A two-component spraying method and device for automotive interior products

By obtaining the appearance characteristic data of automobile interior products for zoning and speed compensation, the problems of difficult process control, high cost and poor spray quality in the existing technology are solved, and more efficient spray quality is achieved.

CN118594875BActive Publication Date: 2024-10-11SHENYANG JINBEI YANFENG AUTOMOTIVE INTERIOR SYST CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411081173.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-08
Publication Date
2024-10-11
Estimated Expiration
2044-08-08

AI Technical Summary

Technical Problem

The existing automobile interior spraying process faces complex and changing product appearance characteristics and high-quality spraying requirements. There are problems such as difficult process control, high cost, and poor spraying quality.

Method used

By obtaining the shape characteristic data of the target product for partitioning, planning the initial spraying path based on the spraying process plan, and performing speed compensation based on the height and thickness of the spray gun, identifying the speed mutation point for variable speed advance compensation, generating a target speed series, and realizing two-component spraying .

Benefits of technology

It reduces process control costs, improves process control efficiency and spraying quality, and achieves higher-quality spraying effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118594875B_ABST
    Figure CN118594875B_ABST
Patent Text Reader

Abstract

The present invention discloses a two-component spraying method and device for automotive interior products, which relates to the field of spraying technology. The method comprises: obtaining the shape feature data of the target product and performing zoning division. According to the zoning division result and the spraying process plan, the spraying path is planned, and the initial spraying path and the initial speed series are obtained. Based on the initial spraying path and the spray gun height series, height-speed compensation is performed to obtain the height compensation speed series. Combined with the shape feature data, the height compensation speed series and the initial spraying path, simulated spraying is performed, and thickness-speed compensation is performed according to the result, and the thickness compensation speed series is output. The speed mutation point in the thickness compensation speed series is identified, and the speed change advance compensation is performed to generate a target speed series. The initial spraying path is associated with the target speed series, and the two-component spraying of the target product is performed. Thereby achieving the technical effect of reducing the process control cost, improving the process control efficiency and the spraying quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of spraying technology, and in particular to a two-component spraying method and device for automobile interior decoration products. Background Art

[0002] The quality and aesthetics of automotive interiors directly affect the market competitiveness and user experience of the entire vehicle. Two-component spraying technology is widely used in the spraying process of automotive interior products because it can provide better coating effects. However, in the face of complex and changeable product appearance characteristics and high-quality spraying requirements, existing spraying processes and methods have technical problems such as difficult process control, high costs, and poor spraying quality. Summary of the invention

[0003] The present invention provides a two-component spraying method and device for automobile interior products, so as to solve the technical problems of difficult process control, high cost and poor spraying quality in the prior art, reduce the process control cost, and improve the process control efficiency and spraying quality.

[0004] In a first aspect, the present invention provides a two-component spraying method for automotive interior products, wherein the method comprises:

[0005] Acquire the shape feature data of the target product, and perform partitioning based on the shape feature data; plan the spray path according to the partitioning result and in combination with the spraying process plan to obtain an initial spray path, wherein the initial spray path is associated with an initial speed series; acquire the spray gun height series based on the initial spray path, and perform height-speed compensation on the initial speed series according to the spray gun height series to obtain a height-compensated speed series; perform simulated spraying based on the shape feature data and in combination with the height-compensated speed series and the initial spray path, and perform thickness-speed compensation according to the simulated spraying result to output a thickness-compensated speed series; identify and extract the speed mutation points in the thickness-compensated speed series to perform advance speed change compensation and generate a target speed series; associate the initial spray path with the target speed series to perform two-component spraying of the target product.

[0006] In a second aspect, the present invention further provides a two-component spraying device for automotive interior products, wherein the device comprises:

[0007] The product division module is used to obtain the appearance feature data of the target product and divide the product into zones based on the appearance feature data.

[0008] An initial path generation module is used to plan the spraying path according to the partition division result and the spraying process plan to obtain an initial spraying path, wherein the initial spraying path is associated with an initial speed series.

[0009] A height compensation module is used to obtain a spray gun height series based on the initial spraying path, and to perform height-speed compensation on the initial speed series according to the spray gun height series to obtain a height compensated speed series.

[0010] A thickness compensation module is used to simulate spraying based on the shape feature data, in combination with the height compensation speed series and the initial spraying path, and to perform thickness-speed compensation according to the simulated spraying results, and output a thickness compensation speed series.

[0011] The speed change compensation module is used to identify and extract the speed mutation points in the thickness compensation speed series to perform speed change advance compensation and generate a target speed series.

[0012] A spraying execution module is used to associate the initial spraying path with the target speed series to perform two-component spraying of a target product.

