Manufacturing equipment and manufacturing method for fixing film thin-walled tube of image forming device
By using equipment with graded extrusion and differential temperature stretching processes in the manufacturing of stainless steel thin-walled tubes, the problems of uneven wall thickness and large internal stress are solved, and high-quality production and diversified thickness adaptation of thin-walled tubes are achieved, extending the extended service life.
Patent Information
- Application Number
- CN202411022112.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing stainless steel thin-walled tube manufacturing process has problems such as uneven wall thickness, poor surface finish, and large internal stress, making it difficult to flexibly adjust the thickness to meet the needs of different printers and copiers.
Using manufacturing equipment including a first spinning mechanism and a second squeezing mechanism, through graded extrusion and differential temperature stretching processes, uniform rotational extrusion and precise squeezing processing of thin-walled tubes can be achieved, and the wall thickness and surface finish can be adjusted. Eliminate internal stress.
It achieves improvements in wall thickness uniformity, dimensional accuracy and mechanical properties of thin-walled tubes, meets different thickness requirements, extends service life and avoids deformation and fracture.
Smart Images

Figure CN118719936A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of soft soil stratum solidification, and in particular to a soft soil solidification device and a solidification process. Background Art
[0002] Existing stainless steel thin-walled tubes are widely used in many fields due to their excellent corrosion resistance and mechanical properties. In the field of printers and copiers, stainless steel thin-walled tubes, as the base mold of the fixing film, play a vital role in the printing quality and stability of the printer. However, the existing stainless steel thin-walled tubes still have many deficiencies in manufacturing process and performance, which need to be improved urgently.
[0003] At present, the traditional manufacturing methods of stainless steel thin-walled tubes mainly include stamping, welding, stretching and other process steps. Although these methods can produce stainless steel thin-walled tubes that meet certain requirements, they have obvious defects in terms of wall thickness uniformity, surface finish and material utilization. The uneven wall thickness of stainless steel thin-walled tubes produced by traditional manufacturing methods can easily cause fluctuations in the fixing film during use, affecting the printing quality.
[0004] In addition, the welding and stretching processes in traditional processes often introduce additional internal stress, causing the thin-walled tube to deform and break easily during use, further affecting the service life and performance of the fixing film. More importantly, it is difficult to flexibly adjust the wall thickness of the thin-walled tube with traditional processes, and it is unable to meet the diverse requirements of different printers and copiers for the thickness of the fixing film base mold. Therefore, how to optimize the manufacturing process and manufacturing equipment of stainless steel thin-walled tubes, improve their wall thickness uniformity and surface finish, and be able to flexibly produce thin-walled tubes of different thicknesses is a technical problem that needs to be solved urgently. Summary of the invention
[0005] The object of the present invention is to provide a device and method for manufacturing a fixing film thin-wall tube of an image forming device, so as to solve the technical problem that it is difficult to flexibly adjust and produce fixing film thin-wall tubes of different thicknesses in the prior art.
[0006] First aspect The present application provides a device for manufacturing a fixing film thin-wall tube of an image forming device, comprising: frame; A first spinning mechanism is installed on the frame and has two extrusion ends arranged opposite to each other, a spinning space is formed between the two extrusion ends, and the raw tube to be spun is placed in the extrusion space; An adjusting component, fixedly connected to the extrusion end, and used to control and adjust the distance between the two extrusion ends; The second stretching mechanism is installed on the frame and arranged close to the first spinning mechanism. The second stretching mechanism has a stretching cavity. The second stretching mechanism is used for stretching the workpiece placed in the stretching cavity by differential temperature.
[0007] By adopting the above technical solution, the first spinning mechanism cooperates with the adjustment component to achieve a graded extrusion effect, and the extrusion distance is gradually adjusted and controlled by two oppositely arranged extrusion ends to achieve uniform rotational extrusion processing of the plain tube to be processed. In addition, the thickness of the plain tube after passing through the first spinning mechanism can be controlled by the adjustment component, and then thin-walled tubes of different thicknesses can be produced by changing the diameter of the squeezing cavity.
[0008] Preferably, the first spinning mechanism comprises: A driving shaft is horizontally arranged on the frame, and the driving shaft can rotate along its own axis relative to the frame; There are two elliptical disks and the extrusion end is located on the elliptical disk. The axis of the elliptical disk is parallel to the axis of the driving shaft. The elliptical disk is located on both sides of the driving shaft.
