Method for immersion bath treatment of components

By locally unevenly distributing the catalyst on the surface of the component, the problem of conflict between optical properties and reactivity during the coating drying and cross-linking processes during the cathodic dipping process is solved, achieving uniform solidification and rapid cross-linking of the coating, and improving corrosion resistance. and optical properties, extending service life and reducing manufacturing costs.

CN118742676APending Publication Date: 2024-10-01BAYERISCHE MOTOREN WERKE AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380023301.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-05-31
Filing Date
2023-05-08
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the prior art cathodic dipping process, there is a target conflict between optical performance and reactivity during the drying and cross-linking process of the coating, resulting in the coating not being fully cured in certain areas, affecting corrosion protection and optical performance.

Method used

By locally unevenly distributing the catalyst on the surface of the component, especially applying different concentrations of catalyst on different sub-areas of the coating, to adjust the cross-linking speed and reactivity, and optimizing the temperature and time during the drying process to ensure the uniformity of the coating Curing and rapid cross-linking.

Benefits of technology

It improves the curing and cross-linking quality of the coating, enhances the corrosion resistance and optical properties of the components, extends the service life, and reduces manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118742676A_ABST
    Figure CN118742676A_ABST
Patent Text Reader

Abstract

The invention relates to a method for the immersion bath treatment (1) of a component (2), in which method a coating (5) applied by electrophoretic deposition (3) to a surface (4) of the component (2) is dried, a catalyst (10) for curing (9) the coating (5) during drying (8) being applied to the surface (4) of the component (2) in a targeted non-uniform distribution.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for immersion treatment of components according to the preamble of patent claim 1. Background Art

[0002] Methods for coating, in particular painting, components are already known from the prior art. In this case, for example, lacquer and / or wax and / or polyvinyl chloride (PVC) are applied to the surface of the component, in particular in multiple layers. The lacquer can be provided, in particular, for protecting the component from corrosion within the scope of cathodic lacquering (CTL). The coating or lacquer is then dried and cured. The lacquer, which can be referred to as CTL, is, for example, the first lacquer layer of the component. For example, a topcoat and / or a clearcoat can be applied to the first lacquer layer. In particular, the lacquer can be applied to the component as a first layer in a lacquer structure and baked before further painting. Summary of the invention

[0003] The object of the present invention is to provide a method for the immersion treatment of a component in such a way that in particular the curing of a coating applied to the surface of the component can be improved.

[0004] This object is achieved according to the invention by a method for the immersion treatment of components having the features of patent claim 1. Advantageous embodiments of the invention are the subject matter of the dependent claims and the description.

[0005] A first aspect of the invention relates to a method for immersion treatment, in particular surface treatment, of at least one component, in particular a component for a motor vehicle, in which method at least one coating applied to at least one surface of the component by electrophoretic deposition, in particular by cathodic dip painting (CTL), is dried at least partially or completely. The coating is, for example, a paint, in particular the lowermost paint layer. Thus, the coating can be referred to, for example, as a paint.

[0006] For example, wax and / or polyvinyl chloride (PVC) can be applied to the coating, in particular at the end of the coating process of the component.

[0007] The method may include applying the coating by means of electrophoretic deposition, in particular by means of cathodic dip painting. This means that the coating can be applied by electrophoretic deposition, in particular by cathodic dip painting, in particular directly onto the surface of the component. The coating applied to the surface of the component can then be dried, in particular crosslinked or cured.

[0008] For example, the component is formed from at least one metal. Thus, the component can be a metal component. The surface is thus configured as a metal surface, for example.

[0009] A coating, in particular a lacquer, is to be understood as meaning in particular a liquid coating material. The coating applied to the surface of the component is dried, for example, by means of a drying device, in particular a so-called dryer, and can preferably be cured or chemically crosslinked in the process. In this case, the coating can change from a liquid state to a solid state. Thus, curing and in particular chemical crosslinking preferably takes place during drying.

[0010] In electrophoretic deposition, in particular in cathodic dip painting, in particular under the influence of an electric field, colloidal particles can be deposited on an electrode, in particular on the component or on the surface. Deposition can be carried out by increasing the pH value on the component surface due to hydrogen deposition. For this purpose, the component can be at least partially, in particular completely, immersed in an immersion tank filled with a fluid. Here, due to the immersion in the fluid, the component, in particular the surface, can be provided or coated at least partially, in particular completely with a coating, in particular referred to as a KTL coating. The coating can contain at least one polymer resin and / or at least one adhesive and / or pigment and / or at least one solvent. When painting, the fluid preferably contains paint, wherein, due to the immersion of the component in the immersion tank or in the fluid, the paint can be applied to the component, in particular to the surface. The coating is preferably provided as a corrosion protection for the component, in particular for the surface. The method can be referred to in particular as a method for coating the surface of a component.

