Preparation method of thin-film solar module

By adding the status inspection and rework steps of P2 wire ducts in the preparation process of thin-film solar modules, the unqualified P2 wire ducts are reworked, which solves the problem of resource waste and cost increase caused by unqualified laser marking, and realizes resource optimization. savings and improvement in preparation efficiency.

CN118737864APending Publication Date: 2024-10-01QUZHOU MICROQUANTA RENEWABLE ENERGY TECHN CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310356571.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the preparation process of thin-film solar modules, unqualified P2 laser scribing results in uneven film layers or machine abnormalities, causing large-area short circuits or open circuits, wasting resources and increasing costs.

Method used

In the preparation method of thin film solar modules, the status inspection and reworking steps of P2 wire ducts are added. By adjusting the processing parameters, the unqualified P2 wire ducts are reworked and marked to ensure that their quality is qualified before proceeding to the next step to achieve P2 laser Utilization of marked-out defective products.

Benefits of technology

Effectively save resources, reduce costs, simplify the rework process of P2 wire ducts, improve preparation efficiency, and ensure product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737864A_ABST
    Figure CN118737864A_ABST
Patent Text Reader

Abstract

The invention relates to a preparation method of a thin-film solar module, which comprises the following steps of: after P2 lineation processing, checking a P2 trunking, and if an unqualified P2 trunking is not found, directly preparing a back electrode layer and P3 lineation processing; if an unqualified P2 wire slot is found, a P2 reworking lineation step is carried out in sequence, and then back electrode layer preparation and P3 lineation processing are carried out; the P2 reworking lineation step comprises the steps that machining parameters are adjusted, corresponding P2 reworking lineation is conducted on the side portion close to each unqualified P2 wire groove, and a front electrode layer is exposed out of the bottom of each P2 reworking wire groove. The reworking method of the P2 wire duct is simple, positioning is convenient and fast, unqualified P2 laser scribing products are reworked and then reused, resources are saved, and cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of solar module preparation, and in particular relates to a method for preparing a thin-film solar module. Background Art

[0002] In the existing thin-film solar module manufacturing process, during the P2 laser scribing process after the conductive film layer, the laser scribing effect is often poor or the scribing position is abnormal due to the unevenness of the film layer or the internal influence of the machine, causing a large area of ​​short circuit or open circuit in the thin-film solar module. If the P2 laser scribing unqualified products are directly discarded or reworked, it will not only waste resources but also increase costs. Summary of the invention

[0003] The technical problem to be solved by the present invention is to provide a method for preparing a thin-film solar module, which can rework and reuse P2 laser-scribed defective products, thereby saving resources and reducing costs.

[0004] The present invention is implemented by providing a method for preparing a thin-film solar module, comprising the following steps: Step 1: prepare a front electrode layer on a clean substrate, perform multiple P1 scribing on the front electrode layer, each P1 line groove of the P1 scribing cuts through the front electrode layer, and the bottom of each P1 line groove exposes the substrate; Step 2: prepare a light absorbing layer on the surface of the front electrode layer and on the surface of each P1 line groove, perform multiple P2 scribing on the light absorbing layer, the P2 line groove of each P2 scribing line is close to the position of its corresponding P1 line groove, each P2 line groove cuts through the light absorbing layer, and the bottom of each P2 line groove exposes the front electrode layer; Step 3, prepare a back electrode layer on the surface of the light absorbing layer and the surface of each P2 line groove, so that the back electrode layer on the surface of the light absorbing layer and the back electrode layer in each P2 line groove are conductively connected to each other, and then perform multiple P3 scribing on the back electrode layer, the P3 line groove of each P3 scribing line is close to the position of its corresponding P2 line groove, each P3 line groove cuts through the back electrode layer, and the bottom of each P3 line groove exposes the light absorbing layer; The method for preparing the thin-film solar module further includes a P2 wire groove status inspection and rework step between step 2 and step 3, which step includes: performing a quality inspection on each P2 wire groove after processing, and if no unqualified P2 wire groove is found, directly proceeding to step 3; if an unqualified P2 wire groove is found, then sequentially performing the P2 rework and scribing step and step III: The P2 rework scribing step includes: adjusting processing parameters, performing corresponding P2 rework scribing on the side of each unqualified P2 line groove, wherein the P2 rework line groove of each P2 rework scribing cuts off the light absorption layer, and the bottom of each P2 rework line groove exposes the front electrode layer; Step III, preparing a back electrode layer on the surface of the light absorbing layer, each P2 line groove and each P2 rework line groove, so that the back electrode layer on the surface of the light absorbing layer and the back electrode layer in each P2 rework line groove are conductively connected to each other, and performing multiple P3 scribing on the back electrode layer, each P3 scribing P3 line groove is close to the position of its corresponding P2 rework line groove, each P3 line groove cuts through the back electrode layer, and the bottom of each P3 line groove exposes the light absorbing layer; The unqualified P2 wire slots include any one of the defects of discontinuity, uneven thickness, and overcutting the substrate surface.

