A method for detecting and analyzing the qualified degree of ceramsite production
By performing three-dimensional scanning and similar grouping of ceram particles, dynamically setting the detection sequence and injection interval, the problems of irregular detection time and independent results in ceram particle size detection are solved, the detection efficiency and result accuracy are improved, and the coherent data are formed to facilitate particle size distribution analysis.
Patent Information
- Application Number
- CN202411039408.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-07-31
AI Technical Summary
In the detection of large-batch ceramic particle sizes, the existing automated operating methods have irregular detection time due to the uncorrelated results of adjacent ceramic particles, which increases the waiting time and detection period, and the particle size detection results are independent and lack reference, which increases the increase The complexity and subjectivity of data analysis.
By performing three-dimensional surface scanning of batches of ceratops, determining the detection group after similar grouping, dynamically setting the injection interval time, and determining the detection sequence according to the shape regularity and quantity, and performing secondary detection calibration to improve the credibility of the detection results.
Shorten the waiting time for particle size detection, improve detection efficiency and equipment utilization, form a coherent data set, facilitate particle size distribution characteristic analysis, minimize the operational impact of detection results, and ensure the accuracy and credibility of results. .
Smart Images

Figure CN118583734B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of ceramsite production qualification analysis, in particular to a ceramsite particle size qualification analysis technology, and specifically discloses a ceramsite production qualification detection and analysis method. Background Art
[0002] As an important filler and cushioning material in the fields of construction and gardening, the physical properties of ceramsite are crucial to its performance. By testing the physical properties of ceramsite, it can be ensured that the product meets the expected standards. Among the physical properties of ceramsite, the particle size test is particularly important, because in gardening applications, the particle size of ceramsite is directly related to the permeability and drainage of gardening construction. Therefore, ensuring the particle size is an important guarantee to ensure the good performance of the product in gardening applications.
[0003] With the development of industries such as construction and gardening, the demand for expanded clay is increasing, which has prompted the transformation of expanded clay particle size qualification detection from single detection to large-scale detection. Automated operation has become inevitable in large-scale detection. However, in the existing automated operation, expanded clay is detected one by one according to the design sequence. Generally speaking, the design sequence is random, so there is no correlation between adjacent expanded clay, resulting in no obvious regularity in the detection time of adjacent expanded clay, making it difficult to accurately predict. This requires waiting for the test result of the previous expanded clay to come out before the next expanded clay can be sent to the detection equipment. In this way, there will be a certain waiting time. As the number of expanded clay tests increases, the accumulated waiting time leads to an extension of the overall detection cycle, resulting in low detection efficiency.
[0004] In addition, since the test results of adjacent expanded clay pellets are unrelated, the particle size test results of each expanded clay pellet are independent. The lack of reference in the particle size qualification analysis will cause certain difficulties in identifying the changes in the particle size distribution of the expanded clay pellets in the entire batch. On the other hand, the particle size test results will be affected by the operation of the testing equipment. The lack of reference for the particle size test results of each expanded clay pellet will increase the challenge of evaluating whether each test result is accurate, thereby invisibly increasing the complexity and subjectivity of data analysis. Summary of the invention
[0005] To this end, one purpose of an embodiment of the present application is to provide a method for detecting and analyzing the qualification of expanded clay production, by grouping batches of expanded clay into similar groups, thereby specifically controlling the injection interval length of each detection group, thereby effectively solving the problems mentioned in the background technology.
[0006] The purpose of the present invention can be achieved by the following technical scheme: a method for detecting and analyzing the production qualification of ceramsite, comprising the following steps: S1, counting the number of batches of ceramsite to be tested for particle size qualification, and performing a three-dimensional surface scan on each ceramsite to obtain the shape profile of each ceramsite.
[0007] S2. Compare the shape profiles of each ceramsite, thereby grouping the batches of ceramsite into similar groups to obtain several test groups.
[0008] S3, analyzing the regularity of the ceramsite shapes corresponding to each detection group, and combining it with the quantity of ceramsite contained in each detection group to determine the detection order of each detection group.
