Vacuum coating device

By using the flow diversion disc and airflow structure in the vacuum coating device to change the movement direction of the coated particles, combined with water-cooled heat dissipation and rotary ring clamp mechanism, the problems of temperature-sensitive substrate deformation and film layer defects are solved, and the coating quality and operating efficiency are improved .

CN118726916BActive Publication Date: 2024-11-15SUZHOU DENAI NANOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411234961.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-15
Estimated Expiration
2044-09-04

AI Technical Summary

Technical Problem

The existing evaporative coating technology has the risk of substrate deformation or damage when dealing with temperature-sensitive substrates, and the high-speed impact of the coating material particles leads to defects in the film layer, affecting the coating quality.

Method used

A vacuum coating device is designed, using a flow dial and airflow structure to change the movement direction of the coating particles, combined with a water-cooled heat dissipation structure to prevent heat from radiating to the substrate, and improve coating uniformity and convenience of sheet removal through the rotating ring and clamp mechanism.

Benefits of technology

It effectively avoids damage to the substrate due to high temperature deformation, reduces the kinetic energy of the coated particles, improves the film quality and working efficiency, and ensures uniform coating and rapid cooling of the substrate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118726916B_ABST
    Figure CN118726916B_ABST
Patent Text Reader

Abstract

The present invention discloses a vacuum coating device, including a coating tank, wherein a loading tray for placing coating materials, an induction heating coil for heating coating materials, and a fixing mechanism for placing substrates are arranged inside the coating tank, a column is welded and fixed to the inner wall at the bottom end of the coating tank, a first air inlet pipe and a second air inlet pipe are penetrated through the wall at the bottom end of the coating tank, a material guide pipe is penetrated through the wall at the top end of the coating tank, a guide ring is welded and fixed to the inner wall of the coating tank, the top end of the column extends into the material guide pipe, and the loading tray is sleeved and fixed on the outer wall of the column. A vacuum coating device of the present invention is provided with a guide tray, which can isolate the inside of the coating tank. Since the fixing mechanism of the substrate is located at the top of the coating tank, and the induction heating coil is located at the bottom of the coating tank, heat radiation to the substrate is avoided, and deformation and damage of the substrate due to high temperature is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of coating equipment, and in particular to a vacuum coating device. Background Art

[0002] Vacuum coating technology is widely used in the fields of optical devices, electronic components and decorations, mainly including three methods: evaporation coating, sputtering coating and ion coating. Among them, evaporation coating is a process in which the coating material is evaporated and deposited on the surface of the substrate by heating. In the evaporation coating process, in order for the coating material to evaporate successfully, it is usually necessary to heat it to a higher temperature. However, since the heating source is usually located under the substrate, the heat radiation generated during the evaporation process will be conducted to the substrate, causing the substrate temperature to rise. For some temperature-sensitive substrate materials, especially resin materials, excessively high temperatures may cause deformation or damage to the substrate, thereby affecting the coating effect and film quality.

[0003] In addition, the evaporated coating material particles directly hit the substrate surface at high speed under high temperature conditions, which may not only cause impact damage to the film layer, but also increase the risk of film defects, ultimately reducing the overall quality of the coating. Therefore, the existing evaporation coating technology has certain limitations when processing temperature-sensitive substrates, and it is necessary to optimize and improve the equipment to overcome these shortcomings and improve the coating quality. Summary of the invention

[0004] The present invention aims to solve at least one of the technical problems existing in the prior art or related art.

[0005] Therefore, the object of the present invention is to provide a vacuum coating device, comprising a coating tank, wherein the coating tank is provided with a loading tray for placing a coating material, an induction heating coil for heating the coating material, and a fixing mechanism for placing a substrate;

[0006] A column is welded and fixed to the inner wall of the bottom end of the coating tank, a first air inlet pipe and a second air inlet pipe are welded and connected to the bottom end wall of the coating tank, a material guide pipe is welded and connected to the top end wall of the coating tank, and a guide ring is welded and fixed to the inner wall of the coating tank;