[0011] In order to be able to improve the curing, in particular chemical crosslinking, of the coating applied to the surface of the component in particular, it is provided according to the invention that at least one catalyst for curing the coating during drying, in particular for chemically crosslinking the coating, is applied to the surface of the component in a targeted, in particular local, inhomogeneous distribution, in particular at least indirectly or directly. In other words, in a first sub-region of the surface of the component, a first amount of catalyst is applied to the surface in a targeted, in particular at least indirectly or directly, and in a second sub-region of the surface of the component that is different from the first sub-region, a second amount of catalyst that is different from the first amount and preferably higher than the first amount is applied to the surface in a targeted, in particular directly. This means that when the coating is dried, in particular immediately at the beginning of drying of the coating, the catalyst is located on the surface, in particular on or in the coating, in particular locally inhomogeneously distributed. Therefore, the catalyst is applied to the surface of the component in a targeted, in particular local, inhomogeneous distribution, in particular at least indirectly or directly, so that when drying or immediately at the beginning of drying of the coating, the first amount of catalyst is located in the first sub-region of the surface, in particular on or in the coating, and the second amount of catalyst is located in the second sub-region of the surface, in particular on or in the coating. In other words again, the catalyst is applied to the surface of the component in a targeted manner so that the local distribution of the concentration of the catalyst on the surface, in particular on or in the coating, is not constant and is therefore in particular locally variable or locally changing. Thus, for example, a first concentration of catalyst is present on a first sub-region of the surface, in particular in or on the coating, and a second concentration of catalyst, for example different from the first concentration, preferably higher than the first concentration, is present on a second sub-region of the surface, in particular in or on the coating.

[0012] For example, in a first sub-region of the surface of the component, a first amount of catalyst is dissolved in a fluid or applied together with a fluid, in particular at least indirectly or directly, to the surface. The fluid may in particular be referred to as a CTL liquid. For example, the coating already contains the catalyst, which is then applied in a targeted, non-uniformly distributed manner to the surface, in particular in or on the coating, in particular in the form of an additional catalyst amount.

[0013] For example, the catalyst is provided to particularly reduce the temperature, in particular the so-called crosslinking temperature, in order to cause, in particular to initiate, chemical crosslinking of the coating. This means that the curing, in particular the crosslinking, of the coating can be at least partially caused or initiated by the catalyst. For example, the catalyst comprises a bismuth compound. Thus, the catalyst can be particularly referred to as a bismuth catalyst. This means that the material forming the catalyst contains at least one chemical compound formed at least partially of bismuth.

[0014] The present invention is based in particular on the following findings and considerations: During electrophoretic deposition, in particular during cathodic dip coating, a conflict of objectives may occur between the optical properties of the dried coating and the crosslinking speed. The optical properties may be referred to in particular as appearance. After electrophoresis, in particular cathodic deposition, particularly slow drying, in particular crosslinking, of the coating may achieve particularly good optical properties of the coating. For example, a particularly good curing or crosslinking process may be ensured here. This means that, in order to achieve particularly good optical properties, the coating may still be dried as a liquid before the coating is particularly catalytically supported and the time period of the component, for example, in a drying device, in particular, called an oven, may be particularly large. However, particularly long oven times (drying of the component, for example, in a drying device or by means of a drying device during this oven time) may cause particularly low reactivity in the crosslinking of the coating, in particular, called a paint material. The reactivity of the coating, in particular, the paint may be controlled by means of the catalyst used, for example, via its chemical properties and / or via its concentration in the coating. The particularly low reactivity of the coating may have a negative impact on the curing, in particular, crosslinking, of the coating on a sub-region of the surface of the component, in particular, called a critical sub-region, because the critical sub-region may have a particularly slow heating rate, in particular, in a drying device. The critical sub-region can be, for example, the corresponding inner surface of the door sill of a motor vehicle (e.g., an electric vehicle (NCAR)). For example, the critical sub-region of the surface does not reach the temperature or holding time required for the complete curing, especially crosslinking, of the coating, so that in conventional methods, for example, after the drying of the coating, especially the so-called KTL drying operation, the coating cannot be completely cured, and therefore, sufficient corrosion protection cannot exist. In conventional methods, the concentration of the catalyst before and after the deposition of the coating, especially the paint, is usually the same at all positions on the surface of the component. This means that, in conventional methods, the catalyst is not applied to the surface in a targeted unevenly distributed manner, but is evenly or identically distributed. Therefore, in conventional methods, the degree of crosslinking of the coating can mainly depend on the temperature reached during drying. Due to this temperature dependence of the degree of crosslinking in conventional methods, uneven crosslinking can occur at different positions or different sub-regions on the surface of the component, especially with different object temperature curves.