[0009] S4. According to the detection order of each detection group, each detection group is sequentially retrieved and placed into the supply device of the detection equipment, and the injection interval time is dynamically set.
[0010] S5. After the test of the current test group is completed, a difference analysis is performed on the particle size of each expanded clay in the current test group to determine whether a secondary particle size test is needed.
[0011] S6. When it is determined that secondary testing is required, the testing equipment shall be calibrated and secondary particle size testing shall be performed on the corresponding testing group.
[0012] S7. After all test groups have been tested, the particle size qualification of the expanded clay is analyzed based on the particle size corresponding to each test group.
[0013] In combination with all the above technical solutions, the positive effects of the present invention are as follows: 1. The present invention takes into account that the shape profile of expanded clay will have a significant impact on the particle size of expanded clay, and thus batches of expanded clay are similarly grouped according to their shape profiles before detection, and then when performing particle size detection of each detection group, the injection interval duration is dynamically set with reference to the detection duration of the previous expanded clay, thereby achieving targeted and flexible sampling during large-scale expanded clay particle size detection, greatly shortening the waiting time for sampling, and improving the utilization rate of detection equipment while improving detection efficiency.
[0014] 2. The present invention obtains a set of ceramsite with similar shape contours by continuously testing the ceramsite in each test group, which helps to form a more coherent and comparable data set. This data set ensures that the particle size test results of each ceramsite will not exist independently, making it easier to perform statistical analysis, thereby more conveniently and accurately evaluating the particle size distribution characteristics in batch ceramsite.
[0015] 3. After the particle size of the expanded clay in each detection group is detected, the present invention performs a difference analysis on the particle size of each expanded clay in the current detection group, thereby performing a secondary detection evaluation and implementation, which can avoid and eliminate the influence of improper operation of the detection equipment on the detection result to the greatest extent during the detection process, ensure the credibility of the final detection result, and at the same time reduce the need to evaluate whether the detection result is accurate when performing data analysis using the subsequent particle size detection result of each expanded clay, which is conducive to improving data analysis efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] The present invention is further described using the accompanying drawings, but the embodiments in the accompanying drawings do not constitute any limitation to the present invention. A person skilled in the art can obtain other drawings based on the following drawings without creative work.
[0017] Figure 1 The present invention is a flowchart of the steps for implementing the method. DETAILED DESCRIPTION
[0018] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0019] See also Figure 1 As shown, the present invention proposes a method for detecting and analyzing the production qualification of ceramsite, comprising the following steps: S1, counting the number of batches of ceramsite to be tested for particle size qualification, and performing a three-dimensional surface scan on each ceramsite to obtain the shape contour of each ceramsite.
[0020] S2. Compare the shape contours of each expanded clay, thereby grouping the batches of expanded clay into similar groups to obtain several test groups, which are specifically implemented as follows: S21. Number each expanded clay in a preset order, and extract each expanded clay in sequence as a target expanded clay in the order of the numbers, and then compare the shape contours corresponding to the target expanded clay with the shape contours of other expanded clays to obtain the overlapping volume, and then compare the overlapping volume with the shape contour volume of the target expanded clay to obtain the shape overlap between each expanded clay as the target expanded clay and other expanded clays.
[0021] S22. Compare the shape overlap of each expanded clay as the target expanded clay with other expanded clays and a set overlap threshold. Exemplarily, the overlap threshold is 0.8, wherein the overlap threshold is initially set, and the setting purpose is to assist in the division of detection groups, from which other expanded clays with shape overlap greater than or equal to the overlap threshold are extracted together with the target expanded clay to form a number of detection groups.
[0022] In the example of the above scheme, the batches of expanded clay are numbered 1, 2, 3, 4, 5, 6, 7, 8, and 9 respectively. Among the expanded clay numbered 1 as the target expanded clay, the shape overlap between 1 and 2 is 0.73, the shape overlap between 1 and 3 is 0.65, the shape overlap between 1 and 4 is 0.92, the shape overlap between 1 and 5 is 0.54, the shape overlap between 1 and 6 is 0.96, the shape overlap between 1 and 7 is 0.92, the shape overlap between 1 and 8 is 0.39, and the shape overlap between 1 and 9 is 0.83. Under the set overlap threshold, the detection groups are 1, 4, 6, 7, and 9.
