ESC electrostatic chuck manufacturing process and ESC electrostatic chuck
By doping T I titanium metal material and Y2O3 in the electrostatic chuck manufacturing process, an aluminum nitride ceramic surface layer and tungsten electrode layer structure with high thermal conductivity and low leakage current is formed, which solves the problem of uneven temperature and poor adsorption effect of the electrostatic chuck. problem, significantly improving the etching accuracy.
Patent Information
- Application Number
- CN202410667995.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-28
- Publication Date
- 2024-10-11
AI Technical Summary
The existing electrostatic chuck has uneven temperature, poor thermal conductivity, and poor adsorption effect, resulting in low etching accuracy.
An ESC electrostatic chuck manufacturing process including mixing, casting, tungsten slurry electrode printing, debinding, sintering molding, assembly and testing is adopted, mixed with TI titanium metal material and Y2O3, to form an electrostatic chuck with high thermal conductivity and low leakage current. Aluminum nitride ceramic surface layer and tungsten electrode layer structure.
The thermal conductivity and adsorption effect of the chuck are improved, and the etching accuracy is improved. The thermal conductivity can reach 170W/M·K, the leakage current is low, and the adsorption effect is significantly improved.
Smart Images

Figure CN118754615A_ABST
Abstract
Description
[Technical field]
[0001] The invention relates to the technical field of electrostatic chuck products in a semiconductor manufacturing process, and in particular to an ESC electrostatic chuck manufacturing process. [Background Technology]
[0002] At present, the carrying device used to carry wafers in semiconductor processing equipment is generally an electrostatic chuck (ESC). An electrostatic chuck is a device that uses electrostatic adsorption to fix the wafer, while controlling the surface temperature of the wafer and providing a DC bias for the wafer. Compared with a mechanical chuck, an electrostatic chuck reduces the probability of wafer damage due to pressure, collision, etc., while increasing the effective processing area of the wafer and reducing the deposition of particles and by-products on the wafer surface. Compared with a vacuum chuck, an electrostatic chuck can work in a vacuum environment. Due to the above advantages, an electrostatic chuck is currently widely used in integrated circuit (IC) manufacturing, especially in plasma etching (ETCH), physical vapor deposition (PVD), chemical vapor deposition (CVD) and other processes.
[0004] The principle is to use electrostatic adsorption to adsorb the chip to be processed to its surface, so that the chip remains flat to prevent deformation during the process, and the temperature of the chip surface can be controlled by back-blowing gas. It is mainly used in chip manufacturing: diffusion, thin film deposition, photolithography, etching, and ion implantation processes.
[0005] The development of electrostatic chucks is difficult, with extremely high technical barriers, and involves the combination of various disciplines, resulting in high R&D costs. The equipment used for R&D is all independently designed and customized, and is restricted by foreign countries.
[0006] The key and difficulty of the electrostatic chuck lies in the temperature control of aluminum nitride with circuit and the welding of metal and aluminum nitride ceramic.
[0007] In the specific product classification, electrostatic chucks are mainly divided into three types: high temperature / low temperature / normal temperature.
[0008] The problems existing in the prior art are: uneven chuck temperature, resulting in low etching accuracy, poor chuck thermal conductivity, and poor adsorption effect. Based on this, how to improve the adsorption performance of the chuck and improve the etching accuracy is a problem considered by technical personnel in this field. [Summary of the invention]
[0009] The problems existing in the prior art solved by this application are:
[0010] The uneven temperature of the chuck results in low etching accuracy, poor thermal conductivity of the chuck, and poor adsorption effect. Based on this, how to improve the adsorption performance of the chuck and improve the etching accuracy is a problem considered by technical personnel in this field.
[0011] The solution to the technical problem of the present invention is:
[0012] Provided is an ESC electrostatic chuck manufacturing process, comprising the following steps:
[0013] S1: mixing; S2: casting; S3: tungsten slurry electrode printing; S4: debinding; S5: sintering; S6: assembly; S7: testing; S8: preparation completed;
[0014] In the sintering process of step S5, TI titanium metal material is doped in an amount of 6-15% (by weight); and Y2O3 is doped in an amount of 4-5% (by weight).
[0015] Preferably, the doping amount of Y2O3 is 4.5%.
[0016] Preferably, an ESC electrostatic chuck is manufactured using the manufacturing process as described above; and comprises a first aluminum nitride ceramic surface layer, a tungsten electrode layer and a second aluminum nitride ceramic surface layer which are sequentially arranged and used to support a wafer; the tungsten electrode layer is a two-layer structure symmetrically arranged on the left and right; and dot protrusions with a diameter size range of 40-60nm are densely arranged on the surface of the first aluminum nitride ceramic surface layer.
