Electrostatic chuck with laser machined mesa
The surface roughness of the electrostatic chuck table is adjusted through laser processing technology, which solves the problem of surface roughness control in the existing technology, achieves fast and precise processing effects, is suitable for high temperature environments and is not easy to crack, and improves the cleanliness of processing. and edge control.
Patent Information
- Application Number
- CN202380022517.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-21
- Filing Date
- 2023-02-21
- Publication Date
- 2024-10-01
AI Technical Summary
During the plasma treatment process of existing electrostatic chucks, it is difficult to control the surface roughness of the table accurately and quickly, and traditional methods have problems with poor cleanliness and poor contact area.
The surface roughness of ceramic or metal tabletops is adjusted through laser processing technology to achieve control of surface smoothness or roughness. Dry and precise methods are used for tabletop contour processing, which is suitable for ceramic and metal materials.
It achieves fast and precise tabletop processing, reduces surface stress, improves processing cleanliness and edge contour control, is suitable for high temperature environments and is not prone to cracking, and is suitable for ceramic and metal materials.
Smart Images

Figure CN118743010A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to U.S. Patent Application No. 17 / 700,203, filed on March 21, 2022, the entire contents of which are hereby incorporated by reference. Technical Field
[0003] Embodiments of the present disclosure relate to the field of reactors or plasma processing chambers, and in particular, to electrostatic chucks having laser machined mesas. Background Art
[0004] Processing systems such as reactors or plasma reactors are used to form devices on substrates such as semiconductor wafers or transparent substrates. The substrate is typically held to a support for processing. The substrate may be held to the support by vacuum, gravity, electrostatic forces, or by other suitable techniques. During processing, a precursor gas or gas mixture in the chamber is excited (e.g., energized) into a plasma by applying power, such as radio frequency (RF) power, to electrodes in the chamber from one or more power sources coupled to the electrodes. The excited gas or gas mixture reacts to form a material layer on the surface of the substrate. The layer may be, for example, a passivation layer, a gate insulator, a buffer layer, and / or an etch stop layer.
[0005] In the semiconductor and other industries, an electrostatic chuck (ESC) is used to hold a workpiece (e.g., a substrate) on a support during processing of the substrate. A typical ESC may include a base, an electrically insulating layer disposed on the base, and one or more electrodes embedded in the electrically insulating layer. The ESC may be equipped with an embedded electric heater, and a fluid coupled to a heat transfer gas source for controlling the substrate temperature during processing. During use, the ESC is fastened to a support in a processing chamber. The electrodes in the ESC are electrically biased relative to the substrate disposed on the ESC by a voltage source. Opposite electrostatic charges accumulate in the electrodes of the ESC and on the surface of the substrate, and the insulating layer prevents the charge from flowing therebetween. During substrate processing, the electrostatic force generated by the electrostatic charge accumulation holds the substrate to the ESC. Summary of the invention
[0006] Embodiments of the present disclosure include an electrostatic chuck (ESC) for use in a reactor or plasma processing chamber and methods of making the ESC.
[0007] In an embodiment, a method of manufacturing a substrate support assembly includes providing a ceramic top plate having a top surface having a processing region. A plurality of mesas are formed within the processing region and on the top surface of the ceramic plate. Laser processing of one or more of the plurality of mesas is performed to reduce surface roughness of the one or more of the plurality of mesas.
[0008] In an embodiment, a method of manufacturing a substrate support assembly includes providing a ceramic top plate having a top surface having a processing region. A plurality of mesas are formed within the processing region and on the top surface of the ceramic plate. Laser processing of one or more of the plurality of mesas is performed to increase the surface roughness of the one or more of the plurality of mesas.
[0009] In an embodiment, the substrate support assembly includes a ceramic top plate having a top surface having a processing region. One or more DC braze joints are located within the ceramic top plate. One or more electrodes are located within the ceramic top plate. A plurality of mesas are located within the processing region and on the top surface of the ceramic plate. One or more mesas are laser processed mesas. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] 1A illustrates a plan view and corresponding enlarged view of a top surface of an electrostatic chuck (ESC) according to an embodiment of the present disclosure.
[0011] 1B illustrates a cross-sectional view of a method of reducing mesa surface roughness by laser machining according to an embodiment of the present disclosure.
[0012] 1C illustrates a cross-sectional view of a method of increasing the surface roughness of a mesa by laser processing according to an embodiment of the present disclosure.
[0013] 2A illustrates a cross-sectional view of an electrostatic chuck (ESC) including a mesa at different locations according to an embodiment of the present disclosure.
[0014] 2B illustrates a cross-sectional view of another electrostatic chuck (ESC) including a mesa at a different position according to another embodiment of the present disclosure.
[0015] 2C illustrates a cross-sectional view of another electrostatic chuck (ESC) including a mesa at a different position according to another embodiment of the present disclosure.
[0016] 3 illustrates a cross-sectional view of an electrostatic chuck (ESC) according to an embodiment of the present disclosure.
[0017] 4 is a schematic cross-sectional view of a processing chamber including a substrate support assembly according to an embodiment of the present disclosure.
[0018] 5 is a partial schematic cross-sectional view of a processing chamber including a substrate support assembly according to an embodiment of the present disclosure.
