A die casting mold

By setting a communication groove in the second chamber of the die-casting mold and setting an inner gate that is biased towards the second chamber on both sides of the mold cavity to control the intersection order and position of the metal liquid, the problem of bubble formation during the metal liquid convergence is solved. Improved product quality.

CN118650134BActive Publication Date: 2024-11-29CHENGDU WEIDA MASCH MFG CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411149791.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-29
Estimated Expiration
2044-08-21

AI Technical Summary

Technical Problem

When using die-casting technology to manufacture tee pipe fittings or products with similar structures, liquid metal is prone to bubbles when it converges, resulting in pores in the product and reducing product quality.

Method used

Design a die-casting mold, by providing a communication groove in the second chamber and symmetrically disposed on both sides of the mold cavity along the reference, the two inner gates connecting to the first chamber at least partially deviate toward the second The chamber is arranged to control the order and position of the metal liquid intersecting.

Benefits of technology

By controlling the intersection order and position of metal liquid, the intense movement of metal liquid during convergence is reduced, the formation of bubbles is reduced, and the pores in the product after cooling and shaping are reduced, and the product quality is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118650134B_ABST
    Figure CN118650134B_ABST
Patent Text Reader

Abstract

The present invention discloses a die-casting mold, wherein a connecting groove is arranged in a second cavity, and two inner gates connected to a first cavity are symmetrically arranged along a reference plane on both sides of the cavity, and the two inner gates are at least partially arranged toward the second cavity. When molten metal enters the cavity from the two inner gates, two streams of molten metal will be generated. The two streams of molten metal have two pairs of fronts moving toward each other, one pair of which intersects at a side where the first cavity is connected to the second cavity, and the other pair of which intersects at a side of the first cavity away from the second cavity. Since the two inner gates are partially arranged toward the second cavity, the former will intersect first and enter the second cavity, resulting in a lower flow rate of the latter, and a gentler intersection, so that air is not easily mixed in. When the former intersects, the molten metal mixed with gas will be discharged to the first overflow groove, thereby reducing the possibility of air holes in the product after cooling and finalization.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of die-casting processing, in particular to a die-casting die. Background Art

[0002] When using die-casting technology to manufacture three-way pipe fittings or products with similar structures, one end face of the main pipeline of the product or the symmetrical surface of the product is usually selected as the parting surface. The former usually selects one side of the end face to set the gate, and the latter usually selects the two opposite sides of the end face to set the gate. Both methods will cause the molten metal to converge along the circumferential direction along the side wall of the main pipeline. The fronts of different streams of molten metal that converge move towards each other, causing the fronts of different streams of molten metal to collide with each other during convergence, causing bubbles to be mixed into the molten metal, and the confluence position is relatively random and difficult to control accurately, making it difficult for the molten metal mixed with bubbles to be discharged from the mold cavity. In this case, when the product is cooled and formed, air holes are likely to be generated, thereby reducing the quality of the product. Summary of the invention

[0003] In order to solve the above-mentioned problems in the prior art, the present invention provides a die-casting mold, which can improve the quality of die-casting of three-way pipe fittings or products with similar structures.

[0004] To achieve the above object, the present invention discloses a die-casting mold, comprising:

[0005] A front mold, the front mold comprising a first surface;

[0006] A rear mold, the rear mold comprising a second surface, the second surface being opposite to and parallel to the first surface; the first surface and the second surface are symmetrically recessed relative to a reference surface to form a mold cavity, the mold cavity at least comprising a first cavity and a second cavity, the first cavity being arranged along a first direction, the second cavity being arranged along a second direction and connected to the first cavity;

[0007] A pouring system, the pouring system comprising an ingate, the ingate being symmetrically arranged on the first surface and the second surface relative to the reference surface, the ingate being at least connected to the first cavity and at least partially arranged toward the second cavity; the ingate being at least used to control the order and position of the intersection of the molten metals;

[0008] The first surface and / or the second surface is further provided with a first overflow groove, and the first overflow groove is connected to at least the distal end of the second chamber relative to the reference surface and the junction of the second chamber and the reference surface through a connecting structure;

[0009] The reference plane is an imaginary plane parallel to and equidistant from the first plane and the second plane; the first direction is the width direction of the rear mold, and the second direction is the length direction of the rear mold.

