Molding method for rapidly heating and cooling thermoplastic composite material
Through the 3D water path design of the mold and the multi-medium heating and cooling system, combined with the high-pressure hot and cold gas switching of the hollow mandrel air bag, the problem of long production cycle and high cost of air bag molding composite materials is solved, and the rapid and uniform heating of composite materials is achieved. Cooling reduces stress and ensures product dimensional stability.
Patent Information
- Application Number
- CN202310370930.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-10
- Publication Date
- 2024-10-15
AI Technical Summary
In the air bag molding method, the existing method of heating the mold results in a long production cycle or high production cost of composite materials, or it is difficult to control the temperature inside and outside the mold, resulting in stress problems.
The mold water channel is designed into a 3D pipeline, and a variety of media are used to alternate between different heating and cooling stages. The heating and cooling system (MHCM) combines the switching of high-pressure hot gas and cold gas in the hollow mandrel air bag to achieve a mold temperature between normal temperature and 320 degrees. Quick conversion between.
Effectively control the heating and cooling temperature and speed of composite plates, reduce production cycles, reduce stress, and ensure stable production of product dimensions.
Smart Images

Figure CN118769518A_ABST
Abstract
Description
[Technical field]
[0001] The invention relates to the technical field of composite material molding, in particular to a molding method of a thermoplastic composite material by rapid heating and cooling. [Background technology]
[0002] General thermoplastic composite materials (a general term for various thermoplastic resins reinforced with glass fiber, carbon fiber, aromatic fiber and other materials) are directly hot-pressed with molds during the hot-pressing process. However, the products formed by this method can only be 2.5D shapes. If you want to form complex 3D hollow products, you need to use the air bag forming method. Air bag forming is to place two pre-formed composite materials in a hollow mandrel air bag and then place them in the mold. The thermoplastic composite materials are softened by heating the mold, and at the same time, air is blown and pressurized on the hollow mandrel to form the thermoplastic composite materials under pressure and diffusion bonding (a process of forming a connection between two different components through interface atomic diffusion) into an integrated shape.
[0003] At present, when using the air bag molding method to mold thermoplastic composite materials, there are many ways to heat the mold: using an external heating box to heat the mold, the mold needs to be heated as a whole, and then placed to cool after the plate is formed. This method has slow heating and cooling speeds, which makes the plate molding cycle long; using a hot plate to contact the mold for conduction heating and a cold plate to contact the mold to reduce the temperature. This method has a long plate molding cycle and requires multiple sets of molds, which increases the production cost of the plate; using electromagnetic induction heating, although this method increases the heating speed, the cooling speed is still slow; using a mandrel air bag to pressurize air at normal temperature, this method has a large temperature difference between the inside and outside of the mold cavity, which makes the heating and cooling speeds slow and easily causes stress (force generated inside an object under the influence of external force) problems.
[0004] In view of the above problems, when the air bag forming method is used to form the sheet, the several methods of heating the mold currently used will lead to long production cycles of the sheet, high production costs of the sheet, or difficulty in controlling the temperature inside and outside the mold cavity.
[0005] In view of this, it is necessary to provide a molding method for thermoplastic composite materials by rapid heating and cooling to solve the above problems. [Summary of the invention]
[0006] The technical problem to be solved by the present invention is that when using the air bag molding method to mold composite materials, the currently used external heating box heating method, the hot plate contacting the mold for conduction heating, the cold plate contacting the mold to reduce the temperature method, the electromagnetic induction heating method, and the method of using normal temperature when the mandrel air bag pressurizes the air will cause the production cycle of the plate to be long, or the production cost of the plate to be high, or the temperature inside and outside the mold cavity in the mold is difficult to control. Therefore, the present invention provides a molding method for rapid heating and cooling of thermoplastic composite materials to solve the above problems.
[0007] The solution to the technical problem of the present invention is: a molding method of thermoplastic composite material by rapid heating and cooling, comprising the following steps:
[0008] S1: Placing the sheet: placing the preformed composite sheet in the hollow mandrel air bag and closing the mold to fix it;
[0009] S2: Heating and pressurizing: The mold is heated, and hot gas is introduced into the hollow mandrel air bag to increase the temperature and pressure of the mold simultaneously;
[0010] S3: Maintaining temperature and pressure: After a period of time, the sheet will soften, form, transfer texture, diffuse and bond, etc.