[0019] FIG. 6 illustrates a block diagram of an exemplary computer system according to an embodiment of the present disclosure. DETAILED DESCRIPTION
[0020] An electrostatic chuck (ESC) for a plasma processing chamber and a method of making an ESC are described. In the following description, numerous specific details are set forth, such as electrostatic chuck components and material systems, in order to provide a thorough understanding of embodiments of the present disclosure. It will be apparent to one skilled in the art that embodiments of the present disclosure may be practiced without these specific details. In other cases, well-known aspects such as plasma enhanced chemical vapor deposition (PECVD) or plasma enhanced atomic layer deposition (PEALD) processes are not described in detail so as not to unnecessarily obscure embodiments of the present disclosure. Furthermore, it should be understood that the various embodiments shown in the figures are exemplary representations and are not necessarily drawn to scale.
[0021] One or more embodiments relate to laser machining of a mesa to produce surface smoothness or to produce surface roughness. Embodiments may include a dry and clean method for making a mesa on top of a ceramic or metal base. In one embodiment, the method described herein provides a fast, accurate method that can be programmed to be repeated. In one or more embodiments, the mesa profile is laser machined.
[0022] To provide context, it may be beneficial to render some surface roughness and profile to the countertop on top of the pedestal. This may involve ceramic or metal edge profile machining and surface roughness (Ra) control. Previous methods have involved polishing, but these may not be as clean.
[0023] Advantages of implementing the embodiments described herein and / or properties of the embodiments described herein may relate to one or more of the following: (1) applications for minimal contact area polishing or roughening; (2) possibility of processing only certain mesas; (3) very fast processing, e.g., seconds per mesa; (4) very clean processing compared to slurry processing; (5) edges can be contoured to remove sharp corners, thereby providing a small number of particles on the wafer; (6) the laser spot can be adjusted; and / or (7) suitability for processing ceramics, such as alumina or AlN.
[0024] In one embodiment, the table is first manufactured to have a surface roughness (Ra) determined by the table manufacturing process (e.g., using sandblasting). The edge of the table is trimmed using a laser to obtain the target profile and Ra. In one embodiment, the surface of the ESC with a first manufactured table of approximately 1 mm diameter having 8-12 RA or 6-8 Ra is laser processed to provide 1-4 Ra. In another embodiment, the surface of the ESC with a first manufactured table of approximately 1 mm diameter having 1-4 Ra is laser processed to provide 6-8 Ra or 8-12 Ra.
[0025] To provide context, a mesa on the surface of the ESC can be used to support a workpiece, such as being slightly raised from the global top surface of the ESC top plate. In an exemplary embodiment, the mesa coverage can be about 65% of the total surface area of the processing surface, but can be larger or smaller. The mesa can be about 15 microns high, but can be taller or shorter. The diameter of the mesa can be about 1 mm, but can be larger or smaller.
[0026] The ESC surface can have a mesa fabricated on the top surface, for example, by grinding or sandblasting. Such a mesa can be described as being continuous with the top surface of the ceramic top plate. The mesa can be formed into the ceramic surface or can be particles, such as diamond particles, added to the ceramic surface. FIG. 1A illustrates a plan view and a corresponding enlarged view 150 of the top surface of an electrostatic chuck (ESC) according to an embodiment of the present disclosure.
[0027] Referring to FIG. 1A , the top surface 102 of the ESC 100 includes an outer region 104 surrounding an inner region 106. The top surface 102 can be a ceramic surface, such as aluminum nitride on an aluminum oxide surface. The inner region 106 can include a processing region 107 having electrode wiring 108 therein (e.g., slightly below the surface of the ceramic). The electrode wiring 108 can be, for example, an electrostatic electrode of the ESC 100. The processing region 107 can also include a DC brazing joint location 110, such as slightly below the surface of the ceramic. A plurality of mesas 112 are made in the surface of the processing region 107. In one embodiment, one or more of the mesas 112 are laser machined mesas, as described below.
[0028] 1B illustrates a cross-sectional view of a method of reducing mesa surface roughness by laser machining according to an embodiment of the present disclosure.
[0029] Referring to FIG1B , a method of manufacturing a substrate support assembly includes providing a ceramic top plate having a top surface having a processing region. A plurality of mesas (e.g., mesas 160) are formed within the processing region and on the top surface of the ceramic plate. Laser processing of one or more of the plurality of mesas is performed to reduce the surface roughness of one or more of the plurality of mesas, for example, to form mesas 170. In one embodiment, reducing the surface roughness includes reducing from between 8-12 microns Ra to between 1-4 microns Ra. In one embodiment, reducing the surface roughness of one or more of the plurality of mesas includes forming fillets on one or more of the plurality of mesas, as shown in FIG1B .
[0030] It should be understood that, depending on the clamping needs or clamping behavior, it may not be optimal to reduce the table surface roughness by laser machining all tables of the ESC. In one embodiment, one or more tables (type 170) of the plurality of tables include less than all tables (type 160) of the plurality of tables, leaving both types 160 and 170 on the ESC surface.
[0031] In one embodiment, the plurality of mesas are continuous with the top surface of the ceramic top plate. In one embodiment, the ceramic top plate comprises aluminum nitride. In one embodiment, the ceramic top plate comprises aluminum oxide. In one embodiment, the method further comprises forming one or more electrodes in the ceramic top plate.
[0032] 1C illustrates a cross-sectional view of a method of increasing the surface roughness of a mesa by laser processing according to an embodiment of the present disclosure.