[0013] The present invention discloses a two-component spraying method and device for automotive interior products, comprising: obtaining shape feature data of a target product, and performing partitioning based on the shape feature data. According to the partitioning result, the spraying path is planned in combination with the spraying process scheme to obtain an initial spraying path, wherein the initial spraying path is associated with an initial speed series. Based on the initial spraying path, a spray gun height series is obtained, and the initial speed series is height-speed compensated according to the spray gun height series to obtain a height-compensated speed series. Based on the shape feature data, simulated spraying is performed in combination with the height-compensated speed series and the initial spraying path, and thickness-speed compensation is performed according to the simulated spraying result to output a thickness-compensated speed series. Speed ​​mutation points in the thickness-compensated speed series are identified and extracted to perform speed change advance compensation to generate a target speed series. The initial spraying path is associated with the target speed series to perform two-component spraying of the target product. The two-component spraying method and device for automotive interior products disclosed by the present invention solve the technical problems of difficult process control, high cost, and poor spraying quality, and achieve the technical effect of reducing process control costs, improving process control efficiency and spraying quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 A schematic diagram of a two-component spraying method for automotive interior products according to the present invention;

[0015] Figure 2The present invention is a schematic structural diagram of a two-component spraying device for automotive interior products.

[0016] Explanation of the reference numerals: product classification module 11 , initial path generation module 12 , height compensation module 13 , thickness compensation module 14 , speed change compensation module 15 , spraying execution module 16 . DETAILED DESCRIPTION

[0017] The technical solution provided in the embodiments of the present invention is to solve the technical problems of difficult process control, high cost and poor spraying quality in the prior art. The overall idea adopted is as follows:

[0018] First, the shape feature data of the target product is obtained, and partitions are performed based on the shape feature data. Then, according to the partition results, the spray path is planned in combination with the spraying process plan to obtain the initial spray path, wherein the initial spray path is associated with an initial speed series. Then, based on the initial spray path, the spray gun height series is obtained, and the initial speed series is height-speed compensated according to the spray gun height series to obtain the height-compensated speed series. Next, based on the shape feature data, simulated spraying is performed in combination with the height-compensated speed series and the initial spray path, and thickness-speed compensation is performed according to the simulated spraying results, and a thickness-compensated speed series is output. Furthermore, the speed mutation points in the thickness-compensated speed series are identified and extracted for advance speed change compensation to generate a target speed series. Finally, the initial spray path is associated with the target speed series to perform two-component spraying of the target product.

[0019] The above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods of the specification to better understand the above technical solution. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments of the present invention. It should be understood that the present invention is not limited to the example embodiments used only to explain the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. In addition, it should be noted that, for the convenience of description, only the parts related to the present invention are shown in the drawings, rather than all of them.

[0020] Embodiment 1

[0021] Figure 1 The present invention is a schematic flow diagram of a two-component spraying method for automotive interior products, wherein the method comprises:

[0022] The appearance feature data of the target product is obtained, and partitioning is performed based on the appearance feature data.

[0023] Specifically, the appearance feature data of the target product includes the appearance dimensions, surface roughness information, material information, etc. of the target automotive interior product. The acquisition method of the appearance feature data includes: scanning the automotive interior target product with a 3D scanning device to obtain the 3D appearance data of the product. Based on the design drawings or existing 3D models, the appearance feature data of the automotive interior target product is acquired. The appearance image of the target product is captured by a high-resolution camera, and the appearance feature data is extracted using image processing technology.

[0024] Specifically, the acquired shape feature data is subjected to surface analysis to identify different surface areas and feature points of the product. First, the shape data is divided into multiple functional areas according to the functional requirements of the automotive interior products. Such as the dashboard area, door panel area, seat area, etc. Then, combined with the spraying process requirements, the shape data is further refined into multiple spraying areas, and each spraying area can be divided according to characteristics such as color, material, and texture. Finally, according to the intra-regional continuity of multiple spraying areas, fine division is performed to obtain the partition division results.

[0025] Optionally, based on visualization technology and visualization path, the partitioning results are visualized to generate a partition map to guide subsequent spraying operations. Through the above steps, the appearance feature data of the target product of the automotive interior is obtained, and scientific and reasonable partitioning is performed based on these data, thereby providing a reasonable spraying base for subsequent spraying decisions and spraying.

[0026] According to the partitioning result, the spraying path is planned in combination with the spraying process plan to obtain an initial spraying path, wherein the initial spraying path is associated with an initial speed series.

[0027] Specifically, the zoning results include multiple target product surface ranges of multiple levels and categories, and different areas are sprayed with different spray particle sizes (spray fan width of the spray gun), corresponding to different spray process solutions. Specifically, the most suitable spray process solution is selected according to the characteristics of the product surface (such as curvature, angle, surface roughness, functional zoning, etc.), so as to achieve a higher quality spray effect.

[0028] Specifically, the spraying process scheme is stored in a preset spraying process library, which includes multiple groups of spraying parameters corresponding to different product characteristics (including product shape, size, surface roughness, curvature, etc.). Exemplarily, the spraying parameters include the spraying fan width, spraying gun speed, spraying pressure, spraying distance, air flow, atomization degree, paint viscosity, etc.

[0029] Specifically, according to the shape and boundary of the partition, a path generation algorithm (such as A* algorithm, genetic algorithm, etc.) is used to smooth the initial spraying path, and the planned initial spraying path is associated with an initial speed series. In other words, each path point has an initial speed associated with it. Among them, the initial speed series is the spraying speed under ideal spraying conditions, and the initial speed series includes multiple fixed spray gun speeds. Exemplarily, the multiple fixed spray gun speeds include straight spray gun speeds (higher) and multiple curved spray gun speeds with different curvatures (the greater the curvature, the lower the speed).

