Manufacturing method of contact hole self-aligned MOSFET

By forming epitaxial layers and trenches on the substrate, and using ion implantation and etching techniques to form contact holes, the problems of thick oxygen oxidation and multiple thermal processes in the existing technology are solved, and the contact hole self-forming under small thermal processes is realized. alignment, reducing cell size and increasing channel current density.

CN118762997APending Publication Date: 2024-10-11SHANGHAI HUAHONG GRACE SEMICON MFG CORP
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410907028.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

In the prior art, polysilicon is over-etched and oxidized on both sides to form a self-aligned contact hole etching barrier layer, which results in thick oxygen oxidation and more thermal processes, affecting the substrate reverse expansion channel.

Method used

Form an epitaxial layer on the substrate and use ion implantation to form the body region, form a hard mask layer and sidewalls, etching to form the first and second gate trenches, form a gate dielectric layer and a polysilicon layer, and remove the mask The interlayer dielectric layer is etched to form contact holes and sidewalls to achieve self-alignment of contact holes.

Benefits of technology

In a small thermal process, the influence of contact hole overlay offset is eliminated, the cell size is reduced, and the channel current density is increased.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118762997A_ABST
    Figure CN118762997A_ABST
Patent Text Reader

Abstract

The invention provides a manufacturing method of a contact hole self-aligned MOSFET (Metal-Oxide-Semiconductor Field Effect Transistor), which comprises the following steps of: providing a substrate, forming an epitaxial layer on the substrate, and forming a body region on the upper surface of the epitaxial layer by utilizing ion implantation; forming a hard mask layer on the epitaxial layer, forming a first gate trench on the hard mask layer and the active region on the epitaxial layer below the hard mask layer, and keeping a preset distance between the bottom end of the first gate trench and the bottom end of the body region; a side wall is formed on the side wall of the first gate trench, the epitaxial layer at the bottom of the first gate trench is etched with the side wall and the hard mask layer as masks, a second gate trench is formed, and the bottom of the second trench extends out of the body region to the epitaxial layer; and forming a contact hole on the active region. The method comprises the following steps of: forming a gate dielectric layer and a gate polycrystalline silicon layer on the gate dielectric layer in the second gate trench; and removing the hard mask layer and the side wall. According to the method, the influence of contact hole overlay offset on the process can be further eliminated on the premise of ensuring a relatively small thermal process, the cell size is further reduced, and the channel current density is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductors, and in particular to a method for manufacturing a MOSFET with self-aligned contact holes. Background Art

[0002] For power MOSFET, contact hole injection will not only affect the well concentration, but also cause gate-source shorting problems.

[0003] Usually, the contact hole trench distance is: Min L + Shift L', where L is the minimum distance to ensure that the well injection does not have an excessive impact on the well, and L' is the lithography OVL (overlay mark) fluctuation.

[0004] For example: if the lithography fluctuation is 0.07um, the minimum line width of the trench is 0.3um, the minimum line width of the contact hole is 0.2um, and the minimum distance from the contact hole to the trench is 0.1um, according to the existing process, the device cell size is 0.3+0.2+0.1*2+0.07=0.77um.

[0005] In the prior art, a self-aligned contact hole etching barrier layer is formed by over-etching polysilicon and oxidizing both sides. The disadvantage is that the thick oxygen oxidation and the more thermal processes lead to the back expansion of the substrate affecting the channel.

[0006] In order to solve the above problems, it is necessary to propose a novel MOSFET manufacturing method with self-aligned contact holes. Summary of the invention

[0007] In view of the shortcomings of the prior art described above, the purpose of the present invention is to provide a MOSFET manufacturing method with self-aligned contact holes, which is used to solve the problem that the prior art uses a method of over-etching polysilicon and oxidizing both sides to form a self-aligned contact hole etching barrier layer, which is prone to cause thick oxygen oxidation and more thermal processes, resulting in substrate back-expansion affecting the channel.