[0005] The present invention is implemented in this way, and also provides a method for preparing a thin-film solar module, comprising the following steps: Step 1, preparing a front electrode layer on a clean substrate, performing a plurality of P1 scribing lines on the front electrode layer, wherein a P1 line groove of each P1 scribing line cuts through the front electrode layer, and the bottom of each P1 line groove exposes the substrate; Step 2, sequentially preparing a first carrier layer, a light absorbing layer, and a second carrier layer on the surface of the front electrode layer and the surface of each P1 line groove, performing multiple P2 scribing on the second carrier layer, wherein the P2 line groove of each P2 scribing line is close to the position of its corresponding P1 line groove, each P2 line groove cuts through the second carrier layer, the light absorbing layer, and the first carrier layer, and the bottom of each P2 line groove exposes the front electrode layer; Step 3, preparing a back electrode layer on the surface of the second carrier layer and on the surface of each P2 line groove, so that the back electrode layer on the surface of the second carrier layer and the back electrode layer in each P2 line groove are conductively connected to each other, and then performing multiple P3 scribing on the back electrode layer, the P3 line groove of each P3 scribing is close to the position of its corresponding P2 line groove, each P3 line groove cuts through the back electrode layer, the second carrier layer, the light absorption layer and the first carrier layer, and the front electrode layer is exposed at the bottom of each P3 line groove; The method for preparing the thin-film solar module further includes a P2 wire groove status inspection and rework step between step 2 and step 3, which step includes: inspecting each P2 wire groove after processing, and if no unqualified P2 wire groove is found, directly proceeding to step 3; if an unqualified P2 wire groove is found, sequentially performing the P2 rework scribing step and step 3′: The P2 rework scribing step includes: adjusting processing parameters, performing corresponding P2 rework scribing on the side of each unqualified P2 line groove, wherein the P2 rework line groove of each P2 rework scribing cuts off the second carrier layer, the light absorption layer and the first carrier layer, and the bottom of each P2 rework line groove exposes the front electrode layer; Step 3′, preparing a back electrode layer on the surface of the second carrier layer, the surface of each P2 line groove and the surface of each P2 rework line groove, so that the back electrode layer on the surface of the second carrier layer and the back electrode layer in each P2 rework line groove are conductively connected to each other, and multiple P3 lines are drawn on the back electrode layer, and the P3 line groove of each P3 line is close to the position of its corresponding P2 rework line groove, and the P2 line groove without P2 rework line groove is close to the position of the P2 line groove, and each P3 line groove cuts the back electrode layer, the second carrier layer, the light absorption layer and the first carrier layer, and the bottom of each P3 line groove exposes the front electrode layer; The unqualified P2 wire slots include any one of the defects of discontinuity, uneven thickness, and overcutting the substrate surface.

[0006] Compared with the prior art, the method for preparing thin-film solar modules of the present invention adds a state inspection and rework step for P2 wire grooves in the existing thin-film solar module preparation process, performs a quality inspection on each P2 wire groove after processing, and directly proceeds to the next step if no unqualified P2 wire grooves are found; if unqualified P2 wire grooves are found, the P2 rework and scribing step is performed before the next step. The present invention has the following characteristics: the rework method of P2 wire grooves is simple, positioning is convenient, and unqualified P2 laser scribing products can be reworked and reused, saving resources and reducing costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] Figure 1 This is a schematic diagram of the internal structure of a thin-film solar module embodiment 1 of the present invention; Figure 2 for Figure 1 Schematic diagram of top view; Figure 3 This is a schematic diagram of the internal structure of a thin-film solar module embodiment 2 of the present invention; Figure 4 for Figure 3 Schematic top view of . Implementation

[0008] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. Example

[0009] Please also refer to Figure 1 and Figure 2 As shown, a preferred embodiment of the method for preparing a thin-film solar module of the present invention comprises the following steps: Step 1: Prepare a front electrode layer 2 on a clean substrate 1, perform multiple P1 scribing on the front electrode layer 2, and each P1 scribing P1 line groove 7 cuts through the front electrode layer 2, and the bottom of each P1 line groove 7 exposes the substrate 1. The P1 line groove 7 separates the front electrode layer 2 into multiple sub-cell areas.

