Rigid-flex printed circuit board manufacturing method for improving signal stability
By opening windows on the flexible insulating dielectric layer and filling it with resin ink, an insulating dielectric layer consistent with the rigid plate material is formed, which solves the problem of unsatisfactory copper uniformity and flatness of the hole wall in through-hole plating, and reduces the The waste of electroplating resources and waste liquid treatment are eliminated, and the signal stability is improved.
Patent Information
- Application Number
- CN202411071292.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-08-06
AI Technical Summary
The existing technology is difficult to ensure the uniformity and flatness of hole wall copper after through-hole plating in high-precision and high-reliability rigid-flex boards, and excessive plating leads to excessive plating waste liquid, which increases the burden of wastewater and waste liquid treatment.
By opening windows on the flexible insulating dielectric layer and filling it with resin ink, an insulating dielectric layer that is consistent with the rigid plate material is formed. The reverse processing process is used to replace the flexible insulating dielectric layer to provide good plating hole wall conditions. Use Perform plating using common plating parameters to reduce process adjustments and resource waste.
It improves the uniformity and flatness of the copper layer on the through-hole wall, reduces the waste of electroplating resources and the amount of waste water and waste liquid treatment, and meets the signal stability requirements.
Smart Images

Figure CN118765049A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of manufacturing a flexible circuit board or a rigid-flexible board, and in particular to a method for manufacturing a rigid-flexible board for improving signal stability. Background Art
[0002] A type of high-precision and high-reliability rigid-flexible board used in the fields of intelligent connected cars and low-altitude aircraft requires high signal transmission performance.
[0003] The vertical stacked structure of the rigid-flex PCB consists of a rigid board layer and a flexible board layer. Generally, the rigid insulating dielectric layer material of the rigid board layer is different from the flexible insulating dielectric layer material of the flexible board layer (for example, the rigid insulating dielectric layer material is epoxy resin, and the flexible insulating dielectric layer material is polyimide). Therefore, during the electroplating process, for the electroplating processing of the through holes of the rigid-flex PCB, due to the different materials, the copper plating effect of the through hole wall is also different, which easily leads to the problem that the through hole electroplating effect of the rigid board layer is better, while the electroplating effect of the flexible board layer is insufficient, resulting in insufficient copper thickness of the hole wall of the flexible board layer, or excessive thickness to produce copper nodules, etc., affecting the transmission of electrical signals or other models through the through hole.
[0004] To address the above issues, currently, the general method used is to adjust the electroplating parameters (for example, adjusting the electroplating current and time, using a small current and long time for electroplating), or to perform plasma treatment on the inner wall of the through hole, so as to improve the same basic conditions of different material layers during the electroplating process.
[0005] However, for products with high requirements on signal stability, this type of method still has difficulty in ensuring that the uniformity and flatness of the hole wall copper after through-hole electroplating meet the application requirements. On the other hand, there is the problem of excessive electroplating waste liquid resulting in excessive electroplating waste liquid, which increases the burden of wastewater and waste liquid treatment.
[0006] Based on the above background and problems, it is necessary to provide a method for manufacturing a rigid-flexible circuit board that improves signal stability. Summary of the invention
[0007] The present invention aims to provide a method for manufacturing a rigid-flexible board with improved signal stability, aiming at a rigid-flexible board with high signal stability requirements. In the through-hole electroplating process, the uniformity and flatness of the hole wall copper are difficult to meet the application requirements, and excessive electroplating generates a lot of waste water and waste liquid. The planar structure of the rigid-flexible board includes a rigid board area and a flexible board area, and the vertical stacked structure includes a rigid board layer and a flexible board layer; the manufacturing method includes the following steps: S10: Take a flexible insulating dielectric layer, make an opening window, and form a window dielectric layer; take a copper layer, and attach the window dielectric layer to one side of the copper layer to form a flexible copper-clad layer, and the through window forms a window groove.
[0008] S20: electroplating a tin layer onto the other side of the copper layer of the flexible copper clad layer to form a flexible copper clad tin-plated structure, taking a pad, and pasting one side of the tin layer onto the pad to form the pad support structure.
[0009] S30: preparing resin ink for the window opening groove, and performing baking, curing and grinding to form a resin filling plate.
[0010] S40: sequentially attaching a rigid-flexible insulating dielectric layer and a second copper layer to one side of the resin ink of the resin-filled board, removing the pad, and forming a flexible core board.
