Processing method for soft board appearance of rigid-flex board

By controlling the window size and alignment accuracy of the semi-cured adhesive sheet, the molding milling cutter is fished in the hard board area, which solves the problem of burrs during the molding of camera modules or consumer electronics soft and hard boards, improving quality and Production efficiency.

CN118765047AActive Publication Date: 2024-10-11GAODE (JIANGSU) ELECTRONIC TECH CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410958069.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-10-11
Estimated Expiration
2044-07-17

AI Technical Summary

Technical Problem

In the existing technology, during the molding process of hard-soft boards of camera modules or consumer electronics, burrs are easily produced when the milling cutter catches the soft boards, leading to poor quality problems such as crushing and scratches, and the looping process also causes problems such as crushing and scratches. Scrap removal wastes time and increases production costs.

Method used

By strictly controlling the window size and alignment accuracy of the semi-cured adhesive sheet, the molding milling cutter is fished in the hard board area, and steps such as quick pressing, baking and alignment fixtures are used to prevent the milling cutter from directly fishing the soft board. Laser cutting process is used to process the shape of the soft board.

Benefits of technology

Without increasing the process flow and cost, it avoids the generation of soft board burrs, improves the molding quality, simplifies waste cleaning, and reduces production time and costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118765047A_ABST
    Figure CN118765047A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of printed circuit boards, and particularly relates to a method for processing the appearance of a flexible board of a rigid-flex board, which comprises the following steps of: S1, providing the flexible board of a rigid-flex printed circuit board, and manufacturing circuit patterns on upper and lower copper foils of the flexible board; s2, laminating a covering film on the bending area after the browning treatment, and quickly pressing and baking the circuit for protecting the bending area; s3, punching the flexible board; s4, preparing a semi-cured adhesive sheet, and windowing and drilling holes in the bending area of the flexible board; s5, an alignment jig is manufactured, and a spring Pin is arranged at the punching position of the flexible board; s6, aligning and pre-pasting the soft board and the semi-cured adhesive sheet; s7, copper foils are arranged on the upper surface and the lower surface of the pre-pasted flexible board for pressing, and the flexible board is manufactured until the appearance is formed; s8, when the formed milling cutter is scooped, the milling cutter is scooped in the hard board area; and S9, processing the appearance of the flexible board. The method can solve the problem that burrs generated by a soft board are fished by a milling cutter when the soft and hard combined board is formed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of printed circuit boards, and specifically relates to a method for processing the appearance of a soft board of a hard-soft combination board, and is particularly suitable for a hard-soft combination board of a camera module or a consumer electronic product. Background Art

[0002] The characteristics of the rigid-flexible board of camera modules or consumer electronic products are thin board thickness, small size and high precision. The shape processing methods of the bending area of ​​the soft board are generally laser cutting or mold punching. During the forming process, the milling cutter will pick up the PI material of the soft board and cause burrs. If the shape processing method of the bending area of ​​the soft board is laser cutting, this burr will cause the laser cutting to be not transparent, and increasing the energy production will cause serious carbonization. If the shape processing method of the bending area of ​​the soft board is mold punching, this burr will stick back and remain on the mold, causing the soft board to be crushed, scratched and other defects. If laser cutting or mold punching is performed first and then forming, there will be the following two problems: First, when the shape of the soft board is only processed in one line, the PI material will be wrapped around the milling cutter, causing the milling cutter to pick up the shape poorly. Second, the shape of the soft board is processed in a round shape. The cleaning of the waste generated during the round shape processing is time-consuming and difficult to clean, which directly increases the production time. At the same time, the round shape processing is longer than the linear path, which also directly increases the production cost. Summary of the invention

[0003] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a method for processing the appearance of a soft board of a hard-flex board. The present invention strictly controls the window size of the semi-cured adhesive sheet and the alignment accuracy of the semi-cured adhesive sheet and the soft board, so that the forming milling cutter is caught in the hard board area, which can solve the problem of burrs when the milling cutter catches the soft board during the forming of the hard-flex board, and solve the problem of poor quality caused by crushing and scratching of the soft board due to burrs. It is especially suitable for the production of hard-flex boards for camera modules or consumer electronic products.

