Method and device for monitoring wafer warping in real time

By real-time monitoring of the heating power change rate and warpage change of the heating tray, and adjusting process conditions, the problem of wafer warpage in semiconductor chip production is solved, the stability and efficiency of the film deposition process are improved, and arc generation is avoided.

CN118773585APending Publication Date: 2024-10-15ACM RES (SHANGHAI) INC +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310387127.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

In the production process of semiconductor chips, the existing technology cannot monitor the warpage of the wafer in real time during the film deposition process, causing the wafer to detach from the heating tray when the film stress is too large, affecting the heating efficiency and film uniformity, and may cause arcing.

Method used

By real-time monitoring of the heating power change rate of each heating area on the heating tray and the wafer warpage change, it is determined whether the wafer is separated from the tray, and the process conditions are adjusted according to the mapping relationship to control the warpage within the target range.

Benefits of technology

It realizes real-time monitoring of wafer warpage during the film deposition process, avoiding the reduction in heating efficiency and poor film uniformity caused by warpage, avoiding the generation of arcs, and eliminating the need for additional measurement machines.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118773585A_ABST
    Figure CN118773585A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of semiconductor chip manufacturing, in particular to a method and device for monitoring wafer warping in real time. In the process of depositing a thin film on a wafer, the heating power change rate of each heating area on a heating tray is monitored in real time, the heating tray comprises at least two heating areas, each heating area is in a set constant-temperature control state, the wafer is arranged on the at least two heating areas, and the heating power change rate of each heating area is in a constant-temperature control state. The wafer is provided with a wafer area corresponding to each heating area; and judging whether the wafer area corresponding to the heating power change rate is separated from the heating tray or not according to the heating power change rate. In the thin film deposition process, the variation of the warping degree of the wafer is monitored in real time by monitoring the change condition of the heating power, and an additional measuring machine is not needed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor chip manufacturing, and in particular to a method and device for real-time monitoring of wafer warping. Background Art

[0002] In the production process of semiconductor chips, plasma enhanced chemical vapor deposition (PECVD) is often used to deposit various dielectric layers, metal layers, etc. The robotic arm places the wafer on a heating tray in the chamber, and the reaction gas enters the chamber through a shower head located directly above the heating tray. Under the action of radio frequency, plasma is formed, and the reaction ions migrate to the surface of the wafer to react, forming thin films such as silicide on the surface of the wafer.

[0003] During the thin film deposition process, due to the different thermal expansion coefficients of the newly formed thin film and the wafer substrate, stress is generated between the two, causing the wafer to warp.

[0004] When the film stress is large, especially when the film thickness is thick, the wafer will bend to a large extent and partially detach from the heating tray, the heating efficiency will be reduced, the film uniformity will deteriorate, and in severe cases, arcing may occur.

[0005] Currently, the industry mainly monitors film stress through measuring equipment before and after film formation to control it within a certain range, but it is not possible to monitor the deformation of the wafer during the film formation process in real time. Summary of the invention

[0006] In view of the above-mentioned problems, the object of the present invention is to provide a method and device for real-time monitoring of wafer warpage, so as to monitor the wafer warpage in real time during the film forming process.

[0007] To achieve the above object, the present invention provides the following technical solutions:

[0008] A method for real-time monitoring of wafer warpage comprises: in a process of depositing a thin film on the wafer, real-time monitoring of a heating power change rate ΔP / P0 of each heating area on a heating tray, wherein ΔP is a heating power change amount of the heating area, and P0 is a heating power of the heating area in an initial state, the heating tray comprises at least two heating areas, each heating area is in a set constant temperature control state, a wafer is arranged on the at least two heating areas, and the wafer has a wafer area corresponding to each of the heating areas; and judging whether the corresponding wafer area is out of the heating tray according to the heating power change rate ΔP / P0.

[0009] The present invention also provides a method for real-time monitoring of wafer warpage, comprising: in a process of depositing a thin film on the wafer, real-time monitoring of a change in wafer warpage ΔBOW;

[0010] If the wafer warpage change ΔBOW exceeds a preset threshold, the process conditions that need to be changed are determined based on the mapping relationship between the wafer warpage change ΔBOW and the process conditions, and the wafer is processed using the changed process conditions, so that the wafer warpage is controlled within the target warpage range.

[0011] The present invention also provides a device for real-time monitoring of wafer warpage, comprising: a memory configured to store at least one mapping relationship, wherein the mapping relationship is a mapping relationship between a wafer warpage change ΔBOW and a process condition; a monitor configured to monitor the wafer warpage change ΔBOW in real time; a controller configured to receive the wafer warpage change ΔBOW, and if the wafer warpage change ΔBOW exceeds a preset threshold, determine the process condition that needs to be changed based on the mapping relationship between the wafer warpage change ΔBOW and the process condition; an operator configured to receive the changed process condition and use the changed process condition to process the wafer.

[0012] Compared with the prior art, the present invention has the following beneficial effects:

[0013] By using this invention, the warpage of the wafer can be monitored in real time during the process of depositing a thin film, that is, the change in the warpage of the wafer ΔBOW can be monitored in real time without the need for an additional measuring machine. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0015] Figure 1 A flow chart of a method for real-time monitoring of wafer warpage provided in Embodiment 1 of the present invention.

[0016] Figure 2 Schematic diagram of the state of the heating tray heating the wafer provided in the first embodiment of the present invention Figure 1 .

[0017] Figure 3 Schematic diagram of the state of the heating tray heating the wafer provided in the first embodiment of the present invention Figure 2 .

[0018] Figure 4 Schematic diagram of the state of the heating tray heating the wafer provided in the first embodiment of the present invention Figure 3 .

[0019] Figure 5This is a fitting curve diagram of the relationship between the change in heating power of the inner heating coil and the outer heating coil and the warpage in Example 1 of the present invention.

[0020] Figure 6 A flow chart of a method for real-time monitoring of wafer warpage provided in Embodiment 2 of the present invention.

[0021] Figure 7 Schematic diagram of a thin film deposition device provided in Embodiment 2 of the present invention.

