Lithium battery cell assembly device
By using a coating heating frame and a laser ranging sensor to detect the coating thickness in the lithium battery cell assembly device, and achieving a close fit between the pole piece and the separator through a synchronized cylinder and winding assembly, the uneven coating of the pole piece is solved. And the problem of insufficient contact improves battery performance and cell quality.
Patent Information
- Application Number
- CN202411023025.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-29
AI Technical Summary
During the assembly process of lithium battery cells, the uneven thickness of the pole piece coating causes battery capacity loss, and the contact between the pole pieces and the separator is not close during the winding process, affecting the quality and life of the cell.
A lithium battery cell assembly device is designed, including a coating heating frame, a laser ranging sensor, a coating component and a protective component. By detecting the thickness of the pole piece coating, the uniformity of the coating is ensured, and the coating is synchronized with the cylinder and winding group. The components achieve a tight fit between the pole piece and the diaphragm.
It achieves uniformity of the thickness of the pole piece coating, improves the charge and discharge performance of the battery, ensures good contact between the pole piece and the separator, and improves the manufacturing quality and performance of the battery core.
Smart Images

Figure CN118554029B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of lithium battery production, and in particular to a lithium battery core assembly device. Background Art
[0002] When using the battery cell, it involves assembly and winding. Winding is a key process in the manufacturing process of lithium-ion batteries, and it has a great impact on the yield rate. The positive and negative electrodes that have been separately manufactured are wound after adding a separator in the middle. The function of the separator is to completely separate the positive and negative electrodes to prevent the battery from short circuiting.
[0003] If the tension is not well controlled during the winding process, the electrode may bend or break, resulting in a large number of wrinkles on the battery electrode during repeated expansion and contraction during charging and discharging, limiting the capacity and possibly causing problems such as lithium deposition; the presence of metallic foreign matter on the diaphragm may cause micro-short circuits inside the battery, severe self-discharge, and safety hazards.
[0004] After searching, the invention patent with publication number CN113328131A discloses a pole core assembly mechanism for automated production of lithium batteries. During the overlapping process, the three parts are limited on the sides so that they can be overlapped and misalignment at the edges can be avoided, thereby eliminating the need for cutting and improving work efficiency.
[0005] In the above scheme, when the positive electrode sheets, separators and negative electrode sheets are wound, there is a problem of uneven coating on the positive electrode sheets and the negative electrode sheets, which leads to battery capacity loss; in addition, a winding needle is used to directly wind the battery cell sheets and separators in a certain order. During this process, the contact between the battery cell sheets and the separators is not tight enough, and the manufactured battery products are of low quality and short service life. Summary of the invention
[0006] The object of the present invention is to provide a lithium battery cell assembly device to solve the problem of battery capacity loss caused by uneven coating thickness on the cell pole piece mentioned in the above background technology.
[0007] The present invention can be implemented by the following technical scheme: a lithium battery cell assembly device, comprising a fixing frame 2 fixed on the top surface of a workbench, a fixing frame 1 is arranged on one side of the fixing frame 2, and two coating and heating frames are arranged on the other side surface of the fixing frame 2, one coating and heating frame acts on the positive electrode sheet, and the other coating and heating frame acts on the negative electrode sheet;
[0008] A winding assembly is slidably provided on one side of the fixed frame 1, and a positive electrode roller and a negative electrode roller for winding up the positive electrode sheet and the negative electrode sheet are rotatably installed inside the fixed frame 2, respectively. The interior of each coating and heating frame is divided into a heating chamber and a coating chamber by a partition, and a laser ranging sensor for detecting the coating thickness of the battery cell electrode sheet is installed at the entrance end of the coating and heating frame, and a coating assembly for double-sided coating of the battery cell electrode sheet is installed in the inner cavity of the coating chamber;
[0009] The coating assembly comprises two coating boxes which are close to or far from each other, and a coating roller which contacts with the electrode sheet of the battery cell is fitted on the liquid outlet end of each coating box, and a plurality of nozzles for spraying high-temperature airflow are arranged on the inner wall surfaces on both sides of the heating chamber, and a high-temperature resistant steel wire mesh is arranged inside the heating chamber and adjacent to the air outlet end of the nozzle;
[0010] A connecting seat is fixedly connected to one side of the top of the coating box, and the connecting seat is rotatably arranged with the coating roller. A liquid inlet is provided on the top surface of the coating box, and a storage cavity communicated with the connecting seat is provided inside the coating box. A push plate is movably provided on the inner wall surface of the storage cavity. An adjusting cylinder for pushing the push plate to move is installed on the surface of the side of the coating box away from the coating roller, and a fitting portion for cooperating with the coating roller is provided at the liquid outlet end of the coating box.