[0004] To achieve the above technical objectives, the technical solution adopted in the embodiment of the present invention is: a method for processing the shape of a soft board of a hard-flex board, comprising the following steps: Step S1, providing a rigid-flexible printed circuit board, wherein the upper and lower surfaces of the flexible printed circuit board respectively have an upper copper foil and a lower copper foil, and circuit patterns are made on the upper copper foil and the lower copper foil as required and circuit quality inspection is performed; Step S2, after the soft board with the circuit pattern made in step S1 is subjected to browning treatment, an upper cover film and a lower cover film are attached to the bending area to protect the circuit in the bending area, and quick pressing and baking are performed; Step S3, punching holes at selected positions on the soft board according to requirements to form no less than 4 first circular holes, and measuring the expansion and contraction ratio R of the soft board layer; Step S4, preparing a semi-cured adhesive sheet, and opening a window at the corresponding bending area of ​​the soft board, and simultaneously drilling a second circular hole at the corresponding punching position of the soft board, wherein the number and size of the second circular holes are the same as those of the first circular holes; Step S5, making a positioning jig, drilling a third circular hole on the jig at a position corresponding to the first circular hole, the third circular holes having the same number and size as the first circular holes, setting a spring pin at the drilling position, the size of the spring pin being 0.05 mm smaller than the size of the first circular hole; Step S6, pre-laminating the soft board and the semi-cured adhesive sheet using a positioning fixture, the pre-laminating temperature is 80-150° C., and the time is 10-60 seconds; Step S7, copper foil is arranged on the upper and lower surfaces of the semi-cured adhesive sheet in step S6, and pressed together, and formed into an outer shape according to the required process; Step S8, when the forming milling cutter is fishing, a fishing path is set 0.6-1.0mm away from the outer shape of the soft board, so that the milling cutter is fished in the hard board area to avoid the milling cutter directly fishing the soft board and causing burrs; Step S9, processing the shape of the soft board to complete the processing of the shape of the soft board of the hard-flex board.

[0005] Furthermore, the expansion / contraction ratio of the window in step S4 is the same as the measured expansion / contraction ratio R of the soft board, and the size of the window is 0.5 mm larger than the outer shape of the soft board.

[0006] Furthermore, the expansion / contraction ratio of the third circular hole in step S5 is the same as the measured expansion / contraction ratio R of the soft board.

[0007] Furthermore, in step S2, the quick pressing pressure of the upper covering film and the lower covering film is: 70-150kg, the quick pressing temperature is: 160-210°C, the quick pressing time is: 1-4 minutes, the baking temperature is: 100-190°C, and the baking time is: 60-200 minutes.

[0008] Furthermore, the semi-cured adhesive sheet in step S4 is a low-glue semi-cured adhesive sheet, and the glue flow amount thereof is less than 0.5 mm when the rigid-flex board is pressed together.

[0009] The technical solution in the embodiment of the present invention has the following beneficial effects: Without increasing the process flow and cost, the present invention takes into account the characteristic that the glue flow of the semi-cured adhesive sheet of the soft and hard combination board is less than 0.5mm when it is pressed, and makes a special design when opening the window, so as to ensure that the semi-cured adhesive sheet will not flow to the soft board, and ensure that the milling cutter will not pick up the PI material of the soft board during molding, thereby avoiding the defects caused by the burrs of the soft board. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1Schematic diagram of the cross-sectional structure of a rigid-flex board in an embodiment of the present invention.

[0011] Figure 2 Schematic diagram of the planar structure of the rigid-flex board in an embodiment of the present invention.

[0012] Figure 3 yes Figure 1 Schematic diagram of the cross-sectional structure of the medium-soft board layer.

[0013] Figure 4 yes Figure 1 Schematic diagram of the planar structure of the medium-soft board layer.

[0014] Figure 5 yes Figure 1 Schematic diagram of the cross-sectional structure of the covering film.

[0015] Figure 6 yes Figure 1 Schematic diagram of the planar structure of the covering membrane.

[0016] Figure 7 yes Figure 1 Schematic diagram of the cross-sectional structure of the semi-cured adhesive sheet.

[0017] Figure 8 yes Figure 1 Schematic diagram of the planar structure of the semi-cured adhesive sheet.

[0018] Fig. 9 yes Figure 1 Schematic diagram of the cross-sectional structure of the copper foil.

[0019] Fig.10 yes Figure 1 Schematic diagram of the cross-sectional structure of the middle fixture.

[0020] Fig.11 yes Figure 1 Schematic diagram of the plane structure of the middle fixture.

[0021] Fig.12 yes Figure 1 Schematic diagram of the cross-sectional structure of the spring pin.

[0022] Fig.13 Schematic diagram of the planar structure of the rigid-flex board in the embodiment of the present invention.

[0023] Fig.14 It is a schematic diagram of laser cutting of the flexible board shape of the present invention.

[0024] Explanation of the reference numerals: 1-flexible board; 1-1-upper copper foil; 1-2-lower copper foil; 1-3-upper covering film; 1-4-lower covering film; 2-first circular hole; 3-semi-cured adhesive sheet; 4-second circular hole; 5-copper foil; 6-spring Pin; 7-third circular hole. DETAILED DESCRIPTION

[0025] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by directional words such as "inside, outside", "up, down", "left, right", etc. are usually based on the directions or positional relationships shown in the drawings. They are only for the convenience of describing the present invention and simplifying the description. Unless otherwise specified, these directional words do not indicate or imply that the device or element referred to must have a specific direction or be constructed and operated in a specific direction. Therefore, they cannot be understood as limiting the scope of protection of the present invention.