[0010] As an optional embodiment, the inner gate is connected to the far end of the first cavity relative to the reference plane along the first direction, and the width of the inner gate gradually increases in the direction approaching the cavity, and the increase ratio toward one side of the second cavity is greater than that on the other side.

[0011] As an optional embodiment, the second chamber further includes a connecting groove, which is provided at a wall surface where the second chamber intersects with the reference surface and connects with a boundary between the first chamber and the reference surface along the second direction.

[0012] As an optional embodiment, the first surface and the second surface are also provided with a second overflow groove, the second overflow groove is arranged opposite to the inner gate, and the second overflow groove is connected to the junction of the first chamber and the reference surface and the far end relative to the reference surface through the connecting structure.

[0013] As an optional embodiment, the connecting structure includes a first channel and a second channel, the first channel is arranged along the first direction or the second direction, one end of the first channel is connected to the first overflow groove or the second overflow groove, and the other end gradually increases in width at least toward one side of the cavity to connect the first chamber or the second chamber with the junction of the reference surface; one end of the second channel is connected to the first overflow groove or the second overflow groove, and the other end is connected to the far end relative to the reference surface along the first direction or the second direction, and the width of the second channel is uniform.

[0014] As an optional embodiment, a piping system is provided inside the front mold, and a cooling fluid flows through the piping system. The piping system includes two longitudinal tubes and one transverse tube, the two longitudinal tubes are arranged along the first direction, and the two longitudinal tubes are arranged opposite to the second chamber along the second direction, the two longitudinal tubes at least pass through one side of the rear mold along the first direction, the transverse tube is arranged inside the front mold along the second direction, and the transverse tube connects the ends of the two longitudinal tubes.

[0015] As an optional embodiment, the die-casting mold also includes a core pulling mechanism, which includes a first core, a second core and a third core, the first core and the second core are arranged along a first direction, the first core extends from one end of the first cavity into the first cavity, the second core extends from the other end of the first cavity into the first cavity, the first core abuts against the end faces of the second core, and the length of the first core in the first cavity is greater than that of the second core; the third core passes through the first cavity from the end face of the second cavity along the second direction, and the end face of the third core is attached to and abuts against the outer peripheral surface of the first core.

[0016] As an optional embodiment, the cavity, the core pulling mechanism, the inner gate and the first overflow groove form a molding system, and the die-casting mold includes two molding systems, and the two molding systems are symmetrically arranged along the second direction relative to the midline of the rear mold length.

[0017] As an optional embodiment, the core pulling mechanism further includes a first slider seat and a second slider seat, the first core and the second core are connected to the first slider seat, the third core is connected to the second slider seat, the first slider seat is arranged on both sides of the rear mold along the first direction, and the second slider seat is arranged on the side of the rear mold along the second direction;

[0018] The first slider seat is provided with a first guide hole, the axis of which is inclined from both sides of the rear mold to the center of the rear mold along the first direction, and the second slider seat is provided with a second guide hole, the axis of which is inclined from both sides of the rear mold to the center of the rear mold along the second direction;

[0019] The front mold is provided with a first oblique guide rod corresponding to the first guide hole, and the first oblique guide rod is slidably matched with the first guide hole; the front mold is provided with a second oblique guide rod corresponding to the second guide hole, and the second oblique guide rod is slidably matched with the second guide hole.

[0020] As an optional embodiment, the core pulling mechanism also includes a screw rod, which is arranged along the first direction, one end of which is connected to the first slider seat, and the other end is connected to a spring, and the spring is fixedly arranged, and the maximum elastic force of the spring is at least greater than 2 times the sum of the gravity of the first slider seat, the screw rod and the first core.

[0021] The beneficial effects of the present invention are:

[0022] The die-casting mold of the present invention arranges a connecting groove in the second cavity, and arranges two inner gates connected to the first cavity symmetrically along the reference plane on both sides of the cavity. The two inner gates are at least partially arranged toward the second cavity. When the molten metal enters the cavity from the two inner gates, two streams of molten metal will be generated. The two streams of molten metal have two pairs of fronts moving toward each other, one pair of which intersects on the side where the first cavity is connected to the second cavity, and the other pair of which intersects on the side of the first cavity away from the second cavity. Since the two inner gates are partially arranged toward the second cavity, the former will intersect first and enter the second cavity, resulting in a lower flow rate of the latter and a gentler intersection, so that it is not easy to mix with air. When the former intersects, the molten metal mixed with gas will be discharged to the first overflow groove, thereby reducing the possibility of pores in the product after cooling and finalization. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 A schematic diagram of the die-casting mold provided by the present invention;

[0024] Figure 2 for Figure 1 Exploded diagram of the die casting mold;

[0025] Figure 3 for Figure 1 A front view of the first side of the middle front mold;

[0026] Figure 4 for Figure 1 A front view of the second side of the middle rear mold;

[0027] Figure 5 for Figure 4 A partial enlarged view of the middle L area;

[0028] Figure 6 It is a schematic diagram of the flow of molten metal in the cavity;

[0029] Figure 7 for Figure 1 Schematic diagram of the cross section of the center front mold along the plane where the pipeline system is located.

