Gallium nitride-based high electron mobility transistor and manufacturing method thereof
By introducing a second P-type gallium nitride layer and a floating island field plate into the gallium nitride-based high electron mobility transistor, an island-like structure is formed, which solves the problem of single particle burning and improves the radiation resistance and stability of the device.
Patent Information
- Application Number
- CN202411053490.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-10-01
AI Technical Summary
Gallium nitride-based high electron mobility transistors are susceptible to single-particle burnout in space radiation environments, leading to device failure. Existing technologies have not been able to effectively improve their ability to resist single-particle burnout.
A gallium nitride-based high electron mobility transistor is designed. By forming a second P-type gallium nitride layer and a floating island field plate on the barrier layer, the boundary of the depletion region is extended, the electric field intensity is reduced, and an island-like structure is formed. It resists single-particle burning, and can optionally form floating island field plates and gate electrodes at the same time during the manufacturing process, reducing processes and costs.
It effectively reduces the probability of single particle burnout and improves the reliability and stability of gallium nitride-based high electron mobility transistors in space radiation environments without affecting their electrical performance.
Smart Images

Figure CN118738115A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a gallium nitride-based high electron mobility transistor and a method for manufacturing the same. Background Art
[0002] In recent years, GaN-based high electron mobility transistors have attracted great interest due to their excellent electrical properties, such as high breakdown voltage, low on-resistance and high switching speed. Compared with traditional silicon-based and silicon carbide-based power devices, GaN-based high electron mobility transistors can meet the requirements of high frequency, high power density, high temperature resistance, small size and light weight in practical applications, and show great potential in power management and conversion. They have been recognized as one of the disruptive components for transforming military electronic systems and architectures. At the same time, GaN-based high electron mobility transistors are also highly competitive in space and aviation power applications.
[0003] In applications under space radiation environments, single-event burnout is a common adverse effect of GaN-based high electron mobility transistors when they are working. Specifically, the device burns out at a voltage far below its rated operating voltage, causing the failure of aerospace electronic systems. Although relevant researchers have gradually begun to pay attention to this phenomenon, there is no effective way to improve its ability to resist single-event burnout. Summary of the invention
[0004] The purpose of the present application is to provide a gallium nitride-based high electron mobility transistor and a manufacturing method thereof, so as to improve the ability of the gallium nitride-based high electron mobility transistor to resist single particle burnout.
[0005] In order to achieve the above-mentioned purpose, in the first aspect, the present application provides a gallium nitride-based high electron mobility transistor including: a semiconductor substrate, a source electrode, a drain electrode, a gallium nitride channel layer, a barrier layer, a gate and a floating island. The source electrode and the drain electrode are formed on the semiconductor substrate and are spaced apart. The gallium nitride channel layer is formed on the semiconductor substrate, the gallium nitride channel layer is located between the source electrode and the drain electrode, and the gallium nitride channel layer is in contact with the source electrode and the drain electrode, respectively. The barrier layer is formed on the gallium nitride channel layer, the barrier layer is located between the source electrode and the drain electrode, and the barrier layer is in contact with the source electrode and the drain electrode, respectively. The gate is formed on the barrier layer, and the gate includes a first P-type gallium nitride layer formed on the barrier layer and a gate electrode formed on the first P-type gallium nitride layer. The floating island is formed on the barrier layer, the floating island is located between the gate and the drain electrode, and the floating island includes a second P-type gallium nitride layer formed on the barrier layer and a floating island field plate formed on the second P-type gallium nitride layer. The source electrode, the gate, the floating island and the drain electrode do not contact each other. The floating island field plate extends from the second P-type gallium nitride layer toward the drain electrode and is longer than the second P-type gallium nitride layer. The floating island field plate does not contact the gate, and the floating island field plate does not contact the drain electrode.
[0006] In the case of adopting the above scheme, the second P-type gallium nitride layer is formed on the barrier layer, the floating island field plate is formed on the barrier layer and is longer than the second P-type gallium nitride layer, and the second P-type gallium nitride layer and the floating island field plate included in the floating island are not in contact with other structures except for contacting the barrier layer, forming an island structure located between the gate and the drain electrode, namely the floating island. Due to the influence of the first P-type gallium nitride layer included in the gate, a depletion region is generated in the barrier layer of the gallium nitride-based high electron mobility transistor near the gate, and the fixed charge in the depletion region generates an electric field in the gallium nitride channel layer and the barrier layer. And the depletion region will no longer extend to the semiconductor substrate after contacting the channel under the gate, but will expand to the drain end. Since the gate has a certain size, the depletion layer also has a boundary at the edge of the gate. In the barrier layer, the depletion region near the edge of the gate quickly bends from the inside of the barrier layer to the surface of the barrier layer, and the fixed charge is also concentrated at the bend, and the electric field lines are also concentrated at the bend, which causes the electric field strength at the bend to increase significantly, and single particle burnout is prone to occur, causing the transistor to be broken down.