[0007] The top end of the column extends into the material guide pipe, and the loading tray is sleeved and fixed on the outer wall of the column;

[0008] The guide tube is sleeved with a guide plate and a sleeve welded thereto, and the outer wall of the guide tube is welded and fixed with a first sealing ring and a second sealing ring from bottom to top;

[0009] The inner wall of the sleeve and the outer circular walls of the first sealing ring and the second sealing ring are all welded and fixed, and a guide plate welded and fixed to the outer wall of the sleeve is sleeved on the outer wall of the sleeve;

[0010] The top ends of the first air inlet pipe and the second air inlet pipe extend into the column and extend out from the top end of the column; the first sealing ring, the second sealing ring, the outer wall of the material guide pipe and the inner wall of the sleeve form a first air collecting cavity; the second sealing ring, the outer wall of the material guide pipe and the inner wall of the sleeve form a second air collecting cavity.

[0011] The material guide pipe wall at the first gas collecting cavity is connected to the first air inlet pipe by welding, the sleeve wall at the first gas collecting cavity is evenly provided with first through holes, the material guide pipe wall at the second gas collecting cavity is connected to the second air inlet pipe by welding, and the sleeve wall at the second gas collecting cavity is evenly provided with second through holes;

[0012] The outer circular wall of the guide plate extends outward obliquely to form a guide step.

[0013] The bottom ends of the first air inlet pipe and the second air inlet pipe are connected to a gas tank through a three-way connection. The gas tank is filled with an inert gas, such as helium, nitrogen, etc., so that when the gas guides the evaporated coating particles, it will not react with the evaporated coating particles, thereby ensuring the subsequent coating quality.

[0014] A threaded hole is provided at the top of the coating tank, and a top cover is screwed into the threaded hole. By opening the top cover, it is convenient to place the substrate on the fixing mechanism, or to take out the coated substrate from the fixing mechanism.

[0015] As the preferred technical solution:

[0016] In the vacuum coating device as described above, the material loading tray is in the shape of a hollow ring, the top surface of the material loading tray is open, a material guiding step is formed on the column, and the bottom of the material guiding step is flush with the top surface of the material loading tray.

[0017] Through the above technical solution, the material guide step is a conical structure, and the side of the material guide step is a slope. In this way, when it is necessary to add coating material, the granular coating material can be put into the material guide tube. After the coating material falls onto the material guide step, it will slide into the loading tray, thereby realizing rapid addition of material.

[0018] In the vacuum coating device as described above, the bottom ends of the guide tube and the sleeve are both open, the diameter of the guide tube is smaller than the inner diameter of the sleeve, the inner diameter of the guide tube is larger than the top diameter of the column, and the guide tube, sleeve and column share a common axis.

[0019] Through the above technical solution, the top of the material guide tube is also open, and the top of the material guide tube is threadedly connected with a sealing plug, so that the material guide tube can be sealed during operation to ensure that the coating operation in the coating tank proceeds normally. At the same time, the diameter of the sleeve is smaller than the inner diameter of the loading tray. This design ensures that after the coating material in the loading tray evaporates, the movement path of the coating particles is outside the sleeve, and will not move to the inside of the material guide tube and the sleeve, thereby avoiding waste of coating materials.

[0020] In the vacuum coating device as described above, the guide plate is in the shape of an inverted truncated cone, the bottom surface of the guide plate is parallel to the guide plate, and the guide plate and the side angle of the guide plate are consistent with the inclination angle of the guide step.

[0021] A guide layer is formed between the bottom surface of the guide disc and the guide plate, and the guide layer is connected to the second through hole;

[0022] The top surfaces of the guide plate and the guide ring are flush, and an annular air guide channel is formed between the outer circular wall of the guide plate and the inner circular wall of the guide ring.

[0023] Through the above technical scheme, the guide plate and the guide plate cooperate with each other, so that the airflow ejected from the second through hole can form a horizontal laminar airflow. The horizontal laminar airflow will flow upward at an angle under the guidance of the side of the guide plate and the guide step, that is, it will flow along the side of the guide plate, thereby changing the movement direction of the coated particles after contacting the coated particles.