[0008] To achieve the above-mentioned object and other related objects, the present invention provides a method for manufacturing a MOSFET with self-aligned contact holes, comprising:

[0009] Step 1: providing a substrate, forming an epitaxial layer on the substrate, and forming a body region on the upper surface of the epitaxial layer by ion implantation;

[0010] Step 2: forming a hard mask layer on the epitaxial layer, and forming a first gate trench on the hard mask layer and the active area on the epitaxial layer below the hard mask layer, wherein a bottom end of the first gate trench maintains a preset distance from a bottom end of the body region;

[0011] Step 3, forming a sidewall on the sidewall of the first gate trench, and etching the epitaxial layer at the bottom of the first gate trench using the sidewall and the hard mask layer as a mask to form a second gate trench, wherein the bottom of the second trench extends out of the body region to the epitaxial layer;

[0012] Step 4: forming a contact hole on the active area, which includes the following steps:

[0013] forming a gate dielectric layer and a gate polysilicon layer on the gate dielectric layer in the second gate trench;

[0014] Removing the hard mask layer and the sidewalls, and forming a source region located in the active region on the exposed epitaxial layer by ion implantation;

[0015] forming an interlayer dielectric layer filling the remaining first trench;

[0016] The epitaxial layer in the selected area is etched using the interlayer dielectric layer as a mask layer, and a contact hole located between the interlayer dielectric layers is formed on the epitaxial layer.

[0017] Preferably, the epitaxial layer in step one further includes a gate lead-out region.

[0018] Preferably, step two also includes forming a first gate trench on the gate lead-out region on the hard mask layer and the epitaxial layer thereunder; the sidewall in step three is also formed on the first gate trench on the gate lead-out region; and the second gate trench is formed at the bottom of the first gate trench on the gate lead-out region in step three.

[0019] Preferably, in step four, the gate dielectric layer is first formed on the gate lead-out region and the second gate trench on the active region; and then the gate polysilicon layer is formed to cover the epitaxial layer and fill the first gate trench.

[0020] Preferably, the method for forming contact holes on the active area and the gate lead-out area in step 4 comprises: forming a photoresist layer on the gate polysilicon layer; photolithographically opening the photoresist layer on the active area to expose the gate polysilicon layer thereon, etching the gate polysilicon layer on the active area to the upper surface of the second gate trench; removing the hard mask layer and the sidewall on the active area; forming a source region located in the active area on the exposed epitaxial layer by ion implantation; forming a source region on the epitaxial layer by deposition and grinding; The invention relates to a method for forming an interlayer dielectric layer covering the active area and the gate lead-out area; forming a groove on the interlayer dielectric layer of the first gate groove in the gate lead-out area by photolithography and etching, and removing the interlayer dielectric layer outside the first gate groove in the active area; etching the epitaxial layer in the active area and the gate lead-out area using the interlayer dielectric layer as a mask layer, forming a contact hole located between the interlayer dielectric layers on the epitaxial layer in the active area, and forming a contact hole on the gate polysilicon on the gate lead-out area.

[0021] Preferably, the method for forming contact holes on the active area and the gate lead-out area in step 4 includes: etching the gate polysilicon layer on the active area and the gate lead-out area to the upper surface of the second gate trench; removing the hard mask layer and the side wall; forming a source area located in the active area on the exposed epitaxial layer by ion implantation; forming the interlayer dielectric layer covering the active area and the gate lead-out area on the epitaxial layer by deposition and grinding methods; removing the interlayer dielectric layer outside the first gate trench in the active area by photolithography and etching methods; forming a groove on the interlayer dielectric layer on the gate lead-out area by photolithography and etching methods to expose the gate polysilicon layer below; etching the epitaxial layer in the active area and the gate lead-out area using the interlayer dielectric layer as a mask layer, forming a contact hole located between the interlayer dielectric layers on the epitaxial layer in the active area, and forming a contact hole on the gate polysilicon on the gate lead-out area.

[0022] Preferably, the method for forming contact holes on the active area and the gate lead-out area in step 4 includes: etching the gate polysilicon layer on the active area and the gate lead-out area to the upper surface of the second gate trench; removing the hard mask layer and the side wall; forming a source area located in the active area on the exposed epitaxial layer by ion implantation; forming the interlayer dielectric layer covering the active area and the gate lead-out area on the epitaxial layer by deposition and grinding methods; grinding the interlayer dielectric layer to the epitaxial layer; forming a groove on the interlayer dielectric layer on the gate lead-out area by photolithography and etching methods, so that the gate polysilicon layer below is exposed; forming a photoresist layer covering the epitaxial layer, photolithography opens the photoresist layer on the active area, and then etches the epitaxial layer using the interlayer dielectric layer as a mask layer, and forming a contact hole located between the interlayer dielectric layers on the epitaxial layer.

[0023] Preferably, the etching method in step three is dry etching.

[0024] Preferably, in step four, the hard mask layer and the sidewalls are removed by wet etching.