[0007] The second P-type gallium nitride layer included in the floating island extends the depletion region to the edge of the second P-type gallium nitride layer in the same principle as the aforementioned gate, that is, the depletion region boundary below the aforementioned gate edge is transferred to the edge of the second P-type gallium nitride layer, so that the depletion layer boundary curvature of the aforementioned area near the gate edge decreases, thereby reducing the electric field strength in this area, which can effectively resist single-particle burnout breakdown, but also introduces an increased electric field strength area at the edge of the floating island. When a positive bias is applied to the floating island field plate included in the floating island, the depletion region is further extended toward the drain electrode, reducing the curvature of the depletion region edge, thereby weakening the electric field at the edge of the second P-type gallium nitride layer, and at the same time, no new increased electric field strength area is introduced, further resisting single-particle burnout breakdown.
[0008] Optionally, the floating island field plate is made of metal material. The floating island field plate can be made of the same metal material as the gate electrode, which can facilitate the formation of the floating island field plate and the gate electrode in a one-step process when manufacturing the gallium nitride-based high electron mobility transistor provided by the present application, thereby reducing the number of steps and the cost.
[0009] Optionally, the distance between the floating island and the gate is 0.5μm to 1.5μm; and / or, the distance between the floating island and the drain electrode is 3.5μm to 4.5μm. If the floating island is too close to the gate, it will be difficult to implement in terms of process, and may cause the insulation performance of the floating island field plate and the gate electrode to deteriorate; if the floating island is too far away from the gate, the depletion layer formed under the gate and under the floating island cannot be effectively connected, and the boundary curvature of the depletion region at the edge of the gate is still large, which cannot resist single-particle burnout. Therefore, within this length range, the floating island can achieve better resistance to single-particle burnout.
[0010] Optionally, the length of the floating island field plate extending out of the second P-type gallium nitride layer is 1μm to 1.5μm. If the floating island field plate is short, it cannot modulate the electric field in the barrier layer and cannot improve the ability to resist single-particle burnout; if the floating island field plate is too long, it will increase the difficulty of forming the floating island field plate process. Therefore, when the length of the floating island field plate is within this range, the floating island can achieve a better effect of resisting single-particle burnout.
[0011] Optionally, the thickness of the second P-type gallium nitride layer is 1μm to 2μm; and / or, the thickness of the floating island field plate is 0.1μm to 0.2μm; and / or, the thickness of the floating island field plate is equal to the thickness of the gate electrode. A second P-type gallium nitride layer that is too thick may cause the two-dimensional electron gas below the second P-type gallium nitride layer to be completely depleted, affecting the performance of the gallium nitride-based high electron mobility transistor. A second P-type gallium nitride layer that is too thin may break down when a voltage is applied to the floating island field plate. Therefore, within this range of the thickness of the second P-type gallium nitride layer, the floating island can achieve better resistance to single-particle burnout.
[0012] Optionally, a groove is provided in the barrier layer, and a part of the first P-type gallium nitride layer is filled in the groove. The first P-type gallium nitride layer is inserted into the barrier layer in the above-mentioned manner, which can raise the potential barrier, so that the potential well at the junction of the barrier layer and the gallium nitride channel layer disappears, and the two-dimensional electron gas originally in the gallium nitride channel layer is exhausted, forming an enhanced gallium nitride-based high electron mobility transistor.
[0013] Optionally, the semiconductor substrate includes: a substrate, and a transition layer and a buffer layer stacked in sequence on the substrate; a source electrode, a drain electrode and a gallium nitride channel layer are arranged on the buffer layer. The aforementioned semiconductor substrate can alleviate problems such as lattice mismatch between the substrate and the gallium nitride channel layer, so that the gallium nitride-based high electron mobility transistor provided in the present application has good performance.
[0014] In a second aspect, the present application also provides a method for manufacturing a gallium nitride-based high electron mobility transistor, comprising: first, providing a semiconductor substrate. Next, forming a source electrode and a drain electrode spaced apart on the semiconductor substrate. Next, forming a gallium nitride channel layer and a barrier layer in sequence on the semiconductor substrate, wherein the gallium nitride channel layer and the barrier layer are both located between the source electrode and the drain electrode. Next, forming a gate on the barrier layer, the gate comprising a first P-type gallium nitride layer formed on the barrier layer and a gate electrode formed on the first P-type gallium nitride layer. Next, forming a floating island on the barrier layer, the floating island being located between the gate and the drain electrode, the floating island comprising a second P-type gallium nitride layer formed on the barrier layer and a floating island field plate formed on the second P-type gallium nitride layer. The floating island field plate extends from the second P-type gallium nitride layer toward the drain electrode and is longer than the second P-type gallium nitride layer, the floating island field plate does not contact the gate, and the floating island field plate does not contact the drain electrode.
