Ammonia nitrogen removal chemical conditioner for alkaline residues

By using ammonia nitrogen removal chemical conditioners in the alkali slag liquid, adjusting the pH and calcium-magnesium ratio, and promoting the precipitation of ammonium and magnesium phosphate, the problems of low ammonia nitrogen removal rate and water pollution in the alkali slag liquid are solved, and rapid and effective alkali treatment is achieved. Slag liquid management.

CN118750854AActive Publication Date: 2024-10-11BEIJING RONGCHUANG GEOTECHNICAL ENG CO LTD
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
CN202410793766.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-19
Publication Date
2024-10-11
Estimated Expiration
2044-06-19

AI Technical Summary

Technical Problem

When the existing technology treats alkali residue liquid with high alkalinity and high salt content, biological methods kill microorganisms, physical methods are ineffective and costly, and chemical methods reduce ammonia nitrogen removal rate in high calcium salt environments, making it difficult to treat quickly. Alkali slag liquid has the risk of dam failure and environmental pollution.

Method used

Provides a chemical conditioner for ammonia nitrogen removal for alkali residues, including an ammonia nitrogen removal component, an excitation component and a chelating component. By adjusting the pH and the calcium-magnesium ratio, it promotes the precipitation of ammonium and magnesium phosphate, rapidly reduces the ammonia nitrogen content, and through The chelating component protects the removal component and avoids water pollution.

Benefits of technology

It achieves rapid ammonia nitrogen removal from alkali residue liquid, improves treatment efficiency, avoids water pollution, and solves the problem of poor denitrification effect of chemical methods in high-calcium and high-salt environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention provides an ammonia nitrogen removal chemical conditioner for alkaline residues, and belongs to the field of industrial solid waste treatment. The chemical conditioner is mainly prepared by uniformly mixing 0.50 to 0.80 part of an ammonia nitrogen removal component, 0.15 to 0.40 part of an excitation component and 0.05 to 0.10 part of a chelating component, and the ammonia nitrogen removal component, the excitation component and the chelating component are mixed uniformly. According to the chemical conditioner, the calcium-magnesium ratio and pH in the alkaline residue liquid are improved, formation of magnesium ammonium phosphate precipitates is promoted, the denitrification speed of the alkaline residue liquid is increased, the problem of denitrification treatment in the alkaline residue liquid through a conventional chemical precipitation method is solved, and rapid treatment of the alkaline residue liquid is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of industrial solid waste treatment, and in particular to a chemical conditioner for removing ammonia nitrogen from alkali residue. Background Art

[0002] Soda ash is one of the important chemical raw materials and is known as the mother of chemical industry. It is widely used in light industry, building materials, chemical industry, food, metallurgy, textile, petroleum, medicine and other fields. The main method of producing soda ash in my country is the ammonia-soda method, which uses ammonia gas to adjust the pH of the solution to absorb carbon dioxide to produce soda ash. However, every ton of soda ash produced will produce 0.3 tons of industrial alkali slag, and 10m3 of alkali slag will be discharged. 3 Alkali slag liquid with excessive ammonia nitrogen content. Since the alkali slag is difficult to dehydrate and use, most alkali-making enterprises adopt the form of building dams to store the difficult-to-manage alkali slag and alkali slag liquid, forming paste-like alkali slag lakes and alkali slag mountains, resulting in a waste of land resources. After years of accumulation, the amount of alkali slag and alkali slag liquid is huge, and there is a risk of dam collapse. With the tightening of environmental protection policies, rapid management is urgently needed.

[0003] Commonly used deamination methods include biological method, physical method and chemical method.

[0004] The biological method mainly uses the nitrification and denitrification of microorganisms to oxidize ammonia nitrogen into nitrite nitrogen, and nitrite is further oxidized into nitrate, and finally nitrate is reduced to nitrogen gas to achieve the purpose of removing ammonia nitrogen. However, the biological method requires the screening of special strains and needs to be carried out under certain water conditions. Alkali slag liquid is a wastewater with high alkalinity and high salt content. Microorganisms will die due to plasmolysis due to water loss in such a high-salt environment. Even for highly salt-tolerant microorganisms, the organic matter content in the alkaline slag liquid is low, and the energy and material sources necessary for the growth of microbial strains are lacking, and they cannot reproduce rapidly. Therefore, the biological method is not suitable for denitrification of alkaline slag liquid.