[0010] Step 2: prepare a light absorbing layer 4 on the surface of the front electrode layer 2 and on the surface of each P1 line groove 7, and perform multiple P2 markings on the light absorbing layer 4. The P2 line groove 8 of each P2 marking is close to the position of its corresponding P1 line groove 7. Each P2 line groove 8 cuts through the light absorbing layer 4, and the bottom of each P2 line groove 8 exposes the front electrode layer 2.

[0011] Step 3: prepare a back electrode layer 6 on the surface of the light absorbing layer 4 and each P2 line groove 8, so that the back electrode layer 6 on the surface of the light absorbing layer 4 and the back electrode layer 6 in each P2 line groove 8 are conductively connected to each other, and then perform multiple P3 scribing on the back electrode layer 6, and the P3 line groove 9 of each P3 scribing is close to the position of the corresponding P2 line groove 8, and each P3 line groove 9 cuts through the back electrode layer 6, and the bottom of each P3 line groove 9 exposes the light absorbing layer 4. Finally, a thin-film solar module is obtained, which is composed of multiple sub-cells.

[0012] The method for preparing the thin-film solar module further includes a state inspection and rework step of the P2 wire groove 8 between step 2 and step 3, which step includes: performing a quality inspection on each P2 wire groove 8 after processing, and directly performing step 3 if no unqualified P2 wire groove 8 is found; if an unqualified P2 wire groove 8 is found, performing the P2 rework and marking step and step III in sequence: The P2 rework scribing step includes: adjusting processing parameters, performing corresponding P2 rework scribing on the side of each unqualified P2 line groove 8, and each P2 rework line groove 8' of the P2 rework scribing cuts off the light absorbing layer 4, and the bottom of each P2 rework line groove 8' exposes the front electrode layer 2, until each P2 line groove 8 is qualified.

[0013] Step III, prepare a back electrode layer 6 on the surface of the light absorbing layer 4, each P2 line groove 8 and each P2 rework line groove 8′, so that the back electrode layer 6 on the surface of the light absorbing layer 4 and the back electrode layer 6 in each P2 rework line groove 8′ are conductively connected to each other, and multiple P3 lines are drawn on the back electrode layer 6, and each P3 line groove 9 of the P3 line is close to the position of its corresponding P2 rework line groove 8′, and each P3 line groove 9 cuts through the back electrode layer 6, and the bottom of each P3 line groove 9 exposes the light absorbing layer 4.

[0014] The unqualified P2 wire slot 8 includes any one of the following defects: intermittent, uneven thickness, and overcutting the surface of the substrate 1. Figure 1 and Figure 2As shown, in the thin-film solar module of this embodiment, the P2 line groove 8 on the left has a discontinuous defect.

[0015] Specifically, the spacing between the P2 rework slots is 0~1mm, and the preferred spacing is 0~200μm. The width of the P2 rework slot can be consistent with the width of the P2 slot, or inconsistent with the width of the P2 slot. If inconsistent, the width of the P2 rework slot is 0.1μm~1mm, and the preferred width is 0.1μm~200μm. Example

[0016] Please also refer to Figure 3 and Figure 4 As shown, the present invention also discloses a method for preparing a thin-film solar module, comprising the following steps: Step 1: prepare a front electrode layer 2 on a clean substrate 1, perform multiple P1 scribing on the front electrode layer 2, and each P1 scribing P1 line groove 7 cuts through the front electrode layer 2, and the bottom of each P1 line groove 7 exposes the substrate 1. The P1 line groove 7 separates the front electrode layer 2 into multiple sub-cell areas.