[0011] A further technical improvement of the present invention is that the coating assembly also includes a bidirectional screw arranged at the top of the inner cavity of the coating chamber and driven by a forward and reverse motor, and adjustment blocks are sleeved on the two threaded outer surfaces of the bidirectional screw, one end of the adjustment block is fixed to the corresponding coating box, and a fixed block is provided on the side of the top surface of the coating box away from the adjustment block, a sliding rod is slidably installed in the fixed block, and the two ends of the sliding rod are fixed to the inner wall surface of the coating chamber.
[0012] A further technical improvement of the present invention is that a diaphragm roller is rotatably arranged in the middle of the inner cavity of the fixed frame 2, and an electric push rod is installed on the top surface of the fixed frame 2 away from the fixed frame 1, the pushing end of the electric push rod is connected to a U-shaped frame, and pressure rollers are installed on both end surfaces of the U-shaped frame, and each of the pressure rollers is in contact with the positive electrode sheet and the negative electrode sheet respectively.
[0013] A further technical improvement of the present invention is that a fixing frame three is arranged on the side of the fixing frame two away from the fixing frame one, and a roller rod one and a roller rod two are rotatably installed in the fixing frame three, and the outer surfaces of the roller rod one and the roller rod two are respectively wound with a positive electrode sheet and a negative electrode sheet coated with a coating.
[0014] A further technical improvement of the present invention is that: a mounting frame is arranged between the fixed frame 1 and the fixed frame 2, a protective component for the diaphragm to pass through is arranged below the mounting frame, the protective component includes two movable side plates installed below the mounting frame, the ends of the two movable side plates are snap-fitted and connected, an abutment roller is rotatably installed inside each of the movable side plates, two synchronous cylinders 1 are installed on the bottom surface of the mounting frame, and the pushing end of each of the synchronous cylinders 1 is fixedly connected to a sliding block that slides on the bottom surface of the mounting frame, and the end of the sliding block is fixedly connected to the upper surface of the movable side plate.
[0015] A further technical improvement of the present invention is that two mounting rods are arranged inside the fixed frame one, and a bonding roller is rotatably installed inside each of the mounting rods. A synchronous cylinder two is arranged on the outer wall surface of the fixed frame one for pushing the corresponding mounting rod to move, and the bonding roller is used to tightly press the contact surfaces of the positive electrode sheet, the diaphragm and the negative electrode sheet.
[0016] A further technical improvement of the present invention is that the winding assembly includes a hollow frame with a built-in driving motor, a winding needle driven by the driving motor is installed on the upper surface of the hollow frame, a blocking plate is provided on the outside of the winding needle, and the winding needle winds up the positive electrode sheet, the diaphragm and the negative electrode sheet in order, the upper surface of the workbench is provided with a slide groove for directional sliding of the hollow frame, and a linear cylinder for pushing the hollow frame to slide is provided on the side of the fixed frame.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] 1. By setting up two coating heating frames, the two sides of the positive electrode sheet and the negative electrode sheet are detected by the laser distance measuring sensors in different coating heating frames for coating thickness. When the coating thickness is inconsistent, the coating component starts to work and drives the two coating boxes to approach each other. At this time, the coating rollers in the two coating heating frames contact the corresponding battery cell sheets (i.e., the positive electrode sheet and the negative electrode sheet), and the coating material on the coating rollers is rotated and transferred to the battery cell sheets, and the positive electrode sheet and the negative electrode sheet are evenly coated to keep the thickness consistent. After being evenly coated, the positive electrode sheet and the negative electrode sheet enter the heating chamber and are dried for the set time. The side high-temperature jet method is used to blow air and heat the two sides of the battery cell pole piece, so that the heating chamber is filled with high-temperature airflow, the surface