[0023] It should be understood that when conducting ceramsite particle size qualification testing, the shape contour is selected for similar grouping because the shape of the ceramsite has a direct impact on its particle size measurement. Although other parameters such as color, density, etc. may also affect some measurements, shape is a more significant factor in particle size testing. Ceramsites of similar shapes are more likely to show similar particle size distributions under the same test conditions, making the test time regular. Therefore, grouping by shape contour can more effectively control the test time; in addition, the shape contour is a relatively intuitive and objective feature, which is easy to compare and analyze using mathematical methods. In contrast, other parameters such as color, density, etc. may be more subjective or subject to the limitations of measuring instruments, and are not easy to use for accurate grouping and comparison.
[0024] S3, analyzing the regularity of the ceramsite shapes corresponding to each detection group, and combining it with the quantity of ceramsite contained in each detection group to determine the detection order of each detection group.
[0025] Applied to the above embodiment, the regularity of the shape of the expanded clay corresponding to each detection group is analyzed by referring to the following steps: regularly shaped expanded clay is selected as the reference expanded clay, and a three-dimensional image of the reference expanded clay is collected to extract the boundary contour, and then the shape parameters of the reference expanded clay are obtained based on the boundary contour of the reference expanded clay using image processing software. In a specific implementation, the shape parameters include roundness, sphericity, aspect ratio, convexity, etc., wherein roundness is a measure of the degree to which the shape of the expanded clay is close to a circle, sphericity is an assessment of the degree to which the shape of the expanded clay is close to a sphere, aspect ratio is an assessment of the length ratio of the main axis and the secondary axis of the expanded clay, and concavity is a measure of the degree of concavity of the expanded clay boundary.
[0026] It is important to know that parameters such as roundness, sphericity, aspect ratio, and convexity are used as indicators to measure the regularity of the shape of expanded clay because these parameters can objectively, comprehensively, and quantitatively describe various aspects of whether the shape of expanded clay is regular. Roundness describes whether the expanded clay is close to a circle, sphericity reflects the degree of its approximation to a sphere, aspect ratio can reveal the degree of stretching of the expanded clay, and concavity measures the degree of surface unevenness. By comparing the shape parameters of the target expanded clay in the test group with the shape parameters of the reference expanded clay, their proximity to regular shapes can be quantitatively evaluated.
[0027] The target ceramsite corresponding to each detection group is similarly extracted for shape parameter extraction, thereby comparing the shape parameters of the target ceramsite corresponding to each detection group with the shape parameters of the reference ceramsite, obtaining the contrast difference of each shape parameter, and comparing the contrast difference of each shape parameter with the shape parameters of the reference ceramsite, and then taking one of the preset constants as the base, wherein the preset constant value is greater than 1, and illustratively, the preset constant can be 3, and the absolute value of the contrast difference of each shape parameter is compared with the shape parameters of the reference ceramsite as the exponent, and the shape regularity of the ceramsite corresponding to each detection group is obtained. It can be seen from the calculation formula that the closer the shape parameters of the target ceramsite in each detection group are to the shape parameters of the reference ceramsite, the greater the shape regularity of the ceramsite corresponding to the detection group.
[0028] It should be noted that since the shape contours of the expanded clay in each test group are relatively similar, when conducting shape regularity analysis, it is only necessary to compare the shape parameters of one expanded clay with the shape parameters of the reference expanded clay, and there is no need to compare all the expanded clays. This can save analysis resources and improve analysis efficiency.
[0029] In the present invention, after similar grouping of batch ceramsite is performed, the detection order of the detection group is also considered, and the shape regularity of ceramsite is one of the bases for determining the detection order of the detection group. Generally speaking, ceramsite with complex and irregular shapes requires longer detection time, while ceramsite with regular shape can generally complete the measurement more quickly. By giving priority to ceramsite that can be detected quickly, the use of detection resources can be optimized, time and human resources can be saved, and the effective advancement of the detection progress can be ensured, and thus the shape regularity analysis of the grouped ceramsite is performed based on this consideration.
