Filter screen coating material for medical-grade air purifier and preparation process of filter screen coating material

By coating the air purifier filter with an adsorption, purification, self-cleaning and protective layer, the problem of impurity adhesion to the filter during the air purification process is solved, the cleanliness and service life of the filter is improved, and air resistance is reduced.

CN118772673AInactive Publication Date: 2024-10-15DONGGUAN PENGCHI INTELLIGENT EQUIP TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411020059.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing air purifier filter coating materials will adhere to a large amount of impurities during the air purification process, which increases the difficulty of cleaning the filter.

Method used

Use filter coating materials including adsorption coating, purification coating, self-cleaning coating and protective coating, through photocatalyst activator, adsorption catalyst, diatomite, nano-silica, calcium carbonate and other components, combined with silane modification Materials such as chemical epoxy resin and DMF solution are used to form a self-cleaning and protective layer, which reduces dirt adhesion and resistance and extends the life of the filter.

Benefits of technology

It improves the smoothness of the filter, reduces dirt adhesion, reduces air resistance, extends the service life of the filter, and maintains high purification efficiency and low energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118772673A_ABST
    Figure CN118772673A_ABST
Patent Text Reader

Abstract

The invention discloses a filter screen coating material for a medical-grade air purifier and a preparation process thereof, the filter screen coating material comprises a filter screen coating material, the filter screen coating material comprises an adsorption coating, a purification coating, a self-cleaning coating and a protective coating, and the adsorption coating is prepared from the following components: the adsorption coating, the purification coating, the self-cleaning coating and the protective coating. The self-cleaning coating comprises the following components in parts by weight: 30-60 parts of a photocatalyst active agent and 30-60 parts of an adsorption catalyst, and the self-cleaning coating comprises the following components in parts by weight: 20-40 parts of silane modified epoxy resin, 20-40 parts of modified titanium dioxide, 20-40 parts of a DMF solution and 20-40 parts of BMI. The adhesion and attachment of dirt and grease impurities on the filter screen are reduced, so that the blockage and resistance of the filter screen are reduced, and the labor capacity of people for cleaning the filter screen is reduced; by arranging the protective coating, a layer of protective film is formed on the outer side of the filter screen, corrosion, abrasion and oxidation of the surface of the filter screen are prevented, and therefore the service life of the filter screen is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of filter screens, and in particular to a filter screen coating material for medical-grade air purifiers and a preparation process thereof. Background Art

[0002] Medical air purifier is a device that can remove harmful substances from the air and purify the air quality. In today's increasingly serious environmental pollution, the importance of medical air purifiers cannot be ignored. First of all, medical air purifiers can effectively remove fine particles in the air through an efficient filter system. Fine particles are tiny particles with a diameter of less than 2.5 microns. They can be suspended in the air and inhaled by the human body, which has a negative impact on health. The filter of the medical air purifier can capture and filter out these fine particles to ensure the cleanliness and freshness of the indoor air. Secondly, medical air purifiers can also remove harmful gases such as formaldehyde in the air. Formaldehyde is a common indoor Air pollutants come from decoration materials, furniture, cosmetics, etc. Long-term exposure to formaldehyde will pose a serious threat to human health. The built-in activated carbon filter of the medical air purifier can effectively adsorb and decompose formaldehyde to protect the health of users. In addition, the medical air purifier also has sterilization and deodorization functions. Bacteria, viruses and other microorganisms in the air can pose a threat to human health. The built-in ultraviolet sterilization lamp of the medical air purifier can kill these microorganisms in the air and ensure the hygiene of indoor air. At the same time, the medical air purifier can also remove odors and smoke in the air to keep the indoor air fresh. The filter is one of the main components of a medical-grade air purifier.

[0003] The filter is usually coated with a material that has adsorption and filtering functions. It can adsorb and capture tiny particles and suspended matter, improve the filtering effect of the filter, and increase the capture capacity of the filter.