[0030] Reference numerals:

[0031] reference surface, 100;

[0032] Front mold, 1; first surface, 11; first overflow groove, 111; second overflow groove, 112; connecting structure, 113; first channel, 1131; second channel, 1132; pipeline system, 12; longitudinal pipe, 121; transverse pipe, 122; clamping groove, 13; locking block, 131; third inclined surface, 1311;

[0033] rear mold, 2; second surface, 21; mold cavity, 22; first cavity, 221; second cavity, 222; connecting groove, 222a;

[0034] Gating system, 3; Ingate, 31; Runner, 32; First branch, 321; Second branch, 322;

[0035] Core pulling mechanism, 4; first core, 41; second core, 42; third core, 43; first slider seat, 44; first guide hole, 441; first oblique guide rod, 442; threaded rod, 443; spring, 444; first clamping portion, 445; first inclined surface, 4451; second slider seat, 45; second guide hole, 451; second oblique guide rod, 452; second clamping portion, 453; second inclined surface, 4531;

[0036] Push rod mechanism, 5;

[0037] The first direction is Y; the second direction is X. DETAILED DESCRIPTION

[0038] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0039] In the present invention, the directions or positional relationships indicated by the terms "upper", "lower", "left", "right", "front", "back", "top", "bottom", "inner", "outer", "middle", "vertical", "horizontal", "lateral", "longitudinal" and the like are based on the directions or positional relationships shown in the drawings. These terms are mainly used to better describe the present invention and its embodiments, and are not used to limit the indicated devices, elements or components to have a specific direction, or to be constructed and operated in a specific direction.

[0040] In addition, some of the above terms may be used to express other meanings in addition to indicating orientation or positional relationship. For example, the term "on" may also be used to express a certain dependency or connection relationship in some cases. For those skilled in the art, the specific meanings of these terms in the present invention can be understood according to specific circumstances.

[0041] In addition, the terms "installed", "set", "provided with", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0042] In addition, the terms "first", "second", etc. are mainly used to distinguish different devices, elements or components (the specific types and structures may be the same or different), and are not used to indicate or imply the relative importance and quantity of the indicated devices, elements or components. Unless otherwise specified, the meaning of "multiple" is two or more. In the description of the embodiments of the present invention, it should be understood that "-" and "~" represent the same range of two numerical values, and the range includes the endpoints. For example: "AB" means a range greater than or equal to A, and less than or equal to B. "A~B" means a range greater than or equal to A, and less than or equal to B.

[0043] In the description of the embodiments of the present invention, the term "and / or" herein is merely a description of the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B may represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " herein generally indicates that the associated objects before and after are in an "or" relationship.

[0044] When using die-casting technology to manufacture three-way pipe fittings or products with similar structures, one end face of the main pipeline of the product (i.e., the pipeline with two openings on the same axis) or the symmetrical surface of the product is usually selected as the parting surface. The former usually selects one side of the end face to set the ingate, and the latter usually selects the two opposite sides of the end face to set the ingate. Both methods will cause the molten metal to converge along the circumferential direction along the side wall of the main pipeline, and the front faces of different strands of molten metal that converge move towards each other, resulting in the front faces of different strands of molten metal colliding with each other during convergence, which is easy to form turbulence and eddy currents, causing bubbles to be mixed in the molten metal. In addition, the confluence position is relatively random and difficult to control accurately, which makes it difficult for the molten metal mixed with bubbles to discharge from the mold cavity and enter the overflow tank, that is, the molten metal mixed with bubbles stays in the mold cavity with other normal molten metal and is cooled and formed, and stays inside the product. In this case, when the product is cooled and formed, it is easy to produce pores, thereby reducing the quality of the product.