[0011] S50: Making a first rigid board layer on the upper surface of the flexible core board and a second rigid board layer on the lower surface to form a multi-layer laminated board.
[0012] S60: drilling through holes in the area of the multi-layer laminate corresponding to the resin ink, and performing electroplating, wherein the through holes form conductive vias, and a conductive via plate is formed as a whole.
[0013] S70: performing a cover-lifting process on the via plate to form the rigid-flexible board.
[0014] Furthermore, the tin layer is adhered to the pad by using an adhesive layer, and the adhesive layer is a polypropylene adhesive layer or an epoxy resin adhesive layer.
[0015] Furthermore, the resin ink is prepared in the window opening groove by using silk screen ink, and the resin ink is filled in the window opening groove by silk screen printing.
[0016] Furthermore, the main component of the resin ink is the same as the material of the rigid insulating medium layer of the rigid board layer.
[0017] Furthermore, the attaching of the rigid-flexible insulating dielectric layer is to attach a rigid insulating dielectric layer to the rigid board area and to attach a flexible insulating dielectric layer to the flexible board area.
[0018] Furthermore, the step of removing the backing plate includes milling from one side of the backing plate to the tin layer or the copper layer using a controlled depth milling method.
[0019] Furthermore, after removing the backing plate, tin stripping and copper reduction treatment is performed.
[0020] Furthermore, the forming of the multi-layer laminate is: Take a plurality of the flexible core boards and stack them. A rigid insulating dielectric layer is provided to the rigid board area between the layers of the adjacent flexible core boards, A flexible insulating dielectric layer is provided to the flexible board area between adjacent layers of the flexible core board.
[0021] Furthermore, the flexible insulating dielectric layer is pre-enlarged toward the rigid board area.
[0022] Furthermore, after the electroplating, the via holes are plugged, baked and cured, and polished in sequence.
[0023] The technical solution of the present invention uses a reverse processing flow to open windows in the flexible insulating dielectric layer and fill it with resin ink to form a pattern of the flexible insulating dielectric layer, so as to achieve the effect of replacing the flexible insulating dielectric layer with the resin ink at the through-hole position, so that the insulating dielectric layer material performance of the through-hole wall is similar, providing a good hole wall condition basis for subsequent electroplating processing, and having a good copper plating effect, effectively improving the uniformity and flatness of the hole wall copper layer. According to application requirements and structural requirements, a reasonable processing process is designed to form an organically coordinated manufacturing method with complete key process processes. At the same time, there is no need to perform special parameter adjustment, process adjustment, time adjustment, etc., and the electroplating parameters of ordinary electroplated through holes can be used for processing, which effectively saves electroplating resources and reduces the treatment and discharge of wastewater and waste liquid. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.
[0025] Figure 1 is a process flow chart of an embodiment of the present invention; Figure 2 A schematic diagram of the cross-sectional structure of a flexible copper clad layer formed in accordance with an embodiment of the present invention; Figure 3 A schematic diagram of a cross-sectional structure of a flexible copper-clad tin-plated structure formed in accordance with an embodiment of the present invention; Figure 4 A schematic diagram of a cross-sectional structure of a pad support structure formed in accordance with an embodiment of the present invention; Figure 5 A schematic diagram of a cross-sectional structure of a resin-filled plate formed in accordance with an embodiment of the present invention; Figure 6 It is a schematic diagram of the cross-sectional structure of the flexible core board formed in the embodiment of the present invention; Figure 7 A schematic diagram of a cross-sectional structure of a multi-layer laminated board formed in accordance with an embodiment of the present invention; Figure 8 A schematic diagram of a cross-sectional structure of a via plate formed in accordance with an embodiment of the present invention; Fig. 9A schematic diagram of a cross-sectional structure of a via-filling plate formed in accordance with an embodiment of the present invention; Fig.10 It is a schematic diagram of the cross-sectional structure of a rigid-flexible board manufactured according to an embodiment of the present invention.
