Anode structure, OLED display panel and preparation method of OLED display panel

By adopting an "I"-shaped anode design in the WOLED display panel and using the bottom insulating material layer, the middle metal layer and the top transparent layer to cut off the organic material layer, the problem of lateral leakage current is solved and a more stable display effect and better performance are achieved. Low risk of leakage.

CN118765124APending Publication Date: 2024-10-11LAKESIDE LIGHTNING SEMICONDUCTOR (JIANGSU) CO
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410939276.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

There is a lateral leakage current problem in existing WOLED display panels, which causes organic semiconductor materials to leak between the pixel definition layers, affecting the display effect.

Method used

An "I"-shaped structure including a complementary metal oxide semiconductor layer, a bottom insulating material layer, a middle metal layer and a top transparent layer is adopted to cut off the organic material layer to prevent leakage, and connect the cathode through the middle metal layer to reduce the risk of leakage.

Benefits of technology

It effectively prevents lateral leakage of organic semiconductor materials, improves the display effect of the OLED display panel, and further reduces the risk of leakage by forming a common cathode.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118765124A_ABST
    Figure CN118765124A_ABST
Patent Text Reader

Abstract

The invention provides an anode structure for relieving and preventing transverse leakage current of a WOLED (White Organic Light Emitting Diode), an OLED display panel and a preparation method of the OLED display panel, and belongs to the field of semiconductors. Comprising a CMOS and N structural units, the N structural units are arranged on the complementary metal oxide semiconductor layer at intervals, N is a positive integer larger than or equal to 1, and the structural units are spaced through anode units; each structural unit comprises a pixel definition layer, a bottom insulating material layer, a middle metal layer and a top transparent layer which are sequentially stacked, and the length of the top transparent layer is larger than that of the middle metal layer; the pixel definition layer is in contact with the complementary metal oxide semiconductor layer; in the vertical direction, the length of the upper surface of the pixel definition layer is larger than that of the upper surface of the anode unit. The anode structure provided by the invention forms an I-shaped structure, and the organic material layer is cut off, so that organic semiconductor material leakage current does not exist between pixel definition layers.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to an anode structure for alleviating and preventing lateral leakage current of WOLED, an OLED display panel and a preparation method thereof. Background Art

[0002] As display panels develop towards being thin, light, low-power, and portable, the new generation of display technology represented by organic light-emitting diodes (OLED) has attracted more and more attention. Compared with liquid crystal display (LCD) display technology, OLED has the advantages of being thin, light, low-power, low-driving voltage, better viewing angle and contrast, and faster response speed.

[0003] The mainstream method for achieving full-color display in OLED display panels is WOLED (White Organic Light Emitting Diode) + CF (Color Filter), and white sub-pixels can be retained to improve the brightness of the screen. Among them, the WOLED and CF superimposed structure does not require a precise mask process, and an open mask plate can be used to achieve high resolution of OLED displays, which is widely used in the field of large-size screen displays. The structure of the OLED display panel formed by WOLED + CF in the prior art is as follows: Figure 1 As shown, Figure 1 In it, CMOS is complementary metal oxide semiconductor layer, PDL is pixel definition layer, TFE (thin film encapsulation) is thin film encapsulation layer, OC (overcoating) is cured film protective layer, CG (coverglass) is cover glass, CF-R is Color filter-R (red filter film), CF-G is Colorfilter-R (green filter film), CF-R is Color filter-B (blue filter film), and there is a leakage problem of organic semiconductor materials between the pixel definition layers. Summary of the invention

[0004] In view of this, the object of the present invention is to provide an anode structure for alleviating and preventing lateral leakage current of WOLED, an OLED display panel and a method for manufacturing the same. The anode structure provided by the present invention forms an "I"-shaped structure using a bottom insulating material layer, an intermediate metal layer and a top transparent layer, cutting off the organic material layer, so that there is no leakage of organic semiconductor material between the pixel definition layers.