coating of the battery cell pole piece is cured, and the uniformity of the coating is improved. In order to prevent the influence of airflow on the curing of the battery cell pole piece coating, a steel wire mesh is added. Since the hole spacing of the steel wire mesh is small, the corresponding high-temperature airflow is reduced accordingly, so that the exhaust volume becomes smaller, the flow rate of the airflow is reduced, and the direct blowing contact between the airflow and the battery cell pole piece coating is avoided. After drying, the positive and negative pole pieces are correspondingly rolled up at a uniform speed by the positive roller and the negative roller to ensure that the coating thickness of the positive and negative pole pieces is uniform, thereby improving the charge and discharge performance of the battery;
[0019] 2. The positive electrode sheet, the separator and the negative electrode sheet are placed in order and aligned, wherein the separator is located between the positive electrode sheet and the negative electrode sheet. When laminating, the positive electrode sheet and the negative electrode sheet are limited by the upper and lower ends of the two laminating rollers, and then the corresponding mounting rods are driven to move closer to the center by the push of the synchronous cylinder 2, so that the positive electrode sheet, the separator and the negative electrode sheet are closely fitted, ensuring good contact between the positive and negative electrode sheets and the separator, improving the manufacturing quality and performance of the battery cell, and avoiding the problem of insufficient lamination;
[0020] 3. By setting up the protection component, the synchronous cylinder pushes the sliding block to slide on the bottom surface of the mounting frame, so that the two movable side plates are opened. At this time, the diaphragm enters between the two opened movable side plates. The synchronous cylinder is reset. At this time, the abutting rollers in the two movable side plates are in contact with the diaphragm. The diaphragm is limited to pass through the two movable side plates, avoiding the problem of internal micro-short circuit of the battery caused by foil debris and diaphragm rupture caused by dust, thereby improving the quality of the battery cell;
[0021] 4. By setting up a winding assembly, the linear cylinder pushes the hollow frame to slide in a directional manner on the workbench, which increases the winding tension during sliding. Then, the winding needle tightly winds the bonded positive electrode sheet, diaphragm and negative electrode sheet, thereby improving the compactness of the battery cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] In order to facilitate understanding by those skilled in the art, the present invention is further described below with reference to the accompanying drawings.
[0023] Figure 1 A top view of the present invention;
[0024] Figure 2 It is a three-dimensional structural schematic diagram of the U-shaped frame and the second fixing frame of the present invention;
[0025] Figure 3 This is a schematic diagram of the internal structure of the coating heating frame of the present invention;
[0026] Figure 4 It is a schematic diagram of the installation structure of the hollow frame and the workbench of the present invention;
[0027] Figure 5 It is a schematic diagram of the three-dimensional installation structure of the coating roller of the present invention;
[0028] Figure 6 It is a schematic diagram of the installation structure of the movable side panel of the present invention;
[0029] Figure 7 It is a three-dimensional structural schematic diagram of the movable side panel of the present invention;
[0030] Figure 8 It is a schematic diagram of the internal structure of the fixing frame 1 of the present invention.
[0031] In the figure: 1, workbench; 2, hollow frame; 3, fixed frame 1; 4, linear cylinder; 5, laminating roller; 6, mounting frame; 7, fixed frame 2; 8, positive roller; 9, coating and heating frame; 10, diaphragm roller; 11, negative roller; 12, electric push rod; 13, U-shaped frame; 14, pressure roller; 15, slide; 16, winding needle; 17, blocking sheet; 18, heating chamber; 19, coating chamber; 20, laser measuring Distance sensor; 21. Nozzle; 22. Wire mesh; 23. Coating box; 24. Adjusting cylinder; 25. Push plate; 26. Storage chamber; 27. Laminating part; 28. Coating roller; 29. Adjusting block; 30. Bidirectional screw; 31. Connecting seat; 32. Liquid inlet; 33. Movable side plate; 34. Synchronous cylinder one; 35. Sliding block; 36. Abutting roller; 37. Synchronous cylinder two; 38. Mounting rod. DETAILED DESCRIPTION
[0032] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in conjunction with the accompanying drawings and preferred embodiments.