[0030] Further applied to the above embodiment, the detection order of each detection group is determined by the following operation: the amount of expanded clay contained in each detection group is compared with the amount of expanded clay in the batch to obtain the proportion of expanded clay corresponding to each detection group.
[0031] The weighted average of the proportion of expanded clay and the regularity of expanded clay shape corresponding to each detection group is calculated. In a specific example, the weight coefficients of the proportion of expanded clay and the regularity of expanded clay shape are 0.4 and 0.6 respectively, and the detection priority corresponding to each detection group is obtained. It can be seen that the greater the proportion of expanded clay in the detection group, the greater the regularity of the expanded clay shape and the greater the detection priority.
[0032] It should be added that the reason for using the proportion of ceramsite as the basis for determining the order of testing groups is that if the proportion of ceramsite in certain groups is large, these groups with larger numbers can be given priority, which helps to ensure the statistical significance and reliability of the data, because the larger the sample size, the higher the accuracy of the measurement results. Therefore, putting the groups with a larger proportion of ceramsite in front can effectively improve the efficiency of testing. Doing so can maximize the use of equipment and human resources, saving time and costs.
[0033] Arrange each detection group in descending order of detection priority to obtain the detection order of each detection group.
[0034] S4. According to the detection order of each detection group, each detection group is sequentially retrieved and placed into the supply device of the detection equipment, and the injection interval time is dynamically set.
[0035] It should be added that the detection equipment used in the present invention for detecting the particle size of ceramsite is a laser particle size analyzer, and its working principle is to emit laser light to the sample through a laser, and the ceramsite will scatter the laser beam. The instrument collects a large number of data points according to the scattered light signal of the sample, and then uses the built-in algorithm and analysis software to process and analyze the collected data to calculate the particle size of the ceramsite. The use of a laser particle size analyzer can usually provide more accurate, comprehensive and rapid particle size data than traditional screening methods for particles such as ceramsite with complex shapes and a wide range of particle sizes. At the same time, the sample does not need to be destroyed during the analysis process, and the same sample can be reused for multiple tests.
[0036] It should be noted that since the laser particle size analyzer can only detect the particle size of a single expanded clay at a time, expanded clay sampling control is performed.
[0037] Optimally, the dynamic setting of the injection interval duration is implemented as follows: S41, when performing the ceramsite particle size distribution detection of each detection group, determining the injection order of the ceramsite in each detection group, so that the first ceramsite to be detected by particle size can be determined.
[0038] S42, after the first ceramsite detection is performed according to the sampling sequence, the detection duration is recorded, thereby initially setting the sampling interval duration of the ceramsite.
[0039] It should be understood that considering possible equipment stability, operating errors or changes in sample characteristics, it is recommended to reserve a certain buffer time in the injection interval to prevent operation interruption or data loss due to emergencies. Usually, the interval time can be set to a multiple of the previous expanded clay test time to ensure that the equipment and operators have enough time to prepare and process the next sample.
[0040] S43, after the next ceramsite is sampled and tested according to the determined sampling interval, record the detection duration, and compare it with the detection duration of the previous ceramsite. If the comparison is consistent, keep the ceramsite sampling interval duration initially set, otherwise execute S44.
[0041] S44, adjusting and correcting the initial set injection interval duration according to the detection duration of the next ceramsite, and then performing subsequent ceramsite injection.
[0042] In the example of the above solution, the detection time of the next ceramsite is , the detection time of the last ceramsite is The initial setting of the injection interval is In this example, the adjusted injection interval duration is calculated as In this calculation formula, when the detection time of the next expanded clay is higher than the detection time of the previous expanded clay, the corrected injection interval is greater than the initially set injection interval; when the detection time of the next expanded clay is lower than the detection time of the previous expanded clay, the corrected injection interval is less than the initially set injection interval.
[0043] The present invention dynamically adjusts the interval according to the actual detection situation to shorten the detection time to the maximum extent, thereby improving the detection efficiency and ensuring the continuity and accuracy of the data.