[0025] Preferably, the method for forming the gate dielectric layer and the gate polysilicon layer in step four includes: depositing the gate dielectric layer and the gate polysilicon layer in the first and second gate trenches in sequence; and then etching the gate dielectric layer and the gate polysilicon layer so that they remain in the second gate trench.

[0026] Preferably, the material of the gate dielectric layer in step 4 is silicon dioxide.

[0027] Preferably, the method of etching the epitaxial layer in step 4 is dry etching.

[0028] Preferably, the method of forming the interlayer dielectric layer filling the remaining first trench in step 4 includes: forming an interlayer dielectric layer covering the epitaxial layer, and etching back the interlayer dielectric layer until the epitaxial layer is exposed.

[0029] Preferably, the material of the interlayer dielectric layer in step 4 is silicon dioxide.

[0030] Preferably, the method of etching the epitaxial layer and the gate polysilicon layer in steps three and four is dry etching.

[0031] Preferably, the contact hole on the active area in step four is etched to below the first gate trench.

[0032] Preferably, the method is used for manufacturing vertical power devices.

[0033] As described above, the contact hole self-aligned MOSFET manufacturing method of the present invention has the following beneficial effects:

[0034] The present invention can further eliminate the influence of contact hole overlay offset on the process under the premise of ensuring a smaller thermal process, thereby further reducing the cell size and improving the channel current density. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 Shown is a schematic diagram of the distance from the contact hole to the trench in the prior art;

[0036] Figure 2 Shown is a schematic diagram of the process flow of Embodiment 1 of the present invention;

[0037] Figure 3 Shown are schematic diagrams of forming a first gate trench according to embodiments 1 to 4 of the present invention;

[0038] Figure 4 Shown are schematic diagrams of forming sidewalls according to embodiments 1 to 4 of the present invention;

[0039] Figure 5 Shown are schematic diagrams of forming a second gate trench according to embodiments 1 to 4 of the present invention;

[0040] Figure 6 It is a schematic diagram showing the formation of a gate dielectric layer and a gate polysilicon layer according to the first embodiment of the present invention;

[0041] Figure 7 It is a schematic diagram of forming a source region according to the first embodiment of the present invention;

[0042] Figure 8 It is a schematic diagram showing the formation of an interlayer dielectric layer according to the first embodiment of the present invention;

[0043] Fig. 9 It is a schematic diagram of a grinding interlayer dielectric layer according to a first embodiment of the present invention;

[0044] Fig.10 It is a schematic diagram showing the formation of a contact hole according to the first embodiment of the present invention;

[0045] Fig.11 Shown are schematic diagrams of forming a first gate trench according to embodiments 2 to 4 of the present invention;

[0046] Fig.12 Shown are schematic diagrams of forming sidewalls in Embodiments 2 to 4 of the present invention;

[0047] Fig.13 Shown are schematic diagrams of forming a second gate trench according to embodiments 2 to 4 of the present invention;

[0048] Fig.14 It is a schematic diagram showing the formation of a gate polysilicon layer according to the second embodiment of the present invention;

[0049] Fig.15 It is a schematic diagram showing the upper surface of etching the gate polysilicon layer on the active area to the second gate trench according to the second embodiment of the present invention;

[0050] Fig.16 It is a schematic diagram of forming a source region according to the second embodiment of the present invention;

[0051] Fig.17 It is a schematic diagram showing the formation of an interlayer dielectric layer according to the second embodiment of the present invention;

[0052] Fig.18 It is a schematic diagram of etching an interlayer dielectric layer according to the second embodiment of the present invention;

[0053] Fig.19 It is a schematic diagram showing the formation of contact holes according to the second embodiment of the present invention;

[0054] Fig. 20 It is a schematic diagram of a patterned gate polysilicon layer according to the third embodiment of the present invention;

[0055] Fig.21 It is a schematic diagram of forming a source region according to the third embodiment of the present invention;

[0056] Fig. 22 It is a schematic diagram showing the formation of an interlayer dielectric layer according to the third embodiment of the present invention;

[0057] Fig.23 It is a schematic diagram of etching an interlayer dielectric layer according to the third embodiment of the present invention;

[0058] Fig.24 It is a schematic diagram showing the formation of a groove on the gate lead-out region according to the third embodiment of the present invention;

[0059] Fig.25 It is a schematic diagram showing the formation of contact holes according to the third embodiment of the present invention;

[0060] Fig.26 It is a schematic diagram of a patterned gate polysilicon layer according to a fourth embodiment of the present invention;