[0045] Based on this, the present invention discloses a die-casting mold, which arranges a connecting groove in the second cavity, and arranges two inner gates connected to the first cavity symmetrically along a reference plane on both sides of the cavity, and the two inner gates are at least partially biased toward the second cavity. When the molten metal enters the cavity from the two inner gates, two streams of molten metal will be generated. The two streams of molten metal have two pairs of fronts moving toward each other, one pair of which intersects on the side where the first cavity is connected to the second cavity, and the other pair of which intersects on the side of the first cavity away from the second cavity. Since the two inner gates are partially biased toward the second cavity, the former will intersect first and enter the second cavity, resulting in a lower flow rate of the latter, and a gentler intersection, so that it is not easy to mix with air. When the former intersects, the molten metal mixed with gas will be discharged to the first overflow groove, thereby reducing the possibility of air holes in the product after cooling and shaping.

[0046] The technical solution of the present invention will be further described below in conjunction with embodiments and drawings.

[0047] See also Figures 1 to 5The present embodiment provides a die-casting mold, comprising: a front mold 1, a rear mold 2, and a pouring system 3. The front mold 1 comprises a first surface 11. The rear mold 2 comprises a second surface 21, and the second surface 21 is arranged opposite to and parallel to the first surface 11. The first surface 11 and the second surface 21 are symmetrically recessed relative to the reference surface 100 to form a cavity 22, and the cavity 22 at least comprises a first cavity 221 and a second cavity 222 in a cylindrical cavity, the first cavity 221 is arranged along a first direction Y, and the second cavity 222 is arranged along a second direction X and connected to the first cavity 221, and the pouring system 3 comprises an inner gate 31, and an inner gate 31 is respectively arranged on the first surface 11 and the second surface 21, and the two inner gates 31 are symmetrically arranged relative to the reference surface 100, and the inner gate 31 is connected to the far end of the first cavity 221 relative to the reference surface 100 along the first direction Y, and the inner gate 31 is arranged at least partially toward the second cavity 222, at least for controlling the order and position of the intersection of the metal liquids.

[0048] The first surface 11 and / or the second surface 21 is further provided with a first overflow groove 111 , which is connected to the far end of the second chamber 222 relative to the reference surface 100 and the junction of the second chamber and the reference surface 100 through a connecting structure 113 .

[0049] The reference plane 100 is an imaginary plane parallel to and equidistant from the first surface 11 and the second surface 21. The first direction Y is the width direction of the rear mold 2, and the second direction X is the length direction of the rear mold 2.

[0050] like Figure 6As shown, when the molten metal enters the mold cavity 22 from the two ingates 31, two streams of molten metal will appear. The two streams of molten metal have two pairs of fronts moving toward each other, hereinafter referred to as A and B. A intersects at the side where the first chamber 221 and the second chamber 222 are connected, and B intersects at the side of the first chamber 221 away from the second chamber 222. Since the two ingates 31 are at least partially disposed toward the second chamber 222, the distance that A needs to flow through for the intersection is shorter, so it will intersect first and enter the second chamber 222, which makes Ade The cross-sectional area of ​​the flow space perpendicular to the streamline of A increases, which will cause A to flow in all directions to fill the surrounding space, thereby reducing the depth of A (especially as shown in the accompanying drawings, the second chamber 222 has a flange-like structure, so that this part itself is lower than the bottom of the first chamber 221), and due to the confluence of A, the volume of the molten metal is larger, the temperature drops more slowly, and the fluidity is better. A combination of various factors makes it easier for the molten metal that subsequently enters the cavity 22 to be replenished to A rather than B, which leads to a decrease in the flow rate of B, thereby reducing the intensity of the front collision when B intersects, reducing the turbulence or eddy current generated after the intersection of B, and making it difficult for B to mix with air. Although the collision of the metal fronts at the confluence of A is more intense, the subsequent replenished molten metal will push the molten metal mixed with gas at the confluence of the former to both sides of the second chamber 222 along the normal direction of the reference surface 100. As the molten metal continues to be injected, these molten metal mixed with bubbles will be discharged to the first overflow groove 111 connected to the far end of the second chamber 222 relative to the reference surface. Even if there is some that is not completely discharged, as the molten metal is further injected, the remaining molten metal mixed with gas will also be discharged to the first overflow groove 111 connected to the junction of the second chamber 222 and the reference surface. It can be seen that the die-casting mold of this embodiment can reduce the possibility of pores after the product is cooled and finalized.