[0009] By adopting the above technical solution, the driving shaft can rotate along its own axial direction, thereby driving the elliptical disk and the extrusion end thereon to rotate synchronously, thereby achieving uniform rotational extrusion of the cylindrical plain tube.
[0010] Preferably, the adjustment component comprises: A fixing rod, one end of which is coaxially arranged and fixedly connected to the elliptical disk, and the other end of which is fixedly connected to the frame; A synchronous rotation driving member is arranged on the frame and is used for synchronously driving the elliptical disk to rotate.
[0011] By adopting the above technical solution, the fixing rod ensures the stability of the position of the elliptical disk during the rotation process, so that the elliptical disk can maintain a smooth rotation path. The synchronous rotation drive controls the synchronous rotation of the elliptical disk, so that the extrusion end can apply pressure evenly during the spinning process. By adjusting the starting position during the spinning process and the rotation angle of the elliptical disk, the relative distance of the extrusion end can be accurately controlled, thereby achieving control of different wall thicknesses of thin-walled tubes.
[0012] Preferably, the synchronous rotating drive component includes a first pulley, an oppositely arranged second pulley, a synchronous transmission belt located on the first pulley and the second pulley, and a servo motor. The servo motor is arranged on the frame, and the output shaft of the servo motor is coaxially arranged with the first pulley. The first pulley and the second pulley are connected to the two ellipses through the fixing rod.
[0013] By adopting the above technical solution, the first pulley is driven to rotate by the servo motor, and then the second pulley coordinated with the first pulley can be driven to rotate synchronously, thereby realizing the synchronous rotation of the elliptical disk.
[0014] Preferably, the first spinning mechanism further comprises: A hydraulic cylinder, fixedly connected to the synchronous rotation driving member, and used to drive the synchronous rotation driving member to move in a horizontal direction; The telescopic ram is coaxially arranged with the driving shaft and rotates relative to the driving shaft, and the telescopic ram is fixedly connected to the frame.
[0015] By adopting the above technical solution, the hydraulic cylinder can accurately control the horizontal movement of the synchronous rotating drive member, thereby adjusting the extrusion position of the elliptical disk and achieving the extrusion of the entire raw tube to be spun. The telescopic head ensures the stable support and positioning of the raw tube during the rotation process, avoiding the workpiece offset during the spinning process and optimizing the spinning quality.
[0016] Preferably, the telescopic plug comprises: The head body rotates relative to the driving shaft; A spring, two ends of which are respectively fixedly connected to the mandrel body and the frame; A guide rod has one end fixedly connected to the mandrel body and the other end slidably connected to the frame.
[0017] By adopting the above technical solution, the cooperation of the hydraulic cylinder and the telescopic mandrel realizes the uniform extrusion of the entire raw pipe to be spun. One end of the guide rod is fixedly connected to the mandrel body, and the other end is slidably connected to the frame to ensure that the mandrel body can move smoothly during the rotation process.
[0018] Preferably, the synchronous rotation driving member comprises: The reducer is arranged on the servo motor and is used for reducing the rotation speed of the servo motor and increasing the torque.
[0019] By adopting the above technical solution, the reducer can stably drive the spinning process under low-speed and high-torque working conditions by reducing the speed of the servo motor and increasing the output torque. At the same time, the increased torque ensures that sufficient extrusion force is applied to the plain tube during the spinning process.
[0020] Preferably, the second pressing mechanism comprises: A main mold, the compression cavity is coaxially opened on the main mold; The punching die has a pressing head, and the pressing head is slidably matched with the pressing cavity; A heating element is arranged on the main mold and is used for heating the main mold.
[0021] By adopting the above technical solution, the sliding cooperation between the rolling head and the rolling cavity realizes the precise rolling processing of thin-walled tubes, ensuring the uniformity of wall thickness and surface finish. Through this hot rolling process, the internal stress that may be introduced during the spinning process is effectively eliminated.
[0022] Preferably, the diameter of the pressure cavity gradually decreases in a direction away from the punching die until it remains constant.
[0023] By adopting the above technical solution, the material can be deformed smoothly in the initial stage and adapt to the stretching process.