[0061] Fig. 27 It is a schematic diagram of forming a source region according to a fourth embodiment of the present invention;

[0062] Fig.28 It is a schematic diagram showing the formation of an interlayer dielectric layer according to a fourth embodiment of the present invention;

[0063] Fig.29 It is a schematic diagram of etching an interlayer dielectric layer according to a fourth embodiment of the present invention;

[0064] Fig.30 It is a schematic diagram showing the formation of a groove on the gate lead-out region according to the fourth embodiment of the present invention;

[0065] Fig.31 It shows a schematic diagram of forming a contact hole according to the fourth embodiment of the present invention;. DETAILED DESCRIPTION

[0066] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0067] Embodiment 1

[0068] See also Figure 2 The present invention provides a method for manufacturing a MOSFET with self-aligned contact holes on an active area, comprising:

[0069] Step 1: providing a substrate, forming an epitaxial layer 101 on the substrate, and forming a body region 102 on the upper surface of the epitaxial layer 101 by ion implantation;

[0070] Step 2: forming a hard mask layer 103 on the epitaxial layer 101, forming a first gate trench A1 on the hard mask layer 103 and the active region on the epitaxial layer 101 below, with the bottom of the first gate trench A1 and the bottom of the body region 102 maintaining a preset distance, forming a Figure 3 The structure shown;

[0071] Step 3: forming a sidewall 104 on the sidewall of the first gate trench A1, forming a sidewall 104 as shown in FIG. Figure 4 The structure shown in FIG. 1 is etched with the sidewall 104 and the hard mask layer 103 as a mask to form the epitaxial layer 101 at the bottom of the first gate trench A1, and the second gate trench A2 is formed. The bottom of the second trench extends out of the body region 102 to the epitaxial layer 101, and the structure shown in FIG. Figure 5 The structure shown;

[0072] Step 4: forming a contact hole on the active area, which includes the following steps:

[0073] A gate dielectric layer 105 and a gate polysilicon layer 106 located on the gate dielectric layer 105 are formed in the second gate trench A2 to form a gate dielectric layer 105. Figure 6 The structure shown;

[0074] The hard mask layer 103 and the sidewall 104 are removed, and a source region 107 located in the active region is formed on the exposed epitaxial layer 101 by ion implantation, so as to form a Figure 7 The structure shown;

[0075] Forming an interlayer dielectric layer 108 filling the remaining first trench A1: forming an interlayer dielectric layer 108 covering the epitaxial layer 101, forming Figure 8 The structure shown in FIG. 1 is formed by etching back the interlayer dielectric layer 108 until the epitaxial layer 101 is exposed. Fig. 9 The structure shown;

[0076] The interlayer dielectric layer 108 is used as a mask layer to etch the epitaxial layer 101 in the selected area, and a contact hole located between the interlayer dielectric layer 108 is formed on the epitaxial layer 101, as shown in FIG. Fig.10 The structure shown.

[0077] In this embodiment, the etching method in step three is dry etching.

[0078] In this embodiment, in step 4, the hard mask layer 103 and the sidewall spacer 104 are removed by wet etching.

[0079] In this embodiment, the method of forming the gate dielectric layer 105 and the gate polysilicon layer 106 in step 4 includes: depositing the gate dielectric layer 105 and the gate polysilicon layer 106 in the first and second gate trenches in sequence; and then etching the gate dielectric layer 105 and the gate polysilicon layer 106 so that they remain in the second gate trench A2.

[0080] In this embodiment, the material of the gate dielectric layer 105 in step 4 is silicon dioxide.

[0081] In this embodiment, the material of the interlayer dielectric layer 108 in step 4 is silicon dioxide.

[0082] In this embodiment, the method of etching the epitaxial layer 101 and the gate polysilicon layer 106 in steps 3 and 4 is dry etching.

[0083] In this embodiment, the contact hole on the active area in step 4 is etched to below the first gate trench A1.

[0084] In this embodiment, the method is used for manufacturing vertical power devices, such as MOSFET, SGT, IGBT, SJ, etc.

[0085] Embodiment 2

[0086] In this embodiment, the epitaxial layer 101 in step 1 further includes a gate lead-out region.