[0026] Description of Figure Numbers: Label name Label name 10 Flexible copper cladding 50 Flexible core board 10A Rigid panel area 510 Rigid-flexible insulation layer 10B Flexible board area 5110 Rigid insulating dielectric layer 110 Window dielectric layer 5120 Flexible insulating dielectric layer 120 Copper Layer 60 Multilayer laminate 1110 Window slot 600 Rigid ply 20 Flexible copper tinned structure 610 First rigid board layer 210 Tin layer 620 Second rigid board layer 30 Pad support structure 70 Via Plate 310 Pad 710 Via holes 320 Adhesive layer 70A Filling vias 40 Resin filling board 710A Filling vias 410 Resin ink 80 Rigid-Flex PCB The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0027] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, inside, outside...) are only used to explain the relative position relationship, movement status, etc. between the components in a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0029] In addition, in the present invention, descriptions such as "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0030] In addition, the technical solutions between the various embodiments of the present invention can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0031] See also Figure 1 , Figure 1 It is a process flow chart of the production method of the present invention.
[0032] The rigid-flexible board for improving signal stability according to the embodiment of the present invention has a planar structure including a rigid board area 10A and a flexible board area 10B, and a vertical laminate structure including a rigid board layer (i.e., a rigid board layer 600 in the attached figure) and a flexible board layer (i.e., a flexible core board 50 in the attached figure); and a manufacturing method thereof includes: Figure 1 The key process flow shown in the figure has specific implementation steps as follows.
[0033] See also Figure 2 , Figure 2 It is a schematic diagram of the cross-sectional structure of a flexible copper clad layer formed in accordance with an embodiment of the present invention.
[0034] Step S10: Take a first flexible insulating dielectric layer, make an opening window, and form a window dielectric layer 110; take a copper layer 120, and attach the window dielectric layer 110 to one side of the copper layer 120 to form a flexible copper clad layer 10, and the through window forms a window groove 1110.
[0035] This embodiment adopts the method of first opening a window in the flexible insulating dielectric layer at the position where a hole needs to be drilled later, and removing the flexible insulating dielectric layer at this position (using resin to fill the hole in the next process), that is, removing the flexible insulating dielectric layer on the hole wall of the through hole, so as to create the basic condition of material consistency for the through hole; and because the flexible insulating dielectric layer needs to be opened to match the drilling position, the single-sided flexible copper clad laminate cannot be used to process the flexible insulating dielectric layer.
[0036] In this embodiment, a window is opened in the flexible insulating dielectric layer 110, and then attached and pressed onto the copper layer 120. Compared with the conventional process, a reverse process is formed (the conventional process is to make a window pattern on the copper layer of the copper clad laminate), which provides basic conditions for further making through holes.
[0037] See also Figure 3 Right now Figure 4 ; Figure 3 A schematic diagram of a cross-sectional structure of a flexible copper-clad tin-plated structure formed in accordance with an embodiment of the present invention; Figure 4 It is a schematic cross-sectional structure diagram of a pad support structure formed in accordance with an embodiment of the present invention.
[0038] Step S20: A tin layer 210 is electroplated on the other side of the copper layer 120 of the flexible copper clad layer 10 to form a flexible copper clad tin plated structure 20 ; a pad 310 is taken, and one side of the tin layer 210 is adhered to the pad to form the pad support structure 30 .
[0039] The electroplated tin layer 210 is processed by electroplating tin in the process of positive film pattern transfer. Before tin plating, a dry film needs to be pasted on the entire surface where the window groove 1110 is located, and a dry film pattern is made on the entire board to cover the entire surface, and a tin layer 210 is electroplated on the other side; the electroplated tin layer 210 can protect the copper layer and provide a transition layer for the processing of sticking the pad 310 and removing the pad 310 to prevent damage to the copper layer 120.
[0040] In this embodiment, the pad 310 is a phenolic resin pad, a wooden pad, an aluminum sheet or an epoxy resin pad; the tin layer is adhered to the pad 310 using an adhesive layer 320, and the adhesive layer 320 is a polypropylene adhesive layer or an epoxy resin adhesive layer.
[0041] The pad 310 supports the flexible board layer when subsequently making resin ink for the window groove and grinding and attaching the rigid-flexible insulating dielectric layer. Therefore, a pad with a certain hardness can be used. Generally, the pad is thicker than the flexible copper-clad tin-plated structure. It is worth mentioning that a scrapped board with a flat and smooth surface can be used as the pad 310, which effectively plays the role of waste recycling.
[0042] The adhesive layer 320 can not only effectively adhere the pad 310, but also because the tin grains of the tin layer 210 are relatively large, when the pad 310 is subsequently removed, the depth of the milling plate is easily caused to cause tin debris to get stuck in the milling cutter, affecting the milling accuracy, and the adhesive layer can promote the discharge of tin debris and improve the milling effect.