[0044] S5. After the test of the current test group is completed, a difference analysis is performed on the particle size of each expanded clay in the current test group to determine whether a secondary particle size test is needed.
[0045] In further implementation of the above scheme, the difference analysis of the particle size of each ceramsite in the current detection group is performed as follows: the particle size of each ceramsite in the current detection group is compared, and the median particle size and the average particle size are selected therefrom.
[0046] The median particle size and average particle size corresponding to the current detection group are subtracted, and the absolute value of the subtraction result is divided by the median particle size to obtain the particle size distribution difference corresponding to the current detection group.
[0047] The greater the difference between the median particle size and the average particle size, the greater the difference in particle size distribution. This is because when there are extreme values or outliers in the data set, these values will have a greater impact on the average, while the median is more robust than the average because it is not affected by outliers. Under the influence of extreme values or outliers, the average value will deviate from the center of the data. Therefore, when the median and the average in a set of data differ greatly, this usually reflects the existence of extreme values or uneven data distribution in the data set, which may lead to a decrease in the overall centralization of the data. Under normal circumstances, the particle size distribution of the same test group should not differ much because the shape and contour of the expanded clay are relatively similar. When the actual difference is large, a secondary test may be considered.
[0048] For further optimization, the following operation is performed to judge whether a secondary particle size detection is needed: the particle size distribution difference corresponding to the current detection group is compared with the pre-configured allowable difference. For example, the allowable difference can be configured as 0.2. If the particle size distribution difference corresponding to the current detection group is greater than the allowable difference, it is judged that a secondary particle size detection is needed.
[0049] S6. When it is determined that secondary testing is required, the testing equipment shall be calibrated and secondary particle size testing shall be performed on the corresponding testing group.
[0050] In the above, when judging that a secondary test is needed for the current test group, the secondary test is carried out after the test equipment is calibrated in order to avoid the influence of improper operation on the test results caused by the uncalibrated test equipment during the first test. On the one hand, the reliability of the secondary test results can be ensured by calibrating and then testing. On the other hand, the results can be compared with the first test results to identify whether the large difference in the first test results is caused by the uncalibrated equipment or the problem of the preparation of the expanded clay itself.
[0051] It is important to understand that when there are significant differences in particle size distribution of ceramsite with the same shape and profile, it may be that there are slight changes or unevenness in the preparation conditions during the preparation of the ceramsite, resulting in significant differences in the size distribution of some ceramsites with the same shape and profile compared to other ceramsites. For example, slight changes in temperature during sintering, uneven mixing of raw materials during molding, etc., may affect the size distribution of the final ceramsite. Another possibility is that there are differences between batches or suppliers of raw materials used. Even under the same preparation conditions, ceramsite from different batches or sources may show different size distributions. These are all problems with the preparation of the ceramsite itself.
[0052] S7. After all test groups are tested, the particle size conformity of the expanded clay is analyzed based on the particle size corresponding to each test group. The specific analysis is as follows: S71. Based on the particle size of each expanded clay in each test group, a expanded clay particle size distribution graph of each test group is drawn, wherein the expanded clay particle size distribution graph can be a frequency distribution histogram or a cumulative distribution curve, usually the horizontal axis represents the particle size range of the expanded clay, and the vertical axis represents the number or cumulative percentage of the expanded clay within the range.
[0053] In the innovative implementation of the above scheme, before drawing the expanded clay particle size distribution map of each detection group based on the particle size of each expanded clay in each detection group, the effective particle size detection data of each detection group must be determined, as follows: identify whether there is a secondary particle size detection for each detection group. If there is a secondary particle size detection for a detection group, the secondary particle size detection data of the detection group is used as the effective particle size detection data of the detection group. This is because the detection equipment has been calibrated during the secondary detection. Otherwise, the first particle size detection data is used as the effective particle size detection data.
[0054] S72, extracting the shape of the particle size distribution diagram from the ceramsite particle size distribution diagram of each detection group, and comparing it with the distribution shape required by the specification, and then dividing the overlapping distribution area by the area of the distribution shape required by the specification to obtain the particle size distribution compliance corresponding to each detection group.
