Foaming sole preparation method

The three-layer structural film is formed by a casting machine and the foaming shaping process is used to solve the problems of the traditional shoe sole preparation process being cumbersome and high equipment investment, achieving efficient and stable sole production, and reducing the defective product rate and equipment costs.

CN118769585APending Publication Date: 2024-10-15袁胜凡
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411200644.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

The traditional sole preparation process is cumbersome, the production efficiency is low, the product quality is unstable, and the equipment investment and maintenance costs are high. The existing technology has low equipment utilization when changing colors, and the embossing cooling step requires additional equipment, which increases production costs.

Method used

A casting machine is used to form a three-layer cast film. The middle layer is a TPU layer without adding pigments, and the sides are a hot melt adhesive layer and a dyeing raw material layer. The sole is made through a foaming and shaping process, omitting the base mold and embossing equipment. It is cut using laser or vibrating knife. The hot-melt adhesive layer is self-shaped, and foaming raw materials are added for heating and foaming.

Benefits of technology

Save manpower and material resources, improve production efficiency, ensure product stability and quality, reduce defective products, zero defective product rate, reduce equipment investment and maintenance costs, and improve equipment utilization.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a foamed shoe sole preparation method, which comprises the steps of casting, rolling, cutting and foaming and shaping, and is characterized in that a casting film with a three-layer structure is formed by adopting a casting process, and the shoe sole is manufactured by adopting a secondary foaming and forming mode after cutting. Compared with a traditional forming process that TPU raw materials are ejected into a negative film mold through a vertical or horizontal ejection machine, the forming process does not need the vertical or horizontal ejection machine, the cost for opening the negative film mold is saved, the plant cost and the mold maintenance cost needed for storing the negative film mold are also saved, the negative film is provided with a hot melt adhesive layer, and the production cost is reduced. The steps of glue brushing, attaching and press-fit shaping are omitted, the stability and quality of products are ensured, manpower and material resources are saved, the production efficiency is improved, and zero defective products can be achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for preparing a shoe material, in particular to a method for preparing a sole. Background Art

[0002] The traditional process of preparing the sole is: after the raw materials are melted, they are injected into the base mold and the outsole mold respectively by a vertical or horizontal injection machine to make the base and the outsole respectively, and then the base and the outsole are glued and pressed together. This processing method requires a large number of base molds, and the gluing and laminating processes are generally done manually. The processing process is relatively cumbersome and the production efficiency is not high. In addition, due to the differences in manual operations, the product quality is unstable and the defective rate is also high.

[0003] To this end, the patent document with publication number CN111269552A discloses a non-slip and wear-resistant shoe material and a preparation method thereof, which adopts the technical scheme of: preparing a semi-finished product through a casting step after melting the raw materials, and then forming a TPU film (i.e., a bottom film, the bottom film made by this molding process is very thin, mainly used as the side wall of the sole, i.e., the part that does not contact the ground) through an embossing cooling step, and then shaping it through a heating and blistering method, and finally pouring PU to make a sole. This method adopts a casting process, and indeed omits the molding mold of the bottom film, but it also has obvious disadvantages. The first disadvantage is that when producing the bottom film, the TPU main material, color masterbatch, anti-slip masterbatch, wear-resistant masterbatch and additives are mixed. The added anti-slip masterbatch, wear-resistant masterbatch and other ingredients will change the physical properties of the TPU main material, reduce the elasticity of the bottom film, and affect the performance of the product. The second disadvantage is that during production, if the color of the bottom film needs to be changed, the casting machine (screw, casting die head and other mechanisms) needs to be stopped and cleaned, which leads to a decrease in equipment utilization and a decrease in production efficiency. The third disadvantage is that the embossing cooling step requires an embossing machine, and the sole manufacturer needs to purchase additional embossing machine equipment and a large number of embossing rollers, which increases the equipment investment of the sole manufacturer, the plant investment for storing the embossing rollers, and the maintenance cost of the embossing rollers. Summary of the invention

[0004] In order to overcome the deficiencies of the prior art, the present invention provides a method for preparing a foamed sole which can save manpower and material resources, improve production efficiency, and achieve zero defective products.

