Method and device for measuring thickness of optical chip based on Fabry-Perot interference principle

Through the optical chip thickness measurement method based on the principle of Faber-Perl interference, using red light auxiliary light source and three-dimensional micro-motion platform, combined with EFPI sensor and Fourier change technology, the problem of slow chip thickness measurement speed in the existing technology is solved and achieved Fast, accurate and low-cost measurement results.

CN118776471AActive Publication Date: 2024-10-15BEIJING RES INST OF TELEMETRY
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410749550.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-12
Publication Date
2024-10-15
Estimated Expiration
2044-06-12

AI Technical Summary

Technical Problem

Existing chip thickness measurement methods have large equipment, high cost, and slow measurement speed, making it difficult to achieve rapid measurement.

Method used

An optical chip thickness measurement method based on the Faber-Perl interference principle is adopted, a red light auxiliary light source is introduced through a fiber circulator and a 1*2 beam splitter, and a three-dimensional micro-motion platform is used to quickly adjust the chip position. Combined with EFPI sensors and Fourier transform technology, it is achieved Fast and accurate chip thickness measurement.

Benefits of technology

It achieves miniaturized, low-cost and fast chip thickness measurement, with a measurement speed of up to 0.02 seconds, and uses visible light to assist in adjusting the position, providing a visualization method and significantly improving measurement efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118776471A_ABST
    Figure CN118776471A_ABST
Patent Text Reader

Abstract

The invention provides an optical chip thickness measuring method and device based on a Fabry-Perot interference principle, and the device comprises an auxiliary light source, a light source in optical connection with the auxiliary light source, an optical fiber circulator, an optical splitter in optical connection with the auxiliary light source and the optical fiber circulator, a light beam collimator in optical connection with the female end of the optical splitter, and a to-be-measured chip disposed at the output end of the light beam collimator. The three-dimensional micro-motion platform is used for containing a chip to be tested; the testing device is connected with the other end of the optical fiber circulator; a Fabry-Perot interference principle is used as a measurement principle, optical signals are transmitted through an optical fiber, and red light is introduced by adding a 1 * 2 optical splitter, so that a visible light auxiliary adjustment function is realized, the position adjustment speed of the chip is accelerated, and the purpose of quickly measuring the thickness of the transparent chip is realized. According to the invention, miniaturization can be realized, the cost is low, and the speed is high; a user can clearly determine the position of a measuring point according to a light beam irradiation point position, and meanwhile visible light provides a visual means for reflected light to enter the collimator.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of measurement and testing technology, and in particular to a method and device for measuring the thickness of an optical chip based on the Fabry-Perot interference principle. Background Art

[0002] Chips play a vital role in modern science and technology and social life. They are high-tech industries with high technical content and added value, and are of great significance to the development of the national economy. Since chips are widely used in almost all high-tech fields, their forms are also destined to be diverse, such as traditional silicon-based chips and sapphire chips processed by MEMS technology that are commonly used in the rapidly developing optical field.

[0003] The thickness of a chip is an important physical indicator of the chip. The current measurement method is to use the principles of spectral confocal, white light confocal, and laser triangulation. Due to the limitation of the principle, the equipment is generally large in size, high in price, and slow in measurement speed.

[0004] Therefore, a fast method for measuring chip thickness is needed. Summary of the invention

[0005] The present invention is to solve the problem of chip thickness measurement rate, and provides an optical chip thickness measurement method and device based on the Fabry-Perot interference principle, including an auxiliary light source, an optically connected light source, an optical fiber circulator, a beam splitter optically connected to the auxiliary light source and the optical fiber circulator, a beam collimator optically connected to the female end of the beam splitter, a chip to be tested arranged at the output end of the beam collimator, a three-dimensional micro-motion platform for holding the chip to be tested, and a test device at the other end of the optical fiber circulator. The present invention uses the Fabry-Perot interference principle as the measurement principle, transmits optical signals through optical fibers, introduces red light by adding a 1*2 beam splitter, realizes the function of auxiliary adjustment of visible light, speeds up the position adjustment speed of the chip, and can accurately measure the accurate measurement position in real time by auxiliary red light, so as to achieve the purpose of rapid measurement of the thickness of the transparent chip. The present invention can be miniaturized, and has low cost and high speed; the user can clearly determine the measurement point position according to the beam irradiation point, and the visible light also provides a visualization means for the reflected light to enter the collimator.

