treatment time is 0.5h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 52℃, the pH is controlled at 6.7, and the digestion time is 10h;

[0137] 4. A high-pressure diaphragm filter press was used to deeply dehydrate the digested sludge. The sludge inlet pressure was 0.2 MPa, the plate and frame pressure was controlled to 1.2 MPa and the pressure was maintained for 15 minutes. The COD removal rate of the sludge was 85.54%, and the solid content of the sludge after dehydration was 52%.

[0138] Example 17:

[0139] 1. Take high-viscosity sludge and microwave it in a microwave treatment device with a microwave power of 500W and a microwave time of 30s. For every 100 parts by weight of the sludge, add 0.7 parts by weight of a polymer coagulant copolymer (the mass ratio of polyferric chloride to polyacrylamide is 5:2), stir for 5 minutes, and then let it stand.

[0140] 2. The sludge from step 1 was passed through an ultrasonic treatment device at a frequency of 30 kHz for 5 min.

[0141] 3. Then it enters the heat treatment device, the heat treatment temperature is 46℃, the heat treatment time is 0.7h; the treated sludge enters the high-temperature anaerobic digester, the digestion temperature is 54℃, the pH is controlled at 6.8, and the digestion time is 12h;

[0142] 4. A high-pressure diaphragm filter press is used to deeply dehydrate the digested sludge. The sludge inlet pressure is 0.2MPa, the plate and frame pressure is controlled to 1.4MPa and the pressure is maintained for 18 minutes. The COD removal rate of the sludge is 97.57%, and the solid content of the sludge after dehydration is 49%.

[0143] The above is a description of a specific embodiment of the present invention. It should be understood that the present invention is not limited to the above embodiment, and the above embodiment and description are only for illustrating the principle of the present invention.

[0144] Those skilled in the art may make various non-substantial changes and improvements to the present invention without departing from the concept of the present invention, and all of these fall within the scope of protection claimed by the present invention.

Claims

1. A method for treating high-viscosity sludge, characterized in that: The steps include: Step 1, subjecting the sludge to microwave treatment, adding a polymer coagulant, stirring and then standing; Step 2, subjecting the sludge treated in step 1 to ultrasonic treatment, and then adding magnetic nano-scale catalyst particles; Step 3, heat treating the sludge treated in step 2, followed by high temperature anaerobic digestion; Step 4, deep dehydrating the sludge treated in step 3 using a plate and frame filter press; Wherein, the microwave power of the microwave treatment in step 1 is 300-600W, the microwave time is 20-50s, the dosage of the polymer coagulant is 0.5-2% of the weight of the sludge, the polymer coagulant is a copolymer of polyferric chloride and polyacrylamide, and the mass ratio of polyferric chloride to polyacrylamide is 5:(2-5); The frequency of the ultrasonic treatment in step 2 is 20-40kHz, the ultrasonic treatment time is 5-10min, the amount of the magnetic nano-scale catalyst particles is 0.5-3% of the weight of the sludge, and the magnetic nano-scale catalyst particles contain 80-90% by weight of metal iron components and 5-20% by weight of metal aluminum components in terms of metal elements; The heat treatment temperature in step 3 is 45-50°C, the heat treatment time is 0.5-1h, the high temperature anaerobic digestion is controlled at a digestion temperature of 50-55°C, the pH is controlled at 6.5-7, and the digestion time is 8-24h; In step 4, when using a plate and frame filter press for deep dehydration, the mud inlet pressure is 0.1-0.3 MPa, the plate and frame pressure is controlled to be 1.0-1.5 MPa and the pressure is maintained for 15-20 minutes.

Citation Information

Cited By

  • Dehydration method of refined sludge