[0024] In a vacuum coating device as described above, a spiral cooling groove is opened in the top wall of the guide plate, one end of the cooling groove is welded to a water inlet pipe, and the other end of the cooling groove is welded to a water outlet pipe, and the top ends of the water inlet pipe and the water outlet pipe penetrate the wall of the coating tank and are connected to the water tank.

[0025] Through the above technical solution, the coolant can be introduced into the cooling tank through the water inlet pipe. After the coolant flows along the cooling tank for a circle, it finally flows back into the water tank through the water outlet pipe, thereby realizing the circulation of the coolant. During the circulation process, the coolant can continuously take away the heat on the guide plate, thereby cooling the guide plate.

[0026] A vacuum coating device as described above, wherein the fixing mechanism includes a rotating ring and a gear ring welded to the inner circular wall of the rotating ring, the outer circular wall of the rotating ring is connected to the inner wall bearing of the coating tank, an electric motor is bolted to the top of the coating tank, and the output shaft of the motor extends into the coating tank and is fixed with a gear meshing with the gear ring by a pin.

[0027] Through the above technical solution, the rotating ring is a rotating movable structure in the coating tank. When the motor is connected to the power grid and started, the motor can drive the gear to rotate. The gear can drive the rotating ring to rotate axially through the meshing action with the ring gear. Then the rotating ring can drive the substrate to rotate, thereby improving the uniformity of the coating.

[0028] In the vacuum coating device as described above, the rotating ring is provided with a plurality of through slots for connecting columns to pass through, the two ends of the connecting columns are respectively welded and fixed with a top plate and a bottom plate, the top plate has a diameter larger than the inner diameter of the through slots, and the bottom end of the bottom plate is attached with a first clamping plate and a second clamping plate,

[0029] A vertical plate is welded and fixed to the outer wall of the first clamping plate, a fixing frame is welded and fixed to the top of the vertical plate, the fixing frame is sleeved on the connecting column, and the inner frame wall of the fixing frame is welded and fixed to the connecting column through an elastic spring.

[0030] Through the above technical solution, the size of the top plate is designed so that it can be placed on the rotating ring without falling from the through groove. When removing or installing the substrate, it is only necessary to pick up the top plate, and then the bottom plate can be brought out through the connecting column, and then the substrate between the first clamping plate and the second clamping plate can be taken out from the rotating ring, which is convenient to use.

[0031] In the vacuum coating device as described above, the fixing frame is in a right-angle U shape, the connecting column is in a rectangular columnar structure, the inner frame wall of the fixing frame is in contact with the outer wall of the connecting column, and the fixing frame is in contact with the top surface of the bottom plate.

[0032] Through the above technical solution, the shape design of the connecting column and the fixed frame allows the fixed frame to only move linearly on the connecting column, that is, the moving direction of the fixed frame is consistent with the expansion and contraction direction of the elastic spring, and the structure is reasonable.

[0033] In the vacuum coating device as described above, the first clamping plate and the second clamping plate are both right-angled, the first clamping plate is attached to the bottom plate but not fixed, and the second clamping plate is welded and fixed to the bottom plate.

[0034] Through the above technical solution, the shape design of the first clamping plate and the second clamping plate allows them to be combined into a square frame when brought together, so that they can clamp and fix the circular substrate, and also can clamp and fix the circular substrate, thereby improving the application range of the device.

[0035] Compared with the prior art, the present invention has at least the following beneficial effects:

[0036] (1) A vacuum coating device of the present invention is provided with a guide plate, which can isolate the inside of the coating tank. Since the fixing mechanism of the substrate is located at the top of the coating tank and the induction heating coil is located at the bottom of the coating tank, the heat generated by the induction heating coil will first be radiated to the guide plate when radiating to the substrate. The guide plate is provided with a water-cooled heat dissipation structure consisting of a water inlet pipe, a cooling trough and a water outlet pipe. In this way, by discharging heat in time, heat radiation to the substrate can be avoided, thereby preventing the substrate from being deformed and damaged due to high temperature.