[0033] Referring to FIG1C , a method of manufacturing a substrate support assembly includes providing a ceramic top plate having a top surface having a processing region. A plurality of mesas (e.g., mesas 180) are formed within the processing region and formed on the top surface of the ceramic plate. Laser processing of one or more of the plurality of mesas is performed to increase the surface roughness of one or more of the plurality of mesas, for example, to form mesas 190. In one embodiment, increasing the surface roughness includes increasing from between 1-4 microns Ra to between 8-12 microns Ra. In one embodiment, increasing the surface roughness of one or more of the plurality of mesas includes forming sharp corners on one or more of the plurality of mesas, as shown in FIG1C .
[0034] It should be understood that, depending on the clamping needs or clamping behavior, increasing the surface roughness of the mesas by laser machining all mesas of the ESC may not be optimal. In one embodiment, one or more mesas of the plurality of mesas (type 190) include only less than all mesas of the plurality of mesas (type 180), leaving both types 180 and 190 on the ESC surface.
[0035] In one embodiment, the plurality of mesas are continuous with a top surface of the ceramic top plate. In one embodiment, the ceramic top plate comprises aluminum nitride. In one embodiment, the ceramic top plate comprises aluminum oxide. In one embodiment, the method further comprises forming one or more electrodes within the ceramic top plate.
[0036] It should be understood that any suitable laser processing may be used to laser process the mesa according to the embodiments described herein. For example, a nanosecond-based laser processing, a picosecond-based laser processing, or a femtosecond-based laser processing may be used.
[0037] In one embodiment, a Gaussian laser beam is used to laser process the table, however, non-Gaussian beams may also be used. Furthermore, the beam may be stationary or rotating. In one embodiment, a femtosecond-based laser is used as the source for the laser processing. For example, in one embodiment, a laser with a wavelength in the visible spectrum plus the ultraviolet (UV) and infrared (IR) ranges (total broadband spectrum) is used to provide a femtosecond-based laser, i.e., a pulse width of the order of femtoseconds (10 -15 seconds) of laser.
[0038] In the case where the laser beam is a femtosecond based laser beam, in one embodiment, the pulse width of the femtosecond laser source is approximately in the range of 10 femtoseconds to 500 femtoseconds, but preferably in the range of 100 femtoseconds to 400 femtoseconds. In one embodiment, the wavelength of the femtosecond laser source is approximately in the range of 1570 nanometers to 200 nanometers, but preferably in the range of 540 nanometers to 250 nanometers. In one embodiment, the laser and corresponding optical system provide a focal point at the working surface in the range of approximately 3 micrometers to 15 micrometers, but preferably in the range of approximately 5 micrometers to 10 micrometers or between 10-15 micrometers.
[0039] In one embodiment, the laser source has a pulse repetition rate in the range of about 200kHz to 10MHz, although preferably in the range of about 500kHz to 5MHz. In one embodiment, the laser source delivers a pulse energy in the range of about 0.5uJ to 100uJ at the work surface, although preferably in the range of about 1uJ to 5uJ. In one embodiment, the laser scribing process is run along the workpiece surface at a speed in the range of about 500mm / sec to 5m / sec, although preferably in the range of about 600mm / sec to 2m / sec.
[0040] The table laser machining process can be run only once (single pass) or multiple passes are allowed, but in one embodiment, it is preferably run 1-2 times. In one embodiment, the laser machining depth in the workpiece is approximately in the range of 5 microns to 50 microns, preferably approximately in the range of 10 microns to 20 microns. In one embodiment, the kerf width of the generated laser beam is approximately in the range of 2 microns to 15 microns.
[0041] In another aspect, one or more embodiments relate to reducing surface stress in an electrostatic chuck (ESC) by table machining, contouring, and ESC material design. Embodiments may include ESC table machining and top material structure design. In one embodiment, one or more tables are laser machined tables.
[0042] To provide context, in the past and in state-of-the-art implementations, mesas are typically placed at a number of locations, including locations based on high stress areas on the ESC surface. Placement in such high stress areas may cause cracking of the top surface of the ESC due to high stress and / or thermal stresses in defective areas.
[0043] According to one or more embodiments of the present disclosure, the table processing and contour configuration of the top ESC material and design are implemented for surface stress reduction. The advantages of implementing one or more embodiments described herein may include the target position of the table, the improved contour of the ESC top surface. The embodiments described herein can be implemented to enable the use of the ESC without cracking due to thermal shock on the top surface at temperatures above 500C. The embodiments described herein can be implemented to remove or alleviate ESC thermal shock stress cracking. In one embodiment, one or more table tops are laser processed table tops, such as described herein.
[0044] To provide exemplary context, referring again to FIG. 1A , and in particular to enlarged view 150, the plurality of mesas 112 include mesas located in a number of locations, including benign regions, and also include mesas 112A located in a region above the region of the DC braze joint location 110. It has been determined that mesas 112A in a region above the region of the DC braze joint location 110 places mesas 112A in a high stress region.
[0045] 2B illustrates a cross-sectional view of an electrostatic chuck (ESC) including a mesa in different locations according to an embodiment of the present disclosure.
[0046] 2A, ESC 200 includes a central region 202, a main region 204, a DC rod 206, and an ESC grid 208. As shown, the DC rod 206 can be located at a central location 210. ESC 200 also includes mesas, such as mesas 212A, 212B, 212C, and 212D. Mesas 212A is above the high voltage connection area 210, such as above the DC rod 206. Mesas 212B is above the electrode edge. Mesas 212C is in an electrode-free region. Mesas 212D is completely above the electrode. Mesas 212A, 212B, 212C, and 212D are relatively shallow from the ESC grid 208. In one embodiment, one or more of the mesas are laser processed mesas, such as described herein.