[0051] Optionally, the ingates 31 are connected to the far end of the first chamber 221 relative to the reference plane 100 along the first direction Y, and the width of the ingates 31 gradually increases in the direction close to the mold cavity 22, and the increase rate toward the second chamber 222 is greater than the other side. In order to achieve A intersecting before B, the two ingates 31 can be arranged eccentrically, that is, the two ingates 31 are arranged toward the second chamber 222 as a whole, or the solution of this embodiment can be adopted. Compared with the former, the solution of this embodiment has a shorter distance for B to reach the intersection position, less mold coating is contacted before the intersection, and the temperature drop is smaller, which is conducive to reducing the probability of cold shut, flow marks or pores and slag holes in the product formed by B metal liquid.

[0052] Optionally, the second chamber 222 further includes a connecting groove 222a, which is disposed at the wall where the second chamber 222 intersects with the reference surface 100, and is connected to the junction of the first chamber 221 and the reference surface 100 along the second direction X. Since the connecting groove 222a is disposed in the area where A converges, A will flow into the connecting groove 222a after converging, providing a guide for the process of A entering the second chamber 222. The molten metal mixed with gas that first enters the second chamber 222 is pushed by the subsequent molten metal that enters from the connecting groove 222a, and is transferred from the middle of the second chamber 222 to both sides, so that the molten metal mixed with gas is more easily discharged into the first overflow groove 111, avoiding it from remaining in the second chamber 222, causing defects such as bubbles to appear in the product after cooling and forming.

[0053] In addition, the metal in the connecting groove 222a can be polished off after the product is cooled and shaped, or it can be retained as a structure similar to a reinforcing rib, thereby enhancing the strength of the product structure.

[0054] Optionally, the first surface 11 and the second surface 21 are further provided with a second overflow groove 112, which is arranged opposite to the inner gate 31, and the second overflow groove 112 is connected to the junction of the first chamber 221 and the reference surface 100 and the far end relative to the reference surface 100 through the connecting structure 113. On the basis of the above, there is still a small possibility of gas mixing when B intersects, and as the molten metal continues to be injected, the molten metal that enters first gradually cools down. In addition, the gas generated by the coating may also be wrapped in the molten metal. The second overflow groove 112 is arranged to be connected to the junction of the first chamber 221 and the reference surface 100 and the far end relative to the reference surface 100, so as to discharge this part of the bad molten metal. Thereby improving the quality of the product after the final cooling and molding.

[0055] Optionally, the connecting structure 113 includes a first channel 1131 and a second channel 1132, wherein the first channel 1131 is arranged along the first direction Y or the second direction X, wherein one end of the first channel 1131 is connected to the first overflow groove 111 or the second overflow groove 112, and the other end gradually increases in width toward at least one side of the cavity 22 to connect to the junction of the first chamber 221 or the second chamber 222 with the reference surface 100; one end of the second channel 1132 is connected to the first overflow groove 111 or the second overflow groove 112, and the other end is connected to the junction of the first chamber 221 and / or the second chamber 222 with the reference surface 100 and the far end relative to the reference surface 100 along the first direction Y or the second direction X, and the width of the second channel 1132 is uniform. The first channel 1131 uses such a form, which can leave a sufficiently large space at the connection with the second overflow groove 112, and the space can be used to arrange the second channel 1132, which can save space on the first surface 11 and the second surface 21.

[0056] like Figure 7As shown, optionally, a piping system 12 is provided inside the front mold 1, and a cooling fluid is passed through the piping system 12. The piping system 12 includes two longitudinal tubes 121 and a transverse tube 122. The two longitudinal tubes 121 are arranged along the first direction Y, and the two longitudinal tubes 121 are arranged opposite to the second chamber 222 along the second direction X. The two longitudinal tubes 121 at least pass through one side of the rear mold 2 along the first direction Y, and the transverse tube 122 is arranged inside the front mold 1 along the second direction X, and the transverse tube 122 connects the ends of the two longitudinal tubes 121. The piping system 12 through which the cooling fluid passes can, on the one hand, reduce the temperature of the front mold 1 and speed up the heat dissipation of the front mold 1, thereby protecting the die-casting mold of this embodiment and extending the life of the die-casting mold. On the other hand, it can reduce the local mold temperature on the side of the first chamber 221 away from the second chamber 222. The lower mold temperature can speed up the cooling rate of the molten metal, reduce the gas solubility and improve the exhaust conditions, thereby helping to promote smoother discharge of the gas in the molten metal during the solidification process, and further reducing the possibility of porosity defects in the product formed by the first chamber 221.