[0004] Comparative document, application number 2018115059294, the present invention discloses a filter that can be used for an air purifier and a preparation method thereof, the filter includes a base layer and an active layer, the base layer is a modified nickel foam mesh coated with a carbon microsphere coating, and the active layer is TiO2 co-doped with Pt, Ag, N, and F; the base layer is obtained by first reacting the nickel foam mesh in a sucrose solution, drying and roasting; then the base layer is immersed in a mixed solution formed by mixing ammonium fluorotitanate, urea and deionized water to react, and then dried and roasted to obtain a filter with a surface coated with N and F co-doped TiO2; chloroplatinic acid and silver nitrate are dissolved in distilled water, stirred at room temperature for 30 minutes, and then sodium dodecylbenzene sulfonate is added and stirred for 30 minutes, and then sodium borohydride solution is dripped into the solution to obtain an impregnation solution; then the filter with a surface coated with N and F co-doped TiO2 is immersed in the impregnation solution to react, and the filter is obtained after drying. The filter of the present invention has low air resistance and good catalytic performance;

[0005] The comparative document, application number CN201811506829.3, discloses a filter for an air purifier and a preparation method thereof, wherein the filter comprises a substrate layer and an active layer, wherein the substrate layer is a modified foam iron mesh coated with a carbon microsphere coating, and the active layer is located outside the substrate layer; the modified foam iron mesh coated with a carbon microsphere coating on the surface, i.e., the substrate layer, is obtained by immersing the foam iron mesh in a sucrose solution, and sequentially undergoing ultrasound, hydrothermal reaction, drying, and roasting; and then the substrate layer is immersed in a mixed solution formed by mixing titanyl sulfate, chloroplatinic acid, urea, and deionized water, and sequentially undergoing hydrothermal reaction, washing, drying, and roasting to obtain a filter mesh with a Pt, N, and S co-doped TiO coating on the surface. The present invention forms a modified foam iron mesh coated with a carbon microsphere coating on the surface of the foam iron mesh, so that it has both filtering and adsorption functions, and after loading the active components, a filter mesh integrating filtration, adsorption, and catalysis is obtained, which further reduces air resistance while improving the catalytic activity of the filter mesh and extending its service life.

[0006] However, the above documents still have the following disadvantages:

[0007] A filter that can be used in an air purifier has low air resistance and good catalytic performance. However, a large amount of impurities will adhere to the surface of the filter coating material during the process of the filter purifying the air, which increases the difficulty of cleaning the filter. Summary of the invention

[0008] The purpose of the present invention is to provide a medical-grade air purifier filter coating material and its preparation process, so as to solve the problem that a filter that can be used for an air purifier proposed in the above background technology has small air resistance and good catalytic performance, but a large amount of impurities will adhere to the surface of the filter coating material during the process of the filter purifying the air, which increases the difficulty of cleaning the filter.

[0009] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a medical-grade air purifier filter coating material, comprising a filter coating material, wherein the filter coating material comprises an adsorption coating, a purification coating, a self-cleaning coating and a protective coating, wherein the adsorption coating comprises the following components, by weight: 30-60 parts of a photocatalyst activator and 30-60 parts of an adsorption catalyst, and the purification coating comprises the following components, by weight: 5-15 parts of diatomaceous earth, 5-15 parts of nano-silicon dioxide, 5-15 parts of calcium carbonate, 5-15 parts of zinc oxide, 10-20 parts of a composite fiber material, and 10-20 parts of a composite fiber material. 0 parts, 10 parts to 20 parts of triethylenetetramine, 10 parts to 20 parts of calcium ferrite complex, 10 parts to 20 parts of surfactant, 10 parts to 20 parts of ethanol and 5 parts to 10 parts of adhesive, the self-cleaning coating comprises the following components, by weight: 20 parts to 40 parts of silane-modified epoxy resin, 20 parts to 40 parts of modified titanium dioxide, 20 parts to 40 parts of DMF solution and 20 parts to 40 parts of BMI, and the protective coating comprises the following components, by weight: 15 parts to 50 parts of bauxite, 20 parts to 35 parts of borax, 15 parts to 50 parts of glass powder and 20 parts to 35 parts of titanium dioxide.

[0010] As a preferred technical solution of the present invention, the adsorption coating comprises the following components, calculated by weight: 40 parts of photocatalyst activator and 60 parts of adsorption catalyst, the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 20 parts of composite fiber material, 10 parts of triethylenetetramine, 10 parts of calcium ferrite complex, 20 parts of surfactant, 10 parts of ethanol and 10 parts of adhesive, the self-cleaning coating comprises the following components, calculated by weight: 20 parts of silane-modified epoxy resin, 20 parts of modified titanium dioxide, 30 parts of DMF solution and 30 parts of BMI, and the protective coating comprises the following components, calculated by weight: 30 parts of bauxite, 20 parts of borax, 30 parts of glass powder and 20 parts of titanium dioxide.

