Filling agent composition as well as preparation method and application thereof

Through the composition of saturated polyester resin, ricinoleic acid-containing materials and starch, the problems of low solid content and high viscosity of existing fillers are solved, and a filler composition with high solid content and low viscosity is realized, which improves the permeability and Filling properties ensure smooth substrate and good painting effect.

CN118755313AActive Publication Date: 2024-10-11PUYANG ZHANCHEN NEW MATERIALS CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202410594219.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-13
Publication Date
2024-10-11
Estimated Expiration
2044-05-13

AI Technical Summary

Technical Problem

Existing fillers have low solid content and high viscosity, resulting in poor permeability and filling properties, making it difficult to effectively fill the wood holes in solid wood furniture, and the primer is prone to chewing or collapse of the filler.

Method used

A composition of saturated polyester resin, ricinoleic acid-containing materials and starch is used. By adjusting the ratio, a filler composition with high solid content and low viscosity is formed. It is used with a curing agent to ensure the permeability, filling and hardness of the filler. .

Benefits of technology

It achieves good permeability and filling properties of the filler, ensuring that the surface of the substrate is smooth, and the primer is not easy to bite the filler or collapse, and improves the wiping and coloring properties. It is suitable for furniture and building fillers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention relates to the technical field of coatings, in particular to a filling agent composition as well as a preparation method and application thereof. The filling agent composition comprises a component A, wherein the component A comprises the following components in parts by weight: 15-20 parts of saturated polyester resin; 5-10 parts of a ricinoleic acid-containing material; and 25-35 parts of starch. Wherein the saturated polyester resin is high in solid content and low in viscosity, and the ricinoleic acid-containing material contains ricinoleic acid with high solid content and low viscosity and starch, so that the filling property is further improved and the transparency is ensured. The three components in parts by weight can be compounded for synergism, the component A and the curing agent are coated on the surface of a substrate, a conduit of the substrate can be permeated and filled with the component A, and the component A and the curing agent are high in hardness after being cured and can be attached to the conduit, so that the surface of the substrate is smooth. After filling and curing, the primer is further coated, so that a filling agent is not easy to bite and collapse is not easy. The component A can also comprise at least one of a defoaming agent, an anti-settling agent, a filler and a solvent. During use, the component A and the curing agent can be mixed for use.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of coating technology, and in particular to a filler composition and a preparation method and application thereof. Background Art

[0002] Solid wood furniture has the characteristics of durability, clear wood grain, elegant appearance, high-end atmosphere, and environmental protection, and has always been loved by consumers. With the increase of consumer spending power, the market demand for solid wood furniture is also increasing. However, since the ducts of the wood used in solid wood furniture are relatively deep, many wood eyes will be formed, and the surface is not flat, which is difficult to fill with primer, especially water-based primer.

[0003] In order to fill the wood well and prevent the primer from collapsing in the wood eyes, solid wood furniture is often wiped with fillers before applying primer. Fillers can not only color the wood and other substrates, but also fill the wood eyes. After filling, the number of primer coatings and the amount of primer can be reduced. Generally speaking, the higher the solid content of the filler, the easier it is to fill in the wood eyes after curing, that is, the better the filling performance; the lower the viscosity, the better the fluidity, and the easier it is to penetrate into the wood eyes, that is, the better the permeability, so the filler used to wipe the wood often needs to have a high solid content and low viscosity.

[0004] However, most of the existing fillers are mainly alkyd resins, which have high viscosity and poor permeability. They have poor filling properties when more solvents are added, and poor solvent resistance of single components. After filling, the primer is easily bitten by the filler and collapsed. For example, in a disclosed polyurethane transparent primer, it is disclosed that component A and component B form a polyurethane transparent primer, and component A includes alkyd resin, polyester resin, etc., and component B includes TDI curing agent, but it is still a primer with a high solid content. For example, in another disclosed wood coloring filler, the solvent content is still relatively high, the solid content is low, and the solvent resistance is poor. For example, in a disclosed high-solid two-component polyurethane environmentally friendly coating, its component A also uses alkyd resin. Therefore, it is urgent to provide a filler with high solid content and low viscosity, which has good permeability and filling properties, and is not easy to bite the filler or collapse after further primer is applied after the filler is used. Summary of the invention

[0005] The purpose of the present application is to provide a filler composition and a preparation method and application thereof, aiming to solve the problems of low solid content, high viscosity, poor permeability and poor filling properties of the filler in the prior art.

[0006] In order to achieve the above application purpose, the technical solution adopted in this application is as follows:

[0007] In a first aspect, the present application provides a filler composition, including component A, wherein component A includes the following components in parts by weight:

[0008] Saturated polyester resin 15-20 parts

[0009] 5-10 parts of ricinoleic acid-containing materials

[0010] 25-35 parts of starch.

[0011] The A component in the filler composition of the present application includes the above three ingredients, wherein the saturated polyester resin has a high solid content and low viscosity, and the ricinoleic acid-containing material contains ricinoleic acid with a high solid content and low viscosity, and starch is conducive to further improving the filling property and ensuring transparency. The above three components are obtained according to the above weight ratio. The three components can be compounded for synergy, giving the filler composition a balance between high solid content and low viscosity, so that the permeability is good, the filling performance is good, and it is also conducive to improving the wiping property and colorability. Therefore, the A component is applied to the surface of the substrate with a curing agent, and the filler composition can penetrate and fill in the conduit of the substrate, and the hardness is high after curing, and it can be attached to the conduit to make the surface of the substrate smooth. After the filler composition is filled and cured, it is further coated with a primer that is not easy to bite the filler and is not easy to collapse.

[0012] In a second aspect, the present application provides a method for preparing a filler composition of the above application, comprising the following steps:

[0013] The ingredients in component A are mixed.