[0015] Optionally, providing a semiconductor substrate includes: providing a substrate; forming a transition layer on the substrate; forming a buffer layer on the transition layer, and the source electrode, the drain electrode and the gallium nitride channel layer are arranged on the buffer layer.
[0016] Optionally, the second P-type gallium nitride layer is formed simultaneously with the first P-type gallium nitride layer; and / or the floating island field plate is formed simultaneously with the gate electrode. Forming multiple structures simultaneously can reduce manufacturing processes and reduce costs.
[0017] Compared with the prior art, the beneficial effects of the method for manufacturing a gallium nitride-based high electron mobility transistor provided in the present application are the same as the beneficial effects of the gallium nitride-based high electron mobility transistor in the above technical solution, which will not be repeated here. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0019] Figure 1 A schematic diagram of a gallium nitride-based high electron mobility transistor in the prior art;
[0020] Figure 2 A schematic diagram of a gallium nitride-based high electron mobility transistor provided in an embodiment of the present application;
[0021] Figure 3 A schematic diagram of the electric field intensity distribution near a gate of a gallium nitride-based high electron mobility transistor in the prior art;
[0022] Figure 4 A schematic diagram of the electric field intensity distribution near the gate of a gallium nitride-based high electron mobility transistor provided in an embodiment of the present application;
[0023] Figure 5 A leakage current curve diagram of a gallium nitride-based high electron mobility transistor provided in an embodiment of the present application and a gallium nitride-based high electron mobility transistor in the prior art after being subjected to radiation of the same intensity but different time.
[0024] Reference numerals:
[0025] 100-semiconductor base, 101-substrate,
[0026] 102-transition layer, 103-buffer layer,
[0027] 200-drain electrode, 300-source electrode,
[0028] 400-GaN channel layer, 401-two-dimensional electron gas,
[0029] 500-barrier layer, 600-gate,
[0030] 601 - first P-type gallium nitride layer, 602 - gate electrode,
[0031] 700-floating island, 701-second P-type gallium nitride layer,
[0032] 702- floating island field plate, 800- passivation layer. DETAILED DESCRIPTION
[0033] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0034] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0035] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, "multiple" means two or more, unless otherwise clearly and specifically defined. "Several" means one or more, unless otherwise clearly and specifically defined.
[0036] In the description of the present application, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", etc., indicating directions or positional relationships are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present application.
[0037] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0038] Gallium nitride-based high electron mobility transistors are being used more and more widely due to their excellent performance. At present, the research on single-particle effects in gallium nitride-based high electron mobility transistors in space radiation environments is still relatively limited, but with the continuous development of space applications and the increasing demand for high-reliability and high-stability devices, research in this area is becoming more and more important. In the space environment, gallium nitride devices will be affected by space radiation, including ion radiation from cosmic rays and solar radiation, which will have an adverse effect on the performance and stability of the device, such as single-particle burnout.
[0039] Due to its excellent electrical properties, GaN-based high electron mobility transistors are more adaptable to the radiation environment in the universe than traditional silicon-based power semiconductors. In order to promote its application in the space field, it is necessary to improve the ability of GaN devices to resist single-particle burnout in the space radiation environment.
[0040] GaN-based high electron mobility transistors have many subtypes, and the enhancement mode GaN-based high electron mobility transistor is a common subtype. The enhancement mode GaN-based high electron mobility transistor is made to be in the off state when the gate is not biased by adding a P-type GaN layer under the gate metal. P-type GaN has a higher Fermi level. The contact between the P-type GaN layer and the barrier layer raises the Fermi level of the heterojunction formed by the barrier layer and the GaN channel layer. The potential well that binds the two-dimensional electron gas formed at the heterojunction also disappears, and the two-dimensional electron gas disappears as well. The transistor is in the off state when the gate is not biased. The remaining fixed charge in the barrier layer forms a depletion region, and at the same time forms an electric field pointing from the edge of the depletion region to the P-type GaN layer. Due to the size limitation of the P-type gallium nitride layer included in the gate, the depletion region formed at the edge of the gate will quickly bend from the inside of the barrier layer to the surface of the barrier layer, that is, the distribution of fixed charges will bend and the field strength of the electric field will increase rapidly.