[0057] Specifically, a lower mold temperature means that the mold can absorb heat from the molten metal faster, thereby accelerating the cooling rate of the molten metal. A faster cooling rate helps to shorten the solidification time of the molten metal, and a faster solidification rate helps to reduce the residence time of the gas in the molten metal, because the solubility of the gas in the molten metal decreases as the temperature decreases. Therefore, at a faster solidification rate, the gas in the molten metal will more easily reach a saturated state and precipitate. In addition, during the solidification process of the molten metal, due to the temperature drop and volume contraction, a certain negative pressure area will be formed inside the molten metal. In addition, the gas in the mold (including the gas dissolved in the molten metal and the air in the cavity 22) will move to the negative pressure area under the action of the pressure difference and try to discharge. A lower mold temperature helps to maintain this pressure difference and promote the discharge of gas. In addition, a lower mold temperature is more conducive to the rapid cooling and solidification of the molten metal in the mold, thereby reducing the time the molten metal stays in the exhaust channel and reducing the risk of increased viscosity due to long-term residence.

[0058] Specifically, one of the two longitudinal pipes 121 is a water inlet pipe, and the other is a water outlet pipe. The cooling fluid (such as water, mineral oil, etc.) enters from the water inlet pipe, flows through a section of the transverse pipe 122 connecting the two longitudinal pipes 121, and then flows out from the water outlet pipe.

[0059] Optionally, the die-casting mold also includes a core pulling mechanism 4, which includes a first core 41, a second core 42 and a third core 43. The first core 41 and the second core 42 are arranged along the first direction Y, the first core 41 extends from one end of the first cavity 221 into the first cavity 221, and the second core 42 extends from the other end of the first cavity 221 into the first cavity 221. The end faces of the first core 41 and the second core 42 are abutted against each other, and the length of the first core 41 in the first cavity 221 is greater than that of the second core 42; the third core 43 passes through the first cavity 221 from the end face of the second cavity 222 along the second direction X, and the end face of the third core 43 is attached to and abuts against the outer peripheral surface of the first core 41. By arranging the first core 41, the second core 42 and the third core 43 in this way, the gaps between the three can be staggered, thereby avoiding the generation of larger gaps at the interconnections among the first core 41, the second core 42 and the third core 43 due to processing and assembly errors, deformation caused by temperature and the like, resulting in the inflow of molten metal and defects such as flash (also known as flying fin defects, mold misalignment, etc.).

[0060] In addition, as shown in the attached drawings, the arrangement of the first core 41 and the second core 42 allows protrusions to be set at the ends of the first core 41 and the second core 42, so that the first chamber 221 produces an inner flange structure here, so that the product has an inner flange in this stroke, thereby improving the processability of the product to meet some special requirements.

[0061] Optionally, the cavity 22, the core pulling mechanism 4, the inner gate 31 and the first overflow groove 111 form a molding system, and the die-casting mold includes two molding systems, and the two molding systems are symmetrically arranged along the second direction X relative to the length midline of the rear mold 2. In this way, two products can be produced by one casting, which is conducive to improving the production efficiency of the die-casting mold of the embodiment.

[0062] Optionally, the core pulling mechanism 4 further includes a first slider seat 44 and a second slider seat 45, the first core 41 and the second core 42 are connected to the first slider seat 44, the third core 43 is connected to the second slider seat 45, the first slider seat 44 is arranged on both sides of the so-called rear mold 2 along the first direction Y, and the second slider seat 45 is arranged on the side of the rear mold 2 along the second direction X. The first slider seat 44 is provided with a first guide hole 441, the axis of which is inclined from both sides of the rear mold 2 to the center of the rear mold 2 along the first direction Y, and the second slider seat 45 is provided with a second guide hole 451, the axis of which is inclined from both sides of the rear mold 2 to the center of the rear mold 2 along the second direction X. The front mold 1 is provided with a first oblique guide rod 442 corresponding to the first guide hole 441, and the first oblique guide rod 442 is slidably matched with the first guide hole 441; the front mold 1 is provided with a second oblique guide rod 452 corresponding to the second guide hole 451, and the second oblique guide rod 452 is slidably matched with the second guide hole 451. The inclined guide rod and the guide hole cooperate to provide the core pulling force of the core pulling mechanism 4, which has a lower cost than hydraulic core pulling, and is beneficial to reducing the manufacturing cost of the die-casting mold of this embodiment. In addition, compared with the hydraulic core pulling method, the structure is simpler and more compact, which is convenient for placement and installation in the production area.