[0047] Referring again to FIG. 2A , the surface of the ESC may include a stress distribution including high stress areas and low stress areas on the top surface based on its manufacturing features. Some high stress areas are caused by the presence of high voltage electrodes approximately 1 mm below the top surface. For example, high stress may exist at (A) the boundary of the edge of the positive or negative polarity electrode, (B) above the brazed connection, and / or at the edge of the ESC. According to an embodiment of the present disclosure, a mesa structure is included above the low stress area but not included above the high stress area. For example, mesas 212A and 212B are in high stress positions, while mesas 212C and 212D are in low stress areas. In one embodiment, the mesa is included in positions 212C and / or 212D but not in positions 212A or 212B. In one embodiment, one or more mesas are laser processed mesas, such as described herein.
[0048] In another aspect, the most advanced ESC surface can have a profile after machining and / or polishing the top surface. The profile can have a bump in the center of the ESC. The size of such a bump in the center can be about 10-20 microns, and there is a 15-micron table after the profile, as shown in FIG. 2B, as described below. When the wafer is placed on the ESC, it can have different contact points. The bump in the center causes the wafer to not contact the table near the center. According to one or more embodiments of the present disclosure, for a given table height, the specification of the vertical (topographic feature) amplitude of the surface relative to the horizontal distance is determined. Heat transfer between the wafer and the ESC and heat transfer from the plasma to the wafer via gas coupling to the ESC can control the wafer temperature in this area. When only the central bump is polished, the wafer can produce a concave contact area with all the table, and the heat transfer is uniform. In one embodiment, before creating the table, the flatness profile is measured on the surface of the ESC and the table is not formed at a position where the vertical slope (e.g., 15 microns / 10mm) is not met. In one embodiment, at the position where the table is formed, one or more table is a laser-processed table, such as described herein.
[0049] 2B illustrates a cross-sectional view of another electrostatic chuck (ESC) including a mesa at a different position according to another embodiment of the present disclosure.
[0050] Referring to FIG. 2B , the support surface topography 250 may include a mesa profile 254 above a ceramic top surface profile 252. The ceramic top surface profile 252 may have a center high point 252A and an edge location 252B. The mesa profile 254 may show grinding locations 256A and 256B having a high center point. A mesa 262 is on the ceramic top surface profile 252. In one embodiment, after determining that the center point is a high point, the center location does not form a mesa 262A. As a result, the wafer profile (dashed line 258) is not formed on the high point of the mesa profile 254, which would otherwise include a mesa 262A. In one embodiment, in the locations where the mesa is formed, one or more of the mesas are laser machined mesas, such as described herein.
[0051] In one embodiment, the top layer above the high voltage electrode is greater than 1 mm and less than 3 mm thick to strengthen the top surface and reduce the surface stress of the AlN ESC. In one embodiment, the brazed high voltage connection is 2-4 mm from the top surface to reduce stress. In one embodiment, the top layer above the electrode is composed of high resistivity and high thermal shock resistance. In one embodiment, the microstructure design provides thermal shock resistance of 400C or higher.
[0052] Referring again to FIGS. 1A, 1B, 1C, 2A, and / or 2B, according to one embodiment of the present disclosure, a substrate support assembly includes a ceramic top plate having a top surface having a processing region. One or more DC braze joints are located within 1-2 mm of the surface of the ceramic top plate. A plurality of mesas are located within the processing region and on the top surface of the ceramic plate. None of the plurality of mesas is vertically located above the one or more DC braze joints. In one embodiment, one or more mesas are laser processed mesas, such as described herein.
[0053] Referring again to FIG. 1A, FIG. 1B, FIG. 1C, FIG. 2A and / or FIG. 2B, according to another embodiment of the present disclosure, the substrate support assembly includes a ceramic top plate having a top surface having a processing area. The top surface has one or more high-topography areas. A plurality of mesas are located within the processing area and on the top surface of the ceramic plate. None of the plurality of mesas are located above the one or more high-topography areas of the top surface of the processing area or above the edge of the high-voltage electrode. In one embodiment, one or more mesas are laser-processed mesas, such as described herein.
[0054] Referring again to FIGS. 1A, 1B, 1C, 2A, and / or 2B, according to another embodiment of the present disclosure, a substrate support assembly includes a ceramic top plate having a top surface having a processing region. The top surface has one or more high stress regions. A plurality of mesas are located within the processing region and on the top surface of the ceramic plate. None of the plurality of mesas are on the one or more high stress regions of the top surface of the processing region. In one embodiment, one or more mesas are laser processed mesas, such as described herein.
[0055] 2C illustrates a cross-sectional view of an electrostatic chuck (ESC) including a mesa at different locations according to another embodiment of the present disclosure.