[0006] The present invention provides an optical chip thickness measurement method based on the Fabry-Perot interference principle, comprising the following steps:

[0007] S1. Build an optical chip thickness measuring device based on the Fabry-Perot interference principle, establish optical connections between the sub-end of the beam splitter and an auxiliary light source and one port of the fiber circulator, establish optical connections between the other port of the fiber circulator and the light source, establish optical connections between the female end of the beam splitter and the beam collimator, and establish optical connections between the third port of the fiber circulator and the test device. The auxiliary light source is a visible light source, the light source is a broadband laser, and the test device includes a demodulator;

[0008] S2, placing the chip to be tested on the three-dimensional micro-motion platform and at the lower end of the beam collimator, the chip to be tested being a transparent chip with optical reflection on both the upper and lower surfaces;

[0009] S3, turning on the auxiliary light source, the auxiliary light is output to the chip to be tested via the beam splitter and the beam collimator, and the position of the chip to be tested is adjusted by adjusting the three-dimensional micro-motion platform so that the auxiliary light reflected by the chip to be tested enters the beam collimator;

[0010] S4, turn on the light source, the output light of the light source passes through the fiber circulator and the beam splitter in turn, enters the beam collimator, and is collimated to the chip to be tested. After reflection from the chip to be tested, it passes through the beam collimator, the beam splitter, and the fiber circulator in turn to output to the test device. The test device uses double-beam interference demodulation to obtain the EFPI sensor reflection spectrum, and then performs Fourier transformation to obtain the EFPI cavity length d. Combined with the refractive index n of the chip to be tested, the thickness D of the chip to be tested is obtained:

[0011]

[0012] A method for measuring the thickness of an optical chip based on the Fabry-Perot interferometry principle was completed.

[0013] The optical chip thickness measurement method based on the Fabry-Perot interferometer principle described in the present invention is, as a preferred embodiment, in step S4, the reflection spectrum of the EFPI sensor is:

[0014] I(v)=C1+C2cos(4πdv);

[0015] in: C1 and C2 are constants, and λ is the wavelength of the light source;

[0016] After filtering out the DC amount of the EFPI sensor reflection spectrum:

[0017] I(v)=∫P(f)exp(i2πfv)df;

[0018] Among them, P is the frequency spectrum distribution corresponding to the interference spectrum, and f is the frequency;

[0019] The distribution of spectral energy with EFPI cavity length is obtained by Fourier transforming the reflection spectrum of the EFPI sensor after the DC quantity is filtered out, and the peak coordinates are read in the distribution of spectral energy with EFPI cavity length to obtain the cavity length d.

[0020] The optical chip thickness measurement method based on the Fabry-Perot interference principle described in the present invention is, as a preferred embodiment, in step S1, an optical connection is established between one sub-end of the splitter and an auxiliary light source, the other sub-end is optically connected to the PORT2 end of the fiber optic circulator, the PORT1 end of the fiber optic circulator is optically connected to the light source, and the PORT3 end of the fiber optic circulator is connected to the test device.

[0021] The optical chip thickness measurement method based on the Fabry-Perot interference principle described in the present invention is, as a preferred method, to wipe and clean the FC / APC optical fiber end face of the splitter using dust-free paper dipped in 2 ml of ethanol solution, and then align the protrusion of the splitter packaging connector with the recess of the optical fiber circulator, so that the optical fiber of the FC / APC ferrule and the white ceramic alignment piece of the optical fiber circulator are maintained in parallel and slowly inserted, and after insertion, the nut fixing part is screwed to the tightest state.

[0022] The optical chip thickness measurement method based on the Fabry-Perot interference principle described in the present invention is, as a preferred embodiment, in step S1, a beam collimator is fixed at a height of 5 to 15 cm in a direction perpendicular to the three-dimensional micro-motion platform, the optical fiber sleeve is stripped at 1.5 cm from the end of the pigtail of the beam collimator, and the coating layer is stripped at 1.2 cm, and 2 ml of ethanol solution is dipped in dust-free paper to clean the stripped optical fiber, and a light cutter is used to cut the optical fiber flat at 1.0 cm from the end and make the fiber end face perpendicular to the axial transmission direction of the optical fiber;

[0023] Remove the fiber ferrule at 1.5cm from the end of the pigtail of the female end of the optical splitter and remove the coating at 1.2cm. Use dust-free paper dipped in 2ml of ethanol solution to clean the stripped fiber. Use a fiber cleaver to cut the fiber flat at 1.0cm from the end and make the fiber end face perpendicular to the axial transmission direction of the fiber.