[0024] Second aspect The present application provides a method for manufacturing a fixing film thin-wall tube of an image forming device, using the above-mentioned fixing film thin-wall tube manufacturing device of an image forming device, comprising the following steps: S1, sleeve and fix the cylindrical plain tube on the central axis of the first spinning mechanism, and use the adjustment component to control and adjust the distance between the two extrusion ends; S2, start the first spinning mechanism, and perform rotational extrusion processing on the cylindrical plain tube through two oppositely arranged extrusion ends, and adjust the distance between the two extrusion ends again in this process so that the distance between the two ends gradually decreases, thereby obtaining a first metal thin-walled tube; S3, moving the first metal thin-walled tube from the first spinning mechanism into the stretching cavity of the second stretching mechanism, starting the second stretching mechanism, and obtaining the second metal thin-walled tube through differential temperature stretching and stretching.
[0025] By adopting the above technical scheme, the adjusting component of the first spinning mechanism realizes the uniform rotational extrusion of the cylindrical plain tube, ensuring the uniformity of the wall thickness and dimensional accuracy of the primary thin-walled tube; secondly, the second stretching mechanism using differential temperature stretching processing further optimizes the surface finish and mechanical properties of the thin-walled tube, and effectively eliminates the internal stress introduced during the spinning process, thereby realizing the stable production of high-quality thin-walled tubes.
[0026] In summary, the present application includes at least one of the following beneficial technical effects: 1. Through the cooperation of the first spinning mechanism and the adjusting component, the cylindrical plain tube is extruded in stages, and the distance between the extrusion ends can be accurately controlled, so that the thin-walled tube is gradually formed during the spinning process, ensuring the uniformity of the wall thickness and dimensional accuracy of the thin-walled tube, and meeting the diverse requirements of different printers and copiers for the thickness of the fixing film base mold; 2. By utilizing the differential temperature stretching and stretching process of the second stretching mechanism, not only the surface finish of the thin-walled tube is optimized, but also the internal stress introduced during the spinning process can be effectively eliminated, thereby improving the mechanical properties and service life of the thin-walled tube and avoiding the deformation and fracture problems that are easily caused by traditional manufacturing methods; 3. By adjusting the thickness of the plain tube after the first spinning mechanism and combining the change of the diameter of the pressing cavity of the second pressing mechanism, thin-walled tubes of different thicknesses can be flexibly adjusted and produced. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a schematic diagram of the overall structure in the embodiment of the present application; Figure 2 is a cross-sectional view of a first spinning mechanism in an embodiment of the present application; Figure 3 is a cross-sectional view of the second squeezing mechanism in the embodiment of the present application; Figure 4 yes Figure 3 An enlarged schematic diagram of point A.
[0028] In the figure: 1. frame; 2. first spinning mechanism; 21. driving shaft; 211. driving motor; 22. elliptical disk; 23. hydraulic cylinder; 24. telescopic ram; 241. ram body; 242. spring; 243. guide rod; 3. adjustment assembly; 31. fixing rod; 32. first pulley; 33. second pulley; 34. servo motor; 35. reducer; 4. second stretching mechanism; 41. main mold; 411. stretching cavity; 42. punching die; 5. first metal thin-walled tube; 6. second metal thin-walled tube. DETAILED DESCRIPTION
[0029] The following is combined with Figure 1 -Attached Figure 4 , further details of this application are given.
[0030] First aspect, embodiment: Reference Figure 1 A fixing film thin-wall tube manufacturing device for an image forming device includes a frame 1, a first spinning mechanism 2, an adjusting component 3 and a second twisting mechanism 4.
[0031] Reference Figure 1 and Figure 2, frame 1 is used to support and fix the entire device, and frame 1 includes an L-shaped fixed plate and a fixed block. The first spinning mechanism 2 is installed on the fixed plate of frame 1, and the first spinning mechanism 2 includes a driving shaft 21, two oppositely arranged elliptical disks 22 and two extrusion ends. The driving shaft 21 is horizontally arranged on the frame 1 and can rotate along its own axis relative to the frame 1. Specifically, a driving motor 211 is installed on the driving shaft 21, and the driving motor 211 can drive the shaft 21 to rotate at high speed. The two elliptical disks 22 are respectively installed on the upper and lower sides of the driving shaft 21, and the axis of the elliptical disk 22 is parallel to the axis of the driving shaft 21. The extrusion end is located on the elliptical disk 22, and a spinning space is formed between the two extrusion ends. When performing preliminary spinning, the cylindrical plain tube to be spun is placed and fixed on the driving shaft 21. Then the motor is started to drive the shaft 21 to rotate along the axial direction, driving the elliptical disk 22 and the extrusion ends thereon to rotate synchronously, thereby realizing uniform rotation and extrusion of the plain tube.
