Reverse blocking insulated gate bipolar transistor
Through silicon wafer substrate bonding and separation diffusion technology, the collector structure of RB-IGBT is optimized, solving the problems of thickness and cost when blocking high voltage in the existing technology, and achieving low loss and flexible voltage optimization.
Patent Information
- Application Number
- CN202410401654.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-06
- Filing Date
- 2024-04-03
- Publication Date
- 2024-10-15
AI Technical Summary
The existing reverse blocking insulated gate bipolar transistor (RB-IGBT) has problems such as inappropriate thickness, high cost and complex structure when blocking high voltages, and it is difficult to optimize the boron separation diffusion structure for low voltage applications.
By bonding two silicon wafer substrates with different doping characteristics to form an aluminum or boron separation diffusion area, and forming a metal oxide semiconductor (MOS) structure and contact diffusion layer on the top surface, combined with the back metallization layer, Optimize collector layer thickness and diffusion characteristics.
It achieves effective blocking of reverse current at lower total loss and cost, is suitable for high-voltage applications, simplifies the manufacturing process, and improves the flexibility of voltage optimization.
Smart Images

Figure CN118782467A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates generally to the field of semiconductor devices, and more particularly to the fabrication of semiconductor devices, and even more particularly to reverse blocking insulated gate bipolar transistors. Background Art
[0002] An insulated gate bipolar transistor (IGBT) is a three-terminal power semiconductor device used as an efficient and fast electronic switch. It consists of four alternating layers (PNPN) controlled using a metal oxide semiconductor (MOS) gate structure. In most applications, IGBTs are used together with a fast anti-parallel diode to allow the inductive load current to flow freely. This means that high voltages never appear at the IGBT collector junction. However, in some applications (e.g., matrix converters, etc.), it may be necessary to block reverse current from flowing in the IGBT. This can be achieved using a series diode, but if the IGBT itself is able to block this current, there are savings in terms of lower overall losses, cost, and space.
[0003] Existing reverse blocking IGBTs (RB-IGBTs) generally require that their back collector junctions be able to block the full rated voltage of the semiconductor device. This means that a soft punch-through (SPT) structure with a collector-side buffer diffusion cannot be used. In addition, although existing RB-IGBTs include a non-punch-through (NPT) structure, this structure is not formed by wafer bonding, is too thick, and is difficult to optimize for a predetermined voltage (e.g., 1200V). In addition, although RB-IGBTs can be manufactured without separation diffusion, a back junction termination structure will be required, which is difficult and expensive to implement. In addition, some existing lower voltage RB-IGBTs have boron separation diffusions instead of aluminum separation diffusions, however, the driving time to form these structures is very long. Summary of the invention
[0004] In certain embodiments, the present subject matter relates to a method of manufacturing a reverse blocking insulated gate bipolar transistor (RB-IGBT). The method may include providing a first silicon wafer substrate and a second silicon wafer substrate, bonding the first silicon wafer substrate and the second silicon wafer substrate, forming one or more separation diffusion regions in the first silicon wafer substrate, forming one or more front metal oxide semiconductor (MOS) structures on a top surface of the first silicon wafer substrate, removing the second silicon wafer substrate, forming a contact diffusion layer on a bottom surface of the first silicon wafer substrate, and forming a back metallization layer on a bottom surface of the contact diffusion layer.
[0005] In certain embodiments, the present subject matter may include one or more of the following optional features. The first silicon wafer substrate may be an N-type doped silicon wafer substrate. The first silicon wafer substrate may have at least one of: a resistivity of about 40-120 ohm-cm, a thickness of about 150-300 μm, and any combination thereof.
[0006] In some embodiments, the second silicon wafer substrate may be a P-type doped silicon wafer substrate. The second silicon wafer substrate may have at least one of the following: a resistivity of about 0.1-10 ohm-cm, a thickness of about 200-500 μm, and any combination thereof. In some embodiments, the method may further include: polishing the second silicon wafer substrate. Alternatively or additionally, polishing may also include polishing the first wafer substrate (e.g., one or more sides thereof).
[0007] In some embodiments, the bonding of the first silicon wafer substrate and the second silicon wafer substrate may include diffusing one or more particles from the second silicon wafer substrate into the first silicon wafer substrate to form a diffusion region. The diffusion region may be a P-type diffusion region. One or more separation diffusion regions may be configured to at least partially merge with the diffusion region to form a junction. In addition, the formation of a contact diffusion layer may include forming a contact diffusion layer adjacent to the diffusion region. The contact diffusion layer may be a P-type contact diffusion layer. The contact diffusion layer may be formed between one or more separation diffusion regions. Alternatively or additionally, in some embodiments, the formation of a contact diffusion layer may include providing a pre-diffused first silicon wafer substrate.