[0017] Step 2: Prepare the first carrier layer 3, the light absorbing layer 4, and the second carrier layer 5 on the surface of the front electrode layer and the surface of each P1 line groove in sequence, and perform multiple P2 markings on the second carrier layer 5. The P2 line groove 8 of each P2 marking is close to the position of its corresponding P1 line groove 7. Each P2 line groove 8 cuts through the second carrier layer 5, the light absorbing layer 4 and the first carrier layer 3. The bottom of each P2 line groove 8 exposes the front electrode layer 2.

[0018] Step 3, prepare a back electrode layer 6 on the surface of the second carrier layer 5 and on the surface of each P2 line groove 8, so that the back electrode layer 6 on the surface of the second carrier layer 5 and the back electrode layer 6 in each P2 line groove 8 are conductively connected to each other, and then perform multiple P3 scribing on the back electrode layer 6, and the P3 line groove 9 of each P3 scribing is close to the position of its corresponding P2 line groove 8, and each P3 line groove 9 cuts the back electrode layer 6, the second carrier layer 5, the light absorption layer 4 and the first carrier layer 3, and the bottom of each P3 line groove 9 exposes the front electrode layer 2. Finally, a thin-film solar module is obtained, which is composed of multiple sub-cells.

[0019] The method for preparing the thin-film solar module further includes a step of inspecting the state of the P2 wire groove 8 and reworking the P2 wire groove 8 between step 2 and step 3, and the step includes: inspecting each P2 wire groove 8 after processing, and if no unqualified P2 wire groove 8 is found, directly proceeding to step 3; if an unqualified P2 wire groove 8 is found, sequentially performing the P2 rework and scribing step and step 3′: The P2 rework scribing step includes: adjusting processing parameters, performing corresponding P2 rework scribing on the side of each unqualified P2 line groove 8, and each P2 rework line groove 8' of the P2 rework scribing cuts off the second carrier layer 5, the light absorption layer 4 and the first carrier layer 3, and the bottom of each P2 rework line groove 8' exposes the front electrode layer 2, until each P2 line groove 8 is qualified.

[0020] Step 3′, prepare a back electrode layer 6 on the surface of the second carrier layer 5, on the surface of each P2 line groove 8, and on the surface of each P2 rework line groove 8′, so that the back electrode layer 6 on the surface of the second carrier layer 5 and the back electrode layer 6 in each P2 rework line groove 8′ are conductively connected to each other. Perform multiple P3 lines on the back electrode layer 6, and each P3 line groove 9 of the P3 lines is close to the location of its corresponding P2 rework line groove 8′, and if there is no P2 rework line groove 8′, it is close to the location of the P2 line groove 8. Each P3 line groove 9 cuts through the back electrode layer 6, the second carrier layer 5, the light absorption layer 4, and the first carrier layer 3, and the bottom of each P3 line groove 9 exposes the front electrode layer 2.

[0021] The unqualified P2 wire slot 8 includes any one of the following defects: intermittent, uneven thickness, and overcutting the surface of the substrate 1. Figure 3 and Figure 4 As shown, in the thin-film solar module of this embodiment, the P2 line groove 8 on the left has the defect of cutting into the surface of the substrate 1.

[0022] Specifically, the spacing between the P2 rework slots is 0~1mm, and the preferred spacing is 0~200μm. The width of the P2 rework slot can be consistent with the width of the P2 slot, or inconsistent with the width of the P2 slot. If inconsistent, the width of the P2 rework slot is 0.1μm~1mm, and the preferred width is 0.1μm~200μm.