[0022] Figure 8-Figure 13 This is a relationship diagram between film stress and process conditions provided in Example 2 of the present invention. DETAILED DESCRIPTION

[0023] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the following is a brief introduction to the drawings required for the description of the embodiments. Obviously, the drawings described below are only some examples or embodiments of the present application. For ordinary technicians in this field, the present application can also be applied to other similar scenarios based on these drawings without creative work. Unless it is obvious from the language environment or otherwise explained, the same reference numerals in the figures represent the same structure or operation.

[0024] As shown in this application and claims, unless the context clearly indicates an exception, the words "a", "an", "an" and / or "the" do not refer to the singular and may also include the plural. Generally speaking, the terms "include" and "comprise" only indicate the inclusion of the steps and elements that have been clearly identified, and these steps and elements do not constitute an exclusive list. The method or device may also include other steps or elements.

[0025] Unless otherwise specifically stated, the relative arrangement, numerical expressions and numerical values ​​of the parts and steps set forth in these embodiments do not limit the scope of the present application. At the same time, it should be understood that, for ease of description, the sizes of the various parts shown in the accompanying drawings are not drawn according to the actual proportional relationship. The technology, method and equipment known to those of ordinary skill in the relevant field may not be discussed in detail, but in appropriate cases, the technology, method and equipment should be considered as a part of the authorization specification. In all examples shown and discussed here, any specific value should be interpreted as being merely exemplary, rather than as a limitation. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters represent similar items in the following drawings, so that once a certain item is defined in an accompanying drawing, it does not need to be further discussed in subsequent drawings.

[0026] In the description of the present application, it should be understood that the directions or positional relationships indicated by directional words such as "front, back, up, down, left, right", "lateral, vertical, perpendicular, horizontal" and "top, bottom" are usually based on the directions or positional relationships shown in the drawings, and are only for the convenience of describing the present application and simplifying the description. Unless otherwise specified, these directional words do not indicate or imply that the device or element referred to must have a specific direction or be constructed and operated in a specific direction, and therefore cannot be understood as limiting the scope of protection of the present application; the directional words "inside and outside" refer to the inside and outside relative to the contours of each component itself.

[0027] For ease of description, spatially relative terms such as "above", "above", "on the upper surface of", "above", etc. may be used here to describe the spatial positional relationship between a device or feature and other devices or features as shown in the figure. It should be understood that spatially relative terms are intended to include different orientations of the device in use or operation in addition to the orientation described in the figure. For example, if the device in the accompanying drawings is inverted, the device described as "above other devices or structures" or "above other devices or structures" will be positioned as "below other devices or structures" or "below other devices or structures". Thus, the exemplary term "above" can include both "above" and "below". The device can also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatially relative descriptions used here are interpreted accordingly.

[0028] In addition, it should be noted that the use of words such as "first" and "second" to define components is only for the convenience of distinguishing the corresponding components. If not otherwise stated, the above words have no special meaning and cannot be understood as limiting the scope of protection of this application. In addition, although the terms used in this application are selected from well-known and commonly used terms, some terms mentioned in the specification of this application may be selected by the applicant at his or her discretion, and their detailed meanings are explained in the relevant parts of the description of this article. In addition, it is required to understand this application not only by the actual terms used, but also by the meaning implied by each term.

[0029] The technical solution of the present invention is further described below with reference to the accompanying drawings and through specific implementation methods.

[0030] Embodiment 1

[0031] See also Figure 1 This embodiment provides a method for real-time monitoring of wafer warpage, and the method of this embodiment includes the following steps:

[0032] Step S110: during the process of depositing a thin film on the wafer, monitoring in real time the heating power change rate ΔP / P0 of each heating area on the heating tray, wherein ΔP is the heating power change amount of the heating area, and P0 is the heating power of the heating area in the initial state, the heating tray comprises at least two heating areas, each heating area is in a set constant temperature control state, the wafer is arranged on the at least two heating areas, and the wafer has a wafer area corresponding to each heating area; and

[0033] Step S120: determining whether the corresponding wafer area is out of the heating tray according to the heating power change rate ΔP / P0.

[0034] The following combination Figures 2 to 5 The above steps S110 and S120 are described below. Figure 2 During the thin film deposition process, the wafer 2 is located on the heating tray 1, and the heating tray 1 heats the wafer 2. The heating tray 1 includes a central heating area 11 and an edge heating area 12, and the edge heating area 12 is arranged on the periphery of the central heating area 11. The heating tray 1 heats the wafer 2 in a dual-zone manner. The edge heating area 12 includes an external heating coil for heating the portion of the wafer located on the edge heating area 12, and the central heating area 11 includes an internal heating coil for heating the portion of the wafer located on the central heating area 11. The edge heating area 12 and the central heating area 11 are combined to heat the entire wafer 2. The internal heating coil and the external heating coil dynamically adjust the heating power so that each heating area of ​​the heating tray 1 is in a set constant temperature control state.

[0035] For example, if the temperature of the heating area is lower or higher than the set temperature, the heating power is increased or decreased through the relay.

[0036] During the film deposition process, when the wafer 2 does not warp, that is, Figure 2 As shown, the wafer 2 is flat as a whole, the central portion of the wafer 2 is in contact with the central heating area 11 , and the edge portion of the wafer 2 is in contact with the edge heating area 12 .

[0037] However, when the wafer 2 is warped, some parts of the wafer will be separated from the heating tray 1, that is, they will not be in contact with the heating tray 1. The method for real-time monitoring of wafer warping of this embodiment determines the warping state of the wafer based on the heating power change rate ΔP(C) / P0(C) of the central heating area 11 and the heating power change rate ΔP(E) / P0(E) of the edge heating area 12. Among them, ΔP(C) represents the heating power change corresponding to the central heating area, ΔP(E) represents the heating power change corresponding to the edge heating area, P0(C) is the heating power corresponding to the central heating area in the initial state, and P0(E) is the heating power corresponding to the edge heating area in the initial state.

[0038] See also Figure 3 If the contact between the edge of the wafer 2 and the edge heating area 12 of the heating tray 1 is reduced, in order to maintain the set temperature, the load of the external heating coil becomes lower, the heating power of the edge heating area 12 will become lower, and the heating power of the central heating area 11 will not change, |ΔP(C) / P0(C)|<|ΔP(E) / P0(E)|, and the wafer 2 will warp upward in a bowl shape.