[0087] In this embodiment, step 2 further includes forming a first gate trench A1 on the gate lead-out region on the hard mask layer 103 and the epitaxial layer 101 thereunder, forming a gate electrode as shown in FIG. Fig.11 The structure shown in step three; the sidewall 104 is also formed on the first gate trench A1 on the gate lead-out region, forming a Fig.12The structure shown in step 3 is formed with a second gate trench at the bottom of the first gate trench A1 on the gate lead-out region, forming a Fig.13 The structure shown.

[0088] In this embodiment, in step 4, a gate dielectric layer 105 is first formed on the gate lead-out region and the second gate trench A2 on the active region; then a gate polysilicon layer 106 is formed covering the epitaxial layer 101 and filling the first gate trench A1, forming Fig.14 The structure shown.

[0089] The contact holes of the gate lead-out region and the active region may also be formed using different processes. For detailed description, the present invention further lists the following embodiments for specific description:

[0090] In this embodiment, the method for forming contact holes on the active area and the gate lead-out area in step 4 includes: forming a photoresist layer on the gate polysilicon layer 106; photolithography opens the photoresist layer on the active area to expose the gate polysilicon layer 106 thereon, and etches the gate polysilicon layer 106 on the active area to the upper surface of the second gate trench to form a structure as shown in 15; removes the hard mask layer 103 and the sidewall 104 on the active area; uses ion implantation to form a source region 107 located in the active area on the exposed epitaxial layer 101, and forms a structure as shown in 15. Fig.16 The structure shown in FIG. 1 is formed by deposition and grinding on the epitaxial layer 101 to cover the active area and the gate lead-out area. The interlayer dielectric layer 108 is formed as shown in FIG. Fig.17 Using photolithography and etching methods, a trench is formed on the interlayer dielectric layer 108 of the first gate trench in the gate lead-out region, and the interlayer dielectric layer 108 outside the first gate trench A1 in the active region is removed to form a Fig.18 The structure shown in FIG. 1 is a structure shown in FIG. 1 ; the epitaxial layer 101 in the active area and the gate lead-out area is etched using the interlayer dielectric layer 108 as a mask layer, a contact hole is formed between the interlayer dielectric layer 108 on the epitaxial layer 101 in the active area, and a contact hole is formed on the gate polysilicon on the gate lead-out area, forming a structure shown in FIG. Fig.19 The structure shown.

[0091] In this embodiment, the etching method in step three is dry etching.

[0092] In this embodiment, in step 4, the hard mask layer 103 and the sidewall spacer 104 are removed by wet etching.

[0093] In this embodiment, the method of forming the gate dielectric layer 105 and the gate polysilicon layer 106 in step 4 includes: depositing the gate dielectric layer 105 and the gate polysilicon layer 106 in the first and second gate trenches in sequence; and then etching the gate dielectric layer 105 and the gate polysilicon layer 106 so that they remain in the second gate trench A2.

[0094] In this embodiment, the material of the gate dielectric layer 105 in step 4 is silicon dioxide.

[0095] In this embodiment, the material of the interlayer dielectric layer 108 in step 4 is silicon dioxide.

[0096] In this embodiment, the method of etching the epitaxial layer 101 and the gate polysilicon layer 106 in steps 3 and 4 is dry etching.

[0097] In this embodiment, the contact hole on the active area in step 4 is etched to below the first gate trench A1.

[0098] In this embodiment, the method is used for manufacturing vertical power devices, such as MOSFET, SGT, IGBT, SJ, etc.

[0099] Embodiment 3

[0100] In this embodiment, the epitaxial layer 101 in step 1 further includes a gate lead-out region.

[0101] In this embodiment, step 2 further includes forming a first gate trench A1 on the gate lead-out region on the hard mask layer 103 and the epitaxial layer 101 thereunder, forming a gate electrode as shown in FIG. Fig.11 The structure shown in step three; the sidewall 104 is also formed on the first gate trench A1 on the gate lead-out region, forming a Fig.12 The structure shown in step 3 is formed with a second gate trench at the bottom of the first gate trench A1 on the gate lead-out region, forming a Fig.13 The structure shown.

[0102] In this embodiment, in step 4, a gate dielectric layer 105 is first formed on the gate lead-out region and the second gate trench A2 on the active region; then a gate polysilicon layer 106 is formed covering the epitaxial layer 101 and filling the first gate trench A1, forming Fig.14 The structure shown.