[0024] Start the fiber fusion splicer, place the processed beam collimator fiber and splitter pipeline in the V-groove respectively and cover the windproof cover of the fusion splicer, then use the fiber fusion splicer to discharge and remove dust from the fiber end face. The end face cutting status can be obtained on the display screen of the fiber fusion splicer; if the on-board detection of the fusion splicer issues an alarm, the end face needs to be re-cut; if the inclination angle between the plane and the fiber cross section is less than 1°, the fiber fusion splicer defaults to a good end face condition.

[0025] The optical chip thickness measurement method based on the Fabry-Perot interference principle described in the present invention is, as a preferred method, to select an LC / APC-FC / APC jumper to connect the demodulator of the test device with a PLC one-to-two splitter connected to the optical fiber circulator.

[0026] The optical chip thickness measurement method based on the Fabry-Perot interference principle described in the present invention is, as a preferred method, to connect the other sub-end of the beam splitter to the auxiliary light source, and the connection method is: after opening the auxiliary light source protection cover, use dust-free paper to dip in 2 ml of ethanol solution to wipe and clean the fiber end face of the FC / APC, and then slowly insert the optical fiber of the FC / APC ferrule to keep it parallel to the white ceramic alignment piece of the optical fiber coupler;

[0027] Use an 8-core transmission network cable to connect the demodulator to the computer network interface, and open the supporting software to read the spectrum signal;

[0028] In step S4, the LABVIEW software is opened, and the demodulation calculation software is called to obtain the thickness of the chip to be tested.

[0029] The present invention provides an optical chip thickness measuring device based on the Fabry-Perot interference principle, comprising an auxiliary light source, an optically connected light source and an optical fiber circulator, an optical splitter optically connected to the auxiliary light source and the optical fiber circulator, a beam collimator optically connected to the female end of the beam collimator, a chip to be tested arranged at the output end of the beam collimator, a three-dimensional micro-motion platform for holding the chip to be tested, and a test device connected to the other end of the optical fiber circulator;

[0030] The auxiliary light source outputs visible light, the light source is a broadband light source, the light passing band of the beam collimator includes the bands of the auxiliary light source and the light source, the beam collimator is perpendicular to the three-dimensional micro-motion platform, and the chip to be tested is located at the center of the three-dimensional micro-motion platform;

[0031] The optical fiber circulator transmits the output light of the light source to the optical splitter and detects the thickness of the chip to be tested. The detection signal reflected back by the chip to be tested reaches the demodulation device of the test device after passing through the optical fiber circulator.

[0032] The optical chip thickness measuring device based on the Fabry-Perot interference principle described in the present invention, as a preferred embodiment, comprises a demodulation device and a computer optically connected to one port of the optical fiber circulator in sequence;

[0033] The optical fiber circulator comprises an optical fiber circulator body and PORT1, PORT2 and PORT3 respectively connected to the optical fiber circulator body; PORT1 is optically connected to a light source, PORT2 is optically connected to a sub-end of an optical splitter, and PORT3 is optically connected to a demodulator;

[0034] The optical splitter is a 1*2 optical splitter including two sub-ends and one female end;

[0035] The auxiliary light source and the optical fiber circulator are optically connected to a sub-end of the optical splitter respectively;

[0036] The three-dimensional micro-motion platform can be adjusted in the x-direction, y-reverse direction, and z-direction.

[0037] The optical chip thickness measuring device based on the Fabry-Perot interference principle described in the present invention is preferably configured such that the auxiliary light source is a red light illuminating optical fiber test pen with a wavelength of 650 nm and can be adapted to an FC optical fiber interface;

[0038] The optical splitter is a PLC optical splitter, the female end is a pigtail form, and the two female ends are FC / APC ferrule packaging;

[0039] The beam collimator is a fiber collimator with a collimation angle of 0.1°;

[0040] The refractive index of the chip to be tested is a known constant, and the chip to be tested is a transparent quartz chip or a sapphire chip;

[0041] The demodulation device is a spectrum demodulator, or a MOI demodulator can be used to replace the light source, the optical fiber circulator and the demodulation device. The computer includes a chassis, a computer display and a computer host.