[0030] Optionally, spray path planning also includes edge refinement of the acquired initial spray path to ensure that the spray path covers all edge areas; smoothing the generated initial path to reduce path turning points and ensure spray stability.

[0031] Based on the initial spraying path, a spray gun height series is obtained, and height-speed compensation is performed on the initial speed series according to the spray gun height series to obtain a height-compensated speed series.

[0032] Specifically, the spray gun height is the relative height value between the spray gun and the reference plane during the spraying process, wherein the reference plane can be the horizontal plane where the paint spraying power device is located or the standard plane when the spraying process plan is defined.

[0033] Specifically, during the spraying process, changes in the height of the spray gun will cause changes in the water head that the paint needs to overcome, thereby affecting the spray pressure of the paint at the spray gun outlet. When the spray pressure output by the spray power device (such as a pump) is constant, it will affect the stability of the discharge rate. For example, if the height of the spray gun is lowered, the water head pressure that the paint needs to overcome will decrease, which may cause the discharge rate to increase, thereby increasing the thickness of the spray. Conversely, if the height of the spray gun is increased, the water head pressure that the paint needs to overcome will increase, thereby reducing the discharge rate, thereby reducing the thickness of the spray.

[0034] Specifically, due to the hysteresis of the output pressure adjustment of the paint spraying power device, in order to ensure uniform spraying thickness, the change in discharge rate caused by height change can be compensated by changing the movement speed of the spray gun. Specifically, if the height of the spray gun is increased, the spraying thickness can be ensured by reducing the movement speed of the spray gun; conversely, if the height of the spray gun is reduced, the spraying thickness can be ensured by increasing the movement speed of the spray gun.

[0035] In some embodiments, based on the initial spraying path, a spray gun height series is obtained, and height-speed compensation is performed on the initial speed series according to the spray gun height series to obtain a height-compensated speed series, including:

[0036] The initial spraying path is parsed to determine the relative height of the target spray gun at each position and store the height as the spray gun height series.

[0037] Calibrate to obtain the target two-component discharge flow-gun height mapping baseline.

[0038] The discharge flow rate-spray gun height mapping baseline is traversed to obtain the discharge flow rate series corresponding to the spray gun height series, and the flow rate deviation between the discharge flow rate series and the spraying process solution is calculated, and the flow rate deviation series is output.

[0039] An altitude-speed compensation coefficient series is calculated based on the flow deviation series, and altitude-speed compensation is performed according to the altitude-speed compensation coefficient series to generate the altitude-compensated speed series.

[0040] Specifically, first, the movement trajectory of the spray gun is analyzed along the initial spray path, and the initial spray path is mapped to the real coordinate system. The mapping process involves the rotation, scaling, translation, etc. of the coordinate points, so that the performance of the path in the real coordinate system is consistent with expectations. Then, the coordinate value of the Z axis of the mapped path is extracted to obtain multiple relative heights of the spray gun, and stored in the spray gun height series based on the sequential relationship of the path. Then, the discharge flow rate-spray gun height mapping baseline of the target two-component material at different spray gun heights is calibrated and established. The discharge flow rate-spray gun height mapping baseline establishes a mapping relationship between the discharge flow rate and the spray gun height, which is used to calculate the deviation of the discharge flow rate. Optionally, the discharge flow rate-spray gun height mapping baseline can be linear or nonlinear.

[0041] Furthermore, the discharge flow rate-spray gun height mapping baseline is traversed, and the discharge flow rate corresponding to each height value is found according to the spray gun height series to generate a discharge flow rate series. Furthermore, the deviation between the discharge flow rate series and the flow value preset in the spraying process plan is calculated to generate a flow rate deviation series.

[0042] Specifically, the spraying speed is adjusted by calculating the height-speed compensation coefficient series to compensate for the flow deviation. First, based on the flow deviation series, the flow deviation ratio is calculated. The flow deviation ratio is a vector that contains the size and direction of the deviation. For example, if the actual discharge flow rate is 20% more than the target flow rate, the flow deviation ratio is +20%; if the actual discharge flow rate is 20% less than the target flow rate, the flow deviation ratio is -20%. Then, according to the flow deviation ratio, the corresponding correction coefficient is generated to adjust the spraying speed. For example, if the flow deviation ratio is +20%, the compensation coefficient is equal to 1 / (1-20%). In other words, in order to compensate for the flow deviation, the spraying speed needs to be increased to 1 / (1-20%) times the original, that is, 125%. Finally, according to the height-speed compensation coefficient series, the spray gun movement speed at the corresponding height is changed accordingly to perform height-speed compensation. Generate a height compensation speed series. The height compensation speed series represents the compensated spraying speed at each spray gun height.

[0043] Through the above steps, the uniformity of the coating during the spraying process is ensured, the problem of uneven coating thickness caused by height changes is avoided, the spraying process is finely controlled, and the spraying quality and efficiency are improved.

[0044] Based on the shape feature data, the height compensation speed series is combined with the initial spraying path to perform simulated spraying, and thickness-speed compensation is performed according to the simulated spraying result to output a thickness compensation speed series.

[0045] In some embodiments, based on the shape feature data, combined with the height compensation speed series and the initial spraying path, simulated spraying is performed, and thickness-speed compensation is performed according to the simulated spraying results, and a thickness compensation speed series is output, including:

[0046] Based on the shape feature data, a simulated spraying space is constructed.