[0039] See also Figure 4 If the central part of the wafer 2 is less in contact with the central heating area 11 of the heating tray 1, the load of the internal heating coil becomes lower, and the heating power of the central heating area 11 becomes lower, |ΔP(C) / P0(C)|>|ΔP(E) / P0(E)|, and the wafer 2 warps downward in an inverted bowl shape. It should be noted that the change range of the heating power of the heating coil varies with the degree of warping of the wafer 2.

[0040] In this application, the BOW value is used to represent the warpage of the wafer 2. The warpage state of the wafer 2 can be distinguished by the positive or negative value of the wafer warpage BOW. Figure 3 and Figure 4 As shown, assuming that the upper surface of wafer 2 is the front side and the lower surface is the back side, the warping state of wafer 2 includes: the edge of wafer 2 is bent toward its back side and the middle is convex, that is, wafer 2 is warped downward, and the wafer warpage BOW is defined as negative, such as Figure 4 As shown; or the edge of the wafer 2 is bent toward its front side and concave in the middle, that is, the wafer 2 is warped upward, and the wafer warpage BOW is defined as positive, such as Figure 3 shown.

[0041] Exemplarily, the heating tray 1 is not limited to including two heating areas, and the heating tray 1 may include multiple heating areas, each heating area is used to heat the wafer 2 .

[0042] According to step S110 and step S120, the method disclosed in the present application monitors the heating power change rate ΔP / P0 of each heating area in real time, and judges whether the portion of the wafer 2 corresponding to the heating area is separated from the heating tray 1 according to the heating power change rate ΔP / P0. For example, judging according to the magnitude of the heating power change rate ΔP / P0, when the heating power change rate ΔP / P0 is less than a certain value, it indicates that the portion of the wafer is separated from the heating tray 1.

[0043] In some embodiments, if ΔP / P0 of a certain heating area is less than 0, it means that the heating power of the heating area has changed, which indicates that the wafer portion corresponding to the heating area has separated from the heating tray 1 .

[0044] In the embodiments disclosed in the present application, the warping state of the wafer 2 is not limited to the above two states. Exemplarily, the overall warping state of the wafer 2 is determined according to the heating power change rate ΔP / P0 of all heating areas. The warping state of the wafer 2 may be saddle-shaped or other special shapes.

[0045] Further research found that there is a corresponding relationship between the heating power change rate ΔP / P0 in the heating area and the wafer warpage change ΔBOW. The wafer warpage change ΔBOW is calculated by the corresponding relationship ΔP(C) / P0(C)=f1'(ΔBOW), ΔP(E) / P0(E)=f2'(ΔBOW), where f1' represents the relationship between ΔP(C) / P0(C) and ΔBOW, and f2' represents the relationship between ΔP(E) / P0(E) and ΔBOW. f1' and f2' can be a function, such as a linear function, a quadratic function, etc., and this application does not impose any restrictions on this. If ΔBOW exceeds a preset threshold, a reminder signal is triggered to the controller. After receiving the reminder signal, the controller can adjust the wafer warpage.

[0046] Exemplarily, the wafer warpage variation ΔBOW is the difference between the current wafer warpage and the initial warpage of the wafer 2. The heating power variation ΔP is the difference between the heating power of the current heating area and the heating power of the heating area in the initial state.

[0047] The above correspondence is established based on experimental acquisition. The experiment may include the following steps:

[0048] Taking the heating tray 1 including the central heating area 11 and the edge heating area 12 as an example, the heating tray 1 and the wafer 2 are arranged in the chamber, and the wafer 2 without thin film deposition is placed on the heating tray 1. After the temperature of the wafer 2 is stabilized to the target process temperature and the chamber is stabilized to the target process temperature, target pressure, target airflow and other conditions, the average heating power of the inner heating coil and the outer heating coil of the heating tray 1 within a certain period of time is collected: P0'(C) and P0'(E). At this time, the wafer 2 is in a straight state, and its wafer warpage BOW0 value is 0, wherein P0'(C) may be the heating power corresponding to the central heating area in the initial state, and P0'(E) may be the heating power corresponding to the edge heating area in the initial state;

[0049] A silicon nitride film of known thickness is deposited on wafer 2. At this time, wafer 2 is bent upward (or downward). At this time, the wafer warpage BOW1 is known. After wafer 2 is stabilized to the target process temperature, target pressure, target airflow and other conditions, the average heating power of the inner heating coil and the outer heating coil of the heating tray 1 within a certain period of time is collected: P1(C) and P1(E);

[0050] Then, a second layer of the same silicon nitride film is deposited on wafer 2. At this time, the wafer warpage BOW2 is known, and the average heating power of the inner heating coil and the outer heating coil of the heating tray 1 within a certain period of time is collected: P2(C) and P2(E);

[0051] By analogy, we can obtain the BOW of wafer 2 after depositing n known film layers. n It is known that the average heating power P of the inner heating coil and the outer heating coil of the heating tray 1 within a certain period of time is collected. n (C) and P n (E).

[0052] See also Figure 5 After fitting, the relationship between the heating power of the inner and outer heating coils of the heating tray 1 and the change in the BOW value of the wafer warpage can be obtained: P(C) = f1(BOW) and P(E) = f2(BOW). Among them, f1 represents the relationship between P(C) and BOW, f2 represents the relationship between P(E) and BOW, f1 and f2 can be a function, such as a linear function, a quadratic function, etc., and this application does not limit this. It should be noted that f1' is different from f1, and f2' is different from f2.

[0053] In the process of thin film deposition, the heating power of heating tray 1 is not only affected by the change in heat transfer caused by the warping of wafer 2, but also by the thermal effects of plasma field, chemical reaction, flow field and thermal field on wafer 2 during PECVD process deposition, which will cause the heating power of heating tray 1 to change. After the thermal effects are in a stable state, the thermal effects brought by plasma field, chemical reaction, flow field and thermal field tend to be constant. At this time, the change in heating power of heating tray 1 is mainly affected by the change in BOW value of wafer warpage. Taking thermal effects into account, the relationship between the heating power of the internal and external heating coils of heating tray 1 and the change in BOW value of wafer warpage is expressed as:

[0054] P(C)=f1(BOW)+C1 and P(E)=f2(BOW)+C2, where C1 and C2 are the heating power constants of the influence of plasma field, chemical reaction, flow field and thermal field on the central heating area 11 and the edge heating area 12 respectively.