[0015] In contrast, by the method according to the invention, the curing of the coating, in particular the crosslinking, can be particularly improved. By applying the catalyst to the surface of the component in a targeted and unevenly distributed manner, the concentration of the catalyst, in particular the catalyst concentration, can be particularly increased in the coating locally. Thus, for example, a particularly increased catalyst activity can be produced at the component position, for example, at a critical sub-region (which only reaches a particularly low temperature during drying, in particular in a drying device), for a particularly fast curing of the coating, in particular a particularly fast crosslinking. This means that the corresponding amount of the catalyst in the corresponding sub-region can be targeted, in particular, adjusted as required. Thus, the reactivity or the crosslinking speed can be locally targeted and thus particularly particularly increased. Applying a relatively large amount of catalyst to the entire surface of the component will usually have a negative impact on the optical properties, for example, in the form of a corrugation of the coating. This can be avoided by applying the catalyst to the surface in a targeted and unevenly distributed manner. Thus, the optical properties, in particular the surface quality, of the component can be particularly improved. Alternatively, for example, at a position on the surface of the component that is not located in the field of vision of a customer, in particular a motor vehicle, the degradation of the optical properties of the surface can be accepted by the increased catalyst concentration. In particular, the corrosion resistance of the surface of a component can be particularly increased by means of the method according to the invention, which means that the service life of the component can be particularly increased.

[0016] The catalyst can be introduced in pure form or, in particular, dissolved in a suitable solvent or as a suspension, distributed in a targeted, in particular locally inhomogeneously on or in the coating. This means that the catalyst can be introduced selectively into the CTL material. As a result, the catalyst concentration can be increased locally in individual, in particular selected, surface areas of the surface.

[0017] In another embodiment, it is provided that before applying the coating, an unevenly distributed, in particular localized, application of the catalyst to the surface of the component is performed. In other words, the catalyst is applied to the surface of the component in a targeted, unevenly distributed manner before applying the coating. This means that first the catalyst can be applied to the surface in a targeted, unevenly distributed manner, and then the coating can be applied to the surface or to the catalyst. Therefore, before depositing the coating, in particular the KTL paint, the catalyst can be applied to the surface of the component to be coated, in particular as a solution or as a suspension. Thus, the catalyst can be applied to the surface particularly advantageously, in particular with particularly low expenditure. Thus, for example, the manufacturing expenditure of the component, in particular the manufacturing cost, can be kept particularly low.

[0018] Preferably, it is provided that the catalyst is applied in a targeted, unevenly distributed manner directly to the surface of the component, in particular the metal. This means that the catalyst is applied in a targeted, unevenly distributed manner and directly to the surface to be coated before the coating. As a result, the catalyst can be applied to the surface with particularly little effort.

[0019] Alternatively or additionally, it is provided that after the coating is applied, the catalyst is applied in a particularly localized, inhomogeneous distribution. In other words, after the coating is applied, the catalyst is applied to the surface, in particular to the coating, in a targeted, in particular localized, inhomogeneous distribution. This means that the coating is applied to the surface, and then the catalyst is provided to the applied coating. Therefore, after electrophoresis or electrolytic deposition, the catalyst can be applied, for example, as a solution or as a suspension to a coating surface, in particular still wet, in particular on a paint surface. A wet coating surface can be referred to in particular as a "wet CTL". Thus, the catalyst can be applied to the surface particularly advantageously, in particular with particularly little effort. In particular, it can be avoided that the catalyst is detached from the surface during coating the surface with the coating. Therefore, it can be avoided that the catalyst moves away into the immersion tank, and in particular, it can be avoided that the catalyst concentration in the immersion tank accumulates or increases.