[0042] The present invention discloses a method and device for measuring the thickness of a transparent chip using optical means under the assistance of visible red light. The device uses the Fabry-Perot interference principle as the measurement principle, transmits optical signals through optical fibers, introduces red light by adding a 1*2 beam splitter, realizes the function of visible light auxiliary adjustment, speeds up the position adjustment speed of the chip, and realizes the purpose of quickly measuring the thickness of the transparent chip.

[0043] The present invention uses optical means to realize a thickness measurement method for a transparent chip with the aid of visible red light. The method is characterized in that it includes the following steps:

[0044] Step 1. Selection of light source, auxiliary light source, fiber collimator, and demodulation device: The light source should match the demodulation module recognition band; the auxiliary light source should be a visible light band laser; the fiber collimator light band should include the light source and auxiliary light source bands; the demodulation device should have a tunable Fabry-Perot filter function.

[0045] Step 2. Build a signal collection and primary processing device: connect one of the sub-ends of the 1*2 splitter to the auxiliary light source, the other sub-end to the PORT2 end of the fiber circulator, the PORT1 end of the circulator to the light source, the PORT3 end to the demodulation device, and the female end of the 1*2 splitter to the collimator.

[0046] Step 3. Build a test device, which consists of the signal collection and primary processing device, computer and three-dimensional micro-motion platform connected in step 2. The signal is collected, processed by the demodulation device, and then transmitted to the computer for software program solution and final measurement result output.

[0047] Step 4. The relative position relationship is that the beam collimator is perpendicular to the three-dimensional micro-motion platform, and the chip to be tested is placed at the center of the three-dimensional micro-motion platform.

[0048] The present invention introduces a PLC beam splitter, allowing the fiber collimator to be connected to a broadband light source and an auxiliary light source at the same time, thereby realizing rapid detection of the thickness of a designated position of a chip with the aid of visible light. When the broadband light source is turned on, the auxiliary light source is also turned on.

[0049] The present invention adopts a customized three-dimensional micro-displacement platform, which can accurately move the chip to be tested and realize the detection of different positions of the optical chip.

[0050] The auxiliary light emitted by the device manufactured by the manufacturing method of the present invention is vertically emitted to the chip to be tested together with the test light beam, and the upper and lower surfaces of the chip to be tested respectively reflect the light beams to form an FP cavity, which enters the demodulation device after being transmitted through the device, and the signal is processed to obtain the cavity length, and then the thickness of the chip is obtained.

[0051] The present invention introduces an optical fiber circulator, which allows the light of a broadband light source to be transmitted to a 1*2 optical splitter, thereby detecting the optical chip. On the other hand, the reflected detection signal reaches a demodulation device after passing through the optical fiber circulator to achieve signal demodulation.

[0052] The present invention has the following advantages:

[0053] (1) Existing devices that can be used to measure the thickness of optical chips are developed based on the principles of spectral confocal, white light confocal, and laser triangulation. Due to the limitation of the principles, the devices are large in size and high in cost. For these three principles, the chip thickness is calculated by the position difference between the upper and lower surfaces. The process of refocusing during measurement causes the measurement speed to be slow. The devices used by the principles of the present invention can be miniaturized and have low costs. The thickness measured by this principle is directly calculated by measuring the FP cavity length constructed by the chip, without repeating the focusing step. The measurement speed is only determined by the speed at which the signal transmission and demodulation device collects the signal. The transmission speed of light is 3×10 8 m / s, the computer's demodulation rate can reach 50 times / second, so after placing the chip to be tested in a suitable position, the thickness information can be obtained within 0.02 seconds, which is very fast.

[0054] (2) By introducing auxiliary light in the visible light band, the measurement position is clear at a glance. The user can clearly identify the measurement point according to the point where the light beam illuminates. At the same time, visible light also provides a visualization means for the reflected light to enter the collimator. BRIEF DESCRIPTION OF THE DRAWINGS

[0055] Figure 1 The flowchart is a method for measuring the thickness of an optical chip based on the Fabry-Perot interferometer principle;

[0056] Figure 2 The schematic diagram of the structure of an optical chip thickness measurement device based on the Fabry-Perot interferometer principle is shown in FIG.

[0057] Figure 3 Create a flow chart for an optical chip thickness measurement method and device based on the Fabry-Perot interferometer principle;

[0058] Figure 4 A schematic diagram of an optical chip thickness measurement method and device assembly based on the Fabry-Perot interferometer principle;

[0059] Figure 5 This is a typical reflection spectrum diagram of an optical chip thickness measurement method and device EFPI based on the Fabry-Perot interferometer principle;

[0060] Figure 6 This is a schematic diagram of an optical chip thickness measurement method based on the Fabry-Perot interferometry principle and the distribution of the device's spectral energy along with the EFPI cavity length.