[0014] The preparation method of the present application includes mixing the components contained in component A, so that a certain weight portion of saturated polyester resin, ricinoleic acid-containing material, starch or further components including defoamer, anti-settling agent, filler, and solvent can be fully mixed and evenly mixed, compounded and enhanced, and a filler composition with high solid content and low viscosity is obtained, which has good permeability and filling properties, as well as wipeability, colorability and other properties when applied on the surface of the substrate. The preparation method process is controllable, and the physical and chemical properties of the obtained filler composition are stable.

[0015] In a third aspect, the present application provides the use of the filler composition of the above application in furniture fillers and building fillers.

[0016] The filler composition of the present application can be applied to the base material of furniture and building walls, and is easy to wipe and collect cleanly when wiped. The surface of the base material after filling and curing is flat, and primer and other paints can be further applied on it. Therefore, the filler composition has the advantages of easy wiping, good filling performance, high hardness, good adhesion, strong coloring, and the paint does not bite the filler or collapse when applied on it, and has a wide range of applications. DETAILED DESCRIPTION

[0017] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application more clearly understood, the present application is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0018] In this application, the term "and / or" describes the association relationship of associated objects, indicating that there may be three relationships. For example, A and / or B can mean: A exists alone, A and B exist at the same time, and B exists alone. A and B can be singular or plural. The character " / " generally indicates that the associated objects are in an "or" relationship.

[0019] In this application, "at least one" means one or more, and "plurality" means two or more. "At least one of the following" or similar expressions refers to any combination of these items, including any combination of single items or plural items. For example, "at least one of a, b, or c", or "at least one of a, b, and c" can all mean: a, b, c, ab (i.e., a and b), ac, bc, or abc, where a, b, c can be single or multiple, respectively.

[0020] It should be understood that in the various embodiments of the present application, the size of the serial numbers of the above-mentioned processes does not mean the order of execution, some or all of the steps can be executed in parallel or sequentially, and the execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of the present application.

[0021] The terms used in the embodiments of the present application are only for the purpose of describing specific embodiments, and are not intended to limit the present application. The singular forms "a", "an" and "the" used in the embodiments of the present application and the appended claims are also intended to include plural forms, unless the context clearly indicates other meanings.

[0022] The weight of the relevant components mentioned in the embodiment description of the present application can not only refer to the specific content of each component, but also represent the proportional relationship between the weights of the components. Therefore, as long as the content of the relevant components is proportionally enlarged or reduced according to the embodiment description of the present application, it is within the scope disclosed in the embodiment description of the present application. Specifically, the mass in the embodiment description of the present application can be μg, mg, g, kg and other mass units known in the chemical industry.

[0023] The terms "first" and "second" are used only for descriptive purposes to distinguish objects such as substances from each other, and should not be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. For example, without departing from the scope of the embodiments of the present application, the first XX may also be referred to as the second XX, and similarly, the second XX may also be referred to as the first XX. Thus, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features.

[0024] Related terms:

[0025] The viscosity in this application refers to the viscosity at a temperature of 25°C.

[0026] The conduits of the substrate in the present application refer to micro cracks in the substrate, such as the texture or gaps of wood.

[0027] The bite filler in this application refers to a filler that is easy to stick to, and the non-bite filler refers to a filler that is further painted after the base material is filled and cured, and the filler is not easy to stick to and peeled off when the paint is removed.

[0028] In a first aspect, an embodiment of the present application provides a filler composition, including component A, wherein component A includes the following components in parts by weight:

[0029] Saturated polyester resin 15-20 parts

[0030] 5-10 parts of ricinoleic acid-containing materials

[0031] 25-35 parts of starch.

[0032] The saturated polyester resin contained in the A component in the filler composition of the present application embodiment is high in solid content and low in viscosity, and the ricinoleic acid-containing material contains ricinoleic acid with high solid content and low viscosity, and starch is conducive to further improving filling and ensuring transparency. The above three components are obtained according to the above-mentioned weight parts ratio. The three components can be compounded for synergy, giving the filler composition a balance between high solid content and low viscosity, so that the permeability is good, the filling performance is good, and it is also conducive to improving the wiping and coloring properties. Therefore, the A component is applied to the surface of the substrate with a curing agent, and the filler composition can penetrate and fill in the conduit of the substrate, and the hardness is high after curing, and it can be attached to the conduit to make the surface of the substrate smooth. After the filler composition is filled and cured, it is further coated with a primer that is not easy to bite the filler and is not easy to collapse.

[0033] The three components in the above filling composition play a synergistic role. The role of each component in the filling composition will be further described below.

[0034] About saturated polyester resin:

[0035] Saturated polyester resin has high solid content and low viscosity, and in some embodiments, no solvent is required in the A component prepared from saturated polyester resin, while the alkyd resin used in the prior art has low solid content, high viscosity, is easy to gel, and requires a solvent. In some embodiments, the saturated polyester resin includes a saturated polyol resin, wherein the saturated polyol resin can be selected from REXIN HSP 30 (solid content of 100%) of Italian Chemical Industry Co., Ltd. (SAPICI). These types of saturated polyester resins have high solid content and low viscosity, which are conducive to further improving the permeability and filling properties of the filler composition.

[0036] In some embodiments, a saturated polyester resin with the following solid content or viscosity can be selected. The solid content of the saturated polyester resin is 95% to 100%, and can be 100%. In the exemplary embodiment, it can include but not limited to any value of 95%, 97%, 99%, 100% or the range between any two values. In some embodiments, the viscosity of the saturated polyester resin is 3000 to 8000 mPa·s. In the exemplary embodiment, it can include but not limited to any value of 3000 mPa·s, 5000 mPa·s, 7000 mPa·s, 8000 mPa·s or the range between any two values. These saturated polyester resins with solid content or viscosity are beneficial to further improve the permeability and filling property of the filler composition. The existing alkyd resin has a solid content of about 60% to 70%, a viscosity of about 6000 to 12000 mPa·s, and requires a solvent.