[0037] (2) A vacuum coating device of the present invention is provided with a first air inlet pipe and a second air inlet pipe. Gas can be introduced into the first air inlet pipe and ejected from the first through hole and the second through hole. The ejected gas can change the movement direction of the evaporated coating particles, so that the coating material vapor can continuously change the forward direction, thereby reducing the kinetic energy of large particles, causing the large particles to lose kinetic energy and fall to the bottom of the evaporation system, thereby making the coating particles contact the substrate at a slow speed, without causing damage to the film layer, thereby ensuring the coating quality.

[0038] (3) In a vacuum coating device of the present invention, after coating is completed, the substrate needs to be cooled before it can be taken out. At this time, the airflow ejected from the first through hole and the second through hole can not only reduce the movement rate of the coating particles, but also cool the substrate by air cooling, thereby reducing the cooling time and helping to improve the overall operating efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which

[0040] Figure 1 It is an internal front view of the present invention;

[0041] Figure 2 is an internal cross-sectional view of the present invention;

[0042] Figure 3 It is an internal top view of the present invention;

[0043] Figure 4 It is a three-dimensional diagram of the guide tube and the sleeve of the present invention;

[0044] Figure 5 For the present invention Figure 2 Enlarged view of point A in the middle;

[0045] Figure 6 For the present invention Figure 2 Enlarged view of point B;

[0046] Figure 7 A top view of the connecting column and the fixing frame of the present invention;

[0047] Figure 8 A three-dimensional diagram of the first clamping plate and the second clamping plate of the present invention;

[0048] Fig. 9 It is a top cross-sectional view of the guide plate and cooling groove of the present invention.

[0049] In the figure: 1, coating tank; 101, guide ring; 2, column; 201, material guide step; 3, loading plate; 4, induction heating coil; 5, guide plate; 6, material guide pipe; 7, sleeve; 8, first air inlet pipe; 9, second air inlet pipe; 10, first sealing ring; 11, second sealing ring; 12, first through hole; 13, second through hole; 14, guide plate; 15, guide step; 16, rotating ring; 17, through groove; 18, top plate; 19, connecting column; 20, bottom plate; 21, first clamping plate; 22, second clamping plate; 23, vertical plate; 24, fixing frame; 25, elastic spring; 26, gear ring; 27, gear; 28, water inlet pipe; 29, cooling trough; 30, water outlet pipe. DETAILED DESCRIPTION

[0050] In order to more clearly understand the above-mentioned purpose, features and advantages of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be noted that the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.

[0051] In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention may also be implemented in other ways different from those described herein. Therefore, the protection scope of the present invention is not limited to the specific embodiments disclosed below.

[0052] like Figure 1 , Figure 2 and Figure 4 As shown, an embodiment of the present invention discloses a vacuum coating device, including a coating tank 1, wherein a material loading tray 3 for placing coating materials, an induction heating coil 4 for heating the coating materials, and a fixing mechanism for placing a substrate are arranged inside the coating tank 1, a column 2 is welded and fixed to the inner wall of the bottom end of the coating tank 1, and the material loading tray 3 is sleeved and fixed on the outer wall of the column 2, the material loading tray 3 is in a hollow annular shape, and the top surface of the material loading tray 3 is open, and a material guiding step 201 is formed on the column 2, and the bottom of the material guiding step 201 is flush with the top surface of the material loading tray 3,

[0053] The top wall of the coating tank 1 is penetrated by a material guide pipe 6 welded thereto, the top of the column 2 extends into the material guide pipe 6, the bottom ends of the material guide pipe 6 and the sleeve 7 are both open, the diameter of the material guide pipe 6 is smaller than the inner diameter of the sleeve 7, the inner diameter of the material guide pipe 6 is larger than the top diameter of the column 2, and the material guide pipe 6, the sleeve 7 and the column 2 are coaxial;

[0054] During operation, the granular coating material can be put into the guide tube 6, and the coating material will roll down along the guide tube 6, and finally fall out from the bottom opening of the guide tube 6 and fall onto the guide step 201 on the column 2. At this time, the coating material will roll down along the guide step 201 to the loading tray 3. After the material adding operation is completed, the top of the guide tube 6 is sealed.