[0061] Reference numerals:

[0062] 1. Auxiliary light source; 2. Light source; 3. Fiber optic circulator; 31. Fiber optic circulator body; 32. PORT1 port; 33. PORT2 port; 34. PORT3 port; 4. Spectrum splitter; 5. Beam collimator; 6. Chip to be tested; 7. Three-dimensional micro-motion platform; 8. Test device; 81. Demodulation device; 82. Computer. DETAILED DESCRIPTION

[0063] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0064] Example 1

[0065] like Figures 1 to 4 As shown, a method and device for measuring the thickness of an optical chip based on the Fabry-Perot interference principle;

[0066] Among them, an optical chip thickness measurement method based on the Fabry-Perot interferometer principle includes:

[0067] (1) Step 1: Selection of auxiliary light source 1, light source 2, fiber collimator 5, and demodulation device 81: The light source 2 should be selected to match the recognition band of the demodulation module 81; the auxiliary light source 1 should be a visible light band laser; the optical band of the fiber collimator 5 should include the bands of the light source 2 and the auxiliary light source 1; the demodulation device 81 should be selected to have a tunable Fabry-Perot filtering function.

[0068] Selection of laser 1, collimator 5, and demodulation device 81: Laser 1 selects a visible light band laser. For example, a commonly used red light illuminating fiber optic test pen with a band of 650nm (hereinafter referred to as red light pen) can be selected. This device can be adapted to the fiber optic interface of FC, which can provide convenient conditions for subsequent use. Collimator 5 selects a wide-band collimator, which is required to allow both the auxiliary visible light band and the test light source band to pass through. The common MOI demodulator on the market is selected as the demodulation device, which includes three parts: light source 2, fiber circulator 3, and demodulation device 81. The female end of the 1*2 splitter 4 adopts a pigtail form, and the two sub-ends select the packaging form of FC / APC ferrule. The chip 6 to be tested is a quartz chip.

[0069] (2) Step 2: Build a signal collection and primary processing device: connect one of the sub-ends of the 1*2 splitter 4 to the auxiliary light source 1, and the other sub-end to the fiber circulator PORT2 end 33, the circulator PORT1 end 32 to the light source 2, the PORT3 end 34 to the demodulation device 81, and the female end of the 1*2 splitter 4 to the collimator 5.

[0070] Choose a broadband collimator 5 with a collimation angle of 0.1° on the market, and fix the collimator 5 at a height of 10CM in a direction perpendicular to the three-dimensional micro-motion platform 7. Strip the fiber sleeve at 1.5cm from the end of the pigtail of the collimator 5, and strip the coating at 1.2cm. Use dust-free paper to dip 2ml of ethanol solution to clean the fiber stripped of the coating, and use a light cutter to cut it flat at 1.0cm from the end so that its end face is perpendicular to the axial transmission direction of the optical fiber. Perform the same operation on the female end of the PLC one-to-two optical splitter 4. Start the optical fiber fusion splicer, place the two processed optical fibers in the V-groove respectively, and cover the windproof cover of the fusion splicer, then use the optical fiber fusion splicer to discharge and remove the dust on the end face of the optical fiber, and the end face cutting status can be obtained on the display screen of the optical fiber fusion splicer. If the on-board detection of the fusion splicer issues an alarm, the end face needs to be re-cut; and if the inclination angle between the plane and the cross section of the optical fiber is less than 1°, the optical fiber fusion splicer defaults to a good end face condition.

[0071] Next, connect one of the sub-ends of the 1*2 splitter 4 to the fiber coupler 3. Before the connection, use dust-free paper dipped in 2 ml of ethanol solution to wipe and clean the fiber end face of the FC / APC. Then align the protrusion of the package connector with the recess of the fiber coupler 3, and slowly insert the optical fiber of the FC / APC ferrule in parallel with the white ceramic alignment piece of the fiber coupler 3. After insertion, screw the nut fixing to the tightest state.

[0072] Use LC / APC-FC / APC jumper to connect MOI demodulator 81 to PLC one-to-two splitter 4 connected to the fiber coupler in the previous step. Insert the LC / APC end jumper into the signal channel 1 of the MOI demodulator until you hear a click of the plastic part, which means the connection is successful. Wipe the FC / APC end of the jumper with 2ml of ethanol solution using dust-free paper, and insert it into the other end of the fiber coupler in the same way as in the previous step and tighten it.