[0055] It should be noted that the wafer film deposition process of the present method includes a PECVD process deposition process. During the process, each time a thin film is deposited, the plasma field, chemical reaction, flow field, and thermal field act on the wafer 2, which will bring about thermal effects. The heat release during the thin film deposition process is divided into three stages, first the first deposition fluctuation stage, then the deposition film stability stage, and finally the second deposition fluctuation stage. The thermal effect in a stable state here refers to the deposition film stability stage. According to these embodiments, when it is determined that the thin film deposition reaction is in the deposition film stability stage, step S110 of real-time monitoring of the heating power change rate ΔP / P0 of each heating area on the heating tray 1 is performed.

[0056] In some embodiments, the wafer deposition film process of the present method includes a CVD process deposition process, in which a thin film is deposited once, and the chemical reaction, flow field, and thermal field will cause thermal effects when acting on the wafer 2. After the thin film deposition reaction is stable, the thermal effects caused by the chemical reaction, flow field, and thermal field tend to be constant. At this time, the change in the heating power of the heating tray 1 is mainly affected by the change in the BOW value of the wafer warpage. According to these embodiments, when it is determined that the thin film deposition reaction is in the stable stage of depositing the thin film, the step of real-time monitoring the heating power change rate ΔP / P0 of each heating area on the heating tray 1 is performed. P(C)=f1(BOW)+C3 and P(E)=f2(BOW)+C4, where C3 and C4 are the heating power constants of the effects of chemical reactions, flow fields, and thermal fields on the central heating area 11 and the edge heating area 12, respectively.

[0057] During the CVD deposition process, the heat release during the thin film deposition process is divided into three stages, first the first deposition fluctuation stage, then the deposition film stability stage, and finally the second deposition fluctuation stage. Here, the thermal influence is in a stable state refers to the deposition film stability stage.

[0058] To obtain the change in heating power, the current heating power P is subtracted from the initial heating power P0, so that the constant terms C1 to C4 in the above formula are eliminated, thereby eliminating the thermal effects of plasma fields, chemical reactions, flow fields, thermal fields, etc.

[0059] Exemplarily, ΔP(C)=(f1(BOW)+C1)-(f1(BOW0)+C1)=f1(BOW)-f1(BOW0), where BOW0 is the initial warpage of the wafer 2 .

[0060] Since ΔP(C) / P0(C)=f1'(ΔBOW),

[0061] f1'(ΔBOW)=(f1(BOW)-f1(BOW0)) / P0(C) is an example of the relationship between f1 and f1'.

[0062] During the film deposition process, starting from the stable stage of film deposition, the heating power P(E) of the central heating area and the heating power P(C) of the edge heating area are read every x seconds, so as to monitor ΔP(C) / P0(C) and ΔP(E) / P0(E) in real time, and obtain the corresponding relationship ΔP(C) / P0(C)=f1'(ΔBOW), ΔP(E) / P0(E)=f2'(ΔBOW), and calculate the change of wafer warpage ΔBOW by ΔP(C) and ΔP(E). If ΔBOW exceeds the preset threshold, the reminder signal is triggered to the controller. Among them, f1' represents the relationship between ΔP(C) / P0(C) and ΔBOW; f2' represents the relationship between ΔP(E) / P0(E) and ΔBOW.

[0063] In summary, the method for monitoring wafer warpage does not require the addition of an additional measuring machine, and directly uses the changes in the heating power of the inner heating coil and the outer heating coil of the heating tray 1 to calculate the wafer warpage change ΔBOW in real time.

[0064] In some embodiments, when the wafer warpage change ΔBOW exceeds a preset threshold, a reminder signal is triggered to the controller. The method of the present application also determines the process conditions that need to be changed based on the mapping relationship between the wafer warpage change ΔBOW and the process conditions, and processes the wafer according to the changed process conditions, so that the wafer warpage is controlled within the target warpage range.

[0065] Embodiment 2

[0066] This embodiment provides a method for real-time monitoring of the warpage of the wafer 2. Figure 6 As shown, the method comprises the following steps:

[0067] Step S210: During the process of depositing a thin film on the wafer, real-time monitoring of the change in wafer warpage ΔBOW;

[0068] Step S220: If the wafer warpage change ΔBOW exceeds a preset threshold, the process conditions that need to be changed are determined based on a mapping relationship between the wafer warpage change ΔBOW and the process conditions, and the wafer is processed using the changed process conditions, so that the wafer warpage is controlled within a target warpage range.

[0069] When the warpage of the wafer 2 is within the target warpage range, the overall stress distribution of the wafer 2 is relatively uniform, and the wafer 2 is relatively flat, which can ensure the smooth progress of subsequent semiconductor manufacturing processes. The warpage of the wafer 2 is represented by the BOW value.

[0070] The following uses a thin film deposition device as an example to schematically illustrate the method for adjusting the warpage of the wafer 2 provided in the present application.

[0071] See also Figure 7 The thin film deposition device includes: a chamber for thin film deposition; a gas supply assembly 3 for supplying process gas to the inside of the chamber; a heating tray 1, arranged below the gas supply assembly 3, for carrying and heating a wafer 2; and a radio frequency source for providing radio frequency power to excite the process gas inside the chamber to dissociate into plasma and form a plasma field 4, and the plasma performs thin film deposition on the wafer 2. The present application does not limit the location of the gas supply assembly 3. In some embodiments, the gas supply assembly 3 can be arranged at the top wall inside the chamber.

[0072] In step S220, the mapping relationship between the wafer warpage variation ΔBOW and the process conditions includes a first corresponding relationship and a second corresponding relationship, wherein the first corresponding relationship is the relationship between the wafer warpage variation ΔBOW and the film stress.

[0073] Exemplarily, the wafer warpage variation ΔBOW is positively correlated with the absolute value of the film stress, that is, ΔBOW increases with the increase of the film stress.

