Preparation method of high-quality 5-(2, 5-dioxotetrahydrofuran)-3-methyl-3-cyclohexene-1, 2-dicarbonic anhydride
By using a mixture of maleic anhydride, 3-methyltetrahydrophenic anhydride and a catalyst in the synthesis of 5-(2,5dioxotetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarboxylic anhydride The reaction, combined with deionization reagent treatment, solves the problems of high high temperature energy consumption, low yield and high production cost in the existing technology, achieves the preparation of high-quality products and safe reaction conditions, and is suitable for large-scale production.
Patent Information
- Application Number
- CN202410855479.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-06-28
AI Technical Summary
The synthesis method of 5-(2,5dioxotetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarboxylic anhydride in the prior art has the problems of high temperature, high energy consumption, low yield, high production cost and Dangerous reactions and poor product quality.
Using a mixed reaction of maleic anhydride, 3-methyltetrahydrophthalic anhydride, catalyst and solvent, through insulation and subsequent deionization reagent treatment, combined with specific molar ratio and temperature conditions, high-quality 5-(2,5-dihydrophosphate is prepared Oxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarboxylic anhydride, using non-metallic catalysts and post-processing to improve product quality.
Achieved the preparation of high-yield, high-quality 5-(2,5dioxotetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarboxylic anhydride, reduced production costs, and improved reaction safety sex, and suitable for large-scale production.
Smart Images

Figure CN118772097A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of organic synthesis, and in particular relates to a method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride. Background Art
[0002] Polyimide (PI) is a polymer composed of amide rings. Due to its unique structure, it has excellent comprehensive properties and is at the forefront of polymer materials. PI has been widely used in flexible displays, aerospace, electrical insulation, microelectronics, batteries, photoresists and other fields.
[0003] Aliphatic polyimide has more excellent optical properties and processability because it contains rigid imide ring and aliphatic ring. 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride is an important polyimide monomer, and the polyimide synthesized from it has broad application prospects.
[0004] At present, the common synthesis method is mainly: using maleic anhydride and 3-methyltetrahydrophthalic anhydride as starting materials, and synthesizing 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride through a high temperature reaction at 200°C. This method has high high temperature energy consumption, low yield (about 20%), poor product quality, dangerous reaction, and high production cost. Invention content
[0005] In view of this, the present invention aims to propose a method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride to solve at least one technical problem in the background technology. The present application can solve the problems of low synthesis yield, high production cost, dangerous reaction and poor product quality.
[0006] To achieve the above object, the technical solution created by the present invention is implemented as follows:
[0007] A method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride comprises the following steps:
[0008] S1: maleic anhydride, 3-methyltetrahydrophthalic anhydride, catalyst and solvent are mixed, stirred and heated to a certain temperature, and kept warm for reaction. After the reaction is completed, a mixed solution is obtained;
[0009] S2: adding a deionizing agent to the mixed solution, stirring and cooling to precipitate a solid, and post-treating the precipitated solid to obtain high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride.
[0010] Furthermore, the molar ratio of the solvent, the catalyst, maleic anhydride and 3-methyltetrahydrophthalic anhydride in step S1 is (15-30):(0.01-0.1):(1-1.5):1.
[0011] Further, the solvent in step S1 is one or more of acetonitrile, tetrahydrofuran, and 1,4-dioxane;
[0012] Preferably, the solvent is acetonitrile.
[0013] Furthermore, the catalyst in step S1 is one or more of triphenylmethylphosphonium iodide, trimethylsilyl trifluoromethanesulfonate, and boron trifluoride etherate.
[0014] Preferably, the catalyst is triphenylmethylphosphonium iodide.
[0015] Furthermore, the reaction temperature in step S1 is 20-50° C., and the reaction time is 2-8 h.
[0016] Further, the deionizing agent in step S2 includes one or more of thioglycolic acid, ammonium thioglycolate, and cysteine;
[0017] Preferably, the deionizing agent is thioglycolic acid;
[0018] Furthermore, the post-treatment of the precipitated solid in step S2 includes cooling the precipitated solid, washing it with a poor solvent, filtering it again, and drying the solid to obtain high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride.
[0019] Furthermore, in step S2, the molar ratio of the poor solvent, the deionizing agent, and 3-methyltetrahydrophthalic anhydride is (10-20):(0.2-1):1.
[0020] Furthermore, the poor solvent includes one or more of n-hexane, toluene, and xylene. Preferably, the poor solvent is toluene.