[0037] In component A, the weight portion of the saturated polyester resin is 15 to 20 parts, and in the exemplary embodiment, it may include but is not limited to any value or a range between any two values ​​of 15, 16, 17, 18, 19, and 20. These weight portions of saturated polyester resin are beneficial to further improve the above properties of the filler composition.

[0038] About Ricinoleic Acid-Containing Materials:

[0039] Ricinoleic acid is an unsaturated fatty acid rich in hydroxyl, alkenyl and carboxyl groups, with high solid content and low viscosity, so the use of ricinoleic acid-containing materials in filler compositions is beneficial to improving permeability and filling properties, and is also beneficial to improving wipeability and colorability. In some embodiments, the ricinoleic acid-containing material includes at least one of blown castor oil, hydrogenated castor oil, and castor oil long oil alkyd resin. Among them, blown castor oil is generally a kind of oil made by heating castor seeds and then cooling them with oxygen to separate the oxidized substances from the oil. Blown castor oil can include at least one of BLO of Taiwan Changchuan Chemical Co., Ltd. and A633 of Taiwan Dali Polymer Industry Co., Ltd. These ricinoleic acid-containing materials are beneficial to the filler composition to further take into account high solid content and low viscosity, improve permeability and filling properties; and further improve the wipeability of the filler composition, so that the filler composition is easier to wipe on the substrate, wipe smooth, and easy to color.

[0040] In some embodiments, the following solid content or viscosity of the ricinoleic acid-containing material can be selected. In some embodiments, the solid content of the ricinoleic acid-containing material is 95% to 100%, and can be 100%. In the exemplary embodiment, it can include but not limited to any value of 95%, 97%, 99%, 100% or the range between any two values. In some embodiments, the viscosity of the ricinoleic acid-containing material is 90 to 120 mPa·s. In the exemplary embodiment, it can include but not limited to any value of 90 mPa·s, 100 mPa·s, 110 mPa·s, 120 mPa·s or the range between any two values. These solid content or viscosity of the ricinoleic acid-containing material is conducive to further improving the permeability, filling and wipeability of the filler composition.

[0041] In component A, the weight portion of the ricinoleic acid-containing material is 5 to 10 parts, and in the exemplary embodiment, it may include but is not limited to any value of 5 parts, 6 parts, 7 parts, 8 parts, 9 parts, 10 parts, or a range between any two values. These weight portions of ricinoleic acid-containing materials are beneficial to further improve the above-mentioned properties of the filler composition.

[0042] About starch:

[0043] Starch can significantly improve the filling property of the filler composition without affecting the transparency of the filler composition. In some embodiments, the starch includes at least one of corn starch, potato starch, and cassava starch. These starches can improve the filling property of the filler composition and ensure transparency. Among them, corn starch can be very fine but not sticky, and the particle size of other types of starch can be slightly larger to avoid sticking together and agglomerating into large secondary particles in the filler composition. The particle size of starch should not be too large. In some embodiments, the starch is at least 325 mesh.

[0044] In component A, the weight of the starch is 25 to 35 parts, and in the exemplary embodiment, it may include but is not limited to any value or a range between any two values ​​of 25, 28, 30, 32, and 35. These weight portions of starch are beneficial to further improve the filling property and transparency of the filler composition.

[0045] About other components:

[0046] In some embodiments, component A also includes at least one of a defoamer, an anti-settling agent, a filler, and a solvent. In the exemplary embodiment, any one of them, or a combination of any two or more thereof, may be included. Among them, the defoamer is beneficial to eliminate bubbles when the filler composition is rubbed on the surface of the substrate. The anti-settling agent can prevent the powder in the filler composition from stratification and precipitation, and improve the dispersion stability. The filler can improve the filling property of the filler composition. The solvent is beneficial to reduce the viscosity of the filler composition, is beneficial to repeatedly wiping and rubbing into the conduit of the substrate, and is also beneficial to improve the dispersibility.

[0047] In some embodiments, the defoamer may include an organic silicon defoamer, which has good compatibility in the filler composition and strong defoaming ability, especially strong defoaming ability when thick coating is performed. In the exemplary embodiment, the organic defoamer includes but is not limited to at least one of BYK-052 of BYK Chemical Co., Ltd. (BYK) of Germany and HX-2500 of Guangzhou Huaxia Additive Chemical Co., Ltd.

[0048] In some embodiments, when a defoaming agent is included in component A, the weight portion of the defoaming agent may be 0.3 to 0.5 parts. In exemplary embodiments, the weight portion may include but is not limited to 0.3 parts, 0.37 parts, 0.44 parts, 0.5 parts, any value, or a range between any two values. These amounts of defoaming agent are beneficial to eliminating bubbles in the filler composition when it is used.

[0049] In some embodiments, the anti-settling agent includes at least one of fumed silica and bentonite. Among them, the fumed silica may include hydrophilic fumed silica, which is beneficial to inhibit the stratification and precipitation of the filler composition. Fumed silica includes but is not limited to at least one of A200 produced by Evonik Industries AG of Germany and M-5 produced by Shanghai Cabot Chemical Co., Ltd. (parent company includes CABOT Corporation of the United States). Bentonite may include organic bentonite, which is beneficial to inhibit the stratification and precipitation of the filler composition, improve the dispersion stability, and at the same time help to improve the adhesion during wiping. Bentonite includes but is not limited to BP-183 produced by Zhejiang Huate New Materials Co., Ltd., BS-1C produced by Zhejiang Fenghong New Materials Co., Ltd., and Bengel828 produced by Deqian (Shanghai) Chemical Co., Ltd. In the exemplary embodiment, fumed silica and bentonite can be added at the same time.