[0074] The second corresponding relationship is the relationship between film stress (Stress) and process conditions.

[0075] For example, when a thin film is deposited on wafer 2, the film stress can be divided into tensile stress and compressive stress. When wafer 2 warps upward, the corresponding film stress is tensile stress; when wafer 2 warps downward, the corresponding film stress is compressive stress.

[0076] Exemplarily, the wafer 2 is warped downward, and the wafer warpage BOW is defined as a negative value; the wafer 2 is warped upward, and the wafer warpage BOW is defined as a positive value.

[0077] The process conditions in step S220 include but are not limited to any one or more combinations of gas flow rate, RF power, chamber pressure, gas composition ratio, film deposition time, terminal matching parameters, and the distance between the gas supply assembly 3 and the wafer 2.

[0078] Exemplarily, the terminal matching parameters include but are not limited to adjustable capacitors (C), frequency matchers, etc. The potential of the heating tray 1 is changed by the adjustable capacitor (C) to adjust the potential difference between the gas supply assembly 3 and the heating tray 1, thereby adjusting the distribution and energy of the plasma field 4 in the chamber, thereby changing the impact force of the plasma on the wafer 2, and when the plasma deposits a thin film on the wafer 2, the film stress changes.

[0079] The frequency matcher is mounted at the rear end of the radio frequency source, and the frequency matcher is adjusted to match the transmitting power source of the radio frequency source with the frequency of the chamber. It should be noted that the interior of the above chamber is a vacuum environment.

[0080] Exemplarily, the film stress is positively correlated with the film deposition time, that is, the longer the film deposition time is and the thicker the film layer is, the greater the corresponding film stress is.

[0081] Different film qualities (silicon nitride / silicon oxide / a-Si / carbon, etc.), different processes, and different composition ratios (recipes) have different response directions and sensitivities to process conditions.

[0082] For example, in the second corresponding relationship, the film stress may change with the change of the process conditions. The relationship between the film stress and the process conditions may be a linear relationship. Of course, the relationship between the film stress and the process conditions may also be a nonlinear relationship, which is specifically related to the influence of the process conditions on the film stress.

[0083] Taking silicon nitride film as an example, the silicon nitride film is made by filling the chamber with silane (SiH4), ammonia (NH3), and nitrogen (N2) at a certain ratio and flow rate, maintaining the set pressure and temperature, and forming plasma (Plasma) through radio frequency (RF) to form a film. Adjust the process conditions to conduct experiments and monitor the stress (Stress) and refractive index (RI) of the film in real time. Stress (Stress) and refractive index (RI) are both properties of the film. When depositing a certain film layer, the purpose of adjusting the process conditions is to change the stress (Stress), but the refractive index (RI) of the film layer remains unchanged. For details, please refer to Figure 8-Figure 13 . The unit of stress is MPa.

[0084] like Figure 8 As shown in the figure, there is a positive correlation between film stress (Stress) and SiH4 flow rate, that is, film stress (Stress) increases with the increase of SiH4 flow rate. There is a positive correlation between refractive index (RI) and SiH4 flow rate, that is, refractive index (RI) increases with the increase of SiH4 flow rate. Among them, the unit of flow rate is sccm, and the flow units of different gases below are the same.

[0085] like Fig. 9 As shown in the figure, there is a positive correlation between film stress (Stress) and NH3 flow rate, that is, film stress (Stress) increases with the increase of NH3 flow rate. There is a negative correlation between refractive index (RI) and NH3 flow rate.

[0086] like Fig.10 As shown in the figure, there is a negative correlation between film stress (Stress) and N2 flow rate, that is, film stress (Stress) decreases with the increase of N2 flow rate. There is a positive correlation between refractive index (RI) and N2 flow rate.

[0087] like Fig.11 As shown in the figure, the film stress (Stress) is negatively correlated with the RF power, that is, the film stress (Stress) decreases with the increase of RF power. The refractive index (RI) is positively correlated with the RF power. The unit of RF power is watt (W).

[0088] like Fig.12 As shown in Figure 1, there is a positive correlation between film stress (Stress) and chamber pressure (Pressure), that is, film stress (Stress) increases with the increase of chamber pressure. There is a negative correlation between refractive index (RI) and chamber pressure. The unit of chamber pressure is Torr.

[0089] like Fig.13 As shown, the film stress (Stress) is positively correlated with the distance (Spacing) between the gas supply assembly 3 and the wafer 2, that is, the film stress (Stress) increases with the increase of Spacing. The refractive index (RI) is negatively correlated with Spacing. The unit of distance is mil.

[0090] By adjusting the film stress based on the relationship between the film stress and the process conditions, the wafer warpage change ΔBOW is adjusted. For example, if the wafer warpage change ΔBOW exceeds a preset threshold, the film stress value can be reduced by reducing the SiH4 flow rate and reducing the Spacing. The film stress can be changed from tensile stress to compressive stress, thereby reducing the wafer warpage change ΔBOW or making ΔBOW=0, while keeping RI unchanged.

[0091] In addition to film stress (Stress) and refractive index (RI), film properties also include etching rate (ER), extinction coefficient (EC), dielectric constant (k), etc. Through experimental research on the relationship between the above properties and process conditions, when it is necessary to adjust the film stress (Stress) without changing other properties, the process conditions that need to be adjusted can be calculated through the above relationship.

[0092] In some embodiments, before the step S210 of real-time monitoring of the wafer warpage variation ΔBOW, it further includes: acquiring a wafer warpage BOW value in real time, and obtaining the wafer warpage variation ΔBOW according to the wafer warpage BOW value.

[0093] During the process of wafer thin film deposition, a first film layer and a second film layer are alternately deposited to form a stacked structure. The first film layer has tensile stress, and the second film layer has compressive stress. The wafer warpage BOW value is obtained in real time, and the warpage of the stacked structure is adjusted by adjusting the film deposition time to change the thickness of one of the film layers.

[0094] Exemplarily, the first film layer is a SiN film layer, and the second film layer is a SiO2 film layer. When the wafer warpage BOW value is positive, the average thickness of subsequent SiO2 film layers is increased or the average thickness of subsequent SiN film layers is decreased; when the wafer warpage BOW value is negative, the average thickness of subsequent SiN film layers is increased or the average thickness of subsequent SiO2 film layers is decreased, so that the wafer warpage is controlled within the target warpage range.

