A low drive loss trench gate silicon carbide VDMOS and preparation method thereof

By building a dual P-type well region and current redistribution layer in a silicon carbide VDMOS device, the problem of high driving loss is solved, the effect of reducing driving voltage and loss is achieved, and the reliability of the device is improved.

CN118676003BActive Publication Date: 2024-11-26(LIUYANG) GLOBAL POWER TECH CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411171279.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-26
Estimated Expiration
2044-08-26

AI Technical Summary

Technical Problem

The driving loss of existing silicon carbide VDMOS devices is high, which affects their high-frequency application performance. Especially when the switching frequency is increased, it is necessary to reduce the driving voltage and driving loss of the device.

Method used

By constructing a double P-type well region structure and current redistribution layer on a silicon carbide substrate, the total charge count of the well region of the gate control inverse is reduced, and the current redistribution layer is distributed in the device structure to reduce the gate leakage capacitance. Achieve low drive loss of the device.

Benefits of technology

It effectively reduces the inverse balancing voltage and driving voltage of the device, reduces driving loss, and improves the gate reliability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118676003B_ABST
    Figure CN118676003B_ABST
Patent Text Reader

Abstract

The invention provides a low-drive-loss trench-gate silicon carbide VDMOS and a preparation method thereof, comprising: depositing metal on the lower side of a silicon carbide substrate to form a drain metal layer, epitaxially growing on the side of the silicon carbide substrate to form a drift layer; forming a barrier layer, etching, and ion implanting to form a current redistribution layer; epitaxially growing the drift layer; removing the original barrier layer, and ion implanting to form a first P-type well region, a second P-type well region, a P-type source region, and an N-type source region in the drift layer; reforming the barrier layer, etching the barrier layer to form a through hole, etching, and dry-oxygen oxidation to form a gate dielectric layer, wherein a groove is provided in the gate dielectric layer; depositing metal to form a gate metal layer and a source metal layer, and removing the barrier layer to complete the preparation, thereby reducing the device driving voltage and driving loss.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a low-driving-loss trench-gate silicon carbide VDMOS and a preparation method thereof. Background Art

[0002] Silicon carbide MOSFET is a typical representative of silicon carbide power devices, which is widely used in electric vehicles, aerospace, power conversion and other fields. The excellent switching characteristics of silicon carbide VDMOS devices are particularly obvious in high-frequency applications. As the switching frequency increases, the drive loss and conduction loss of the device at a certain operating frequency can be comparable. The drive loss becomes an important part of the device loss. Reducing the device drive loss is more important in silicon carbide devices. Summary of the invention

[0003] The technical problem to be solved by the present invention is to provide a low driving loss trench gate silicon carbide VDMOS and a preparation method thereof, so as to reduce the device driving voltage and driving loss.

[0004] In a first aspect, the present invention provides a method for preparing a low drive loss trench gate silicon carbide VDMOS, comprising the following steps:

[0005] Step 1: depositing metal on the lower side of the silicon carbide substrate to form a drain metal layer, and epitaxially growing on the side of the silicon carbide substrate to form a drift layer;

[0006] Step 2: forming a barrier layer on the drift layer, etching the barrier layer to form a through hole, and performing ion implantation on the drift layer to form a current redistribution layer;

[0007] Step 3, removing the original barrier layer, and epitaxially growing a drift layer on the drift layer and the current redistribution layer;

[0008] Step 4, performing ion implantation on the drift layer to form a first P-type well region in the drift layer;

[0009] Step 5, forming a barrier layer on the drift layer, etching the barrier layer to form a through hole, and performing ion implantation into the drift layer to form a second P-type well region in the first P-type well region;

[0010] Step 6: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, and perform ion implantation into the drift layer to form a P-type source region;

[0011] Step 7, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, and performing ion implantation into the drift layer to form an N-type source region;

[0012] Step 8, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, etching the drift layer, the second P-type well region and the first P-type well region to form a groove, performing dry oxygen oxidation in the groove to form a gate dielectric layer, wherein the gate dielectric layer is provided with a groove;

[0013] Step 9, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, depositing metal, and forming a gate metal layer;

[0014] Step 10: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, etch the drift layer, deposit metal to form a source metal layer, remove the barrier layer, and complete the preparation.

[0015] In a second aspect, the present invention provides a low drive loss trench gate silicon carbide VDMOS, wherein the silicon carbide VDMOS is prepared by the method for preparing a low drive loss trench gate silicon carbide VDMOS according to the first aspect.