[0008] In certain embodiments, the one or more separation diffusion regions may include at least one of: one or more aluminum separation diffusion regions, one or more boron separation diffusion regions, one or more P-type dopant separation diffusion regions, and / or any combination thereof.
[0009] In certain embodiments, one or more MOS structures may be formed between one or more separate diffusion regions on the top surface of the first silicon wafer substrate.
[0010] In some embodiments, the removing may include removing a wafer bonding layer formed by bonding. The removing may include at least one of: grinding, etching, and any combination thereof.
[0011] In some embodiments, the back metallization layer may include at least one of: an aluminum back metallization layer, a titanium back metallization layer, a nickel back metallization layer, a silver back metallization layer, a gold metallization layer, a metal back metallization layer, a metal oxide back metallization layer, and any combination thereof.
[0012] In certain embodiments, the present subject matter relates to a semiconductor device such as a RB-IGBT. The semiconductor device may include a first silicon wafer substrate having a diffusion region produced by bonding the first silicon wafer substrate to a second silicon wafer substrate. The second silicon wafer substrate may be removed. One or more dopant particles from the second silicon wafer substrate may be configured to diffuse into the first silicon wafer substrate. The device may also include one or more separate diffusion regions formed in the first silicon wafer substrate, one or more front metal oxide semiconductor (MOS) structures on the top surface of the first silicon wafer substrate, a contact diffusion layer formed on the bottom surface of the first silicon wafer substrate, and a back metallization layer formed on the bottom surface of the contact diffusion layer.
[0013] In certain embodiments, the present subject matter may include one or more of the following optional features. In a semiconductor device, the first silicon wafer substrate may be an N-type doped silicon wafer substrate. The diffusion region may be a P-type diffusion region. A contact diffusion layer may be formed adjacent to the diffusion region. The contact diffusion layer may be a P-type contact diffusion layer. The contact diffusion layer may be formed between one or more separation diffusion regions. Alternatively or additionally, the contact diffusion layer may be a pre-diffusion layer. In certain embodiments, one or more MOS structures may be formed between one or more separation diffusion regions on the top surface of the first silicon wafer substrate. The back metallization layer may include at least one of the following: an aluminum back metallization layer, a titanium back metallization layer, a nickel back metallization layer, a silver back metallization layer, a gold back metallization layer, a metal back metallization layer, a metal oxide back metallization layer, and any combination thereof.
[0014] The details of one or more variations of the subject matter described herein are set forth in the accompanying drawings and the description below. Other features and advantages of the subject matter described herein will be apparent from the description and drawings, and from the claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate certain aspects of the subject matter disclosed herein and, together with the description, help explain some principles associated with the disclosed embodiments.
[0016] Figure 1a -d illustrates an exemplary method for fabricating a semiconductor device according to some embodiments of the current subject matter; and
[0017] Figure 2 An example method for fabricating a semiconductor device according to some implementations of the current subject matter is shown.
[0018] The drawings are not necessarily drawn to scale. The drawings are merely representations and are not intended to depict specific parameters of the present disclosure. The drawings are intended to depict exemplary embodiments of the present subject matter and should not be considered limiting of the scope. In the drawings, the same reference numerals represent the same elements.
[0019] In addition, for the sake of clarity, some elements in some of the figures may be omitted and / or not shown to scale. For the sake of clarity, the cross-sectional views may be in the form of "slices" and / or "close-up" cross-sectional views, omitting some background lines that would be visible in a "true" cross-sectional view. In addition, for the sake of clarity, some reference numerals may be omitted in some of the figures. DETAILED DESCRIPTION
[0020] Various methods according to the present disclosure will be described more fully below with reference to the accompanying drawings, in which embodiments of the systems and methods are shown. Devices, one or more systems, one or more components, etc. may be embodied in many different forms and should not be construed as being limited to the example embodiments set forth herein. Rather, these example embodiments are provided so that the present disclosure will be thorough and complete and will fully convey the scope of the current subject matter to those skilled in the art.
[0021] To address these and potential other deficiencies of currently available solutions, one or more embodiments of the present subject matter are directed to methods, systems, articles of manufacture, etc., and these methods, systems, articles of manufacture, etc., can provide, among other possible advantages, systems and methods for manufacturing semiconductor devices, and in particular, systems and methods for manufacturing reverse blocking insulated gate bipolar transistors (IGBTs).