[0005] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:

[0006] The present invention provides an anode structure for alleviating and preventing lateral leakage current of WOLED, comprising a complementary metal oxide semiconductor layer and N structural units, wherein the N structural units are arranged on the complementary metal oxide semiconductor layer at intervals, wherein N is a positive integer ≥ 1, and the N structural units are spaced apart by anode units;

[0007] Each structural unit comprises a pixel definition layer, a bottom insulating material layer, an intermediate metal layer and a top transparent layer stacked in sequence, wherein the length of the top transparent layer is greater than the length of the intermediate metal layer; the pixel definition layer is in contact with the complementary metal oxide semiconductor layer;

[0008] In a vertical direction, a length of an upper surface of the pixel definition layer is greater than a length of an upper surface of the anode unit.

[0009] Preferably, the material of the bottom insulating material layer includes one or more of silicon oxide material, silicon nitride material and silicon oxynitride material.

[0010] Preferably, the material of the intermediate metal layer includes W and / or Mo.

[0011] Preferably, the material of the top transparent layer includes one or more of silicon oxide material, silicon nitride material, indium tin oxide and conductive glass.

[0012] The present invention also provides a method for preparing the anode structure described in the above technical solution, comprising the following steps:

[0013] Disposing anode units at intervals on the surface of the complementary metal oxide semiconductor layer, and then performing a first deposition to form a pixel deposition layer;

[0014] Performing patterned etching on the pixel deposition layer to obtain the pixel definition layer;

[0015] A second deposition, a third deposition and a fourth deposition are performed on the surface of the pixel definition layer to obtain a bottom insulating material deposition layer, an intermediate metal deposition layer and a top transparent deposition layer in sequence, and the bottom insulating material deposition layer, the intermediate metal deposition layer and the top transparent deposition layer are graphically etched to obtain the bottom insulating material layer, the intermediate metal layer and the top transparent layer, respectively, to obtain the anode structure.

[0016] The present invention further provides an OLED display panel, comprising the anode structure described in the above technical solution, and further comprising:

[0017] A first organic material layer, wherein the first organic material layer is disposed on a surface of the anode unit, and a thickness of the first organic material layer is less than a thickness of the bottom insulating material layer;

[0018] a first cathode, wherein the first cathode is disposed on the surface of the first organic material layer, and the first cathode forms an ohmic contact with the intermediate metal layer; the thickness of the bottom insulating material layer is less than the sum of the thicknesses of the first organic material layer and the first cathode;

[0019] a second organic material layer, wherein the second organic material layer is disposed on a surface of the top transparent layer;

[0020] a second cathode, the second cathode being disposed on a surface of the second organic material layer;

[0021] Thin film encapsulation layer;

[0022] A color filter film is arranged on the upper surface of the thin film encapsulation layer.

[0023] Preferably, the thin film encapsulation layer is made of a water and oxygen barrier material.

[0024] Preferably, the thin film encapsulation layer is made of silicon oxide material, silicon nitride material or aluminum oxide material.

[0025] Preferably, the color filter film includes a red filter film, a green filter film and a blue filter film.

[0026] The present invention also provides a method for preparing the OLED display panel according to the above technical solution, comprising the following steps:

[0027] Vapor-depositing an organic material on the surface of the anode structure to form the first organic material layer and the second organic material layer;

[0028] Performing cathode film formation on the surfaces of the first organic material layer and the second organic material layer respectively to form the first cathode and the second cathode, and then performing encapsulation to form the thin film encapsulation layer;

[0029] A color filter is prepared on the surface of the thin film encapsulation layer to form the color filter film.

[0030] The present invention provides an anode structure for alleviating and preventing lateral leakage current of WOLED, comprising a complementary metal oxide semiconductor layer and N structural units, wherein the N structural units are arranged on the complementary metal oxide semiconductor layer at intervals, N is a positive integer ≥1, and the N structural units are spaced apart by anode units; each structural unit comprises a pixel definition layer, a bottom insulating material layer, an intermediate metal layer and a top transparent layer which are stacked in sequence, wherein the length of the top transparent layer is greater than the length of the intermediate metal layer; the pixel definition layer is in contact with the complementary metal oxide semiconductor layer; in the vertical direction, the length of the upper surface of the pixel definition layer is greater than the length of the upper surface of the anode unit.