[0055] The distribution shape required in the above specifications mainly refers to the ceramsite particle size distribution shape specified in the technical standards, such as normal distribution and uniform distribution shape.
[0056] The invention reflects the particle size conformity of the ceramsite by comparing the particle size distribution shape of the ceramsite in the test group with the distribution shape required by the specification, and can intuitively evaluate the particle size conformity of the ceramsite. The specification requirements usually include an ideal particle size distribution curve or range. By comparing the actual distribution with these requirements, it can be immediately determined whether the ceramsite meets the standards.
[0057] S73. Collect the particle size data of historical qualified expanded clay samples as reference particle size data to determine the qualified particle size range corresponding to each test group.
[0058] It should be added that due to the differences in shape contours among different test groups, which have a significant impact on the particle size of expanded clay, it is impossible to determine a unified and reasonable particle size range for all test groups. At this time, the particle size data of historical expanded clay with qualified particle sizes are collected to compare the shape contours of qualified expanded clay with the shape contours of expanded clay in each test group. The historical qualified expanded clay that meets the shape contours of expanded clay in each test group is screened out from the historical qualified expanded clay, and then the qualified particle size range corresponding to each test group is determined based on the particle size of the screened out historical qualified expanded clay.
[0059] In the example of the above scheme, if there are 5 historical qualified expanded clay granules of a certain detection group with expanded clay shape contours, the particle sizes of these expanded clay granules are obtained respectively, and then the maximum and minimum values of these particle sizes are taken to form the qualified particle size range corresponding to the detection group.
[0060] It should be further explained that in order to ensure the reliability of the determination of the qualified particle size range corresponding to each test group, it is necessary to ensure that a sufficient number of historical qualified expanded clay that meets the shape profile of the expanded clay in each test group is screened out to avoid affecting the accuracy and reliability of the determination results due to too small a number.
[0061] S74, comparing the particle size of each ceramsite in each test group with the qualified particle size range corresponding to the corresponding test group, and counting the proportion of ceramsite falling within the qualified particle size range.
[0062] The present invention reflects the particle size qualification of expanded clay by using the proportion of expanded clay that falls within the qualified particle size range in each test group, which can directly quantify the situation of expanded clay falling within the qualified particle size range in each test group. It is not only objective, but also allows people to clearly understand the qualification of each test group, and at the same time can judge the differences between different test groups, which is very useful for quality control and product evaluation, and can quickly discover potential problems or trends.
[0063] S75. The particle size distribution conformity corresponding to each test group is combined with the proportion of expanded clay falling within the qualified particle size range and then weighted averaged to obtain the expanded clay particle size conformity corresponding to each test group. In the specific example of this content, considering that the overall particle size conformity of a batch of expanded clay is being analyzed, the proportion falling within the qualified particle size range may be more important, so that the weight factors corresponding to the particle size distribution conformity and the proportion of expanded clay falling within the qualified particle size range are 0.3 and 0.7 respectively.
[0064] The present invention can provide a more comprehensive evaluation by taking both the particle size distribution conformity and the proportion of expanded clay falling within the qualified particle size range as the basis for evaluating the particle size conformity. The combination of the two can fully demonstrate multiple aspects of the expanded clay particle size conformity. At the same time, the particle size distribution conformity and the qualified particle size proportion are usually complementary indicators. Their joint use can improve the accuracy and reliability of the evaluation. This comprehensive evaluation reduces the possible misleading or one-sidedness of a single indicator.
[0065] S76. Compare the compliance of the expanded clay particle size corresponding to each test group with the set compliance of the standard. Exemplarily, the compliance of the standard can be set to 0.85. The purpose of setting the compliance of the standard is to assist in the calculation of the qualified degree of the expanded clay particle size of the batch, and to obtain the qualified degree of the particle size of the batch expanded clay by counting the percentage of the test groups that meet the compliance of the standard.