[0033] See also Figure 1-Figure 8As shown, the present invention provides a lithium battery cell assembly device, including a workbench 1, a fixed frame 27 is fixed on the top surface of the workbench 1, a fixed frame 13 is arranged on one side of the fixed frame 27, and two coating heating frames 9 are arranged on the other side surface of the fixed frame 27, one coating heating frame 9 acts on the positive electrode sheet, and the other coating heating frame 9 acts on the negative electrode sheet, a winding assembly is slidably arranged on one side of the fixed frame 13, a positive electrode roller 8 and a negative electrode roller 11 for winding the positive electrode sheet and the negative electrode sheet are rotatably installed inside the fixed frame 27, the interior of each coating heating frame 9 is divided into a heating chamber 18 and a coating chamber 19 by a partition, and a coating heating chamber 19 for detecting the coating of the cell electrode sheet is installed at the entrance end of the coating heating frame 9. A laser ranging sensor 20 for measuring the layer thickness is provided. The inner cavity of the coating chamber 19 is provided with a coating component for double-sided coating of the battery cell pole piece. The coating component includes two coating boxes 23 which are close to or far away from each other. The liquid outlet end of each coating box 23 is fitted with a coating roller 28 which is in contact with the battery cell pole piece. The inner wall surfaces on both sides of the heating chamber 18 are provided with a plurality of nozzles 21 for ejecting high-temperature airflow. A high-temperature resistant steel wire mesh 22 is provided inside the heating chamber 18 and adjacent to the air outlet end of the nozzle 21. The battery cell pole piece includes a positive pole piece and a negative pole piece. The positive pole piece and the negative pole piece have been coated before entering the two coating heating frames 9, and respectively enter the two different coating heating frames 9. In the coating heating frame 9 , the laser distance measuring sensor 20 in different coating heating frames 9 detects the coating thickness of the positive electrode sheet and the negative electrode sheet. When the coating thickness of the positive electrode sheet and the negative electrode sheet is inconsistent, the coating assembly starts to work and drives the two coating boxes 23 to approach each other. At this time, the coating rollers 28 in the two coating heating frames 9 are in contact with the corresponding battery cell sheets (i.e., the positive electrode sheet and the negative electrode sheet), and the coating material on the coating rollers 28 is rotated and transferred to the battery cell sheets, and the positive electrode sheets and the negative electrode sheets are evenly coated to keep the thickness consistent. After being evenly coated, the positive electrode sheets and the negative electrode sheets enter the heating chamber 18 and are dried to the set time. The two sides of the battery cell sheets are heated by blowing air from high-temperature jets on both sides. The heating chamber 18 is filled with high-temperature airflow to solidify the coating on the surface of the battery cell pole piece and improve the uniformity of the coating. In order to prevent the influence of the airflow on the solidification of the coating on the battery cell pole piece, a steel wire mesh 22 is added. Since the hole spacing of the steel wire mesh 22 is small, the corresponding high-temperature airflow is reduced accordingly, so that the exhaust volume becomes smaller, and the flow rate of the airflow is reduced to avoid direct blowing contact between the airflow and the coating on the battery cell pole piece. After drying, the positive electrode roller 8 and the negative electrode roller 11 are correspondingly rolled up at a uniform speed on the positive electrode piece and the negative electrode piece to ensure that the coating thickness of the positive electrode piece and the negative electrode piece is uniform, thereby improving the charge and discharge performance of the battery and avoiding the deviation between the actual capacity of the battery and the theoretical design value due to uneven coating and the problem of lithium precipitation caused by capacity mismatch.