[0073] Connect the other end of the 1*2 splitter 4 to the red light pen 1. The connection method is: open the protective cover of the red light pen 1, and then use dust-free paper dipped in 2 ml of ethanol solution to wipe and clean the fiber end face of the FC / APC. Then, keep the optical fiber of the FC / APC ferrule parallel to the white ceramic alignment piece of the fiber coupler 3 and slowly insert it. The appropriate depth is when you feel the damping of the spring.

[0074] (3) Step 3: Build a test device, which consists of the signal collection and primary processing device connected in step 2, the computer 82 and the three-dimensional micro-motion platform 7. Fix the beam collimator in a direction perpendicular to the three-dimensional micro-motion platform 7.

[0075] Use an 8-core transmission network cable to connect the MOI demodulator 81 to the network cable interface of the computer 82, open the MOI supporting software to read the MOI signal. Open the LABVIEW software, call the corresponding demodulation calculation software, and the measurement signal and the thickness information of the chip 6 to be measured can be displayed.

[0076] (4) Step 4: Place the transparent chip 6 to be tested on the three-dimensional micro-motion platform 7, and adjust the three-dimensional micro-motion platform 7 so that the light beam is irradiated on the point to be tested, and at the same time confirm that the light beam reflected by the transparent chip 6 enters the collimator 5.

[0077] After the operator wears laser goggles, he turns on the red light pen 1 switch to the normally on state, places the sapphire chip 6 to be tested in the middle part of the three-dimensional micro-motion platform 7, observes the auxiliary light in the visible band, and selects the position where the thickness is to be measured by adjusting the three-dimensional micro-motion platform 7 to ensure that the auxiliary light is irradiated on the position to be tested, and the light beam reflected by the transparent chip 6 enters the collimator 5.

[0078] (5) Step 5: After the primary processing by the demodulation device and the demodulation processing by the computer 82, the thickness of the chip 6 to be tested can be displayed in real time on the computer.

[0079] By inputting the refractive index of the chip 6 to be measured in the computer display interface, the thickness information of the chip 6 can be read to complete the measurement.

[0080] The demodulation method used in the demodulation device is double-beam interference demodulation. The typical reflection spectrum of the EFPI sensor obtained by the demodulation terminal is as follows, and its schematic diagram is as follows Figure 5 As shown:

[0081] I(v)=C1+C2cos(4πdv) (1)

[0082] in: C1 and C2 are constant terms, λ is the wavelength, and d is the cavity length of the FP cavity. After filtering out the DC quantity, equation (1) can be written as:

[0083] I(v)=∫P(f)exp(i2πfv)df (2)

[0084] Among them, P is the frequency spectrum distribution corresponding to the interference spectrum, f is the frequency, and the Fourier transform is performed to obtain the distribution of spectral energy with the EFPI cavity length, as shown in the schematic diagram. Figure 6 As shown, the horizontal coordinate of the peak value is read, and the cavity length is 785 microns, combined with the thickness conversion formula:

[0085]

[0086] Wherein, d is the cavity length of the FP cavity, n is the refractive index of the material of the chip 6 to be tested. Since the chip in this example is made of quartz, its refractive index is 1.575, and its thickness is:

[0087]

[0088] After the measurement is completed, the computer interface shows that the thickness is 0.4984mm.