[0055] Then place the substrate to be coated on the fixing mechanism.

[0056] The coating tank 1 is connected to a vacuum pump through a vacuum tube, and the vacuum pump can be used to evacuate the coating tank 1. After the vacuuming is completed, the induction heating coil 4 can be connected to the power supply and run. The induction heating coil 4 can heat the coating material in the loading tray 3. After heating, the coating material evaporates and moves upward in the form of particles, and finally deposited on the substrate to complete the coating operation. After the coating is completed, the substrate can be taken out from the fixing mechanism after cooling.

[0057] like Figure 2 , Figure 4 and Figure 5 As shown, in this embodiment, the bottom wall of the coating tank 1 is penetrated by a first air inlet pipe 8 and a second air inlet pipe 9 welded thereto, a guide plate 5 and a sleeve 7 welded thereto are sleeved on the guide pipe 6, a first sealing ring 10 and a second sealing ring 11 are welded and fixed to the outer wall of the guide pipe 6 from bottom to top, the inner wall of the sleeve 7 and the outer circular walls of the first sealing ring 10 and the second sealing ring 11 are welded and fixed, the top ends of the first air inlet pipe 8 and the second air inlet pipe 9 extend into the column 2 and extend from the top end of the column 2, and the first sealing ring 10 and the second sealing ring 11 are welded and fixed. A first air collecting cavity is formed between the ring 10, the second sealing ring 11, the outer wall of the material guide tube 6 and the inner wall of the sleeve 7, a second air collecting cavity is formed between the second sealing ring 11, the outer wall of the material guide tube 6 and the inner wall of the sleeve 7, the wall of the material guide tube 6 at the first air collecting cavity is welded and connected to the first air inlet pipe 8, the wall of the sleeve 7 at the first air collecting cavity is evenly provided with first through holes 12, the wall of the material guide tube 6 at the second air collecting cavity is welded and connected to the second air inlet pipe 9, and the wall of the sleeve 7 at the second air collecting cavity is evenly provided with second through holes 13.

[0058] While the induction heating coil 4 heats the coating material, the gas can be introduced into the first air inlet pipe 8 and the second air inlet pipe 9. The first air inlet pipe 8 and the second air inlet pipe 9 are both provided with flow regulating valves to adjust the flow rate of the gas so that the gas can change the movement direction of the coating particles without blowing away the coating particles.

[0059] The gas in the first air inlet pipe 8 can be passed into the first gas collecting cavity, and finally ejected horizontally from the first through hole 12. The horizontally ejected gas will collide with the coating particles moving upward, and then the ejected gas will carry the coating particles to move horizontally. At this time, the running direction of the coating particles changes for the first time.

[0060] After the horizontally moving coated particles are separated from the gas, they will move upward again, that is, move upward toward the side of the guide plate 5;

[0061] The gas in the second air inlet pipe 9 can be passed into the second air collecting cavity, and finally ejected horizontally from the second through hole 13. Under the guidance of the guide plate 5, the guide plate 14 and the guide step 15, the ejected airflow will flow upward along the side of the guide plate 5. After the obliquely flowing gas collides with the upwardly moving gas, it will carry the coating particles to synchronously tilt, and at this time, the running direction of the coating particles changes for the second time.

[0062] After the tilted coating particles leave the gas, they move upward again, that is, move upward toward the fixing mechanism, and finally deposit on the substrate surface to complete the coating operation;

[0063] After the coated particles have changed their movement direction twice, the movement speed of the coated particles will be reduced to a gentle level, and the coated particles at this time will not cause damage to the substrate after contacting with the substrate;

[0064] It is understandable that the present invention adopts a specially designed gas path structure to make the coating material vapor change direction multiple times during the forward process, thereby reducing the kinetic energy of large particles. After the kinetic energy is reduced, the large particles settle to the bottom of the evaporation system, reducing their impact on the film layer, thereby avoiding the generation of film layer defects.