[0032] Reference Figure 1 and Figure 2 , the adjustment component 3 is fixedly connected to the extrusion end, and the adjustment component 3 is used to control and adjust the distance between the two extrusion ends. The adjustment component 3 includes a fixed rod 31 and a synchronous rotation drive member, one end of the fixed rod 31 is coaxially arranged and fixedly connected to the elliptical disk 22, and the other end is fixedly connected to the frame 1. The synchronous rotation drive member is arranged on the frame 1 and is used to synchronously drive the elliptical disk 22 to rotate. The fixed rod 31 ensures the stability of the position of the elliptical disk 22 during the rotation process, so that the elliptical disk 22 can maintain a smooth rotation path. The synchronous rotation drive member controls the synchronous rotation of the elliptical disk 22 so that the extrusion end can apply pressure evenly during the spinning process. The major axis and minor axis of the elliptical disk 22 have different radii. As the elliptical disk 22 rotates, the position of the extrusion end changes continuously, resulting in the distance between the extrusion ends changing continuously. In the major axis direction of the elliptical disk 22, the distance between the extrusion ends is the largest. In the minor axis direction, the distance between the extrusion ends is the smallest. By adjusting the starting position during the spinning process and the rotation angle of the elliptical disk 22, the relative distance between the extrusion ends can be accurately controlled, thereby achieving control of different wall thicknesses of the thin-walled tube.
[0033] The synchronous rotation driving member includes a first pulley 32, a second pulley 33 arranged oppositely, a synchronous transmission belt located on the first pulley 32 and the second pulley 33, and a driving motor 211. The driving motor 211 is arranged on the frame 1, and the output shaft of the driving motor 211 is coaxially arranged with the first pulley 32. The first pulley 32 and the second pulley 33 are connected to the two ellipses through a fixing rod 31. In this embodiment, the driving motor 211 is a high-speed motor, which can drive the driving shaft 21 and the raw tube to be spun fixed thereon to rotate at high speed. The first pulley 32 is driven to rotate by the driving motor 211, and then the second pulley 33 that cooperates with the first pulley 32 can be driven to rotate synchronously, thereby realizing the synchronous rotation of the elliptical disk 22. The synchronous transmission belt ensures the rotation consistency of the elliptical disks 22 on both sides, and avoids the uneven extrusion phenomenon caused by asynchronous rotation. Through the synchronous drive design, the extrusion end can evenly apply pressure during the spinning process, further ensuring the uniformity and dimensional accuracy of the wall thickness of the thin-walled tube.
[0034] Reference Figure 1 and Figure 2 The first spinning mechanism 2 also includes a hydraulic cylinder 23 and a telescopic jack 24. The hydraulic cylinder 23 is fixedly connected to the synchronously rotating driving member, and is used to drive the synchronously rotating driving member to move in the horizontal direction. The telescopic jack 24 is coaxially arranged with the driving rotation and rotates relative to the driving shaft 21, and the telescopic jack 24 is fixedly connected to the fixed block of the frame 1. The hydraulic cylinder 23 can be used to accurately control the horizontal movement of the synchronously rotating driving member, thereby adjusting the extrusion position of the elliptical disk 22 to achieve the extrusion of the entire raw tube to be spun. The telescopic jack 24 ensures the stable support and positioning of the raw tube during the rotation process, avoids the workpiece offset during the spinning process, and optimizes the spinning quality.
