A method for preparing a SGT device and an epitaxial wafer

By depositing a composite layer on the N-type substrate in the SGT MOSFET device and adjusting the electric field intensity curve distribution, the problem of performance degradation of the gate oxide layer under long-term high field intensity conditions is solved and the reliability of the device is improved.

CN118553763BActive Publication Date: 2024-10-18JIANGXI SARUI MICROELECTRONICS TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410994244.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-10-18
Estimated Expiration
2044-07-24

AI Technical Summary

Technical Problem

Because the gate oxide layer of existing SGT MOSFET devices is exposed to high field strength conditions for a long time, performance declines, leakage increases, and even breakdown, seriously affecting the reliability of the device.

Method used

A composite layer is deposited on the N-type substrate, including a first sub-layer, a second sub-layer, a third sub-layer and a fourth sub-layer deposited in sequence, wherein the first sub-layer, the second sub-layer and the fourth sub-layer are The epitaxial layer is uniformly doped with phosphorus, and the third sub-layer is an epitaxial layer that is uniformly doped with boron. The four-layer epitaxial layer structure with different doping concentrations adjusts the electric field intensity curve distribution and reduces the electric field intensity that the gate oxide layer bears.

Benefits of technology

It effectively reduces the electric field intensity at the PN junction formed by the well region of the high-voltage SGT device and EPI, prevents the performance degradation of the gate oxide layer, and improves the reliability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118553763B_ABST
    Figure CN118553763B_ABST
Patent Text Reader

Abstract

The present invention provides a method for preparing an SGT device and an epitaxial wafer, wherein a composite layer is deposited on an N-type substrate, wherein the composite layer includes a first sublayer, a second sublayer, a third sublayer and a fourth sublayer deposited in sequence; wherein the first sublayer, the second sublayer and the fourth sublayer are epitaxial layers uniformly doped with phosphorus, and the third sublayer is an epitaxial layer uniformly doped with boron, and the thickness of the third sublayer is the smallest. Specifically, a four-layer epitaxial method with different doping concentrations is adopted, and the phosphorus-doped epitaxial layer and the boron-doped epitaxial layer are interspersed, which effectively adjusts the distribution of the electric field strength curve, greatly reduces the electric field strength at the PN junction formed by the high-voltage SGT well region and the EPI, thereby reducing the electric field strength borne by the adjacent gate oxide layer, preventing the performance degradation caused by the gate oxide layer being in high field strength conditions for a long time, resulting in an increase in MOS tube leakage or even a breakdown of the gate oxide layer, and improving the reliability of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor device manufacturing, and in particular to a SGT device preparation method and an epitaxial wafer. Background Art

[0002] MOSFET can be roughly divided into the following categories: planar MOSFET; Trench MOSFET, mainly used in low voltage fields; SGT (Shielded Gate Transistor, shielded gate trench) MOSFET, mainly used in medium voltage and low voltage fields; SJ- (super junction) MOSFET, mainly used in high voltage fields.

[0003] Among them, the SGT MOSFET structure has a charge coupling effect, and introduces horizontal depletion on the basis of vertical depletion of the PN junction of traditional trench MOSFET devices. Under the condition of using the same doping concentration of epitaxial material specifications, the device can obtain a higher breakdown voltage. The deeper trench depth can use more silicon volume to absorb EAS (Energy Avalanche Stress, avalanche energy test) energy, so SGT can do better in avalanche and can better withstand avalanche breakdown and surge current. In application fields such as switching power supplies, motor control, and power battery systems, SGT MOSFET combined with advanced packaging is very helpful in improving the efficiency and power density of the system.

[0004] For low-voltage SGT (below 100V), a single-layer epitaxial layer can generally meet the required performance. As the voltage resistance increases, the required epitaxial layer doping concentration becomes lower. If a high voltage resistance is required, an epitaxial layer with a very low doping concentration and a very thick thickness is required, which will cause a significant increase in the on-resistance. In order to reduce the on-resistance, it is usually necessary to prepare multiple epitaxial layers, but this increases the complexity of the process.