[0022] As mentioned above, the IGBT consists of four alternating P, N layers controlled by a MOS gate structure. The IGBT cell has a structure similar to an n-channel vertical structure power MOSFET, however, the n+ drain is replaced by a p+ collector layer, forming a vertical PNP bipolar junction transistor. The p+ region creates a cascade connection of the PNP bipolar junction transistor with the surface n-channel MOSFET. The IGBT structure is also similar to a MOS gate thyristor, however, the thyristor action is suppressed and only transistor action is allowed throughout the device operating range. IGBTs are designed to synthesize complex waveforms through pulse width modulation and low-pass filters, and can be used in switching amplifiers (e.g., sound systems, industrial control systems, etc.).
[0023] The reverse blocking IGBT (RB-IGBT) is a bidirectional switch with a specific IGBT capable of sustaining voltage in both directions. In particular, the RB-IGBT is an IGBT in non-punch-through (NPT) technology with an additional isolation p+ region that is capable of sustaining reverse voltage without degrading reverse leakage current performance. The forward on-state voltage and conduction losses are lower than the bidirectional switch structure of the IGBT and external blocking diode combination. The RB-IGBT blocking diode is optimized for low on-state voltage. In addition, the reverse recovery current of the internal diode and the conduction losses of the IGBT are larger in the 1200V range.
[0024] In some cases, the optimum silicon thickness for 1200V class RB-IGBTs is around 170μm. This is the minimum thickness that can reliably block 1200V with an NPT structure. Large diameter 170μm thick wafers are too brittle to be fully processed in standard wafer manufacturing processes. Standard low voltage (1200V) soft punch-through (SPT) IGBTs use some of the following manufacturing solutions. One of these solutions involves using an epitaxial layer with the required properties deposited on a wafer substrate. Near the end of the process, the substrate can be thinned or removed by grinding and etching. However, wafers with 170μm epitaxial layers are too expensive to provide a practical solution for 1200V RB-IGBTs. In practice, the RB-IGBT epilayer may need to be thicker to allow the collector to diffuse upward during separation diffusion.
[0025] Another manufacturing solution involves processing a wafer of standard processing thickness with the desired N-type drift resistivity to near completion and then thinning it (e.g., using grinding and / or etching) to an optimal thickness. The collector layer can then be implanted into the back side of the wafer and activated. However, such a thin implanted collector layer is not suitable for supporting high reverse voltages.
[0026] In RB-IGBTs, the process can start with an N-type wafer with a deep diffused P+ (e.g., boron) layer, where the tail of the diffusion can form the collector layer after grinding. It should be noted that existing SPT IGBTs can start with a wafer with a deep N+ diffusion, where the tail of the diffusion can form the buffer after grinding. However, this approach lacks flexibility and the tail is very lightly doped. This optical collector layer may need to be deep to block the full voltage, resulting in high losses and control of the collector layer injection efficiency may be poor.
[0027] In certain embodiments, in order to address the above-mentioned shortcomings of conventional processes, the present subject matter relates to a wafer bonding process for manufacturing rubidium IGBTs. The process can start with two wafer substrates having different doping characteristics. For example, one wafer substrate can be a P-type wafer, which can be removed at a later stage of the process. The other wafer substrate can be an N-type wafer. The wafers are then bonded together. The bonding can be completed in a desired manner. As discussed herein, the final RB-IGBT device can be completed as a result of the bonding of these two wafer substrates.
[0028] In some exemplary non-limiting embodiments, the P-type wafer substrate may have a predetermined thickness to provide suitable mechanical support during standard front-side processing (e.g., creating MOS structures, etc.). For example, it may have a boron concentration that may be used as a suitable diffusion source for the collector layer of the RB-IGBT. The collector layer diffusion may occur during the aluminum separation diffusion thermal cycle.
[0029] The N-type wafer substrate may have a predetermined resistivity, which may be selected for the RG-IGBT drift layer. After bonding the two wafers, the thickness of the resulting layer may be adjusted by grinding and / or etching. In some exemplary non-limiting embodiments, for a 1200V RB-IGBT, the final N-type drift layer may have a thickness of approximately 170 μm, which may account for the upward diffusion of the collector layer. It is understood that any other thickness of layer may be used. In addition, the current subject process may be applied to the manufacture of any other type of semiconductor device.