[0026] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0027] Example 1 A method for processing the shape of a soft board of a hard-flex board comprises the following steps: Step S1. Figure 3 and 4 As shown, a rigid-flexible printed circuit board 1 is provided, and the upper and lower surfaces of the flexible board 1 respectively have an upper copper foil 1-1 and a lower copper foil 1-2, and circuit patterns are made on the upper copper foil 1-1 and the lower copper foil 1-2 as required and circuit quality inspection is performed; Step S2. Figure 5 and 6 As shown, the soft board 1 on which the circuit pattern is made in step S1 is subjected to browning treatment, and then the upper cover film 1-3 and the lower cover film 1-4 are attached to the bending area to protect the circuit in the bending area, and the fast pressing and baking are performed, the fast pressing temperature is 170°C, the fast pressing time is 180s, the pressure is 80kg, the baking temperature is 150°C, and the baking time is 90 minutes; Step S3. Use a CCD punching machine to punch out the first circular hole 2 for alignment with the semi-cured adhesive sheet 3 at the position selected according to the requirements on the soft board 1. The aperture of the first circular hole 2 is 2.0 mm, and the number is 20. The expansion and contraction ratio of the soft board is 50 ppm. Step S4. Figure 7 and 8 As shown, a low-flow semi-cured adhesive sheet 3 is prepared, and a window is simultaneously opened on the semi-cured adhesive sheet 3 corresponding to the bending area of ​​the soft board 1. The window expansion and contraction ratio is 50ppm, and the window size is 0.5mm larger than the shape of the soft board 1. Simultaneously, second circular holes 4 are drilled on the semi-cured adhesive sheet 3 corresponding to the punching position of the soft board. The number of the second circular holes 4 is 20, and the hole diameter is 2.0mm; Step S5. Fig.10 and 11As shown, a positioning jig is made, and a third circular hole 7 is drilled on the jig at a position corresponding to the first circular hole 2. The expansion and contraction ratio of the third circular hole 7 is 50ppm. A spring Pin 6 is set at the drilling position. The size of the spring Pin 6 is 1.95mm. Fig.12 and 13 As shown; Step S6. Pre-align the soft board 1 in step S3 and the semi-cured adhesive sheet 3 in step S4 using the alignment jig in step S5, with the pre-alignment temperature at 100° C. and the time for 20 seconds; Step S7. Fig. 9 As shown, in step S6, copper foil 5 is arranged on the upper and lower surfaces of the semi-cured adhesive sheet 3, and pressed together, and then formed into an outer shape according to the required process; Step S8. When the forming milling cutter is fishing, a fishing path is set 0.65mm away from the soft board shape, so that the milling cutter is fished in the hard board area, which solves the problem of the milling cutter directly fishing the soft board and causing burrs. Fig.14 As shown; Step S9. Use laser cutting technology to process the side shape of the flexible board 1 to complete the processing of the flexible board shape of the rigid-flexible board. Figure 1 , 2 and 13.

[0028] Example 2 A method for processing the shape of a soft board of a hard-flex board, comprising the following steps: Step S1. Provide a rigid-flexible printed circuit board 1, wherein the upper and lower surfaces of the flexible circuit board 1 have an upper copper foil 1-1 and a lower copper foil 1-2, respectively, and make circuit patterns on the upper copper foil 1-1 and the lower copper foil 1-2 as required and perform circuit quality inspection; Step S2. After the soft board 1 with the circuit pattern made in step S1 is browned, the upper cover film 1-3 and the lower cover film 1-4 are attached to the bending area to protect the circuit in the bending area and perform fast pressing and baking. The fast pressing temperature is 180°C, the fast pressing time is 170s, the pressure is 100kg, the baking temperature is 170°C, and the baking time is 60 minutes; Step S3. A first circular hole 2 for alignment with the semi-cured adhesive sheet 3 is punched out at a selected position on the soft board 1 using a CCD punching machine. The diameter of the first circular hole 2 is 2.55 mm, and the number is 30. The expansion and contraction ratio of the soft board is 80 ppm. Step S4. Prepare a low-flow semi-cured adhesive sheet 3, and simultaneously open a window on the semi-cured adhesive sheet 3 corresponding to the bending area of ​​the soft board 1, the window expansion and contraction ratio is 80ppm, and the window size is 0.6mm larger than the shape of the soft board 1, and simultaneously drill a second circular hole 4 on the semi-cured adhesive sheet 3 corresponding to the punching position of the soft board 1, the number of the second circular holes 4 is 30, and the hole diameter is 2.55mm; Step S5. Make a positioning jig, drill a third circular hole 7 on the jig at a position corresponding to the first circular hole 2, the expansion and contraction ratio of the third circular hole 7 is 80ppm, and set a spring pin 6 at the drilling position, the size of the spring pin 6 is 2.5mm; Step S6. Pre-align the soft board 1 in step S3 and the semi-cured adhesive sheet 3 in step S4 using the alignment jig in step S5, with the pre-alignment temperature at 110° C. and the time for 15 seconds; Step S7. Copper foil 5 is arranged on the upper and lower surfaces of the semi-cured adhesive sheet 3 in step S6, and pressed together, and formed into an outer shape according to the required process; Step S8. When the forming milling cutter fishes out the shape, a fishing path is set at 0.75 mm away from the shape of the soft board, so that the milling cutter fishes in the hard board area, thereby solving the problem of the milling cutter directly fishing out the soft board and causing burrs; Step S9. Finally, the side profile of the flexible board 1 is processed by laser cutting technology to complete the processing of the flexible board profile of the rigid-flexible board.