[0035] The telescopic ram 24 includes a ram body 241, a spring 242 and a guide rod 243. The ram body 241 is conical and rotates relative to the driving shaft 21. The two ends of the spring 242 are fixedly connected to the ram body 241 and the frame 1 respectively. One end of the guide rod 243 is fixedly connected to the ram body 241, and the other end is slidably connected in the fixed block of the frame 1. The fixed block of the frame 1 is provided with a guide groove, and the guide rod 243 slides in the guide groove. The cooperation between the hydraulic cylinder 23 and the telescopic ram 24 realizes the uniform extrusion of the entire plain pipe to be spun. One end of the guide rod 243 is fixedly connected to the ram body 241, and the other end is slidably connected in the frame 1 to ensure that the ram body 241 can move smoothly during the rotation process. The cooperation between the ram body 241, the spring 242 and the guide rod 243 makes it easier for the ram body 241 to always stably support and position the driving shaft 21.
[0036] The synchronous rotation driving member includes a reducer 35, which is arranged on the servo motor 34 and is used to reduce the rotation speed of the servo motor 34 and increase the torque. The servo motor 34 provides precise rotation control to ensure the synchronous rotation of the extrusion end during the spinning process. The reducer 35 can stably drive the spinning process under the working conditions of low speed and high torque by reducing the rotation speed of the servo motor 34 and increasing the output torque. At the same time, the increased torque ensures that sufficient extrusion force is applied to the plain tube during the spinning process, so that the wall thickness uniformity and dimensional accuracy of the thin-walled tube are effectively guaranteed.
[0037] When performing the first spinning, first fix the cylindrical tube to be spun on the driving shaft 21. Then start the servo motor 34, and the rotation of the shaft of the servo motor 34 drives the first pulley 32 to rotate. The rotation of the first pulley 32 drives the fixed rod 31 to rotate, and the rotation of the fixed rod 31 drives the elliptical disk 22 to rotate, so that one end of the elliptical disk 22 abuts against the tube to be spun. At this time, turn off the servo motor 34 and start the driving motor 211. The rotation of the driving motor 211 drives the driving shaft 21 to rotate, and the rotation of the driving shaft 21 drives the tube fixed thereon to rotate relative to the extrusion end of the elliptical disk 22. While driving the driving shaft 21 to rotate, start the hydraulic cylinder 23, which has a retractable output shaft, and the output shaft drives the driving motor 211 and the driving shaft 21 fixedly connected thereto to move in the horizontal direction, thereby driving the tube to move horizontally relative to the elliptical disk 22, so as to achieve the spinning of the entire tube. In addition, since the spinning process needs to be repeated for many times, the servo motor 34 is controlled and adjusted to rotate slightly, so that the distance between the extrusion ends of the two elliptical disks 22 is gradually reduced, and the extrusion process is gradually carried out. Gradual extrusion can effectively reduce the stress concentration and uneven deformation during the extrusion process, and ensure the uniformity of the wall thickness and dimensional accuracy of the primary thin-walled tube.
[0038] Reference Figure 3 and Figure 4The second tensile mechanism 4 is installed on the frame 1 and is arranged close to the first spinning mechanism 2. The second tensile mechanism 4 has a tensile cavity 411. The second tensile mechanism 4 is used to differentially stretch the workpiece placed in the tensile cavity 411. The second tensile mechanism 4 includes a main mold 41 and a punch 42. The tensile cavity 411 is coaxially opened on the main mold 41. The punch 42 has a tensile head, and the tensile head is slidably matched with the tensile cavity 411. The diameter of the tensile cavity 411 gradually decreases in the direction away from the punch 42 until it remains unchanged. During the tensile process, the metal material first enters the wider cavity mouth and is subjected to a smaller initial extrusion force, so that the material can be smoothly deformed and adapt to the tensile process in the initial stage. As the material gradually enters the gradually decreasing tensioning cavity 411, the extrusion pressure gradually increases. This progressive extrusion can effectively disperse the stress of the material during the deformation process, reduce stress concentration, and avoid sudden deformation or breakage of the material during the tensioning process. At the same time, the gradually decreasing diameter can compress the material layer by layer during the deformation process, making the wall thickness reduction more uniform, thereby ensuring the consistency of the wall thickness of the finished thin-walled tube. When the material enters the unchanged diameter section, the tensioning cavity 411 provides a constant extrusion environment to further correct and stabilize the final size and shape of the thin-walled tube. The tensioning of the constant diameter section can eliminate the slight dimensional errors that may occur during the deformation process of the previous section, so that the finished thin-walled tube is highly consistent in shape and size.