[0030] In some embodiments, an aluminum separation diffusion may be used to bring the collector junction to the top surface for termination (e.g., which may be accomplished in any desired manner, such as using a guard ring, etc.). During separation, drive step boron may also diffuse upward from the substrate to form the collector layer. The final collector layer configuration may be controlled by selecting the substrate doping concentration and / or the final target thickness of the semiconductor device.
[0031] After separation diffusion, the front side of the wafer can be polished to a standard compatible with MOS processing. Standard front side IGBT processing can also be followed. When completed, the substrate silicon can be completely removed by grinding (e.g., TAIKO, full surface and / or any other type of process) and / or etching through the wafer bonding and into the collector diffusion area. The process can be completed with back side metallization. Back side contact implantation and / or annealing can be added before metallization to improve collector contact and implantation efficiency.
[0032] Figure 1a-d shows an exemplary method 100 for manufacturing a semiconductor device (shown in a two-dimensional view) according to some embodiments of the current subject matter. The method 100 can be used to manufacture an exemplary insulated gate bipolar transistor (IGBT), in particular a reverse blocking IGBT (RB-IGBT). It is understood that the method 100 can be used to manufacture any other type of semiconductor device.
[0033] refer to Figure 1a , a first wafer substrate 102 and a second wafer substrate 104 may be provided. The first wafer substrate 102 may be an N-type device silicon wafer substrate. The second wafer substrate 104 may be a P-type device silicon wafer substrate. The top surface of the first wafer substrate 102 may correspond to a front side 108 of a semiconductor device to be formed by the method 100. The bottom surface of the second wafer substrate 104 may correspond to a back side 110, which may be removed at a stage during the method 100.
[0034] The first wafer substrate 102 may be bonded to the second wafer substrate 104 using wafer bonding 106. The bonding between the first wafer substrate 102 and the second wafer substrate 104 may be accomplished using any desired method.
[0035] In some exemplary non-limiting embodiments, for the purpose of manufacturing a 1200V RB-IGBT, the first wafer substrate 102 (e.g., a device wafer) can be doped with a phosphorus resistivity dopant with a resistivity in the range of about 40-120 ohm-cm (e.g., about 60 ohm-cm). The first wafer substrate 102 can have a thickness in the range of about 150-300 μm (e.g., about 220 μm). In addition, for the purpose of wafer bonding, the first wafer substrate 102 can be polished on one side. The resistivity of the first wafer substrate 102 can be configured to support about 1200V in a non-punch-through mode.
[0036] The second wafer substrate 104 (e.g., the wafer substrate to be removed during the final grinding stage) can be doped with a boron resistivity dopant having a resistivity in the range of approximately 0.1-10 ohm-cm (e.g., approximately 1 ohm-cm). The second wafer substrate 104 can have a thickness in the range of approximately 200-500 μm (e.g., approximately 300 μm). The second wafer substrate 104 can also be polished on one side for wafer bonding. Such polishing can be configured to remove approximately 10-20 μm. The resistivity of the second wafer substrate 104 can be configured to determine one or more properties of the collector, such as concentration, depth, etc., which may originate from dopants (e.g., boron) diffused into the substrate 102 during the separation diffusion thermal cycle.
[0037] The bonding of the two wafer substrates 102, 104 can be configured to produce a bonded wafer having a thickness in the range of about 300-650 μm (e.g., about 500 μm, which may depend on the wafer diameter and wafer manufacturing process capabilities). As part of the wafer bonding process, both wafer substrates 102, 104 can have polished sides facing each other for bonding purposes. The wafer substrates 102, 104 can be cleaned and contacted underwater for bonding. The bonded wafers can also be annealed to improve the strength of the wafer bond 106.
[0038] refer to Figure 1b , a collector or P-type diffusion layer 112 and a separation diffusion region 114 (a, b) may be formed. In some example embodiments, the separation diffusion region 114 may be configured to merge with the collector diffusion layer 112 to form and / or bring an unbroken junction to the top surface, wherein the junction may be configured to have a suitable concentration capable of supporting a predetermined voltage (e.g., 1200V). One or more factors (e.g., drive time, temperature, etc.) may be used to define, influence, and / or configure the processes involved in the formation of the separation diffusion and / or P-type diffusion regions / layers, which in turn may be used to determine various aspects of the formed regions / layers and / or portions thereof, such as the depth of the P-type diffusion layer 112. The P-type diffusion layer 112 may be configured to be formed when boron particles are diffused from the second wafer substrate 104 into the first wafer substrate 102. The diffusion region 114 and / or the collector diffusion layer 112 may be formed simultaneously and / or substantially simultaneously. Alternatively or additionally, the formation of the region 114 and the layer 112 may be completed in a predetermined order. In addition, one or more configuration parameters (e.g., depth, concentration, etc.) of the collector diffusion layer 112 can be determined and / or controlled by the resistivity of the wafer substrate 104 and / or the extent to which the wafer substrate 104 is ground and / or etched during the method 100. Alternatively or additionally, the first wafer substrate 102 can be pre-diffused, whereby the tail end of the substrate 102 can be configured to form a collector. In this case, the second wafer substrate (and the processes associated with the second wafer substrate) may not be necessary (e.g., can be omitted from the process), and other processes associated with the first wafer substrate as described herein (e.g., forming a separate diffusion region, back grinding, etc.) can be performed. The P-type diffusion in the pre-diffused first wafer substrate 102 can have a sufficient depth to provide a robust overall thickness.