[0095] It should be noted that the first film layer is a film layer with tensile stress, and the second film layer is a film layer with compressive stress. The first film layer and the second film layer may include multiple film layers or a single film layer, and the number of film layers is not limited here.

[0096] In an optional embodiment, the heating tray 1 includes at least two heating areas. In step S210, the change in wafer warpage ΔBOW is monitored according to a heating power change rate ΔP / P0 of the heating areas.

[0097] Exemplarily, the heating tray 1 includes a central heating area 11 and an edge heating area 12, and the edge heating area 12 is arranged at the periphery of the central heating area 11. Step S210 is specifically implemented as follows: real-time monitoring of the heating power change rate ΔP(C) / P0(C) of the central heating area 11 and the heating power change rate ΔP(E) / P0(E) of the edge heating area 12, and judging the warping state of the wafer 2 according to ΔP(C) / P0(C) and ΔP(E) / P0(E); if |ΔP(C) / P0(C)|>|ΔP(E) / P0(E)|, it is judged that the edge of the wafer 2 is bent toward its back side and convex in the middle, that is, it is bent downward; if |ΔP(C) / P0(C)|<|ΔP(E) / P0(E)|, it is judged that the edge of the wafer 2 is bent toward its front side and concave in the middle, that is, it is bent upward.

[0098] The wafer warpage variation ΔBOW is calculated by the corresponding relationship ΔP(C) / P0(C)=f1'(ΔBOW), ΔP(E) / P0(E)=f2'(ΔBOW). If ΔBOW exceeds a preset threshold, a reminder signal is triggered to the controller.

[0099] In some embodiments, after receiving the reminder signal, the controller activates a film forming process condition adjustment program. When the film forming process condition adjustment program is executed, it is used to obtain the mapping relationship between the wafer warpage change ΔBOW and the process conditions, determine the process conditions that need to be changed based on the mapping relationship, and use the changed process conditions to process the wafer 2, so that the warpage of the wafer 2 is controlled within the target warpage range.

[0100] In an optional embodiment, the heating tray 1 includes an electrostatic chuck, the process conditions in step S220 include a voltage of the electrostatic chuck, and the method further includes: changing the voltage of the electrostatic chuck according to a change in wafer warpage ΔBOW, thereby improving the wafer warpage.

[0101] Exemplarily, the adsorption force of the heating tray 1 on the wafer 2 is increased by increasing the voltage of the electrostatic chuck, so as to improve the warping state of the wafer 2 on the heating tray 1 .

[0102] In summary, during the process of depositing the thin film, the warping state of the wafer 2 in the chamber is monitored in real time. If the change in the wafer warping ΔBOW exceeds the preset threshold, the film forming process condition adjustment program is automatically activated to change the warping state of the wafer 2, thereby avoiding the deterioration of the film quality and arcing caused by the warping of the wafer 2. Since the thicker the film layer, the more likely it is to warp, the method of real-time monitoring of the warping of the wafer 2 is of greater significance for films with high film stress and high thickness. Compared with Example 1, the technical solution of Example 2 not only obtains the wafer warping and its change, but also adjusts the process conditions according to these results to improve the wafer warping.

[0103] Embodiment 3

[0104] Corresponding to the method for real-time monitoring of the warpage of the wafer 2 provided in the second embodiment, this embodiment matches a device for real-time monitoring of the warpage of the wafer 2. The device for monitoring the warpage of the wafer 2 includes a memory, a monitor, a controller and an operator.

[0105] The memory is configured to store at least one mapping relationship, where the mapping relationship is a mapping relationship between a wafer warpage variation ΔBOW and a process condition.

[0106] Exemplarily, a device for real-time monitoring of the warpage of the wafer 2 is used in a thin film deposition process, and the process conditions include any one or more combinations of gas flow, RF power, chamber pressure, gas composition ratio, terminal matching parameters, and the distance between the gas supply assembly 3 and the wafer 2.

[0107] The thin film deposition process is realized with the help of a thin film deposition device. The thin film deposition device includes: a chamber for thin film deposition; a gas supply assembly 3 for supplying process gas to the inside of the chamber; a heating tray 1, which is arranged below the gas supply assembly 3 and is used to carry and heat the wafer 2; and a radio frequency source for providing radio frequency power to excite the process gas inside the chamber to dissociate into plasma gas, and the plasma gas is used to deposit thin films on the wafer 2.

[0108] Exemplarily, the mapping relationship includes a first corresponding relationship and a second corresponding relationship, and the memory is further configured to store the first corresponding relationship and the second corresponding relationship.

[0109] The first corresponding relationship is the relationship between the wafer warpage change ΔBOW and the film stress, and the second corresponding relationship is the relationship between the film stress and the process conditions.

[0110] The monitor is configured to monitor a change in wafer warpage ΔBOW.

[0111] Exemplarily, the monitor is configured to monitor the heating power change rate ΔP / P0 of each heating zone on the heating tray, and determine the corresponding wafer warpage change ΔBOW based on the heating power change rate ΔP / P0 of each zone, wherein ΔP is the heating power change of the heating zone, and P0 is the heating power of the heating zone in the initial state. The heating tray includes at least two heating zones, each heating zone is in a set constant temperature control state, and the wafer is set on the at least two heating zones, and the wafer has a wafer area corresponding to each heating zone.

[0112] The controller is configured to receive information from the monitor, the information including the wafer warpage variation ΔBOW, and then activate the film forming process condition adjustment program and determine the changed process conditions according to the corresponding mapping relationship.

[0113] Exemplarily, the monitor is connected to the controller by electrical signals. The mapping relationships include multiple mapping relationships, and the controller determines the mapping relationship to be used from the multiple mapping relationships, thereby determining the process conditions to be changed according to the mapping relationship.

[0114] The operator is configured to receive the changed process conditions from the controller and process the wafer 2 using the changed process conditions.