[0050] In some embodiments, when component A includes an anti-settling agent, the weight portion of the anti-settling agent in component A is 1.5 to 2.5 parts, and in exemplary embodiments, it can include any value of 1.5, 1.8, 2.2, or 2.5 parts, or a range between any two values. When the anti-settling agent includes fumed silica and bentonite, the weight portion of the fumed silica can be 0.5 to 1.0 parts, and the weight portion of the bentonite can be 1.0 to 1.5 parts. These weight portions of anti-settling agent are beneficial to inhibiting the stratification and precipitation of the filler composition and improving the dispersion stability.

[0051] In some embodiments, the filler includes at least one of mica powder, silica powder, and talc. Mica powder can improve the filling property of the filler composition without affecting the wiping property. In the exemplary embodiment, the mica powder includes 400 mesh wet-process mica powder, and the wet-process sericite powder can be selected from GA-1 of Anhui Ge Rui New Materials Technology Co., Ltd. Silica powder can improve the filling property of the filler composition without affecting the transparency. In the exemplary embodiment, the silica powder can include silica powder with 1250 mesh, and JLH-G6 of Shenzhen Jin Hao Hui Mining Development Co., Ltd. can be selected. In the exemplary embodiment, mica powder and silica powder can be added at the same time.

[0052] In some embodiments, when component A includes an anti-settling agent, the weight of the filler is 20 to 30 parts, and in the exemplary embodiment, it can include any value of 20 parts, 22 parts, 25 parts, 27 parts, 30 parts, or a range between any two values. When the filler includes mica powder and silica powder, the weight of the mica powder can be 10 to 15 parts, and the weight of the silica powder can be 10 to 15 parts. These weights of fillers can further improve the filling property of the filler composition, while also taking into account the wipeability and transparency.

[0053] In some embodiments, the solvent includes at least one of glycerol acetone acetal and propylene glycol methyl ether propionate. Adding a solvent is beneficial to improving the dispersibility of the filler composition, reducing the viscosity, and facilitating repeated wiping and rubbing to penetrate into the conduit of the substrate. Among them, glycerol acetone acetal, as a high boiling point solvent, belongs to an environmentally friendly solvent with a high boiling point, slow volatilization, and very low odor, which reduces the viscosity of the filler composition and facilitates repeated wiping and rubbing into the conduit. Glycol acetone acetal includes but is not limited to AUGEOSL191 environmentally friendly solvent of Rhodia Co., Ltd. in the United States, Augeo-SL191 environmentally friendly solvent of Solvay Group (Solvay) in Brazil, and at least one of glycerol acetone acetal of Shanghai Tichem Industrial Co., Ltd.

[0054] In some embodiments, when component A includes a solvent, the weight of the solvent is 7 to 10 parts. In exemplary embodiments, the weight of the solvent may include but is not limited to any value of 7 parts, 8 parts, 9 parts, 10 parts, or a range between any two values.

[0055] In an exemplary embodiment, when component A further includes a defoamer, an anti-settling agent, a filler, and a solvent, component A may include the following components in parts by weight:

[0056]

[0057] The components in the A component obtained by these components and weight parts can be compounded to enhance the synergy, which is beneficial for the filler composition to have low viscosity and high solid content, improve permeability and filling, and further improve the properties of wiping, stability, etc. After the filler composition is filled and cured, it is not easy to bite the filler and collapse when further coated with a primer.

[0058] About Component A:

[0059] In some embodiments, the solid content of component A is 90% to 100%, optionally 90% to 100%, optionally 92%, optionally 98%, and in the exemplary examples, it may include but is not limited to any value of 90%, 91%, 92%, 93% or the range between any two values. In some embodiments, the viscosity of component A is 3000 to 8000 mPa·s, and in the exemplary examples, it may include but is not limited to any value of 3000 mPa·s, 5000 mPa·s, 7000 mPa·s, 8000 mPa·s or the range between any two values. These solid contents are higher than the solid contents of the prior art fillers, and the viscosity is lower than the viscosity of the prior art fillers, so that the filler composition has good permeability and filling properties.

[0060] About Component B:

[0061] Although component A has a high solid content and low viscosity, it is often necessary to add a curing agent to solidify the filler composition, harden it, and fill and bind it in the conduit of the substrate when it is used. Therefore, in some embodiments, the filler composition also includes component B, and component B includes the following components: polyurethane curing agent. Component B of the polyurethane curing agent can be used together with the above-mentioned component A as a component in the filler composition. When not in use, component A and component B can be prepared and separated separately. When it is needed to wipe the substrate, component A and component B are mixed and treated to wipe the substrate for filling and curing.

[0062] Since component A contains saturated polyester resin and blown castor oil materials, which are rich in hydroxyl groups and contain active hydrogen, and polyurethane curing agent refers to the component containing isocyanate group (NCO) in the two-component polyurethane product, it can be used with component A containing active hydrogen to undergo cross-linking reaction and cure. In the exemplary embodiment, component A contains a large amount of R-OH, and the polyurethane curing agent of component B contains R'-NH-R" and OCN-R1-NCO. Mixing component A and component B can produce a series of cross-linking reactions, which may include but are not limited to the following cross-linking reactions:

[0063]

[0064] The large amount of hydroxyl groups in component A can increase the cross-linking sites, and when mixed with component B, the cross-linking structure can be strengthened, thereby improving the stability and mechanical strength of the filler composition during use.

[0065] When used, component A and component B are applied to the surface of the substrate for filling and curing to form a filler film layer with good flexibility, good solvent resistance and high hardness. Therefore, when paint is applied on the cured filler film layer, good solvent resistance means that the cured filler will not be dissolved and destroyed by the paint; high hardness and good filling property means that the paint will not bite the filler (that is, when removing the paint, the filler will not stick to it and be removed together), and it will not collapse.