[0011] As a preferred technical solution of the present invention, the adsorption coating comprises the following components, calculated by weight: 45 parts of photocatalyst activator and 55 parts of adsorption catalyst, the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 10 parts of composite fiber material, 20 parts of triethylenetetramine, 20 parts of calcium ferrite complex, 10 parts of surfactant, 10 parts of ethanol and 10 parts of adhesive, the self-cleaning coating comprises the following components, calculated by weight: 30 parts of silane-modified epoxy resin, 20 parts of modified titanium dioxide, 30 parts of DMF solution and 20 parts of BMI, and the protective coating comprises the following components, calculated by weight: 15 parts of bauxite, 35 parts of borax, 15 parts of glass powder and 35 parts of titanium dioxide.

[0012] As a preferred technical solution of the present invention, the adsorption coating comprises the following components, calculated by weight: 50 parts of photocatalyst activator and 50 parts of adsorption catalyst, the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 120 parts of composite fiber material, 10 parts of triethylenetetramine, 15 parts of calcium ferrite complex, 20 parts of surfactant, 10 parts of ethanol and 5 parts of adhesive, the self-cleaning coating comprises the following components, calculated by weight: 20 parts of silane-modified epoxy resin, 30 parts of modified titanium dioxide, 20 parts of DMF solution and 30 parts of BMI, and the protective coating comprises the following components, calculated by weight: 20 parts of bauxite, 20 parts of borax, 40 parts of glass powder and 20 parts of titanium dioxide.

[0013] As a preferred technical solution of the present invention, the adsorption coating comprises the following components, calculated by weight: 55 parts of photocatalyst activator and 45 parts of adsorption catalyst, the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 15 parts of composite fiber material, 15 parts of triethylenetetramine, 15 parts of calcium ferrite complex, 10 parts of surfactant, 20 parts of ethanol and 5 parts of adhesive, the self-cleaning coating comprises the following components, calculated by weight: 25 parts of silane-modified epoxy resin, 25 parts of modified titanium dioxide, 25 parts of DMF solution and 25 parts of BMI, and the protective coating comprises the following components, calculated by weight: 20 parts of bauxite, 30 parts of borax, 25 parts of glass powder and 25 parts of titanium dioxide.

[0014] As a preferred technical solution of the present invention, the photocatalyst activator includes titanium dioxide and a perovskite-type composite photocatalyst, and the adsorption catalyst is specifically a composite adsorption material with a microporous structure.

[0015] The present invention provides a preparation process of a filter coating material for a medical-grade air purifier, comprising the following steps:

[0016] Step 1: Preparation of filter coating material: Mix the adsorption coating and the purification coating and press them into a plate-like object with pores;

[0017] Step 2: Preparation of protective coating material: mixing the self-cleaning coating and the protective coating, and pressing them into a plate-like object with pores;

[0018] Step 3: bonding: bonding the prepared filtering coating material and protective coating material together to obtain a product;

[0019] Step 4: Material coating: Coat the product prepared in step 3 on the filter surface.

[0020] As a preferred technical solution of the present invention, the specific process of preparing the adsorption coating in step 1 is: 30-60 parts of the photocatalyst activator and 30-60 parts of the adsorption catalyst are mixed in a reactor, and the specific process of preparing the purification coating in step 1 is: 5-15 parts of diatomaceous earth, 5-15 parts of nano-silicon dioxide, 5-15 parts of calcium carbonate, 5-15 parts of zinc oxide, 10-20 parts of composite fiber material, 10-20 parts of triethylenetetramine, 10-20 parts of calcium ferrite complex, 10-20 parts of surfactant are added. The specific process of preparing the cleaning coating in the step 2 is as follows: 20 parts to 40 parts of silane-modified epoxy resin, 20 parts to 40 parts of modified titanium dioxide, 20 parts to 40 parts of DMF solution and 20 parts to 40 parts of BMI are mixed in a reactor; the specific process of preparing the protective coating in the step 2 is as follows: 15 parts to 50 parts of bauxite, 20 parts to 35 parts of borax, 15 parts to 50 parts of glass powder and 20 parts to 35 parts of titanium dioxide are mixed in a reactor.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] 1. By setting a self-cleaning coating, the smoothness of the filter surface is increased, and the adhesion and adhesion of dirt and grease impurities on the filter are reduced, thereby reducing the blockage and resistance of the filter and reducing the labor of people cleaning the filter;

