Low-smoke halogen-free low-toxicity flame-retardant longitudinal water-sealed power cable for ships and warships

By adopting a triple water-blocking structure and low-smoke, halogen-free, low-toxic flame-retardant materials in longitudinal water-sealed power cables for ships, the problem of reduced water-blocking performance of existing cables is solved, and higher longitudinal sealing and water-blocking effects are achieved. , and provides excellent flame retardant protection.

CN118737549APending Publication Date: 2024-10-01ANHUI CABLE
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410942525.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing longitudinal water-sealed power cables for ships only have one layer of armor between the filler and the outer sheath, which cannot effectively protect against water. As a result, the water-blocking performance of the cable decreases rapidly when the outer sheath ruptures, affecting its use.

Method used

A triple water-blocking structure is adopted, including filling the cable cores with water-blocking halogen-free sealant, a second wrapping layer placed outside the filling layer to support the connection between the filling layer and the inner lining layer, and low-smoke non-toxic sealant used outside the armor layer. Halogen flame retardant tape wrapping , the outer sheath is made of low-smoke, halogen-free, low-toxic, flame-retardant, cross-linked polyolefin material to form a twisted-fill water-blocking halogen-free sealant, a wire-core cable-filled water-blocking halogen-free sealant, and a braided armored outer wrap with low The combined structure of smoke halogen-free water blocking tape.

Benefits of technology

The longitudinal water-blocking performance and sealing effect of the cable are improved. Even if the outer sheath is broken, the internal water-blocking performance can be maintained. The outer sheath has excellent flame retardant effect, reducing damage during use of the cable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737549A_ABST
    Figure CN118737549A_ABST
Patent Text Reader

Abstract

The invention discloses a low-smoke halogen-free low-toxicity flame-retardant longitudinal water-sealed power cable for ships, which relates to the technical field of cables and comprises a conductor, and a wrapping layer I is compounded on the outer ring surface of the conductor. According to the invention, the waterproof halogen-free sealant is filled between the cable cores, and a non-fiber material is arranged, so that the tightness degree of connection after the single wires are twisted can be improved; a triple water-blocking structure consisting of stranded wire injection glue, a filling layer and a wrapping layer III is adopted, namely, water-blocking halogen-free sealant is filled in a stranded manner, water-blocking halogen-free sealant is filled in cable core cabling, and a low-smoke halogen-free water-blocking tape is wrapped outside a braided armor, so that the longitudinal water-blocking performance in the cable can be improved, and the longitudinal sealing effect of the cable is improved; the second wrapping layer is arranged outside the filling layer and can support the filling layer and assist connection of the filling layer and the lining layer, and the outer sheath is made of low-smoke halogen-free low-toxicity flame-retardant cross-linked polyolefin, has an excellent flame-retardant effect and can perform flame-retardant protection on the outside of the cable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of cables, in particular to a low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships. Background Art

[0002] With the development of the global marine economy, the market for longitudinal watertight power cables for ships is showing a rapid growth trend. This type of cable has the characteristics of being waterproof, moisture-proof, and corrosion-resistant, and can operate stably in harsh marine environments, so it is widely used in the fields of ships, marine engineering, etc.

[0003] For example, Chinese patent CN203102996U discloses a low-smoke halogen-free flame-retardant longitudinal watertight longitudinal airtight power cable, which has a structure of using a regular twisted tinned copper wire conductor, the outer periphery of which is an inner insulation of irradiated cross-linked polyethylene, the outer periphery of the inner insulation is an outer insulation of irradiated cross-linked ethylene-propylene rubber, the outer periphery of the outer insulation is a filling glue filled with hot melt adhesive in the middle and edge gaps after the multi-core cabling, and the outer periphery of the filling glue is a low-smoke halogen-free flame-retardant polyolefin material as an outer sheath.

[0004] In the above-mentioned patent, although the problem of poor longitudinal water vapor sealing of existing cables is solved by continuous injection of glue and outer sheath, only one layer of armor is arranged between the filling glue and the outer sheath. The armor is made of tinned copper wire and cannot provide water-blocking protection between the armor layer and the outer sheath. When the outer sheath is broken, the overall water-blocking performance of the cable decreases rapidly, thereby affecting the overall use of the cable.