[0034] See also Figure 3 and Figure 5As shown, a connecting seat 31 is fixedly connected to one side of the top of the coating box 23, and the connecting seat 31 is rotatably arranged with the coating roller 28. A liquid inlet 32 is arranged on the top surface of the coating box 23, and the coating liquid of the positive electrode sheet and the negative electrode sheet are injected into the coating box 23 in the two coating heating frames 9 to ensure that the coating of the battery cell electrode sheets is uniform. A storage chamber 26 communicating with the connecting seat 31 is arranged inside the coating box 23, and a push plate 25 is movably arranged on the inner wall surface of the storage chamber 26. An adjusting cylinder 24 for pushing the push plate 25 to move is installed on the surface of the side of the coating box 23 away from the coating roller 28, and a fitting portion 27 used in conjunction with the coating roller 28 is arranged at the liquid outlet end of the coating box 23. When a positive electrode sheet is detected, the coating box 23 is opened. When there is a difference in thickness between the coatings of the positive electrode sheet and the negative electrode sheet, the two coating boxes 23 drive the corresponding coating rollers 28 to contact the fitting surface of the positive electrode sheet or the negative electrode sheet, and push the push plate 25 in the storage chamber 26 by adjusting the cylinder 24 to squeeze the coating liquid. The coating liquid is discharged from the liquid outlet and contacts the rotation of the coating roller 28 through the fitting part 27 to ensure that the coating liquid does not leak out, and the coating liquid is adsorbed and transferred to the coating roller 28. Since the coating roller 28 can rotate autonomously, when the battery cell electrode sheet rolls through between the two coating rollers 28, the coating surface of the battery cell electrode sheet is brushed to the set thickness to ensure the consistency of the thickness of the positive electrode sheet and the negative electrode sheet battery, thereby improving the quality of the battery cell.
[0035] See also Figure 5 As shown, the coating assembly also includes a bidirectional screw 30 which is arranged at the top of the inner cavity of the coating chamber 19 and driven by a forward and reverse motor. Adjustment blocks 29 are sleeved on the outer surfaces of the two threads of the bidirectional screw 30. One end of the adjustment block 29 is fixed to the corresponding coating box 23. A fixed block is provided on the side of the top surface of the coating box 23 away from the adjustment block 29. A sliding rod is slidably installed in the fixed block. The two ends of the sliding rod are fixed to the inner wall surface of the coating chamber 19. When the bidirectional screw 30 rotates, due to the connection between the forward and reverse threads of the adjustment block 29 and the bidirectional screw 30, the two coating boxes 23 are brought close to each other, and the fixed block is driven to slide on the sliding rod to ensure the stable sliding of the two coating boxes 23.
[0036] See also Figure 1 and Figure 2As shown, a diaphragm roller 10 is rotatably arranged in the middle of the inner cavity of the fixed frame 2 7, and an electric push rod 12 is installed on the top surface of the fixed frame 2 7 away from the fixed frame 1 3. The pushing end of the electric push rod 12 is connected to a U-shaped frame 13, and pressure rollers 14 are installed on the two end faces of the U-shaped frame 13. Each pressure roller 14 is in contact with the positive electrode sheet and the negative electrode sheet respectively. Initially, one pressure roller 14 is in contact with the positive electrode sheet, and the other pressure roller 14 is in contact with the negative electrode sheet. When the positive electrode sheet and the negative electrode sheet enter the coating and heating frame 9, the electric push rod 12 pushes the U-shaped frame 13 to move toward the side away from the fixed frame 3. In this process, the two pressure rollers 14 squeeze the positive electrode sheet and the negative electrode sheet respectively, so that the battery cell electrode sheets are in a tensioned state, thereby avoiding the problem of wrinkles limiting the capacity during coating.
[0037] See also Figure 1 As shown, a fixing frame three is provided on the side of the fixing frame two 7 away from the fixing frame one 3, and a roller rod one and a roller rod two are rotatably installed in the fixing frame three, and the outer surfaces of the roller rod one and the roller rod two are respectively wound with the positive electrode sheet and the negative electrode sheet coated with a coating, and the roller rod one and the roller rod two serve as raw material rollers for the positive electrode sheet and the negative electrode sheet.