[0023] 2. By setting a protective coating, a protective film is formed on the outside of the filter to prevent corrosion, wear and oxidation on the filter surface, thereby extending the service life of the filter;

[0024] 3. By setting the adsorption coating and purification coating, the filter substrate has strong adhesion, high purification efficiency, low energy consumption, extended service life, no secondary pollution and good photocatalytic performance under visible light. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a flow chart of the present invention. DETAILED DESCRIPTION

[0026] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0027] Embodiment 1:

[0028] See also Figure 1The present invention provides a medical-grade air purifier filter coating material, including a filter coating material, the filter coating material including an adsorption coating, a purification coating, a self-cleaning coating and a protective coating, the adsorption coating including the following components, by weight: 30-60 parts of a photocatalyst activator and 30-60 parts of an adsorption catalyst, the purification coating including the following components, by weight: 5-15 parts of diatomaceous earth, 5-15 parts of nano silicon dioxide, 5-15 parts of calcium carbonate, 5-15 parts of zinc oxide, 10-20 parts of a composite fiber material, and triethylenetetramine The self-cleaning coating comprises the following components, by weight: 20-40 parts of silane-modified epoxy resin, 20-40 parts of modified titanium dioxide, 20-40 parts of DMF solution and 20-40 parts of BMI; the protective coating comprises the following components, by weight: 15-50 parts of bauxite, 20-35 parts of borax, 15-50 parts of glass powder and 20-35 parts of titanium dioxide.

[0029] The photocatalyst active agent includes titanium dioxide and a perovskite-type composite photocatalyst, and the adsorption catalyst is specifically a composite adsorption material with a microporous structure.

[0030] The present invention provides a preparation process of a filter coating material for a medical-grade air purifier, comprising the following steps:

[0031] Step 1: Preparation of filter coating material: Mix the adsorption coating and the purification coating and press them into a plate-like object with pores;

[0032] Step 2: Preparation of protective coating material: mixing the self-cleaning coating and the protective coating, and pressing them into a plate-like object with pores;

[0033] Step 3: bonding: bonding the prepared filtering coating material and protective coating material together to obtain a product;

[0034] Step 4: Material coating: Coat the product prepared in step 3 on the filter surface.

[0035] The specific process of preparing the adsorption coating in step 1 is as follows: 30-60 parts of photocatalyst activator and 30-60 parts of adsorption catalyst are mixed in a reactor; the specific process of preparing the purification coating in step 1 is as follows: 5-15 parts of diatomaceous earth, 5-15 parts of nano-silicon dioxide, 5-15 parts of calcium carbonate, 5-15 parts of zinc oxide, 10-20 parts of composite fiber material, 10-20 parts of triethylenetetramine, 10-20 parts of calcium ferrite complex, 10-20 parts of surfactant, 10-20 parts of ethanol are added; The specific process for preparing the cleaning coating in step 2 is: mixing 20 parts to 40 parts of silane-modified epoxy resin, 20 parts to 40 parts of modified titanium dioxide, 20 parts to 40 parts of DMF solution and 20 parts to 40 parts of BMI in a reactor; the specific process for preparing the protective coating in step 2 is: mixing 15 parts to 50 parts of bauxite, 20 parts to 35 parts of borax, 15 parts to 50 parts of glass powder and 20 parts to 35 parts of titanium dioxide in a reactor.

[0036] Embodiment 2:

[0037] See also Figure 1 The present invention provides a medical-grade air purifier filter coating material, including a filter coating material, the filter coating material including an adsorption coating, a purification coating, a self-cleaning coating and a protective coating, the adsorption coating including the following components, by weight: 40 parts of a photocatalyst activator and 60 parts of an adsorption catalyst, the purification coating including the following components, by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 20 parts of a composite fiber material, 10 parts of triethylenetetramine, 10 parts of a calcium ferrite complex, 20 parts of a surfactant, 10 parts of ethanol and 10 parts of an adhesive, the self-cleaning coating including the following components, by weight: 20 parts of a silane-modified epoxy resin, 20 parts of a modified titanium dioxide, 30 parts of a DMF solution and 30 parts of BMI, and the protective coating including the following components, by weight: 30 parts of bauxite, 20 parts of borax, 30 parts of glass powder and 20 parts of titanium dioxide.