[0017] Preferably, the diameter of the dot protrusions is 50 nm.
[0018] Preferably, the ESC electrostatic chuck further comprises a temperature control functional layer and a base for arranging the first aluminum nitride ceramic surface layer, the tungsten electrode layer, the second aluminum nitride ceramic surface layer and the temperature control functional layer; the base is matched and connected with an external process chamber.
[0019] Preferably, an ESC electrostatic chuck is manufactured using the manufacturing process as described above; it includes a positioning plate; the positioning plate has an aluminum nitride ceramic chuck surface; at least one circumferential air groove, a plurality of radial air grooves and a plurality of split air grooves are provided on the aluminum nitride ceramic chuck surface; a central through hole for connecting with a gas source is provided at the center of the aluminum nitride ceramic chuck surface; the circumferential air grooves are centered on the central through hole and diffuse toward the edge of the aluminum nitride ceramic chuck surface; the radial air grooves extend from the circumferential air grooves close to the central through hole to the edge of the aluminum nitride ceramic chuck surface; some of the radial air grooves are connected to the central through hole; and it also includes magnetron sputtered T IN dots with a diameter of 2 nm densely arranged on the surface of the aluminum nitride ceramic chuck surface.
[0020] Preferably, the color of the TiN is brown, and the ethylene content is increased during PVD sputtering, so that the dots after sputtering are harder and more wear-resistant.
[0021] Preferably, the ESC electrostatic chuck further comprises a temperature control functional layer and a base for arranging the aluminum nitride ceramic surface layer, the adsorption electrode layer and the temperature control functional layer; the base is matched and connected with the external process chamber.
[0022] Preferably, an ESC electrostatic chuck is manufactured using the manufacturing process as described above; it includes a positioning plate; the positioning plate has an aluminum nitride ceramic surface layer for supporting a wafer and an adsorption electrode layer; the adsorption electrode layer includes an adsorption electrode unit that is symmetrically arranged on the left and right; the adsorption electrode layer is a two-piece symmetrical adsorption electrode; the adsorption electrode unit has a semicircular structure.
[0023] Preferably, at least one circumferential air groove, several radial air grooves and several dividing air grooves are provided on the aluminum nitride ceramic surface layer; a central through hole for connecting with the air source is provided at the center of the aluminum nitride ceramic surface layer; the circumferential air groove is centered on the central through hole and diffuses toward the edge of the aluminum nitride ceramic surface layer; the radial air grooves extend from the circumferential air grooves close to the central through hole to the edge of the aluminum nitride ceramic surface layer.
[0024] The technical effects of this application in solving the technical problem are as follows:
[0025] Compared with the prior art, the ESC electrostatic chuck and manufacturing process of the present invention adopt the following steps S1: mixing; S2: casting; S3: tungsten slurry electrode printing; S4: debinding; S5: sintering and forming; S6: assembly; S7: detection; S8: preparation completion. In the sintering process of step S5, TI titanium metal material is doped with a doping amount of 6-15% (weight ratio), and the doping amount of Y2O3 is doped with 4-5% (weight ratio), which will replace the original conventional (alumina ceramic, resin or polyimide) electrostatic chuck surface, and has the characteristics of thermal conductivity up to 170W / M·K, low leakage current, good adsorption effect, etc. [Drawings]
[0026] Figure 1 The present invention is a schematic diagram of the manufacturing process of an ESC electrostatic chuck. [Specific implementation method]
[0027] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0028] See also Figure 1The present invention provides an ESC electrostatic chuck manufacturing process 1, comprising the following steps:
[0029] S1: mixing; S2: casting; S3: tungsten slurry electrode printing; S4: debinding; S5: sintering; S6: assembly; S7: testing; S8: preparation completed;
[0030] In the sintering process of step S5, TI titanium metal material is doped in an amount of 6-15% (by weight); and Y2O3 is doped in an amount of 4-5% (by weight).
[0031] The present application adopts the following steps S1: mixing; S2: casting; S3: tungsten slurry electrode printing; S4: debinding; S5: sintering; S6: assembly; S7: testing; S8: preparation completion. During the sintering process in step S5, TI titanium metal material is doped in an amount of 6-15% (weight ratio), and the doping amount of Y2O3 is 4-5% (weight ratio). The original conventional (alumina ceramic, resin or polyimide) electrostatic chuck surface will be replaced, and the thermal conductivity can reach 170W / M·K, low leakage current, good adsorption effect and other characteristics.