[0066] In some embodiments, the polyurethane curing agent includes a moisture-curing polyurethane curing agent, and the moisture-curing polyurethane curing agent contains a diphenylmethane diisocyanate prepolymer (MDI). The moisture-curing polyurethane curing agent has a high solid content, which is much higher than the TDI curing agent commonly used in the prior art, and has a low viscosity, which is beneficial to improving the permeability, filling and hardness of the filler composition after curing. In some embodiments, the solid content of the polyurethane curing agent is 95% to 100%; in the exemplary examples, it can include but is not limited to any value of 95%, 96%, 97%, 98%, 100% or a range between any two values, and can be selected as 100%. In some embodiments, the viscosity of the polyurethane curing agent is 500 to 700 mPa·s; in the exemplary examples, it can include but is not limited to any value of 500 mPa·s, 550 mPa·s, 650 mPa·s, 700 mPa·s or a range between any two values.

[0067] In some embodiments, in the above filler composition, the weight of component B can be 100 parts. In some embodiments, the weight ratio of component A to component B is 1:(0.5-0.8), and in the exemplary examples, it can include but is not limited to any ratio of 1:0.5, 1:0.6, 1:0.7, 1:0.8 or the range between any two ratios. The amount of component B or the weight ratio of component A to component B is conducive to good permeability, filling, wiping and other properties when component A and component B are used together.

[0068] When the filler composition contains both component A and component B, the solid content of the filler composition is 93% to 100%, optionally 93% to 98%, optionally 100%. In the exemplary embodiment, it may include but is not limited to any value of 93%, 95%, 98%, 100% or a range between any two values. The solid content of the filler composition here refers to the solid content of component A and component B as a whole when the two components are placed separately before use.

[0069] The second aspect of the present application provides a method for preparing the filler composition of the above application example, comprising the following steps:

[0070] S10: Mixing the ingredients contained in component A.

[0071] The preparation method of the embodiment of the present application includes mixing the ingredients contained in component A, so that a certain weight portion of saturated polyester resin, ricinoleic acid-containing material, starch or further components including defoamer, anti-settling agent, filler, and solvent can be fully mixed and evenly mixed, compounded and synergized to obtain a filler composition with high solid content and low viscosity, which has good permeability and filling properties, as well as wipeability, colorability and other properties when applied on the surface of the substrate. The preparation method process is controllable, and the obtained filler composition has stable physical and chemical properties.

[0072] Wherein, component A may include the saturated polyester resin, ricinoleic acid-containing material, and starch in the filler composition of the above-mentioned application examples. In some embodiments, component A may further contain the defoamer, anti-settling agent, filler, and solvent in the filler composition of the above-mentioned application examples; in this case, the mixing process in step S10 may include the following steps:

[0073] S11: performing a first mixing process on the saturated polyester resin, the ricinoleic acid-containing material, and the defoaming agent to obtain a first mixed material;

[0074] S12: performing a second mixing process on the first mixed material, starch, anti-settling agent, and filler to obtain a second mixed material;

[0075] S13: performing a third mixing process on the second mixed material and the solvent.

[0076] When component A also contains defoamer, anti-settling agent, filler, and solvent, its solid content is high and contains a variety of powdered solid materials. If directly blended, agglomeration is likely to occur. Therefore, the order of the above-mentioned mixing treatment is optimized according to the properties of each material in component A, and the filler composition obtained according to the treatment method of step S11 to step S13 has good dispersibility and is not easy to agglomerate. Wherein step S11 first mixes two main materials with high solid content and low viscosity with a defoamer to obtain a first mixed material with high solid content and low viscosity, and then mixes with a powder with high solid content for a second treatment, so that each component is fully dispersed and uniform, and finally mixes with a solvent for a third treatment to further reduce viscosity. Therefore, the obtained filler composition is uniformly dispersed, has a high solid content, and has a low viscosity, which is conducive to improving permeability, filling, wiping, etc., and the preparation method is simple, low cost, high efficiency, and suitable for industrial promotion.

[0077] In some embodiments, the temperature of the first mixing treatment in step S11 is 20-45°C, and the mixing speed is 700-800rpm. In some embodiments, the temperature of the second mixing treatment in step S12 is 20-50°C, and the mixing speed is 1000-1200rpm. In some embodiments, the temperature of the third mixing treatment in step S13 is 20-45°C, and the mixing speed is 700-800rpm. The use of the above mixing temperature and mixing speed in steps S11 to S13 is conducive to uniform mixing of the components, improving dispersibility and preventing agglomeration.

[0078] The third aspect of the embodiments of the present application provides the application of the filler composition of the embodiments of the present application in furniture fillers and building fillers.

[0079] The filler composition of the embodiment of the present application can be applied to the base material of furniture and building walls, and is easy to wipe and clean. The surface of the base material after filling and curing is flat, and primer and other paints can be further applied on it. Therefore, the filler composition has the advantages of easy wiping, good filling performance, high hardness, good adhesion, strong coloring, and the paint does not bite the filler or collapse when applied on it, and has a wide range of applications.

[0080] The following describes the invention in conjunction with specific embodiments.

[0081] Example 1

[0082] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 1 and component B 1, wherein component A 1 comprises components in parts by weight as shown in Table 1 below:

[0083] Table 1

[0084]

[0085] The preparation method of the filler composition of component A 1 comprises the following steps:

[0086] S01. Weigh the raw materials of each component according to the components and their weight parts in Table 1 above;

[0087] S02, mixing the saturated polyester resin, blown castor oil, and defoamer at a temperature lower than 45° C. and a stirring speed of 800 rpm, and stirring for 5 minutes to obtain a first mixed material;

[0088] S03, mixing the first mixed material, fumed silica, bentonite, corn starch, wet-process sericite powder, and silicon powder at a temperature below 50° C. and a stirring speed of 1200 rpm for 30 minutes to obtain a second mixed material;

[0089] S04: The second mixed material and the solvent are mixed at a temperature lower than 45° C. and a speed of 800 rpm, and stirred for 15 minutes to obtain component A 1.