[0089] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. An optical chip thickness measurement method based on the Fabry-Perot interferometer principle, Features: The following steps are involved: S1. Build an optical chip thickness measuring device based on the Fabry-Perot interference principle, establish optical connections between the sub-end of the beam splitter (4) and an auxiliary light source (1) and one port of the optical fiber circulator (3), respectively, establish optical connection between the other port of the optical fiber circulator (3) and the light source (2), establish optical connection between the female end of the beam splitter (4) and the beam collimator (5), establish optical connection between the third port of the optical fiber circulator (3) and the testing device (8), the auxiliary light source (1) is a visible light source, the light source (2) is a broadband laser, and the testing device (8) includes a demodulation device; S2, placing the chip to be tested (6) on the three-dimensional micro-motion platform (7) at the lower end of the beam collimator (5), wherein the chip to be tested (6) is a transparent chip with optical reflection on both the upper and lower surfaces; S3, turning on the auxiliary light source (1), outputting the auxiliary light to the chip to be tested (6) via the beam splitter (4) and the beam collimator (5), and adjusting the position of the chip to be tested (6) by adjusting the three-dimensional micro-motion platform (7) so that the auxiliary light reflected by the chip to be tested (6) enters the beam collimator (5); S4, turn on the light source (2), the output light of the light source (2) passes through the optical fiber circulator (3) and the optical splitter (4) in sequence, enters the beam collimator (5), and is emitted to the chip to be tested (6) after being collimated. After being reflected by the chip to be tested (6), the light is output to the test device (8) in sequence through the beam collimator (5), the optical splitter (4), and the optical fiber circulator (3). The test device (8) uses double-beam interference demodulation to obtain the EFPI sensor reflection spectrum, and then performs Fourier transformation to obtain the EFPI cavity length d. Combined with the refractive index n of the chip to be tested (6), the thickness D of the chip to be tested (6) is obtained: A method for measuring the thickness of an optical chip based on the Fabry-Perot interferometry principle was completed.

2. The optical chip thickness measurement method based on Fabry-Perot interferometry principle according to claim 1, Features: In step S4, the reflection spectrum of the EFPI sensor is: I(v)=C 1 +C 2 cos(4πdv); in: 1 , C 2 is a constant, λ is the wavelength of the light source (2); After filtering out the DC amount of the EFPI sensor reflection spectrum: I(v)=∫P(f)exp(i2πfv)df; Among them, P is the frequency spectrum distribution corresponding to the interference spectrum, and f is the frequency; The EFPI sensor reflection spectrum after the DC quantity is filtered out is subjected to Fourier transformation to obtain the distribution of spectral energy with the EFPI cavity length, and the peak coordinates are read from the distribution of spectral energy with the EFPI cavity length to obtain the cavity length d.

3. The optical chip thickness measurement method based on Fabry-Perot interferometry principle according to claim 1, Features: In step S1, one sub-end of the optical splitter (4) is optically connected to the auxiliary light source (1), and the other sub-end is optically connected to the PORT2 end of the optical fiber circulator (3). The PORT1 end of the optical fiber circulator (3) is optically connected to the light source (2), and the PORT3 end of the optical fiber circulator (3) is connected to the test device (8).

4. The optical chip thickness measurement method based on Fabry-Perot interferometry principle according to claim 3, Features: Use dust-free paper dipped in 2 ml of ethanol solution to wipe and clean the FC / APC optical fiber end face of the splitter (4), then align the protrusion of the package connector of the splitter (4) with the recessed part of the optical fiber circulator (3), and slowly insert the optical fiber of the FC / APC ferrule in parallel with the white ceramic alignment piece of the optical fiber circulator (3). After insertion, screw the nut fixing part to the tightest state.

5. The optical chip thickness measurement method based on Fabry-Perot interferometry principle according to claim 1, Features: In step S1, the beam collimator (5) is fixed at a height of 5 to 15 cm in a direction perpendicular to the three-dimensional micro-motion platform (7), the optical fiber sleeve is stripped at 1.5 cm from the end of the pigtail of the beam collimator (5), and the coating is stripped at 1.2 cm, and the optical fiber with the coating stripped is cleaned with 2 ml of ethanol solution dipped in dust-free paper, and the optical fiber is cut flat at 1.0 cm from the end with a light cutter so that the fiber end face is perpendicular to the axial transmission direction of the optical fiber; Strip the fiber optic sleeve 1.5 cm from the end of the pigtail at the female end of the optical splitter (4) and strip the coating layer 1.2 cm from the end, use dust-free paper dipped in 2 ml of ethanol solution to clean the stripped fiber optic, use a light cleaver to cut the fiber optic at 1.0 cm from the end and make the fiber end face perpendicular to the axial transmission direction of the fiber optic; Start the fiber fusion splicer, place the processed optical fiber of the beam collimator (5) and the optical splitter (4) pipeline in the V-groove respectively and cover the windproof cover of the fusion splicer, then use the fiber fusion splicer to discharge and clean the dust on the end face of the optical fiber, and the end face cutting status can be obtained on the display screen of the fiber fusion splicer; if the on-board detection of the fusion splicer issues an alarm, the end face needs to be re-cut; if the inclination angle between the plane and the cross section of the optical fiber is less than 1°, the fiber fusion splicer defaults that the end face is in good condition.