[0005] At present, the withstand voltage of SGT can be characterized by the integral area of ​​the electric field strength curve along the trench direction. The larger the integral area, the higher the withstand voltage. Although the traditional SGT introduces horizontal depletion, the peak of the electric field strength is at the PN junction formed by the well region and EPI (silicon grown by epitaxial technology) and the bottom of the trench, and the electric field strength distribution is "M" shaped. With the increase of the withstand voltage of SGT, the electric field strength required to withstand the PN junction formed by the well region and EPI increases, and the electric field strength borne by the adjacent gate oxide layer also increases accordingly. Since the gate oxide layer is relatively thin, long-term exposure to high field strength conditions will accelerate the decline of the oxide layer performance, resulting in increased leakage or even breakdown, reducing the reliability of the device. Summary of the invention

[0006] Based on this, the purpose of the present invention is to provide a method for preparing an SGT device and an epitaxial wafer, aiming to solve the problem in the prior art that the gate oxide layer is exposed to high field strength conditions for a long time, causing performance degradation, resulting in increased MOS tube leakage, and even gate oxide layer breakdown, which seriously affects the device reliability.

[0007] An epitaxial wafer according to an embodiment of the present invention is used to prepare an SGT device, the epitaxial wafer comprising an N-type substrate and a composite layer deposited on the N-type substrate, the composite layer comprising a first sublayer, a second sublayer, a third sublayer and a fourth sublayer deposited in sequence;

[0008] The first sublayer, the second sublayer and the fourth sublayer are all epitaxial layers uniformly doped with phosphorus, the third sublayer is an epitaxial layer uniformly doped with boron, the third sublayer has the smallest thickness, the first sublayer has a thickness of 8 μm to 11 μm, the second sublayer has a thickness of 1 μm to 3 μm, the third sublayer has a thickness of 0.2 μm to 0.8 μm, and the fourth sublayer has a thickness of 2 μm to 5 μm;

[0009] The doping concentration of the first sublayer is 1E14 atoms / cm 3 ~1E15 atoms / cm 3 The doping concentration of the second sub-layer is 1E16 atoms / cm 3 ~5E16 atoms / cm 3 The doping concentration of the third sublayer is 4E16 atoms / cm 3 ~1E17 atoms / cm 3 The doping concentration of the fourth sublayer is 7E15 atoms / cm 3 ~3E16 atoms / cm 3 .

[0010] Furthermore, the growth temperature of the composite layer is 500°C to 700°C.

[0011] According to another embodiment of the present invention, a method for preparing an SGT device is prepared on the basis of the above-mentioned epitaxial wafer, and the method comprises:

[0012] Etching a groove on the epitaxial wafer, and growing a first oxide layer in the groove by thermal oxidation to form a dielectric layer of the shield gate sidewall;

[0013] Filling the shield gate polysilicon in the trench with the oxide layer, grinding and etching back using CMP technology, and then depositing a second oxide layer to form isolation between the shield gate polysilicon and the gate;

[0014] Growing a third oxide layer on the second oxide layer by thermal oxidation to form a gate oxide layer, then depositing polysilicon to form a gate, and polishing it by CMP technology;

[0015] The source electrode is formed and gold wire bonding is performed to form the electrode.

[0016] Furthermore, the depth of the groove is 5.5 μm to 6.5 μm.

[0017] Furthermore, the thickness of the first oxide layer is 5600Å~6500Å.

[0018] Furthermore, the shield gate polysilicon is filled in the trench where the oxide layer is grown, and after being polished and etched back using the CMP technology, the distance between the shield gate polysilicon and the upper surface of the epitaxial wafer is 1.3 μm to 1.7 μm.

[0019] Furthermore, the thickness of the second oxide layer is 0.3 μm to 0.5 μm.

[0020] Furthermore, the thickness of the third oxide layer is 400Å~600Å.

[0021] Compared with the prior art: the present invention provides a method for preparing an SGT device and an epitaxial wafer, by depositing a composite layer on an N-type substrate, the composite layer includes a first sublayer, a second sublayer, a third sublayer and a fourth sublayer deposited in sequence; wherein the first sublayer, the second sublayer and the fourth sublayer are epitaxial layers uniformly doped with phosphorus, the third sublayer is an epitaxial layer uniformly doped with boron, and the thickness of the third sublayer is the smallest. Specifically, a four-layer epitaxial method with different doping concentrations is adopted, and the phosphorus-doped epitaxial layer and the boron-doped epitaxial layer are interspersed, which effectively adjusts the distribution of the electric field strength curve, greatly reduces the electric field strength at the PN junction formed by the high-voltage SGT well region and the EPI, thereby reducing the electric field strength borne by the adjacent gate oxide layer, preventing the performance degradation caused by the gate oxide layer being in high field strength conditions for a long time, resulting in an increase in MOS tube leakage or even a breakdown of the gate oxide layer, and improving the reliability of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 A schematic diagram of the structure of an epitaxial wafer provided in an embodiment of the present invention;