[0020] Preferably, provision is made for the component to be immersed in an immersion tank filled with a fluid in order to apply the coating. In other words, the fluid is contained in the immersion tank, wherein the component is at least partially, in particular completely, immersed in the immersion tank or in the fluid, whereby the coating present in the fluid, in particular in liquid form, is applied to the surface of the component. Thus, the fluid is, for example, a mixture comprising the coating. For example, the fluid comprises water or is water.

[0021] It is preferably provided that the catalyst is present in the fluid. This means that the immersion tank is filled with a mixture comprising a fluid and a catalyst. Alternatively, the fluid can be a mixture comprising a catalyst. It is preferably provided that, because the catalyst is present in the fluid, when the coating is applied by immersing the component, in particular the surface of the component, in the fluid, the catalyst is applied to the surface in a first layer, in particular uniformly distributed. In other words, since the component, in particular the surface is immersed in the fluid, the catalyst is applied to the surface in a first layer, wherein the same amount of catalyst is applied in the first and second sub-regions, respectively. This means that the concentration of the catalyst on the surface of the component or in the coating is locally uniformly distributed or constant in the first layer. Again in other words, the coating already includes a catalyst that is in particular uniformly distributed. Thus, the catalyst can be applied to the surface with particularly little expenditure. Therefore, for example, the manufacturing cost of the component can be kept particularly low. Here, the first layer can be understood as referring in particular to the base layer of the catalyst, in particular the base concentration.

[0022] It is preferably provided that the catalyst is applied or introduced onto the surface, particularly onto or into the coating, with a second layer different from the first layer when applied in a particularly locally targeted inhomogeneous distribution. This means that the catalyst is applied onto the surface in a uniform distribution with the first layer and is applied onto the surface of the component in a targeted inhomogeneous distribution with the second layer. In other words, the coating already includes the catalyst, particularly uniformly distributed, with a concentration lower than the second layer, wherein the catalyst is subsequently applied to the second layer to increase the concentration, particularly locally. The first layer can be applied before or after the second layer. The first layer can be referred to as a uniform layer in particular, and the second layer can be referred to as an inhomogeneous layer in particular. The corresponding catalysts applied in the first layer and in the second layer are preferably the same catalyst, i.e. the same catalyst material. This means that the same catalytically active substances are used in the fluid, particularly in the KTL tank material, in the immersion tank as when applied onto the surface in a targeted, inhomogeneous distribution. Thus, the catalyst can be applied onto the surface with particularly little effort. In particular, if the second layer is applied to the surface before the first layer, any, in particular slight, carryover or "bleeding" of the catalyst applied to the surface of the component in the second layer into the fluid when the component is immersed in the immersion tank is not a problem, in particular because the catalyst applied to the surface in the second layer is not a foreign substance since the catalyst used to apply the first layer is present in the fluid.

[0023] Preferably, provision is made for the component, in particular the surface, to be acted upon by a fluid flow, in particular an air flow, in order to dry the coating. In other words, the fluid, in particular the air, flows around or onto the component, in particular the surface, while the coating is drying. As a result, the coating can be cured, in particular crosslinked, particularly well. The fluid flow can be generated, for example, by means of a ventilator of the drying device. The ventilator can in particular be referred to as a blower or fan.

[0024] Preferably, provision is made for the component, in particular the surface, to be heated in order to dry the coating. In other words, heat is supplied to the component, in particular the surface, while the coating is drying. As a result, the coating can be cured, in particular crosslinked, particularly well. For example, the drying device has a heating device, by means of which the component, in particular the surface, can be heated or heated. For example, the component can be heated directly by means of the heating device or the fluid flow can be heated by means of the heating device, whereby the component, in particular the surface, can be heated by means of the heated fluid flow.

[0025] During drying or curing, at least one drying temperature, in particular the curing temperature, and at least one time period can be set, in which the drying or curing takes place. Preferably, in this case, particularly predetermined criteria regarding the drying temperature and the time period are met, which can be understood in particular to mean that the drying temperature and the time period are selected in a targeted manner so that the drying or curing can take place particularly advantageously.