[0038] The photocatalyst active agent includes titanium dioxide and a perovskite-type composite photocatalyst, and the adsorption catalyst is specifically a composite adsorption material with a microporous structure.

[0039] The present invention provides a preparation process of a filter coating material for a medical-grade air purifier, comprising the following steps:

[0040] Step 1: Preparation of filter coating material: Mix the adsorption coating and the purification coating and press them into a plate-like object with pores;

[0041] Step 2: Preparation of protective coating material: mixing the self-cleaning coating and the protective coating, and pressing them into a plate-like object with pores;

[0042] Step 3: bonding: bonding the prepared filtering coating material and protective coating material together to obtain a product;

[0043] Step 4: Material coating: Coat the product prepared in step 3 on the filter surface.

[0044] The specific process for preparing the adsorption coating in step one is: mixing 40 parts of photocatalyst activator and 60 parts of adsorption catalyst in a reactor, the specific process for preparing the purification coating in step one is: mixing 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 20 parts of composite fiber material, 10 parts of triethylenetetramine, 10 parts of calcium ferrite complex, 20 parts of surfactant, 10 parts of ethanol and 10 parts of adhesive in a reactor, the specific process for preparing the cleaning coating in step two is: mixing 20 parts of silane-modified epoxy resin, 20 parts of modified titanium dioxide, 30 parts of DMF solution and 30 parts of BMI in a reactor, and the specific process for preparing the protective coating in step two is: mixing 30 parts of bauxite, 20 parts of borax, 30 parts of glass powder and 20 parts of titanium dioxide in a reactor.

[0045] Embodiment 3:

[0046] See also Figure 1 The present invention provides a medical-grade air purifier filter coating material, including a filter coating material, the filter coating material including an adsorption coating, a purification coating, a self-cleaning coating and a protective coating, the adsorption coating including the following components, by weight: 45 parts of a photocatalyst activator and 55 parts of an adsorption catalyst, the purification coating including the following components, by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 10 parts of a composite fiber material, 20 parts of triethylenetetramine, 20 parts of a calcium ferrite complex, 10 parts of a surfactant, 10 parts of ethanol and 10 parts of an adhesive, the self-cleaning coating including the following components, by weight: 30 parts of a silane-modified epoxy resin, 20 parts of a modified titanium dioxide, 30 parts of a DMF solution and 20 parts of BMI, and the protective coating including the following components, by weight: 15 parts of bauxite, 35 parts of borax, 15 parts of glass powder and 35 parts of titanium dioxide.

[0047] The photocatalyst active agent includes titanium dioxide and a perovskite-type composite photocatalyst, and the adsorption catalyst is specifically a composite adsorption material with a microporous structure.

[0048] The present invention provides a preparation process of a filter coating material for a medical-grade air purifier, comprising the following steps:

[0049] Step 1: Preparation of filter coating material: Mix the adsorption coating and the purification coating and press them into a plate-like object with pores;

[0050] Step 2: Preparation of protective coating material: mixing the self-cleaning coating and the protective coating, and pressing them into a plate-like object with pores;

[0051] Step 3: bonding: bonding the prepared filtering coating material and protective coating material together to obtain a product;

[0052] Step 4: Material coating: Coat the product prepared in step 3 on the filter surface.

[0053] The specific process for preparing the adsorption coating in step one is: mixing 45 parts of photocatalyst activator and 55 parts of adsorption catalyst in a reactor, the specific process for preparing the purification coating in step one is: mixing 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 10 parts of composite fiber material, 20 parts of triethylenetetramine, 20 parts of calcium ferrite complex, 10 parts of surfactant, 10 parts of ethanol and 10 parts of adhesive in a reactor, the specific process for preparing the cleaning coating in step two is: mixing 30 parts of silane-modified epoxy resin, 20 parts of modified titanium dioxide, 30 parts of DMF solution and 20 parts of BMI in a reactor, and the specific process for preparing the protective coating in step two is: mixing 15 parts of bauxite, 35 parts of borax, 15 parts of glass powder and 35 parts of titanium dioxide in a reactor.