[0005] Therefore, the present invention provides a low-smoke, halogen-free, low-toxicity, flame-retardant, longitudinal water-sealed power cable for ships, which is used to solve the above-mentioned related technical problems. Summary of the invention

[0006] The purpose of the present invention is to provide a low-smoke, halogen-free, low-toxic, flame-retardant, longitudinal water-sealed power cable for ships, so as to solve the problem proposed in the above background technology that only one layer of armor is arranged between the filling rubber and the outer sheath, and the armor is made of tinned copper wire, and water-blocking protection cannot be provided between the armor layer and the outer sheath. When the outer sheath is broken, the overall water-blocking performance of the cable decreases rapidly, thereby affecting the overall use of the cable.

[0007] To achieve the above object, the present invention provides the following technical solutions: The present invention provides a low-smoke, halogen-free, low-toxic, flame-retardant, longitudinal water-sealed power cable for ships, comprising a conductor, wherein the outer annular surface of the conductor is compounded with a first winding layer, the outer annular surface of the first winding layer is compounded with an insulating layer, the outer annular surface of the insulating layer is provided with a second winding layer, a filling layer is provided between the second winding layer and the insulating layer, the outer annular surface of the second winding layer is compounded with an inner lining layer, the outer annular surface of the inner lining layer is provided with an armor layer, the outer annular surface of the armor layer is compounded with a third winding layer, and the outer annular surface of the third winding layer is compounded with an outer sheath.

[0008] The present invention is further configured as follows: the conductor is made of tinned copper wire and rubber wire, and the armor layer is made of tinned copper wire braided.

[0009] The present invention is further configured as follows: the first wrapping layer and the second wrapping layer are both made of insulating water-blocking tape.

[0010] The present invention is further configured as follows: the insulating layer is made of 150° C. high-strength, oil-resistant, halogen-free, low-smoke irradiated insulating material, and the filling layer is made of water-blocking halogen-free sealant.

[0011] The present invention is further configured as follows: the inner lining layer and the outer sheath are both made of 125°C oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material.

[0012] The present invention is further configured as follows: the wrapping layer three is made of a low-smoke, halogen-free, flame-retardant tape, and the low-smoke, halogen-free, and low-toxic flame-retardant cross-linked polyolefin is contained in the low-smoke, halogen-free, and low-toxicity flame-retardant tape.

[0013] The present invention is further configured to include the following steps: S1. Raw material pretreatment: clean the surface of the tinned copper wire, dry the surface of the copper wire for 5-10 minutes, and feed the copper wire into a wire drawing machine to draw the wire into a single wire; S2, twisted wire and primary glue injection: glue is injected during twisting to form a wire core, a wrapping layer and an insulating layer are arranged outside the wire core, the insulating material is wrapped around the outside of the conductor, and the wire is sent to the irradiation process to form a wire harness; S3, secondary glue injection and cabling: After arranging the wire harness, use the insulating water-blocking tape to wrap the outside of the wire harness to form the second wrapping layer, inject glue between the second wrapping layer and the wire harness, scrape off the excess glue, and form a filling layer; S4, inner sheath, braiding and wrapping: feed 125℃ oil-resistant halogen-free low-smoke flame-retardant irradiated cable material into an extruder, extrude it after heating treatment in the extruder, attach it to the outer surface of the second wrapping layer, cool and solidify it for 3-6 hours to make an inner lining layer, use a braiding machine to weave tinned copper wire into an armor layer, combine the armor layer and the inner lining layer, inject glue again, and wrap it with a low-smoke halogen-free flame-retardant tape on the outside of the armor layer after drying to make the third wrapping layer; S5. Sheath and testing: Use an extruder to extrude the 125℃ oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material, wrap the cable material around the outside of the third sheath, cool and solidify the cable to make an outer sheath, complete the overall cable processing, and perform a drip test and a water pressure test on the finished cable to test the sealing performance of the cable.

[0014] The present invention is further configured as follows: in step S4, when the wrapping layer is extruded three times, the screw speed of the extruder is 20-22 r / min, and the extrusion temperature is 155-175°C.