[0043] See also Figure 5 ; Figure 5 It is a schematic diagram of the cross-sectional structure of the resin filling plate formed in the embodiment of the present invention.
[0044] Step S30: A resin ink 410 is prepared in the window opening groove, and then baked, cured and polished to form a resin filling plate 40 .
[0045] In this embodiment, the resin ink 410 is made into the window groove 1110 by silk-screen printing ink, and the resin ink 410 is silk-screened and filled into the window groove; the main component of the resin ink 410 is the same as the material of the rigid insulating medium layer of the rigid board layer.
[0046] As described above, in this embodiment, the flexible insulating dielectric layer 110 at the position where a hole needs to be drilled is removed, and then a window groove 1110 is formed. Here, the window groove 1110 is filled with resin ink 410, which is equivalent to replacing the flexible insulating dielectric layer 110 at the position where a hole needs to be drilled with resin ink 410, so that the consistency of the material of the insulating dielectric layer on the hole wall of the through hole is improved, and in only one step, the main agent component of the resin ink 410 is the same as the material of the rigid insulating dielectric layer of the rigid board layer (for example: the rigid insulating dielectric layer is an epoxy resin composite glass fiber material, and the main agent component of the resin ink 410 is an epoxy resin material), which can effectively ensure the consistency of the material of the insulating dielectric layer on the hole wall, and provide a good consistency basic condition for the subsequent copper plating process on the hole wall of the through hole.
[0047] After the resin ink 410 is filled, it needs to be baked and cured, and then polished. Since the pad 310 plays a supporting role, a good baking, curing and polishing process can be formed. At the same time, it plays a restraining role to prevent the resin filling plate 40 from expanding and shrinking excessively during baking, curing and polishing.
[0048] See also Figure 6 , Figure 6 It is a schematic diagram of the cross-sectional structure of the flexible core board formed in the embodiment of the present invention.
[0049] Step S40: A rigid-flex insulating dielectric layer 510 (not marked in the drawings) and a second copper layer 520 are sequentially attached to one side of the resin ink 410 of the resin filling board 40 , and the pad 310 is removed to form a flexible core board 50 .
[0050] In this embodiment, the rigid-flexible insulating dielectric layer 510 is attached by attaching a rigid insulating dielectric layer 5110 to the rigid board area 10A and attaching a flexible insulating dielectric layer 5120 to the flexible board area 10B; the flexible insulating dielectric layer 5120 is pre-enlarged toward the rigid board area 10A, generally by 10μm to 100μm.
[0051] This processing method is a processing method of the reverse process of the ordinary processing process. The ordinary processing method is to use a double-sided copper clad laminate to make a circuit pattern, while the processing method of this embodiment is to first make an opening window on the flexible insulating dielectric layer 110, and then attach the pressed copper layer 120 to form a single-sided flexible copper clad laminate with a window pattern on the flexible insulating dielectric layer 110. Here, the insulating dielectric layer and the second copper layer 520 are attached to the single-sided flexible copper clad laminate (after the resin ink 410 is made), which is equivalent to forming a structural double-sided copper clad laminate.
[0052] Since it is necessary to ensure the rigidity of the rigid board area 10A, ensure the consistency of the insulating dielectric layer material of the through-hole wall, and ensure the flexibility of the flexible board area 10B, a rigid insulating dielectric layer 5110 is attached to the rigid board area 10A, and a flexible insulating dielectric layer 5120 is attached to the flexible board area 10B, thereby effectively adhering the second copper layer and ensuring the consistency of the materials.
[0053] The flexible insulating dielectric layer 5120 is pre-enlarged toward the rigid board area 10A, which can effectively ensure that when the subsequent layers of the rigid-flexible board are pressed together, the rigid board layer covers the flexible board layer, thereby preventing the flexible insulating dielectric layer 5120 of the flexible board layer from being delaminated.
[0054] In this embodiment, the step of removing the backing plate 310 is to use a controlled depth milling method to mill from one side of the backing plate 310 to the tin layer 210 or the copper layer 120 .
[0055] The pad 310 is an auxiliary tool layer in the processing process. After the processing process is completed, the pad 310 no longer needs to be retained. Since the copper layer 120 is covered with the tin layer 210, the depth control milling plate can use the tin layer 210 as a reference layer, that is, when the depth control milling reaches the tin layer 210, the depth milling will no longer continue. The tin layer 210 can effectively protect the copper layer 120 and prevent the milling plate from damaging the copper layer 120.