[0056] Referring to FIG. 2C , ESC 270 includes a center region 272, a main region 274, a DC rod 276, and an ESC grid 278. As shown, the DC rod 276 can be located at a central location 280. ESC 270 also includes a table, such as table 282A, 282B, 282C, and 282D. Table 282A is above the high voltage connection area 280, such as above the DC rod 276. Table 282B is above the electrode edge. Table 282C is in the electrode-free area. Table 282D is completely above the electrode. The distance between table 282A, 282B, 282C, and 282D and ESC grid 278 is relatively shallow. Unlike FIG. 2A , in one embodiment, the ESC 270 of FIG. 2C includes a molybdenum high voltage electrode grid 278 connected to a brazed nickel rod 276 several millimeters (e.g., 1-4 mm) into the ceramic via a through hole 292 of approximately 0.5 mm through a metal paste 290. In one such embodiment, the arrangement reduces stress on the top while maintaining electrical connection from the nickel rod to the molybdenum grid via a fine paste layer in the horizontal grid plane and in the vertical direction. In one embodiment, the mesa 282D is in a relatively lower stress position than the mesa 212D of FIG. 2A . In one embodiment, one or more of the mesas are laser machined mesas, such as described herein.
[0057] More generally, FIG. 3 illustrates a cross-sectional view of an electrostatic chuck (ESC) according to an embodiment of the present disclosure, as an exemplary fabricated ESC.
[0058] 3 , the ESC 300 includes a ceramic base plate 302 having a heater coil 304 therein. The heater coil 304 may be coupled to a heater connection 305 (it should be understood that in another embodiment, for cast AlN or AlN plate materials used for ESC fabrication, the heater electrode is screen printed). A shaft 306 is coupled to the bottom surface of the ceramic base plate 302. The ESC 300 also includes a ceramic top plate 308. The ceramic top plate 308 has an ESC (clamping) electrode 310 or electrode assembly therein. A layer 312 such as a metal layer or a diffusion bonded layer may be used to bond the ceramic top plate 308 to the top surface of the ceramic base plate 302. A thermocouple 314 extends through an opening 315 in the ceramic base plate 302 and the metal layer 312. A high voltage insulator 316 extends through an opening 315 in the ceramic base plate 302 and the metal layer 312 and accommodates an ESC high voltage connection 318. The surface 399 covered with a table may be a table surface manufactured according to the above-described embodiments. In one embodiment, one or more mesas are laser machined mesas, such as described herein.
[0059] 3, according to an embodiment of the present disclosure, the substrate support assembly 300 includes a ceramic bottom plate 302 having a heater element 304 therein. The substrate support assembly 300 also includes a ceramic top plate 308 having an electrode 310 therein. A metal layer 312 is located between the ceramic top plate 308 and the ceramic bottom plate 302. The ceramic top plate 308 is in direct contact with the metal layer 312, and the metal layer 312 is in direct contact with the ceramic bottom plate 302.
[0060] A standard method of manufacturing an ESC is to join the plates together by hot pressing and then diffusion bond the plates to the shaft. In embodiments without diffusion bonding, the metal layer 312 provides a metal bond in place of a ceramic-to-ceramic diffusion bond that would otherwise change the resistivity of the top ceramic during diffusion bond formation. In one embodiment, the metal layer 312 is a metal foil, such as an aluminum foil. In one such embodiment, the metal layer 312 is an aluminum foil impregnated with about 2% to 20% (e.g., in atomic % of the total foil composition) of Si, with the remainder being aluminum or substantially all aluminum (i.e., the aluminum foil includes silicon at an atomic concentration in the range of 2%–20% of the aluminum foil). In one embodiment, the metal layer 312 is pre-patterned, for example, to include openings 315 and / or additional openings to accommodate lift pins, etc. In one embodiment, the metal layer 312 is an aluminum foil having a thickness in the range of 50-500 microns (and may be approximately 250 microns). In one embodiment, the metal layer 312 is an aluminum foil and is cleaned before being included in the ESC manufacturing process, for example to remove a passivation layer prior to bonding. In one embodiment, the metal layer 312 is an aluminum foil and can withstand corrosion processes, such as chlorine-based processes, without etching or degradation of the metal layer 312 when the ESC is in use. However, if used for non-chlorine-based processes, the metal layer 312 can be composed of a silver-copper alloy, such as with or without the addition of titanium. In one embodiment, the metal layer 312 is bonded to the top plate 308 and the bottom plate 302 at a temperature below 600 degrees Celsius (and more specifically below 300 degrees Celsius). It should be understood that if the metal bonding is performed with a high temperature metal bond (such as silver-copper or gold-nickel) with a temperature far below 1400 degrees Celsius but far above 650 degrees Celsius, a higher ESC use temperature, such as a 650 degree Celsius use temperature, can be used.
[0061] Referring to the ceramic top plate 308 having the ESC (clamping) electrode 310 therein, in one embodiment, the body of the top plate may be formed by sintering a ceramic material, such as aluminum nitride (AlN) or aluminum oxide powder or other suitable material. The RF grid may be embedded in the body. The RF grid may have an electrical connection extending through the bottom surface of the body. The RF grid may include a mesh of molybdenum or other suitable metal material. In one embodiment, the mesh is a mesh of approximately 125 microns in diameter. These materials may be sintered to form a single structure. In one embodiment, the electrode 310 is made of a metal material, such as molybdenum, which may have a thermal expansion coefficient similar to that of the body. In one embodiment, the ceramic top plate 308 is targeted to maintain a temperature below 350 degrees Celsius, such as between 150-300 degrees Celsius, and may include dopants for optimizing operation in such a target temperature range.