[0103] The contact holes of the gate lead-out region and the active region may also be formed using different processes. For detailed description, the present invention further lists the following embodiments for specific description:

[0104] In this embodiment, the method of forming the contact hole on the active area and the gate lead-out area in step 4 includes: etching the gate polysilicon layer 106 on the active area and the gate lead-out area to the upper surface of the second gate trench to form Fig. 20 The structure shown; removing the hard mask layer 103 and the sidewall 104; using ion implantation to form a source region 107 located in the active region on the exposed epitaxial layer 101, forming a Fig.21 The structure shown in FIG. 1 is formed by deposition and grinding on the epitaxial layer 101 to cover the active area and the gate lead-out area. The interlayer dielectric layer 108 is formed as shown in FIG. Fig. 22The structure shown in FIG. 1 is a structure shown in FIG. 1; the interlayer dielectric layer 108 outside the first gate trench in the active area is removed by photolithography and etching to form a structure shown in FIG. Fig.23 Using photolithography and etching methods, a groove is formed on the interlayer dielectric layer 108 on the gate lead-out region, so that the gate polysilicon layer 106 below is exposed, forming a Fig.24 The structure shown in FIG. 1 is a structure shown in FIG. 1 ; the epitaxial layer 101 in the active area and the gate lead-out area is etched using the interlayer dielectric layer 108 as a mask layer, a contact hole is formed between the interlayer dielectric layer 108 on the epitaxial layer 101 in the active area, and a contact hole is formed on the gate polysilicon on the gate lead-out area, forming a structure shown in FIG. Fig.25 The structure shown.

[0105] In this embodiment, the etching method in step three is dry etching.

[0106] In this embodiment, in step 4, the hard mask layer 103 and the sidewall spacer 104 are removed by wet etching.

[0107] In this embodiment, the method of forming the gate dielectric layer 105 and the gate polysilicon layer 106 in step 4 includes: depositing the gate dielectric layer 105 and the gate polysilicon layer 106 in the first and second gate trenches in sequence; and then etching the gate dielectric layer 105 and the gate polysilicon layer 106 so that they remain in the second gate trench A2.

[0108] In this embodiment, the material of the gate dielectric layer 105 in step 4 is silicon dioxide.

[0109] In this embodiment, the material of the interlayer dielectric layer 108 in step 4 is silicon dioxide.

[0110] In this embodiment, the method of etching the epitaxial layer 101 and the gate polysilicon layer 106 in steps 3 and 4 is dry etching.

[0111] In this embodiment, the contact hole on the active area in step 4 is etched to below the first gate trench A1.

[0112] In this embodiment, the method is used for manufacturing vertical power devices, such as MOSFET, SGT, IGBT, SJ, etc.

[0113] Embodiment 4

[0114] In this embodiment, the epitaxial layer 101 in step 1 further includes a gate lead-out region.

[0115] In this embodiment, step 2 further includes forming a first gate trench A1 on the gate lead-out region on the hard mask layer 103 and the epitaxial layer 101 thereunder, forming a gate electrode as shown in FIG. Fig.11 The structure shown in step three; the sidewall 104 is also formed on the first gate trench A1 on the gate lead-out region, forming a Fig.12 The structure shown in step 3 is formed with a second gate trench at the bottom of the first gate trench A1 on the gate lead-out region, forming a Fig.13 The structure shown.

[0116] In this embodiment, in step 4, a gate dielectric layer 105 is first formed on the gate lead-out region and the second gate trench A2 on the active region; then a gate polysilicon layer 106 is formed covering the epitaxial layer 101 and filling the first gate trench A1, forming Fig.14 The structure shown.

[0117] The contact holes of the gate lead-out region and the active region may also be formed using different processes. For detailed description, the present invention further lists the following embodiments for specific description:

[0118] In this embodiment, the method of forming the contact hole on the active area and the gate lead-out area in step 4 includes: etching the gate polysilicon layer 106 on the active area and the gate lead-out area to the upper surface of the second gate trench to form Fig.26 The structure shown; removing the hard mask layer 103 and the sidewall 104; using ion implantation to form a source region 107 located in the active region on the exposed epitaxial layer 101, forming a Fig. 27 The structure shown in FIG. 1 is formed by deposition and grinding on the epitaxial layer 101 to cover the active area and the gate lead-out area. The interlayer dielectric layer 108 is formed as shown in FIG. Fig.28 Grinding the interlayer dielectric layer 108 to the epitaxial layer 101, forming a Fig.29 Using photolithography and etching methods, a groove is formed on the interlayer dielectric layer 108 on the gate lead-out region, so that the gate polysilicon layer 106 below is exposed, forming a Fig.30 The structure shown in FIG. 1 is formed by forming a photoresist layer covering the epitaxial layer 101, photolithography opens the photoresist layer on the active area, and then the epitaxial layer 101 is etched with the interlayer dielectric layer 108 as a mask layer, and a contact hole is formed on the epitaxial layer 101 between the interlayer dielectric layer 108, forming a structure as shown in FIG. Fig.31 The structure shown.