[0047] Based on the spraying process scheme, the spraying process parameters and the nozzle starting position are initialized in the simulated spraying space.

[0048] The height compensation speed series is fitted to the initial spraying path, simulated spraying is performed in the simulated spraying space, and simulated thickness distribution data is obtained.

[0049] The thickness difference analysis between the simulated thickness distribution data and the target thickness data is performed, and the difference correction coefficient distribution is calculated to perform thickness-speed compensation, and a thickness compensation speed series is output.

[0050] Specifically, simulated spraying is performed, and thickness-speed compensation is performed based on the simulation results to further optimize the spraying process. First, the space is simulated based on the shape feature data of the workpiece, such as size, shape, position, model and other information. Then, according to the preset spraying process plan, the parameters of the simulated spraying are set, such as the spraying fan width, spraying speed, spraying pressure, spraying distance, air flow, atomization degree, paint viscosity, etc.; at the same time, the starting position of the spray gun is set.

[0051] Optionally, the simulated spraying is regarded as an ideal situation, and the output per unit time of the main component of the coating is calculated based on the mixing ratio and viscosity characteristics of the two components of the coating. The output per unit time is defined to be evenly distributed within the spraying fan range of the target nozzle during spraying, and to scatter as the spraying distance increases, so as to perform simplified simulated spraying.

[0052] Furthermore, the height compensation speed series is combined with the initial spraying path to simulate the spraying. The thickness distribution data of the spraying is obtained. The thickness distribution data reflects the distribution of the spraying thickness at various positions. Among them, during the simulation process, the spray gun usually sprays at a certain angle (such as a fan shape), and the paint particles will fly away as the distance from the spray gun increases, which causes the paint to be unevenly distributed on the surface of the target product. Specifically, the closer the area is to the spray gun, the greater the cumulative thickness of the paint is usually; and the farther the area is from the spray gun, the less the cumulative thickness of the paint will be. This forms a coating distribution that is thick in the middle and thinner as it goes out.

[0053] Specifically, the simulated thickness distribution data and the target thickness data are compared to obtain the thickness difference. The target thickness data is preset and represents the ideal spraying thickness. Then, according to the thickness difference, the difference correction coefficient is calculated, and the spraying speed is adjusted according to the difference correction coefficient to compensate for the thickness difference. Finally, the thickness compensation speed series is output, which represents the spraying speed after thickness-speed compensation.

[0054] For example, for a convex curved surface, the spraying edge is farther away from the nozzle, resulting in a thinner coating layer. In other words, for fan-shaped divergent paint, a larger coating layer area is produced when it falls on a convex curved surface. That is, when spraying on a convex curved surface, the same unit time of discharge is distributed on a larger target product surface, thereby producing a thinner coating. By adjusting the spraying speed, the spraying time on the protruding part can be made longer, thereby increasing the coating thickness to achieve the desired goal.

[0055] The speed mutation points in the thickness compensation speed series are identified and extracted to perform advance speed change compensation, thereby generating a target speed series.

[0056] In some embodiments, identifying and extracting the speed mutation point in the thickness compensation speed series to perform speed change advance compensation and generate a target speed series includes:

[0057] The height compensation speed series is analyzed, speed mutation points are identified, and a speed inflection point set is obtained, wherein the speed inflection point set is marked with an inflection point speed change amount.

[0058] The speed inflection point set is traversed, the speed change amount of the inflection point is extracted to calculate the speed change compensation amount, and the speed change compensation data is obtained.

[0059] The speed control point positions in the thickness compensation speed series are updated based on the speed change compensation data to obtain a target speed series.

[0060] Specifically, the speed change is optimized during the spraying process. First, the height compensation speed series is analyzed, the speed change rate of adjacent time points is calculated, the speed mutation points are identified, and the speed change amount is marked and recorded. All identified speed mutation points are summarized to generate a speed inflection point set. Among them, the speed mutation point is the inflection point of the speed. For example, a threshold value of the speed change rate is set. When the change rate exceeds the threshold, the corresponding time point is marked as a speed mutation point.

[0061] Specifically, all the speed inflection points in the speed inflection point set are traversed, and the corresponding speed compensation is calculated according to the speed change at each inflection point. The speed compensation can be understood as the acceleration time (delay) required by the nozzle during the speed change process, and the speed compensation is calculated based on the speed change at the speed inflection point and the preset nozzle acceleration.

[0062] Specifically, updating the position of the speed control point in the thickness compensation speed series according to the speed change compensation data means adaptively advancing or delaying the speed change positions at multiple speed inflection points according to the speed change compensation data.

[0063] By using the speed compensation data to make advance speed compensation, the smoothness and accuracy of the spraying path can be ensured, and the thickness of the coating layer at the nozzle speed change point caused by a sudden change in speed can be avoided, which in turn affects the spraying effect. This helps to achieve an efficient and accurate two-component spraying process.

[0064] The initial spraying path is associated with the target speed series to perform two-component spraying of a target product.