[0041] The triggering mechanism of single-particle burnout includes the back channel effect and the subsequent impact ionization dominated by electrons in the high-field region. Due to the single-particle incident, a large number of electron-hole pairs are generated at the incident trajectory. The ionized electrons move toward the drain end under the action of the electric field, forming a leakage current. These electrons flow to the high electric field strength interval between the gate and the drain, especially at the gate edge. They are affected by the high electric field at the boundary of the barrier layer in the barrier layer below the gate edge, and obtain higher energy. These electrons will bombard the barrier layer, causing the extranuclear electrons of the atoms in the barrier layer to separate from the nuclei, generating more electron-hole pairs, significantly increasing the electron concentration and hole concentration of the barrier layer, and reducing the resistivity of the barrier layer, resulting in a sudden change in the current between the source and the drain, exceeding the carrying capacity of the transistor, and finally causing single-particle burnout of the GaN-based high electron mobility transistor.
[0042] To solve the above problems, in the first aspect, the present application provides a gallium nitride-based high electron mobility transistor. Figure 2 The gallium nitride-based high electron mobility transistor provided in the embodiment of the present application includes: a semiconductor substrate 100, a source electrode 300, a drain electrode 200, a gallium nitride channel layer 400, a barrier layer 500, a gate 600 and a floating island 700. The source electrode 300 and the drain electrode 200 are formed on the semiconductor substrate 100 and are spaced apart. The gallium nitride channel layer 400 is formed on the semiconductor substrate 100, the gallium nitride channel layer 400 is located between the source electrode 300 and the drain electrode 200, and the gallium nitride channel layer 400 is in contact with the source electrode 300 and the drain electrode 200, respectively. The barrier layer 500 is formed on the gallium nitride channel layer 400, the barrier layer 500 is located between the source electrode 300 and the drain electrode 200, and the barrier layer 500 is in contact with the source electrode 300 and the drain electrode 200, respectively. The gate 600 is formed on the barrier layer 500, and the gate 600 includes a first P-type gallium nitride layer 601 formed on the barrier layer 500 and a gate electrode 602 formed on the first P-type gallium nitride layer 601. The floating island 700 is formed on the barrier layer 500, and the floating island 700 is located between the gate 600 and the drain electrode 200, and the floating island 700 includes a second P-type gallium nitride layer 701 formed on the barrier layer 500 and a floating island field plate 702 formed on the second P-type gallium nitride layer 701. The source electrode 300, the gate 600, the floating island 700 and the drain electrode 200 do not contact each other; the floating island field plate 702 extends from the second P-type gallium nitride layer 701 to the drain electrode 200 and is longer than the second P-type gallium nitride layer 701, and the floating island field plate 702 does not contact the gate 600, and the floating island field plate 702 does not contact the drain electrode 200.
[0043] When using the above technical solution, please refer to Figure 2The second P-type gallium nitride layer 701 and the floating island field plate 702 included in the floating island 700 are arranged on the barrier layer 500 and located between the gate 600 and the drain electrode 200. The floating island 700 does not contact other structures except the barrier layer 500 and the passivation layer 800, forming an island structure, namely the floating island 700; please refer to Figure 1 , Figure 1 The structure of a gallium nitride-based high electron mobility transistor in the prior art is shown in FIG. Figure 1 Compared with the prior art, the embodiment of the present application additionally provides the aforementioned floating island 700.
[0044] Please refer to Figure 3 The depletion layer generated by the barrier layer 500 affected by the first P-type gallium nitride layer 601 produces an area at the edge of the first P-type gallium nitride layer 601 where the electric field strength is significantly higher than that in the non-edge area. According to the above analysis, a stronger electric field force will be applied to the electron-hole pairs generated by the single particle incident, thereby causing the occurrence of single particle burnout.
[0045] Please refer to Figure 4 In a gallium nitride-based high electron mobility transistor provided in an embodiment of the present application, the second P-type silicon nitride layer included in the added floating island 700 generates a depletion region through the same principle as the gate 600 generates a depletion region, so that the high electric field intensity region below the edge of the gate 600 is transferred to below the edge of the second P-type silicon nitride layer close to the drain electrode 200. At the same time, the floating field plate can change the fixed charge distribution in the barrier layer 500, further extend the depletion region toward the drain electrode 200, reduce the curvature of the depletion region boundary, and thus reduce the electric field at the depletion region boundary, thereby avoiding the barrier layer 500 below the second P-type silicon nitride layer from being easily incident by a single particle, further causing the device to be burned by a single particle, and the existence of the floating island 700 will not affect the electrical performance of the gallium nitride-based high electron mobility transistor.
