Preparation methods of catalyst, DMAA precursor and alumina film
By preparing the co-catalyst MOF-X and DMAA precursor, using water as the reaction medium and ultrasound-assisted synthesis technology, the flammability and toxicity problems of the TMA precursor are solved, achieving higher safety and environmental protection, and increasing the reaction rate. and selectivity to prepare safe and environmentally friendly alumina films.
Patent Information
- Application Number
- CN202410932850.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-10-15
AI Technical Summary
In the current manufacturing of photovoltaic cells, trimethylaluminum TMA as a precursor material has problems of flammability, high toxicity, and violent reactions, resulting in dangerous operations and environmental pollution. It is necessary to develop new precursor materials that are safe and environmentally friendly.
By preparing the co-catalyst MOF-X and DMAA precursors, using water as the reaction medium, combined with ultrasound-assisted synthesis technology, an alumina film is prepared to avoid the use of harmful organic solvents and improve the reaction rate and selectivity.
It achieves higher safety, environmental protection and ease of operation, reduces energy consumption, improves reaction rate and selectivity, and avoids the use of harmful organic solvents.
Smart Images

Figure CN118772429A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of photovoltaic cell manufacturing, and in particular to a method for preparing a composite catalyst, a DMAA precursor and an aluminum oxide film. Background Art
[0002] At present, in the manufacture of photovoltaic cells, atomic layer deposition technology ALD is widely used to deposit aluminum oxide Al2O3 thin films as passivation layers and dielectric layers of the battery. Trimethylaluminum TMA is a commonly used precursor material, which shows excellent reactivity during the deposition process. However, TMA has the disadvantages of being highly flammable, highly toxic, and violently reactive, which brings about dangerous operations and environmental problems. Therefore, it is of great significance to develop new safe and environmentally friendly precursor materials. Summary of the invention
[0003] The purpose of the present invention is to design a preparation method of a composite catalyst, a DMAA precursor and an aluminum oxide film in order to solve the above problems.
[0004] The present invention achieves the above-mentioned purpose through the following technical solutions: A method for preparing a catalyst comprises: S1. Dissolve zinc nitrate hexahydrate Zn(NO3)2·6H2O and 1,4-phthalic acid in N,N-dimethylformamide solvent, mix well, and obtain solution A; S2, heating the sealed solution A for reaction; S3, after cooling to room temperature, filtering and separating the solid product; S4, washing the solid product with N,N-dimethylformamide and ethanol; S5. Dry the washed solid product to obtain the catalyst MOF-X.
[0005] The preparation method of DMAA precursor comprises: A1, dimethylamine HNMe2 and aluminum chloride AlCl3 are placed in a three-necked flask; A2. Add the catalyst MOF-X prepared by the above preparation method into a three-necked flask and stir to react; A3, subjecting the reaction system in the three-necked flask to ultrasonic treatment; A4, removing the solvent after the reaction is completed to obtain a crude product of dimethylaluminum amine DMAA precursor; A5. Purify the crude product and dry it to obtain dimethylaluminum amine DMAA precursor.
[0006] The method for preparing an aluminum oxide film comprises injecting a dimethylaluminum amine DMAA precursor prepared by the above-mentioned preparation method and an oxygen-containing precursor into an ALD reaction chamber by alternating pulse injection, reacting with a substrate surface to form an aluminum oxide film.
[0007] The beneficial effects of the present invention are: using water as a reaction medium to avoid the use of harmful organic solvents; preparing a new metal organic framework catalyst MOF-X, and preparing a dimethylaluminum amine DMAA precursor through the catalyst MOF-X, thereby improving the reaction rate and selectivity; utilizing ultrasound-assisted synthesis technology to accelerate the reaction process and reduce energy consumption; and the dimethylaluminum amine DMAA precursor prepared by the method of the present invention has higher safety, environmental protection and ease of operation compared with a traditional TMA precursor synthesis method. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 is a flow chart of the method for preparing the catalyst of the present invention; Figure 2 It is a flow chart of the preparation method of the DMAA precursor of the present invention. DETAILED DESCRIPTION
[0009] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0010] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0011] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0012] In the description of the present invention, it should be understood that the terms "upper", "lower", "inside", "outside", "left", "right", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, or are directions or positional relationships in which the product of the invention is usually placed when in use, or are directions or positional relationships commonly understood by those skilled in the art. These directions or positional relationships are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore should not be understood as a limitation on the present invention.
[0013] Furthermore, the terms “first”, “second”, etc. are merely used for distinguishing descriptions and are not to be understood as indicating or implying relative importance.
[0014] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms such as "setting" and "connection" should be understood in a broad sense. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0015] The specific implementation modes of the present invention are described in detail below in conjunction with the accompanying drawings.
[0016] like Figure 1 As shown, the method for preparing the catalyst comprises: S1. In a nitrogen atmosphere, zinc nitrate hexahydrate Zn(NO3)2·6H2O and 1,4-phthalic acid are dissolved in N,N-dimethylformamide solvent in a molar ratio of 1:1, and mixed evenly to obtain solution A; S2, pouring solution A into a stainless steel autoclave lined with polytetrafluoroethylene and sealing it, and then placing it in an oven preheated to 120°C to react for 24 hours; S3, after naturally cooling to room temperature, filtering and separating the solid product; S4, washing the solid product with N,N-dimethylformamide and ethanol to remove unreacted raw materials and by-products; S5. The washed solid product is dried in a vacuum drying oven for at least 12 hours to obtain the catalyst MOF-X.