[0062] The clamping electrode 310 may include at least a first electrode and a second electrode. During operation, a negative charge may be applied to the first electrode and a positive charge may be applied to the second electrode, or vice versa, to generate an electrostatic force. During clamping, the electrostatic force generated from the electrode holds the substrate disposed thereon in a fixed position. When the power supplied from the power source is turned off, the charge present in the interface between the electrodes may be retained for a long time. In order to release the substrate fixed on the electrostatic chuck, a short pulse power of opposite polarity may be supplied to the electrode to remove the charge present in the interface.
[0063] The electrode assembly may be formed of a metal rod, sheet, bar, foil, and may be preformed, precast, and prefabricated and placed on the surface of an insulating base during manufacture of the electrostatic chuck. Alternatively, a metal deposition process may be performed to deposit and form the electrode assembly directly on the top surface of the insulating base. Suitable deposition processes may include PVD, CVD, electroplating, inkjet printing, rubber stamping, screen printing, or aerosol printing processes. In addition, a metal paste / metal wire may be formed on the top surface of the insulating base. The metal paste / metal wire may initially be a liquid, paste, or metal gel, which may be patterned onto the surface of an object to form electrode fingers having different configurations or sizes on the top surface of the insulating base.
[0064] The ceramic top plate 308 or the ceramic bottom plate 302 may include, but are not limited to, aluminum nitride, glass, silicon carbide, aluminum oxide, yttrium-containing materials, yttrium oxide (Y2O3), yttrium aluminum garnet (YAG), titanium oxide (TiO), or titanium nitride (TiN). Referring to the ceramic bottom plate 302, in one embodiment, the ceramic bottom plate 308 is targeted to maintain a temperature of up to 650 degrees Celsius and may include dopants for optimizing operation in such a target temperature range. In one embodiment, the ceramic bottom plate 302 has an aluminum nitride composition that is different from the aluminum nitride composition of the ceramic top plate 308. The heating element 304 included in the ceramic bottom plate 302 may use any suitable heating technology, such as resistive heating or induction heating. The heating element 304 may be composed of a resistive metal, a resistive metal alloy, or a combination of the two. Materials suitable for the heating element may include materials with high heat resistance, such as tungsten, molybdenum, titanium, etc. In one embodiment, the heating element 304 is composed of molybdenum wire. The heating element 304 may also be fabricated from a material having thermal properties (eg, coefficient of thermal expansion) that substantially matches at least one or both of the aluminum nitride bodies to reduce stress caused by mismatched thermal expansion.
[0065] In one embodiment, a ceramic top plate 308 is fabricated and then bonded to a ceramic bottom plate through a metal layer 312 (which may have included one or more openings patterned therein). In one embodiment, the metal layer 312 is bonded to the ceramic top plate 308 while the metal layer 312 is bonded to the ceramic bottom plate 302. In another embodiment, the metal layer 312 is first bonded to the ceramic top plate 308 and then the ceramic top plate / metal layer 312 pair is bonded to the ceramic bottom plate 302. In another embodiment, the metal layer 312 is first bonded to the ceramic bottom plate 302 and then the ceramic bottom plate / metal layer 312 pair is bonded to the ceramic top plate 308. In any case, in a particular embodiment, the ceramic top plate is formed from sintered aluminum nitride (AlN) or aluminum oxide (Al2O3) powder and a metal mesh.
[0066] In one embodiment, bonding the ceramic top plate 308 to the ceramic bottom plate 302 with the metal layer 312 includes heating the ceramic bottom plate 302, the metal layer 312, and the ceramic top plate 308 to a temperature less than 600 degrees Celsius. In one embodiment, the metal layer 312 is an aluminum foil, and the method includes cleaning a surface of the aluminum foil to remove a passivation layer of the aluminum foil before bonding the ceramic top plate 308 to the ceramic bottom plate 302 with the metal layer 312.
[0067] In another aspect, FIG. 4 is a schematic cross-sectional view of a processing chamber 400 including a substrate support assembly 428 according to an embodiment of the present disclosure. In the example of FIG. 4 , the processing chamber 400 is a plasma enhanced chemical vapor deposition (PECVD) chamber. As shown in FIG. 4 , the processing chamber 400 includes one or more sidewalls 402, a bottom 404, a gas distribution plate 410, and a cover plate 412. The sidewalls 402, the bottom 404, and the cover plate 412 together define a processing volume 406. The gas distribution plate 410 and the substrate support assembly 428 are disposed in the processing volume 406. The processing volume 406 is accessed through a sealable slit valve opening 408 formed through the sidewall 402 so that the substrate 405 can be transferred in and out of the processing chamber 400. A vacuum pump 409 is coupled to the chamber 400 to control the pressure within the processing volume 406.
[0068] The gas distribution plate 410 is connected at its periphery to the cover plate 412. A gas source 420 is coupled to the cover plate 412 to provide one or more gases through the cover plate 412 to a plurality of gas channels 411 formed in the cover plate 412. The gases flow through the gas channels 411 and into the processing volume 406 toward the substrate receiving surface 432.