[0066] S8. Identify the operating specifications of the detection equipment based on the comparison between the first particle size detection data and the secondary particle size detection data in the detection group with secondary particle size detection. The specific implementation is as follows: S81. Compare the first particle size detection data and the secondary particle size detection data in the detection group with secondary particle size detection to obtain the particle size detection difference.
[0067] S82, comparing the particle size detection difference with the precision error range corresponding to the detection equipment. If the particle size detection difference falls within the precision error range corresponding to the detection equipment, it is identified that the operation of the detection equipment is in compliance with the standard. Otherwise, it is identified that the operation of the detection equipment is not in compliance with the standard.
[0068] It should be understood that the above-mentioned non-standard operation of the testing equipment refers to the failure to calibrate. When calibration is not performed, there is a high possibility that the particle size detection difference exceeds the precision error range corresponding to the testing equipment. When the operation is non-standard and there is a large difference in particle size, it is most likely caused by operational problems. If the particle size detection difference falls within the precision error range corresponding to the testing equipment, it means that the first test is already a calibrated test result. In this case, if there is still a large difference in particle size, it is a problem in the preparation of expanded clay.
[0069] The present invention can provide a reliable basis for the difference of ceramsite particle size detection results within a detection group by comparing the first particle size detection data with the secondary particle size detection data.
[0070] The above contents are merely examples and explanations of the structure of the present invention. The technicians in this technical field may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the structure of the invention or exceed the scope defined by the present invention, they should all fall within the protection scope of the present invention.
Claims
1. A method for detecting and analyzing the qualification of ceramsite production, It is characterized in that The following steps are involved: S1, counting the number of batches of ceramsite to be tested for particle size qualification, and performing three-dimensional surface scanning on each ceramsite to obtain the shape profile of each ceramsite; S2, comparing the shape profiles of each ceramsite, thereby grouping the batches of ceramsite into similar groups to obtain several test groups; S3, analyzing the regularity of the ceramsite shape corresponding to each detection group, and combining it with the amount of ceramsite contained in each detection group to determine the detection order of each detection group; S4, according to the detection order of each detection group, each detection group is sequentially retrieved and placed into the supply device of the detection device, and the injection interval time is dynamically set; S5. After the current test group is tested, a difference analysis is performed on the particle sizes of each ceramsite in the current test group to determine whether a secondary particle size test is required; S6. When it is determined that secondary testing is required, the testing equipment is calibrated and secondary particle size testing is performed on the corresponding testing group; S7, after all test groups have been tested, the particle size qualification of the ceramsite is analyzed based on the particle size corresponding to each test group; The batch ceramsite is carried out into similar groups and implemented as follows: S21, numbering each ceramsite in a preset order, and extracting each ceramsite in sequence as a target ceramsite in the order of the numbers, and then overlapping and comparing the shape contours corresponding to the target ceramsite with the shape contours of other ceramsites, to obtain the shape overlap between each ceramsite as the target ceramsite and other ceramsites; S22, comparing the shape coincidence of each ceramsite as the target ceramsite with other ceramsites with a set coincidence threshold, and extracting other ceramsites with shape coincidence greater than or equal to the coincidence threshold together with the target ceramsite to form a plurality of detection groups; The analysis of the regularity of the ceramsite shape corresponding to each test group refers to the following steps: Selecting ceramsite with regular shape as reference ceramsite, collecting a three-dimensional image of the reference ceramsite, extracting the boundary contour from the image, and then using image processing software to obtain the shape parameters of the reference ceramsite based on the boundary contour of the reference ceramsite; The target ceramsite corresponding to each detection group is similarly extracted for shape parameter extraction, thereby comparing the shape parameters of the target ceramsite corresponding to each detection group with the shape parameters of the reference ceramsite, obtaining the contrast difference of each shape parameter, and comparing the contrast difference of each shape parameter with the shape parameters of the reference ceramsite, and then taking one of the preset constants as the base, taking the absolute value of the contrast difference of each shape parameter with the shape parameters of the reference ceramsite as the cumulative value of the result of comparing the absolute value of the contrast difference of each shape parameter with the shape parameters of the reference ceramsite as the exponent, and obtaining the shape regularity of the ceramsite