[0026] In another embodiment, it is provided that the component on whose surface a coating applied by electrophoretic deposition, in particular by cathodic dip painting, is dried is constructed as a body-in-white component for a body-in-white of a motor vehicle. This means that the component is a body-in-white component of a body-in-white. Therefore, the method can be understood in particular as a method for bath-treating a body-in-white component. In other words, the coating applied to the surface of the body-in-white component by means of electrophoretic deposition, in particular cathodic dip painting, can be dried. In particular, a catalyst for curing the coating during drying, in particular chemical cross-linking, can be applied to the surface of the body-in-white component in a targeted, in particular local, unevenly distributed, in particular at least indirectly or directly. As a result, the coating applied to the body-in-white component can be cured particularly well. As a result, the corrosion resistance of the body-in-white component can be particularly improved.

[0027] The body-in-white is understood to be in particular a structure of a motor vehicle. The structure is preferably designed as a body of the motor vehicle, in particular a self-supporting body. The body-in-white components can be, for example, components of the body-in-white or in particular components referred to as body components. The body-in-white components, in particular components, can be designed in one piece or in multiple pieces. The motor vehicle is preferably designed as a motor vehicle, in particular a passenger car, a commercial vehicle or a truck.

[0028] Further features of the invention are apparent from the claims, the drawings and the figure description. The features and feature combinations mentioned above in the description and the features and feature combinations mentioned below in the description of the drawings and / or shown alone in the drawings can be used not only in the respectively given combination but also in other combinations or alone. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] The invention will now be explained in more detail with the aid of preferred embodiments and with reference to the accompanying drawings. In the drawings:

[0030] Figure 1 A schematic flow chart showing a method according to the present invention; and

[0031] Figure 2 shows a schematic front view of a component which is provided for immersion treatment by means of the method according to the invention; and

[0032] Figure 3 The schematic partial sectional view shows a component and an immersion tank which are provided for an immersion treatment by means of the method according to the invention.

[0033] In the figures, identical or functionally identical elements are provided with the same reference symbols. DETAILED DESCRIPTION

[0034] Figure 1A schematic process diagram of a method for immersion treatment 1 of a component 2 is shown. Figure 2 A schematic front view of a component 2 is shown.

[0035] In the method, provision is preferably made for the coating 5 to be applied, in particular directly, to the surface 4 of the component 2 by electrophoretic deposition 3, in particular by cathodic dip coating (CTL). The coating 5 is preferably applied to the surface 4 by an immersion process. Preferably, the component 2, in particular the surface 4, is immersed in an immersion tank 7 filled with a fluid 6 in order to apply the coating 5. Figure 3 The component 2 is shown in a schematic partial sectional view immersed in an immersion tank 7 filled with a fluid 6 .

[0036] The coating 5 applied to the surface 4 of the component 2 by means of electrophoretic deposition 3 , in particular by means of cathodic dip coating, is dried, for example, by means of a drying device. This may be referred to in particular as drying 8 of the coating 5 .

[0037] In order to improve the curing 9, in particular the chemical crosslinking, of the coating 5 applied to the surface 4, it is provided that the catalyst 10 is applied to the surface 4 of the component 2 in a targeted, non-uniformly distributed manner in order to cure 9, in particular crosslink the coating 5 during drying 8. This means, for example, that a first amount of catalyst is applied to a first sub-region 11 of the surface 4 of the component 2 and a second amount of catalyst, which is different from the first amount, is applied to a second sub-region of the surface 4 of the component 2, which is different from the first sub-region 11. Thus, during the drying 8 of the coating 5 or immediately at the beginning of the drying 8 of the coating 5, for example, the first amount of catalyst 10 is present in the first sub-region 11 and the second amount of catalyst 10 is present in the second sub-region 12. Thus, by selective use of catalysts, in particular by a non-uniform distribution of catalysts, the curing 9 or crosslinking of the coating 5, in particular, can be optimized. Thus, for example, surface locations that only reach particularly low temperatures during drying can have, for example, a particularly high catalyst concentration, thereby being able to bring about particularly rapid crosslinking of the coating 5, in particular locally. Thus, particularly good, particularly uniform curing 9, in particular crosslinking of the coating 5 can be achieved. In this way, the corrosion resistance of the component 2 , in particular of the surface 4 , can be increased in particular.

[0038] The sub-regions 11, 12 can adjoin one another at least indirectly, in particular directly. The sub-regions 11, 12 can be spaced apart from one another.

[0039] exist Figure 1 In the exemplary embodiment shown, provision is made for an inhomogeneously distributed application of the catalyst 10 to take place after the application of the coating 5, in particular after the electrophoretic deposition 3. The catalyst 10 can thus be introduced in particular directly onto or into the coating 5.