[0031] Compared with the prior art, the present invention has the following beneficial effects:

[0032] The anode structure provided by the present invention forms an I-shaped structure using a bottom insulating material layer, an intermediate metal layer and a top transparent layer, cutting off the organic material layer so that there is no leakage of organic semiconductor material between pixel definition layers.

[0033] The present invention also provides an OLED display panel, including the anode structure described in the above technical solution, which can not only cut off the organic material layer, but also connect the cathode. During the OLED evaporation process, the top transparent layer in the "I"-shaped structure separates the organic material due to the protruding part. The middle metal layer can connect the metal cathodes of the OLED together to form a common cathode, further reducing the leakage of the organic semiconductor material between the pixel definition layers. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 It is a schematic diagram of the structure of an OLED display panel formed by using WOLED+CF in the prior art;

[0035] Figure 2 It is a schematic structural diagram of an anode structure for alleviating and preventing lateral leakage current of WOLED according to the present invention;

[0036] Figure 3 A schematic diagram of a structure for forming a pixel deposition layer;

[0037] Figure 4 A schematic diagram of a structure for coating a pixel deposition layer with photoresist;

[0038] Figure 5 A schematic diagram of a structure for etching a pixel deposition layer;

[0039] Figure 6 is a schematic diagram of the structure after the second deposition;

[0040] Figure 7A schematic diagram of a structure for coating a photoresist on a bottom insulating material layer deposition layer, a middle metal layer deposition layer and a top transparent layer deposition layer;

[0041] Figure 8 It is a structural schematic diagram of the OLED display panel of the present invention;

[0042] Fig. 9 A schematic diagram of a structure in which an organic material is evaporated on the surface of the anode structure to form a first organic material layer and a second organic material layer;

[0043] Fig.10 A schematic diagram of a structure for forming a first cathode and a second cathode;

[0044] Fig.11 A schematic diagram of the structure for forming a thin film encapsulation layer. DETAILED DESCRIPTION

[0045] The present invention provides an anode structure for alleviating and preventing lateral leakage current of WOLED, comprising a complementary metal oxide semiconductor layer and N structural units, wherein the N structural units are arranged on the complementary metal oxide semiconductor layer at intervals, wherein N is a positive integer ≥ 1, and the N structural units are spaced apart by anode units;

[0046] Each structural unit comprises a pixel definition layer, a bottom insulating material layer, an intermediate metal layer and a top transparent layer which are stacked in sequence, wherein the length of the top transparent layer is greater than the length of the intermediate metal layer; the pixel definition layer is in contact with the complementary metal oxide semiconductor layer;

[0047] In a vertical direction, a length of an upper surface of the pixel definition layer is greater than a length of an upper surface of the anode unit.

[0048] Figure 2 The schematic diagram of the anode structure of the present invention for alleviating and preventing the lateral leakage current of WOLED is shown below. Figure 2 The anode structure of the present invention will be described.

[0049] In the present invention, the anode structure includes a complementary metal oxide semiconductor layer (CMOS). The present invention has no special restrictions on the material and size of the complementary metal oxide semiconductor layer, and any solution known to those skilled in the art can be used.

[0050] In the present invention, the anode structure includes N structural units, the N structural units are arranged on the complementary metal oxide semiconductor layer at intervals, N is a positive integer ≥ 1, and the N structural units are spaced apart by anode units.

[0051] The present invention has no special limitation on the material and size of the anode unit (Anode), and any solution familiar to those skilled in the art may be adopted, such as ITO, Al, TiN, Ti, Ag or several layers of laminated composite metal.

[0052] In the present invention, the structural unit includes a pixel definition layer, a bottom insulating material layer, an intermediate metal layer and a top transparent layer which are stacked in sequence, and the length of the top transparent layer is greater than the length of the intermediate metal layer; the pixel definition layer is in contact with the complementary metal oxide semiconductor layer; in the vertical direction, the length of the upper surface of the pixel definition layer is greater than the length of the upper surface of the anode unit.