[0054] Embodiment 4:

[0055] See also Figure 1 The present invention provides a medical-grade air purifier filter coating material, including a filter coating material, the filter coating material including an adsorption coating, a purification coating, a self-cleaning coating and a protective coating, the adsorption coating including the following components, by weight: 50 parts of a photocatalyst activator and 50 parts of an adsorption catalyst, the purification coating including the following components, by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 120 parts of a composite fiber material, 10 parts of triethylenetetramine, 15 parts of a calcium ferrite complex, 20 parts of a surfactant, 10 parts of ethanol and 5 parts of an adhesive, the self-cleaning coating including the following components, by weight: 20 parts of a silane-modified epoxy resin, 30 parts of a modified titanium dioxide, 20 parts of a DMF solution and 30 parts of BMI, and the protective coating including the following components, by weight: 20 parts of bauxite, 20 parts of borax, 40 parts of glass powder and 20 parts of titanium dioxide.

[0056] The photocatalyst active agent includes titanium dioxide and a perovskite-type composite photocatalyst, and the adsorption catalyst is specifically a composite adsorption material with a microporous structure.

[0057] The present invention provides a preparation process of a filter coating material for a medical-grade air purifier, comprising the following steps:

[0058] Step 1: Preparation of filter coating material: Mix the adsorption coating and the purification coating and press them into a plate-like object with pores;

[0059] Step 2: Preparation of protective coating material: mixing the self-cleaning coating and the protective coating, and pressing them into a plate-like object with pores;

[0060] Step 3: bonding: bonding the prepared filtering coating material and protective coating material together to obtain a product;

[0061] Step 4: Material coating: Coat the product prepared in step 3 on the filter surface.

[0062] The specific process for preparing the adsorption coating in step one is: mixing 50 parts of photocatalyst activator and 50 parts of adsorption catalyst in a reactor, the specific process for preparing the purification coating in step one is: mixing 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 120 parts of composite fiber material, 10 parts of triethylenetetramine, 15 parts of calcium ferrite complex, 20 parts of surfactant, 10 parts of ethanol and 5 parts of adhesive in a reactor, the specific process for preparing the cleaning coating in step two is: mixing 20 parts of silane-modified epoxy resin, 30 parts of modified titanium dioxide, 20 parts of DMF solution and 30 parts of BMI in a reactor, and the specific process for preparing the protective coating in step two is: mixing 20 parts of bauxite, 20 parts of borax, 40 parts of glass powder and 20 parts of titanium dioxide in a reactor.

[0063] Embodiment 5:

[0064] See also Figure 1 The present invention provides a medical-grade air purifier filter coating material, including a filter coating material, the filter coating material including an adsorption coating, a purification coating, a self-cleaning coating and a protective coating, the adsorption coating including the following components, by weight: 55 parts of a photocatalyst activator and 45 parts of an adsorption catalyst, the purification coating including the following components, by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 15 parts of a composite fiber material, 15 parts of triethylenetetramine, 15 parts of a calcium ferrite complex, 10 parts of a surfactant, 20 parts of ethanol and 5 parts of an adhesive, the self-cleaning coating including the following components, by weight: 25 parts of a silane-modified epoxy resin, 25 parts of a modified titanium dioxide, 25 parts of a DMF solution and 25 parts of BMI, the protective coating including the following components, by weight: 20 parts of bauxite, 30 parts of borax, 25 parts of glass powder and 25 parts of titanium dioxide.

[0065] The photocatalyst active agent includes titanium dioxide and a perovskite-type composite photocatalyst, and the adsorption catalyst is specifically a composite adsorption material with a microporous structure.

[0066] The present invention provides a preparation process of a filter coating material for a medical-grade air purifier, comprising the following steps:

[0067] Step 1: Preparation of filter coating material: Mix the adsorption coating and the purification coating and press them into a plate-like object with pores;

[0068] Step 2: Preparation of protective coating material: mixing the self-cleaning coating and the protective coating, and pressing them into a plate-like object with pores;

[0069] Step 3: bonding: bonding the prepared filtering coating material and protective coating material together to obtain a product;

[0070] Step 4: Material coating: Coat the product prepared in step 3 on the filter surface.