[0016] The advantages of the present invention are:

[0017] 1. The device constructs a dual P-type well region structure based on the trench gate VDMOS device structure. The second P-type well region is low-doped, which reduces the total charge number of the well region where the gate of the device controls the inversion, and can effectively reduce the inversion equilibrium voltage of the device and reduce the device driving voltage;

[0018] Second, a current redistribution layer is constructed on the silicon carbide substrate of the device, which reduces the gate-drain capacitance of the device, can effectively reduce the gate charge of the device and reduce the driving loss of the device;

[0019] 3. The current redistribution layer of the device is distributed directly below and on the left and right sides of the gate, which can redistribute the current on the left and right sides of the gate to the entire area of ​​the device at the drain, thus playing the role of current balancing;

[0020] Fourth, the current redistribution layer of the device can also concentrate the drain current to the current redistribution area, avoiding the impact of large drain current on the corner of the device gate and improving the reliability of the device gate. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The present invention will be further described below in conjunction with embodiments with reference to the accompanying drawings.

[0022] Figure 1 The present invention is a flow chart of a method for preparing a low drive loss trench gate silicon carbide VDMOS.

[0023] Figure 2 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 1 .

[0024] Figure 3A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 2 .

[0025] Figure 4 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 3 .

[0026] Figure 5 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 4 .

[0027] Figure 6 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 5 .

[0028] Figure 7 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 6 .

[0029] Figure 8 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 7 .

[0030] Fig. 9 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 8 .

[0031] Fig.10 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 9 .

[0032] Fig.11 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 10 .

[0033] Fig.12 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 10 one.

[0034] Fig.13 A cross-sectional view of the process of manufacturing a low drive loss trench gate silicon carbide VDMOS according to the present invention Figure 10 two.

[0035] Fig.14 The schematic diagram of a low drive loss trench gate silicon carbide VDMOS of the present invention is shown. DETAILED DESCRIPTION

[0036] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. Embodiments of the present application are provided in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.

[0037] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.

[0038] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "in contact with ...", "directly connected to" or "directly coupled to" other elements or layers, there is no intervening element or layer. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers, doping types and / or parts, these elements, components, regions, layers, doping types and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, doping type or part from another element, component, region, layer, doping type or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer, doping type or part discussed below can be represented as a second element, component, region, layer or part.

[0039] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," and the like may be used herein to describe the relationship of one element or feature described in the figures to other elements or features. It should be understood that, in addition to the orientations described in the figures, spatially relative terms also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, an element or feature described as "under other elements" or "under it" or "under it" will be oriented as being "above" the other elements or features. Thus, the exemplary terms "under" and "under" may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.

[0040] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "include / comprise" or "have" and the like specify the presence of stated features, wholes, steps, operations, components, parts, or combinations thereof, but do not exclude the possibility of the presence or addition of one or more other features, wholes, steps, operations, components, parts, or combinations thereof. At the same time, in this specification, the term "and / or" includes any and all combinations of the relevant listed items.

[0041] like Figures 1 to 13 As shown, the embodiment of the present application provides a method for preparing a low drive loss trench gate silicon carbide VDMOS, comprising the following steps:

[0042] Step 1: depositing metal on the lower side of the silicon carbide substrate 101 to form a drain metal layer 110, and epitaxially growing on the side of the silicon carbide substrate 101 to form a drift layer 103;

[0043] Step 2: forming a barrier layer a on the drift layer 103, etching the barrier layer a to form a through hole, and performing ion implantation on the drift layer 103 to form a current redistribution layer 102, wherein the ion implantation energy is 10-100 keV;

[0044] Step 3, removing the original barrier layer a, and epitaxially growing the drift layer 103 on the drift layer 103 and the current redistribution layer 102;

[0045] Step 4: perform ion implantation on the drift layer 103 to form a first P-type well region 104 in the drift layer 103, and the ion implantation energy is 200-300kev;

[0046] Step 5, forming a barrier layer b on the drift layer 103, etching the barrier layer b to form a through hole, and performing ion implantation into the drift layer 103 to form a second P-type well region 1041 in the first P-type well region 104, wherein the ion implantation energy is 200-270kev;

[0047] Step 6: remove the original barrier layer b, re-form the barrier layer c, etch the barrier layer c to form a through hole, and perform ion implantation into the drift layer 103 to form a P-type source region 105. The ion implantation energy is 100-200 keV.

[0048] Step 7, remove the original barrier layer c, re-form the barrier layer d, etch the barrier layer d to form a through hole, perform ion implantation into the drift layer 103 to form an N-type source region 106, and the ion implantation energy is 100-200kev;

[0049] Step 8, remove the original barrier layer d, re-form the barrier layer e, etch the barrier layer e to form a through hole, etch the drift layer 103, the second P-type well region 1041 and the first P-type well region 104 to form a groove 111, the etching depth is 800nm, dry oxygen oxidation is performed in the groove 111 to form a gate dielectric layer 107, and a groove 1071 is provided in the gate dielectric layer 107;

[0050] Step 9, removing the original barrier layer e, re-forming the barrier layer f, etching the barrier layer f to form a through hole, depositing metal, and forming a gate metal layer 108;

[0051] Step 10, remove the original barrier layer f, re-form the barrier layer g, etch the barrier layer g to form a through hole, etch the drift layer 103 to a depth of 300nm, deposit metal to form a source metal layer 109, remove the barrier layer g, and complete the preparation.