[0065] Specifically, for two-component spraying of the target product, first, prepare the two-component spraying materials according to the spraying requirements. Make sure the materials are within the validity period and are accurately proportioned. Then, check the status of the spraying equipment, including the spray gun, pipeline, mixing device, filter device, etc., to ensure that the equipment is in good working condition. Next, conduct a trial spraying and debugging to check the spraying effect to ensure that the spraying is uniform, without blockage, sagging, etc. Then, perform the two-component spraying operation according to the set spraying process parameters.

[0066] Optionally, monitor the working status and spraying effect of the spraying equipment in real time to promptly discover and deal with problems that arise during the spraying process. After the spraying is completed, conduct a comprehensive inspection of the spraying effect to ensure that the spraying quality meets the requirements.

[0067] Furthermore, the method further comprises:

[0068] Obtain a spray gun wear relationship model. Collect target spray gun control records and traverse to extract key loss information sets. Take the key loss information set as input parameters, call the spray gun wear relationship model to perform wear integration, and obtain the wear accumulation information of the target spray gun. Establish a wear-speed correction model, correct the spray speed according to the wear accumulation information of the target spray gun, and obtain the wear correction coefficient. Update the target spray gun control record in real time, and based on the spray gun wear relationship model and the wear-speed correction model, update the wear correction coefficient, and obtain the dynamic wear correction coefficient for speed correction.

[0069] Specifically, first, a spray gun wear relationship model is established to describe the effect of spray gun wear on spraying effect. This means that based on experimental data and historical records, the wear degree of key components during the use of the spray gun is analyzed, and the relationship between spray gun wear and spraying speed and spraying quality is established.

[0070] Specifically, the target spray gun control record refers to information including operating parameters, spraying time, usage times, etc. during the use of the target spray gun since it was put into operation. The key wear information set is the data in the target spray gun control record that plays a major role in the wear and tear of the target nozzle.

[0071] Specifically, the wear relationship model is called to calculate the loss information of the spray gun under specific working conditions based on the input parameters. Then, the integral algorithm is used to accumulate the loss information to generate the wear accumulation information of the target spray gun.

[0072] Optionally, based on experimental data, the relationship between nozzle wear information and nozzle diameter, and the relationship between nozzle diameter and the amount of paint discharged per unit time and distribution area are obtained, and then a correction relationship between wear and spraying speed is established.

[0073] Specifically, based on the same principle of the aforementioned thickness-speed compensation method, the wear correction coefficient is obtained according to the wear accumulation information to correct the spraying speed. Exemplarily, the wear correction coefficient reflects the gap between the real-time target nozzle performance and the ideal nozzle performance, and the spraying speed is corrected by multiplying the target speed series by the wear correction coefficient.

[0074] The above steps and technical means dynamically adjust the spraying speed based on the real-time wear of the spray gun to ensure the spraying quality. Through automated monitoring and adjustment, manual intervention is reduced, and spraying efficiency and production consistency are improved.

[0075] In some implementations, obtaining a spray gun wear relationship model includes:

[0076] A historical spray gun loss data set is obtained, and key loss factors are determined by analysis, wherein the historical spray gun loss data set includes historical wear information and historical operation information.

[0077] Based on the key loss factors, the historical spray gun loss data set is lightened to generate a lightened historical spray gun loss data set.

[0078] The light industry historical spray gun loss data set is used as sample data to construct a spray gun wear relationship model, wherein the historical operation information is the model input sample, and the historical wear information is the model output sample.

[0079] Specifically, first, collect and organize historical spray gun loss data, including historical wear information and historical operation information. Then, through data analysis methods (such as correlation analysis, covariance matrix, principal component analysis, etc.), determine the key factors affecting spray gun wear. Then, according to the determined key loss factors, the historical spray gun loss data set is lightweighted. Including data cleaning, data screening, feature selection, data conversion and other steps to generate a lighter historical spray gun loss data set with smaller data scale, less redundant data and higher data quality.

[0080] Furthermore, the light-weight historical spray gun loss dataset is used to construct a spray gun wear relationship model, which describes the relationship between the wear of the spray gun and the operation information. In this model, the historical operation information is the input of the model, and the historical wear information is the output of the model.

[0081] Optionally, the spray gun wear relationship model can be a neural network model or a numerical model based on regression analysis, which is determined based on specific application scenarios and requirements. For example, if the relationship between the spray gun wear condition and the operation information is very complex, or the data set is large, the spray gun wear relationship model is constructed and trained based on a neural network. If the relationship between the spray gun wear condition and the operation information is relatively simple, or the data set is not large, the numerical model based on regression analysis has better performance.

[0082] Optionally, based on the knowledge distillation method, the acquired spray gun wear relationship model is simplified to reduce the computational requirements of the spray gun wear relationship model while maintaining the model performance, thereby increasing the running speed, which in turn helps in the application and promotion in actual spraying.

[0083] Furthermore, the method further comprises:

[0084] Obtain the historical cleaning and maintenance data of the target spray gun, and determine the fault-operation duration characteristic information of the target spray gun based on the statistical analysis method. Define the cumulative self-cleaning constraint based on the fault-operation duration characteristic information and the preset safety factor. Based on the performance specification data of the target spray gun, extract the average trouble-free operation time of the target spray gun and configure it as a periodic self-cleaning constraint. Configure the intermittent self-cleaning constraint based on the real-time two-component dry-solid characteristics. Combine the cumulative self-cleaning constraint, the periodic self-cleaning constraint and the intermittent self-cleaning constraint to perform self-cleaning management of the target spray gun.