[0017] like Figure 2 As shown, the preparation method of DMAA precursor comprises: A1. In an anhydrous environment, dimethylamine HNMe2 and aluminum chloride AlCl3 were placed in a three-necked flask equipped with a mechanical stirrer, a temperature control system and a nitrogen introduction system in a molar ratio of 1:1; A2. Add the catalyst MOF-X prepared by the above preparation method into a three-necked flask at 0-10°C and stir the mixture under nitrogen protection to ensure that the reactants are fully mixed. A3, the reaction system in the three-necked flask was subjected to ultrasonic treatment for 2 hours, the ultrasonic frequency was 40kHz, and the power was 100W; A4, removing the solvent after the reaction is completed by rotary evaporation under reduced pressure to obtain a crude product of dimethylaluminum amine DMAA precursor; A5. The crude product is purified by high performance liquid chromatography (HPLC), and the DMAA fraction is collected and dried under nitrogen protection to obtain dimethylaluminum amine DMAA precursor.
[0018] Use water as the reaction medium to avoid the use of harmful organic solvents; prepare a new metal organic framework catalyst MOF-X, and use the catalyst MOF-X to prepare the dimethylaluminum amine DMAA precursor to improve the reaction rate and selectivity; use ultrasound-assisted synthesis technology to accelerate the reaction process and reduce energy consumption.
[0019] The present invention uses water as a reaction medium, MOF-X as a catalyst and ultrasound-assisted synthesis technology. Compared with the traditional TMA precursor synthesis method, the present invention has higher safety, environmental protection and ease of operation.
[0020] The method for preparing an aluminum oxide film comprises controlling the substrate temperature between 150° C. and 250° C., injecting a dimethylaluminum amine DMAA precursor and an oxygen-containing precursor prepared by the above-mentioned preparation method into an ALD reaction chamber by alternating pulse injection, reacting with the substrate surface to form an aluminum oxide film; and precisely controlling the growth rate and thickness of the film by controlling the pulse time, interval time and number of cycles.
[0021] The technical solution of the present invention is not limited to the above-mentioned specific embodiments. All technical variations made according to the technical solution of the present invention fall within the protection scope of the present invention.
Claims
1. A method for preparing a catalyst, characterized in that: include: S1. Dissolve zinc nitrate hexahydrate Zn(NO3)2·6H2O and 1,4-phthalic acid in N,N-dimethylformamide solvent, mix well, and obtain solution A; S2, heating the sealed solution A for reaction; S3, after cooling to room temperature, filtering and separating the solid product; S4, washing the solid product with N,N-dimethylformamide and ethanol; S5. Dry the washed solid product to obtain the catalyst MOF-X.
2. The method for preparing a catalyst according to claim 1, characterized in that: In S1, in a nitrogen atmosphere, zinc nitrate hexahydrate Zn(NO3)2·6H2O and 1,4-phthalic acid are dissolved in an N,N-dimethylformamide solvent at a molar ratio of 1:
1.
3. The method for preparing the catalyst according to claim 1, characterized in that: In S2, the heating reaction temperature is 120°C and the reaction time is 24 hours.
4. The method for preparing the catalyst according to claim 1, characterized in that: In S5, the washed solid is dried in a vacuum oven for at least 12 hours.
5. A method for preparing a DMAA precursor, characterized in that: include: A1, dimethylamine HNMe2 and aluminum chloride AlCl3 are placed in a three-necked flask; A2. Add the catalyst MOF-X prepared by the preparation method according to any one of claims 1 to 4 into a three-necked flask and stir to react; A3, subjecting the reaction system in the three-necked flask to ultrasonic treatment; A4, removing the solvent after the reaction is completed to obtain a crude product of dimethylaluminum amine DMAA precursor; A5. Purify the crude product and dry it to obtain dimethylaluminum amine DMAA precursor.
6. The method for preparing a DMAA precursor according to claim 5, characterized in that: In A1, under anhydrous environment, dimethylamine HNMe2 and aluminum chloride AlCl3 are placed in a three-necked flask in a molar ratio of 1:
1.
7. The method for preparing a DMAA precursor according to claim 5, characterized in that: In A2, the catalyst MOF-X is added into a three-necked flask at 0-10°C and stirred for reaction under nitrogen protection.
8. The method for preparing a DMAA precursor according to claim 5, characterized in that: In A3, the ultrasonic frequency was 40 kHz, the power was 100 W, and the ultrasonic treatment time was 2 hours.
9. A method for preparing an aluminum oxide film, characterized in that: The method comprises injecting a dimethylaluminum amine DMAA precursor prepared by the preparation method according to any one of claims 5 to 8 and an oxygen-containing precursor into an ALD reaction chamber by alternating pulse injection, reacting with the surface of a substrate to form an aluminum oxide film.
10. The method for preparing an aluminum oxide film according to claim 9, characterized in that: The substrate temperature was controlled between 150°C and 250°C.