corresponding to each detection group; The detection order of each detection group is determined as follows: Compare the amount of ceramsite contained in each test group with the amount of ceramsite in the batch to obtain the proportion of ceramsite corresponding to each test group; The weighted average calculation of the ceramsite proportion and ceramsite shape regularity corresponding to each detection group is performed to obtain the detection priority corresponding to each detection group; Arrange each detection group in descending order of detection priority to obtain a detection order for each detection group; The dynamic setting of the injection interval duration is implemented as follows: S41, determining the sampling order of the ceramsite in each detection group when performing the ceramsite particle size distribution detection of each detection group; S42, after the first ceramsite detection is performed according to the sampling order, the detection duration is recorded, thereby initially setting the sampling interval duration of the ceramsite; S43, after the next ceramsite is sampled and tested according to the determined sampling interval, the detection time is recorded and compared with the detection time of the previous ceramsite. If the comparison is consistent, the initial setting of the ceramsite sampling interval is maintained, otherwise S44 is executed; S44, adjusting and correcting the initial set sampling interval duration according to the detection duration of the next ceramsite, and then performing subsequent ceramsite sampling; The difference analysis of the particle size of each ceramsite in the current detection group is shown in the following process: Compare the particle sizes of each ceramsite in the current test group, and select the median particle size and the average particle size; Subtract the median particle size and the average particle size corresponding to the current detection group, and divide the absolute value of the difference result by the median particle size to obtain the particle size distribution difference corresponding to the current detection group; The following steps are performed to determine whether secondary particle size detection is required: Compare the particle size distribution difference corresponding to the current test group with the pre-set allowable difference. If the particle size distribution difference corresponding to the current test group is greater than the allowable difference, it is judged that a secondary particle size test is required. The ceramsite particle size qualification analysis is as follows: S71, drawing a ceramsite particle size distribution diagram of each detection group based on the particle size of each ceramsite in each detection group; S72, extracting the shape of the particle size distribution diagram from the ceramsite particle size distribution diagram of each test group, and comparing it with the distribution shape required by the specification to obtain the particle size distribution compliance corresponding to each test group; S73, collecting the particle size data of historical qualified ceramsite samples as reference particle size data to determine the qualified particle size range corresponding to each test group; S74, comparing the particle size of each ceramsite in each test group with the qualified particle size range corresponding to the corresponding test group, and counting the proportion of ceramsite falling within the qualified particle size range; S75, combining the particle size distribution conformity corresponding to each test group with the ceramsite proportion value falling within the qualified particle size range to obtain the ceramsite particle size conformity corresponding to each test group; S76. Compare the compliance of the expanded clay particle size corresponding to each test group with the set compliance of the standard, and calculate the percentage of the test groups that meet the compliance of the standard to obtain the particle size qualification of the batch expanded clay.
2. A method for detecting and analyzing the qualified degree of ceramsite production according to claim 1, Features: Before drawing the ceramsite particle size distribution diagram of each detection group based on the particle size of each ceramsite in each detection group, the effective particle size detection data of each detection group must be determined, as follows: Identify whether there is secondary particle size detection in each detection group. If there is secondary particle size detection in a detection group, the secondary particle size detection data of the detection group is used as the effective particle size detection data of the detection group. Otherwise, the primary particle size detection data is used as the effective particle size detection data.
3. A method for detecting and analyzing the qualified degree of ceramsite production according to claim 2, Features: It also includes S8, identifying the operating specifications of the detection equipment based on the comparison between the first particle size detection data and the secondary particle size detection data in the detection group with secondary particle size detection, which is specifically implemented as follows: S81, comparing the initial particle size detection data with the secondary particle size detection data in the detection group with secondary particle size detection to obtain a particle size detection difference; S82, comparing the particle size detection difference with the precision error range corresponding to the detection equipment. If the particle size detection difference falls within the precision error range corresponding to the detection equipment, it is identified that the operation of the detection equipment is in compliance with the standard. Otherwise, it is identified that the operation of the detection equipment is not in compliance with the standard.