[0046] In the actual application process, the semiconductor substrate 100 may be a substrate without any structure formed thereon; or, the semiconductor substrate 100 may be a substrate with some structures formed thereon. Specifically, the structure formed on the substrate may be set according to actual needs. For example, the semiconductor substrate 100 may include a substrate and a buffer layer. Another example is that the semiconductor substrate 100 may include a substrate, a transition layer and a buffer layer. Specifically, the material of the substrate may be sapphire, silicon carbide or silicon substrate, the material of the buffer layer may be aluminum nitride, and the material of the buffer layer may be gallium nitride or aluminum gallium nitride; if it is necessary to make the gallium nitride-based high electron mobility transistor obtain a higher withstand voltage value, a gallium nitride stress compensation layer may be added between the transition layer and the buffer layer, and on the buffer layer.
[0047] For example, please refer to Figure 1 and Figure 2The semiconductor substrate 100 includes a substrate 101, a transition layer 102 and a buffer layer 103. The substrate 101 is made of P-type silicon, the transition layer 102 is made of aluminum nitride, and the buffer layer 103 is made of aluminum gallium nitride or gallium nitride. The silicon substrate is selected because it is compatible with existing silicon-based processes during processing, thereby reducing costs. Secondly, the price of silicon is significantly lower than that of other substrate materials, thereby reducing costs.
[0048] Preferably, the material of the buffer layer 103 is Al 0.05 Ga 0.95 N, the thickness is 2 μm, and the thickness of the transition layer 102 is 5 nm.
[0049] As for the GaN channel layer 400 , the present application does not impose any limitation on its thickness and doping concentration, and its thickness and doping concentration can be determined according to performance requirements.
[0050] Preferably, the GaN channel layer 400 has a thickness of 0.2 μm and is N-type doped with a concentration of 1×10 15 cm -3 .
[0051] As for the barrier layer 500 , its material is aluminum gallium nitride. In addition, the present application does not impose any restrictions on its thickness and doping concentration, and its thickness and doping concentration can be determined according to performance requirements.
[0052] Preferably, the material is Al 0.23 Ga 0.77 N, thickness is 15nm, N-type doping, concentration is 1×10 18 cm -3 .
[0053] As for the source electrode 300 and the drain electrode 200, please refer to Figure 2 , both form Schottky contacts with the barrier layer 500 and the channel layer. In addition, the present application does not limit the size and material of the source electrode 300 and the drain electrode 200, as long as the aforementioned Schottky contact can be achieved.
[0054] Preferably, the source electrode 300 and the drain electrode 200 are made of metal materials, such as copper, aluminum, tungsten, etc.
[0055] The present application does not impose any restrictions on the doping concentrations of the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701, as long as their thicknesses are matched so that the two-dimensional electron gas 401 in the channel layer below the first P-type gallium nitride layer 601 is completely consumed, and the two-dimensional electron gas 401 in the channel layer below the second P-type gallium nitride layer 701 is not completely consumed. Preferably, the doping concentrations of the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701 are the same, and are both 1×10 18 cm -3 .
[0056] Regarding the groove of the barrier layer 500 below the first P-type gallium nitride layer 601, its depth is 2nm to 5nm. Within this range, the first P-type gallium nitride layer 601 inserted into the barrier layer 500 can effectively deplete the two-dimensional electron gas 401 to form a gallium nitride-based high electron mobility transistor with better performance.
[0057] For the thickness of the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701, please refer to Figure 2 In the present application, the difference in thickness between the two is the thickness of the aforementioned groove, that is, the thickness of the first P-type gallium nitride layer 601 above the barrier layer 500 is equal to the thickness of the second P-type gallium nitride layer 701. In this way, when manufacturing the gallium nitride-based high electron mobility transistor provided in the embodiment of the present application, the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701 can be formed at the same time, thereby reducing the process steps and reducing the cost.
[0058] As a possible implementation manner, the thickness of the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701 are both 1 μm to 2 μm.
[0059] The present application does not limit the length of the gate 600, as long as it can meet the performance requirements of the gallium nitride-based high electron mobility transistor provided in the embodiment of the present application, and the first P-type gallium nitride layer 601 and the gate electrode 602 included in the gate 600 have the same length. Preferably, the first P-type gallium nitride layer 601 and the gate electrode 602 included in the gate 600 are both 1.4 μm long.