[0032] In some preferred embodiments, the doping amount of Y2O3 is 4.5%.
[0033] The surface of conventional -100℃-350℃ electrostatic chucks is alumina ceramics, resin or polyimide. The surface of the present invention is aluminum nitride ceramic doped with Y2O3 and titanium powder, with the doping amount being about 6-15% (weight ratio) and the Y2O3 doping amount being about 4.5%. The color of the finished product after sintering is brown or tan, and the volume resistivity is E8-E10.
[0034] In some other embodiments, the ESC electrostatic chuck corresponding to the aforementioned manufacturing process is manufactured using the aforementioned manufacturing process; and includes a first aluminum nitride ceramic surface layer, a tungsten electrode layer, and a second aluminum nitride ceramic surface layer which are sequentially arranged and used to support a wafer; the tungsten electrode layer is a two-layer structure symmetrically arranged on the left and right; and dot protrusions with a diameter size range of 40-60nm are densely arranged on the surface of the first aluminum nitride ceramic surface layer.
[0035] Furthermore, the diameter of the dot protrusions is 50 nm.
[0036] Furthermore, the ESC electrostatic chuck also includes a temperature control functional layer and a base for arranging the first aluminum nitride ceramic surface layer, the tungsten electrode layer, the second aluminum nitride ceramic surface layer and the temperature control functional layer; the base is matched and connected with the external process chamber.
[0037] In some other embodiments, the ESC electrostatic chuck corresponding to the aforementioned manufacturing process is manufactured using the aforementioned manufacturing process; it includes a positioning plate; the positioning plate has an aluminum nitride ceramic chuck surface; at least one circumferential air groove, a plurality of radial air grooves and a plurality of dividing air grooves are provided on the aluminum nitride ceramic chuck surface; a central through hole for connecting with a gas source is provided at the center of the aluminum nitride ceramic chuck surface; the circumferential air groove is centered on the central through hole and diffuses toward the edge of the aluminum nitride ceramic chuck surface; the radial air grooves extend from the circumferential air grooves close to the central through hole to the edge of the aluminum nitride ceramic chuck surface; some of the radial air grooves are connected to the central through hole; and it also includes magnetron sputtered T IN dots with a diameter of 2 nm densely arranged on the surface of the aluminum nitride ceramic chuck surface.
[0038] Furthermore, the color of the Ti N is brown, and the ethylene content is increased during PVD sputtering, so that the dots after sputtering are harder and more wear-resistant.
[0039] Furthermore, the ESC electrostatic chuck also includes a temperature control functional layer and a base for arranging the aluminum nitride ceramic surface layer, the adsorption electrode layer and the temperature control functional layer; the base is matched and connected with the external process chamber.
[0040] In some other embodiments, the ESC electrostatic chuck corresponding to the aforementioned manufacturing process is manufactured using the aforementioned manufacturing process; it includes a positioning plate; the positioning plate has an aluminum nitride ceramic surface layer for supporting a wafer and an adsorption electrode layer; the adsorption electrode layer includes an adsorption electrode unit symmetrically arranged on the left and right; the adsorption electrode layer is a two-piece symmetrical adsorption electrode; the adsorption electrode unit has a semicircular structure.
[0041] Furthermore, at least one circumferential air groove, a plurality of radial air grooves and a plurality of dividing air grooves are provided on the aluminum nitride ceramic surface layer; a central through hole for connecting with an air source is provided at the center of the aluminum nitride ceramic surface layer; the circumferential air groove is centered on the central through hole and diffuses toward the edge of the aluminum nitride ceramic surface layer; the radial air grooves extend from the circumferential air grooves close to the central through hole to the edge of the aluminum nitride ceramic surface layer.
[0042] The technical effects of this application in solving the technical problem are as follows:
[0043] Compared with the prior art, the ESC electrostatic chuck manufacturing process 1 of the present invention adopts the following steps S1: mixing; S2: casting; S3: tungsten slurry electrode printing; S4: debinding; S5: sintering; S6: assembly; S7: detection; S8: preparation completion. In the sintering process of step S5, TI titanium metal material is doped with a doping amount of 6-15% (weight ratio), and the doping amount of Y2O3 is 4-5% (weight ratio), which will replace the original conventional (alumina ceramic, resin or polyimide) electrostatic chuck surface, and has the characteristics of thermal conductivity up to 170W / M·K, low leakage current, good adsorption effect, etc.