[0090] The appearance of the obtained component A 1 is a white paste;

[0091] Component B 1 is a curing agent, specifically a moisture-curing polyurethane curing agent, and UCOPOL M621 produced by Italian Chemical Industry Co., Ltd. is selected, which contains diphenylmethane diisocyanate prepolymer (MDI), has a solid content of 100%, a viscosity of 520 mPa·s, and a weight of 80 parts. It is separated from component A 1 when not in use and mixed with component A 1 when in use.

[0092] Example 2

[0093] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 2 and component B 1, wherein component A 2 comprises components in parts by weight as shown in Table 2 below:

[0094] Table 2

[0095] Components Weight Product Model Saturated polyester resin 15 REXIN HSP 50 from Italian Chemical Industry Co., Ltd. Blowing castor oil 10 A633 from Taiwan Dali Polymer Industry Co., Ltd. Defoaming agent 0.4 HX-2500 from Guangzhou Huaxia Additive Chemical Co., Ltd. Fumed Silica 1.0 M-5 from Shanghai Cabot Chemical Co., Ltd. Bentonite 0.5 BS-1C produced by Zhejiang Fenghong New Materials Co., Ltd. Corn starch 30 Wet process sericite powder 15 GA-1 from Anhui Ge Rui New Material Technology Co., Ltd. Silica powder 15 JLH-G6 from Shenzhen Jinhaohui Mining Development Co., Ltd. Acetone glycerol acetal 7 Augeo-SL191 from Solvay Brazil

[0096] The preparation method of the filler composition of component A 2 comprises the following steps:

[0097] S01. Weigh the raw materials of each component according to the components and their weight parts in Table 1 above;

[0098] S02, mixing the saturated polyester resin, blown castor oil, and defoamer at a temperature lower than 45° C. and a stirring speed of 800 rpm, and stirring for 5 minutes to obtain a first mixed material;

[0099] S03, mixing the first mixed material, fumed silica, bentonite, corn starch, wet-process sericite powder, and silicon powder at a temperature below 50° C. and a stirring speed of 1000 rpm, and stirring for 35 minutes to obtain a second mixed material;

[0100] S04. Mix the second mixed material with the solvent at a temperature lower than 45° C. and a speed of 800 rpm, and stir for 15 minutes to obtain component A 2.

[0101] The appearance of the obtained A component 2 is a white paste;

[0102] B component 1 is the same as B component 1 of Example 1.

[0103] Example 3

[0104] This embodiment provides a filler composition and a preparation method thereof. The filler composition includes component A 3 and component B 1, wherein component A 3 includes components in parts by weight as shown in Table 3 below:

[0105] Table 3

[0106] Components Weight Product Model Saturated polyester resin 18 REXIN HSP 50 from Italian Chemical Industry Co., Ltd. Blowing castor oil 7 BLO of Taiwan Changchuan Chemical Industry Co., Ltd. Defoaming agent 0.5 BYK-052 produced by BYK Chemical Co., Ltd., Germany Fumed Silica 0.8 M-5 from Shanghai Cabot Chemical Co., Ltd. Bentonite 1.2 Bengel 828 produced by Deqian (Shanghai) Chemical Co., Ltd. Corn starch 35 Wet process sericite powder 12 GA-1 from Anhui Ge Rui New Material Technology Co., Ltd. Silica powder 13 JLH-G6 from Shenzhen Jinhaohui Mining Development Co., Ltd. Acetone glycerol acetal 10 Acetone glycerol acetal from Shanghai Tichem Industrial Co., Ltd.

[0107] The preparation method of component A 3 is the same as that of component A 1;

[0108] B component 1 is the same as B component 1 of Example 1.

[0109] Example 4

[0110] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 4 and component B 1, wherein component A 4 comprises components in parts by weight as shown in Table 4 below:

[0111] Table 4

[0112]

[0113]

[0114] The preparation method of component A 4 is the same as that of component A 1;

[0115] B component 1 is the same as B component 1 of Example 1.

[0116] Example 5

[0117] This embodiment provides a filler composition and a preparation method thereof. The filler composition includes component A 5 and component B 1, wherein component A 5 includes components in parts by weight as shown in Table 5 below:

[0118] Table 5

[0119] Components Weight Product Model Saturated polyester resin 16 REXIN HSP 50 from Italian Chemical Industry Co., Ltd. Blowing castor oil 9 A633 from Taiwan Dali Polymer Industry Co., Ltd. Defoaming agent 0.5 HX-2500 silicone defoamer from Guangzhou Huaxia Additive Chemical Co., Ltd. Fumed Silica 1.0 M-5 from Shanghai Cabot Chemical Co., Ltd. Bentonite 1.0 BS-1C produced by Zhejiang Fenghong New Materials Co., Ltd. Corn starch 25 Wet process sericite powder 15 GA-1 from Anhui Ge Rui New Material Technology Co., Ltd. Silica powder 15 JLH-G6 from Shenzhen Jinhaohui Mining Development Co., Ltd. Acetone glycerol acetal 9 Acetone glycerol acetal from Shanghai Tichem Industrial Co., Ltd.

[0120] The preparation method of component A 5 is the same as that of component A 1;

[0121] B component 1 is the same as B component 1 of Example 1.

[0122] Example 6

[0123] This embodiment provides a filler composition and a preparation method thereof. The filler composition includes component A 6 and component B 1, wherein component A 6 includes components in parts by weight as shown in Table 6 below:

[0124] Table 6

[0125]

[0126] The preparation method of component A 6 is the same as that of component A 1;

[0127] B component 1 is the same as B component 1 of Example 1.

[0128] Example 7

[0129] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 7 and component B 1, wherein component A 7 differs from embodiment 1 only in that: no solvent is added;

[0130] The preparation method of component A 7 is the same as that of component A 1;

[0131] B component 1 is the same as B component 1 of Example 1.