[0056] When the copper layer 120 is thicker, the depth-control milling plate may also be milled vertically to the copper layer 120 so as to better observe the depth of the depth-control milling plate.
[0057] In this embodiment, after removing the pad 310, tin stripping and copper reduction treatment are performed. Tin stripping is to use chemical methods and liquid medicine to remove excess tin layer 210 to prevent the invisible tin layer 210 from being not cleaned; when the selected copper layer 120 is a thicker copper layer, the copper layer 120 needs to be subjected to copper reduction treatment after tin stripping to meet the required copper thickness standard.
[0058] See also Figure 7 , Figure 7 It is a schematic diagram of the cross-sectional structure of a multi-layer laminated board formed in accordance with an embodiment of the present invention.
[0059] Step S50: A first rigid board layer 610 is fabricated on the upper surface of the flexible core board 50 , and a second rigid board layer 620 is fabricated on the lower surface, so as to form a multi-layer laminate board 60 .
[0060] In one embodiment, the multilayer laminate is formed by stacking a plurality of the flexible core boards 50, setting a rigid insulating medium layer 5110 in the rigid board area 10A between the layers of adjacent flexible core boards 50, and setting a flexible insulating medium layer 5120 in the flexible board area 10B between the layers of adjacent flexible core boards 50.
[0061] When the flexible board layer of the manufactured product is only a single-sided or double-sided flexible board, the flexible core board 50 is a single layer, and the first rigid board layer 610 and the second rigid board layer 610 are set and pressed together. When there are more than or equal to 3 layers of flexible boards and the flexible boards are layered structures, multiple flexible core boards 50 are required, which are stacked in sequence, and then the first rigid board layer 610 and the second rigid board layer 610 are set on the outermost layer and pressed together.
[0062] In this embodiment, the flexible insulating dielectric layer 5120 is pre-enlarged toward the rigid board area 10A. The reason for the pre-enlargement is the same as the above-mentioned pre-enlargement.
[0063] See also Figure 8 , Figure 8 It is a schematic diagram of the cross-sectional structure of the via plate formed in the embodiment of the present invention.
[0064] Step S60: Through holes are drilled in the area of the multi-layer laminate 60 corresponding to the resin ink 410 and electroplated, and the through holes form via holes 710, thereby forming a via hole plate 70 as a whole.
[0065] See also Fig. 9 , Fig. 9 It is a schematic diagram of the cross-sectional structure of the manufacturing method of the plugged via plate according to the embodiment of the present invention.
[0066] In this embodiment, the forming of the via plate 70 further includes: after the electroplating, the via holes 710 are plugged, baked and cured, and polished in sequence to form the plugged via holes 710A, and the entire board is formed into the plugged via plate 70A.
[0067] It can be seen that the position of the opening window processing of the flexible insulating dielectric layer 5120 and the position of the filling of the resin ink 410 correspond to the position of the through hole. The resin ink 410 replaces the flexible insulating dielectric layer 5120 of the corresponding layer, so that the insulating dielectric layer material of the hole wall has a consistent basis, so that the electroplated through hole processing does not need special parameter adjustment, process adjustment, time adjustment, etc., and the electroplating parameters of ordinary electroplated through holes can be used for processing, which effectively saves electroplating resources, reduces the treatment and discharge of wastewater and waste liquid, and the uniformity and flatness of the copper layer on the hole wall are also effectively improved.
[0068] It is worth noting that a single side of the area of the resin ink 410 is larger than the aperture of the through hole, and is generally 20 μm to 100 μm larger depending on the space allowed.
[0069] Furthermore, the via hole can be plugged, which is beneficial to improving the reliability of the via hole and enhancing the signal transmission performance of the via hole.
[0070] See also Fig.10 , Fig.10 It is a schematic diagram of the cross-sectional structure of a rigid-flexible board manufactured according to an embodiment of the present invention.
[0071] Step S70: The via plate 70 is uncovered to form the rigid-flexible board 80 ; the uncovering process may be performed using a conventional rigid-flexible board uncovering process.
[0072] It can be seen that the key to this embodiment is to first realize the process of designing and making the flexible insulating medium layer 5120 that replaces the through-hole area of the corresponding layer with the resin ink 410, then realize the process of effectively making the via 710, and realize the process of designing and making the flexible core board 50 to form the rigid-flexible board 80. The overall process has the characteristics of continuity and coordination between the previous and next steps. The filling process of the resin ink 410 is designed according to the production requirements of the via 710, thereby forming the processing process of the overall rigid-flexible board 80.