[0065] Through the above design, the direction of the coating particles can be changed in the first half of the movement, and the direction of the coating particles in the second half will not be affected. In this way, there is no need to change the placement of the substrate, that is, the substrate can be placed horizontally, thereby ensuring the uniformity of the substrate coating, and the ejected gas will not participate in the coating operation, thereby not interfering with the coating operation.

[0066] like Figure 1 and Figure 2As shown, in this embodiment, a guide ring 101 is welded and fixed on the inner wall of the coating tank 1, and a guide plate 14 welded and fixed thereto is sleeved on the outer wall of the sleeve 7, and the outer circular wall of the guide plate 14 extends outward obliquely to form a guide step 15, and the guide plate 5 is in the shape of an inverted truncated cone, and the bottom surface of the guide plate 5 is parallel to the guide plate 14, and the guide plate 5 and the side angle of the guide plate 5 are consistent with the inclination angle of the guide step 15, and a guide layer is formed between the bottom surface of the guide plate 5 and the guide plate 14, and the guide layer is connected to the second through hole 13, and the guide plate 5 is flush with the top surface of the guide ring 101, and an annular air guide channel is formed between the outer circular wall of the guide plate 5 and the inner circular wall of the guide ring 101;

[0067] When the coating operation is completed, in order to increase the cooling rate of the substrate, only the second air inlet pipe 9 can be opened at this time, and the gas flow rate can be increased. The gas in the second air inlet pipe 9 will eventually be ejected through the second through hole 13, and the ejected gas will flow between the guide disk 5 and the guide plate 14, and finally under the guidance of the guide step 15, it will flow upward along the side of the guide disk 5, and finally flow upward through the air guide channel. The upward flowing gas can contact the substrate on the fixing mechanism, and can perform convection heat dissipation.

[0068] like Figure 2 , Figure 3 , Figure 6 , Figure 7 and Figure 8 As shown, in this embodiment, the fixing mechanism includes a rotating ring 16, and a gear ring 26 welded on the inner circular wall of the rotating ring 16, the outer circular wall of the rotating ring 16 is connected to the inner wall bearing of the coating tank 1, a motor is fixed to the top bolt of the coating tank 1, the output shaft of the motor extends into the coating tank 1 and is fixed with a gear 27 meshing with the gear ring 26 by a bayonet, a plurality of through grooves 17 for the connecting column 19 to penetrate are opened on the rotating ring 16, and a top plate 18 and a bottom plate 20 are welded and fixed at both ends of the connecting column 19, and the diameter of the top plate 18 is larger than the inner diameter of the through groove 17, and a first clamping plate 21 and a second clamping plate 22 are attached to the bottom end of the bottom plate 20, and the first clamping plate 21 and the second clamping plate 22 are both right-angled, the first clamping plate 21 is attached to the bottom plate 20 and is not fixed, and the second clamping plate 22 is welded and fixed to the bottom plate 20.

[0069] A vertical plate 23 is welded and fixed to the outer wall of the first clamping plate 21, and a fixed frame 24 is welded and fixed to the top of the vertical plate 23. The fixed frame 24 is sleeved on the connecting column 19, and the inner frame wall of the fixed frame 24 is welded and fixed to the connecting column 19 through an elastic spring 25. The fixed frame 24 is a right-angle U-shape, and the connecting column 19 is a rectangular columnar structure. The inner frame wall of the fixed frame 24 is in contact with the outer wall of the connecting column 19, and the fixed frame 24 is in contact with the top surface of the bottom plate 20.

[0070] Before operation, first open the top cover on the coating tank 1, then press the fixing frame 24 by hand, at this time the fixing frame 24 will move along the connecting column 19, the elastic spring 25 is in a compressed state, when the fixing frame 24 moves, it will drive the first clamping plate 21 to move through the vertical plate 23, so that the first clamping plate 21 and the second clamping plate 22 are away from each other, then place the substrate between the first clamping plate 21 and the second clamping plate 22 and release the fixing frame 24, the fixing frame 24 is reset under the elastic force of the elastic spring 25, so that the first clamping plate 21 and the second clamping plate 22 are close to each other and clamp the substrate, when the fixing is completed, pass the connecting column 19 and the bottom plate 20 through the through slot 17 and put the top plate 18 on the rotating ring 16, when the substrate needs to be taken out, the opposite operation can be performed.