[0015] The present invention is further configured as follows: in the step S5, when performing the drip test, a cable sample of a predetermined length is selected, the sample is hung on the test equipment, the copper oxide heater is ignited, and the lower end of the cable is exposed to the flame. The test temperature is 90°C, the test time is 18 hours, and whether the cable drips is observed, and the shape of the dripping is recorded. The dripping material is collected, recorded and analyzed, and the dripping performance of the cable is evaluated according to the dripping condition of the cable.

[0016] The present invention is further configured as follows: in step S5, when performing the water pressure test, the following contents are also included: S51. Pretreatment of test supplies: put the cable into the dryer and dry it for 2-5 minutes, take out the cable, cool it to room temperature, clamp the dried cable sample with a clamp, inject a predetermined volume of test water into the water tank, and weigh the mass of the test water; S52, water flow, water pressure adjustment and testing: Use a water pump to increase the water flow, so that the test water level reaches the standard upper limit, set the test pressure to 7MPa, the test time to 6h, and test the water flow and pressure changes on the water pressure test bench; S53. Obtain test results: observe whether the cable leaks or breaks under water pressure, and evaluate the pressure resistance of the cable.

[0017] Compared with the prior art, the present invention has the following beneficial effects: In the present invention, by filling water-blocking halogen-free sealant between cable cores and arranging non-fiber materials, the tightness of the connection of the monofilament twisted wire can be improved; a triple water-blocking structure consisting of twisted wire injection, filling layer and sheathing layer is adopted, that is, the twisted wire is filled with water-blocking halogen-free sealant, the core is filled with water-blocking halogen-free sealant, and the braided armor is wrapped with low-smoke halogen-free water-blocking tape. The triple structure can improve the longitudinal water-blocking performance inside the cable, thereby improving the longitudinal sealing effect of the cable, and when the outer sheath is broken, the internal water-blocking performance can still be guaranteed; the sheathing layer 2 is arranged outside the filling layer, which can support the filling layer and assist the connection between the filling layer and the inner lining layer. The outer sheath adopts low-smoke halogen-free and low-toxic flame-retardant cross-linked polyolefin, which reaches Class A flame retardant level and has excellent flame retardant effect. It can provide flame retardant protection for the outside of the cable and reduce damage to the cable during use. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0019] Figure 1This is a flow chart of the low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships of the present invention; Figure 2 It is a schematic cross-sectional view of the low-smoke, halogen-free, low-toxicity, flame-retardant, longitudinal water-sealed power cable for ships of the present invention.

[0020] In the figure: 1. conductor; 2. winding layer 1; 3. insulation layer; 4. filling layer; 5. winding layer 2; 6. lining layer; 7. armor layer; 8. winding layer 3; 9. outer sheath. DETAILED DESCRIPTION

[0021] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Embodiment 1

[0022] Please refer to Figure 1-2 As shown, this embodiment provides a low-smoke, halogen-free, low-toxic, flame-retardant, longitudinal water-sealed power cable for ships, including a conductor 1, the outer surface of the conductor 1 is compounded with a wrapping layer 2, the outer surface of the wrapping layer 2 is compounded with an insulating layer 3, the outer surface of the insulating layer 3 is provided with a wrapping layer 2 5, a filling layer 4 is provided between the wrapping layer 2 5 and the insulating layer 3, the outer surface of the wrapping layer 2 5 is compounded with an inner lining layer 6, the outer surface of the inner lining layer 6 is provided with an armor layer 7, the outer surface of the armor layer 7 is compounded with a wrapping layer 3 8, and the outer surface of the wrapping layer 3 8 is compounded with an outer sheath 9.

[0023] The conductor 1 is made of tinned copper wire and rubber wire, the armor layer 7 is made of tinned copper wire braiding, the sheath layer 1 2 and the sheath layer 2 5 are both made of insulating water-blocking tape, the insulating layer 3 is made of 150°C high-strength oil-resistant halogen-free and low-smoke irradiated insulating material, the filling layer 4 is filled with water-blocking halogen-free sealant, the inner lining layer 6 and the outer sheath 9 are both made of 125°C oil-resistant halogen-free and low-smoke flame-retardant irradiated cable material, the sheath layer 3 8 is made of low-smoke halogen-free flame-retardant tape, and the low-smoke halogen-free flame-retardant tape contains low-smoke halogen-free and low-toxic flame-retardant cross-linked polyolefin. Embodiment 2

