Production process of high-toughness corrosion-resistant damping aluminum profile for doors and windows

By using electric thermal expansion rings and carbon brushes to control the connection strength between the rotating secondary shaft and the main shaft during drilling and milling, as well as the settings of cooling grooves and cutting fluid circulation paths, the end mill is able to rotate at low speed during the drilling and milling process, solving the problem of high speed The problem of easy chipping of rotating tools extends the service life and improves safety.

CN118768615AInactive Publication Date: 2024-10-15JIAN SHANJIANSULIN WHOLE HOUSE CUSTOMIZATION CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410947380.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the drilling and milling process, the high-speed rotating end mill produces a violent impact when it comes into contact with the stationary aluminum profile, causing the tool to easily break, affecting its service life and posing safety risks.

Method used

The electric thermal expansion ring and carbon brush control circuit of the rotating secondary shaft and the rotating main shaft are used to control the connection strength of the rotating secondary shaft and the rotating main shaft through the thermal expansion of the electric thermal expansion ring, so that the end mill contacts the aluminum profile when rotating at low speed, and when in contact Then gradually increase the rotation speed, combined with the cooling groove and cutting fluid flow path, to ensure that the tool rotates at low speed when in contact to avoid cracking.

Benefits of technology

It effectively reduces the impact damage when the high-speed rotating end mill comes into contact with the aluminum profile, extends the service life of the tool, improves safety and reliability, and avoids cracking.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118768615A_ABST
    Figure CN118768615A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of drilling and milling transmission parts, and discloses a production process of a high-toughness corrosion-resistant damping aluminum profile for doors and windows. A rotating countershaft is included, a rotating main shaft is arranged at the top of the outer surface of the rotating countershaft, and the top end of the rotating main shaft is fixedly connected with a transmission main shaft; the outer surface of the rotating main shaft is movably sleeved with an outer shell, the mechanism is fixedly installed on a milling machine through the outer shell, and an electric thermal expansion ring is arranged in the middle of the outer surface of the rotating auxiliary shaft. According to the production process of the aluminum profile for the high-toughness and corrosion-resistant damping doors and windows, the electric thermal expansion ring and a control circuit on the electric thermal expansion ring are arranged, and the connection strength between the rotating auxiliary shaft and the rotating main shaft can be regulated and controlled through the electric thermal expansion state of the electric thermal expansion ring; therefore, the end mill can be in contact with the aluminum profile in a low-speed rotating state, and violent impact on the aluminum profile at the moment when the end mill rotating at a high speed is in contact with the aluminum profile is effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of drilling and milling transmission components, and in particular to a production process of a high-toughness, corrosion-resistant aluminum profile for shock-absorbing doors and windows. Background Art

[0002] When using aluminum profiles to process doors and windows, in order to facilitate the assembly of frames and the installation of door and window structures, it is necessary to drill and mill circular holes or waist-shaped holes at specific locations. Drilling and milling is a processing technology that uses high-speed rotating multi-edge tools to cut workpieces, and is widely used in the precision processing of various holes and grooves on planes.

[0003] However, in the existing drilling and milling process, the high-speed rotating end mill will produce a severe impact on the relatively stationary aluminum profile at the moment of contact. The end mill itself has extremely high hardness, and it is very easy to cause impact damage or even cracking under the severe impact, which not only affects the service life of the milling cutter, but also poses a great safety hazard to the tool that cracks under high-speed rotation.

[0004] Therefore, there is an urgent need for a spindle transmission component used in the drilling and milling process to solve the defects existing in the actual operation of the above-mentioned existing drilling and milling processes. Summary of the invention

[0005] The present application proposes a production process for high-toughness, corrosion-resistant, shock-absorbing aluminum profiles for doors and windows, which has the advantages of enabling the end mill to come into contact with the aluminum profile at a relatively low rotation speed, thereby effectively reducing the impact damage to the end mill at the moment of contact and extending its service life, with the advantages of high safety and reliability. It is used to solve the problem that in the existing drilling and milling process, the high-speed rotating end mill will produce a severe impact on the relatively stationary aluminum profile at the moment of contact, and the end mill itself has extremely high hardness, and is easily damaged by impact or even cracked under severe impact, which not only affects the service life of the milling cutter, but also poses a major safety hazard to the tool that cracks under high-speed rotation.

[0006] To achieve the above-mentioned purpose, the present application adopts the following technical scheme: a production process for high-toughness, corrosion-resistant, shock-absorbing aluminum profiles for doors and windows, including a rotating secondary shaft, a vertical milling cutter is fixedly installed at the bottom end of the rotating secondary shaft, a rotating main shaft is provided at the top of the outer surface of the rotating secondary shaft, and the top of the rotating main shaft is fixedly connected to the transmission main shaft, and an outer shell is movably sleeved on the outer surface of the rotating main shaft, and the mechanism is fixedly installed on the milling machine through the outer shell, an electric thermal expansion ring is provided in the middle of the outer surface of the rotating secondary shaft, and a carbon brush is fixedly installed at the top of the rotating secondary shaft, and the electric thermal expansion ring is conductively connected through the carbon brush to form a control circuit.