[0069] The RF power source 422 is coupled to the cover plate 412 and / or directly coupled to the gas distribution plate 410 through the RF feedthrough 424 to provide RF power to the gas distribution plate 410. Various RF frequencies can be used. For example, the frequency can be between about 0.3 MHz and about 200 MHz, such as about 13.56 MHz. The RF return path 425 couples the substrate support assembly 428 to the RF power source 422 via the sidewall 402. The RF power source 422 generates an electric field between the gas distribution plate 410 and the substrate support assembly 428. The electric field causes the gas present between the gas distribution plate 410 and the substrate support assembly 428 to form a plasma. The RF return path 425 completes the circuit for the RF energy, preventing stray plasma from causing RF arcs due to the voltage difference between the substrate support assembly 428 and the sidewall 402. Therefore, the RF return path 425 mitigates arcs that cause process drift, particle contamination, and damage to chamber components.
[0070] The substrate support assembly 124 includes a substrate support 130 and a rod 132. The rod 434 is coupled to a lift system 436, which is adapted to raise and lower the substrate support assembly 428. The substrate support 430 includes a substrate receiving surface 432 for supporting the substrate 405 during processing. Lift pins 438 are movably disposed through the substrate support 430 to move the substrate 405 to and from the substrate receiving surface 432 to facilitate substrate transfer. The actuator 414 is used to extend and retract the lift pins 438. The ring assembly 433 can be placed over the periphery of the substrate 405 during processing. The ring assembly 433 is configured to prevent or reduce unwanted deposition on surfaces of the substrate support 430 that are not covered by the substrate 405 during processing.
[0071] The substrate support 430 may also include a heating and / or cooling element 439 to maintain the substrate support 430 and the substrate 405 disposed thereon at a desired temperature. In one embodiment, the heating and / or cooling element 439 may be used to maintain the temperature of the substrate support 430 and the substrate 405 disposed thereon at less than about 800 degrees Celsius or less during processing. In one embodiment, the heating and / or cooling element 439 may be used to control the substrate temperature to less than 650 degrees Celsius, such as between 300 degrees Celsius and about 400 degrees Celsius. In one embodiment, the substrate support 430 / substrate support assembly 428 is as described above.
[0072] In another aspect, FIG. 5 is a partial schematic cross-sectional view of a processing chamber 500 including a substrate support assembly 300 according to an embodiment of the present disclosure. The processing chamber 500 has a body 501. The body has a sidewall 502, a bottom 504, and a showerhead 512. The sidewall 502, the bottom 504, and the showerhead 512 define an interior space 506. In one embodiment, the substrate support assembly 300 as described above is disposed within the interior space 506. An RF generator 580 may be coupled to an electrode 582 in the showerhead 512. The RF generator 580 may have an associated RF return path 588 for completing an RF circuit when plasma is present. Advantageously, an RF ground path for maintaining plasma may be maintained and a long service life may be provided for the substrate support assembly 300.
[0073] In one embodiment, the semiconductor wafer or substrate supported by the substrate support assembly 300 is composed of a material suitable for undergoing manufacturing processing and a semiconductor processing layer can be appropriately disposed thereon. For example, in one embodiment, the semiconductor wafer or substrate is composed of a Group IV based material, such as but not limited to crystalline silicon, germanium, or silicon / germanium. In an embodiment, the semiconductor wafer includes a single crystal silicon substrate. In one embodiment, the single crystal silicon substrate is doped with impurity atoms. In another embodiment, the semiconductor wafer or substrate is composed of a Group III-V material.
[0074] Embodiments of the present disclosure may be provided as a computer program product or software, which may include a machine-readable medium having instructions stored thereon, which may be used to program a computer system (or other electronic device) to perform embodiments according to the present disclosure. In one embodiment, a computer system is coupled to the processing chamber 400 and substrate support assembly 428 described above in conjunction with FIG. 4 or the processing chamber 500 and substrate support assembly 300 described in conjunction with FIG. 5. Machine-readable media include any mechanism for storing or transmitting information in a form that is readable by a machine (e.g., a computer). For example, machine-readable (e.g., computer-readable) media include machine-readable (e.g., computer) storage media (e.g., read-only memory ("ROM"), random access memory ("RAM"), magnetic disk storage media, optical storage media, flash memory devices, etc.), machine-readable (e.g., computer) transmission media (electrical, optical, acoustic or other forms of propagation signals (e.g., infrared signals, digital signals, etc.)), etc.
[0075] FIG. 6 illustrates a diagrammatic representation of a machine in the exemplary form of a computer system 600, in which a set of instructions can be executed to cause the machine to perform any one or more methods described herein. In alternative embodiments, the machine can be connected (e.g., networked) to other machines in a local area network (LAN), an intranet, an extranet, or an internet. The machine can operate as a server or client machine in a client-server network environment, or as a peer machine in a peer-to-peer (or distributed) network environment. The machine can be a personal computer (PC), a tablet computer, a set-top box (STB), a personal digital assistant (PDA), a cellular phone, a network device, a server, a network router, a switch or a bridge, or any machine capable of executing a set of instructions (sequentially or otherwise) that specify the actions to be taken by the machine. In addition, although only one machine is described, the term "machine" should also be deemed to include any collection of machines (e.g., computers) that execute a set (or multiple sets) of instructions individually or jointly to perform any one or more instructions of the methods described herein.
[0076] The exemplary computer system 600 includes a system processor 602, a main memory 604 (e.g., read-only memory (ROM), flash memory, dynamic random access memory (DRAM) such as synchronous DRAM (SDRAM) or Rambus DRAM (RDRAM)), etc.), a static memory 606 (e.g., flash memory, static random access memory (SRAM), etc.), and an auxiliary memory 618 (e.g., a data storage device) that communicate with each other via a bus 630.