[0005] Physical methods mainly use air stripping for denitrification. The basic principle of air stripping for treating ammonia nitrogen is that ammonium ions can be converted into free ammonia in an alkaline environment, and then through intense contact between gas and liquid, free ammonia is converted into N2, thereby achieving the purpose of removing ammonia nitrogen. The air stripping method is easy to operate, simple in process, and stable in treatment effect. It is suitable for the pretreatment of high-concentration ammonia nitrogen wastewater and is currently widely used in the industrial treatment of various types of high-concentration ammonia nitrogen wastewater. However, the air stripping method is affected by factors such as pH, temperature, gas-liquid ratio, residence time, and filler in the water body: (1) Air stripping cannot be performed when the temperature is below 0°C; (2) The air stripping method has a poor effect on the treatment of medium and low concentration ammonia nitrogen wastewater, and it is difficult to achieve the standard in one air stripping; (3) The air stripping equipment is prone to filler fouling during actual application. The alkaline slag liquid of the ammonia-alkali method has a low ammonia nitrogen concentration, usually 80-300 mg·L -1, the air stripping effect is not obvious. At the same time, due to the long residence time, the air stripping method is slow to treat the accumulated tens of millions of cubic meters of alkali slag waste liquid. It requires large amounts of equipment and high processing costs in a short period of time.

[0006] Chemical treatment of ammonia nitrogen mainly uses NH4 + With Mg 2+ and PO4 3- The insoluble complex salt MgNH4PO4·6H2O (magnesium ammonium phosphate, commonly known as struvite, is insoluble in water) is formed to achieve the purpose of removing ammonia nitrogen. The magnesium ammonium phosphate precipitate obtained by chemical treatment of ammonia nitrogen wastewater is a slow-release compound fertilizer containing nitrogen, phosphorus, and magnesium. It is used for crops, turning waste into treasure and realizing the rational and effective utilization of resources. This method has a fast and efficient ammonia nitrogen removal speed, but it introduces chloride ions and residual phosphorus while removing ammonia nitrogen, which can easily cause secondary pollution to the environment. The alkali slag liquid contains a large amount of magnesium source and ammonia nitrogen. The application of chemical method to remove ammonia nitrogen has advantages. Only a phosphorus source needs to be added to form struvite precipitate. However, the alkali slag liquid contains a large amount of calcium salts and other metal ions, which will also react with the added PO4 3 -reaction, which reduces the ammonia nitrogen removal rate. Summary of the invention

[0007] In view of this, the present invention provides a chemical conditioner for removing ammonia nitrogen from alkali slag, which can effectively improve the calcium-magnesium ratio and pH in the alkali slag liquid to promote the formation of magnesium ammonium phosphate precipitation, accelerate the denitrification rate of the alkali slag liquid, improve the treatment efficiency, solve the problem of denitrification treatment in the alkali slag liquid by conventional chemical precipitation method, and realize the rapid treatment of the alkali slag liquid.

[0008] The chemical conditioning agent for removing ammonia nitrogen from alkali slag provided by the present invention is characterized by comprising the following components:

[0009] Ammonia nitrogen removal component 0.50-0.80 parts,

[0010] Excitation component 0.15-0.40 parts;

[0011] Chelating component 0.05-0.10 parts.

[0012] Preferably, the ammonia nitrogen removal component is one or more of sodium hypophosphite, sodium phosphate, sodium metaphosphate, polysodium hexametaphosphate, potassium dihydrogen phosphate, and dipotassium hydrogen phosphate.

[0013] Preferably, the exciting component is one or more of sodium carbonate, sodium sulfate, sodium oxalate, sodium acetate, and sodium silicate.

[0014] Preferably, the chelating component is one or more of sodium alginate, ethylenediaminetetraacetic acid, sodium ethylenediaminetetraacetate, citric acid, sodium citrate, ferric citrate, and sodium tartrate.