[0073] It is worth noting that due to the fact that the rigid-flexible board in the actual design and processing process is relatively precise, the actual structure diagram and the thickness of each layer, line width and other dimensions are all at the micron level. For example, the thickness of each layer is generally 5μm to 50μm. If the drawings in the specification are made according to the actual proportion, there will be a problem of unclear drawings. Therefore, in order to more clearly show the implementation process of the manufacturing method, the drawings of this embodiment are all schematic diagrams that enlarge the technical features, which do not represent the size of the actual structure diagram, nor do they represent enlarged views of the actual structure diagram in proportion.
[0074] The above are only preferred embodiments of the present invention, and are not intended to limit the patent scope of the present invention. All equivalent structural changes made using the contents of the present invention's specification and drawings, or directly / indirectly applied in other related technical fields, are included in the patent protection scope of the present invention.
Claims
1. A method for manufacturing a rigid-flexible board for improving signal stability, wherein the planar structure of the rigid-flexible board includes a rigid board area and a flexible board area, and the vertical stacked structure includes a rigid board layer and a flexible board layer; It is characterized in that The production method comprises the following steps: S10: taking a flexible insulating dielectric layer, making an opening window, and forming a window dielectric layer; taking a copper layer, and attaching the window dielectric layer to one side of the copper layer to form a flexible copper-clad layer, and the opening window forms a window groove; S20: electroplating a tin layer on the other side of the copper layer of the flexible copper-clad layer to form a flexible copper-clad tin-plated structure, taking a pad, and pasting one side of the tin layer on the pad to form the pad support structure; S30: preparing resin ink for the window opening groove, and performing baking, curing and grinding to form a resin filling plate; S40: attaching a rigid-flexible insulating dielectric layer and a second copper layer to one side of the resin ink of the resin-filled board in sequence, removing the backing plate, and forming a flexible core board; S50: forming a first rigid board layer on the upper surface of the flexible core board and a second rigid board layer on the lower surface to form a multi-layer laminated board; S60: drilling through holes in the area of the multi-layer laminate corresponding to the resin ink, and performing electroplating, wherein the through holes form conductive vias, and a conductive via plate is formed as a whole; S70: performing a cover-lifting process on the via plate to form the rigid-flexible board.
2. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1, characterized in that: The tin layer is adhered to the pad by using an adhesive layer, wherein the adhesive layer is a polypropylene adhesive layer or an epoxy resin adhesive layer.
3. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1, characterized in that: The resin ink is prepared into the window opening groove by using silk screen ink, and the resin ink is filled into the window opening groove by silk screen printing.
4. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1 or 3, characterized in that: The main component of the resin ink is the same as the material of the rigid insulating medium layer of the rigid board layer.
5. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1, characterized in that: The method of attaching the rigid-flexible insulating dielectric layer is to attach the rigid insulating dielectric layer to the rigid board area and to attach the flexible insulating dielectric layer to the flexible board area.
6. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1, characterized in that: The step of removing the backing plate is to use a controlled depth milling method to mill from one side of the backing plate to the tin layer or the copper layer.
7. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1 or 6, characterized in that: After the backing plate is removed, tin stripping and copper reduction treatment are performed.
8. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1, characterized in that: The forming of the multi-layer laminated board is to stack a plurality of the flexible core boards; Providing a rigid insulating dielectric layer to the rigid board area between adjacent layers of the flexible core board; A flexible insulating dielectric layer is provided to the flexible board area between adjacent layers of the flexible core board.
9. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 5 or 8, characterized in that: The flexible insulating dielectric layer is pre-enlarged toward the rigid board area.
10. A method for manufacturing a rigid-flexible board for improving signal stability as claimed in claim 1, characterized in that: The forming of the via plate further comprises: after the electroplating, plugging, baking and curing, and polishing the via holes in sequence.
Citation Information
Patent Citations
Rigid-flex board and manufacture method thereof
CN103974559A
Rigid-flex printed circuit board and manufacturing method thereof
CN112020217A
Rigid-flex printed circuit board with plug-in holes and manufacturing method of rigid-flex printed circuit board
CN114340220A
Rigid -flex board
CN206118161U
Method for preparing PCB, and PCB
WO2023109051A1