[0077] Processor 602 represents one or more general-purpose processing devices, such as a microprocessor, a central processing unit, and the like. More specifically, processing device 602 may be a complex instruction set computing (CISC) microprocessor, a reduced instruction set computing (RISC) microprocessor, a very long instruction word (VLIW) microprocessor, a microprocessor implementing other types of instruction sets, or a microprocessor implementing a combination of multiple types of instruction sets. Processor 602 may also be one or more specific-purpose processing devices, such as an application-specific integrated circuit (ASIC), a field programmable gate array (FPGA), a digital signal processor (DSP), a network processor, and the like. Processor 602 is configured to execute processing logic 626 to perform the operations described herein.
[0078] The computer system 600 may further include a network interface device 608. The computer system 600 may also include a video display unit 610 (e.g., a liquid crystal display (LCD), a light emitting diode display (LED), or a cathode ray tube (CRT)), an alphanumeric input device 612 (e.g., a keyboard), a cursor control device 614 (e.g., a mouse), and a signal generating device 616 (e.g., a speaker).
[0079] The secondary memory 618 may include a machine-accessible storage medium 632 (or more specifically, a computer-readable storage medium) on which is stored one or more sets of instructions (e.g., software 622) that embody any one or more of the methodologies or functions described herein. The software 622 may also reside completely or at least partially within the main memory 604 and / or within the processor 602 during execution by the computer system 600, the main memory 604 and the system processor 602 also constituting machine-readable storage media. The software 622 may also be transmitted or received over the network 620 via the network interface device 608.
[0080] Although the machine-accessible storage medium 632 is shown as a single medium in the exemplary embodiment, the term "machine-readable storage medium" should be deemed to include a single medium or multiple media (such as centralized or distributed databases, and / or associated caches and servers) that store one or more sets of instructions. The term "machine-readable storage medium" should also be deemed to include any medium that can store or encode a set of instructions for execution by a machine and cause the machine to perform any one or more of the methods of the present disclosure. The term "machine-readable storage medium" should accordingly be deemed to include, but is not limited to, solid-state memories, and optical and magnetic media.
[0081] Thus, an electrostatic chuck (ESC) for use in a reactor or plasma processing chamber and a method of making the ESC have been disclosed.
Claims
1. A method for manufacturing a substrate support assembly, the method comprising the following steps: providing a ceramic top plate having a top surface, the top surface having a processing area; forming a plurality of mesas within the processing area and on the top surface of the ceramic plate; and One or more of the plurality of mesas are laser processed to reduce a surface roughness of the one or more of the plurality of mesas.
2. The method according to claim 1, wherein the step of reducing the surface roughness comprises the following steps: From 8-12 microns Ra to 1-4 microns Ra.
3. The method of claim 1 , wherein the step of reducing the surface roughness of the one or more of the plurality of mesas comprises the steps of: Rounded corners are formed on the one or more mesas of the plurality of mesas. The method of claim 1 , wherein the plurality of mesas are continuous with the top surface of the ceramic top plate. 5 . The method of claim 1 , wherein the one or more of the plurality of mesas include less than all of the plurality of mesas. The method of claim 1 , wherein the ceramic top plate comprises aluminum nitride. The method of claim 1 , wherein the ceramic top plate comprises alumina.
8. The method according to claim 1, further comprising the steps of: One or more electrodes are formed in the ceramic top plate.
9. A method for manufacturing a substrate support assembly, the method comprising the steps of: providing a ceramic top plate having a top surface, the top surface having a processing area; forming a plurality of mesas within the processing area and on the top surface of the ceramic plate; and One or more of the plurality of mesas are laser processed to increase a surface roughness of the one or more of the plurality of mesas.
10. The method of claim 9, wherein the step of increasing the surface roughness comprises the step of increasing from between 1 and 4 microns Ra to between 8 and 12 microns Ra.
11. The method of claim 9, wherein the step of reducing the surface roughness of the one or more of the plurality of mesas comprises the steps of: Sharp corners are formed on the one or more mesas among the plurality of mesas.
12. The method of claim 9, wherein the plurality of mesas are continuous with the top surface of the ceramic top plate.
13. The method of claim 9, wherein the one or more of the plurality of mesas include less than all of the plurality of mesas.
14. The method of claim 9, wherein the ceramic top plate comprises aluminum nitride.
15. The method of claim 9, wherein the ceramic top plate comprises alumina.
16. The method according to claim 9, further comprising the steps of: One or more electrodes are formed in the ceramic top plate.
17. A substrate support assembly comprising: a ceramic top plate having a top surface with a processing area; one or more DC braze joints, the one or more DC braze joints being located within the ceramic top plate; one or more electrodes, the one or more electrodes being located within the ceramic top plate; as well as A plurality of mesas are located within the processing region and on the top surface of the ceramic plate, wherein one or more of the mesas are laser processed mesas.
18. The substrate support assembly of claim 17, wherein none of the plurality of mesas is vertically located above the one or more DC brazed bonds or vertically located above an edge of one of the one or more electrodes.
19. The substrate support assembly of claim 17, wherein the plurality of mesas are continuous with the top surface of the ceramic top plate.
20. The substrate support assembly of claim 17, wherein the ceramic top plate comprises aluminum nitride.
21. The substrate support assembly of claim 17, wherein the ceramic top plate comprises alumina.
22. The substrate support assembly of claim 17, wherein the one or more electrodes comprise molybdenum.