[0007] Furthermore, a weak current system is provided between the outer surface of the rotating secondary shaft and the worktable of the milling machine, and a feedback loop is formed to regulate the triggering timing and on-off state of the control loop in the electrothermal expansion ring.

[0008] Furthermore, in the initial state, when the electrothermal expansion ring does not undergo thermal expansion, its outer diameter is smaller than the inner diameter of the bottom of the rotating main shaft, and when the electrothermal expansion ring undergoes thermal expansion due to conduction, its outer diameter after expansion is larger than the inner diameter of the rotating main shaft.

[0009] Furthermore, an inner chamber is provided inside the rotating spindle, and the inner chamber is connected to the cutting fluid pipeline system through a through hole inside the rotating spindle, and a linkage component for controlling the flow timing of the cutting fluid in the inner chamber is provided inside the rotating spindle and below the inner chamber, and a cooling groove extending to the bottom of its outer surface is provided inside the rotating spindle.

[0010] Furthermore, an annular groove is provided inside the rotating main shaft and below the inner chamber, and a linkage component is provided inside the annular groove. The linkage component includes a sealing disk arranged in the annular groove, and the inner wall of the sealing disk is fixedly connected to the rotating main shaft through an elastic colloid, and a guide hole corresponding to the position of the cooling groove is provided inside the sealing disk.

[0011] Furthermore, the guide holes correspond one-to-one with the cooling grooves and are interconnected in the initial stage. When the rotating spindle rotates at high speed, under the action of centrifugal force, the sealing disk shifts outward and pulls the elastic colloid, so that the positions of the guide holes and the cooling grooves are staggered and the cooling grooves are blocked.

[0012] Furthermore, the cooling groove is configured as a zigzag structure, and a section of the cooling groove passes through the electrothermal expansion ring and is parallel to the central axis thereof, while a tail section of the cooling groove extends outwardly at an angle.

[0013] The present invention application has the following technical effects:

[0014] 1. The present application provides a production process for a high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows. For the arrangement of an electrothermal expansion ring and a control circuit thereon, the electrothermal expansion state of the electrothermal expansion ring can be used to regulate the connection strength between the rotating sub-shaft and the rotating main shaft, so that the end mill can come into contact with the aluminum profile in a low-speed rotating state, and after the contact occurs, the connection strength between the rotating sub-shaft and the rotating main shaft is continuously improved through the thermal expansion of the electrothermal expansion ring until the rotating sub-shaft and the rotating main shaft synchronously rotate at a high speed to perform drilling and milling operations on the surface of the aluminum profile, thereby effectively reducing the impact damage caused to the relatively stationary aluminum profile by the high-speed rotating end mill at the moment of contact with the relatively stationary aluminum profile, and avoiding the end mill from cracking due to severe impact.

[0015] 2. The present application provides a production process for a high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows. Regarding the setting of a cooling groove and a cutting fluid flow path thereon, when the rotating main shaft stops rotating and is in the process of moving and adjusting the drilling and milling position of the end mill, the cutting fluid temporarily stored in its inner chamber can flow through the cooling groove and be discharged outward, and the electric thermal expansion ring on the rotating secondary shaft is cooled, causing its temperature to gradually drop, thereby gradually reducing the connection strength between the rotating secondary shaft and the rotating main shaft. When it comes into contact with the aluminum profile again and performs drilling and milling operations, it can be ensured that the end mill is in a low-speed rotating state again. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The accompanying drawings, which constitute a part of the specification, illustrate embodiments disclosed in the present application and, together with the description, serve to explain the principles disclosed in the present application.

[0017] The present application can be more clearly understood from the following detailed description with reference to the accompanying drawings, in which:

[0018] Figure 1 It is a schematic diagram of the structure of the present invention;

[0019] Figure 2 It is a front view of the structure of the present invention;

[0020] Figure 3 It is a structural schematic diagram of the rotating main shaft of the present invention;

[0021] Figure 4 It is a structural schematic diagram of the rotating secondary shaft of the present invention;

[0022] Figure 5 The structure of the present invention Figure 1 An enlarged schematic diagram of point A.