[0021] And / or, the temperature for precipitation in step S2 is 5 to -10°C;
[0022] And / or, the vacuum drying temperature in step S2 is 90-130° C., and the vacuum drying time is 8-12 hours.
[0023] The high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride prepared by the above-mentioned preparation method of high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride is characterized in that: the chromaticity YI is less than 0.3 and the total metal ion is less than 100 ppb;
[0024] Preferably, the polymerization viscosity of high-quality 5-(2,5-dioxotetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride and 2,2'-bis(trifluoromethyl)-(1,1'-diphenyl)-4,4'-diamine (TFMB), 2,2-bis(4-aminophenyl)hexafluoropropane (FA), and 4,4'-diaminodiphenyl ether (ODA) is at least 1.35 million, and preferably the polymerization viscosity is 1.45 to 1.8 million.
[0025] Compared with the prior art, the method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride created by the present invention has the following advantages:
[0026] The preparation method of the invention adopts a new process system, takes maleic anhydride and 3-methyltetrahydrophthalic anhydride as raw materials, innovatively uses a non-metallic catalyst, and reacts to prepare high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride. The preparation method of the invention is simple, safe to operate, has a high yield and high quality of the synthesized product, and is suitable for large-scale production. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The drawings constituting part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments and descriptions of the present invention are used to explain the present invention and do not constitute an improper limitation on the present invention. In the drawings:
[0028] Figure 1 The synthetic route of 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride of the present invention is as follows;
[0029] Figure 2 This is the HPLC chart of 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride prepared in Example 1 of the present invention. DETAILED DESCRIPTION
[0030] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.
[0031] The present invention will be described in detail below with reference to the accompanying drawings and in combination with embodiments.
[0032] Example 1
[0033] 20g 3-methyltetrahydrophthalic anhydride, 14.17g maleic anhydride and 1g triphenylmethylphosphonium iodide were added to 100g acetonitrile, stirred until dissolved, the reaction temperature was raised to 40°C, and the reaction was kept warm for 3h. 1.1g thioglycolic acid was added to the system and stirred for 2h. The temperature was lowered to 0°C, and a large amount of white crystals were precipitated. After filtering, 150g toluene was used to wash for 1h. After filtering, the solid was vacuum dried at 110°C for 12h to obtain 29.21g 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride, with a molar yield of 91.87%, a purity of 99.99%, YI=0.11, a total metal ion of 50ppb, and a polymerization viscosity of 1.68 million with TFMB.
[0034] Example 2
[0035] 20g 3-methyltetrahydrophthalic anhydride, 13.01g maleic anhydride and 1.2g triphenylmethylphosphonium iodide were added to 138g tetrahydrofuran acetonitrile, stirred until dissolved, the reaction temperature was raised to 35°C, and the reaction was kept warm for 3.5h. 1.5g thioglycolic acid was added to the system and stirred for 2h. The temperature was lowered to 5°C, and a large amount of white crystals were precipitated. After filtering, 150g toluene was used to wash for 1h. After filtering, the solid was vacuum dried at 110°C for 12h to obtain 28.51g 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride, with a molar yield of 89.64%, a purity of 99.96%, YI=0.19, a total metal ion of 63ppb, and a polymerization viscosity of 1.59 million with FA.
[0036] Example 3
[0037] 20g 3-methyltetrahydrophthalic anhydride, 14.45g maleic anhydride and 1.15g triphenylmethylphosphonium iodide were added to 107g 1,4-dioxane, stirred until dissolved, the reaction temperature was raised to 45°C, and the reaction was kept warm for 4h. 1.3g thioglycolic acid was added to the system and stirred for 2h. The temperature was lowered to -10°C, and a large amount of white crystals were precipitated. After filtering, 150g toluene was used to wash for 1h. After filtering, the solid was vacuum dried at 110°C for 12h to obtain 27.93g 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride, with a molar yield of 87.84%, a purity of 99.94%, YI=0.23, a total metal ion of 75ppb, and a polymerization viscosity of 1.61 million with ODA.