[0053] In the present invention, the material of the pixel definition layer (PDL) is not particularly limited, and a solution familiar to those skilled in the art may be used. In a specific embodiment of the present invention, the material of the pixel definition layer (PDL) is preferably silicon oxide (SiO) material or silicon nitride (SiN) material, the silicon oxide (SiO) material is preferably SiO2, and the silicon nitride (SiN) material is preferably Si3N4.

[0054] In the present invention, in the vertical direction, the length of the upper surface of the pixel definition layer is greater than the length of the upper surface of the anode unit, so that the pixel definition layer covers the edge of the Anode.

[0055] In the present invention, the bottom insulating material layer, the middle metal layer and the top transparent layer form an I-shaped structure, cutting off the organic material layer, so that there is no leakage of organic semiconductor material between the pixel definition layers.

[0056] In the present invention, the material of the bottom insulating material layer preferably includes one or more of silicon oxide (SiO) material, silicon nitride (SiN) material and silicon oxynitride (SiON) material.

[0057] In the present invention, the silicon oxide (SiO) material is preferably SiO2, and the silicon nitride (SiN) material is preferably Si3N4.

[0058] In the present invention, the material of the intermediate metal layer preferably includes W and / or Mo. The material of the intermediate metal layer does not react with the cathode and can maintain good physical and chemical properties in a water and oxygen environment. In the present invention, after the I-shape is formed, the entire device needs to undergo subsequent processes to prepare an OLED display panel. The I-shape structure will be exposed to the air. If it reacts with water, oxygen, etc. in the air (or other chemical substances in subsequent processes), it will damage the metal in the I-shape, resulting in abnormalities in its electrical properties.

[0059] In the present invention, the material of the top transparent layer preferably includes one or more of silicon oxide (SiO) material, silicon nitride (SiN) material, indium tin oxide (ITO) and conductive glass (FTO); the material of the top transparent layer is a transparent substance, which can ensure that light can pass through the "eaves" (formed because the length of the top transparent layer is greater than the length of the middle metal layer) during the exposure process to react to the photoresist (graphic etching).

[0060] The present invention also provides a method for preparing the anode structure described in the above technical solution, comprising the following steps:

[0061] Disposing anode units at intervals on the surface of the complementary metal oxide semiconductor layer, and then performing a first deposition to form a pixel definition layer deposition layer;

[0062] Performing patterned etching on the pixel definition layer deposition layer to obtain the pixel definition layer;

[0063] A second deposition, a third deposition and a fourth deposition are performed on the surface of the pixel definition layer to obtain a bottom insulating material layer deposition layer, an intermediate metal layer deposition layer and a top transparent layer deposition layer in sequence, and the bottom insulating material layer deposition layer, the intermediate metal layer deposition layer and the top transparent layer deposition layer are graphically etched to obtain the bottom insulating material layer, the intermediate metal layer and the top transparent layer, respectively, to obtain the anode structure.

[0064] In the present invention, unless otherwise specified, the raw materials used are all commercially available products in the art.

[0065] Combine the following Figures 3 to 7 The method for preparing the anode structure is described.

[0066] The present invention arranges anode units at intervals on the surface of the complementary metal oxide semiconductor layer, and then performs a first deposition to form a pixel deposition layer, such as Figure 3 shown.

[0067] In the present invention, the first deposition is preferably chemical vapor deposition (CVD). The present invention has no special limitation on the specific parameters of the first deposition, and a method familiar to those skilled in the art may be used.

[0068] After forming the pixel deposition layer, the present invention performs patterning etching on the pixel deposition layer to obtain the pixel definition layer, such as Figures 4-5 shown.

[0069] In the present invention, the patterned etching is preferably performed by first coating a photoresist (PR), that is, Figure 4 The yellow light patterning scheme is then followed by an etching process to obtain the following Figure 5In the structure shown, the length of the upper surface of the PDL is greater than the length of the upper surface of the anode unit, so that the pixel definition layer covers the edge of the Anode.

[0070] After obtaining the pixel definition layer, the present invention performs a second deposition, a third deposition and a fourth deposition on the surface of the pixel definition layer to sequentially obtain a bottom insulating material deposition layer, an intermediate metal deposition layer and a top transparent deposition layer, and graphically etches the bottom insulating material deposition layer, the intermediate metal deposition layer and the top transparent deposition layer to respectively obtain the bottom insulating material layer, the intermediate metal layer and the top transparent layer to obtain the anode structure.