[0038] See also Figure 1 , Figure 6 and Figure 7 As shown, a mounting frame 6 is provided between the fixed frame 1 3 and the fixed frame 2 7, and a protective assembly for the diaphragm to pass through is provided below the mounting frame 6. The protective assembly includes two movable side plates 33 installed below the mounting frame 6, and the ends of the two movable side plates 33 are snap-fitted and connected. An abutment roller 36 is rotatably installed inside each movable side plate 33. Two synchronous cylinders 1 34 are installed on the bottom surface of the mounting frame 6, and the pushing end of each synchronous cylinder 1 34 is fixedly connected to a sliding block 35 sliding on the bottom surface of the mounting frame 6, and the end of the sliding block 35 is fixedly connected to the bottom surface of the mounting frame 6. The upper surface of the movable side plate 33 is fixedly connected to the upper surface of the movable side plate 33. Initially, the synchronous cylinder 34 pushes the sliding block 35 to slide on the bottom surface of the mounting frame 6, so that the two movable side plates 33 are opened. At this time, the diaphragm enters between the two opened movable side plates 33, and the synchronous cylinder 34 is reset. At this time, the abutting rollers 36 in the two movable side plates 33 are in contact with the diaphragm, and the diaphragm is limited to pass through the two movable side plates 33, avoiding the problem of foil debris causing micro-short circuit inside the battery and dust causing diaphragm rupture, thereby improving the quality of the battery cell.
[0039] See also Figure 1 and Figure 8As shown, two mounting rods 38 are arranged inside the fixed frame 3, and a bonding roller 5 is rotatably installed inside each mounting rod 38. A synchronous cylinder 2 37 is arranged on the outer wall of the fixed frame 3 to push the corresponding mounting rod 38 to move. The bonding roller 5 is used to tightly press the contact surfaces of the positive electrode sheet, the diaphragm and the negative electrode sheet. Before winding the battery cell, the positive electrode sheet, the diaphragm and the negative electrode sheet are placed in sequence and aligned, wherein the diaphragm is located between the positive electrode sheet and the negative electrode sheet. When bonding, the positive electrode sheet and the negative electrode sheet are limited by the upper and lower ends of the two bonding rollers 5, and then the corresponding mounting rod 38 is driven to move toward the center by the push of the synchronous cylinder 2 37, so that the positive electrode sheet, the diaphragm and the negative electrode sheet are tightly fitted, ensuring good contact between the positive and negative electrode sheets and the diaphragm, and reducing the risk of internal defects and short circuits of the battery cell.
[0040] See also Figure 1 and Figure 4 As shown, the winding assembly includes a hollow frame 2 with a built-in driving motor, and a winding needle 16 driven by the driving motor is installed on the upper surface of the hollow frame 2. A blocking plate 17 is arranged on the outside of the winding needle 16, and the winding needle 16 winds up the positive electrode sheet, the diaphragm and the negative electrode sheet in order. The upper surface of the workbench 1 is provided with a slide groove 15 for directional sliding of the hollow frame 2, and the side of the fixed frame 3 is provided with a linear cylinder 4 for pushing the hollow frame 2 to slide. After the positive and negative electrode sheets and the diaphragm are tightly fitted, winding is carried out. During winding, the linear cylinder 4 pushes the hollow frame 2 to slide in a directional manner on the workbench 1, and the winding tension is increased during sliding. Then, the winding needle 16 tightly winds the fitted positive electrode sheet, diaphragm and negative electrode sheet, thereby improving the compactness of the battery cell.