[0071] Since multiple base plates 20 are provided, the rotating ring 16 can be driven to rotate by starting the motor, so that multiple substrates can be installed and fixed;

[0072] In order to prevent the top plate 18 from shaking on the rotating ring 16 , the through groove 17 is designed as a countersunk structure, so that a portion of the top plate 18 will sink into the through groove 17 .

[0073] Since the fixing frame 24 and the first clamping plate 21 can only move linearly in contact with the bottom plate 20, the first clamping plate 21 can be prevented from deflecting, thereby ensuring the clamping and fixing effect of the substrate.

[0074] like Figure 1 and Fig. 9 As shown, in this embodiment, a spiral cooling groove 29 is opened in the top wall of the guide plate 5, one end of the cooling groove 29 is welded to a water inlet pipe 28, and the other end of the cooling groove 29 is welded to a water outlet pipe 30. The top ends of the water inlet pipe 28 and the water outlet pipe 30 penetrate the wall of the coating tank 1 and are connected to the water tank.

[0075] The fixing mechanism is located at the top of the coating tank 1, and the induction heating coil 4 is located at the bottom of the coating tank 1, and the two are separated by the guide plate 5, so that the heat at the induction heating coil 4 will be indirectly radiated to the fixing mechanism through the guide plate 5. Therefore, it is only necessary to cool the guide plate 5 to prevent heat from being radiated to the fixing mechanism, thereby avoiding damage to the substrate due to high temperature.

[0076] The water inlet pipe 28 , the water outlet pipe 30 , the cooling groove 29 and the water tank can be combined into a water-cooled heat dissipation mechanism. When the coolant flows in the cooling groove 29 , the heat on the guide plate 5 can be taken away, thereby cooling the guide plate 5 .

[0077] In the description of this specification, "connection", "installation", "fixation" and the like should be understood in a broad sense. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0078] In the description of this specification, the description of the terms "one embodiment", "some embodiments", "specific embodiments", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0079] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A vacuum coating device, comprising a coating tank (1), wherein the coating tank (1) is provided with a material loading tray (3) for placing coating materials, an induction heating coil (4) for heating the coating materials, and a fixing mechanism for placing a substrate; Features: The fixing mechanism is located at the top of the coating tank (1), and the induction heating coil (4) is located at the bottom of the coating tank (1); a column (2) is welded and fixed to the inner wall of the bottom end of the coating tank (1); a first air inlet pipe (8) and a second air inlet pipe (9) are welded and connected to the bottom end wall of the coating tank (1); a material guide pipe (6) is welded and connected to the top end wall of the coating tank (1); and a guide ring (101) is welded and fixed to the inner wall of the coating tank (1); The top end of the column (2) extends into the material guide pipe (6), and the material loading tray (3) is sleeved and fixed on the outer wall of the column (2); The guide tube (6) is sleeved with a guide plate (5) and a sleeve (7) which are welded to the guide tube, and the outer wall of the guide tube (6) is welded with a first sealing ring (10) and a second sealing ring (11) in sequence from bottom to top; The inner wall of the sleeve (7) and the outer circular walls of the first sealing ring (10) and the second sealing ring (11) are welded and fixed, and a guide plate (14) is sleeved on the outer wall of the sleeve (7) and welded and fixed thereto; The top ends of the first air inlet pipe (8) and the second air inlet pipe (9) extend into the column (2) and extend out from the top end of the column (2); the first sealing ring (10), the second sealing ring (11), the outer wall of the material guide pipe (6) and the inner wall of the sleeve (7) form a first air collecting cavity; the second sealing ring (11), the outer wall of the material guide pipe (6) and the inner wall of the sleeve (7) form a second air collecting cavity. The wall of the material guide pipe (6) at the first gas collection cavity is connected to the first air inlet pipe (8) by welding, the wall of the sleeve (7) at the first gas collection cavity is evenly provided with first through holes (12), the wall of the material guide pipe (6) at the second gas collection cavity is connected to the second air inlet pipe (9) by welding, and the wall of the sleeve (7) at the second gas collection cavity is evenly provided with second through holes (13); The outer circular wall of the guide plate (14) extends outwardly at an angle to form a guide step (15); The guide plate (5) is in the shape of an inverted truncated cone, the bottom surface of the guide plate (5) is parallel to the guide plate (14), and the angle of the side surface of the guide plate (5) is consistent with the inclination angle of the guide step (15); A guide layer is formed between the bottom surface of the guide disc (5) and the guide plate (14), and the guide layer is connected to the second through hole (13); The top surfaces of the guide plate (5) and the guide ring (101) are flush, and an annular air guide channel is formed between the outer circular wall of the guide plate (5) and the inner circular wall of the guide ring (101); The guide plate and the guide plate cooperate with each other, so that the airflow ejected from the second through hole forms a horizontal laminar airflow, and the horizontal laminar airflow will flow upward obliquely under the guidance of the side of the guide plate and the guide step, that is, it will flow along the side of the guide plate, thereby changing the movement direction of the coated particles after contacting with the coated particles; The fixing mechanism comprises a rotating ring (16) and a gear ring (26) welded to the inner circular wall of the rotating ring (16); the outer circular wall of the rotating ring (16) is connected to the inner wall bearing of the coating tank (1); a motor is bolted to the top of the coating tank (1); the output shaft of the motor extends into the coating tank (1) and is fixed with a gear (27) meshing with the gear ring (26) by a latch.