[0060] For the length of Floating Island 700, please refer to Figure 2 , the length of the second P-type gallium nitride layer 701 included in the floating island 700 is 1 μm to 2 μm; the floating island field plate 702 included in the floating island 700 is flush with the second P-type gallium nitride layer 701 on the side close to the gate 600, and the floating island field plate 702 is 1 μm to 1.5 μm longer than the second P-type gallium nitride layer 701 on the side close to the drain electrode 200. Based on this, when the lengths of the second P-type gallium nitride layer 701 and the floating island field plate 702 included in the floating island 700 are within the aforementioned range, a better electric field relief effect can be achieved, thereby obtaining a better effect of resisting single particle burnout.
[0061] As for the thickness and material of the floating island field plate 702, this application does not make any specific restrictions, as long as the effect of relieving the electric field can be achieved. At the same time, this application does not limit the thickness and material of the gate electrode 602, as long as it can meet the performance requirements of the GaN-based high electron mobility transistor for the gate 600.
[0062] As a possible implementation, the thickness and material of the floating island field plate 702 and the gate electrode 602 are the same, and both are 0.1 μm to 0.2 μm. The floating island field plate 702 and the gate electrode 602 of the same thickness can be manufactured through the same set of processes, reducing the number of separate manufacturing steps and reducing costs.
[0063] Regarding the position of the floating island 700 between the gate 600 and the drain electrode 200 , according to the analysis in the invention content, the floating island 700 can obtain a better electric field relief effect when the distance from the gate 600 is 0.5 μm to 1.5 μm and the distance from the drain electrode 200 is 3.5 μm to 4.5 μm.
[0064] As a possible implementation, please refer to Figure 2 A passivation layer 800 is also formed on the source electrode 300, the gate 600, the floating island field plate 702, the drain electrode 200 and the barrier layer 500. The present application does not limit the thickness and material of the passivation layer 800, as long as it can completely cover the source electrode 300, the gate 600, the floating island field plate 702, the drain electrode 200 and the barrier layer 500. Preferably, the material of the passivation layer 800 is silicon nitride. The passivation layer 800 plays an important role in reducing the current collapse of the drain electrode 200 and maintaining the two-dimensional electron gas 401 generated by the polarization characteristics, further improving the working performance of the gallium nitride-based high electron mobility transistor provided in the embodiment of the present application.
[0065] Please refer to the above solution. In one embodiment, when the GaN-based high electron mobility transistor is in an off-state bias, such as the source electrode 300 to ground voltage V S =0V, gate 600 to ground voltage V G =1V, drain electrode 200 to ground voltage V D =200V. Please refer to Figure 3 In the prior art without floating islands, the depletion region will bend rapidly at the edge of the gate 600, and the electric field strength will increase rapidly, forming a weak area for single particle burnout. Please refer to Figure 4 The floating island 700 extends the depletion region and greatly reduces the curvature of the depletion region boundary, so that the electric field strength at the boundary is significantly reduced, and the ability to resist single particle burnout is improved. Heavy particle radiation is performed on the barrier layer 500 at the edge of the gate 600 of the two gallium nitride-based high electron mobility transistors provided in the prior art and the embodiment of the present application, and the device performance diagram obtained is as follows: Figure 5 . The radiation starts from 0 and lasts to 5x 10 -12 s, the linear energy transfer (LET) intensity of the radiation is 5pC / μm, and the incident depth of the radiation penetrates the entire device. Figure 5The vertical axis is the simulation time, and the vertical axis is the leakage current. Obviously, the GaN-based high electron mobility transistor provided by the embodiment of the present application has a smaller source-drain current in the off state when subjected to the same intensity of radiation than the prior art, and is less prone to single-particle burnout.
[0066] In the second aspect, the embodiment of the present application also provides a method for manufacturing a gallium nitride-based high electron mobility transistor. The gallium nitride-based high electron mobility transistor manufactured by the manufacturing method provided in the embodiment of the present application has the same structure, material and size as the gallium nitride-based high electron mobility transistor provided in the first aspect. Therefore, the structure, material and size of the semiconductor substrate can be referred to in the previous text and will not be repeated here.
[0067] Please refer to Figure 2 , the manufacturing method comprises the following steps:
[0068] First, a semiconductor substrate 100 is provided. The specific structure and material of the semiconductor substrate 100 can be referred to above and will not be described here. It can be understood that when the structure of the semiconductor substrate 100 is different, the method of forming the semiconductor substrate 100 may also be different, so the formation process of the semiconductor substrate 100 can be determined according to the structure of the semiconductor substrate 100.
[0069] In one embodiment, providing the semiconductor substrate 100 may include the following steps: providing a substrate 101; depositing a transition layer 102 on the substrate 101; and heteroepitaxially growing a buffer layer 103 on the transition layer 102. The materials of the substrate 101, the transition layer 102, and the buffer layer 103 are described above and will not be described again.