[0132] Example 8

[0133] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 8 and component B 1, wherein the difference between component A 8 and embodiment 1 is only that: two fillers are non-humidified sericite powder and silica powder;

[0134] The preparation method of component A 8 is the same as that of component A 1;

[0135] B component 1 is the same as B component 1 of Example 1.

[0136] Example 9

[0137] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 1 and component B 2, wherein component A 1 is the same as component A 1 in embodiment 1;

[0138] The difference between component B 2 and component B 1 of Example 1 is that the weight parts are changed to 70 parts.

[0139] Example 10

[0140] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 2 and component B 2, wherein component A 2 is the same as component A 2 in embodiment 2;

[0141] The difference between component B 2 and component B 1 of Example 2 is that the weight parts are changed to 70 parts.

[0142] Embodiment 11

[0143] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 3 and component B 2, wherein component A 3 is the same as component A 3 in embodiment 3;

[0144] The difference between component B 2 and component B 1 of Example 3 is that the weight parts are changed to 70 parts.

[0145] Example 12

[0146] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 4 and component B 2, wherein component A 4 is the same as component A 4 in embodiment 4;

[0147] The difference between component B 2 and component B 1 of Example 4 is that the weight parts are changed to 70 parts.

[0148] Embodiment 13

[0149] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 5 and component B 2, wherein component A 5 is the same as component A 5 in embodiment 5;

[0150] The difference between component B 2 and component B 1 of Example 5 is that the weight parts are changed to 70 parts.

[0151] Embodiment 14

[0152] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 6 and component B 2, wherein component A 6 is the same as component A 6 in embodiment 6;

[0153] The difference between component B 2 and component B 1 of Example 6 is that the weight parts are changed to 70 parts.

[0154] Embodiment 15

[0155] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 7 and component B 2, wherein component A 7 is the same as component A 7 in embodiment 7;

[0156] The difference between component B 2 and component B 1 of Example 7 is that the weight parts are changed to 70 parts.

[0157] Example 16

[0158] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 8 and component B 2, wherein component A 8 is the same as component A 8 in embodiment 8;

[0159] The difference between component B 2 and component B 1 of Example 8 is that the weight parts are changed to 70 parts.

[0160] Embodiment 17

[0161] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 1 and component B 3, wherein component A 1 is the same as component A 1 in embodiment 1;

[0162] The difference between component B 3 and component B 1 of Example 1 is that the weight parts are changed to 50 parts.

[0163] Embodiment 18

[0164] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 2 and component B 3, wherein component A 2 is the same as component A 2 in embodiment 2;

[0165] The difference between component B 3 and component B 1 of Example 2 is that the weight parts are changed to 50 parts.

[0166] Embodiment 19

[0167] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 3 and component B 3, wherein component A 3 is the same as component A 3 in embodiment 3;

[0168] The difference between component B 3 and component B 1 of Example 3 is that the weight parts are changed to 50 parts.

[0169] Embodiment 20

[0170] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 4 and component B 3, wherein component A 4 is the same as component A 4 in embodiment 4;

[0171] The difference between component B 3 and component B 1 of Example 4 is that the weight parts are changed to 50 parts.

[0172] Embodiment 21

[0173] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 5 and component B 3, wherein component A 5 is the same as component A 5 in embodiment 5;

[0174] The difference between component B 3 and component B 1 of Example 5 is that the weight parts are changed to 50 parts.

[0175] Embodiment 22

[0176] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 6 and component B 3, wherein component A 6 is the same as component A 6 in embodiment 6;

[0177] The difference between component B 3 and component B 1 of Example 6 is that the weight parts are changed to 50 parts.

[0178] Embodiment 23

[0179] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 7 and component B 3, wherein component A 7 is the same as component A 7 in embodiment 7;

[0180] The difference between component B 3 and component B 1 of Example 7 is that the weight parts are changed to 50 parts.

[0181] Embodiment 24

[0182] This embodiment provides a filler composition and a preparation method thereof. The filler composition comprises component A 8 and component B 3, wherein component A 8 is the same as component A 8 in embodiment 8;

[0183] The difference between component B 3 and component B 1 of Example 8 is that the weight parts are changed to 50 parts.

[0184] Comparative Example 1

[0185] This comparative example provides a filler composition and a preparation method thereof. The filler composition comprises component A and component B, wherein the difference between component A and component A1 in Example 1 is that the saturated polyester resin is replaced with an alkyd resin, which is found to have too high viscosity, poor fluidity and permeability, and is almost difficult to be used on a substrate, so that the solvent content needs to be increased to further obtain a usable component A;

[0186] The B component is the same as the B component 1 of Example 1.

[0187] Comparative Example 2

[0188] This comparative example provides a filler composition and a preparation method thereof. The filler composition comprises component A and component B, wherein the difference between component A and component A1 in Example 1 is that the blown castor oil is replaced with an alkyd resin, which is found to have too high viscosity, poor fluidity and permeability, and is almost difficult to use on a substrate, so that the solvent content needs to be increased to further obtain a usable component A;

[0189] The B component is the same as the B component 1 of Example 1.

[0190] Comparative Example 3

[0191] This comparative example provides a filler composition and a preparation method thereof. The filler composition comprises component A and component B, wherein the difference between component A and component A1 in Example 1 is that the blown castor oil is replaced with an alkyd resin, which is found to have too high viscosity, poor fluidity and permeability, and is almost difficult to use on a substrate, so that the solvent content needs to be increased to further obtain a usable component A;

[0192] The difference between component B and component B 1 of Example 1 is that the curing agent is replaced with toluene diisocyanate curing agent, namely TDI, with a solid content of 75% and a viscosity of 1800 mPa·s.