[0023] Figure 2 A flowchart of a method for preparing an SGT device provided by an embodiment of the present invention;

[0024] FIG3 (a) is a schematic diagram of the structure of adding a P-type doped epitaxial layer to an N-type doped epitaxial layer;

[0025] FIG3( b ) is a doping concentration curve corresponding to the structure in FIG3( a );

[0026] FIG4 (a) is a schematic diagram of the impact ionization of the SGT device prepared in Comparative Example 1;

[0027] FIG4( b ) is a schematic diagram of collision ionization of the SGT device prepared in Example 2 of the present invention;

[0028] Figure 5 The electric field intensity distribution curves of the SGT device prepared in comparative example 1 and the SGT device prepared in embodiment 2 of the present invention are shown. DETAILED DESCRIPTION

[0029] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. Several embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.

[0030] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only.

[0031] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.

[0032] refer to Figure 1 , Figure 1 A schematic structural diagram of an epitaxial wafer provided in an embodiment of the present invention, the epitaxial wafer comprises an N-type substrate 1 and a composite layer deposited on the N-type substrate 1, the composite layer comprising a first sublayer 2, a second sublayer 3, a third sublayer 4 and a fourth sublayer 5 deposited in sequence;

[0033] The first sublayer 2 , the second sublayer 3 , and the fourth sublayer 5 are all epitaxial layers uniformly doped with phosphorus, and the third sublayer 4 is an epitaxial layer uniformly doped with boron, and the thickness of the third sublayer is the smallest.

[0034] Specifically, the thickness of the first sublayer 2 is 8μm~11μm. Exemplarily, the thickness of the first sublayer 2 is 8μm, 9μm, 10μm or 11μm, etc., but not limited to this; the thickness of the second sublayer 3 is 1μm~3μm. Exemplarily, the thickness of the second sublayer 3 is 1μm, 1.5μm, 2μm, 2.5μm or 3μm, etc., but not limited to this; the thickness of the third sublayer 4 is 0.2μm~0.8μm. Exemplarily, the thickness of the third sublayer 4 is 0.2μm, 0.3μm, 0.4μm, 0.5μm, 0.6μm, 0.7μm or 0.8μm, etc., but not limited to this; the thickness of the fourth sublayer 5 is 2μm~5μm. Exemplarily, the thickness of the fourth sublayer 5 is 2μm, 2.5μm, 3μm, 3.5μm, 4μm, 4.5μm or 5μm, etc., but not limited to this.

[0035] More specifically, the doping concentration of the first sublayer 2 is 1E14 atoms / cm 3 ~1E15 atoms / cm 3 The doping concentration of the second sublayer 3 is 1E16 atoms / cm 3 ~5E16 atoms / cm 3 , the doping concentration of the third sublayer 4 is 4E16 atoms / cm 3 ~1E17 atoms / cm 3 The doping concentration of the fourth sublayer 5 is 7E15 atoms / cm 3 ~3E16 atoms / cm 3 It can be understood that the third sublayer 4 is a P-type doped epitaxial layer. It should be noted that the first sublayer 2 is a low-concentration phosphorus-doped epitaxial layer, which mainly plays a role in pressure resistance. The second sublayer 3 is a high-concentration phosphorus-doped epitaxial layer, which can reduce the on-resistance in cooperation with the shielding gate. The main purpose of the third sublayer 4 is to inhibit the high-concentration impurities of the second sublayer 3 from diffusing into the fourth sublayer, which can effectively produce a large concentration difference at a very short distance at the junction of the second sublayer 3 and the fourth sublayer 5, so as to achieve the purpose of adjusting the distribution of the electric field strength curve.

[0036] In addition, the doping time of each sublayer in the composite layer is 5min~10min, and the growth temperature of the composite layer is 500℃~700℃.

[0037] refer to Figure 2 , Figure 2 A flowchart of a method for preparing an SGT device provided in an embodiment of the present invention is provided. The method is performed on the basis of the above-mentioned epitaxial wafer and specifically comprises the following steps:

[0038] Step S01 , etching a trench on the epitaxial wafer, and growing a first oxide layer in the trench by thermal oxidation to form a dielectric layer of the shield gate sidewall.