[0041] When the present invention is in use, two coating and heating frames 9 are set up, and the two sides of the positive electrode sheet and the negative electrode sheet are detected by the laser distance measuring sensors 20 in different coating and heating frames 9 for coating thickness detection. When the coating thickness is inconsistent, the coating assembly starts to work at this time, driving the two coating boxes 23 to approach each other. At this time, the coating rollers 28 in the two coating and heating frames 9 are in contact with the corresponding battery cell sheets (i.e., the positive electrode sheet and the negative electrode sheet), and the coating material on the coating rollers 28 is rotated and transferred to the battery cell sheets, and the positive electrode sheet and the negative electrode sheet are evenly coated to keep the thickness consistent. The evenly coated positive electrode sheet and the negative electrode sheet enter the heating chamber 18 and are dried for a set time. , using the method of high-temperature jet from both sides to blow air and heat the two sides of the battery cell pole piece, so that the heating chamber 18 is filled with high-temperature airflow, the surface coating of the battery cell pole piece is cured, and the uniformity of the coating is improved. In order to prevent the influence of airflow on the curing of the battery cell pole piece coating, a steel wire mesh 22 is added. Since the hole spacing of the steel wire mesh 22 is small, the corresponding high-temperature airflow is reduced accordingly, so that the exhaust volume becomes smaller, the flow rate of the airflow is reduced, and the direct blowing contact between the airflow and the battery cell pole piece coating is avoided. After drying, the positive electrode roller 8 and the negative electrode roller 11 are correspondingly rolled up at a uniform speed to ensure that the coating thickness of the positive electrode sheet and the negative electrode sheet is uniform, thereby improving the charge and discharge performance of the battery;
[0042] The positive electrode sheet, the separator and the negative electrode sheet are placed in order and aligned, wherein the separator is located between the positive electrode sheet and the negative electrode sheet. When laminating, the positive electrode sheet and the negative electrode sheet are limited by the upper and lower ends of the two laminating rollers 5, and then the corresponding mounting rods 38 are driven to approach the center by the push of the synchronous cylinder 2 37, so that the positive electrode sheet, the separator and the negative electrode sheet are closely fitted, ensuring good contact between the positive and negative electrode sheets and the separator, improving the manufacturing quality and performance of the battery cell, and avoiding the problem of insufficient lamination;
[0043] By setting the protection component, the synchronous cylinder 1 34 pushes the sliding block 35 to slide on the bottom surface of the mounting frame 6, so that the two movable side plates 33 are opened. At this time, the diaphragm enters between the two opened movable side plates 33, and the synchronous cylinder 1 34 is reset. At this time, the abutting rollers 36 in the two movable side plates 33 are in contact with the diaphragm, and the diaphragm is limited to pass through the two movable side plates 33, thereby avoiding the problem of foil debris causing micro short circuit inside the battery and dust causing diaphragm rupture, thereby improving the quality of the battery cell;
[0044] By setting up a winding assembly, the linear cylinder 4 pushes the hollow frame 2 to slide in a directional manner on the workbench 1, increasing the winding tension during sliding, and then the winding needle 16 tightly winds the bonded positive electrode sheet, diaphragm and negative electrode sheet, thereby improving the compactness of the battery cell.
[0045] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still fall within the scope of the technical solution of the present invention.
Claims
1. A lithium battery cell assembly device, comprising a fixing frame 2 (7) fixed on the top surface of a workbench (1), characterized in that: A fixing frame 1 (3) is arranged on one side of the fixing frame 2 (7), and two coating and heating frames (9) are arranged on the other side surface of the fixing frame 2 (7), one coating and heating frame (9) acts on the positive electrode sheet, and the other coating and heating frame (9) acts on the negative electrode sheet; A winding assembly is slidably arranged on one side of the fixing frame 1 (3), a positive electrode roller (8) and a negative electrode roller (11) for winding up the positive electrode sheet and the negative electrode sheet are rotatably arranged inside the fixing frame 2 (7), the interior of each coating and heating frame (9) is divided into a heating chamber (18) and a coating chamber (19) via a partition, and a laser distance measuring sensor (20) for detecting the coating thickness of the battery cell sheet is installed at the entrance end of the coating and heating frame (9), and a coating assembly for double-sided coating of the battery cell sheet is installed in the inner cavity of the coating chamber (19); The coating assembly comprises two coating boxes (23) that are close to or far from each other, a coating roller (28) that contacts the battery cell pole piece is fitted on the liquid outlet end of each coating box (23), a plurality of nozzles (21) that eject high-temperature airflow are arranged on the inner wall surfaces on both sides of the heating chamber (18), and a high-temperature resistant steel wire mesh (22) is arranged inside the heating chamber (18) and adjacent to the air outlet end of the nozzle (21); A connecting seat (31) is fixedly connected to one side of the top of the coating box (23), and the connecting seat (31) is rotatably arranged with the coating roller (28). A liquid inlet (32) is arranged on the top surface of the coating box (23), and a storage chamber (26) communicating with the connecting seat (31) is arranged inside the coating box (23). A push plate (25) is movably arranged on the inner wall surface of the storage chamber (26). An adjusting cylinder (24) for pushing the push plate (25) to move is installed on the surface of the side of the coating box (23) away from the coating roller (28), and a fitting portion (27) for use with the coating roller (28) is arranged at the liquid outlet end of the coating box (23); Before entering the two coating and heating frames (9), the positive electrode sheet and the negative electrode sheet have been coated and respectively enter two different coating and heating frames (9). In the coating and heating frames (9), the coating thickness of the positive electrode sheet and the negative electrode sheet is detected by the laser distance measuring sensors (20) in the different coating and heating frames (9). When the coating thickness of the positive electrode sheet and the negative electrode sheet is inconsistent, the coating assembly starts to work and drives the two coating boxes (23) to approach each other. At this time, the coating rollers (28) in the two coating and heating frames (9) contact the corresponding positive electrode sheet and the negative electrode sheet, and rotate the coating material on the coating rollers (28) to transfer to the battery cell sheet, so that the positive electrode sheet and the negative electrode sheet are evenly coated to maintain a consistent thickness.