[0024] Please refer to Figure 1-2 As shown, this embodiment provides a low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships, and also includes the following steps: Step 1: Raw material pretreatment: clean the surface of the tinned copper wire, dry the surface of the copper wire for 6 minutes, and feed the copper wire into a wire drawing machine to draw the wire into a single wire; Step 2, twisting the wire and injecting glue once: inject glue when twisting the wire to make a wire core, set a wrapping layer 2 and an insulating layer 3 on the outside of the wire core, wrap the insulating material on the outside of the conductor 1, send it to the irradiation process, and make a wire harness; Step 3, secondary glue injection and cabling: After arranging the wire harness, use an insulating water-blocking tape to wrap the outside of the wire harness to form a second wrapping layer 5, inject glue between the second wrapping layer 5 and the wire harness, scrape off excess glue, and form a filling layer 4; Step 4, inner sheath, braiding and wrapping: feed 125°C oil-resistant halogen-free low-smoke flame-retardant irradiated cable material into an extruder, extrude it after heating treatment by the extruder, adhere it to the outer surface of the wrapping layer 2 5, cool and solidify it for 4 hours, make an inner lining layer 6, use a braiding machine to weave tinned copper wire into an armor layer 7, combine the armor layer 7 with the inner lining layer 6, inject glue again, and wrap it on the outside of the armor layer 7 with a low-smoke halogen-free flame-retardant tape after drying to make a wrapping layer 3 8. When extruding the wrapping layer 3 8, the screw speed of the extruder is 22r / min, and the extrusion temperature is 170°C; Step 5, sheath and testing: use an extruder to extrude the 125°C oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material, wrap the cable material around the outside of the wrapping layer 8, cool and solidify the cable to form an outer sheath 9, complete the overall processing of the cable, perform a drop test and a water pressure test on the finished cable, and test the sealing performance of the cable; When conducting a drip test, select a cable sample of a predetermined length, hang the sample on the test equipment, ignite the copper oxide heater, expose the lower end of the cable to the flame, the test temperature is 90°C, the test duration is 18 hours, observe whether the cable drips, record the shape of the dripping, collect and record the dripping, and evaluate the dripping performance of the cable based on the dripping condition of the cable; When conducting a water pressure test, the following contents are also included: 51. Pretreatment of test supplies: Place the cable in a dryer and dry for 3 minutes, take out the cable, cool it to room temperature, clamp the dried cable sample with a clamp, inject a predetermined volume of test water into the water tank, and weigh the mass of the test water; 52. Water flow and water pressure adjustment and testing: Use a water pump to increase the water flow so that the test water level reaches the standard upper limit, set the test pressure to 7MPa and the test time to 6h, and test the water flow and pressure changes on the water pressure test bench; 53. Obtain test results: Observe whether the cable leaks or breaks under water pressure and evaluate the pressure resistance of the cable. Embodiment 3

[0025] Please refer to Figure 1-2 As shown, this embodiment provides a low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships, and also includes the following steps: Step 1: Raw material pretreatment: clean the surface of the tinned copper wire, dry the surface of the copper wire for 6 minutes, and feed the copper wire into a wire drawing machine to draw the wire into a single wire; Step 2, twisting the wire and injecting glue once: inject glue when twisting the wire to make a wire core, set a wrapping layer 2 and an insulating layer 3 on the outside of the wire core, wrap the insulating material on the outside of the conductor 1, send it to the irradiation process, and make a wire harness; Step 3, secondary glue injection and cabling: After arranging the wire harness, use an insulating water-blocking tape to wrap the outside of the wire harness to form a second wrapping layer 5, inject glue between the second wrapping layer 5 and the wire harness, scrape off excess glue, and form a filling layer 4; Step 4, inner sheath, braiding and wrapping: feed 125℃ oil-resistant halogen-free low-smoke flame-retardant irradiated cable material into the extruder, extrude it after heating treatment by the extruder, adhere it to the outer surface of the wrapping layer 2 5, cool and solidify it for 4 hours to make the inner lining layer 6, use a braiding machine to weave tinned copper wire into an armor layer 7, combine the armor layer 7 with the inner lining layer 6, inject glue again, and wrap it on the outside of the armor layer 7 with a low-smoke halogen-free flame-retardant tape after drying to make a wrapping layer 3 8. When extruding the wrapping layer 3 8, the screw speed of the extruder is 20r / min and the extrusion temperature is 160℃; Step 5, sheath and testing: use an extruder to extrude the 125°C oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material, wrap the cable material around the outside of the wrapping layer 8, cool and solidify the cable to form an outer sheath 9, complete the overall processing of the cable, perform a drop test and a water pressure test on the finished cable, and test the sealing performance of the cable; When conducting a drip test, select a cable sample of a predetermined length, hang the sample on the test equipment, ignite the copper oxide heater, expose the lower end of the cable to the flame, the test temperature is 90°C, the test duration is 18 hours, observe whether the cable drips, record the shape of the dripping, collect and record the dripping, and evaluate the dripping performance of the cable based on the dripping condition of the cable; When conducting a water pressure test, the following contents are also included: 51. Pretreatment of test supplies: Place the cable in a dryer and dry for 3 minutes, take out the cable, cool it to room temperature, clamp the dried cable sample with a clamp, inject a predetermined volume of test water into the water tank, and weigh the mass of the test water; 52. Water flow and water pressure adjustment and testing: Use a water pump to increase the water flow so that the test water level reaches the standard upper limit, set the test pressure to 7MPa and the test time to 6h, and test the water flow and pressure changes on the water pressure test bench; 53. Obtain test results: Observe whether the cable leaks or breaks under water pressure and evaluate the pressure resistance of the cable. Embodiment 4