[0070] Optionally, according to the withstand voltage requirement of the GaN-based high electron mobility transistor, a GaN stress release layer may be heteroepitaxially grown between the transition layer 102 and the buffer layer 103 and on the buffer layer 103 .
[0071] Next, the source electrode 300 and the drain electrode 200 are deposited on the buffer layer 103 included in the semiconductor substrate 100 .
[0072] Again, the buffer layer 103 included on the semiconductor substrate 100 is sequentially formed into a gallium nitride channel layer 400 and a barrier layer 500 by epitaxy, and both the gallium nitride channel layer 400 and the barrier layer 500 are located between the source electrode 300 and the drain electrode 200. The materials and dimensions of the gallium nitride channel layer 400 and the barrier layer 500 are referred to above and will not be described again.
[0073] After forming the barrier layer 500 by epitaxy, before forming the gate 600 and the floating island 700, the process further includes: forming a groove by etching at the position where the gate 600 is to be formed on the barrier layer 500. The size of the groove is referred to above and will not be described again.
[0074] Next, a gate 600 and a floating island 700 are formed on the barrier layer 500. In the actual manufacturing process, according to the above scheme, regarding the formation of the gate 600 and the floating island 700, the present application provides two manufacturing processes of Example 1 and Example 2. It should be noted that Example 1 and Example 2 are only used to more clearly illustrate the technical solution provided by the embodiment of the present application, and cannot be used to limit the protection scope of the embodiment of the present application.
[0075] Embodiment 1:
[0076] The gate 600 and the floating island 700 are formed at the same time. The materials and dimensions of the gate 600 and the floating island 700 are referred to above and will not be described again. The gate 600 and the floating island 700 are formed at the same time to reduce the process of forming the gate 600 and the floating island 700 separately, thereby reducing the cost.
[0077] Specifically, a first mask is first formed on the barrier layer 500 and patterned, the first mask has a groove with a size determined according to the requirements at the position where the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701 are to be formed, and then the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701 are formed in the groove by epitaxy or deposition; next, a second mask is formed on the first mask, the first P-type gallium nitride layer 601 and the second P-type gallium nitride layer 701 and patterned, the second mask has a groove with a size determined according to the requirements at the position where the gate electrode 602 and the floating island field plate 702 are to be formed, and then the gate electrode 602 and the floating island field plate 702 are formed in the groove by deposition; finally, the first mask and the second mask are removed. Compared with the separate formation of the gate 600 and the floating island 700, the above scheme saves two masks and corresponding materials and processes, and effectively reduces the cost.
[0078] Embodiment 2:
[0079] The gate 600 and the floating island 700 are formed separately, specifically including:
[0080] S1: A third mask is formed on the barrier layer 500 and patterned, the third mask has a groove with a size determined according to requirements at the position where the first P-type gallium nitride layer 601 is to be formed, and then the second P-type gallium nitride layer 701 is formed in the groove by epitaxy or deposition; next, a fourth mask is formed on the third mask and the first P-type gallium nitride layer 601 and patterned, the fourth mask has a groove with a size determined according to requirements at the position where the gate electrode 602 is to be formed, and then the gate electrode 602 is formed in the groove by deposition; finally, the third mask and the fourth mask are removed.
[0081] S2: A fifth mask is formed and patterned on the barrier layer 500, wherein the fifth mask has a groove of a size determined according to requirements at a position where the second P-type gallium nitride layer 701 is to be formed, and then the second P-type gallium nitride layer 701 is formed in the groove by epitaxy or deposition; next, a sixth mask is formed and patterned on the fifth mask and the second P-type gallium nitride layer 701, wherein the sixth mask has a groove of a size determined according to requirements at a position where the floating island field plate 702 is to be formed, and then the floating island field plate 702 is formed in the groove by deposition; finally, the fifth mask and the sixth mask are removed.
[0082] The order of S1 and S2 included in this embodiment can be exchanged according to process requirements and is not limited here.
[0083] Finally, a passivation layer 800 is deposited on the source electrode 300 , the gate 600 , the floating island field plate 702 , the drain electrode 200 and the barrier layer 500 . The passivation layer 800 completely covers the source electrode 300 , the gate 600 , the floating island field plate 702 , the drain electrode 200 and the barrier layer 500 .
[0084] Compared with the prior art, the beneficial effects of the method for manufacturing a gallium nitride-based high electron mobility transistor provided in the embodiment of the present application are the same as the beneficial effects of the above-mentioned gallium nitride-based high electron mobility transistor, which will not be elaborated here.
[0085] In the above description, the technical details of the patterning and etching of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.