[0052] The doping concentration of the first P-type well region 104 is greater than the doping concentration of the second P-type well region 1041. The lower side of the second P-type well region 1041 and the lower side of the gate metal layer 108 are located in the same plane. The current redistribution layer 102 includes a first distribution area 1021, a second distribution area 1022 and a third distribution area 1023. The first distribution area 1021, the second distribution area 1022 and the third distribution area 1023 are arranged at intervals, and the second distribution area 1022 is arranged directly below the gate dielectric layer 107, and the width of the second distribution area 1022 is equal to the width of the gate dielectric layer 107. The current redistribution layer 102, the silicon carbide substrate 101 and the drift layer 103 are all N-type, and the doping concentration of the silicon carbide substrate 101 is 2e18cm -3 The doping concentration of the drift layer 103 is 5e16cm -3 The doping concentration of the current redistribution layer 102 is 5e17cm -3 The doping concentration of the first P-type well region 104 is 5e17 cm -3 The doping concentration of the second P-type well region 1041 is 1e17 cm -3 The doping concentration of the N-type source region 106 is 5e18cm -3 The doping concentration of the P-type source region 105 is 8e18cm -3 .

[0053] The gate dielectric layer 107 is silicon dioxide, the gate metal layer 108 is Al, the source metal layer 109 is Al, and the drain metal layer 110 is Ni and Al alloy, with a ratio of 2:8. The thickness of the silicon carbide substrate 101 of the device is 1 μm, the thickness of the drift layer 103 is 20-30 μm, the thickness of the current redistribution layer 102 is 290-310 nm, the thickness of the first P-type well region 104 is 300 nm, the thickness of the second P-type well region 1041 is 200 nm, and its bottom is flush with the bottom of the gate metal layer 108. The width of the second P-type well region 1041 is 100 nm, the bottom thickness of the gate dielectric layer 107 is 30 nm, the side wall thickness is 20 nm, the thickness of the N-type source region 106 is 300 nm, the thickness of the P-type source region 105 is 300 nm, the thickness from the top of the source metal layer 109 to the top of the N-type source region 106 is 300 nm, the thickness of the gate metal layer 108 is 800 nm, and the device withstand voltage is 1200-3000 V;

[0054] The concentration of the silicon carbide substrate 101 is to form a low-resistance ohmic contact with the drain metal layer 110 to reduce the on-resistance of the device. Its thickness is to ensure support during device epitaxy and improve process stability. The doping concentration of the current redistribution layer 102 is to achieve a doping concentration transition between the silicon carbide substrate 101 and the drift layer 103 to ensure the function of current redistribution.

[0055] The current redistribution layer 102 can shield the capacitance effect from the gate to the n+SiC substrate, reduce the gate-drain capacitance of the device, effectively reduce the gate charge of the device, and reduce the driving loss of the device.

[0056] The current redistribution layer 102 of the device can make the drain current concentrate to the current redistribution layer area, avoid the impact of the drain current on the corner of the device gate, and improve the reliability of the device gate;

[0057] The doping concentration of the first P-type well region 104 of the device is greater than that of the second P-type well region 1041, so the first P-type well region 104 can achieve inversion and high electron concentration at a smaller gate voltage. This well region structure can reduce the gate drive voltage of the device, thereby reducing the drive loss of the device. The doping concentration of the first P-type well region 104 of the device is relatively high, and the bottom of the first P-type well region 104 is at the same height as the bottom of the gate dielectric layer 107, which can suppress the electric field concentration at the gate corner and improve the gate reliability.