[0023] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for preparing a thin-film solar module, characterized in that: The steps include: Step 1: prepare a front electrode layer on a clean substrate, perform multiple P1 scribing on the front electrode layer, each P1 line groove of the P1 scribing cuts through the front electrode layer, and the bottom of each P1 line groove exposes the substrate; Step 2: prepare a light absorbing layer on the surface of the front electrode layer and on the surface of each P1 line groove, perform multiple P2 scribing on the light absorbing layer, the P2 line groove of each P2 scribing line is close to the position of its corresponding P1 line groove, each P2 line groove cuts through the light absorbing layer, and the bottom of each P2 line groove exposes the front electrode layer; Step 3, prepare a back electrode layer on the surface of the light absorbing layer and the surface of each P2 line groove, so that the back electrode layer on the surface of the light absorbing layer and the back electrode layer in each P2 line groove are conductively connected to each other, and then perform multiple P3 scribing on the back electrode layer, the P3 line groove of each P3 scribing line is close to the position of its corresponding P2 line groove, each P3 line groove cuts through the back electrode layer, and the bottom of each P3 line groove exposes the light absorbing layer; The method for preparing the thin-film solar module further includes a P2 wire groove status inspection and rework step between step 2 and step 3, which step includes: performing a quality inspection on each P2 wire groove after processing, and if no unqualified P2 wire groove is found, directly proceeding to step 3; if an unqualified P2 wire groove is found, then sequentially performing the P2 rework and scribing step and step III: The P2 rework scribing step includes: adjusting processing parameters, performing corresponding P2 rework scribing on the side of each unqualified P2 line groove, wherein the P2 rework line groove of each P2 rework scribing cuts off the light absorption layer, and the bottom of each P2 rework line groove exposes the front electrode layer; Step III, preparing a back electrode layer on the surface of the light absorbing layer, each P2 line groove and each P2 rework line groove, so that the back electrode layer on the surface of the light absorbing layer and the back electrode layer in each P2 rework line groove are conductively connected to each other, and performing multiple P3 scribing on the back electrode layer, each P3 scribing P3 line groove is close to the position of its corresponding P2 rework line groove, each P3 line groove cuts through the back electrode layer, and the bottom of each P3 line groove exposes the light absorbing layer; The unqualified P2 wire slots include any one of the defects of discontinuity, uneven thickness, and overcutting the substrate surface.

2. A method for preparing a thin-film solar module, characterized in that: The steps include: Step 1, preparing a front electrode layer on a clean substrate, performing a plurality of P1 scribing lines on the front electrode layer, wherein a P1 line groove of each P1 scribing line cuts through the front electrode layer, and the bottom of each P1 line groove exposes the substrate; Step 2, sequentially preparing a first carrier layer, a light absorbing layer, and a second carrier layer on the surface of the front electrode layer and the surface of each P1 line groove, performing multiple P2 scribing on the second carrier layer, wherein the P2 line groove of each P2 scribing line is close to the position of its corresponding P1 line groove, each P2 line groove cuts through the second carrier layer, the light absorbing layer, and the first carrier layer, and the bottom of each P2 line groove exposes the front electrode layer; Step 3, preparing a back electrode layer on the surface of the second carrier layer and on the surface of each P2 line groove, so that the back electrode layer on the surface of the second carrier layer and the back electrode layer in each P2 line groove are conductively connected to each other, and then performing multiple P3 scribing on the back electrode layer, the P3 line groove of each P3 scribing is close to the position of its corresponding P2 line groove, each P3 line groove cuts through the back electrode layer, the second carrier layer, the light absorption layer and the first carrier layer, and the front electrode layer is exposed at the bottom of each P3 line groove; The method for preparing the thin-film solar module further includes a P2 wire groove status inspection and rework step between step 2 and step 3, which step includes: inspecting each P2 wire groove after processing, and if no unqualified P2 wire groove is found, directly proceeding to step 3; if an unqualified P2 wire groove is found, sequentially performing the P2 rework scribing step and step 3′: The P2 rework scribing step includes: adjusting processing parameters, performing corresponding P2 rework scribing on the side of each unqualified P2 line groove, wherein the P2 rework line groove of each P2 rework scribing cuts off the second carrier layer, the light absorption layer and the first carrier layer, and the bottom of each P2 rework line groove exposes the front electrode layer; Step 3′, preparing a back electrode layer on the surface of the second carrier layer, the surface of each P2 line groove and the surface of each P2 rework line groove, so that the back electrode layer on the surface of the second carrier layer and the back electrode layer in each P2 rework line groove are conductively connected to each other, and multiple P3 lines are drawn on the back electrode layer, and the P3 line groove of each P3 line is close to the position of its corresponding P2 rework line groove, and the P2 line groove without P2 rework line groove is close to the position of the P2 line groove, and each P3 line groove cuts the back electrode layer, the second carrier layer, the light absorption layer and the first carrier layer, and the bottom of each P3 line groove exposes the front electrode layer; The unqualified P2 wire slots include any one of the defects of discontinuity, uneven thickness, and overcutting the substrate surface.

3. The method for preparing a thin-film solar module according to claim 1 or 2, characterized in that: The spacing between the P2 rework slots is 0~1mm, the width of the P2 rework slots is consistent with the width of the P2 slots, or the width of the P2 rework slots is 0.1μm~1mm.