[0039] In some example, non-limiting embodiments, the diffusion region 114 can be formed by evaporating aluminum onto an N-type surface (i.e., the first wafer substrate 102) and patterning it using photolithography, wherein the aluminum is diffused in selected areas. Alternatively or additionally, boron and / or any other P-type dopant can be used to form a separate diffusion region. For example, such a separate diffusion region may be useful in lower voltage applications. In some example, non-limiting embodiments, the aluminum diffusion can be configured to extend to meet the dopant (e.g., boron) diffused into the first wafer substrate 102 from the second wafer substrate 104, thereby bringing the back side 110 (corresponding to the collector layer of the IGBT) junction to the top surface. The aluminum diffusion can also be configured to completely surround the active portion of the IGBT device (due to Figure 1a -d shows a two-dimensional view of the semiconductor device, it should be noted that the diffusion region 114 forms a single diffusion region surrounding / surrounding the IGBT device). In some exemplary non-limiting embodiments, the aluminum diffusion can be completed using ion implantation and / or thermal drive. The aluminum diffusion can be completed using a temperature range of about 1200°C-1350°C (e.g., about 1250°C) within a predetermined time period, such as about 60 hours (for 1250°C). It will be appreciated that any other temperature and / or time period is possible.
[0040] As a non-limiting example, the boron diffusion into the first wafer substrate 102 may be an approximately 20 μm deep junction, which may correspond to the thickness of the P-type diffusion layer 112. The diffusion may be configured to form a collector layer diffusion for a RB-IGBT device, resulting in a blocking junction characterized by appropriate concentration, thickness, and / or quality parameters capable of blocking voltages greater than approximately 1200 V with low defectivity. In some exemplary non-limiting embodiments, the diffusion layer 112 may also be configured to be suitable for an IGBT collector and / or for hole injection efficiency, which may be adjusted for desired performance and / or end-user applications.
[0041] refer to Figure 1c , one or more front side MOS structures 116 may be added to the front side 108 of the semiconductor device produced by the method 100. The structures may be added after the front side 108 is polished.
[0042] In some exemplary non-limiting embodiments, the residual aluminum (resulting from the formation of one or more separation diffusion regions 114) can be etched away, and the wafer polishing can be performed to produce a top surface suitable for any MOS and / or termination processing. For example, such etching and / or water polishing can be configured to remove approximately 10 μm of material. In addition, MOS processing can include adding one or more trenches, planar gates, and / or performing any other standard MOS processing. In some exemplary non-limiting embodiments, MOS processing can include gate and / or emitter contact metallization, which can be suitable for wire bonding connections and / or any other operations.
[0043] Additionally, junction termination structures may be located between any active MOS features that have been added and the diffusion region 114 (eg, guard ring, passivation layer). The junction termination structures may be used to support forward and / or reverse blocking voltages.
[0044] refer to Figure 1d , backside processing may be performed as some final stages of the method 100 for producing a semiconductor device 120 (eg, a RB-IGBT). Figure 1d As part of the processing shown in , the second wafer substrate 104 can be removed. The removal of the second wafer substrate 104 can be accomplished by grinding. In some exemplary non-limiting embodiments, the removal of the second wafer substrate 104 can be the complete removal of the wafer substrate 104 including any bonding (e.g., wafer bonding layer 106) between the first wafer substrate 102 and the second wafer substrate 104. The grinding of the second wafer substrate 104 can also include removing any silicon crystal damage (e.g., silicon crystal damage) that may be associated with the creation of the wafer bonding layer 106. Figure 1a shown).