[0038] Example 4
[0039] 20g 3-methyltetrahydrophthalic anhydride, 14.21g maleic anhydride and 1.33g trimethylsilyl trifluoromethanesulfonate were added to 100g acetonitrile, stirred until dissolved, the reaction temperature was raised to 40°C, and the reaction was kept warm for 3h. 1.1g thioglycolic acid was added to the system and stirred for 2h. The temperature was lowered to 0°C, and a large amount of white crystals were precipitated. After filtering, 150g toluene was used to wash for 1h. After filtering, the solid was vacuum dried at 110°C for 12h to obtain 27.96g 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride, with a molar yield of 87.94%, a purity of 99.97%, YI=0.24, a total metal ion of 54ppb, and a polymerization viscosity of 1.53 million with TFMB.
[0040] Comparative Example 1
[0041] 20 g of 3-methyltetrahydrophthalic anhydride and 23.67 g of maleic anhydride were heated to 200°C and kept for reaction for 4 hours. The temperature was maintained and the raw materials were recovered by vacuum distillation to obtain 9.37 g of brown crude product. 30 g of methyl isobutyl ketone was added and the temperature was raised to 110°C for dissolution. The temperature was lowered to room temperature to precipitate gray-white crystals. The crystals were vacuum dried at 110°C for 12 hours to obtain 5.37 g of 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride. The molar yield was 16.89%, the purity was 99.27%, the YI was 10.98, the total metal ions were 6.7 ppm, and the polymerization viscosity with TFMB was 730,000.
[0042] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
[0043] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride, characterized in that: The steps include: S1: maleic anhydride, 3-methyltetrahydrophthalic anhydride, catalyst and solvent are mixed, stirred and heated to a certain temperature, and kept warm for reaction. After the reaction is completed, a mixed solution is obtained; S2: adding a deionizing agent to the mixed solution, stirring and cooling to precipitate a solid, and post-treating the precipitated solid to obtain high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride.
2. The method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 1, characterized in that: The molar ratio of the solvent, the catalyst, maleic anhydride and 3-methyltetrahydrophthalic anhydride in step S1 is (15-30):(0.01-0.1):(1-1.5):
1.
3. The method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 1, characterized in that: The solvent in step S1 is one or more of acetonitrile, tetrahydrofuran, and 1,4-dioxane; Preferably, the solvent is acetonitrile.
4. The method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 1, characterized in that: The catalyst in step S1 is one or more of triphenylmethylphosphonium iodide, trimethylsilyl trifluoromethanesulfonate, and boron trifluoride etherate. Preferably, the catalyst is triphenylmethylphosphonium iodide.
5. The method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 1, characterized in that: The reaction temperature in step S1 is 20-50° C., and the reaction time is 2-8 hours.
6. A method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 1, characterized in that: The deionizing agent in step S2 includes one or more of thioglycolic acid, ammonium thioglycolate, and cysteine; Preferably, the deionizing agent is thioglycolic acid.
7. A method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 1, characterized in that: The post-treatment of the precipitated solid in step S2 includes cooling the precipitated solid, washing with a poor solvent, filtering again, and drying the solid to obtain high-quality 5-(2,5-dioxotetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride.
8. The method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 7, characterized in that: In step S2, the molar ratio of the poor solvent, the deionizing agent, and 3-methyltetrahydrophthalic anhydride is (10-20):(0.2-1):
1.
9. The method for preparing high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to claim 7, characterized in that: The poor solvent includes one or more of n-hexane, toluene, and xylene. Preferably, the poor solvent is toluene; And / or, the temperature for precipitation in step S2 is 5 to -10°C; And / or, the vacuum drying temperature in step S2 is 90-130° C., and the vacuum drying time is 8-12 hours.
10. A high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride prepared by the method for preparing a high-quality 5-(2,5-dioxytetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride according to any one of claims 1 to 9, characterized in that: Chromaticity YI is less than 0.3, total metal ions are less than 100ppb; Preferably, the polymerization viscosity of high-quality 5-(2,5-dioxotetrahydrofuran)-3-methyl-3-cyclohexene-1,2-dicarbonic anhydride and 2,2'-bis(trifluoromethyl)-(1,1'-diphenyl)-4,4'-diamine (TFMB), 2,2-bis(4-aminophenyl)hexafluoropropane (FA), and 4,4'-diaminodiphenyl ether (ODA) is at least 1.35 million, and preferably the polymerization viscosity is 1.45 to 1.8 million.
Citation Information
Patent Citations
5-(2,5-Dioxotetrahydrofuryl)-3-methyl-3-cyclohexene-1,2-dicarboxylic anhydride
US4271079A
Active ester composition
WO2018173500A1