[0005] The technical solution adopted by the present invention to solve its technical problem is: A method for preparing a foamed sole, the preparation method is as follows: (1) Casting: A three-layer cast film is formed by casting using a casting machine. The middle layer is a main raw material layer without adding pigments. One side of the middle layer is a hot melt adhesive layer, and the other side is a dyeing raw material layer with added pigments. The melting temperature of the hot melt adhesive layer is lower than the melting temperature of the main raw material layer and the dyeing raw material layer. The raw material of the main raw material layer is TPU, the raw material of the dyeing raw material layer is a mixture of TPU and masterbatch, and the raw material of the hot melt adhesive layer is EVA. The thickness of the hot melt adhesive layer is 0.1 to 0.12 mm, the thickness of the middle layer is 0.5 to 3 mm, and the thickness of the dyeing raw material layer is 0.5 to 3 mm.

[0006] (2) Rolling up: A release paper is attached to the dyeing material layer side of the cast film and rolled up to form a roll. The release paper has a concave-convex texture on one side thereof that is in contact with the dyeing material layer.

[0007] (3) Cutting: Use cutting equipment to cut the roll into films of required specifications, retaining the release paper during cutting. In this step, laser cutting equipment or vibrating knife cutting machine is used to cut the roll.

[0008] (4) Foaming and shaping: With the hot melt adhesive layer facing upward, place the bottom film into the lower mold of the molding mold, then add the foaming raw material, close the upper mold, and take it out after heating and foaming to obtain the foamed sole. In this step, the temperature of the lower mold is greater than or equal to the melting temperature of the hot melt adhesive layer but less than the melting temperature of the main raw material layer and the dyeing raw material layer, so that the hot melt adhesive layer melts, the main raw material layer and the dyeing raw material layer soften but do not melt, and the foaming raw material is a mixture of EVA and foaming powder. In this step, the temperature of the lower mold is 80 to 120°C, and the temperature of the upper mold is 180 to 200°C. In this step, the foaming raw material added is a pre-made block mold base.

[0009] The beneficial effects of the present invention are as follows: the present invention adopts casting to form a three-layer structure of the cast film, and then manufactures the sole by secondary foaming molding, thereby omitting the cost of opening a bottom film mold, and also saving the factory cost and mold maintenance cost required for storing the bottom film mold. The bottom film has its own hot-melt adhesive layer, eliminating the steps of brushing glue, laminating, and pressing to finalize the shape, thereby ensuring the stability and quality of the product, saving manpower and material resources, improving production efficiency, and achieving zero defective products. DETAILED DESCRIPTION

[0010] A method for preparing a foamed sole, the preparation method is as follows: (1) Casting: A three-layer cast film is formed by casting using a casting machine. The middle layer is a main raw material layer without adding pigments. One side of the middle layer is a hot melt adhesive layer, and the other side is a dyeing raw material layer with added pigments. The melting temperature of the hot melt adhesive layer is lower than the melting temperature of the main raw material layer and the dyeing raw material layer. From bottom to top, the order of the three-layer structure can be hot melt adhesive layer-middle layer-dyeing raw material layer, or dyeing raw material layer-middle layer-hot melt adhesive layer. There are no special requirements for the operation and process of the casting equipment, and it can be operated according to general routines.

[0011] In this embodiment, the raw material of the main raw material layer is pure TPU (thermoplastic polyurethane elastomer). The raw material of the dyeing raw material layer is a mixture of pure TPU and masterbatch. The mixing ratio can be adjusted according to the required color according to the routine. Of course, the main raw material layer can also be other materials, and the dyeing raw material layer can also add other ingredients. The raw material of the hot melt adhesive layer is EVA (ethylene-vinyl acetate copolymer). The thickness of the hot melt adhesive layer is 0.1 to 0.12 mm, the thickness of the intermediate layer is 0.5 to 3 mm, and the thickness of the dyeing raw material layer is 0.5 to 3 mm.

[0012] The casting temperature of the hot melt adhesive layer, i.e. EVA, is 80 to 120°C, and is heated in an incremental manner. The casting temperature of the middle layer, i.e. TPU, is 180 to 190°C, and is heated in a five-stage temperature increment manner. The starting temperature of the hot melt screw is 80 to 90°C, and the ending temperature is 180 to 190°C (the 5-stage temperature here is set to: 80.120.160.190.185, respectively). The casting temperature of the dyeing material layer, i.e. the mixture of TPU and masterbatch, is 180 to 190°C, and is heated in a five-stage temperature increment manner. The starting temperature of the hot melt screw is 80 to 90°C, and the ending temperature is 180 to 190°C.