[0115] Exemplarily, the operator is connected to the controller by electrical signals. After receiving the changed process conditions, the operator inputs the corresponding process conditions into the thin film deposition device. The process conditions are adjusted to change the film stress, thereby changing the warpage of the wafer 2.

[0116] In summary, during the thin film deposition process, the warping of wafer 2 is monitored in real time. If the change in wafer warping ΔBOW exceeds a preset threshold, the preset film forming process condition adjustment program is activated, and the corresponding mapping relationship is called to calculate and change the film forming process conditions, thereby changing the subsequent thin film stress, so that the warping of wafer 2 can be controlled, and the warped wafer 2 can even be restored to a flat state by using the opposite thin film stress.

[0117] The basic concepts have been described above. Obviously, for those skilled in the art, the above invention disclosure is only used as an example and does not constitute a limitation of the present application. Although not explicitly stated herein, those skilled in the art may make various modifications, improvements and amendments to the present application. Such modifications, improvements and amendments are suggested in the present application, so such modifications, improvements and amendments still belong to the spirit and scope of the exemplary embodiments of the present application.

[0118] At the same time, the present application uses specific words to describe the embodiments of the present application. For example, "one embodiment", "an embodiment", and / or "some embodiments" refer to a certain feature, structure or characteristic related to at least one embodiment of the present application. Therefore, it should be emphasized and noted that "one embodiment" or "an embodiment" or "an alternative embodiment" or "exemplary" mentioned twice or multiple times in different positions in this specification do not necessarily refer to the same embodiment. In addition, some features, structures or characteristics in one or more embodiments of the present application can be appropriately combined.

[0119] Similarly, it should be noted that in order to simplify the description of the disclosure of this application and thus help understand one or more embodiments of the invention, in the above description of the embodiments of this application, multiple features are sometimes combined into one embodiment, figure or description thereof. However, this disclosure method does not mean that the features required by the object of this application are more than the features mentioned in the claims. In fact, the features of the embodiments are less than all the features of the single embodiment disclosed above.

Claims

1. A method for real-time monitoring of wafer warpage, characterized in that: include: During the process of depositing a thin film on a wafer, a heating power change rate ΔP / P0 of each heating area on the heating tray is monitored in real time, wherein ΔP is the heating power change amount of the heating area, and P0 is the heating power of the heating area in the initial state, the heating tray comprises at least two heating areas, each heating area is in a set constant temperature control state, the wafer is arranged on the at least two heating areas, and the wafer has a wafer area corresponding to each of the heating areas; as well as It is determined according to the heating power change rate ΔP / P0 whether the corresponding wafer area is out of the heating tray.

2. The method for real-time monitoring of wafer warpage according to claim 1, characterized in that: The step of judging whether the corresponding wafer area is separated from the heating tray according to the heating power change rate ΔP / P0 includes: when the heating power change rate ΔP / P0<0, the wafer area corresponding to the corresponding heating area is separated from the heating tray.

3. The method for real-time monitoring of wafer warpage according to claim 1, characterized in that: The at least two heating regions include a central heating region and an edge heating region, wherein the edge heating region is arranged at the periphery of the central heating region; The step of judging whether the corresponding wafer area is out of the heating tray according to the heating power change rate ΔP / P0 comprises: If |ΔP(C) / P0(C)|>|ΔP(E) / P0(E)|, it is determined that the edge of the wafer is bent toward its back side and convex in the middle; if |ΔP(C) / P0(C)|<|ΔP(E) / P0(E)|, it is determined that the edge of the wafer is bent toward its front side and concave in the middle, wherein ΔP(C) represents the change in heating power corresponding to the central heating area, ΔP(E) represents the change in heating power corresponding to the edge heating area, P0(C) is the heating power corresponding to the central heating area in the initial state, and P0(E) is the heating power corresponding to the edge heating area in the initial state.

4. The method for real-time monitoring of wafer warpage according to claim 3, characterized in that: Also includes: Obtain the correspondence between the heating power change rate ΔP / P0 and the wafer warpage change ΔBOW, and obtain the wafer warpage change ΔBOW corresponding to the current heating power change rate ΔP / P0 according to the correspondence. If the wafer warpage change ΔBOW exceeds a preset threshold, trigger a reminder signal to the controller.

5. The method for real-time monitoring of wafer warpage according to claim 4, characterized in that: The corresponding relationship includes: ΔP(C) / P0(C)=f1'(ΔBOW) and ΔP(E) / P0(E)=f2'(ΔBOW), wherein f1' represents the relationship between ΔP(C) / P0(C) and ΔBOW, and f2' represents the relationship between ΔP(E) / P0(E) and ΔBOW.

6. The method for real-time monitoring of wafer warpage according to claim 1, characterized in that: The process of depositing a thin film on a wafer includes a PECVD process deposition process. Before the step of real-time monitoring the heating power change rate ΔP / P0 of each heating area on the heating tray, it also includes: determining that the thermal effects of the plasma field, chemical reaction, flow field, and thermal field on the heating tray are in a stable state.

7. The method for real-time monitoring of wafer warpage according to claim 1, characterized in that: The process of depositing a thin film on a wafer includes a CVD process deposition process. Before the step of real-time monitoring the heating power change rate ΔP / P0 of each heating area on the heating tray, it also includes: determining that the thermal effects of chemical reactions, flow fields, and thermal fields on the heating tray are in a stable state.

8. The method for real-time monitoring of wafer warpage according to claim 4, characterized in that: After receiving the reminder signal, the controller determines the process conditions that need to be changed based on the mapping relationship between the wafer warpage change ΔBOW and the process conditions, and processes the wafer according to the changed process conditions, so that the wafer warpage is controlled within the target warpage range.

9. A method for real-time monitoring of wafer warpage, characterized in that: include: During the process of thin film deposition on the wafer, the change in wafer warpage ΔBOW is monitored in real time; If the wafer warpage change ΔBOW exceeds a preset threshold, the process conditions that need to be changed are determined based on the mapping relationship between the wafer warpage change ΔBOW and the process conditions, and the wafer is processed using the changed process conditions, so that the wafer warpage is controlled within the target warpage range.