[0039] The fourth sublayer is etched toward the N-type substrate, but the N-type substrate is not exposed, and the depth of the etched groove is 5.5μm~6.5μm. Specifically, the thermal oxidation process is to introduce oxygen at a temperature of 800℃~1100℃ to grow a high-quality oxide layer as the dielectric layer of the shield gate sidewall.

[0040] In this embodiment, the thickness of the first oxide layer is 5600Å~6500Å. It should be noted that high-quality OX is generated by thermal oxidation to effectively isolate the subsequent shielding gate from the substrate. If the thickness is too thin, the isolation will be poor, and if it is too thick, there will be problems with POLY filling, and gaps will be generated in the middle.

[0041] Step S02, filling the shield gate polysilicon in the trench with the oxide layer, grinding and etching back using CMP technology, and then depositing a second oxide layer to form isolation between the shield gate polysilicon and the gate.

[0042] Specifically, after being polished and etched back using CMP (Chemical Mechanical Polishing) technology, the distance between the shielding gate polysilicon and the upper surface of the epitaxial wafer is 1.3μm~1.7μm, in order to form the shielding gate of the SGT as a horizontally depleted field plate.

[0043] In addition, the thickness of the second oxide layer is 0.3 μm to 0.5 μm, and the oxide layer serves as isolation between the shielding gate polysilicon and the gate.

[0044] Step S03, growing a third oxide layer on the second oxide layer by thermal oxidation to form a gate oxide layer, then depositing polysilicon to form a gate, and polishing it by CMP technology.

[0045] Among them, a high-quality oxide layer of 400Å~600Å is grown by thermal oxidation to form a gate oxide layer, also known as the third oxide layer, and then 1.2μm~1.4μm polysilicon is deposited to form a gate, and finally CMP technology is used to smooth it.

[0046] Step S04, generating a source electrode and performing gold wire bonding to form an electrode.

[0047] In this embodiment, the source is formed by first doping P-type ions on the epitaxial layer next to the trench as a well, then doping a layer of N-type ions above the well, and then annealing. The N-type doped area is the source area.

[0048] In this embodiment, a low concentration area is generated at the junction of N-type doping and P-type doping, and the uniformly doped epitaxial layer has a better effect and a steeper gradient curve. As shown in Figure 3 (a), it is a schematic diagram of the structure of adding a P-type doped epitaxial layer to an N-type doped epitaxial layer. Figure 3 (b) is a doping concentration curve corresponding to the structure in Figure 3 (a). It can be seen that the doping concentration at position A in Figure 3 (b) has a sudden change. It can be understood that a low concentration area will produce a large potential difference, which can effectively transfer the distribution of the electric field. The embodiment of the present invention is to insert a thinner P-type epitaxial layer into a conventional N-type epitaxial layer. Since the thickness of the added P epitaxial layer is very thin, a PN junction that affects the normal operation of the device will not be formed.

[0049] In summary, the present invention provides a method for preparing an SGT device and an epitaxial wafer, by depositing a composite layer on an N-type substrate, the composite layer includes a first sublayer, a second sublayer, a third sublayer and a fourth sublayer deposited in sequence; wherein the first sublayer, the second sublayer and the fourth sublayer are epitaxial layers uniformly doped with phosphorus, the third sublayer is an epitaxial layer uniformly doped with boron, and the thickness of the third sublayer is the smallest. Specifically, a four-layer epitaxial method with different doping concentrations is adopted, and the phosphorus-doped epitaxial layer and the boron-doped epitaxial layer are interspersed, which effectively adjusts the distribution of the electric field strength curve, greatly reduces the electric field strength at the PN junction formed by the high-voltage SGT well region and the EPI, thereby reducing the electric field strength borne by the adjacent gate oxide layer, preventing the performance degradation caused by the gate oxide layer being in high field strength conditions for a long time, resulting in an increase in MOS tube leakage or even a breakdown of the gate oxide layer, and improving the reliability of the device.

[0050] In order to facilitate understanding of the present invention, several embodiments of the present invention are provided below. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.