[0011] S4: Cooling and holding pressure: The mold starts to cool down and the sheet is cooled. The hollow mandrel air bag is replaced by cold gas to synchronize with the mold temperature so that the temperature inside and outside the sheet is cooled evenly and quickly. Then the composite sheet is cooled in the mold and has a shaping effect under the pressure of the hollow mandrel air bag.
[0012] S5: Open the mold and take out the material: the hollow mandrel air bag releases the pressure, and the mold is opened to take out the sheet.
[0013] Preferably, after the plate is placed, the mold water channel is designed as a 3D pipeline, and a heating and cooling system (MHCM) is used to start heating and heating, and low-pressure gas (about 1-10 atmospheres) is introduced into the hollow core shaft.
[0014] Preferably, the mold water channel is designed as a 3D pipeline using a multi-medium heating and cooling system (MHCM), the heating heat source can be steam, hot water, hot oil, and the cooling cold source can be air, cold water, and cold oil.
[0015] Preferably, the temperature at which the mold is heated is adjusted according to the melting point of the thermoplastic material of the composite plate and the pressed shape of the product.
[0016] Preferably, the medium introduced into the hollow core shaft air bag is high-pressure hot gas or cold gas, the high-pressure hot gas can be water vapor or air, the cold gas can be air, and the gas introduced into the hollow core shaft air bag can be internal heating gas or external heating gas.
[0017] The beneficial effect of the present invention is that the mold water channel is mainly designed as a 3D water channel, and a variety of media are used to alternately heat and cool the mold pipeline at different stages of heating and cooling, and high-pressure hot gas and cold gas are introduced into the hollow core shaft air bag to switch and quickly heat and cool the mold temperature between room temperature and 320 degrees. The temperature and speed of heating and cooling of the composite plate are effectively and stably controlled, so that the plate is quickly and evenly heated or cooled inside and outside the mold, which reduces the production cycle of the product, and reduces the stress of the plate when heated or cooled in the mold, so that the product size can be stably produced.
Brief Description of the Drawings
[0018] Figure 1 The present invention is a flow chart of a method for rapidly heating and cooling a thermoplastic composite material. [Specific implementation method]
[0019] To further illustrate the technical means and effects adopted by the present invention, the following is a detailed description in conjunction with the embodiments of the present invention and the accompanying drawings.
[0020] The present invention provides a molding method of a thermoplastic composite material by rapid heating and cooling, comprising the following steps:
[0021] S1: Placing the sheet: placing the preformed composite sheet in the hollow mandrel air bag and closing the mold to fix it;
[0022] S2: Heating and pressurizing: The mold is heated, and hot gas is introduced into the hollow mandrel air bag to increase the temperature and pressure of the mold simultaneously (the pressure in the air bag comes from the introduced gas);
[0023] S3: Maintaining temperature and pressure: After a period of time, the board will soften and form (a processing technology that heats the composite board to soften it and then forms it through a mold), transfer texture (refers to the process of processing different bright and matte lines on the mold surface to combine various texture patterns during the manufacturing process, and transferring the pattern on the mold to the surface of the composite board by high temperature and high pressure), diffusion bonding (refers to the process of heating and pressing two or more materials at a certain temperature, pressure and time during the manufacturing process of the composite board, so that the thermoplastic material softens and causes diffusion reaction between its molecules, thereby achieving a firm bond of the composite material), etc.
[0024] S4: Cooling and holding pressure: The mold starts to cool down and the sheet is cooled. The hollow mandrel air bag is replaced by cold gas to synchronize with the mold temperature so that the temperature inside and outside the sheet is cooled evenly and quickly. Then the composite sheet is cooled in the mold and has a shaping effect under the pressure of the hollow mandrel air bag.
[0025] S5: Open the mold and take out the material: the hollow mandrel air bag releases the pressure, and the mold is opened to take out the sheet.
[0026] Among them, after the plate is placed, the mold water channel is designed into a 3D pipeline, and a heating and cooling system (MHCM) is used to start heating and heating, and low-pressure gas (about 1-10 atmospheres) is passed into the hollow core shaft.