[0085] Specifically, configure self-cleaning constraints, including cumulative self-cleaning constraints, periodic self-cleaning constraints, and intermittent self-cleaning constraints. Among them, the periodic self-cleaning constraint sets the cleaning cycle of the spraying equipment. For example, cleaning is performed every 8 hours or after work every day.

[0086] Specifically, the cumulative self-cleaning constraint is used to set a threshold of the cumulative spraying workload of the spraying equipment, including a threshold of the spraying time or the spraying volume. For example, when the cumulative spraying time of the spraying equipment reaches 40 hours or the cumulative spraying volume reaches 1000 liters, cleaning is performed.

[0087] Specifically, the intermittent self-cleaning constraint defines how long the operation is expected to be suspended or interrupted before self-cleaning is required. The intermittent self-cleaning constraint is determined by analyzing the curing time of the two-component material. For example, if the curing time of the two-component after mixing is 30 minutes, the intermittent self-cleaning constraint can be set to trigger self-cleaning when the expected interruption exceeds 20 minutes, to clean the residue inside the spray equipment and the spray gun, and prevent the dry solid material from clogging the nozzle or affecting the subsequent spraying quality.

[0088] Specifically, when any one of the periodic self-cleaning constraint, cumulative self-cleaning constraint, and intermittent self-cleaning constraint is met, the cleaning procedure of the spray equipment is executed. Including: disassembling the spray gun, using a special cleaning fluid to thoroughly clean the inside of the spray gun and the nozzle to ensure that there is no residue blocking the nozzle; using a special cleaning fluid to flush the spray pipeline to ensure that there is no residue inside the pipeline. Clean the two-component mixing device to ensure that there is no residue in the mixing device that affects the mixing effect. Clean or replace the filter device to ensure a good filtering effect. After cleaning, dry the spray device to ensure that the inside is dry and free of residue.

[0089] By configuring self-cleaning constraints and performing regular cleaning, you can ensure the continued efficient operation of the spray equipment, avoid problems such as blockage and uneven mixing during the spraying process, thereby improving the spraying quality, extending the equipment life, and reducing maintenance costs.

[0090] In summary, the two-component spraying method for automotive interior products provided by the present invention has the following technical effects:

[0091] By obtaining the shape feature data of the target product and dividing it into zones. According to the zone division results and the spraying process plan, the spraying path is planned, and the initial spraying path of the initial speed series is obtained and marked. Based on the initial spraying path, the spray gun height series is obtained, and the initial speed series is height-speed compensated to obtain the height-compensated speed series. Combined with the shape feature data, the initial spraying path and the height-compensated speed series, simulated spraying is performed, and thickness-speed compensation is performed according to the results to obtain the thickness-compensated speed series. The speed mutation points in the thickness-compensated speed series are extracted for advance speed compensation to generate the target speed series. Finally, the initial spraying path is associated with the target speed series to perform two-component spraying of the target product. Thereby achieving the technical effect of reducing the process control cost and improving the process control efficiency and spraying quality.

[0092] Embodiment 2

[0093] Figure 2 Schematic diagram of the structure of a two-component spraying device for automotive interior products according to the present invention. Figure 1 The schematic flow diagram of a two-component spraying method for automotive interior products of the present invention can be shown as follows: Figure 2 The structure shown is implemented.

[0094] Based on the same concept as the two-component spraying method for automobile interior products in the embodiment, the present invention also provides a two-component spraying device for automobile interior products, comprising:

[0095] The product classification module 11 is used to obtain the appearance feature data of the target product and perform partitioning based on the appearance feature data.

[0096] The initial path generation module 12 is used to plan the spraying path according to the partition division result and the spraying process scheme to obtain the initial spraying path, wherein the initial spraying path is associated with an initial speed series.

[0097] The height compensation module 13 is used to obtain a spray gun height series based on the initial spraying path, and to perform height-speed compensation on the initial speed series according to the spray gun height series to obtain a height-compensated speed series.

[0098] The thickness compensation module 14 is used to perform simulated spraying based on the shape feature data, in combination with the height compensation speed series and the initial spraying path, and perform thickness-speed compensation according to the simulated spraying results to output a thickness compensation speed series.

[0099] The speed change compensation module 15 is used to identify and extract the speed mutation points in the thickness compensation speed series to perform speed change advance compensation and generate a target speed series.

[0100] The spraying execution module 16 is used to associate the initial spraying path with the target speed series to perform two-component spraying of the target product.

[0101] Wherein, the height compensation module 13 comprises:

[0102] The height calculation unit is used to analyze the initial spraying path, determine the relative height of the target spray gun at each position, and store it as the spray gun height series.

[0103] The mapping calibration unit is used to calibrate and obtain the discharge flow rate-spray gun height mapping baseline of the target two-component.

[0104] The flow deviation calculation unit is used to traverse the discharge flow-spray gun height mapping baseline, obtain the discharge flow series corresponding to the spray gun height series, calculate the flow deviation between the discharge flow series and the spraying process solution, and output the flow deviation series.

[0105] The compensation analysis and compensation unit is used to calculate and obtain a height-speed compensation coefficient series based on the flow deviation series, perform height-speed compensation according to the height-speed compensation coefficient series, and generate the height-compensated speed series.