[0063] Optionally, the core pulling mechanism 4 further includes a threaded rod 443, which is arranged along the first direction Y, one end of which is connected to the first slider seat 44, and the other end of which is connected to a spring 444, which is fixedly arranged, and the maximum elastic force of the spring 444 is at least twice the sum of the gravity of the first slider seat 44, the threaded rod 443 and the first core 41. Preferably, the threaded rod 443 is only arranged on the first slider seat 44 located on the upper side of the rear mold 2. In actual production, the first slider seat 44 here is in a vertical state, and the threaded rod 443 and the spring 444 can pull the first slider seat 44 to prevent the first slider seat 44 from falling before the mold is closed, which affects the spraying of the paint and the coordination of the guide hole and the inclined guide rod during the mold closing.

[0064] It should be noted that the spring 444 can be fixed to structures such as the die-casting machine and the wall of the workshop.

[0065] Optionally, the first slider seat 44 and the second slider seat 45 include a first clamping portion 445, the first clamping portion 445 includes a first inclined surface 4451, the first inclined surface 4451 is parallel to the second direction X, and is inclined from the center of the rear mold 2 to the outer edge along the first direction Y; the second slider seat 45 includes a second clamping portion 453, the second clamping portion 453 includes a second inclined surface 4531, the second inclined surface 4531 is parallel to the first direction Y, and is inclined from the center of the rear mold 2 to the outer edge along the second direction X. A plurality of clamping grooves 13 are provided on the first surface 11, and the projection of each clamping groove 13 on the second surface 21 surrounds the first clamping portion 445 or the second clamping portion 453. A locking block 131 is provided on the side wall of the clamping groove 13, and the locking block 131 includes a third inclined surface 1311, and the third inclined surface 1311 is parallel to the first inclined surface 4451 or the second inclined surface 4531. The projection of the third inclined surface 1311 on the second surface 21 at least partially overlaps with the projection of the first inclined surface 4451 or the second inclined surface 4531 on the second surface 21. After mold closing, the locking block 131 presses the first clamping portion 445 and the second clamping portion 453 to overcome the expansion force during the pressing process and ensure the quality of product molding. In addition, it is easy to understand that different locking effects can be obtained by adjusting the thickness of the locking block 131 and the inclination angle of the third inclined surface 1311.

[0066] Optionally, the pouring system 3 further includes a runner 32, which is disposed on the second surface 21 and extends from the center line of the rear mold 2 to the first core 41 along the second direction X. A first branch channel 321 and a second branch channel 322 are further disposed at the end of the runner 32. The first branch channel 321 is disposed on the second surface 21 and extends from one side to the other side of the third core 43 along the second direction X. The inner gate 31 located on the first surface 11 is connected to the first branch channel 321; the second branch channel 322 is disposed on the first surface 11 and extends along the second direction X to be connected to the inner gate 31;

[0067] A push rod mechanism 5 is provided at the bottom of the first overflow trough 111, the second overflow trough 112, the runner 32 and the end of the first branch channel 321. The push rod mechanism 5 is used to push out the metal in the first overflow trough 111, the second overflow trough 112, the runner 32 and the end of the first branch channel 321. When blanking, the push rod mechanism 5 pushes out the metal in the first overflow trough 111, the second overflow trough 112, the runner 32 and the end of the first branch channel 321, and the products connected to these metals in the cavity 22 can be pushed out together, without the need to set a push rod on the wall of the cavity 22. The latter is easy to leave marks on the product due to factors such as the push rod or the gap between the push rod and the installation hole of the push rod, resulting in a decrease in the surface quality of the product.