[0071] The specific process for preparing the adsorption coating in step one is: mixing 55 parts of photocatalyst activator and 45 parts of adsorption catalyst in a reactor, the specific process for preparing the purification coating in step one is: mixing 5 parts of diatomaceous earth, 5 parts of nano-silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 15 parts of composite fiber material, 15 parts of triethylenetetramine, 15 parts of calcium ferrite complex, 10 parts of surfactant, 20 parts of ethanol and 5 parts of adhesive in a reactor, the specific process for preparing the cleaning coating in step two is: mixing 25 parts of silane-modified epoxy resin, 25 parts of modified titanium dioxide, 25 parts of DMF solution and 25 parts of BMI in a reactor, and the specific process for preparing the protective coating in step two is: mixing 20 parts of bauxite, 30 parts of borax, 25 parts of glass powder and 25 parts of titanium dioxide in a reactor.

[0072] In the present invention, the adsorption coating and the purification coating are mixed and pressed into a plate-like object with pores; the specific process of preparing the adsorption coating is: 30-60 parts of a photocatalyst activator and 30-60 parts of an adsorption catalyst are mixed in a reaction kettle; the specific process of preparing the purification coating is: 5-15 parts of diatomaceous earth, 5-15 parts of nano silicon dioxide, 5-15 parts of calcium carbonate, 5-15 parts of zinc oxide, 10-20 parts of a composite fiber material, 10-20 parts of triethylenetetramine, 10-20 parts of a calcium ferrite complex, 10-20 parts of a surfactant, 10-20 parts of ethanol and 5-10 parts of a binder are mixed in a reaction kettle; The self-cleaning coating and the protective coating are mixed in a kettle, and pressed into a plate-like object with pores; the specific process for preparing the cleaning coating is: 20-40 parts of silane-modified epoxy resin, 20-40 parts of modified titanium dioxide, 20-40 parts of DMF solution and 20-40 parts of BMI are mixed in a reactor; the specific process for preparing the protective coating is: 15-50 parts of bauxite, 20-35 parts of borax, 15-50 parts of glass powder and 20-35 parts of titanium dioxide are mixed in a reactor, and the prepared filtration coating material and protective coating material are bonded together to obtain a product; and the prepared product is coated on the surface of the filter.

[0073] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A filter coating material for a medical-grade air purifier, comprising a filter coating material, characterized in that: The filter screen coating material includes an adsorption coating, a purification coating, a self-cleaning coating and a protective coating. The adsorption coating includes the following components, calculated by weight: 30-60 parts of a photocatalyst activator and 30-60 parts of an adsorption catalyst. The purification coating includes the following components, calculated by weight: 5-15 parts of diatomaceous earth, 5-15 parts of nano silicon dioxide, 5-15 parts of calcium carbonate, 5-15 parts of zinc oxide, 10-20 parts of a composite fiber material, 10-20 parts of triethylenetetramine, and 10-20 parts of a calcium ferrite complex. The self-cleaning coating comprises the following components, by weight: 20-40 parts of silane-modified epoxy resin, 20-40 parts of modified titanium dioxide, 20-40 parts of DMF solution and 20-40 parts of BMI; the protective coating comprises the following components, by weight: 15-50 parts of bauxite, 20-35 parts of borax, 15-50 parts of glass powder and 20-35 parts of titanium dioxide.

2. The medical grade air purifier filter coating material according to claim 1, characterized in that: The adsorption coating comprises the following components, calculated by weight: 40 parts of photocatalyst activator and 60 parts of adsorption catalyst; the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 20 parts of composite fiber material, 10 parts of triethylenetetramine, 10 parts of calcium ferrite complex, 20 parts of surfactant, 10 parts of ethanol and 10 parts of adhesive; the self-cleaning coating comprises the following components, calculated by weight: 20 parts of silane-modified epoxy resin, 20 parts of modified titanium dioxide, 30 parts of DMF solution and 30 parts of BMI; the protective coating comprises the following components, calculated by weight: 30 parts of bauxite, 20 parts of borax, 30 parts of glass powder and 20 parts of titanium dioxide.