[0071] In the present invention, the structure after the fourth deposition is as follows Figure 6 The present invention has no special limitation on the specific parameters of the second deposition, the third deposition and the fourth deposition, and can form the bottom insulating material deposition layer, the middle metal deposition layer and the top transparent deposition layer.

[0072] In the present invention, the patterned etching is preferably performed by first coating a photoresist (PR), that is, Figure 7 The yellow light patterning scheme is then followed by an etching process to obtain the following Figure 2 In the structure shown, after the graphic etching, the length of the top transparent layer must exceed the length of the middle metal layer. The excess length can ensure that the organic material is cut off in the subsequent process of preparing the OLED display panel.

[0073] The present invention further provides an OLED display panel, comprising the anode structure described in the above technical solution, and further comprising:

[0074] A first organic material layer, wherein the first organic material layer is disposed on a surface of the anode unit, and a thickness of the first organic material layer is less than a thickness of the bottom insulating material layer;

[0075] a first cathode, wherein the first cathode is disposed on the surface of the first organic material layer, and the first cathode forms an ohmic contact with the intermediate metal layer; the thickness of the bottom insulating material layer is less than the sum of the thicknesses of the first organic material layer and the first cathode;

[0076] a second organic material layer, wherein the second organic material layer is disposed on a surface of the top transparent layer;

[0077] a second cathode, the second cathode being disposed on a surface of the second organic material layer;

[0078] Thin film encapsulation layer;

[0079] A color filter film is arranged on the upper surface of the thin film encapsulation layer.

[0080] Figure 8 The structure diagram of the OLED display panel of the present invention is shown below. Figure 8 The OLED display panel of the present invention is described.

[0081] The OLED display panel of the present invention includes the anode structure described in the above technical solution.

[0082] The OLED display panel of the present invention comprises a first organic material layer (first Organic), wherein the first organic material layer is arranged on the surface of the anode unit, and the thickness of the first organic material layer is less than the thickness of the bottom insulating material layer.

[0083] In the present invention, the thickness of the first organic material layer is less than the thickness of the bottom insulating material layer, so that the connection of the organic material layers can be avoided, and thus there is no leakage of the organic semiconductor material.

[0084] The present invention has no special limitation on the material of the first organic material layer, and any material well known to those skilled in the art may be used.

[0085] The OLED display panel of the present invention includes a first cathode (first cathode), which is arranged on the surface of the first organic material layer and forms an ohmic contact with the intermediate metal layer; the thickness of the bottom insulating material layer is less than the sum of the thicknesses of the first organic material layer and the first cathode.

[0086] In the present invention, the thickness of the bottom insulating material layer is less than the sum of the thickness of the first organic material layer and the first cathode, which can ensure that the first cathode overlaps the intermediate metal layer and ensures that different cathodes are connected and conductive.

[0087] The present invention has no special limitation on the material of the first cathode, and any material well known to those skilled in the art may be used, such as Mg, Ag or ITO.

[0088] The OLED display panel of the present invention comprises a second organic material layer (second Organic), and the second organic material layer is arranged on the surface of the top transparent layer.

[0089] The present invention has no special limitation on the material and thickness of the second organic material layer, and any solution familiar to those skilled in the art may be adopted.

[0090] The OLED display panel of the present invention comprises a second cathode (second cathode), and the second cathode is arranged on the surface of the second organic material layer.

[0091] The present invention has no special limitation on the material and thickness of the second cathode, and any solution known to those skilled in the art may be used.

[0092] The OLED display panel of the present invention includes a thin film encapsulation layer (TFE).

[0093] In the present invention, the material of the thin film encapsulation layer is preferably a water and oxygen barrier material, more preferably a silicon oxide (SiO) material, a silicon nitride (SiN) material or an aluminum oxide (AlO) material. The silicon oxide (SiO) material is preferably SiO2, the silicon nitride (SiN) material is preferably Si3N4, and the aluminum oxide (AlO) material is preferably Al2O3.