[0045] The grinding of the second wafer substrate 104 may also be followed by a backside etching process. This process may also remove any remaining damage that may have been caused by the grinding of the second wafer substrate 104. In some exemplary non-limiting embodiments, etching may include removing approximately 10-15 μm of material. Once removed, the thickness of the remaining device may be in the range of approximately 150-300 μm (e.g., approximately 190 μm).
[0046] After the above process, the P+ contact layer 124 can be created by performing a back contact implant and anneal. This may be advantageous in improving the contact with the back metallization layer 126 and the efficiency of the back collector 130. The metallization layer 126 can then be added to the back side of the contact layer 124. The metallization layer 126 can be used for solder contact (e.g., with a printed circuit board, electronic components, etc.). The metallization layer 126 can be made of at least one of the following materials: aluminum, titanium, nickel, silver, gold and / or any other metal and / or metal component, and / or any combination thereof. The method 100 can be accomplished with various standard semiconductor device manufacturing processes, such as wafer probing, dicing, assembly, soldering to the substrate of a semiconductor package, etc.
[0047] Figure 2 An example method 200 for manufacturing a semiconductor device according to some embodiments of the current subject matter is shown. The method 200 can be used to manufacture a semiconductor device 120 (e.g., an insulated gate bipolar transistor semiconductor device, more specifically, a reverse blocking insulated gate bipolar transistor semiconductor device) (e.g., Figure 1d shown).
[0048] At 202, a first silicon wafer substrate and a second silicon wafer substrate may be provided. The first silicon wafer substrate (eg, substrate 102) may be an N-type doped silicon wafer substrate. The second silicon wafer substrate (eg, substrate 104) may be a P-type doped silicon wafer substrate.
[0049] The first silicon wafer substrate and the second silicon wafer substrate may be bonded together at 204. A wafer bond (eg, wafer bonding layer 106) may be created.
[0050] At 206, one or more separate diffusion regions (e.g., regions 114a and 114b) may be formed in the first silicon wafer substrate. In addition, as a result of the bonding of the first silicon wafer layer to the second silicon wafer layer, a P-type diffusion layer (e.g., layer 112) may be formed in the first silicon wafer layer. As described above, region 114 may be merged with layer 112 to form and / or bring an uninterrupted junction to the top surface. The junction may have a suitable concentration capable of supporting a predetermined voltage (e.g., 1200V). As described above, one or more factors may be used to configure various aspects of the formed regions / layers and / or portions thereof. For example, the depth of the P-type diffusion layer 112 may be configured based on, for example, drive time, temperature, and / or any other factor and / or any combination thereof. As discussed herein, the formation of region 114 and layer 112 may be accomplished simultaneously, substantially simultaneously, in a predetermined order, and / or in any other manner. One or more configuration parameters of the layer 112, such as depth, concentration, etc., may depend on the resistivity of the wafer substrate 104, the grinding / etching of the wafer substrate 104, and / or any other factors. Alternatively or additionally, a pre-diffused first wafer substrate 102 may be used, the tail end of which may form the collector, and as described above, the second wafer substrate and related processes may be omitted while other operations (e.g., forming a separate diffusion region, back grinding, etc.) may be performed.
[0051] One or more front side metal oxide semiconductor (MOS) structures may be formed on the top surface of the first silicon wafer substrate at 208. The MOS structures may be formed between the isolated diffusion regions and / or may be surrounded by the isolated diffusion regions (on the top surface of the first silicon wafer substrate).
[0052] The second silicon wafer substrate layer and the wafer bonding layer may be removed at 210. The removal of the second silicon wafer substrate layer and / or the wafer bonding layer may be accomplished using grinding, etching, and / or any other suitable process and / or any combination thereof.
[0053] At 212, a P-type contact diffusion layer may be formed on the bottom surface of the first silicon wafer substrate. The P-type contact diffusion layer (e.g., layer 124) may be formed adjacent to the P-type diffusion layer (e.g., layer 112). The P-type contact diffusion layer may be configured to span between two separation diffusion layers. As described above, it may be configured to improve contact with a subsequently formed back metallization layer.
[0054] At 214, a backside metallization layer (eg, layer 126) may be formed on the bottom surface of the P-type contact diffusion layer to form a semiconductor device. This allows the semiconductor device to be coupled to one or more electronic components, printed circuit boards, semiconductor packages, and the like.
[0055] The components and features of the above devices may be implemented using any combination of discrete circuits, application specific integrated circuits (ASICs), logic gates, and / or single chip architectures. In addition, where appropriate, the features of the devices may be implemented using microcontrollers, programmable logic arrays, and / or microprocessors, or any combination of the above. It should be noted that hardware, firmware, and / or software elements may be collectively or individually referred to herein as "logic" or "circuitry."