[0013] This embodiment uses an intermediate layer without adding other substances, that is, a pure TPU layer. On the one hand, the physical properties of the intermediate layer will not be changed, so that the intermediate layer can maintain the original advantages of the raw material such as high strength, high toughness, and high elasticity. On the other hand, when the color of the sole needs to be changed, it is only necessary to stop the screw and the casting head of the dyeing raw material layer, and the casting machine can continue to produce transparent bottom film made of pure TPU material. The phenomenon of the entire casting machine being shut down due to cleaning of the screw and the casting head will not occur, which effectively improves the utilization rate of the equipment and improves production efficiency.

[0014] For shoe sole manufacturers, using traditional production processes, they often need to open hundreds of sets of film molds (the patterns of the film molds are different, and the film molds of each pattern have various specifications), and need to pay a lot of fees for opening the film molds. Storing these film molds also requires a large space. Moreover, for film molds that have not been used for a long time, regular maintenance is also required to prevent rust, etc., and maintaining the film molds also requires a lot of manpower and material resources. Since the present invention adopts the casting process to form the three-layer structure of the film, the cost of opening the film mold is omitted, and the factory cost and mold maintenance cost required for storing the film mold are also saved.

[0015] (2) Rolling: Add release paper to the dyeing material layer side of the cast film and roll it up to form a roll. According to the design requirements, the release paper can be smooth or embossed on one or both sides. It only needs to be provided with a concave-convex texture on the side of the release paper that is in contact with the dyeing material layer. When rolling up, the temperature of the dyeing material layer is high and it is in a softened state. When rolling up, the layers are tightly squeezed, and the fine concave-convex texture on the release paper can be transferred to the dyeing material layer. If it is a double-sided embossed release paper, a concave-convex texture will also be formed on the hot melt adhesive layer. However, in the later foaming and shaping, the hot melt adhesive layer needs to be melted, which will not affect the performance of the product. The release paper is provided by a special release paper manufacturer. The embossing machine, technology and other equipment and processes of the release paper manufacturer are mature, and its production cost is very low. The sole manufacturer does not need to be equipped with embossing machines and other equipment, which saves the purchase cost of embossing machines and a large number of embossing rollers, and also saves the storage and maintenance costs of embossing rollers.

[0016] (3) Cutting: Cut the coil into films of required specifications using cutting equipment. Keep the release paper during cutting. The release paper is attached to the film. This is because if the release paper is removed, the TPU films will stick together when they are packed. Therefore, for the convenience of packing, the release paper is kept in this step. In this step, the coil can be cut by laser cutting equipment or by a vibrating knife cutting machine. There are no special requirements for these two types of equipment. They can be operated according to the normal procedures. Both cutting methods do not require the opening of cutting dies of various sizes, thus saving the purchase, storage and maintenance costs of cutting dies.

[0017] (4) Foaming and shaping: With the hot melt adhesive layer facing upward, place the bottom sheet into the lower mold of the molding mold, then add the foaming raw material, close the upper mold, and take it out after heating and foaming to obtain the foamed sole. In this step, the temperature of the lower mold is greater than or equal to the melting temperature of the hot melt adhesive layer but lower than the melting temperature of the main raw material layer and the dyeing raw material layer, so that the hot melt adhesive layer melts and the main raw material layer and the dyeing raw material layer soften, without destroying the concave and convex texture formed during winding.

[0018] In this embodiment, the foaming raw material is a mixture of EVA and foaming powder. The melting point of EVA is 80 to 120°C, and the melting point of the high-temperature TPU used is 180 to 190°C. In this step, the temperature of the lower mold is 80 to 120°C. At this time, the hot melt adhesive layer, i.e., EVA, can be fully melted. The middle layer and the dyeing raw material layer are only softened because they have not yet reached the melting point. After closing the upper mold, at 180-200°C, the foaming raw material is heated and foamed in the closed mold cavity. The foaming pressure will be transmitted to all sides, making the foaming layer and the bottom film more tightly and firmly combined. At the same time, the foaming pressure will also squeeze the middle layer and the dyeing raw material layer. The lower mold can be a plane, and the concave-convex texture formed during winding is retained after molding. A concave-convex structure can be set in the lower mold to produce a concave-convex structure on the molded sole. The difference between the concave-convex structure formed in the foaming step and the concave-convex texture formed in the winding process is that the concave-convex texture formed in the winding process has a small difference in height and a finer texture, while the concave-convex structure formed in the foaming step has a large difference in height, and mainly forms a functional concave-convex structure such as anti-slip.