[0094] In the present invention, in terms of horizontal height, the upper surface of the thin film encapsulation layer is higher than the upper surface of the second cathode.

[0095] The OLED display panel of the present invention comprises a color filter, and the color filter is arranged on the upper surface of the thin film encapsulation layer.

[0096] In the present invention, the color filter film preferably includes a red filter film, a green filter film and a blue filter film.

[0097] The present invention has no special limitation on the material and thickness of the color filter film, and any solution known to those skilled in the art may be adopted.

[0098] The present invention also provides a method for preparing the OLED display panel according to the above technical solution, comprising the following steps:

[0099] Vapor-depositing an organic material on the surface of the anode structure to form the first organic material layer and the second organic material layer;

[0100] Performing cathode film formation on the surfaces of the first organic material layer and the second organic material layer respectively to form the first cathode and the second cathode, and then performing encapsulation to form the thin film encapsulation layer;

[0101] A color filter is prepared on the surface of the thin film encapsulation layer to form the color filter film.

[0102] Combine the following Figures 9-11 The preparation method of the OLED display panel is described.

[0103] The present invention evaporates organic material on the surface of the anode structure to form the first organic material layer and the second organic material layer. Fig. 9 shown.

[0104] The present invention has no special limitation on the specific parameters of the evaporation, and a method familiar to those skilled in the art may be used.

[0105] After forming the first organic material layer and the second organic material layer, the present invention performs cathode film formation on the surfaces of the first organic material layer and the second organic material layer to form the first cathode and the second cathode, and then performs encapsulation to form the thin film encapsulation layer.

[0106] In the present invention, the cathode film is preferably formed by thermal evaporation or sputtering. The present invention has no special limitation on the specific parameters of the cathode film, and a method familiar to those skilled in the art may be used.

[0107] In the present invention, the structure after forming the first cathode and the second cathode is as follows Fig.10 shown.

[0108] The present invention has no special limitation on the specific method of the packaging, and a method familiar to those skilled in the art may be used, such as atomic layer deposition (ALD) combined with chemical vapor deposition (CVD) or ALD combined with ALD. The present invention has no special limitation on the specific parameters of the ALD and CVD, and a method familiar to those skilled in the art may be used.

[0109] In the present invention, the structure after forming the thin film encapsulation layer is as follows Fig.11 shown.

[0110] After the thin film encapsulation layer is formed, the present invention prepares a color filter on the surface of the thin film encapsulation layer to form the color filter film.

[0111] The present invention has no particular limitation on the specific method for preparing the color filter, and any method well known to those skilled in the art may be used.

[0112] The technical solutions in the present invention will be described clearly and completely below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0113] Example 1

[0114] The method of preparing an OLED display panel comprises the following steps:

[0115] Anode units (ITO) are arranged at intervals on the surface of the complementary metal oxide semiconductor layer, and then chemical vapor deposition is performed to form a pixel deposition layer (SiO2), a photoresist is first coated on the surface of the pixel deposition layer, and then an etching process is performed to obtain a pixel definition layer. The etching result ensures that the length of the upper surface of the pixel definition layer is greater than the length of the upper surface of the anode unit, so that the pixel definition layer covers the edge of the Anode;

[0116] A second deposition is performed on the surface of the pixel definition layer to obtain a bottom insulating material deposition layer (SiO2), an intermediate metal deposition layer (W) and a top transparent deposition layer (ITO) in sequence, and the bottom insulating material deposition layer, the intermediate metal deposition layer and the top transparent deposition layer are patterned and etched (by first coating with photoresist and then etching). After the patterned etching, the length of the top transparent layer exceeds the length of the intermediate metal layer, and a bottom insulating material layer, an intermediate metal layer and a top transparent layer are obtained respectively, and an anode structure (such as Figure 2 shown);

[0117] Depositing an organic material on the surface of the anode structure to form a first organic material layer and a second organic material layer, wherein the first organic material layer is disposed on the surface of the anode unit and the second organic material layer is disposed on the surface of the top transparent layer;

[0118] Thermal evaporation is performed on the surfaces of the first organic material layer and the second organic material layer to form a first cathode (Mg) and a second cathode (Mg), respectively, wherein the first cathode is arranged on the surface of the first organic material layer, the first cathode forms an ohmic contact with the intermediate metal layer, and the thickness of the bottom insulating material layer is less than the sum of the thicknesses of the first organic material layer and the first cathode;

[0119] Then encapsulation (ALD+ALD) is performed to form a thin film encapsulation layer;

[0120] A color filter is prepared on the surface of the thin film encapsulation layer to form a color filter film, which includes a red filter film, a green filter film and a blue filter film.