[0193] The differences between Examples 1 to 24 and Comparative Examples 1 to 3 are shown in Table 7:

[0194] Table 7

[0195]

[0196] An appropriate amount of color paste or color concentrate was added to the filler compositions of Examples 1 to 24 and Comparative Examples 1 to 3 to adjust the base color, and the respective A components and B components were mixed and applied on the base material. After curing, a primer was applied on the base material, and the properties of the filler compositions such as wiping time, filling property, adhesion, tinting power, and wiping property were measured. The measurement results are shown in Table 8:

[0197] Table 8

[0198]

[0199]

[0200] The test results show that in Examples 1 to 24, the filler compositions all have high solid content and low viscosity. Most of the filler compositions can be wiped for ≥20 minutes. The adhesion is level 1. The duct penetration is good. The duct can be filled well after wiping once. The wiping is smooth. The base color is transparent and shiny. The wood grain is clear. The primer sprayed on it does not bite the base color and does not collapse. Some of the cases can also be made without adding solvents or fillers.

[0201] The A component in the filler composition provided in the embodiment of the present application is compounded with saturated polyester resin, ricinoleic acid-containing material, and starch as the main raw materials, and can further add anti-settling agent, defoamer, filler, solvent and other ingredients, and then the A component can be used in combination with a curing agent. When the filler composition contains a curing agent, the curing agent can be a moisture-curing polyurethane curing agent containing diphenylmethane diisocyanate prepolymer in the B component, and the A component and the B component are compounded for use. The cross-linking reaction speed and cross-linking structure of the saturated polyester resin, the ricinoleic acid-containing material and the moisture-curing polyurethane curing agent are adjusted, so that the film formed after the filler construction has good permeability, good filling, anti-collapse, strong tinting power, good flexibility, and good solvent resistance.

[0202] The comparative examples use the alkyd resin system composition of the prior art as component A, or use the TDI curing agent of the prior art as component B, both of which have a relatively high viscosity and a relatively low solid content. When used, their permeability, wiping properties, filling properties and other properties are reduced to varying degrees compared to the properties of the filler composition of the embodiment of the present application.

[0203] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A filler composition, characterized in that: Comprising component A, the component A comprises the following components in parts by weight: Saturated polyester resin 15-20 parts 5-10 parts of ricinoleic acid-containing materials 25-35 parts of starch.

2. The filler composition according to claim 1, characterized in that: The ricinoleic acid-containing material comprises at least one of blown castor oil, hydrogenated castor oil, and castor oil long oil alkyd resin; And / or, the solid content of the ricinoleic acid-containing material is 95% to 100%; and / or, the viscosity of the ricinoleic acid-containing material is 90 to 120 mPa·s; And / or, the saturated polyester resin comprises a saturated polyol resin; And / or, the solid content of the saturated polyester resin is 95% to 100%; And / or, the viscosity of the saturated polyester resin is 3000-8000 mPa·s; And / or, the starch includes at least one of corn starch, potato starch, and tapioca starch; And / or, the starch is at least 325 mesh; And / or, the solid content of component A is 90% to 100%; And / or, the viscosity of component A is 3000-8000 mPa·s.

3. The filler composition according to claim 1 or 2, characterized in that: Also included is a B component, which includes the following components: Polyurethane curing agent; wherein, The polyurethane curing agent includes a moisture-curing polyurethane curing agent, and the moisture-curing polyurethane curing agent contains a diphenylmethane diisocyanate prepolymer; And / or, the solid content of the polyurethane curing agent is 95% to 100%; And / or, the viscosity of the polyurethane curing agent is 500-700 mPa·s.

4. The filler composition according to claim 3, characterized in that: In the filler composition, the weight portion of the B component is 100 parts; And / or, the weight ratio of the component A to the component B is 1:(0.5-0.8); And / or, the solid content of the filler composition is 93% to 100%.

5. The filler composition according to any one of claims 1, 2 and 4, characterized in that: The component A also includes at least one of a defoamer, an anti-settling agent, a filler, and a solvent.

6. The filler composition according to claim 5, characterized in that: In the A component, The weight portion of the defoamer is 0.3 to 0.5 parts; and / or, the weight portion of the anti-settling agent is 1.5 to 2.5 parts; And / or, the anti-settling agent includes at least one of fumed silica and bentonite; And / or, the weight portion of the filler is 20 to 30 parts; And / or, the filler includes at least one of mica powder, silica powder and talc powder; And / or, the weight parts of the solvent are 7 to 10 parts; And / or, the solvent includes at least one of glycerol acetone acetal and propylene glycol methyl ether propionate.

7. A method for preparing the filler composition according to any one of claims 1 to 6, characterized in that: The steps include: The ingredients contained in the A component are mixed.

8. The method for preparing the filler composition according to claim 7, characterized in that: The component A contains the defoamer, anti-settling agent, filler and solvent in the filler composition according to claim 5 or 6; the mixing process comprises the following steps: The saturated polyester resin, the ricinoleic acid-containing material, and the defoamer are subjected to a first mixing treatment to obtain a first mixed material; Performing a second mixing process on the first mixed material, the starch, the anti-settling agent, and the filler to obtain a second mixed material; The second mixed material and the solvent are subjected to a third mixing process.

9. The method for preparing the filler composition according to claim 8, characterized in that: The temperature of the first mixing treatment is 20-45° C., and the mixing speed is 700-800 rpm; And / or, the temperature of the second mixing treatment is 20-50° C., and the mixing speed is 1000-1200 rpm; And / or, the temperature of the third mixing treatment is 20-45° C., and the mixing speed is 700-800 rpm.

10. Use of the filler composition according to any one of claims 1 to 6 in furniture fillers and building fillers.

Citation Information

Patent Citations

  • Starch-based aqueous macromolecule-isocyanate wood adhesive and preparation method thereof

    CN101157833A

  • Water paint composition

    CN102827518A

  • Solvent-free two-component reactive type polyurethane adhesive applied to woodworking industry and using method of adhesive

    CN108531122A

  • Treated porous material

    CN109789596A

  • High-filling-property wood coloring filler

    CN109913041A