[0015] In the ammonia nitrogen removal chemical conditioner for alkali slag provided by the present invention, the ammonia nitrogen removal component has good pH compatibility, can effectively provide a phosphorus source, can quickly react with ammonium ions and magnesium ions in the high alkaline environment of the alkali slag, and reduce the ammonia nitrogen content of the alkali slag liquid. The excess phosphorus source can also continue to react with calcium insoluble matter to prevent phosphating pollution of water bodies; the exciting component can effectively react with metal ions such as calcium ions in the solution to produce insoluble matter, play a role in removing ions and assisting the reaction of the ammonia nitrogen removal component, and achieve the effect of strengthening and accelerating the formation of struvite precipitation; the chelating component can chelate high-valent ions in the alkali slag solution, protect the ammonia nitrogen removal component, and improve the calcium-magnesium ratio.

[0016] The present invention also provides a method for preparing an ammonia nitrogen removal chemical conditioner for alkali slag, the specific steps of which are to weigh the raw materials of an ammonia nitrogen removal component, an excitation component and a chelating component according to the above mass ratio, mix them evenly, and thus obtain the ammonia nitrogen removal chemical conditioner.

[0017] According to a specific embodiment of the present invention, in the ammonia nitrogen removal chemical conditioner for alkali slag, mixing is a conventional technical means in the field, and stirring can be performed during the mixing process to make the ammonia nitrogen removal component, the excitation component, and the chelating component mix more fully to prevent local agglomeration.

[0018] According to a specific embodiment of the present invention, in the chemical conditioner for removing ammonia nitrogen from alkali slag of the present invention, there is no specific requirement for the order of adding the ammonia nitrogen removing component, the exciting component and the chelating component, and those skilled in the art can reasonably adjust the order of adding these raw materials according to the needs of on-site operations.

[0019] For example, in a specific embodiment of the present invention, the ammonia nitrogen removal component can be first put into the mixer for mixing, then the chelating component can be put into the mixer for mixing, and finally the exciting component can be put into the mixer for mixing.

[0020] Compared with the prior art, the present invention has the following beneficial effects: the chemical conditioner in the present invention is mainly composed of a uniform mixture of an ammonia nitrogen removal component, an excitation component and a chelating component, which solves the problem of poor chemical denitrification effect in the treatment of high-calcium and high-salt alkali slag, realizes rapid removal of ammonia nitrogen from alkali slag liquid, and avoids water pollution by chemical conditioners. DETAILED DESCRIPTION

[0021] In order to have a clearer understanding of the technical features, purposes and beneficial effects of the present invention, the technical scheme of the present invention is now described in detail in conjunction with the following specific embodiments, but it should not be understood as limiting the applicable scope of the present invention.

[0022] Example 1

[0023] A chemical conditioning agent for removing ammonia nitrogen from alkali slag, comprising the following raw materials:

[0024] Ammonia nitrogen removal components: sodium phosphate, sodium metaphosphate;

[0025] Exciting components: sodium oxalate, sodium acetate;

[0026] Chelating component: ethylenediaminetetraacetic acid. The specific proportions of the raw materials are shown in Table 1.

[0027] Weigh the raw materials according to the above mass, put them into a mixer and mix them until they are evenly mixed to form a powdered chemical conditioner, which is then sealed and stored.

[0028] The prepared chemical conditioner is weighed according to 5‰ of the mass of the alkali slag, mixed with the alkali slag liquid, stirred evenly and then the ammonia nitrogen content is determined.

[0029] Embodiments 2 to 5

[0030] The raw material types, preparation methods and application methods of Examples 2 to 5 are the same as those of Example 1, except that the raw material ratios are changed. The ratios of the raw materials are shown in Table 1:

[0031] Table 1

[0032]

[0033] Example 6

[0034] A chemical conditioning agent for removing ammonia nitrogen from alkali slag, comprising the following raw materials:

[0035] Ammonia nitrogen removal components: sodium phosphate, sodium metaphosphate;

[0036] Exciting components: sodium oxalate, sodium acetate;

[0037] Chelating component: sodium citrate. The specific proportions of the raw materials are shown in Table 2.

[0038] Weigh the raw materials according to the above mass, put them into a mixer and mix them until they are evenly mixed to form a powdered chemical conditioner, which is then sealed and stored.