[0040] Alternatively or additionally, provision can be made for an inhomogeneously distributed application of the catalyst 10 to take place before the application of the coating 5. Provision is preferably made here for the catalyst 10 to be applied in a targeted, inhomogeneously distributed manner directly onto the, in particular metallic, surface 4 of the component 2.

[0041] In another embodiment, it is provided that the catalyst 10 is present in the fluid 6, so that when the coating 5 is applied by immersing the component 2, in particular the surface 4, in the fluid 6, the catalyst 10 is applied to the surface 4 in a first layer 13, in particular in a uniform distribution. This means that the first layer 13 of the catalyst 10 is applied to the surface 4 together with the coating 5. This can be understood in particular that the catalyst 10, in particular the first layer 13, is present in the coating 5. When the catalyst 10 is applied to the surface 4 in a targeted inhomogeneous distribution, the catalyst 10 is applied to the surface 4, in particular to the coating 5 or to the first layer 13, in a second layer 14 different from the first layer 13.

[0042] The second layer 14 can be applied to the surface 4 after the first layer 13. The second layer 14 can thus be applied to the first layer 13. Alternatively, the second layer 14 can be applied to the surface 4 before the first layer 13. The first layer 13 and in particular the coating 5 can thus be applied to the second layer 14.

[0043] In another embodiment, it is provided that the component 2, in particular the surface 4, is acted upon by a fluid stream 15 to dry 8 the coating 5. Alternatively or additionally, it can be provided that the component 2, in particular the surface 4, is heated to dry 8 the coating 5. This means that heat 16 is supplied to the component 2, in particular the surface 4, to dry 8 the coating 5.

[0044] For example, the component 2 is designed as a body-in-shell component 17 for a motor vehicle body-in-shell. This means that the component 2, on whose surface 4 a coating 5 applied by electrophoretic deposition 3 is dry-coated, is designed as a body-in-shell component 17 for a motor vehicle body-in-shell. Reference numerals list

[0045] 1. Immersion treatment

[0046] 2 Components

[0047] 3 Electrophoretic deposition

[0048] 4 Surface

[0049] 5. Coating

[0050] 6 Fluid

[0051] 7. Dipping tank

[0052] 8 Drying

[0053] 9. Curing

[0054] 10 Catalyst

[0055] 11 The first sub-area

[0056] 12 Second sub-area

[0057] 13First floor

[0058] 14 Second Floor

[0059] 15 Fluid Flow

[0060] 16 calories

[0061] 17 Body-in-white components

Claims

1. A method for the immersion treatment (1) of a component (2), in which a coating (5) applied to a surface (4) of the component (2) by means of electrophoretic deposition (3) is dried, characterized in that: A catalyst (10) for curing (9) the coating (5) during drying (8) is applied in a targeted, non-uniformly distributed manner to the surface (4) of the component (2).

2. The method according to claim 1, characterized in that The catalyst (10) is applied in an inhomogeneously distributed manner before the coating (5) is applied.

3. The method according to claim 2, characterized in that The catalyst (10) is applied in a targeted, non-uniformly distributed manner directly to the surface (4) of the component (2).

4. The method according to any one of the preceding claims, characterized in that After the coating (5) has been applied, the catalyst (5) is applied in an inhomogeneously distributed manner.

5. The method according to any one of the preceding claims, characterized in that The component (2) is immersed in a dipping tank (7) filled with a fluid (6) to apply the coating (5).

6. The method according to claim 5, characterized in that The catalyst (10) is present in the fluid (6), whereby the catalyst (10) is applied to the surface (4) in a first layer (13) when the coating (5) is applied by immersing the component (2) in the fluid (6), and the catalyst (10) is applied to the surface (4) in a targeted, non-uniformly distributed manner in a second layer (14) that is different from the first layer (13).

7. The method according to any one of the preceding claims, characterized in that The component (2) is impinged with a fluid stream (15) in order to dry (8) the coating (5).

8. The method according to any one of the preceding claims, characterized in that The component (2) is heated to dry (8) the coating (5).

9. The method according to any one of the preceding claims, characterized in that The component (2), on which a coating (5) applied by means of electrophoretic deposition (3) is dried on the surface (4) of the component, is designed as a body-in-shell component (17) for a body-in-shell of a motor vehicle.