3. The medical grade air purifier filter coating material according to claim 1, characterized in that: The adsorption coating comprises the following components, calculated by weight: 45 parts of photocatalyst activator and 55 parts of adsorption catalyst; the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 10 parts of composite fiber material, 20 parts of triethylenetetramine, 20 parts of calcium ferrite complex, 10 parts of surfactant, 10 parts of ethanol and 10 parts of adhesive; the self-cleaning coating comprises the following components, calculated by weight: 30 parts of silane-modified epoxy resin, 20 parts of modified titanium dioxide, 30 parts of DMF solution and 20 parts of BMI; the protective coating comprises the following components, calculated by weight: 15 parts of bauxite, 35 parts of borax, 15 parts of glass powder and 35 parts of titanium dioxide.

4. The medical grade air purifier filter coating material according to claim 1, characterized in that: The adsorption coating comprises the following components, calculated by weight: 50 parts of photocatalyst activator and 50 parts of adsorption catalyst; the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 120 parts of composite fiber material, 10 parts of triethylenetetramine, 15 parts of calcium ferrite complex, 20 parts of surfactant, 10 parts of ethanol and 5 parts of adhesive; the self-cleaning coating comprises the following components, calculated by weight: 20 parts of silane-modified epoxy resin, 30 parts of modified titanium dioxide, 20 parts of DMF solution and 30 parts of BMI; the protective coating comprises the following components, calculated by weight: 20 parts of bauxite, 20 parts of borax, 40 parts of glass powder and 20 parts of titanium dioxide.

5. The medical grade air purifier filter coating material according to claim 1, characterized in that: The adsorption coating comprises the following components, calculated by weight: 55 parts of photocatalyst activator and 45 parts of adsorption catalyst; the purification coating comprises the following components, calculated by weight: 5 parts of diatomaceous earth, 5 parts of nano silicon dioxide, 5 parts of calcium carbonate, 5 parts of zinc oxide, 15 parts of composite fiber material, 15 parts of triethylenetetramine, 15 parts of calcium ferrite complex, 10 parts of surfactant, 20 parts of ethanol and 5 parts of adhesive; the self-cleaning coating comprises the following components, calculated by weight: 25 parts of silane-modified epoxy resin, 25 parts of modified titanium dioxide, 25 parts of DMF solution and 25 parts of BMI; the protective coating comprises the following components, calculated by weight: 20 parts of bauxite, 30 parts of borax, 25 parts of glass powder and 25 parts of titanium dioxide.

6. The medical grade air purifier filter coating material according to claim 1, characterized in that: The photocatalyst activator comprises titanium dioxide and a perovskite-type composite photocatalyst, and the adsorption catalyst is specifically a composite adsorption material with a microporous structure.

7. The preparation process of a medical grade air purifier filter coating material according to claims 1-6, characterized in that: The following steps are involved: Step 1: Preparation of filter coating material: Mix the adsorption coating and the purification coating and press them into a plate-like object with pores; Step 2: Preparation of protective coating material: mixing the self-cleaning coating and the protective coating, and pressing them into a plate-like object with pores; Step 3: bonding: bonding the prepared filtering coating material and protective coating material together to obtain a product; Step 4: Material coating: Coat the product prepared in step 3 on the filter surface.

8. The preparation process of a medical grade air purifier filter coating material according to claim 7, characterized in that: The specific process of preparing the adsorption coating in step 1 is: 30-60 parts of photocatalyst activator and 30-60 parts of adsorption catalyst are mixed in a reaction kettle; the specific process of preparing the purification coating in step 1 is: 5-15 parts of diatomaceous earth, 5-15 parts of nano silicon dioxide, 5-15 parts of calcium carbonate, 5-15 parts of zinc oxide, 10-20 parts of composite fiber material, 10-20 parts of triethylenetetramine, 10-20 parts of calcium ferrite complex, 10-20 parts of surfactant, 10-20 parts of ethanol are added. The specific process for preparing the cleaning coating in the step 2 is: mixing 20 parts to 40 parts of silane-modified epoxy resin, 20 parts to 40 parts of modified titanium dioxide, 20 parts to 40 parts of DMF solution and 20 parts to 40 parts of BMI in a reactor; the specific process for preparing the protective coating in the step 2 is: mixing 15 parts to 50 parts of bauxite, 20 parts to 35 parts of borax, 15 parts to 50 parts of glass powder and 20 parts to 35 parts of titanium dioxide in a reactor.