[0056] It should be understood that the exemplary devices shown in the above block diagrams can represent a functional descriptive example of many potential implementations. Therefore, the division, omission or inclusion of block functions depicted in the drawings does not mean that the hardware components, circuits, software and / or elements used to implement these functions must be divided, omitted or included in the embodiments.
[0057] Certain embodiments may be described using "one embodiment" or "an embodiment" and their derivatives. These terms mean that a particular feature, structure, or characteristic described in conjunction with the embodiment is included in at least one embodiment. The phrase "in one embodiment" (or its derivatives) appearing in various places in the specification does not necessarily refer to the same embodiment. In addition, unless otherwise stated, the above-mentioned features are identified as being usable together in any combination. Therefore, any features discussed separately can be used in combination with each other unless it is noted that the features are incompatible with each other.
[0058] It should be emphasized that the abstract of the present disclosure is provided to allow the reader to quickly determine the nature of the technical disclosure. The present disclosure is submitted based on the understanding that the present disclosure will not be used to interpret or limit the scope or meaning of the claims. In addition, in the previous detailed description, it can be seen that various features are combined together in a single embodiment for the purpose of simplifying the present disclosure. This disclosure method should not be interpreted as reflecting the intention that the claimed embodiment requires more features than the features explicitly recited in each claim. On the contrary, as reflected in the following claims, the subject matter of the invention does not lie in all the features of a single disclosed embodiment. Therefore, the following claims are incorporated into the detailed description, and each claim is independently a separate embodiment. In the appended claims, the terms "including" and "in which" are used as the plain English equivalents of the corresponding terms "comprising" and "wherein", respectively. In addition, the terms "first", "second", "third", etc. are used only as labels and are not intended to impose numerical requirements on their objects. Furthermore, the use of "including," "comprising," or "having," and variations thereof herein are intended to encompass the items listed thereafter and equivalents thereof as well as additional items. Thus, the terms "including," "comprising," or "having," and variations thereof, are open-ended expressions and are used interchangeably herein.
[0059] The foregoing includes examples of the disclosed architecture. Of course, it is not possible to describe every conceivable combination of components and / or methods, but one of ordinary skill in the art will recognize that many further combinations and permutations are possible. Therefore, the novel architecture is intended to embrace all such changes, modifications and variations that fall within the spirit and scope of the appended claims.
[0060] For the purpose of illustration and description, the above description of example embodiments is given. It is not intended to be exhaustive or to limit the present disclosure to the precise form disclosed. Many modifications and variations are possible according to the present disclosure. It is intended that the scope of the present disclosure is not limited by this detailed description, but by the appended claims. Applications filed in the future claiming priority to the present application may claim the disclosed subject matter in different ways, and may generally include any set of one or more limitations disclosed differently or otherwise demonstrated herein.
[0061] All directional references (e.g., proximal, distal, up, down, upward, downward, left, right, lateral, longitudinal, front, back, top, bottom, above, below, vertical, horizontal, radial, axial, clockwise, and counterclockwise) are used for identification purposes only to assist the reader in understanding the present disclosure and are not intended to be limiting, particularly with respect to the location, orientation, or use of the present disclosure. Unless otherwise indicated, connection references (e.g., attached, coupled, connected, and combined) are to be understood broadly and may include intermediate members between a collection of elements and relative movement between elements. Thus, connection references do not necessarily mean that two elements are directly connected and have a fixed relationship to each other.
[0062] Furthermore, identifying references (e.g., primary, secondary, first, second, third, fourth, etc.) does not imply importance or priority, but is used to distinguish one feature from another. The drawings are for illustration purposes only, and the size, position, order, and relative sizes reflected in the drawings may vary.
[0063] The scope of the present disclosure is not limited by the specific embodiments described herein. In fact, in addition to those described herein, various other embodiments and modifications of the present disclosure will be apparent to those of ordinary skill in the art based on the foregoing description and drawings. Therefore, such other embodiments and modifications are intended to fall within the scope of the present disclosure. In addition, the present disclosure has been described herein in the context of a specific embodiment in a specific environment for a specific purpose. Those of ordinary skill in the art will recognize that validity is not limited thereto, and the present disclosure can be advantageously implemented in any number of environments for any number of purposes. Therefore, the claims set forth below should be interpreted in light of the full scope and spirit of the present disclosure as described herein.