[0029] Finally, it should be noted that the above specific implementation methods are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to examples, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.

Claims

1. A method for processing the shape of a soft board of a hard-flex board, characterized in that: The following steps are involved: Step S1, providing a rigid-flexible printed circuit board (1), wherein the upper and lower surfaces of the flexible circuit board (1) respectively have an upper copper foil (1-1) and a lower copper foil (1-2), and circuit patterns are produced on the upper copper foil (1-1) and the lower copper foil (1-2) as required and circuit quality inspection is performed; Step S2, after the soft board (1) on which the circuit pattern is made in step S1 is subjected to browning treatment, an upper covering film (1-3) and a lower covering film (1-4) are attached to the bending area to protect the circuit in the bending area, and rapid pressing and baking are performed; Step S3, punching holes at selected positions on the soft board (1) as required to form no less than four first circular holes (2), and measuring the expansion / contraction ratio R of the soft board layer; Step S4, preparing a semi-cured adhesive sheet (3), and opening a window in the corresponding bending area of ​​the soft board, and simultaneously drilling a second circular hole (4) at the corresponding punching position of the soft board, wherein the second circular holes (4) are the same in number and size as the first circular holes (2); Step S5, making a positioning jig, drilling a third circular hole (7) on the jig at a position corresponding to the first circular hole (2), the third circular holes (7) being the same in number and size as the first circular holes (2), and setting a spring pin (6) at the drilling position, the size of the spring pin (6) being 0.05 mm smaller than the size of the first circular hole (2); Step S6, using an alignment jig to pre-laminate the soft board (1) and the semi-cured adhesive sheet (3), the pre-lamination temperature being 80-150° C. and the time being 10-60 seconds; Step S7, placing copper foil (5) on the upper and lower surfaces of the semi-cured adhesive sheet (3) in step S6, pressing them together, and shaping them into an outer shape according to a required process; Step S8, when the forming milling cutter is fishing, a fishing path is set at 0.6-1.0mm away from the outer shape of the soft board, so that the milling cutter is fished in the hard board area to avoid the milling cutter directly fishing the soft board and causing burrs; Step S9, processing the shape of the soft board (1) to complete the processing of the shape of the soft board of the hard-flex board.

2. The method for processing the shape of a rigid-flexible board according to claim 1, characterized in that: The expansion / contraction ratio of the window in step S4 is the same as the measured expansion / contraction ratio R of the soft board (1), and the size of the window is 0.5 mm larger than the outer shape of the soft board.

3. The method for processing the shape of a rigid-flex board according to claim 1, characterized in that: In step S5, the expansion / contraction ratio of the third circular hole (7) is the same as the measured expansion / contraction ratio R of the soft board (1).

4. The method for processing the shape of a rigid-flex board according to claim 1, characterized in that: In step S2, the quick pressing pressure of the upper covering film (1-3) and the lower covering film (1-4) is 70-150 kg, the quick pressing temperature is 160-210° C., the quick pressing time is 1-4 minutes, the baking temperature is 100-190° C., and the baking time is 60-200 minutes.

5. The method for processing the shape of a rigid-flex board according to claim 1, characterized in that: The semi-cured adhesive sheet (3) in step S4 is a low-glue semi-cured adhesive sheet, and its glue flow is less than 0.5 mm when the rigid-flex board is pressed together.

Citation Information

Patent Citations

  • Shape machining method for flexible printed circuit board of rigid-flexible combined circuit board

    CN104470214A

  • Rigid-flexible PCB high-precision molding method

    CN110337199A

  • Rigid-flexible printed circuit board

    KR1020100011584A