[0086] The embodiments of the present application are described above. However, these embodiments are only for the purpose of illustrating the content of the present application, and are not intended to limit the scope of the present application. The scope of the present application is limited by the attached claims and their equivalents. Without departing from the scope of the present application, those skilled in the art may make various substitutions and modifications, which should all fall within the scope of the present application.
Claims
1. A gallium nitride-based high electron mobility transistor, characterized in that: include: Semiconductor substrate; A source electrode and a drain electrode formed on the semiconductor substrate and distributed at intervals; A gallium nitride channel layer is formed on the semiconductor substrate, wherein the gallium nitride channel layer is located between the source electrode and the drain electrode, and the gallium nitride channel layer is in contact with the source electrode and the drain electrode respectively; A barrier layer is formed on the gallium nitride channel layer, the barrier layer is located between the source electrode and the drain electrode, and the barrier layer is in contact with the source electrode and the drain electrode respectively; A gate formed on the barrier layer, the gate comprising a first P-type gallium nitride layer formed on the barrier layer and a gate electrode formed on the first P-type gallium nitride layer; A floating island is formed on the barrier layer, the floating island is located between the gate and the drain electrode, the floating island includes a second P-type gallium nitride layer formed on the barrier layer and a floating island field plate formed on the second P-type gallium nitride layer; the source electrode, the gate, the floating island and the drain electrode are not in contact with each other; the floating island field plate extends from the second P-type gallium nitride layer toward the drain electrode and is longer than the second P-type gallium nitride layer, the floating island field plate is not in contact with the gate, and the floating island field plate is not in contact with the drain electrode.
2. The gallium nitride-based high electron mobility transistor according to claim 1, characterized in that: The floating island field plate is a metal material layer.
3. The gallium nitride-based high electron mobility transistor according to claim 1, characterized in that: The distance between the floating island and the gate is 0.5 μm to 1.5 μm; And / or, the distance between the floating island and the drain electrode is 3.5 μm to 4.5 μm.
4. The gallium nitride-based high electron mobility transistor according to claim 1, characterized in that: The length of the floating island field plate extending out of the second P-type gallium nitride layer is 1 μm to 1.5 μm.
5. The gallium nitride-based high electron mobility transistor according to claim 1, characterized in that: The thickness of the second P-type gallium nitride layer is 1 μm to 2 μm; And / or, the thickness of the floating island field plates is 0.1 μm to 0.2 μm; And / or, the thickness of the floating island field plate is equal to the thickness of the gate electrode.
6. The gallium nitride-based high electron mobility transistor according to claim 1, characterized in that: A groove is provided in the barrier layer, and a part of the first P-type gallium nitride layer is filled in the groove.
7. The gallium nitride-based high electron mobility transistor according to claim 1, characterized in that: The semiconductor substrate comprises: a substrate, and a transition layer and a buffer layer sequentially stacked on the substrate; The source electrode, the drain electrode, and the gallium nitride channel layer are disposed on the buffer layer.
8. A method for manufacturing a gallium nitride-based high electron mobility transistor, characterized in that: include: providing a semiconductor substrate; forming a source electrode and a drain electrode which are spaced apart from each other on the semiconductor substrate; forming a gallium nitride channel layer and a barrier layer in sequence on the semiconductor substrate, wherein the gallium nitride channel layer and the barrier layer are both located between the source electrode and the drain electrode; forming a gate on the barrier layer, wherein the gate comprises a first P-type gallium nitride layer formed on the barrier layer and a gate electrode formed on the first P-type gallium nitride layer; A floating island is formed on the barrier layer, the floating island is located between the gate and the drain electrode, the floating island includes a second P-type gallium nitride layer formed on the barrier layer and a floating island field plate formed on the second P-type gallium nitride layer; the source electrode, the gate, the floating island and the drain electrode are not in contact with each other; the floating island field plate extends from the second P-type gallium nitride layer toward the drain electrode and is longer than the second P-type gallium nitride layer, the floating island field plate is not in contact with the gate, and the floating island field plate is not in contact with the drain electrode.
9. The method for manufacturing a gallium nitride-based high electron mobility transistor according to claim 8, characterized in that: Providing a semiconductor substrate comprises: providing a substrate; forming a transition layer on the substrate; A buffer layer is formed on the transition layer, and the source electrode, the drain electrode and the gallium nitride channel layer are arranged on the buffer layer.
10. The method for manufacturing a gallium nitride-based high electron mobility transistor according to claim 8, characterized in that: The second P-type gallium nitride layer is formed simultaneously with the first P-type gallium nitride layer; And / or, the floating island field plate and the gate electrode are formed simultaneously.
Citation Information
Cited By
Heterojunction semiconductor device
WO2026138665A1