2. A lithium battery cell assembly device according to claim 1, characterized in that: The coating assembly also includes a bidirectional screw (30) disposed at the top of the inner cavity of the coating chamber (19) and driven by a forward and reverse motor, and an adjustment block (29) is sleeved on the two threaded outer surfaces of the bidirectional screw (30), and one end of the adjustment block (29) is fixed to the corresponding coating box (23), and a fixing block is provided on the side of the top surface of the coating box (23) away from the adjustment block (29), and a sliding rod is slidably installed in the fixing block, and the two ends of the sliding rod are fixed to the inner wall surface of the coating chamber (19).
3. A lithium battery cell assembly device according to claim 1, characterized in that: A diaphragm roller (10) is rotatably arranged in the middle of the inner cavity of the second fixed frame (7), and an electric push rod (12) is installed on the top surface of the second fixed frame (7) away from the first fixed frame (3), and the pushing end of the electric push rod (12) is connected to a U-shaped frame (13), and pressure rollers (14) are installed on both end surfaces of the U-shaped frame (13), and each of the pressure rollers (14) is in contact with the positive electrode sheet and the negative electrode sheet respectively.
4. A lithium battery cell assembly device according to claim 1, characterized in that: A fixing frame 3 is arranged on one side of the fixing frame 2 (7) away from the fixing frame 1 (3), and a roller rod 1 and a roller rod 2 are rotatably mounted inside the fixing frame 3, and the outer surfaces of the roller rod 1 and the roller rod 2 are respectively wound with a positive electrode sheet and a negative electrode sheet coated with a coating.
5. A lithium battery cell assembly device according to claim 1, characterized in that: A mounting frame (6) is provided between the fixed frame 1 (3) and the fixed frame 2 (7), and a protective component for the diaphragm to pass through is provided below the mounting frame (6), and the protective component comprises two movable side plates (33) installed below the mounting frame (6), the ends of the two movable side plates (33) are snap-fitted and connected, and an abutment roller (36) is rotatably installed inside each of the movable side plates (33), and two synchronous cylinders 1 (34) are installed on the bottom surface of the mounting frame (6), and the pushing end of each of the synchronous cylinders 1 (34) is fixedly connected to a sliding block (35) that slides on the bottom surface of the mounting frame (6), and the end of the sliding block (35) is fixedly connected to the upper surface of the movable side plate (33).
6. A lithium battery cell assembly device according to claim 1, characterized in that: Two mounting rods (38) are arranged inside the fixing frame (3), and a bonding roller (5) is rotatably mounted inside each of the mounting rods (38). A synchronous cylinder (37) for pushing the corresponding mounting rod (38) to move is arranged on the outer wall surface of the fixing frame (3), and the bonding roller (5) is used to tightly press the contact surfaces of the positive electrode sheet, the diaphragm and the negative electrode sheet.
7. A lithium battery cell assembly device according to claim 1, characterized in that: The winding assembly comprises a hollow frame (2) with a built-in driving motor, a winding needle (16) driven by the driving motor is installed on the upper surface of the hollow frame (2), a blocking plate (17) is arranged outside the winding needle (16), and the winding needle (16) winds up the positive electrode sheet, the diaphragm and the negative electrode sheet in sequence, the upper surface of the workbench (1) is provided with a slide groove (15) for directional sliding of the hollow frame (2), and a linear cylinder (4) for pushing the hollow frame (2) to slide is arranged on the side of the fixed frame (3).