[0044] The above-described embodiments of the present invention do not constitute a limitation on the protection scope of the present invention. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention shall be included in the protection scope of the claims of the present invention.
Claims
1. A process for manufacturing an ESC electrostatic chuck, characterized in that: The following steps are included: S1: mixing; S2: casting; S3: tungsten slurry electrode printing; S4: debinding; S5: sintering; S6: assembly; S7: Detection; S8: Preparation completed; In the sintering process of step S5, TI titanium metal material is doped in an amount of 6-15% (by weight); and Y2O3 is doped in an amount of 4-5% (by weight).
2. The ESC electrostatic chuck manufacturing process according to claim 1, characterized in that: The doping amount of Y2O3 is 4.5%.
3. An ESC electrostatic chuck, characterized in that: It is manufactured using the manufacturing process as claimed in claim 1 or 2; and includes a first aluminum nitride ceramic surface layer, a tungsten electrode layer and a second aluminum nitride ceramic surface layer which are arranged in sequence and used to support a wafer; the tungsten electrode layer is a two-layer structure symmetrically arranged on the left and right; and dot protrusions with a diameter size range of 40-60nm are densely arranged on the surface of the first aluminum nitride ceramic surface layer.
4. An ESC electrostatic chuck as claimed in claim 3, characterized in that: The diameter of the dot protrusions is 50 nm.
5. An ESC electrostatic chuck as claimed in claim 3, characterized in that: The ESC electrostatic chuck also includes a temperature control functional layer and a base for arranging the first aluminum nitride ceramic surface layer, the tungsten electrode layer, the second aluminum nitride ceramic surface layer and the temperature control functional layer; the base is matched and connected with an external process chamber.
6. An ESC electrostatic chuck, characterized in that: Manufactured using the manufacturing process as claimed in claim 1 or 2; comprising a positioning plate; the positioning plate has an aluminum nitride ceramic chuck surface; at least one circumferential air groove, a plurality of radial air grooves and a plurality of split air grooves are provided on the aluminum nitride ceramic chuck surface; a central through hole for connecting with a gas source is provided at the center of the aluminum nitride ceramic chuck surface; the circumferential air grooves are centered on the central through hole and diffuse toward the edge of the aluminum nitride ceramic chuck surface; the radial air grooves extend from the circumferential air grooves close to the central through hole to the edge of the aluminum nitride ceramic chuck surface; some of the radial air grooves are connected to the central through hole; and also includes magnetron sputtering TIN dots with a diameter of 2 nm densely arranged on the surface of the aluminum nitride ceramic chuck surface.
7. An ESC electrostatic chuck according to claim 6, characterized in that: The TiN is brown in color, and the ethylene content is increased during PVD sputtering, so that the dots after sputtering are harder and more wear-resistant.
8. An ESC electrostatic chuck according to claim 6, characterized in that: The ESC electrostatic chuck also includes a temperature control functional layer and a base for arranging the aluminum nitride ceramic surface layer, the adsorption electrode layer and the temperature control functional layer; the base is matched and connected with an external process chamber.
9. An ESC electrostatic chuck, characterized in that: It is manufactured using the manufacturing process as claimed in claim 1 or 2; it includes a positioning plate; the positioning plate has an aluminum nitride ceramic surface layer for supporting a wafer and an adsorption electrode layer; the adsorption electrode layer includes adsorption electrode units that are symmetrically arranged on the left and right; the adsorption electrode layer is a two-piece symmetrical adsorption electrode; the adsorption electrode unit has a semicircular structure.
10. An ESC electrostatic chuck according to claim 9, characterized in that: At least one circumferential air groove, a plurality of radial air grooves and a plurality of dividing air grooves are provided on the aluminum nitride ceramic surface layer; a central through hole for connecting with an air source is provided at the center of the aluminum nitride ceramic surface layer; the circumferential air groove is centered on the central through hole and diffuses toward the edge of the aluminum nitride ceramic surface layer; the radial air grooves extend from the circumferential air grooves close to the central through hole to the edge of the aluminum nitride ceramic surface layer.
Citation Information
Patent Citations
Novel electrostatic adsorption chuck
CN112768401A
Aluminum nitride-based functional ceramic material and preparation method thereof
CN112811910A
Electrostatic chuck processing method for semiconductor
CN116403963A
ESC electrostatic chuck
CN116779521A
Electrostatic chuck
JP2000332090A