[0027] Among them, the mold water channel is designed as a 3D pipeline using a multi-media heating and cooling system (MHCM). The heating heat source can be steam, hot water, hot oil, and the cooling cold source can be air, cold water, and cold oil.
[0028] The temperature at which the mold is heated is adjusted according to the melting point of the thermoplastic material of the composite plate and the pressed shape of the product.
[0029] Among them, the medium introduced into the hollow core shaft air bag is high-pressure hot gas or cold gas, the high-pressure hot gas can be water vapor or air, the cold gas can be air, and the gas introduced into the hollow core shaft air bag can be internal heating gas (referring to the gas heated inside the mold, usually by introducing a heating medium such as an electric heating coil into the mold to achieve heating) or external heating gas (referring to the gas heated outside the mold, usually by electric heating or boiler steam to achieve heating).
[0030] The beneficial effect of the present invention is that the mold water channel is mainly designed as a 3D water channel, and a variety of media are used to alternately heat and cool the mold pipeline at different stages of heating and cooling, and high-pressure hot gas and cold gas are introduced into the hollow core shaft air bag to switch and quickly heat and cool the mold temperature between room temperature and 320 degrees. The temperature and speed of heating and cooling of the composite plate are effectively and stably controlled, so that the plate is quickly and evenly heated or cooled inside and outside the mold, which reduces the production cycle of the product, and reduces the stress of the plate when heated or cooled in the mold, so that the product size can be stably produced.
[0031] It should be pointed out that the present invention is not limited to the above-mentioned implementation modes, and any simple modifications, equivalent changes and modifications made to the above-mentioned embodiments by any technician familiar with the profession based on the technical solution of the present invention fall within the protection scope of the present invention.
Claims
1. A method for rapidly heating and cooling a thermoplastic composite material, characterized in that: The following steps are involved: S1: Placing the sheet: placing the preformed composite sheet in the hollow mandrel air bag and closing the mold to fix it; S2: Heating and pressurizing: The mold is heated, and hot gas is introduced into the hollow mandrel air bag to increase the temperature and pressure of the mold simultaneously; S3: Maintaining temperature and pressure: After a period of time, the sheet will soften, form, transfer texture, diffuse and bond, etc. S4: Cooling and holding pressure: The mold starts to cool down and the sheet is cooled. The hollow mandrel air bag is replaced by cold gas to synchronize with the mold temperature so that the temperature inside and outside the sheet is cooled evenly and quickly. Then the composite sheet is cooled in the mold and has a shaping effect under the pressure of the hollow mandrel air bag. S5: Open the mold and take out the material: the hollow mandrel air bag releases the pressure, and the mold is opened to take out the sheet.
2. A method for rapidly heating and cooling a thermoplastic composite material as claimed in claim 1, characterized in that: in, After the plate is placed, the mold water channel is designed into a 3D pipeline, and the heating and cooling system (MHCM) is used to start heating and heating, and low-pressure gas (about 1-10 atmospheres) is passed into the hollow core shaft.
3. A method for rapidly heating and cooling a thermoplastic composite material as claimed in claim 1, characterized in that: The mold water channel is designed as a 3D pipeline and adopts a multi-medium heating and cooling system (MHCM). The heating source can be steam, hot water, hot oil, and the cooling source can be air, cold water, and cold oil.
4. A method for rapidly heating and cooling a thermoplastic composite material as claimed in claim 1, characterized in that: The temperature at which the mold is heated is adjusted according to the melting point of the thermoplastic material of the composite plate and the pressed shape of the product.
5. A method for rapidly heating and cooling a thermoplastic composite material as claimed in claim 1, characterized in that: The medium introduced into the hollow core shaft air bag is high-pressure hot gas or cold gas, the high-pressure hot gas can be water vapor or air, the cold gas can be air, and the gas introduced into the hollow core shaft air bag can be internal heating gas or external heating gas.
Citation Information
Patent Citations
Inner and outer heating forming process for composition material tubing
CN101767461A
Acrylic aquarium forming die and application method thereof
CN104249423A
Injection molding process of salad plate
CN109693334A
Rotary tube making device
CN110744782A
Manufacturing method of carbon fiber automobile hub
CN113021850A