[0039] The prepared chemical conditioner is weighed according to 5‰ of the mass of the alkali residue, mixed with the alkali residue slurry, stirred evenly and then the ammonia nitrogen content is determined.

[0040] Embodiment 7-8

[0041] The raw material types, preparation methods and application methods of Examples 7 to 8 are the same as those of Example 6, except that the raw material ratios are changed. The ratios of the raw materials are shown in Table 2:

[0042] Table 2

[0043]

[0044]

[0045] Example 9

[0046] A chemical conditioning agent for removing ammonia nitrogen from alkali slag, comprising the following raw materials:

[0047] Ammonia nitrogen removal components: sodium phosphate, sodium hypophosphite;

[0048] Exciting components: sodium oxalate, sodium acetate;

[0049] Chelating component: sodium citrate. The specific proportions of the raw materials are shown in Table 3.

[0050] Weigh the raw materials according to the above mass, put them into a mixer and mix them until they are evenly mixed to form a powdered chemical conditioner, which is then sealed and stored.

[0051] The prepared chemical conditioner is weighed according to 5‰ of the mass of the alkali residue, mixed with the alkali residue slurry, stirred evenly and then the ammonia nitrogen content is determined.

[0052] Embodiments 10 to 11

[0053] The raw material types, preparation methods and application methods of Examples 10 to 11 are the same as those of Example 9, except that the raw material ratios are changed. The ratios of the raw materials are shown in Table 3:

[0054] Table 3

[0055]

[0056] Comparative Example 1

[0057] Weigh sodium phosphate according to 5‰ of the mass of the alkali slag, mix it with the alkali slag slurry, stir it evenly and then determine its ammonia nitrogen content.

[0058] The results of adding the chemical conditioning agents of Examples 1-11 and Comparative Example 1 to the flocculation sedimentation time and volume sedimentation rate are shown in Table 4.

[0059] Table 4

[0060]

[0061]

[0062] The above description is only an illustrative embodiment of the present invention and is not intended to limit the scope of the present invention. The components of the present invention can be combined with each other without conflict, and any equivalent changes and modifications made by any technician in the field without departing from the concept and principle of the present invention should fall within the scope of protection of the present invention.

Claims

1. A chemical conditioner for removing ammonia nitrogen from alkali residue, characterized in that: The composition comprises the following components in parts by weight: Ammonia nitrogen removal component 0.50-0.80 parts, Excitation component 0.15-0.40 parts; Chelating component 0.05-0.10 parts.

2. The chemical conditioner for removing ammonia nitrogen from alkali residue according to claim 1, characterized in that: The ammonia nitrogen removal component is one or more of sodium hypophosphite, sodium phosphate, sodium metaphosphate, polysodium hexametaphosphate, potassium dihydrogen phosphate, and dipotassium hydrogen phosphate.

3. The chemical conditioner for removing ammonia nitrogen from alkali residue according to claim 1, characterized in that: The exciting component is one or more of sodium carbonate, sodium sulfate, sodium oxalate, sodium acetate and sodium silicate.

4. The chemical conditioner for removing ammonia nitrogen from alkali residue according to claim 1, characterized in that: The chelating component is one or more of sodium alginate, ethylenediaminetetraacetic acid, sodium ethylenediaminetetraacetate, citric acid, sodium citrate, ferric citrate and sodium tartrate.

5. The method for preparing the ammonia nitrogen removal chemical conditioner for alkali residue according to any one of claims 1 to 4, characterized in that: The raw materials of the ammonia nitrogen removal component, the exciting component and the chelating component weighed according to the above mass parts are mixed evenly to prepare the ammonia nitrogen removal chemical conditioner.

Citation Information

Patent Citations

  • Fine chemical waste water treating agent for efficiently removing ammonia nitrogen

    CN103896380A

  • Denitrification, desalination and recycling process of stainless steel cold rolling acidic waste water

    CN104058548A

  • Red-mud citric acid dealkalizing technique

    CN105170307A

  • Industrial wastewater treating agent

    CN106745350A

  • High-calcium high-salt sewage denitrification carbon source

    CN107777790A