[0023] In the figure: 1. rotating secondary shaft; 2. end mill; 3. rotating main shaft; 4. outer shell; 5. inner chamber; 6. linkage component; 7. cooling groove; 8. electrothermal expansion ring; 9. carbon brush; 10. elastic colloid; 11. sealing disk; 12. guide hole. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0025] like Figure 1As shown, a production process of high-toughness, corrosion-resistant, shock-absorbing aluminum profiles for doors and windows includes a rotating secondary shaft 1, a vertical milling cutter 2 for finishing the surface of the aluminum profile by high-speed rotation is fixedly installed at the bottom end of the rotating secondary shaft 1, a rotating main shaft 3 is provided at the top of the outer surface of the rotating secondary shaft 1, and the top end of the rotating main shaft 3 is fixedly connected to the transmission main shaft, thereby driving the rotating main shaft 3 to rotate at a high speed, and an outer shell 4 is movably sleeved on the outer surface of the rotating main shaft 3, and the mechanism is fixedly installed on the milling machine through the outer shell 4, and can drive the mechanism to perform linear movement along the X-axis, Y-axis and Z-axis, as shown in FIG. Figure 4 As shown, an electrothermal expansion ring 8 is provided in the middle of the outer surface of the rotating secondary shaft 1, and a carbon brush 9 is fixedly installed on the top of the rotating secondary shaft 1. The electrothermal expansion ring 8 is conductively connected through the carbon brush 9 to form a control circuit, thereby adjusting and controlling whether the electrothermal expansion ring 8 is energized and undergoes electrothermal expansion.

[0026] In this technical solution, a weak current system is provided between the outer surface of the rotating secondary shaft 1 and the worktable of the milling machine, and a feedback loop is formed to regulate the triggering timing and on / off state of the control loop in the electrothermal expansion ring 8:

[0027] When the end mill 2 comes into contact with the aluminum profile clamped on the workbench, the feedback loop is triggered to connect the control loop, and then the current loop on the electric thermal expansion ring 8 is connected through the carbon brush 9, and the electric thermal expansion ring 8 is forced to expand, gradually coming into compression contact with the inner wall of the rotating main shaft 3, so as to synchronously drive the rotating secondary shaft 1 and the end mill 2 thereon to rotate at high speed;

[0028] Furthermore, in the initial stage, the rotating main shaft 3 drives the rotating secondary shaft 1 and the end mill 2 thereon to rotate at a low speed. When the end mill 2 contacts the aluminum profile, the electric thermal expansion ring 8 is triggered and the rotation speed of the rotating secondary shaft 1 and the end mill 2 thereon is gradually increased until they rotate at a high speed synchronously with the rotating main shaft 3. In the process of moving the aluminum profile or the high-speed rotating end mill 2, the drilling and milling operations on the surface of the aluminum profile are completed.

[0029] like Figure 2 As shown, in the present technical solution, in the initial state, when the electrothermal expansion ring 8 has not undergone thermal expansion, its outer diameter is smaller than the inner diameter of the bottom of the rotating main shaft 3, thereby causing the rotating secondary shaft 1 and the rotating main shaft 3 to be disconnected from each other at the initial stage. When the electrothermal expansion ring 8 undergoes thermal expansion due to electrical conduction, its expanded outer diameter is larger than the inner diameter of the rotating main shaft 3, thereby ensuring the thermal expansion connection strength between the rotating secondary shaft 1 and the rotating main shaft 3, making it less likely for the end mill 2 to "slip" during high-speed rotary drilling and milling of the aluminum profile surface, thereby ensuring its drilling and milling accuracy for the aluminum profile surface.

[0030] like Figure 3As shown, in the present technical solution, an inner chamber 5 is provided inside the rotating spindle 3, and the inner chamber 5 is connected to the cutting fluid pipeline system through a through hole inside the rotating spindle 3, and a linkage component 6 for controlling the flow timing of the cutting fluid in the inner chamber 5 is provided inside the rotating spindle 3 and below the inner chamber 5, and a plurality of groups of cooling grooves 7 arranged in a ring array and extending to the bottom of its outer surface are provided inside the rotating spindle 3;

[0031] Furthermore, when the rotating main shaft 3 stops rotating and in the process of moving and adjusting the drilling and milling position of the end mill 2, the feedback loop is no longer triggered due to the separation between the end mill 2 and the aluminum profile, and the conductive connection to the electric thermal expansion ring 8 is cut off. At the same time, the cutting fluid temporarily stored in the inner chamber 5 flows through the cooling groove 7 and is discharged outward, and the electric thermal expansion ring 8 on the rotating secondary shaft 1 is cooled, causing the temperature of the electric thermal expansion ring 8 to gradually decrease, and the connection strength between the rotating secondary shaft 1 and the rotating main shaft 3 is gradually reduced. When the end mill 2 contacts the aluminum profile again for drilling and milling operations, it is ensured that the end mill 2 is in a low-speed rotating motion state at the beginning.