10. The method for real-time monitoring of wafer warpage according to claim 9, characterized in that: The mapping relationship includes a first corresponding relationship and a second corresponding relationship, wherein: The first corresponding relationship includes the relationship between the wafer warpage variation ΔBOW and film stress, and the second corresponding relationship includes the relationship between the film stress and the process conditions.

11. The method for real-time monitoring of wafer warpage according to claim 9, characterized in that: The step of real-time monitoring the wafer warpage change ΔBOW includes: real-time monitoring the heating power change rate ΔP / P0 of each heating area on the heating tray, and real-time monitoring the wafer warpage change ΔBOW according to the heating power change rate ΔP / P0, wherein the heating tray includes at least two heating areas, each heating area is in a set constant temperature control state, the wafer is arranged on the at least two heating areas, the wafer has a wafer area corresponding to each of the heating areas, ΔP is the heating power change of the heating area, and P0 is the heating power of the heating area in the initial state.

12. The method for real-time monitoring of wafer warpage according to claim 11, characterized in that: The at least two heating regions include a central heating region and an edge heating region, wherein the edge heating region is arranged at the periphery of the central heating region; The steps of real-time monitoring of the wafer warpage variation ΔBOW also include: If |ΔP(C) / P0(C)|>|ΔP(E) / P0(E)|, it is determined that the edge of the wafer is bent toward its back side and convex in the middle; if |ΔP(C) / P0(C)|<|ΔP(E) / P0(E)|, it is determined that the edge of the wafer is bent toward its front side and concave in the middle, wherein ΔP(C) / P0(C) represents the rate of change of heating power corresponding to the central heating area, ΔP(E) / P0(E) represents the rate of change of heating power corresponding to the edge heating area, P0(C) is the heating power corresponding to the central heating area in the initial state, and P0(E) is the heating power corresponding to the edge heating area in the initial state.

13. The method for real-time monitoring of wafer warpage according to claim 12, characterized in that: Also includes: Obtain the correspondence between the heating power change rate ΔP / P0 and the wafer warpage change ΔBOW, and obtain the wafer warpage change ΔBOW corresponding to the current heating power change rate ΔP / P0 according to the correspondence. If the wafer warpage change ΔBOW exceeds a preset threshold, trigger a reminder signal to the controller.

14. The method for real-time monitoring of wafer warpage according to claim 13, characterized in that: The corresponding relationship includes: ΔP(C) / P0(C)=f1'(ΔBOW) and ΔP(E) / P0(E)=f2'(ΔBOW), wherein f1' represents the relationship between ΔP(C) / P0(C) and ΔBOW, and f2' represents the relationship between ΔP(E) / P0(E) and ΔBOW.

15. The method for real-time monitoring of wafer warpage according to claim 9, characterized in that: The process conditions include one or any combination of gas flow rate, radio frequency power, chamber pressure, gas composition ratio, terminal matching parameters, and film deposition time.

16. The method for real-time monitoring of wafer warpage according to claim 11, characterized in that: The heating tray is arranged below a gas supply assembly, and the gas supply assembly is used to supply process gas deposited on the surface of the wafer; the process conditions include the distance between the gas supply assembly and the wafer.

17. The method for real-time monitoring of wafer warpage according to claim 9, characterized in that: Before the step of real-time monitoring the wafer warpage variation ΔBOW, the method further includes: acquiring a wafer warpage BOW value in real time, and obtaining the wafer warpage variation ΔBOW according to the wafer warpage BOW value.

18. The method for real-time monitoring of wafer warpage according to claim 17, characterized in that: During the process of depositing a thin film on a wafer, a first film layer and a second film layer are alternately deposited to form a stacked structure, the first film layer has tensile stress, and the second film layer has compressive stress. The method also includes: when the wafer warpage BOW value is positive, increasing the average thickness of the subsequent second film layer or reducing the average thickness of the subsequent first film layer; when the wafer warpage BOW value is negative, increasing the average thickness of the subsequent first film layer or reducing the average thickness of the subsequent second film layer, so that the wafer warpage is controlled within the target warpage range.

19. The method for real-time monitoring of wafer warpage according to claim 18, characterized in that: The first film layer is a SiN film layer, and the second film layer is a SiO2 film layer.

20. The method for real-time monitoring of wafer warpage according to claim 10, characterized in that: The wafer warpage variation ΔBOW is positively correlated with the absolute value of the film stress.

21. The method for real-time monitoring of wafer warpage according to claim 10, characterized in that: The process conditions include film deposition time, and the film stress is positively correlated with the film deposition time.

22. The method for real-time monitoring of wafer warpage according to claim 11, characterized in that: The heating tray includes an electrostatic chuck, the process conditions include a voltage of the electrostatic chuck, and the method further includes: adjusting the voltage of the electrostatic chuck according to the wafer warpage variation ΔBOW.

23. A device for real-time monitoring of wafer warpage, characterized in that: include: A memory configured to store at least one mapping relationship, wherein the mapping relationship is a mapping relationship between a wafer warpage variation ΔBOW and a process condition; A monitor configured to monitor the wafer warpage variation ΔBOW in real time; A controller configured to receive the wafer warpage variation ΔBOW, and if the wafer warpage variation ΔBOW exceeds a preset threshold, determine the process conditions that need to be changed according to a mapping relationship between the wafer warpage variation ΔBOW and the process conditions; The operator is configured to receive the changed process conditions and process the wafer using the changed process conditions.

24. The device for real-time monitoring of wafer warpage according to claim 23, characterized in that: The mapping relationship includes a first corresponding relationship and a second corresponding relationship; The first corresponding relationship includes the relationship between the wafer warpage variation ΔBOW and film stress, and the second corresponding relationship includes the relationship between the film stress and the process conditions.

25. The device for real-time monitoring of wafer warpage according to claim 23, characterized in that: The monitor is configured to monitor the heating power change rate ΔP / P0 of each heating area on the heating tray, and determine the corresponding wafer warpage change ΔBOW according to the heating power change rate ΔP / P0 of each area, wherein ΔP is the heating power change of the heating area, and P0 is the heating power of the heating area in the initial state. The heating tray includes at least two heating areas, each heating area is in a set constant temperature control state, and the wafer is arranged on the at least two heating areas, and the wafer has a wafer area corresponding to each of the heating areas.