[0039] A resistance heating element is arranged inside the main mold 41. The resistance heating element can be in the form of a resistance wire or an electric heating rod, and is evenly distributed in the area of the main mold 41 near the stretching cavity 411. The resistance heating element is connected to the power supply through a wire, and the output voltage and current of the power supply can be adjusted by the control system. The control system includes a temperature sensor, a regulator and a controller. The temperature sensor is installed in the area of the main mold 41 near the stretching cavity 411, monitors the internal temperature of the main mold 41 in real time, and feeds the data back to the controller. The controller adjusts the output power of the power supply according to the preset temperature range to keep the temperature of the main mold 41 stable. When the stretching process starts, the control system starts the power supply and the heating element starts working. When the current passes through the resistance heating element, the resistance element generates heat due to the resistance effect, thereby heating the main mold 41. Resistance heating maintains the temperature of the main mold 41 and the stretching cavity 411 within a preset range, reduces the hardness and internal stress of the metal material during the stretching process, enhances the machinability of the material, and makes the metal material easier to deform and form during the stretching process.
[0040] The secondary differential temperature stretching process further improves the quality of thin-walled tubes. After the first metal thin-walled tube 5 is moved into the second stretching mechanism 4, the differential temperature stretching process not only optimizes the surface finish of the thin-walled tube, but also effectively eliminates the internal stress that may be introduced during the spinning process. In addition, by adjusting the component 3, the thickness of the plain tube after the first spinning mechanism 2 can be controlled, and then by changing the diameter of the stretching cavity 411, thin-walled tubes of different thicknesses can be produced. The sliding cooperation between the stretching head and the stretching cavity 411 realizes the precise stretching of the thin-walled tube, ensuring the uniformity of the wall thickness and the surface finish. Through this hot stretching process, the internal stress that may be introduced during the spinning process is effectively eliminated, and the mechanical properties and dimensional accuracy of the thin-walled tube are further optimized.
[0041] Second aspect The present application provides a method for manufacturing a fixing film thin-wall tube of an image forming device, using the above-mentioned fixing film thin-wall tube manufacturing device of an image forming device, comprising the following steps: S1, sleeve and fix the cylindrical plain tube on the central axis of the first spinning mechanism 2, and use the adjustment component 3 to control and adjust the distance between the two extrusion ends; S2, start the first spinning mechanism 2, and perform rotational extrusion processing on the cylindrical plain tube through two oppositely arranged extrusion ends. In this process, the distance between the two extrusion ends is adjusted again so that the distance between the two ends gradually decreases, thereby obtaining a first metal thin-walled tube 5; S3, moving the first metal thin-walled tube 5 from the first spinning mechanism 2 into the stretching cavity 411 of the second stretching mechanism 4, starting the second stretching mechanism 4, and obtaining the second metal thin-walled tube 6 through differential temperature stretching and stretching.
[0042] By adopting the above technical scheme, the adjusting component 3 of the first spinning mechanism 2 realizes the uniform rotational extrusion of the cylindrical plain tube, ensuring the uniformity of the wall thickness and dimensional accuracy of the primary thin-walled tube; secondly, the second stretching mechanism 4 using differential temperature stretching processing further optimizes the surface finish and mechanical properties of the thin-walled tube, and effectively eliminates the internal stress introduced during the spinning process, thereby realizing the stable production of high-quality thin-walled tubes.
[0043] It should be noted that the servo motor 34, reducer 35 and resistance heating element in this embodiment are all devices purchased on the market, and the models can be selected or customized according to actual needs. In this application, we only use them and do not improve their structure and function. For technicians in this field, their setting method, installation method and electrical connection method only need to be debugged according to the requirements of their instruction manual, and they will not be repeated here.
[0044] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A device for manufacturing a fixing film thin-wall tube of an image forming device, characterized in that: include: Rack(1); A first spinning mechanism (2) is mounted on the frame (1) and has two extrusion ends arranged opposite to each other, a spinning space is formed between the two extrusion ends, and the plain tube to be spun is placed in the extrusion space; An adjustment component (3) fixedly connected to the extrusion end, the adjustment component (3) being used to control and adjust the distance between the two extrusion ends; The second stretching mechanism (4) is mounted on the frame (1) and arranged close to the first spinning mechanism (2), the second stretching mechanism (4) having a stretching cavity (411), and the second stretching mechanism (4) is used to stretch a workpiece placed in the stretching cavity (411) by differential temperature.