[0121] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be regarded as the protection scope of the present invention.

Claims

1. An anode structure for alleviating and preventing lateral leakage current of WOLED, characterized in that: It comprises a complementary metal oxide semiconductor layer and N structural units, wherein the N structural units are arranged on the complementary metal oxide semiconductor layer at intervals, wherein N is a positive integer ≥ 1, and the N structural units are spaced apart by anode units; Each of the structural units comprises a pixel definition layer, a bottom insulating material layer, an intermediate metal layer and a top transparent layer stacked in sequence, wherein the length of the top transparent layer is greater than the length of the intermediate metal layer; the pixel definition layer is in contact with the complementary metal oxide semiconductor layer; In a vertical direction, a length of an upper surface of the pixel definition layer is greater than a length of an upper surface of the anode unit.

2. The anode structure according to claim 1, characterized in that: The material of the bottom insulating material layer includes one or more of silicon oxide material, silicon nitride material and silicon oxynitride material.

3. The anode structure according to claim 1, characterized in that: The material of the intermediate metal layer includes W and / or Mo.

4. The anode structure according to claim 1, characterized in that: The material of the top transparent layer includes one or more of silicon oxide material, silicon nitride material, indium tin oxide and conductive glass.

5. The method for preparing the anode structure according to claims 1 to 4, characterized in that: The following steps are involved: Disposing anode units at intervals on the surface of the complementary metal oxide semiconductor layer, and then performing a first deposition to form a pixel deposition layer; Performing patterned etching on the pixel deposition layer to obtain the pixel definition layer; A second deposition, a third deposition and a fourth deposition are performed on the surface of the pixel definition layer to obtain a bottom insulating material deposition layer, an intermediate metal deposition layer and a top transparent deposition layer in sequence, and the bottom insulating material deposition layer, the intermediate metal deposition layer and the top transparent deposition layer are graphically etched to obtain the bottom insulating material layer, the intermediate metal layer and the top transparent layer, respectively, to obtain the anode structure.

6. An OLED display panel, characterized in that: The anode structure according to any one of claims 1 to 4 further comprises: A first organic material layer, wherein the first organic material layer is disposed on a surface of the anode unit, and a thickness of the first organic material layer is less than a thickness of the bottom insulating material layer; a first cathode, wherein the first cathode is disposed on the surface of the first organic material layer, and the first cathode forms an ohmic contact with the intermediate metal layer; the thickness of the bottom insulating material layer is less than the sum of the thicknesses of the first organic material layer and the first cathode; a second organic material layer, wherein the second organic material layer is disposed on a surface of the top transparent layer; a second cathode, the second cathode being disposed on a surface of the second organic material layer; Thin film encapsulation layer; A color filter film is arranged on the upper surface of the thin film encapsulation layer.

7. The OLED display panel according to claim 6, characterized in that: The material of the thin film encapsulation layer is a water and oxygen barrier material.

8. The OLED display panel according to claim 6 or 7, characterized in that: The material of the thin film encapsulation layer is silicon oxide material, silicon nitride material or aluminum oxide material.

9. The OLED display panel according to claim 6, characterized in that: The color filter film includes a red filter film, a green filter film and a blue filter film.

10. The method for preparing an OLED display panel according to any one of claims 6 to 9, characterized in that: The following steps are involved: Vapor-depositing an organic material on the surface of the anode structure to form the first organic material layer and the second organic material layer; Performing cathode film formation on the surfaces of the first organic material layer and the second organic material layer respectively to form the first cathode and the second cathode, and then performing encapsulation to form the thin film encapsulation layer; A color filter is prepared on the surface of the thin film encapsulation layer to form the color filter film.