6. The optical chip thickness measurement method based on Fabry-Perot interferometry principle according to claim 5, Features: An LC / APC-FC / APC jumper is selected to connect the demodulator of the test device (8) to the PLC one-to-two optical splitter connected to the optical fiber circulator (3).

7. The optical chip thickness measurement method based on Fabry-Perot interferometry principle according to claim 6, Features: The other end of the optical splitter (4) is connected to the auxiliary light source (1) in the following manner: after opening the protective cover of the auxiliary light source (1), use a dust-free paper dipped in 2 ml of ethanol solution to wipe and clean the end face of the FC / APC optical fiber, and then slowly insert the optical fiber of the FC / APC ferrule in parallel with the white ceramic alignment piece of the optical fiber coupler; Use an 8-core transmission network cable to connect the demodulator to the computer network interface, and open the supporting software to read the spectrum signal; In step S4, the LABVIEW software is opened and the demodulation calculation software is called to obtain the thickness of the chip (6) to be tested.

8. An optical chip thickness measuring device based on Fabry-Perot interferometry principle according to any one of claims 1 to 6, Features: The invention comprises an auxiliary light source (1), an optically connected light source (2), an optical fiber circulator (3), an optical splitter (4) optically connected to the auxiliary light source (1) and the optical fiber circulator (3), a beam collimator (5) optically connected to the female end of the beam splitter (4), a chip to be tested (6) arranged at the output end of the beam collimator (5), a three-dimensional micro-motion platform (7) for holding the chip to be tested (6), and a test device (8) connected to the other end of the optical fiber circulator (3); The auxiliary light source (1) outputs visible light, the light source (2) is a broadband light source, the light transmission band of the beam collimator (5) includes the bands of the auxiliary light source (1) and the light source (2), the beam collimator (5) is perpendicular to the three-dimensional micro-motion platform (7), and the chip to be tested (6) is located at the center of the three-dimensional micro-motion platform (7); The optical fiber circulator (3) transmits the output light of the light source (2) to the optical splitter (4) and detects the thickness of the chip to be tested (6); the detection signal reflected back by the chip to be tested (6) reaches the demodulation device of the test device (8) after passing through the optical fiber circulator (3).

9. The optical chip thickness measuring device based on Fabry-Perot interferometry principle according to claim 8, Features: The testing device (8) comprises a demodulation device (81) and a computer (82) optically connected in sequence to one port of the optical fiber circulator (3); The optical fiber circulator (3) comprises an optical fiber circulator body (31) and a PORT1 port (32), a PORT2 port (33), and a PORT3 port (34) respectively connected to the optical fiber circulator body (31); the PORT1 port (32) is optically connected to the light source (2), the PORT2 port (33) is optically connected to a sub-end of the optical splitter (4), and the PORT3 port (34) is optically connected to the demodulation device (81); The optical splitter (4) is a 1*2 optical splitter including two sub-ends and one female end; The auxiliary light source (1) and the optical fiber circulator (3) are optically connected to a sub-end of the optical splitter (4) respectively; The three-dimensional micro-motion platform (7) can be adjusted in the x direction, the y direction, and the z direction.

10. The optical chip thickness measuring device based on Fabry-Perot interferometry principle according to claim 9, Features: The auxiliary light source (1) is a red light optical fiber test pen with a wavelength of 650 nm and can be adapted to an FC optical fiber interface; The optical splitter (4) is a PLC optical splitter, the female end is in the form of a pigtail, and the two female ends are FC / APC ferrule packages; The beam collimator (5) is a fiber collimator with a collimation angle of 0.1°; The refractive index of the chip to be tested (6) is a known constant, and the chip to be tested (6) is a transparent quartz chip or a sapphire chip; The demodulation device (81) is a spectrum demodulator, or a MOI demodulator can be used to replace the light source (2), the optical fiber circulator (3) and the demodulation device (81); The computer (82) comprises a computer case, a computer display and a computer host.

Citation Information

Patent Citations

  • Transparent material refractive index and thickness measuring device and measuring method based on spectrum interference

    CN103983609A

  • System for measuring film thickness by broadband-spectrum light interference method

    CN104034272A

  • Hollow photonic crystal fiber core size measuring device and method based on Fabry-Perot interference

    CN108645344A

  • Device and method for measuring glass tube wall based on time-domain spectral interference

    CN116772713A

  • Method and system for measuring optical and physical thicknesses of optically transparent object

    JP2004163438A