[0068] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A die-casting mold for forming a three-way pipe fitting, characterized in that: include: A front mold, the front mold comprising a first surface; A rear mold, the rear mold comprising a second surface, the second surface being opposite to and parallel to the first surface; the first surface and the second surface are symmetrically recessed relative to a reference surface to form a mold cavity, the mold cavity at least comprising a first cavity and a second cavity, the first cavity being arranged along a first direction, the second cavity being arranged along a second direction and connected to the first cavity; A pouring system, the pouring system comprising an ingate, the ingate being symmetrically arranged on the first surface and the second surface relative to the reference surface, the ingate being at least connected to the first cavity and at least partially arranged toward the second cavity; the ingate being at least used to control the order and position of the intersection of the molten metals; The first surface and / or the second surface is further provided with a first overflow groove, and the first overflow groove is connected to at least the distal end of the second chamber relative to the reference surface and the junction of the second chamber and the reference surface through a connecting structure; Wherein, the reference plane is an imaginary plane parallel to and equidistant from the first plane and the second plane; the first direction is the width direction of the rear mold, and the second direction is the length direction of the rear mold; The second chamber further comprises a connecting groove, which is arranged at a wall surface where the second chamber intersects with the reference surface and connects with a junction of the first chamber and the reference surface along the second direction; The first surface and the second surface are further provided with a second overflow groove, the second overflow groove is arranged opposite to the inner gate, and the second overflow groove is connected to the junction of the first cavity and the reference surface and the far end relative to the reference surface through the connecting structure; The connecting structure includes a first channel and a second channel, the first channel is arranged along the first direction or the second direction, one end of the first channel is connected to the first overflow groove or the second overflow groove, and the other end gradually increases in width toward at least one side of the cavity to connect the first chamber or the second chamber with the intersection of the reference surface; one end of the second channel is connected to the first overflow groove or the second overflow groove, and the other end is connected to the far end of the first chamber or the second chamber relative to the reference surface along the first direction or the second direction, and the width of the second channel is uniform; The die-casting mold also includes a core pulling mechanism, which includes a first core, a second core and a third core. The first core and the second core are arranged along a first direction, the first core extends from one end of the first cavity into the first cavity, and the second core extends from the other end of the first cavity into the first cavity. The first core abuts against the end faces of the second core, and the length of the first core in the first cavity is greater than that of the second core; the third core penetrates from the end face of the second cavity to the first cavity along the second direction, and the end face of the third core is attached to and abuts against the outer circumferential surface of the first core.

2. A die-casting mold according to claim 1, characterized in that: The inner gate is connected to the far end of the first cavity relative to the reference surface along the first direction, and the width of the inner gate gradually increases along the direction approaching the cavity, and the increase ratio toward one side of the second cavity is greater than that on the other side.

3. A die-casting mold according to claim 1, characterized in that: A piping system is provided inside the front mold, and a cooling fluid flows through the piping system. The piping system includes two longitudinal tubes and one transverse tube, the two longitudinal tubes are arranged along the first direction, and the two longitudinal tubes are arranged opposite to the second chamber along the second direction, the two longitudinal tubes at least penetrate one side of the rear mold along the first direction, the transverse tube is arranged inside the front mold along the second direction, and the transverse tube connects the ends of the two longitudinal tubes.

4. A die-casting mold according to claim 1, characterized in that: The cavity, the core pulling mechanism, the inner gate and the first overflow groove form a molding system. The die-casting mold includes two molding systems, and the two molding systems are symmetrically arranged along the second direction relative to the midline of the rear mold length.

5. The die-casting mold according to claim 1, characterized in that: The core pulling mechanism further includes a first slider seat and a second slider seat, the first core and the second core are connected to the first slider seat, the third core is connected to the second slider seat, the first slider seat is arranged on both sides of the rear mold along the first direction, and the second slider seat is arranged on the side of the rear mold along the second direction; The first slider seat is provided with a first guide hole, the axis of which is inclined from both sides of the rear mold to the center of the rear mold along the first direction, and the second slider seat is provided with a second guide hole, the axis of which is inclined from both sides of the rear mold to the center of the rear mold along the second direction; The front mold is provided with a first oblique guide rod corresponding to the first guide hole, and the first oblique guide rod is slidably matched with the first guide hole; the front mold is provided with a second oblique guide rod corresponding to the second guide hole, and the second oblique guide rod is slidably matched with the second guide hole.

6. The die-casting mold according to claim 1, characterized in that: The core pulling mechanism also includes a threaded rod, which is arranged along the first direction, one end of which is connected to the first slider seat, and the other end is connected to a spring. The spring is fixedly arranged, and the maximum elastic force of the spring is at least twice the sum of the gravity of the first slider seat, the threaded rod and the first core.

Citation Information

Patent Citations

  • Casting device and casting method for wheel disc workpieces

    CN103212687A

  • Manufacture of corrosion proof pipe joint

    JP1987035812A