[0032] like Figure 5 As shown, in the present technical scheme, an annular groove is provided inside the rotating spindle 3 and below the inner chamber 5, and a linkage component 6 is provided inside the annular groove, the linkage component 6 includes a sealing disk 11 arranged in the annular groove, and the inner wall of the sealing disk 11 is fixedly connected to the rotating spindle 3 through an elastic colloid 10, and a plurality of groups of guide holes 12 corresponding to the position of the cooling groove 7 are provided inside the sealing disk 11, and then the timing of the cutting fluid temporarily stored in the inner chamber 5 flowing to the cooling groove 7 is adjusted and controlled by the linkage component 6.

[0033] In the present technical solution, the guide holes 12 correspond one-to-one with the cooling grooves 7 and are interconnected in the initial stage. When the rotating spindle 3 rotates at high speed, under the action of centrifugal force, the sealing disk 11 shifts outward and pulls the elastic colloid 10, so that the positions of the guide holes 12 and the cooling grooves 7 are offset from each other and the cooling grooves 7 are blocked, so that the cutting fluid temporarily stored in the inner chamber 5 cannot flow.

[0034] like Figure 4 As shown, in the present technical solution, the cooling groove 7 is configured as a zigzag structure, and the cooling groove 7 passes through a section of the electrothermal expansion ring 8 and is parallel to the central axis thereof, while the tail section of the cooling groove 7 extends outward at an angle, wherein the zigzag structure of the cooling groove 7 is configured so that when the rotating spindle 3 rotates at a high speed, the cutting fluid retained in the cooling groove 7 can be thrown out under the action of centrifugal force, thereby effectively avoiding heat loss of the electrothermal expansion ring 8 during thermal expansion.

Claims

1. A production process for high-toughness, corrosion-resistant, shock-absorbing aluminum profiles for doors and windows, comprising a rotating secondary shaft (1), a vertical milling cutter (2) being fixedly mounted at the bottom end of the rotating secondary shaft (1), characterized in that: A rotating main shaft (3) is provided at the top of the outer surface of the rotating secondary shaft (1), and the top end of the rotating main shaft (3) is fixedly connected to the transmission main shaft, and an outer shell (4) is movably sleeved on the outer surface of the rotating main shaft (3), and the mechanism is fixedly installed on the milling machine through the outer shell (4), and an electric thermal expansion ring (8) is provided in the middle of the outer surface of the rotating secondary shaft (1), and a carbon brush (9) is fixedly installed at the top end of the rotating secondary shaft (1), and the electric thermal expansion ring (8) is conductively connected through the carbon brush (9) to form a control circuit.

2. The production process of the high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows according to claim 1 is characterized in that: A weak current system is provided between the outer surface of the rotating secondary shaft (1) and the worktable of the milling machine, and a feedback loop is formed to regulate the triggering timing and the on-off state of the control loop in the electrothermal expansion ring (8).

3. The production process of the high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows according to claim 2 is characterized in that: In the initial state, when the electrothermal expansion ring (8) has not undergone thermal expansion, its outer diameter is smaller than the inner diameter of the bottom of the rotating main shaft (3); and when the electrothermal expansion ring (8) undergoes thermal expansion due to electrical conduction, its outer diameter after expansion is larger than the inner diameter of the rotating main shaft (3).

4. The production process of the high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows according to claim 3 is characterized in that: An inner chamber (5) is provided inside the rotating spindle (3), and the inner chamber (5) is connected to a cutting fluid pipeline system via a through hole inside the rotating spindle (3). A linkage component (6) for controlling the flow timing of the cutting fluid in the inner chamber (5) is provided inside the rotating spindle (3) and below the inner chamber (5). A cooling groove (7) extending to the bottom of its outer surface is provided inside the rotating spindle (3).

5. The production process of the high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows according to claim 4 is characterized in that: An annular groove is provided inside the rotating main shaft (3) and below the inner chamber (5), and a linkage component (6) is provided inside the annular groove. The linkage component (6) includes a sealing disk (11) provided in the annular groove, and the inner wall of the sealing disk (11) is fixedly connected to the rotating main shaft (3) via an elastic colloid (10), and a guide hole (12) corresponding to the position of the cooling groove (7) is provided inside the sealing disk (11).

6. The production process of the high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows according to claim 5 is characterized in that: The guide holes (12) correspond to the cooling grooves (7) one by one and are interconnected in the initial stage. When the rotating main shaft (3) rotates at a high speed, under the action of centrifugal force, the sealing disk (11) deviates outward and pulls the elastic colloid (10), so that the positions of the guide holes (12) and the cooling grooves (7) are offset from each other and the cooling grooves (7) are blocked.

7. The production process of the high-toughness, corrosion-resistant, shock-absorbing aluminum profile for doors and windows according to claim 6 is characterized in that: The cooling groove (7) is configured as a zigzag structure, and a section of the cooling groove (7) passes through the electrothermal expansion ring (8) and is parallel to the central axis thereof, while the tail section of the cooling groove (7) extends outwardly at an angle.