[0051] Example 1

[0052] Embodiment 1 of the present invention provides a method for preparing an SGT device and an epitaxial wafer. Specifically, the epitaxial wafer includes an N-type substrate and a composite layer deposited on the N-type substrate, and the composite layer includes a first sublayer, a second sublayer, a third sublayer, and a fourth sublayer deposited in sequence;

[0053] The first sublayer, the second sublayer and the fourth sublayer are all epitaxial layers uniformly doped with phosphorus, and the third sublayer is an epitaxial layer uniformly doped with boron, and the thickness of the third sublayer is the smallest. Specifically, the thickness of the first sublayer is 10 μm, and the doping concentration of the first sublayer is 1.7E15 atoms / cm 3, the corresponding resistivity is 2.8Ω·cm; the thickness of the second sublayer is 2μm, and the doping concentration of the second sublayer is 3.2E16 atoms / cm 3 , the corresponding resistivity is 0.2Ω·cm; the thickness of the third sublayer is 0.5μm, and the doping concentration of the third sublayer is 6.1E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm; the thickness of the fourth sublayer is 3.5μm, and the doping concentration of the fourth sublayer is 1.4E16 atoms / cm 3 , the corresponding resistivity is 0.4Ω·cm. It can be understood that the thickness and concentration will affect the range of concentration change and the size of the concentration gradient after diffusion. The epitaxial concentration can also be characterized by resistivity. More specifically, the growth temperature of the composite layer is 600℃.

[0054] Furthermore, the SGT device preparation method includes:

[0055] Etching into the first sub-layer on the epitaxial wafer provided in the embodiment of the present invention, etching a groove with a depth of 6 μm, and growing a first oxide layer with a thickness of 6000 Å in the groove by thermal oxidation, specifically, introducing oxygen at 1000° C. to form a dielectric layer of the side wall of the shield gate;

[0056] Fill the shield gate polysilicon in the trench where the oxide layer is grown, and use CMP technology to grind and etch back. At this time, the distance between the shield gate polysilicon and the upper surface of the epitaxial wafer is 1.5μm, and then deposit a second oxide layer with a thickness of 0.4μm to form isolation between the shield gate polysilicon and the gate;

[0057] A third oxide layer with a thickness of 500 Å is grown on the second oxide layer by thermal oxidation. Specifically, oxygen is introduced at 1000°C to form a gate oxide layer, and then polysilicon with a thickness of 1.2 μm is deposited to form a gate, which is then polished by CMP technology.

[0058] The source electrode is formed and gold wire bonding is performed to form the electrode.

[0059] Example 2

[0060] Embodiment 2 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.9E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm.

[0061] Example 3

[0062] Embodiment 3 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.4E16 atoms / cm 3 , the corresponding resistivity is 0.4Ω·cm.

[0063] Example 4

[0064] Embodiment 4 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.9E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm, and the thickness of the third sublayer is 0.3μm.

[0065] Example 5

[0066] Embodiment 5 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.9E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm, and the thickness of the third sublayer is 0.7μm.

[0067] Example 6

[0068] Embodiment 6 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.9E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm, and the thickness of the second sublayer is 1μm.

[0069] Example 7

[0070] Embodiment 7 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.9E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm, and the thickness of the second sublayer is 3μm.

[0071] Example 8

[0072] Embodiment 8 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.9E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm, and the doping concentration of the third sublayer is 1E17 atoms / cm 3 , the corresponding resistivity is 0.2Ω·cm.

[0073] Example 9

[0074] Embodiment 9 of the present invention also provides a method for preparing an SGT device and an epitaxial wafer. The difference from Embodiment 1 of the present invention is that the doping concentration of the second sublayer is 1.9E16 atoms / cm 3 , the corresponding resistivity is 0.3Ω·cm, and the doping concentration of the third sublayer is 4.3E16 atoms / cm 3 , the corresponding resistivity is 0.4Ω·cm.

[0075] Comparative Example 1

[0076] Comparative Example 1 of the present invention provides a method for preparing an SGT device and an epitaxial wafer, which is different from Example 1 in that the composite layer in the epitaxial wafer does not contain a third sublayer, but only includes a first sublayer, a second sublayer and a fourth sublayer deposited in sequence.

[0077] The SGT devices prepared in Examples 1 to 9 of the present invention and Comparative Example 1 were subjected to BV (breakdown voltage), RON (on-resistance) and electric field strength tests. The specific test results are shown in the following table:

[0078]

[0079] It can be found that the electric field strength at the PN junction of the SGT devices prepared in the embodiments of the present invention is improved to varying degrees. Among them, the electric field strength at the PN junction of the SGT device in Example 2 of the present invention is reduced by 4.9 times compared with that in Comparative Example 1 without affecting BV and RON.