[0026] Please refer to Figure 1-2 As shown, this embodiment provides a low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships, and also includes the following steps: Step 1: Raw material pretreatment: clean the surface of the tinned copper wire, dry the surface of the copper wire for 6 minutes, and feed the copper wire into a wire drawing machine to draw the wire into a single wire; Step 2, twisting the wire and injecting glue once: inject glue when twisting the wire to make a wire core, set a wrapping layer 2 and an insulating layer 3 on the outside of the wire core, wrap the insulating material on the outside of the conductor 1, send it to the irradiation process, and make a wire harness; Step 3, secondary glue injection and cabling: After arranging the wire harness, use an insulating water-blocking tape to wrap the outside of the wire harness to form a second wrapping layer 5, inject glue between the second wrapping layer 5 and the wire harness, scrape off excess glue, and form a filling layer 4; Step 4, inner sheath, braiding and wrapping: feed 125℃ oil-resistant halogen-free low-smoke flame-retardant irradiated cable material into the extruder, extrude it after heating treatment by the extruder, adhere it to the outer surface of the wrapping layer 2 5, cool and solidify it for 4 hours to make the inner lining layer 6, use a braiding machine to weave tinned copper wire into an armor layer 7, combine the armor layer 7 with the inner lining layer 6, inject glue again, and wrap it on the outside of the armor layer 7 with a low-smoke halogen-free flame-retardant tape after drying to make a wrapping layer 3 8. When extruding the wrapping layer 3 8, the screw speed of the extruder is 22r / min, and the extrusion temperature is 150℃; Step 5, sheath and testing: use an extruder to extrude the 125°C oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material, wrap the cable material around the outside of the wrapping layer 8, cool and solidify the cable to form an outer sheath 9, complete the overall processing of the cable, perform a drop test and a water pressure test on the finished cable, and test the sealing performance of the cable; When conducting a drip test, select a cable sample of a predetermined length, hang the sample on the test equipment, ignite the copper oxide heater, expose the lower end of the cable to the flame, the test temperature is 90°C, the test duration is 18 hours, observe whether the cable drips, record the shape of the dripping, collect and record the dripping, and evaluate the dripping performance of the cable based on the dripping condition of the cable; When conducting a water pressure test, the following contents are also included: 51. Pretreatment of test supplies: Place the cable in a dryer and dry for 3 minutes, take out the cable, cool it to room temperature, clamp the dried cable sample with a clamp, inject a predetermined volume of test water into the water tank, and weigh the mass of the test water; 52. Water flow and water pressure adjustment and testing: Use a water pump to increase the water flow so that the test water level reaches the standard upper limit, set the test pressure to 7MPa and the test time to 6h, and test the water flow and pressure changes on the water pressure test bench; 53. Obtain test results: Observe whether the cable leaks or breaks under water pressure and evaluate the pressure resistance of the cable.