[0106] In some embodiments, the thickness compensation module 14 includes:

[0107] The simulation construction unit is used to construct a simulation spraying space based on the shape feature data.

[0108] An initialization unit is used to initialize the spraying process parameters and the starting position of the nozzle in the simulated spraying space based on the spraying process plan.

[0109] The simulated spraying unit is used to fit the height compensation speed series and the initial spraying path, perform simulated spraying in the simulated spraying space, and obtain simulated thickness distribution data.

[0110] The thickness difference compensation unit is used to analyze the thickness difference between the simulated thickness distribution data and the target thickness data, calculate and obtain the difference correction coefficient distribution to perform thickness-speed compensation, and output a thickness compensation speed series.

[0111] In some embodiments, the speed change compensation module 15 includes:

[0112] The inflection point acquisition unit is used to analyze the height compensation speed series, identify the speed mutation point, and obtain a speed inflection point set, wherein the speed inflection point set is marked with an inflection point speed change amount.

[0113] The speed change compensation calculation unit is used to traverse the speed inflection point set, extract the inflection point speed change amount to calculate the speed change compensation amount, and obtain the speed change compensation data.

[0114] The compensation updating unit is used to update the speed control point position in the thickness compensation speed series based on the speed change compensation data to obtain a target speed series.

[0115] Furthermore, the device also includes:

[0116] The wear relationship unit is used to obtain the spray gun wear relationship model.

[0117] The record acquisition unit is used to collect the target spray gun control records and traverse and extract the key loss information set.

[0118] The cumulative calculation unit is used to use the key loss information set as an input parameter, call the spray gun wear relationship model to perform wear integration, and obtain the wear accumulation information of the target spray gun.

[0119] The wear correction conversion unit is used to establish a wear-speed correction model, correct the spraying speed according to the wear accumulation information of the target spray gun, and obtain the wear correction coefficient.

[0120] The dynamic correction unit is used to update the target spray gun control record in real time, and based on the spray gun wear relationship model and the wear-speed correction model, update the wear correction coefficient, and obtain the dynamic wear correction coefficient for speed correction.

[0121] In some implementations, the wear relationship unit includes:

[0122] The loss factor unit is used to obtain a historical spray gun loss data set and analyze and determine key loss factors, wherein the historical spray gun loss data set includes historical wear information and historical operation information.

[0123] The data reduction unit is used to perform lightening processing on the historical spray gun loss data set based on the key loss factor to generate a lightened historical spray gun loss data set.

[0124] The model building unit is used to build a spray gun wear relationship model using the light historical spray gun loss data set as sample data, wherein the historical operation information is the model input sample and the historical wear information is the model output sample.

[0125] Furthermore, the device also includes:

[0126] The characteristic analysis unit is used to obtain the historical cleaning and maintenance data of the target spray gun, and determine the fault-operation duration characteristic information of the target spray gun based on the statistical analysis method.

[0127] The cumulative constraint unit is used to define the cumulative self-cleaning constraint according to the fault-operation duration characteristic information in combination with a preset safety factor.

[0128] The cycle constraint unit is used to extract the mean trouble-free operation time of the target spray gun based on the performance specification data of the target spray gun, and is configured as a cycle self-cleaning constraint.

[0129] The intermittent constraint unit is used to configure intermittent self-cleaning constraints based on the real-time two-component dry-solid characteristics.

[0130] The self-cleaning control unit is used to perform self-cleaning management of the target spray gun by combining the cumulative self-cleaning constraint, the periodic self-cleaning constraint and the intermittent self-cleaning constraint.

[0131] It should be understood that the embodiments mentioned in this specification focus on their differences from other embodiments. The specific embodiments in the aforementioned embodiment one are also applicable to a two-component spray device for automotive interior products described in embodiment two. For the sake of brevity of the specification, no further elaboration is given here.

[0132] It should be understood that the embodiments disclosed in the present invention and the above description can enable those skilled in the art to use the present invention to implement the present invention. At the same time, the present invention is not limited to the above-mentioned embodiments. It should be understood that those skilled in the art can still modify the technical solutions recorded in the above-mentioned embodiments, or replace some of the technical features therein by equivalents; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention, and should be included in the protection scope of the present invention.

Claims

1. A two-component spraying method for automotive interior products, characterized in that: The method comprises: Acquire appearance feature data of the target product, and divide the product into zones based on the appearance feature data; According to the partitioning result, the spraying path is planned in combination with the spraying process plan to obtain an initial spraying path, wherein the initial spraying path is associated with an initial speed series; Based on the initial spraying path, a spray gun height series is obtained, and height-speed compensation is performed on the initial speed series according to the spray gun height series to obtain a height-compensated speed series; Based on the shape feature data, the height compensation speed series and the initial spraying path are combined to perform simulated spraying, and thickness-speed compensation is performed according to the simulated spraying results to output a thickness compensation speed series; Identify and extract the speed mutation points in the thickness compensation speed series to perform speed change advance compensation and generate a target speed series; The initial spraying path is associated with the target speed series to perform two-component spraying of a target product.