2. The device for manufacturing a fixing film thin-wall tube of an image forming device according to claim 1, characterized in that: The first spinning mechanism (2) comprises: A driving shaft (21) is horizontally arranged on the frame (1), and the driving shaft (21) is capable of rotating along its own axis relative to the frame (1); There are two elliptical disks (22), and the extrusion ends are located on the elliptical disks (22). The axes of the elliptical disks (22) are parallel to the axis of the driving shaft (21), and the elliptical disks (22) are located on both sides of the driving shaft (21).
3. The device for manufacturing a fixing film thin-wall tube of an image forming device according to claim 2, characterized in that: The regulating component (3) comprises: A fixing rod (31), one end of which is coaxially arranged and fixedly connected to the elliptical disk (22), and the other end of which is fixedly connected to the frame (1); A synchronous rotation driving member is arranged on the frame (1) and is used for synchronously driving the elliptical disk (22) to rotate.
4. The device for manufacturing a fixing film thin-wall tube for an image forming device according to claim 3, characterized in that: The synchronous rotation driving member comprises a first pulley (32), a second pulley (33) arranged opposite to the first pulley (32), a synchronous transmission belt located on the first pulley (32) and the second pulley (33), and a servo motor (34); the servo motor (34) is arranged on the frame (1); an output shaft of the servo motor (34) is coaxially arranged with the first pulley (32); the first pulley (32) and the second pulley (33) are connected to the two ellipses via the fixing rod (31).
5. The device for manufacturing a fixing film thin-wall tube for an image forming device according to claim 3, characterized in that: The first spinning mechanism (2) further comprises: A hydraulic cylinder (23) fixedly connected to the synchronous rotation driving member and used for driving the synchronous rotation driving member to move in a horizontal direction; The telescopic ram (24) is coaxially arranged with the driving shaft (21) and rotates relative to the driving shaft (21); the telescopic ram (24) is fixedly connected to the frame (1).
6. The device for manufacturing a fixing film thin-wall tube for an image forming device according to claim 5, characterized in that: The telescopic top (24) comprises: The mandrel body (241) rotates relative to the driving shaft (21); A spring (242), two ends of which are respectively fixedly connected to the mandrel body (241) and the frame (1); A guide rod (243) has one end fixedly connected to the head body (241) and the other end slidably connected inside the frame (1).
7. The device for manufacturing a fixing film thin-wall tube for an image forming device according to claim 4, characterized in that: The synchronous rotation driving member comprises: A reducer (35) is arranged on the servo motor (34) and is used to reduce the rotation speed of the servo motor (34) and increase the torque.
8. The device for manufacturing a fixing film thin-wall tube of an image forming device according to claim 1, characterized in that: The second pressing mechanism (4) comprises: A main mold (41), wherein the smoothing cavity (411) is coaxially opened on the main mold (41); The punching die (42) has a pressing head, the pressing head being in sliding engagement with the pressing cavity (411); A heating element is arranged on the main mold (41) and is used to heat the main mold (41).
9. The device for manufacturing a fixing film thin-wall tube for an image forming device according to claim 8, characterized in that: The diameter of the pressing cavity (411) gradually decreases in a direction away from the punching die (42) until it remains constant.
10. A method for manufacturing a fixing film thin-wall tube of an image forming device, using the manufacturing device for a fixing film thin-wall tube of an image forming device as described in any one of claims 1 to 9, characterized in that: The following steps are involved: S1, sleeve and fix the cylindrical plain tube on the central axis of the first spinning mechanism (2), and use the adjustment component (3) to control and adjust the distance between the two extrusion ends; S2, starting the first spinning mechanism (2), rotating and extruding the cylindrical plain tube through two oppositely disposed extrusion ends, and adjusting the distance between the two extrusion ends again during this process so that the distance between the two extrusion ends gradually decreases, thereby obtaining a first metal thin-walled tube (5); S3, moving the first metal thin-walled tube (5) from the first spinning mechanism (2) into the stretching chamber (411) of the second stretching mechanism (4), starting the second stretching mechanism (4), and performing a temperature differential stretching process to obtain a second metal thin-walled tube (6).