2. A vacuum coating device according to claim 1, characterized in that: The material loading tray (3) is in the shape of a hollow ring, the top surface of the material loading tray (3) is open, a material guiding step (201) is formed on the column (2), and the bottom of the material guiding step (201) is flush with the top surface of the material loading tray (3).

3. The vacuum coating device according to claim 1, characterized in that: The bottom ends of the material guide tube (6) and the sleeve (7) are both open, the diameter of the material guide tube (6) is smaller than the inner diameter of the sleeve (7), the inner diameter of the material guide tube (6) is larger than the top diameter of the column (2), and the material guide tube (6), the sleeve (7) and the column (2) are coaxial.

4. The vacuum coating device according to claim 1, characterized in that: A spiral cooling groove (29) is provided in the wall of the top end of the guide plate (5); one end of the cooling groove (29) is welded to a water inlet pipe (28); the other end of the cooling groove (29) is welded to a water outlet pipe (30); the top ends of the water inlet pipe (28) and the water outlet pipe (30) penetrate the wall of the coating tank (1) and are connected to the water tank.

5. The vacuum coating device according to claim 1, characterized in that: The rotating ring (16) is provided with a plurality of through slots (17) for the connecting columns (19) to pass through. A top plate (18) and a bottom plate (20) are respectively welded and fixed to both ends of the connecting columns (19). The diameter of the top plate (18) is larger than the inner diameter of the through slots (17). The bottom end of the bottom plate (20) is fitted with a first clamping plate (21) and a second clamping plate (22). A vertical plate (23) is welded and fixed to the outer wall of the first clamping plate (21), a fixing frame (24) is welded and fixed to the top of the vertical plate (23), the fixing frame (24) is sleeved on the connecting column (19), and the inner frame wall of the fixing frame (24) is welded and fixed to the connecting column (19) via an elastic spring (25).

6. A vacuum coating device according to claim 5, characterized in that: The fixing frame (24) is in a right-angled U shape, the connecting column (19) is in a rectangular columnar structure, the inner frame wall of the fixing frame (24) is in contact with the outer wall of the connecting column (19), and the fixing frame (24) is in contact with the top surface of the bottom plate (20).

7. The vacuum coating device according to claim 5, characterized in that: The first clamping plate (21) and the second clamping plate (22) are both in a right-angle shape; the first clamping plate (21) is attached to the bottom plate (20) but is not fixed thereto; and the second clamping plate (22) is welded and fixed to the bottom plate (20).