[0058] like Fig.14 As shown, the silicon carbide VDMOS obtained by the above manufacturing method includes:

[0059] A silicon carbide substrate 101, a current redistribution layer 102, wherein the lower side of the current redistribution layer 102 is connected to the upper side of the silicon carbide substrate 101;

[0060] A drift layer 103 , wherein the lower side of the drift layer 103 is connected to the upper side of the silicon carbide substrate 101 and the current redistribution layer 102 ;

[0061] A first P-type well region 104 , wherein a lower side of the first P-type well region 104 is connected to an upper side of the drift layer 103 , and a second P-type well region 1041 is disposed on the first P-type well region 104 ;

[0062] A P-type source region 105 , wherein the lower side of the P-type source region 105 is connected to the upper side of the first P-type well region 104 ;

[0063] An N-type source region 106, wherein the lower side of the N-type source region 106 is respectively connected to the upper side of the first P-type well region 104 and the upper side of the second P-type well region 1041, and the outer side of the N-type source region 106 is connected to the inner side of the P-type source region 105;

[0064] A gate dielectric layer 107, wherein the lower side of the gate dielectric layer 107 is connected to the upper side of the drift layer 103, and the outer side of the gate dielectric layer 107 is respectively connected to the first P-type well region 104, the second P-type well region 1041 and the N-type source region 106; a groove 1071 is provided in the gate dielectric layer 107;

[0065] A gate metal layer 108, wherein the gate metal layer 108 is disposed in the groove 1071;

[0066] A source metal layer 109 , wherein the source metal layer 109 is connected to the N-type source region 106 and the P-type source region 105 ;

[0067] and a drain metal layer 110 , wherein the drain metal layer 110 is connected to the lower side of the silicon carbide substrate 101 .

[0068] Although the specific implementation mode of the present invention is described above, those skilled in the art should understand that the specific embodiments described are only illustrative and are not intended to limit the scope of the present invention. Equivalent modifications and changes made by those skilled in the art in accordance with the spirit of the present invention should be included in the scope of protection of the claims of the present invention.

Claims

1. A method for preparing a low drive loss trench gate silicon carbide VDMOS, characterized in that: The steps include: Step 1: depositing metal on the lower side of the silicon carbide substrate to form a drain metal layer, and epitaxially growing on the side of the silicon carbide substrate to form a drift layer; Step 2: forming a barrier layer on the drift layer, etching the barrier layer to form a through hole, and performing ion implantation on the drift layer to form a current redistribution layer; Step 3, removing the original barrier layer, and epitaxially growing a drift layer on the drift layer and the current redistribution layer; Step 4, performing ion implantation on the drift layer to form a first P-type well region in the drift layer; Step 5, forming a barrier layer on the drift layer, etching the barrier layer to form a through hole, and performing ion implantation into the drift layer to form a second P-type well region in the first P-type well region; Step 6: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, and perform ion implantation into the drift layer to form a P-type source region; Step 7, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, and performing ion implantation into the drift layer to form an N-type source region; Step 8, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, etching the drift layer, the second P-type well region and the first P-type well region to form a groove, performing dry oxygen oxidation in the groove to form a gate dielectric layer, wherein the gate dielectric layer is provided with a groove; Step 9, removing the original barrier layer, re-forming the barrier layer, etching the barrier layer to form a through hole, depositing metal, and forming a gate metal layer; Step 10: remove the original barrier layer, re-form the barrier layer, etch the barrier layer to form a through hole, etch the drift layer, deposit metal to form a source metal layer, remove the barrier layer, and complete the preparation; The doping concentration of the first P-type well region is greater than the doping concentration of the second P-type well region, the lower side of the second P-type well region and the lower side of the gate metal layer are located in the same plane, the current redistribution layer includes a first distribution area, a second distribution area and a third distribution area, the first distribution area, the second distribution area and the third distribution area are arranged at intervals, and the second distribution area is arranged directly below the gate dielectric layer, and the width of the second distribution area is equal to the width of the gate dielectric layer.

2. The method for preparing a low drive loss trench gate silicon carbide VDMOS according to claim 1, characterized in that: The thickness of the current redistribution layer is 290-310 nm.

3. The method for preparing a low drive loss trench gate silicon carbide VDMOS according to claim 1, characterized in that: The current redistribution layer, the silicon carbide substrate and the drift layer are all N-type.

4. The method for preparing a low drive loss trench gate silicon carbide VDMOS according to claim 1, characterized in that: The doping concentration of the silicon carbide substrate is 2e18cm -3 The doping concentration of the drift layer is 5e16cm -3 The doping concentration of the current redistribution layer is 5e17cm -3 The doping concentration of the first P-type well region is 5e17 cm -3 The doping concentration of the second P-type well region is 1e17 cm -3 The doping concentration of the N-type source region is 5e18cm -3 .

5. A low drive loss trench gate silicon carbide VDMOS, characterized in that: The silicon carbide VDMOS is prepared by any one of the preparation methods of claim 1 to claim 4.

Citation Information

Patent Citations

  • Diamond trench gate VDMOS device and preparation method thereof

    CN118448463A

  • Semiconductor device and semiconductor device manufacturing method

    JP2013219161A

  • Semiconductor device

    JP2020043309A

  • Silicon carbide semiconductor device

    US20090090920A1

  • Semiconductor Device and Manufacturing Method Thereof

    US20160099316A1