[0080] In addition, the SGT device prepared in Example 2 of the present invention and the SGT device prepared in Comparative Example 1 were simulated respectively to obtain collision ionization results. Please refer to Figures 4 (a) and 4 (b), Figure 4 (a) is a schematic diagram of the collision ionization of the SGT device prepared in Comparative Example 1, and Figure 4 (b) is a schematic diagram of the collision ionization of the SGT device prepared in Example 2 of the present invention. Area B in Figure 4 (a) and area C in Figure 4 (b) represent the PN junction formed by the well region and EPI and the bottom area of ​​the gate oxide layer, respectively. It can be seen that the SGT device prepared in Comparative Example 1 has a high degree of collision ionization here. The higher the collision ionization, the greater the leakage current. In addition, please refer to Figure 5 , which is a graph of the electric field strength distribution of the SGT device prepared in comparative example 1 and the SGT device prepared in Example 2 of the present invention. The horizontal axis is the thickness of the epitaxial layer, which can be understood as the distance from the source to the drain of the device, and the vertical axis is the electric field strength. It can be clearly seen that the SGT device prepared in Example 2 of the present invention effectively readjusts the distribution of the electric field strength, improves the original "M" type distribution, and reduces the electric field strength at D.

[0081] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. An epitaxial wafer, It is characterized in that For preparing an SGT device, the epitaxial wafer comprises an N-type substrate and a composite layer deposited on the N-type substrate, the composite layer comprising a first sublayer, a second sublayer, a third sublayer and a fourth sublayer deposited in sequence; The first sublayer, the second sublayer and the fourth sublayer are all epitaxial layers uniformly doped with phosphorus, the third sublayer is an epitaxial layer uniformly doped with boron, and the thickness of the third sublayer is the smallest. The thickness of the first sublayer is 8 μm to 11 μm, the thickness of the second sublayer is 1 μm to 3 μm, the thickness of the third sublayer is 0.2 μm to 0.8 μm, and the thickness of the fourth sublayer is 2 μm to 5 μm; The doping concentration of the first sublayer is 1E14 atoms / cm 3 ~1E15 atoms / cm 3 The doping concentration of the second sub-layer is 1E16 atoms / cm 3 ~5E16 atoms / cm 3 The doping concentration of the third sub-layer is 4E16 atoms / cm 3 ~1E17atoms / cm 3 The doping concentration of the fourth sublayer is 7E15 atoms / cm 3 ~3E16 atoms / cm 3 .

2. The epitaxial wafer according to claim 1, It is characterized in that The growth temperature of the composite layer is 500°C to 700°C.

3. A method for preparing a SGT device, It is characterized in that Prepared on the basis of the epitaxial wafer according to any one of claims 1 to 2, the method comprising: Etching a groove on the epitaxial wafer, and growing a first oxide layer in the groove by thermal oxidation to form a dielectric layer of the shield gate sidewall; Filling the shield gate polysilicon in the trench with the oxide layer, grinding and etching back using CMP technology, and then depositing a second oxide layer to form isolation between the shield gate polysilicon and the gate; Growing a third oxide layer on the second oxide layer by thermal oxidation to form a gate oxide layer, then depositing polysilicon to form a gate, and polishing it by CMP technology; The source electrode is formed and gold wire bonding is performed to form the electrode.

4. The method for preparing a SGT device according to claim 3, It is characterized in that The depth of the groove is 5.5 μm to 6.5 μm.

5. The method for preparing the SGT device according to claim 3, It is characterized in that The thickness of the first oxide layer is 5600Å~6500Å.

6. The method for preparing a SGT device according to claim 3, It is characterized in that The shield gate polysilicon is filled in the trench where the oxide layer is grown. After being polished and etched back using the CMP technology, the distance between the shield gate polysilicon and the upper surface of the epitaxial wafer is 1.3μm~1.7μm.

7. The method for preparing a SGT device according to claim 3, It is characterized in that The thickness of the second oxide layer is 0.3 μm-0.5 μm.

8. The method for preparing a SGT device according to claim 3, It is characterized in that The thickness of the third oxide layer is 400Å~600Å.

Citation Information

Patent Citations

  • SiC-based groove-type field effect transistor and preparation method thereof

    CN106449757A

  • Split-gate trench MOS with optimized electric field characteristics and manufacturing method thereof

    CN113823567A