[0019] In this step, the added foaming raw material can be a mixture of untreated EVA particles and foaming powder, which may cause density differences in various places and affect the quality of the product. It can also be a pre-made block mold base, that is, the EVA particles and foaming powder are first mixed according to the proportion, and then added to the mold base mold, and heated to make the EVA particles close to a molten state to make a sheet mold base with a similar shape but smaller specifications. When making the mold base, the foaming temperature of the foaming powder has not yet been reached, and the raw material will not foam. After being placed in the upper mold, it is foamed at high temperature to make the density consistent everywhere.

[0020] In this step, since the film has its own hot-melt adhesive layer, the steps of brushing glue, laminating, and pressing are omitted, thus ensuring the stability and quality of the product, saving manpower and material resources, improving production efficiency, and achieving zero defective products.

[0021] The above implementation modes cannot limit the protection scope of the present invention. The equivalent modifications and changes made by those skilled in the art without departing from the overall concept of the present invention are still within the scope of the present invention.

Claims

1. A method for preparing a foamed sole, Features The preparation method is as follows: (1) Casting: A three-layer cast film is formed by casting using a casting machine. The middle layer is a main raw material layer without adding pigments. One side of the middle layer is a hot melt adhesive layer, and the other side is a dyeing raw material layer with added pigments. The melting temperature of the hot melt adhesive layer is lower than the melting temperature of the main raw material layer and the dyeing raw material layer. (2) Winding: Attach release paper to the dyeing material layer side of the cast film and roll it up to form a roll; (3) Cutting: Use cutting equipment to cut the roll into films of required specifications, and keep the release paper during cutting; (4) Foaming and shaping: With the hot melt adhesive layer facing upward, place the bottom sheet into the lower mold of the molding mold, then add the foaming raw material, close the upper mold, and take it out after heating and foaming to obtain the foamed sole; in this step, the temperature of the lower mold is greater than or equal to the melting temperature of the hot melt adhesive layer but less than the melting temperature of the main raw material layer and the dyeing raw material layer, so that the hot melt adhesive layer melts and the main raw material layer and the dyeing raw material layer soften.

2. The method for preparing a foamed sole according to claim 1, Features The main raw material layer is pure TPU.

3. The method for preparing a foamed sole according to claim 2, Features The dyeing material layer is a mixture of TPU and masterbatch.

4. The method for preparing a foamed sole according to claim 3, Features The hot melt adhesive layer is EVA.

5. The method for preparing a foamed sole according to claim 4, Features The foaming raw material is a mixture of EVA and foaming powder.

6. The method for preparing a foamed sole according to claim 5, Features In the step (4), the temperature of the lower mold is 80 to 120°C, and the temperature of the upper mold is 180 to 200°C.

7. The method for preparing a foamed sole according to claim 1, Features A side of the release paper that is attached to the dyeing material layer is provided with a concave-convex texture.

8. The method for preparing a foamed sole according to claim 1, Features In the step (3), the coil is cut by using a laser cutting device or a vibrating knife cutting machine.

9. The method for preparing a foamed sole according to claim 1, Features The thickness of the hot melt adhesive layer is 0.1 to 0.12 mm, the thickness of the intermediate layer is 0.5 to 3 mm, and the thickness of the dyeing material layer is 0.5 to 3 mm.

10. The method for preparing a foamed sole according to claim 1, Features In the step (4), the foaming raw material added is a pre-made block-shaped mold base.

Citation Information

Patent Citations

  • Antiskid wear-resistant shoe material and preparation method thereof

    CN111269552A

  • Manufacturing method for composite shoe solesof large bottom suction forming

    CN108081651A

  • Method for manufacturing shoe outsole with TPU high-low-temperature film

    CN108099240A