2. A two-component spraying method for automotive interior products according to claim 1, characterized in that: Based on the initial spraying path, a spray gun height series is obtained, and height-speed compensation is performed on the initial speed series according to the spray gun height series to obtain a height-compensated speed series, including: Parsing the initial spraying path, determining the relative height of the target spray gun at each position, and storing it as the spray gun height series; Calibrate to obtain the discharge flow rate-spray gun height mapping baseline of the target two-component; Traversing the discharge flow rate-spray gun height mapping baseline, obtaining the discharge flow rate series corresponding to the spray gun height series, calculating the flow rate deviation between the discharge flow rate series and the spraying process solution, and outputting the flow rate deviation series; An altitude-speed compensation coefficient series is calculated based on the flow deviation series, and altitude-speed compensation is performed according to the altitude-speed compensation coefficient series to generate the altitude-compensated speed series.

3. A two-component spraying method for automotive interior products as claimed in claim 2, characterized in that: Based on the shape feature data, the height compensation speed series and the initial spraying path are combined to perform simulated spraying, and thickness-speed compensation is performed according to the simulated spraying results to output a thickness compensation speed series, including: Based on the shape feature data, construct a simulated spraying space; Initializing spraying process parameters and a nozzle starting position in the simulated spraying space based on the spraying process scheme; Fitting the height compensation speed series with the initial spraying path, performing simulated spraying in the simulated spraying space, and obtaining simulated thickness distribution data; The thickness difference analysis between the simulated thickness distribution data and the target thickness data is performed, and the difference correction coefficient distribution is calculated to perform thickness-speed compensation, and a thickness compensation speed series is output.

4. A two-component spraying method for automotive interior products as claimed in claim 3, characterized in that: Identifying and extracting the speed mutation point in the thickness compensation speed series to perform speed change advance compensation and generate a target speed series, including: Analyze the height compensation speed series, identify the speed mutation point, and obtain a speed inflection point set, wherein the speed inflection point set is marked with an inflection point speed change amount; Traversing the speed inflection point set, extracting the inflection point speed change amount to calculate the speed change compensation amount, and obtaining the speed change compensation data; The speed control point positions in the thickness compensation speed series are updated based on the speed change compensation data to obtain a target speed series.

5. A two-component spraying method for automotive interior products according to claim 1, characterized in that: The method further includes: performing speed correction based on the wear condition of the target spray gun, specifically including: Obtaining a spray gun wear relationship model; Collect target spray gun control records and traverse to extract key loss information sets; Taking the key loss information set as input parameters, calling the spray gun wear relationship model to perform wear integration, and obtaining wear accumulation information of the target spray gun; Establishing a wear-speed correction model, correcting the spraying speed according to the wear accumulation information of the target spray gun, and obtaining a wear correction coefficient; The target spray gun control record is updated in real time, and based on the spray gun wear relationship model and the wear-speed correction model, the wear correction coefficient is updated, and a dynamic wear correction coefficient is obtained to perform speed correction.

6. The method according to claim 5, characterized in that Get the spray gun wear relationship model, including: Acquire a historical spray gun loss data set, analyze and determine key loss factors, wherein the historical spray gun loss data set includes historical wear information and historical operation information; Based on the key loss factors, the historical spray gun loss data set is lightened to generate a lightened historical spray gun loss data set; The light industry historical spray gun loss data set is used as sample data to construct a spray gun wear relationship model, wherein the historical operation information is the model input sample, and the historical wear information is the model output sample.

7. A two-component spraying method for automotive interior products according to claim 1, characterized in that: The method further includes: performing self-cleaning management on the target spray gun, specifically including: Obtain historical cleaning and maintenance data of the target spray gun, and determine the fault-operation duration characteristic information of the target spray gun based on statistical analysis methods; According to the fault-operation duration characteristic information and in combination with a preset safety factor, a cumulative self-cleaning constraint is defined; Based on the performance specification data of the target spray gun, the mean trouble-free operation time of the target spray gun is extracted and configured as a periodic self-cleaning constraint; Based on the real-time two-component dry-solid characteristics, configure intermittent self-cleaning constraints; The cumulative self-cleaning constraint, the periodic self-cleaning constraint and the intermittent self-cleaning constraint are combined to perform self-cleaning management of the target spray gun.

8. A two-component spraying device for automotive interior products, characterized in that: The device is used to perform a two-component spraying method for automotive interior products according to any one of claims 1 to 7, and the device comprises: A product division module, the product division module is used to obtain the appearance feature data of the target product and divide the product into zones based on the appearance feature data; An initial path generation module, the initial path generation module is used to plan the spraying path according to the partition division result and the spraying process scheme, and obtain an initial spraying path, wherein the initial spraying path is associated with an initial speed series; A height compensation module, the height compensation module is used to obtain a spray gun height series based on the initial spraying path, and perform height-speed compensation on the initial speed series according to the spray gun height series to obtain a height compensated speed series; A thickness compensation module, the thickness compensation module is used to perform simulated spraying based on the shape feature data, in combination with the height compensation speed series and the initial spraying path, and perform thickness-speed compensation according to the simulated spraying result, and output a thickness compensation speed series; A speed change compensation module, the speed change compensation module is used to identify and extract speed mutation points in the thickness compensation speed series to perform speed change advance compensation and generate a target speed series; A spraying execution module is used to associate the initial spraying path with the target speed series to perform two-component spraying of a target product.