[0119] In this embodiment, the etching method in step three is dry etching.

[0120] In this embodiment, in step 4, the hard mask layer 103 and the sidewall spacer 104 are removed by wet etching.

[0121] In this embodiment, the method of forming the gate dielectric layer 105 and the gate polysilicon layer 106 in step 4 includes: depositing the gate dielectric layer 105 and the gate polysilicon layer 106 in the first and second gate trenches in sequence; and then etching the gate dielectric layer 105 and the gate polysilicon layer 106 so that they remain in the second gate trench A2.

[0122] In this embodiment, the material of the gate dielectric layer 105 in step 4 is silicon dioxide.

[0123] In this embodiment, the material of the interlayer dielectric layer 108 in step 4 is silicon dioxide.

[0124] In this embodiment, the method of etching the epitaxial layer 101 and the gate polysilicon layer 106 in steps 3 and 4 is dry etching.

[0125] In this embodiment, the contact hole on the active area in step 4 is etched to below the first gate trench A1.

[0126] In this embodiment, the method is used for manufacturing vertical power devices, such as MOSFET, SGT, IGBT, SJ, etc.

[0127] That is, the present invention adopts two-step trench etching, and a side wall 104 is formed between the first step trench etching and the second step trench etching to achieve a stepped trench morphology, wherein the lower second gate trench A2 is used as a gate oxide and polysilicon filling area, and the upper trench is filled with an interlayer dielectric layer 108 as a contact hole self-aligned etching barrier layer, thereby ensuring self-aligned etching of the contact hole.

[0128] With the self-alignment process, the minimum distance from the contact hole to the trench is determined by the sidewall 104, and there is no need to consider the misalignment between the contact hole and the trench; on the other hand, the line width of the contact hole in the cell area is determined by the gate line width of the first gate trench A1, which is not limited by the contact hole lithography machine, and can be 0.1um or less. For example, the size of the device cell can be reduced to: 0.3+0.1+0.1*2+0=0.6um, and the cell area density is increased by 12%, that is, the channel conduction current is increased by 12%.

[0129] This process can further eliminate the impact of contact hole overlay offset on the process while ensuring a smaller thermal process, thereby further reducing the cell size and improving the channel current density.

[0130] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner. Therefore, the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0131] In summary, the present invention can further eliminate the influence of contact hole overlay offset on the process under the premise of ensuring a smaller thermal process, thereby further reducing the cell size and improving the channel current density. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0132] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for manufacturing a MOSFET with self-aligned contact holes. It is characterized in that At least: Step 1: providing a substrate, forming an epitaxial layer on the substrate, and forming a body region on the upper surface of the epitaxial layer by ion implantation; Step 2: forming a hard mask layer on the epitaxial layer, and forming a first gate trench on the hard mask layer and the active area on the epitaxial layer below the hard mask layer, wherein a bottom end of the first gate trench maintains a preset distance from a bottom end of the body region; Step 3, forming a sidewall on the sidewall of the first gate trench, and etching the epitaxial layer at the bottom of the first gate trench using the sidewall and the hard mask layer as a mask to form a second gate trench, wherein the bottom of the second trench extends out of the body region to the epitaxial layer; Step 4: forming a contact hole on the active area, which includes the following steps: forming a gate dielectric layer and a gate polysilicon layer on the gate dielectric layer in the second gate trench; Removing the hard mask layer and the sidewalls, and forming a source region located in the active region on the exposed epitaxial layer by ion implantation; forming an interlayer dielectric layer filling the remaining first trench; The epitaxial layer in the selected area is etched using the interlayer dielectric layer as a mask layer, and a contact hole located between the interlayer dielectric layers is formed on the epitaxial layer.

2. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, Features: The epitaxial layer in step one also includes a gate lead-out region.

3. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 2, Features: Step two also includes forming a first gate trench on the gate lead-out region on the hard mask layer and the epitaxial layer thereunder; the sidewall in step three is also formed on the first gate trench on the gate lead-out region; and the second gate trench is formed at the bottom of the first gate trench on the gate lead-out region in step three.

4. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 3, Features: In step 4, the gate dielectric layer is first formed on the gate lead-out region and the second gate trench on the active region; and then the gate polysilicon layer is formed to cover the epitaxial layer and fill the first gate trench.

5. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 4, Features: The method for forming contact holes on the active area and the gate lead-out area in step 4 includes: forming a photoresist layer on the gate polysilicon layer; photolithographically opening the photoresist layer on the active area to expose the gate polysilicon layer thereon, etching the gate polysilicon layer on the active area to the upper surface of the second gate trench; removing the hard mask layer and the sidewall on the active area; forming a source region located in the active area on the exposed epitaxial layer by ion implantation; forming a covering layer on the epitaxial layer by deposition and grinding; The interlayer dielectric layer covers the active area and the gate lead-out area; using photolithography and etching methods, a groove is formed on the interlayer dielectric layer of the first gate groove in the gate lead-out area, and the interlayer dielectric layer outside the first gate groove in the active area is removed; using the interlayer dielectric layer as a mask layer to etch the epitaxial layer in the active area and the gate lead-out area, forming a contact hole located between the interlayer dielectric layers on the epitaxial layer in the active area, and forming a contact hole on the gate polysilicon on the gate lead-out area.

6. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, Features: The method for forming contact holes on the active area and the gate lead-out area in step 4 includes: etching the gate polysilicon layer on the active area and the gate lead-out area to the upper surface of the second gate trench; removing the hard mask layer and the side wall; forming a source area located in the active area on the exposed epitaxial layer by ion implantation; forming the interlayer dielectric layer covering the active area and the gate lead-out area on the epitaxial layer by deposition and grinding methods; removing the interlayer dielectric layer outside the first gate trench in the active area by photolithography and etching methods; forming a groove on the interlayer dielectric layer on the gate lead-out area by photolithography and etching methods to expose the gate polysilicon layer below; etching the epitaxial layer in the active area and the gate lead-out area using the interlayer dielectric layer as a mask layer, forming a contact hole located between the interlayer dielectric layers on the epitaxial layer in the active area, and forming a contact hole on the gate polysilicon on the gate lead-out area.

7. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, Features: The method for forming contact holes on the active area and the gate lead-out area in step 4 includes: etching the gate polysilicon layer on the active area and the gate lead-out area to the upper surface of the second gate trench; removing the hard mask layer and the side wall; forming a source area located in the active area on the exposed epitaxial layer by ion implantation; forming the interlayer dielectric layer covering the active area and the gate lead-out area on the epitaxial layer by deposition and grinding methods; grinding the interlayer dielectric layer to the epitaxial layer; forming a groove on the interlayer dielectric layer on the gate lead-out area by photolithography and etching methods, so that the gate polysilicon layer below is exposed; forming a photoresist layer covering the epitaxial layer, photolithography opens the photoresist layer on the active area, and then etches the epitaxial layer using the interlayer dielectric layer as a mask layer, and forming a contact hole located between the interlayer dielectric layers on the epitaxial layer.

8. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: The etching method in step three is dry etching.

9. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: In step 4, the hard mask layer and the sidewalls are removed by wet etching.

10. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: The method for forming the gate dielectric layer and the gate polysilicon layer in step 4 includes: depositing the gate dielectric layer and the gate polysilicon layer in the first and second gate trenches in sequence; and then etching the gate dielectric layer and the gate polysilicon layer so that they remain in the second gate trench.

11. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: The material of the gate dielectric layer in step 4 is silicon dioxide.

12. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: The method for etching the epitaxial layer and the gate polysilicon layer in steps three and four is dry etching.

13. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, Features: The method of forming an interlayer dielectric layer filling the remaining first trench in step 4 includes: forming an interlayer dielectric layer covering the epitaxial layer, and etching back the interlayer dielectric layer until the epitaxial layer is exposed.

14. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: The material of the interlayer dielectric layer in step 4 is silicon dioxide.

15. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: In step 4, the method for etching the epitaxial layer and the gate polysilicon layer is dry etching.

16. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, 5, 6 or 7, Features: In step 4, the contact hole on the active area is etched to below the first gate trench.

17. The method for manufacturing a MOSFET with self-aligned contact holes according to claim 1, Features: The method is used for manufacturing vertical power devices.

Citation Information

Cited By

  • Power semiconductor device structure and manufacturing method thereof

    CN119815850A

  • Manufacturing method of U-shaped trench gate with inner side wall structure

    CN119947228A