[0027] Comparative Example 1 Please refer to Figure 1-2As shown, this embodiment provides a low-smoke, halogen-free, low-toxicity, flame-retardant, longitudinal water-sealed power cable for ships, and its preparation method is roughly the same as that of embodiment 1, with the main difference being that in step 2, no glue injection treatment is performed when twisting the wires.

[0028] Comparative Example 2 Please refer to Figure 1-2 As shown, this embodiment provides a low-smoke, halogen-free, low-toxicity, flame-retardant, longitudinal water-sealed power cable for ships, and its preparation method is roughly the same as that of Example 1, with the main difference being that in step three, no sealing glue is used to fill between the insulating layer 3 and the second winding layer 5.

[0029] Comparative Example 3 Please refer to Figure 1-2 As shown, this embodiment provides a low-smoke, halogen-free, low-toxicity, flame-retardant, longitudinal water-sealed power cable for ships, and its preparation method is roughly the same as that of Example 1, with the main difference being that in step three, no wrapping layer 8 is provided between the armor layer 7 and the outer sheath 9.

[0030] Test Trial: The cables obtained by the treatment of Examples 2, 3 and 4 are recorded as Example Groups 1 to 3, and the cables obtained by the treatment of Comparative Examples 1 to 3 are recorded as Comparative Groups 1 to 3. According to GJB 774A-2020 and GJB 774A-2020 standards, the dripping of the cables of Example Groups 1 to 3 and Comparative Groups 1 to 3 and the displacement of the components of the test ends exposed to the water tank relative to the test sheath are tested, and the relevant test data are recorded in Table 1.

[0031] Table 1: Test data record table

[0032] As can be seen from Table 1, the cables obtained by processing Example Groups 1 to 3 did not produce dripping, and the displacement was ≤2.7mm, which is smaller than the standard 6.4mm. Therefore, the cables obtained by processing Example Groups 1 to 3 have good flame retardant properties, good longitudinal sealing properties, and strong water blocking ability.

[0033] By removing the glue injection during the twisting, the flame retardant performance of the cable is less affected, but the longitudinal sealing and water blocking ability of the cable are reduced. By removing the glue filled between the insulating layer 3 and the second sheath 5, the cable has no obvious dripping during the drip test, and the displacement of the end assembly of the cable in the water tank relative to the test sheath increases. At this time, the longitudinal sealing and water blocking ability of the cable are reduced. By removing the third sheath 8 between the armor layer 7 and the outer sheath 9, a small amount of dripping occurs during the drip test, the displacement distance is significantly increased, the longitudinal sealing performance is insufficient, and the water blocking ability is weak. In the present invention, by filling water-blocking halogen-free sealant between cable cores and arranging non-fiber materials, the tightness of the connection after the monofilament twisted wire is improved; a triple water-blocking structure consisting of twisted wire injection, filling layer 4 and winding layer 8 is adopted, that is, the twisted wire is filled with water-blocking halogen-free sealant, the core is filled with water-blocking halogen-free sealant, and the braided armor is wrapped with low-smoke halogen-free water-blocking tape. The triple structure can improve the longitudinal water-blocking performance inside the cable, thereby improving the longitudinal sealing effect of the cable; the winding layer 5 is arranged outside the filling layer 4, which can support the filling layer 4 and assist the connection between the filling layer 4 and the inner lining layer 6. The outer sheath 9 adopts low-smoke halogen-free and low-toxic flame-retardant cross-linked polyolefin to achieve Class A flame retardant level, has excellent flame retardant effect, can flame retardantly protect the outside of the cable, and reduce damage to the cable during use.

[0034] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0035] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.

Claims

1. A low-smoke, halogen-free, low-toxicity, flame-retardant, longitudinal water-sealed power cable for ships, comprising a conductor (1), characterized in that: The outer annular surface of the conductor (1) is compounded with a first winding layer (2), the outer annular surface of the first winding layer (2) is compounded with an insulating layer (3), the outer annular surface of the insulating layer (3) is provided with a second winding layer (5), a filling layer (4) is provided between the second winding layer (5) and the insulating layer (3), the outer annular surface of the second winding layer (5) is compounded with an inner lining layer (6), the outer annular surface of the inner lining layer (6) is provided with an armor layer (7), the outer annular surface of the armor layer (7) is compounded with a third winding layer (8), and the outer annular surface of the third winding layer (8) is compounded with an outer sheath (9).

2. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 1, characterized in that: The conductor (1) is made of tinned copper wire and rubber wire, and the armor layer (7) is made of braided tinned copper wire.

3. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 1, characterized in that: The first wrapping layer (2) and the second wrapping layer (5) are both made of insulating water-blocking tape.

4. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 1, characterized in that: The insulating layer (3) is made of 150°C high-strength oil-resistant halogen-free low-smoke irradiated insulating material, and the filling layer (4) is made of water-blocking halogen-free sealant.

5. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 1, characterized in that: The inner lining layer (6) and the outer sheath (9) are both made of 125°C oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material.

6. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 1, characterized in that: The wrapping layer three (8) is made of low-smoke halogen-free flame-retardant tape, and the low-smoke halogen-free flame-retardant tape contains low-smoke halogen-free low-toxic flame-retardant cross-linked polyolefin.

7. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 1, characterized in that: The following steps are also included: S1. Raw material pretreatment: clean the surface of the tinned copper wire, dry the surface of the copper wire for 5-10 minutes, and feed the copper wire into a wire drawing machine to draw the wire into a single wire; S2, twisting the wire and injecting glue once: injecting glue when twisting the wire to form a wire core, arranging a wrapping layer (2) and an insulating layer (3) outside the wire core, wrapping the insulating material around the outside of the conductor (1), and sending it to the irradiation process to form a wire bundle; S3, secondary glue injection and cabling: after arranging the wire harness, use an insulating water-blocking tape to wrap the outside of the wire harness to form a second wrapping layer (5), inject glue between the second wrapping layer (5) and the wire harness, scrape off excess glue, and form a filling layer (4); S4, inner sheath, braiding and wrapping: feed 125°C oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material into an extruder, heat-treat it in the extruder and extrude it, attach it to the outer surface of the second wrapping layer (5), cool and solidify it for 3-6 hours to form an inner lining layer (6), use a braiding machine to braid tinned copper wire into an armor layer (7), combine the armor layer (7) and the inner lining layer (6), inject glue again, and wrap it around the outside of the armor layer (7) with a low-smoke, halogen-free, flame-retardant tape after drying to form a wrapping layer (8); S5. Sheath and testing: Use an extruder to extrude the 125°C oil-resistant, halogen-free, low-smoke, flame-retardant irradiated cable material, wrap the cable material around the outside of the third sheath (8), cool and solidify the cable to form an outer sheath (9), complete the overall processing of the cable, and perform a drip test and a water pressure test on the finished cable to test the sealing performance of the cable.

8. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 7, characterized in that: In step S4, when the wrapping layer three (8) is extruded, the screw speed of the extruder is 20-22 r / min, and the extrusion temperature is 155-175°C.

9. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 7, characterized in that: In step S5, when performing the drip test, a cable sample of a predetermined length is selected, the sample is hung on the test equipment, the copper oxide heater is ignited, and the lower end of the cable is exposed to the flame. The test temperature is 90° C. and the test time is 18 hours. It is observed whether the cable drips, and the shape of the dripping is recorded. The dripping material is collected, recorded and analyzed, and the dripping performance of the cable is evaluated based on the dripping condition of the cable.

10. The low-smoke, halogen-free, low-toxicity, flame-retardant longitudinal water-sealed power cable for ships according to claim 8, characterized in that: In step S5, when performing the water pressure test, the following contents are also included: S51. Pretreatment of test supplies: put the cable into the dryer and dry it for 2-5 minutes, take out the cable, cool it to room temperature, clamp the dried cable sample with a clamp, inject a predetermined volume of test water into the water tank, and weigh the mass of the test water; S52, water flow, water pressure adjustment and testing: Use a water pump to increase the water flow, so that the test water level reaches the standard upper limit, set the test pressure to 7MPa, the test time to 6h, and test the water flow and pressure changes on the water pressure test bench; S53. Obtain test results: observe whether the cable leaks or breaks under water pressure, and evaluate the pressure resistance of the cable.

Citation Information

Patent Citations

  • Low-smoke zero-halogen flame retardant longitudinal watertight and airtight power cable

    CN203102996U