Claims
1. A method, include: Providing a first silicon wafer substrate and a second silicon wafer substrate; Bonding the first silicon wafer substrate and the second silicon wafer substrate; forming one or more separate diffusion regions in the first silicon wafer substrate; forming one or more front side metal oxide semiconductor (MOS) structures on a top surface of the first silicon wafer substrate; removing the second silicon wafer substrate; forming a contact diffusion layer on a bottom surface of the first silicon wafer substrate; as well as A backside metallization layer is formed on a bottom surface of the contact diffusion layer.
2. The method according to claim 1, in, The first silicon wafer substrate is an N-type doped silicon wafer substrate.
3. The method according to claim 2, in, The first silicon wafer substrate has at least one of: a resistivity of about 40-120 ohm-cm, a thickness of about 150-300 μm, and any combination thereof.
4. The method according to claim 1, in, The second silicon wafer substrate is a P-type doped silicon wafer substrate.
5. The method according to claim 4, in, The second silicon wafer substrate has at least one of: a resistivity of about 0.1-10 ohm-cm, a thickness of about 200-500 μm, and any combination thereof.
6. The method according to claim 4, further comprising polishing the second silicon wafer substrate.
7. The method of claim 1, wherein bonding the first silicon wafer substrate and the second silicon wafer substrate comprises diffusing one or more particles from the second silicon wafer substrate into the first silicon wafer substrate to form a diffusion region.
8. The method according to claim 7, in, The diffusion region is a P-type diffusion region.
9. The method according to claim 7, in, The one or more separate diffusion regions are configured to at least partially merge with the diffusion region to form a junction.
10. The method according to claim 7, in, Forming the contact diffusion layer includes forming the contact diffusion layer adjacent to the diffusion region.
11. The method according to claim 10, in, The contact diffusion layer is a P-type contact diffusion layer.
12. The method according to claim 10, in, The diffusion region is formed between the one or more separate diffusion regions.
13. The method of claim 10, wherein forming the contact diffusion layer comprises providing a pre-diffused first silicon wafer substrate.
14. The method according to claim 1, in, The one or more separation diffusion regions include at least one of the following: one or more aluminum separation diffusion regions, one or more boron separation diffusion regions, one or more P-type dopant separation diffusion regions, and any combination thereof.
15. The method according to claim 1, in, The one or more MOS structures are formed between the one or more separate diffusion regions on the top surface of the first silicon wafer substrate.
16. The method according to claim 1, in, The removing includes removing a wafer bonding layer formed by the bonding.
17. The method according to claim 1, in, The removing includes at least one of the following: grinding, etching and any combination thereof.
18. The method according to claim 1, in, The back metallization layer includes at least one of the following: an aluminum back metallization layer, a titanium back metallization layer, a nickel back metallization layer, a silver back metallization layer, a gold metallization layer, a metal back metallization layer, a metal oxide back metallization layer and any combination thereof.
19. A semiconductor device, include: a first silicon wafer substrate having a diffusion region resulting from bonding the first silicon wafer substrate to a second silicon wafer substrate, wherein the second silicon wafer substrate is removed, wherein one or more dopant particles from the second silicon wafer substrate are configured to diffuse into the first silicon wafer substrate; one or more separate diffusion regions formed in the first silicon wafer substrate; one or more front side metal oxide semiconductor (MOS) structures on a top surface of said first silicon wafer substrate; a contact diffusion layer formed on a bottom surface of the first silicon wafer substrate; as well as A backside metallization layer is formed on a bottom surface of the contact diffusion layer.
20. The semiconductor device according to claim 19, in, The first silicon wafer substrate is an N-type doped silicon wafer substrate.
21. The semiconductor device according to claim 19, in, The diffusion region is a P-type diffusion region.
22. The semiconductor device according to claim 19, in, The contact diffusion layer is formed adjacent to the diffusion region.
23. The semiconductor device according to claim 22, in, The contact diffusion layer is a P-type contact diffusion layer.
24. The semiconductor device according to claim 22, in, The contact diffusion layer is formed between the one or more separation diffusion regions.
25. The semiconductor device according to claim 19, in, The contact diffusion layer is a pre-diffusion layer.
26. The semiconductor device according to claim 19, in, The one or more MOS structures are formed between the one or more separate diffusion regions on the top surface of the first silicon wafer substrate.
27. The semiconductor device according to claim 19, in, The back metallization layer includes at least one of the following: an aluminum back metallization layer, a titanium back metallization layer, a nickel back metallization layer, a silver back metallization layer, a gold back metallization layer, a metal back metallization layer, a metal oxide back metallization layer and any combination thereof.